Highly reliable, low-defect semiconductor light-emitting device and method for manufacturing same

The semiconductor light emitting device incorporates a protective layer and current limiting insulating layer to address manufacturing defects, enhancing reliability and reducing costs by preventing scratches and dirt, thus improving performance.

JP7573053B2Active Publication Date: 2024-10-24SUZHOU EVERBRIGHT PHOTONICS CO LTD +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2022579921
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-03-04
Filing Date
2022-07-20
Publication Date
2024-10-24
Estimated Expiration
2042-07-20

AI Technical Summary

Technical Problem

Conventional semiconductor light emitting devices face challenges in achieving both high reliability and low process cost, with defects such as scratches and dirt introduced during manufacturing leading to reduced device performance.

Method used

A semiconductor light emitting device design featuring a protective layer on the edge region of the doped semiconductor contact layer, with the surface electrode layer positioned lower than the protective layer, and a current limiting insulating layer to prevent external damage and current leakage.

Benefits of technology

The design enhances device reliability by preventing defects and reducing manufacturing complexity while maintaining low costs, thereby improving carrier mobility and reducing optical damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573053000001
    Figure 0007573053000001
  • Figure 0007573053000002
    Figure 0007573053000002
  • Figure 0007573053000003
    Figure 0007573053000003
Patent Text Reader

Abstract

A highly reliable and low-defect semiconductor light-emitting device and a method for manufacturing the same, comprising: a semiconductor substrate layer; an active layer located on the semiconductor substrate layer; a doped semiconductor contact layer located on a side of the active layer away from the semiconductor substrate layer and including a first region and an edge region surrounding the first region; a protective layer located on the edge region of the doped semiconductor contact layer away from the active layer; and a surface electrode layer located on the first region away from the active layer, wherein an upper surface of the surface electrode layer in the first region is lower than an upper surface of the protective layer. The semiconductor light-emitting device achieves both high reliability and low process costs.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application relates to the field of semiconductors, and more particularly to highly reliable, low defect semiconductor light emitting devices and methods for fabricating same.

[0002] This application claims priority to a Chinese patent application filed with the China Patent Office on March 4, 2022, bearing application number 202210205786.5 and entitled "High-reliability, low-defect semiconductor light-emitting device and its manufacturing method," the entire contents of which are incorporated herein by reference. [Background technology]

[0003] A semiconductor light emitting device uses a specific semiconductor material as the operating material to generate stimulated emission, and its operating principle is as follows: A specific excitation method is used to realize a particle number inversion of non-equilibrium carriers between the energy bands (conduction band and valence band) of the semiconductor material, or between the energy band of the semiconductor material and the impurity (acceptor or donor) level, and stimulated emission occurs when a large number of electrons and holes in the particle number inversion state recombine; such semiconductor light emitting devices are widely used due to their small volume and high electrical-to-optical conversion efficiency.

[0004] Conventional defect optimization techniques for the surface of semiconductor light-emitting devices have difficulty in achieving both improved reliability and reduced process costs. Summary of the Invention [Problem to be solved by the invention]

[0005] Therefore, the technical problem that this application aims to solve is to solve the problem in the conventional technology that it is difficult to achieve both high reliability and low process costs, and to provide a highly reliable, low-defect semiconductor light-emitting device and a manufacturing method thereof. [Means for solving the problem]

[0006] The present application provides a highly reliable and low-defect semiconductor light-emitting device comprising: a semiconductor substrate layer; an active layer located on the semiconductor substrate layer; a doped semiconductor contact layer located on a side of the active layer away from the semiconductor substrate layer and including a first region and an edge region surrounding the first region; a protective layer located on a side of the edge region of the doped semiconductor contact layer away from the active layer; and a surface electrode layer located on the first region away from the active layer, wherein an upper surface of the surface electrode layer in the first region is lower than an upper surface of the protective layer.

[0007] Optionally, the difference in height between the upper surface of the protective layer and the upper surface of the front electrode layer located in the first region is 0.05 μm to 5 μm.

[0008] Optionally, the protective layer has a thickness in a direction perpendicular to the surface of the semiconductor substrate layer of 0.1 μm to 5 μm.

[0009] Optionally, the high-reliability, low-defect semiconductor light-emitting device has opposite front and rear cavity surfaces, the front and rear cavity surfaces both exposing a sidewall surface of the active layer and a sidewall surface of the doped semiconductor contact layer, the protective layer includes opposite first and second sub-protective regions, the first and second sub-protective regions are arranged along a light emission direction, an outer wall of the first sub-protective region is flush with the exposed sidewall surface of the active layer of the front cavity surface and the exposed sidewall surface of the doped semiconductor contact layer of the front cavity surface, and an outer wall of the second sub-protective region is flush with the exposed sidewall surface of the active layer of the rear cavity surface and the exposed sidewall surface of the doped semiconductor contact layer of the rear cavity surface.

[0010] Optionally, the material of the doped semiconductor contact layer is a first body semiconductor material doped with a first conductive ion and the material of the protective layer is an undoped second body semiconductor material, or the material of the protective layer is a second body semiconductor material doped with a second conductive ion having a conductivity type opposite to that of the first conductive ion, or the material of the protective layer is a second body semiconductor material doped with a second conductive ion having a conductivity type the same as that of the first conductive ion and a doping concentration of the second conductive ion less than that of the first conductive ion.

[0011] When the conductivity type of the second conductive ions is the same as that of the first conductive ions, the doping concentration of the second conductive ions is 10 times that of the first conductive ions. -6 Times to 10 -1 It is double.

[0012] Optionally, the average lattice mismatch between said second body semiconductor material and said first body semiconductor material is less than or equal to 1%.

[0013] Optionally, the second body semiconductor material is the same as the first body semiconductor material.

[0014] Optionally, the protective layer is a single layer or a multi-layer structure.

[0015] Optionally, when the semiconductor substrate layer is a GaAs substrate, the material of the protective layer is doped or undoped GaAs, doped or undoped AlGaAs, doped or undoped InGaP, doped or undoped InGaAsP, or doped or undoped InGaAs; when the material of the semiconductor substrate layer is an InP substrate, the material of the protective layer is doped or undoped InGaAsP, doped or undoped InGaAlAs, doped or undoped InGaAs, doped or undoped InAlAs, or doped or undoped InP; when the material of the semiconductor substrate layer is a GaN substrate, the material of the protective layer is doped or undoped AlGaN, doped or undoped GaN, or doped or undoped InAlGaN.

[0016] Optionally, the surface electrode layer is located on a side of the protective layer away from the doped semiconductor contact layer and further includes a current limiting insulating layer located on the protective layer between the surface electrode layer and the protective layer and on a side of the edge of the first region away from the active layer.

[0017] Optionally, the doped semiconductor contact layer includes a first subdoped semiconductor layer and a second subdoped semiconductor layer located on a surface of the first subdoped semiconductor layer facing away from the active layer, the second subdoped semiconductor layer having a doping concentration greater than the doping concentration of the first subdoped semiconductor layer.

[0018] Optionally, the doping concentration of the second sub-doped semiconductor layer is between 10 and 50 times higher than the doping concentration of the first sub-doped semiconductor layer.

[0019] Optionally, the semiconductor device may further include an upper waveguide layer located between the doped semiconductor contact layer and the active layer, an upper confinement layer located between the upper waveguide layer and the doped semiconductor contact layer, a lower waveguide layer located between the active layer and a semiconductor substrate layer, a lower confinement layer located between the lower waveguide layer and a semiconductor substrate layer, and a back electrode layer located on the surface of the semiconductor substrate layer away from the active layer.

[0020] The present application further provides a method for manufacturing a high-reliability and low-defect semiconductor light-emitting device, comprising the steps of providing a semiconductor substrate layer; forming an active layer on the semiconductor substrate layer; forming a doped semiconductor contact layer on a side of the active layer away from the semiconductor substrate layer, the doped semiconductor contact layer including a first region and an edge region surrounding the first region; forming a protective layer on a side of the edge region of the doped semiconductor contact layer away from the active layer; and forming a surface electrode layer on a side of the first region away from the active layer, wherein an upper surface of the surface electrode layer in the first region is lower than an upper surface of the protective layer.

[0021] Optionally, the step of forming the protective layer includes epitaxially growing an initial protective layer on the side of the first region and the edge region away from the active layer, and etching away the initial protective layer in the first region to form a protective layer exposing a surface of the first region.

[0022] Optionally, the doped semiconductor contact layer and the initial protective layer are formed in sequence in the same epitaxial process.

[0023] Optionally, before forming the surface electrode layer, a protective layer and a current-limiting insulating layer located on a side of a portion of the first region edge away from the active layer are formed, and in the step of forming the surface electrode layer, the surface electrode layer is also formed on the side of the current-limiting insulating layer away from the protective layer.

[0024] Optionally, the step of forming the doped semiconductor contact layer includes forming a first sub-doped semiconductor layer on a side of the active layer away from the semiconductor substrate layer, and forming a second sub-doped semiconductor layer on a surface of the first sub-doped semiconductor layer away from the active layer, the second sub-doped semiconductor layer having a doping concentration greater than a doping concentration of the first sub-doped semiconductor layer.

[0025] Optionally, before forming the surface electrode layer, the number of first regions is multiple, and there is a cutting region between the peripheral edge regions of different first regions, and the method further includes cutting the surface electrode layer, the current limiting insulating layer, the protective layer, the doped semiconductor contact layer, the active layer and the semiconductor substrate layer along the cutting region. Effect of the Invention

[0026] The technical solution of the present application has the following beneficial effects: The high-reliability, low-defect semiconductor light-emitting device according to the technical solution of the present application includes a protective layer located on the edge region of the doped semiconductor contact layer away from the active layer, the protective layer being used to raise the edge region of the doped semiconductor contact layer, so that the upper surface of the front electrode layer in the first region is lower than the upper surface of the protective layer. Since the upper surface of the front electrode layer in the first region is lower than the upper surface of the protective layer, the protective layer protects the front electrode layer in the first region. Thus, the protective layer can prevent the semiconductor light-emitting device from being subjected to external forces in the manufacturing process to generate defects such as scratches and dirt, and the introduction of the protective layer increases the distance from the front electrode layer on the protective layer to the active layer, which greatly reduces the impact on the active layer of cutting defects generated on the cavity surface and side surface of the semiconductor light-emitting device. Even if a small amount of material of the front electrode layer extends to a part of the cavity surface of the semiconductor light-emitting device, the presence of the protective layer can prevent the material of the front electrode layer from extending to the active layer, thereby reducing the shielding of the material of the front electrode layer against the plating film on the cavity surface and reducing the optical damage of the cavity surface. As described above, the reliability of the semiconductor light emitting device is improved. In addition, the protective layer is easily provided, the technical difficulty is reduced, and the cost is low.

[0027] Optionally, when the conductivity type of the second conductive ions is opposite to that of the first conductive ions, the doped semiconductor contact layer and the protective layer are electrically isolated, and the current in the edge region of the doped semiconductor contact layer is restricted. When the conductivity type of the second conductive ions is the same as that of the first conductive ions, the doping concentration of the second conductive ions is smaller than that of the first conductive ions, so that the protective layer is less conductive and has a certain restricting effect on the current in the edge region of the doped semiconductor contact layer.

[0028] Optionally, the doping concentration of the second conductive ions is 10 times that of the first conductive ions. -6 Times to 10 -1 Thus, the protective layer performs an additional electrical insulating function, and the current in the edge region of the doped semiconductor contact layer is double-limited by the current-limiting insulating layer and the protective layer.

[0029] Optionally, the material of the doped semiconductor contact layer is a first body semiconductor material doped with ions of a first conductivity and the material of the protective layer is an undoped second body semiconductor material, or the material of the protective layer is a second body semiconductor material doped with ions of a second conductivity. The average lattice mismatch between the second body semiconductor material and the first body semiconductor material is 1% or less, which reduces stress at the interface between the doped semiconductor contact layer and the protective layer and improves the lattice match at the interface between the doped semiconductor contact layer and the protective layer, which makes it easier to form the protective layer on the doped semiconductor contact layer.

[0030] Optionally, the doped semiconductor contact layer includes a first subdoped semiconductor layer and a second subdoped semiconductor layer located on a surface of the first subdoped semiconductor layer facing away from the active layer, the second subdoped semiconductor layer having a doping concentration greater than that of the first subdoped semiconductor layer. The high doping concentration of the second subdoped semiconductor layer reduces the contact resistance between the second subdoped semiconductor layer and the front electrode layer. The low doping concentration of the first subdoped semiconductor layer and the second subdoped semiconductor layer are farther away from the active layer than the first subdoped semiconductor layer, thereby reducing the effect of doping ions in the doped semiconductor contact layer on the absorption loss of light emitted from the active layer.

[0031] In the method for manufacturing a highly reliable and low-defect semiconductor light-emitting device according to the technical solution of the present application, a protective layer is formed on the edge region of the doped semiconductor contact layer on the side away from the active layer, and the protective layer is used to raise the edge region of the doped semiconductor contact layer, so that the upper surface of the front electrode layer in the first region is lower than the upper surface of the protective layer. Since the upper surface of the front electrode layer in the first region is lower than the upper surface of the protective layer, the protective layer protects the front electrode layer in the first region. The protective layer can prevent the semiconductor light-emitting device from being subjected to external forces in the manufacturing process to generate defects such as scratches and dirt, and the introduction of the protective layer increases the distance from the front electrode layer on the protective layer to the active layer, which greatly reduces the impact on the active layer of cutting defects generated on the cavity surface and side surface of the semiconductor light-emitting device. Even if a small amount of material of the front electrode layer extends to a part of the cavity surface of the semiconductor light-emitting device, the existence of the protective layer can prevent the material of the front electrode layer from extending to the active layer, thereby reducing the shielding of the material of the front electrode layer against the plating film on the cavity surface and reducing the optical damage of the cavity surface. As described above, the reliability of the semiconductor light emitting device is improved. In addition, the protective layer is easily provided, the technical difficulty is reduced, and the cost is low.

[0032] Optionally, the doped semiconductor contact layer and the initial protective layer are formed in the same epitaxial step in sequence, thereby simplifying the process. Furthermore, since the doped semiconductor contact layer and the initial protective layer are formed in sequence, the introduction of defects between the doped semiconductor contact layer and the initial protective layer is avoided, and the defects between the protective layer and the edge region of the doped semiconductor contact layer are reduced, thereby avoiding affecting carrier mobility and avoiding causing an increase in the resistance voltage of the device.

[0033] Optionally, even if there is a defect on the upper surface of the protective layer before the current-limiting insulating layer is formed, and a stacking fault occurs during the formation of the current-limiting insulating layer on the protective layer, the electrical isolation function of the protective layer can prevent the occurrence of a dielectric breakdown phenomenon caused by an increase in charge in the current-limiting insulating layer, and can prevent aging, shortening of the life span, or leakage and burning of the semiconductor light-emitting device.

[0034] In order to more clearly describe the specific embodiments of the present application or the technical solutions of the prior art, the following will briefly describe the drawings used to describe the specific embodiments or the prior art. Obviously, the drawings in the following description are some embodiments of the present application, and those skilled in the art can also obtain other drawings based on these drawings without creative efforts. [Brief description of the drawings]

[0035] [Figure 1] FIG. 1 is a schematic diagram showing the structure of a highly reliable and low-defect semiconductor light-emitting device according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a structural diagram of a manufacturing process for a highly reliable and low-defect semiconductor light-emitting device according to another embodiment of the present application. [Diagram 3] FIG. 3 is a structural diagram of a manufacturing process for a highly reliable and low-defect semiconductor light-emitting device according to another embodiment of the present application. [Figure 4] FIG. 4 is a structural diagram of a manufacturing process for a highly reliable and low-defect semiconductor light-emitting device according to another embodiment of the present application. [Diagram 5] FIG. 5 is a structural diagram of a manufacturing process for a highly reliable and low-defect semiconductor light-emitting device according to another embodiment of the present application. [Figure 6] FIG. 6 is a structural diagram of a manufacturing process for a highly reliable and low-defect semiconductor light-emitting device according to another embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] With the expansion of the market and application of high-power semiconductor light-emitting devices, semiconductor light-emitting devices are required to have high reliability and low cost, so manufacturers attach great importance to the fault tolerance of high-power semiconductor light-emitting devices during long-term operation. The failure of semiconductor light-emitting devices is generally caused by defects such as dirt and scratches introduced on the surface of the wafer during the manufacturing process and packaging process, or by cutting the chip, plating the film, or cutting defects close to the surface of the chip cavity surface during the packaging process. Surface defects cause stacking defects in the dielectric film during deposition, and when such anomalies occur near the light-emitting region, for example, the carrier mobility is affected, the resistance voltage of the device increases, or the charge of the dielectric layer increases, causing dielectric breakdown phenomena, which causes aging, shortening of the life, leakage, and burnout of the semiconductor light-emitting device. The surface defects of the wafer also cause packaging defects in the current injection region of the chip, which results in higher local temperatures and higher stresses in the chip, leading to failure of the active materials. Cutting defects close to the surface of the cavity surface and side surface can cause catastrophic damage to the cavity surface, which causes bypass leakage and burnout during the packaging process. Therefore, it is common to strictly control the processes of epitaxial growth regulation, wafer fabrication, cavity plating and packaging to improve device reliability. However, all of the above techniques cause drawbacks such as technical complexity, reduced process stability and increased process costs.

[0037] The technical solutions of the present application will be described below clearly and completely with reference to the drawings, and it is obvious that the described embodiments are only some of the embodiments of the present application, and not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative labor all belong to the patent scope of the present application.

[0038] In the description of this application, the orientations or positional relationships indicated by the terms "center," "upper," "lower," "left," "right," "vertical," "horizontal," "inner," "outer," etc. are based on the orientations or positional relationships shown in the drawings, and are used only to facilitate and simplify the description of this application, and do not indicate or suggest that the relevant devices or components necessarily have a specific orientation or are constructed or operated in a specific orientation, and should not be understood as limiting this application. In addition, it should be understood that the terms "first," "second," and "third" are used for the purpose of description only, and do not indicate or suggest relative importance.

[0039] In addition, the technical features according to the various embodiments of the present application described below can be combined with each other unless they are inconsistent.

[0040] Example 1 One embodiment of the present application provides a highly reliable, low defect semiconductor light emitting device, with reference to FIG. 1, comprising: A semiconductor substrate layer 100; an active layer 130 located on the semiconductor substrate layer; a doped semiconductor contact layer 160 located on a side of the active layer 130 away from the semiconductor substrate layer 100 and including a first region and an edge region surrounding the first region; a protective layer 170 located on the edge region of the doped semiconductor contact layer 160 away from the active layer 130; The surface electrode layer is located on a side of the first region away from the active layer, and an upper surface of the surface electrode layer in the first region is lower than an upper surface of the protective layer.

[0041] In this embodiment, the protective layer 170 is used to raise the edge region of the doped semiconductor contact layer 160, so that the top surface of the front electrode layer 190 in the first region is lower than the top surface of the protective layer 170. Since the top surface of the front electrode layer 190 in the first region is lower than the top surface of the protective layer 170, the protective layer protects the front electrode layer 190 in the first region. Therefore, the protective layer 170 can prevent the semiconductor light emitting device from being subjected to external forces during the manufacturing process to generate defects such as scratches and dirt, and the introduction of the protective layer 170 increases the distance from the front electrode layer 190 to the active layer on the protective layer 170, which greatly reduces the impact of cutting defects generated on the cavity surface and side surface of the semiconductor light emitting device on the active layer. Even if a small amount of the material of the front electrode layer 190 extends to a part of the cavity surface of the semiconductor light emitting device, the presence of the protective layer 170 can prevent the material of the front electrode layer 190 from extending to the active layer 130, thereby reducing the shielding of the material of the front electrode layer 190 against the plating film on the cavity surface and reducing optical damage to the cavity surface. As described above, the reliability of the semiconductor light emitting device is improved. In addition, the protective layer 170 is easy to install, reducing technical difficulty and cost.

[0042] In one embodiment, the height difference between the upper surface of the protective layer 170 and the upper surface of the front electrode layer 190 located in the first region is 0.05 μm to 5 μm, for example, 0.05 μm, 0.1 μm, 0.5 μm, 2 μm, 3 μm, 4 μm, or 5 μm. If the height difference between the upper surface of the protective layer 170 and the upper surface of the front electrode layer 190 located in the first region is less than 0.05 μm, the protective layer 170 has a weak protective effect on the first region and the active layer 130, and if the height difference between the upper surface of the protective layer 170 and the upper surface of the front electrode layer 190 located in the first region is more than 5 μm, the height of the semiconductor light emitting device is too high and is disadvantageous for miniaturization.

[0043] In one embodiment, the thickness of the protective layer 170 in the direction perpendicular to the surface of the semiconductor substrate layer 100 is 0.1 μm to 5 μm, for example, 0.1 μm, 0.5 μm, 2 μm, 3 μm, 4 μm, or 5 μm. If the thickness of the protective layer 170 in the direction perpendicular to the surface of the semiconductor substrate layer 100 is too small, the protective layer 170 has a weak protective effect on the first region and the active layer 130, whereas if the thickness of the protective layer 170 in the direction perpendicular to the surface of the semiconductor substrate layer 100 is too large, the height of the semiconductor light emitting device is too high, which is disadvantageous for miniaturization.

[0044] The protective layer 170 has a ring-shaped structure. The protective layer 170 is not disposed above the first region.

[0045] The high-reliability, low-defect semiconductor light-emitting device has a front cavity surface and a rear cavity surface arranged opposite to each other, the front cavity surface and the rear cavity surface both exposing a sidewall surface of the active layer 130 and a sidewall surface of the doped semiconductor contact layer 160, the protective layer 170 includes a first sub-protection region and a second sub-protection region arranged opposite to each other, the first sub-protection region and the second sub-protection region are arranged along a light emission direction, an outer wall of the first sub-protection region is flush with the exposed sidewall surface of the active layer 130 of the front cavity surface and the exposed sidewall surface of the doped semiconductor contact layer 160 of the front cavity surface, and an outer wall of the second sub-protection region is flush with the exposed sidewall surface of the active layer 130 of the rear cavity surface and the exposed sidewall surface of the doped semiconductor contact layer 160 of the rear cavity surface.

[0046] The protective layer 170 further includes a third sub-protection region and a fourth sub-protection region arranged opposite each other, the third sub-protection region being connected to the first sub-protection region and the second sub-protection region, respectively, and the fourth sub-protection region being connected to the first sub-protection region and the second sub-protection region, respectively.

[0047] The material of the protective layer 170 is an undoped second body semiconductor material, or the material of the protective layer 170 is a second body semiconductor material doped with second conductive ions, the conductivity type of the second conductive ions being opposite to the conductivity type of the first conductive ions, or the material of the protective layer 170 is a second body semiconductor material doped with second conductive ions, the conductivity type of the second conductive ions being the same as the conductivity type of the first conductive ions, and the doping concentration of the second conductive ions being less than the doping concentration of the first conductive ions.

[0048] When the conductivity type of the second conductive ions is opposite to that of the first conductive ions, the doped semiconductor contact layer 160 and the protective layer 170 are electrically isolated, limiting the current flow in the edge region of the doped semiconductor contact layer 160. In a specific embodiment, the conductivity type of the doped semiconductor contact layer 160 is N-type, and the conductivity type of the protective layer 170 is P-type.

[0049] When the conductivity type of the second conductive ions is the same as that of the first conductive ions, the doping concentration of the second conductive ions is less than that of the first conductive ions, so that the protective layer 170 is less conductive and has a certain limiting effect on the current in the edge region of the doped semiconductor contact layer 160.

[0050] In one embodiment, an average lattice mismatch of 1% or less between the second body semiconductor material and the first body semiconductor material reduces stress at the interface between the doped semiconductor contact layer 160 and the protective layer 170 and improves the lattice match at the interface between the doped semiconductor contact layer 160 and the protective layer 170, which makes it easier to form the protective layer 170 on the doped semiconductor contact layer.

[0051] Moreover, in one embodiment, the second body semiconductor material is the same as the first body semiconductor material. The doped semiconductor contact layer 160 and the protective layer 170 adopt similar body semiconductor materials, which further reduces the stress at the interface between the doped semiconductor contact layer 160 and the protective layer 170 and further improves the lattice matching at the interface between the doped semiconductor contact layer 160 and the protective layer 170.

[0052] The protective layer 170 may be a single layer or a multi-layer structure.

[0053] In one embodiment, the material of the protective layer 170 is a P-type semiconductor protective layer, an N-type semiconductor protective layer, or an intrinsic semiconductor protective layer. Specifically, when the semiconductor substrate layer 100 is a GaAs substrate, the material of the protective layer 170 is doped or undoped GaAs, doped or undoped AlGaAs, doped or undoped InGaP, doped or undoped InGaAsP, or doped or undoped InGaAs; when the material of the semiconductor substrate layer 100 is an InP substrate, the material of the protective layer 170 is doped or undoped InGaAsP, doped or undoped InP, doped or undoped InGaALAs, doped or undoped InGaAs, or doped or undoped InAlAs; when the material of the semiconductor substrate layer 100 is a GaN substrate, the material of the protective layer 170 is doped or undoped AlGaN, doped or undoped GaN, or doped or undoped InAlGaN.

[0054] When the protective layer 170 has a multi-layer structure, the protective layer 170 includes a first sub-protective layer through an Nth sub-protective layer (where N is an integer greater than or equal to 2), and the k+1th sub-protective layer (where k is an integer greater than or equal to 1 and less than or equal to N) is located on the side of the kth sub-protective layer away from the semiconductor substrate layer 100.

[0055] In a specific embodiment, the conductivity type of the (k+1)th sub-protective layer is opposite to the conductivity type of the kth sub-protective layer, and the conductivity type of the 1st sub-protective layer is opposite to the conductivity type of the doped semiconductor contact layer. In one embodiment, the conductivity types of the 1st through Nth sub-protective layers are all opposite to the conductivity type of the doped semiconductor contact layer.

[0056] In this embodiment, the front electrode layer 190 is further located on the side of the protective layer 170 away from the doped semiconductor contact layer 160, and the high reliability low defect semiconductor light emitting device further includes a current limiting insulating layer 180 located on the protective layer 170 between the front electrode layer 190 and the protective layer 170. The material of the current limiting insulating layer 180 includes silicon oxide.

[0057] Furthermore, the doping concentration of the second conductive ions is 10 times that of the first conductive ions. -6 Times to 10 -1 times, e.g. 10 -6 Double, 10 -5 Double, 10 -4 Double, 10 -3 Double, 10 -2 Double or 10 -1 Thus, the protective layer 170 serves an additional electrical insulating function, so that the current flowing through the edge region of the doped semiconductor contact layer 160 is double-limited by the current-limiting insulating layer 180 and the protective layer 170.

[0058] Furthermore, the current-limiting insulating layer 180 is located between the surface electrode layer 190 on the protective layer 170 and the protective layer 170, and on the side of the edge of the first region that is away from the active layer 130, and the current-limiting insulating layer 180 further covers the inner wall of the protective layer 170. In this case, the region of the first region that is not covered with the current-limiting insulating layer 180 is defined as a current injection region. In this case, when injecting a current into the current injection region, the current injection region has a certain distance from the interface between the protective layer 170 and the edge region of the doped semiconductor contact layer 160, so that there is an advantage that the interface between the protective layer 170 and the edge region of the doped semiconductor contact layer 160 is unlikely to become a leak path.

[0059] If the current-limiting insulating layer 180 is further located on the edge of the first region away from the active layer 130, the surface electrode layer 190 further covers the current-limiting insulating layer 180 in the first region.

[0060] The width by which the current-limiting insulating layer 180 covers the edge of the first region refers to the width by which the current-limiting insulating layer 180 covers either one side of the edge of the first region.

[0061] In this embodiment, the doped semiconductor contact layer 160 includes a first subdoped semiconductor layer 161 and a second subdoped semiconductor layer 162 located on a surface of the first subdoped semiconductor layer 161 away from the active layer 130, and the doping concentration of the second subdoped semiconductor layer 162 is higher than that of the first subdoped semiconductor layer 161. Since the doping concentration of the second subdoped semiconductor layer 162 is high, the contact resistance between the second subdoped semiconductor layer 162 and the surface electrode layer 190 is low. Since the doping concentration of the first subdoped semiconductor layer 161 is low and the second subdoped semiconductor layer 162 is farther away from the active layer 130 than the first subdoped semiconductor layer 161, the influence of the doped ions of the doped semiconductor contact layer 160 on the absorption loss of light emitted from the active layer 130 is reduced.

[0062] In one embodiment, the doping concentration of the second sub-doped semiconductor layer 162 is 10 to 50 times higher than the doping concentration of the first sub-doped semiconductor layer 161. This satisfactorily achieves both a reduction in the contact resistance between the second sub-doped semiconductor layer 162 and the front electrode layer 190 and a reduction in the effect on light absorption loss.

[0063] In another embodiment, the doped semiconductor contact layer may be a single layer structure, the first region of the doped semiconductor contact layer being used to contact the surface electrode layer, reducing the contact electrode.

[0064] The high-reliability, low-defect semiconductor light-emitting device further includes an upper waveguide layer 140 located between the doped semiconductor contact layer 160 and the active layer 130, an upper confinement layer 150 located between the upper waveguide layer 140 and the doped semiconductor contact layer 160, a lower waveguide layer 120 located between the active layer 130 of the semiconductor substrate layer 100, a lower confinement layer 110 located between the lower waveguide layer 120 and the semiconductor substrate layer 100, and a back electrode layer 101 located on the surface of the semiconductor substrate layer 100 away from the active layer 130.

[0065] In this embodiment, when the high-reliability, low-defect semiconductor light-emitting device and the heat sink are welded together, the protective layer 170 increases the distance between the solder and the active layer during the welding process, reducing element leakage and burnout failures caused by the solder bumps, thereby improving the reliability of the semiconductor light-emitting device.

[0066] In this embodiment, an anti-reflection film covering the front cavity surface and a reflective film covering the rear cavity surface are further included.

[0067] Example 2 This embodiment provides a method for manufacturing a highly reliable and low-defect semiconductor light-emitting device. Referring to FIG. 1, the method includes: Step S1 of providing a semiconductor substrate layer; Step S2 of forming an active layer on the semiconductor substrate layer; forming a doped semiconductor contact layer on the side of the active layer facing away from the semiconductor substrate layer, the doped semiconductor contact layer including a first region and an edge region surrounding the first region; forming a protective layer on an edge region of the doped semiconductor contact layer away from the active layer; forming a surface electrode layer on a side of the first region away from the active layer, The upper surface of the front electrode layer in the first region includes a step S5 that is lower than the upper surface of the protective layer.

[0068] 2, the method includes the steps of providing a semiconductor substrate layer 100, forming a lower confinement layer 110 on the semiconductor substrate layer 100, forming a lower waveguide layer 120 on a side of the lower confinement layer 110 away from the semiconductor substrate layer 100, forming an active layer 130 on a side of the lower waveguide layer away from the semiconductor substrate layer 100, forming an upper waveguide layer 140 on a side of the active layer 130 away from the semiconductor substrate layer 100, forming an upper confinement layer 150 on a side of the upper waveguide layer 140 away from the active layer 130, and forming a doped semiconductor contact layer 160 on a side of the upper confinement layer 150 away from the active layer 130.

[0069] In this embodiment, the step of forming the doped semiconductor contact layer 160 includes forming a first sub-doped semiconductor layer 161 on a side of the active layer 130 away from the semiconductor substrate layer 100, and forming a second sub-doped semiconductor layer 162 on a surface of the first sub-doped semiconductor layer 161 away from the active layer 130, where the doping concentration of the second sub-doped semiconductor layer 162 is greater than the doping concentration of the first sub-doped semiconductor layer 161. For parameters of the first sub-doped semiconductor layer 161 and the second sub-doped semiconductor layer 162, refer to the above-mentioned embodiment.

[0070] In another embodiment, the doped semiconductor contact layer is a single layer structure.

[0071] In step S4, a protective layer 170 is formed on the edge region of the doped semiconductor contact layer away from the active layer. The step of forming the protective layer 170 includes epitaxially growing an initial protective layer 17 on the first region and the edge region away from the active layer 130 (see FIG. 2), and etching and removing the initial protective layer 17 in the first region to form a protective layer 170 exposing the surface of the first region (see FIG. 3).

[0072] The initial protective layer 17 may have a single-layer structure or a multi-layer structure.

[0073] When the initial protective layer 17 has a multilayer structure, the initial protective layer 17 includes, from bottom to top, a first sub-initial protective layer to an Nth sub-initial protective layer, and the initial protective layer 17 in the first region is etched and removed, so that the kth sub-initial protective layer becomes the kth sub-protective layer, and the k+1th sub-initial protective layer becomes the k+1th sub-protective layer.

[0074] In one embodiment, when the initial protective layer 17 has a multilayer structure, in the step of etching and removing the initial protective layer 17 in the first region, the etching selectivity between the material of any of the k+1th sub-initial protective layers and the material of the first sub-initial protective layer is 5 or more, for example, 5, 8, 10, 15 or 20, and the etching selectivity between the material of the first sub-initial protective layer and the material of the doped semiconductor contact layer 160 is 5 or more, for example, 5, 8, 10, 15 or 20.

[0075] The etching selectivity between the material of the first sub-initial protective layer and the material of the second sub-doped semiconductor layer 162 is 5 or more.

[0076] Processes for forming the initial protective layer include metal-organic chemical vapor deposition (MOCVD) and molecular beam epitaxy (MEB).

[0077] In one embodiment, the doped semiconductor contact layer 160 and the initial protective layer 17 are formed in the same epitaxial step in sequence, thereby simplifying the process. Since the doped semiconductor contact layer 160 and the initial protective layer 17 are formed in sequence, the introduction of defects between the doped semiconductor contact layer 160 and the initial protective layer 17 is avoided, and the defects between the protective layer 170 and the edge region of the doped semiconductor contact layer 160 are reduced, thereby avoiding affecting the carrier mobility and avoiding causing an increase in the resistance voltage of the device.

[0078] The doped semiconductor contact layer 160 and the initial protective layer 17 are successively formed in the same cavity.

[0079] For the description of specific parameters regarding the protective layer, please refer to Example 1 and will not be described in detail.

[0080] Referring to FIG. 4 , a current-limiting insulating layer 180 is formed, and the current-limiting insulating layer 180 is located on a side of the protective layer 170 away from the active layer 130, and further, the current-limiting insulating layer 180 is located on a side of the protective layer 170 away from the active layer 130, a side of the edge of the first region away from the active layer 130, and an inner wall of the protective layer 170.

[0081] Referring to FIG. 5, a surface electrode layer is formed on the side of the first region away from the active layer, and an upper surface of the surface electrode layer in the first region is lower than an upper surface of the protective layer.

[0082] In the step of forming the surface electrode layer, the surface electrode layer is also formed on the side of the current limiting insulating layer that is away from the protective layer.

[0083] In this embodiment, even if there is a defect on the upper surface of the protective layer before the current-limiting insulating layer is formed and a stacking fault occurs during the formation of the current-limiting insulating layer on the protective layer, the electrical isolation effect of the protective layer can prevent the occurrence of a dielectric breakdown phenomenon caused by an increase in charge in the current-limiting insulating layer, and can prevent aging, shortened lifespan, leakage, and burnout of the semiconductor light-emitting device.

[0084] 6, a back electrode layer 101 is formed on the surface of the semiconductor substrate layer 100 away from the active layer 130. As shown in FIG.

[0085] In this embodiment, before forming the surface electrode layer, the number of first regions is multiple, with cutting regions between the peripheral edge regions of different first regions, and the manufacturing method for the high-reliability low-defect semiconductor light-emitting device further includes a step of cutting the surface electrode layer, the current-limiting insulating layer, the protective layer, the doped semiconductor contact layer, the upper limiting layer, the upper waveguide layer, the active layer, the lower waveguide layer, the lower limiting layer and the semiconductor substrate layer along the cutting regions.

[0086] This embodiment further includes the steps of forming an anti-reflection coating on the front cavity surface and forming a reflective coating on the rear cavity surface.

[0087] Obviously, the above examples are merely illustrative and do not limit the embodiments. Those skilled in the art can make various other changes or modifications based on the above description. It is not necessary to cover all the embodiments here, and it is impossible to cover all the embodiments. Any obvious changes or modifications derived from these are also within the scope of the present invention.

Claims

1. A highly reliable, low-defect semiconductor light-emitting device, a semiconductor substrate layer; an active layer located on the semiconductor substrate layer; a doped semiconductor contact layer located on a side of the active layer away from the semiconductor substrate layer and including a first region and an edge region surrounding the first region; a protective layer located on an edge region of the doped semiconductor contact layer away from the active layer; a surface electrode layer located on a side of the first region away from the active layer, the surface electrode layer having an upper surface lower than an upper surface of the protective layer in the first region; the surface electrode layer is further disposed on a side of the protective layer away from the doped semiconductor contact layer; a current limiting insulating layer located between the surface electrode layer on the protective layer and the protective layer and on a side of an edge of the first region away from the active layer; The current limiting insulating layer further covers an inner wall on the protective layer. A highly reliable and low defect semiconductor light emitting device.

2. 2. The highly reliable and low-defect semiconductor light emitting device according to claim 1, wherein the difference in height between the upper surface of said protective layer and the upper surface of said front electrode layer located in said first region is 0.05 μm to 5 μm.

3. 3. The highly reliable and low-defect semiconductor light-emitting device according to claim 1, wherein the thickness of said protective layer in the direction perpendicular to the surface of said semiconductor substrate layer is 0.1 μm to 5 μm.

4. 2. The high-reliability, low-defect semiconductor light-emitting device of claim 1, further comprising: a front cavity surface and a rear cavity surface arranged opposite to each other, the front cavity surface and the rear cavity surface both exposing a sidewall surface of the active layer and a sidewall surface of the doped semiconductor contact layer, the protective layer including a first sub-protection region and a second sub-protection region arranged opposite to each other, the first sub-protection region and the second sub-protection region being arranged along a light emission direction, an outer wall of the first sub-protection region being flush with the sidewall surface of the exposed active layer of the front cavity surface and the sidewall surface of the exposed doped semiconductor contact layer of the front cavity surface, and an outer wall of the second sub-protection region being flush with the sidewall surface of the exposed active layer of the rear cavity surface and the sidewall surface of the exposed doped semiconductor contact layer of the rear cavity surface.

5. 2. The high-reliability, low-defect semiconductor light-emitting device of claim 1, wherein the material of the doped semiconductor contact layer is a first body semiconductor material doped with a first conductive ion and the material of the protective layer is an undoped second body semiconductor material; or the material of the protective layer is a second body semiconductor material doped with a second conductive ion, the conductivity type of the second conductive ion being opposite to the conductivity type of the first conductive ion; or the material of the protective layer is a second body semiconductor material doped with a second conductive ion, the conductivity type of the second conductive ion being the same as the conductivity type of the first conductive ion, and the doping concentration of the second conductive ion being less than the doping concentration of the first conductive ion.

6. The conductivity type of the second conductive ions is the same as that of the first conductive ions, and the doping concentration of the second conductive ions is 10 times that of the first conductive ions. -6 Times to 10 -1 6. The highly reliable and low defect semiconductor light emitting device according to claim 5, wherein the number of the first and second electrodes is 100 to 1000.

7. 6. The high-reliability, low-defect semiconductor light-emitting device according to claim 5, wherein an average lattice mismatch between said second body semiconductor material and said first body semiconductor material is 1% or less.

8. 8. The high reliability, low defect semiconductor light emitting device of claim 7, wherein said second body semiconductor material is the same as said first body semiconductor material.

9. 2. A highly reliable and low-defect semiconductor light-emitting device according to claim 1, wherein said protective layer has a single-layer structure or a multi-layer structure.

10. The semiconductor substrate layer is a GaAs substrate, and the material of the protective layer is doped or undoped GaAs, doped or undoped AlGaAs, doped or undoped InGaP, doped or undoped InGaAsP, or doped or undoped InGaAs, or The material of the semiconductor substrate layer is an InP substrate, and the material of the protective layer is doped or undoped InGaAsP, doped or undoped InGaAlAs, doped or undoped InGaAs, doped or undoped InAlAs, or doped or undoped InP, or 10. The high-reliability, low-defect semiconductor light-emitting device according to claim 1, wherein the material of the semiconductor substrate layer is a GaN substrate, and the material of the protective layer is doped or undoped AlGaN, doped or undoped GaN, or doped or undoped InAlGaN.

11. 2. The high-reliability, low-defect semiconductor light-emitting device of claim 1, wherein the doped semiconductor contact layer includes a first sub-doped semiconductor layer and a second sub-doped semiconductor layer located on a surface of the first sub-doped semiconductor layer away from the active layer, and the doping concentration of the second sub-doped semiconductor layer is greater than the doping concentration of the first sub-doped semiconductor layer.

12. 2. The highly reliable and low-defect semiconductor light emitting device according to claim 1, wherein the doping concentration of the second sub-doped semiconductor layer is 10 to 50 times that of the first sub-doped semiconductor layer.

13. an upper waveguide layer located between the doped semiconductor contact layer and the active layer; an upper confinement layer located between the upper waveguide layer and the doped semiconductor contact layer; a lower waveguide layer located between the active layer and a semiconductor substrate layer; a lower confinement layer located between the lower waveguide layer and a semiconductor substrate layer; 2. The highly reliable and low-defect semiconductor light emitting device according to claim 1, further comprising: a back electrode layer located on a surface of the semiconductor substrate layer away from the active layer.

14. A method for manufacturing a highly reliable, low-defect semiconductor light-emitting device, comprising: Providing a semiconductor substrate layer; forming an active layer on the semiconductor substrate layer; forming a doped semiconductor contact layer on a side of the active layer remote from the semiconductor substrate layer, the doped semiconductor contact layer including a first region and an edge region surrounding the first region; forming a protective layer on an edge region of the doped semiconductor contact layer away from the active layer; forming a surface electrode layer on a side of the first region away from the active layer, an upper surface of the surface electrode layer in the first region includes a step that is lower than an upper surface of the protection layer; forming a current limiting insulating layer located on a side of the protective layer away from the active layer, on a side of the edge of the first region away from the active layer, and on an inner wall of the protective layer, before forming the surface electrode layer; In the step of forming the surface electrode layer, the surface electrode layer is also formed on a side of the current limiting insulating layer that is away from the protective layer.

4. A method for producing a highly reliable and low defect semiconductor light emitting device comprising the steps of:

15. The step of forming the protective layer includes: epitaxially growing an initial protective layer on the first region and the edge region away from the active layer; 15. The method for manufacturing a highly reliable and low-defect semiconductor light-emitting device according to claim 14, further comprising: etching and removing the initial protective layer in the first region to form a protective layer exposing the surface of the first region.

16. 16. The method of claim 15, wherein the doped semiconductor contact layer and the initial protective layer are formed in sequence in the same epitaxial process.

17. The step of forming the doped semiconductor contact layer comprises: forming a first sub-doped semiconductor layer on a side of the active layer away from the semiconductor substrate layer; forming a second sub-doped semiconductor layer on a surface of the first sub-doped semiconductor layer away from the active layer; 15. The method of claim 14, wherein the doping concentration of the second sub-doped semiconductor layer is greater than the doping concentration of the first sub-doped semiconductor layer.

18. Before forming the surface electrode layer, the number of the first regions is plural, and has a cut region between the peripheral edge regions of different first regions; 15. The method for manufacturing a high-reliability, low-defect semiconductor light-emitting device of claim 14, further comprising the step of cutting the front electrode layer, the current-limiting insulating layer, the protective layer, the doped semiconductor contact layer, the active layer and the semiconductor substrate layer along the cutting region.

Citation Information

Patent Citations

  • JP1974094292A

  • Semiconductor laser and manufacture thereof

    JP1995007220A

  • Group iii nitride compound semiconductor light emitting element

    JP2001185758A

  • Semiconductor laser

    JP2001257423A

  • Semiconductor light emitting device

    JP2004319912A