Apparatus for producing non-aqueous electrolyte and method for producing non-aqueous electrolyte
A styrene-based resin with a tertiary amino group in the non-aqueous electrolyte manufacturing device addresses the inefficacy of conventional resins in removing hydrofluoric acid, resulting in improved electrolyte quality and battery performance.
Patent Information
- Application Number
- JP2018199869
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2018-10-24
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2038-10-24
AI Technical Summary
Existing methods for removing acidic impurities like hydrofluoric acid from non-aqueous electrolytes in lithium-ion batteries are ineffective, leading to reduced battery capacity and potential corrosion, as conventional weakly basic anion exchange resins fail to achieve the required quality.
A non-aqueous electrolyte manufacturing device and method using a styrene-based resin with a specific tertiary amino group as a weakly basic anion exchange group to effectively adsorb and reduce hydrofluoric acid content in non-aqueous electrolytes.
The device and method enable the production of non-aqueous electrolytes with significantly reduced hydrofluoric acid content, enhancing battery performance and safety by effectively adsorbing acidic impurities.
Smart Images

Figure 0007573356000015 
Figure 0007573356000016 
Figure 0007573356000001
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus for producing a non-aqueous electrolyte solution and a method for producing a non-aqueous electrolyte solution. [Background technology]
[0002] In lithium ion batteries, a non-aqueous electrolyte solution in which a lithium-based electrolyte such as lithium hexafluorophosphate (LiPF6) is dissolved in a carbonate ester solvent is used as the electrolyte solution.
[0003] However, trace amounts of water remain in the carbonate ester solvent and the lithium-based electrolyte constituting the electrolytic solution. This water reacts with the lithium-based electrolyte such as LiPF6 to produce hydrogen fluoride (HF) and the like, for example, as shown in the following reaction formulas (1) to (3). (1) LiPF6+H2O → LiF+2HF+POF3 (2) POF3+H2O → POF2(OH)+HF (3)POF2(OH)+H2O → POF(OH)2+HF
[0004] If acidic impurities such as hydrogen fluoride (hydrofluoric acid) are present in the electrolyte, they can reduce the battery capacity and charge / discharge cycle characteristics of the lithium-ion battery, and can make the inside of the battery more susceptible to corrosion (see Patent Document 1 (JP 2011-71111 A), etc.). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2011-71111 A Summary of the Invention [Problem to be solved by the invention]
[0006] For this reason, a method for removing acidic impurities such as hydrofluoric acid from the electrolyte has been desired. One possible method for removing such acidic impurities is to bring the electrolyte for a lithium ion battery into contact with a weakly basic anion exchange resin that contains an anion exchange group having a tertiary amine structure (a tertiary amino group).
[0007] However, the inventors have found through their investigations that, unlike in water, in a non-aqueous electrolyte solution, depending on the type of the weakly basic anion exchange resin, the performance of removing acidic impurities such as hydrofluoric acid may not be exhibited well, and the quality of the electrolyte solution may not be as targeted.
[0008] Under such circumstances, an object of the present invention is to provide an apparatus for producing a nonaqueous electrolyte solution capable of easily preparing a nonaqueous electrolyte solution, such as an electrolyte solution for a lithium ion battery, in which acidic impurities such as hydrofluoric acid are effectively adsorbed to reduce the content of the acidic impurities, and to provide a method for producing a nonaqueous electrolyte solution.
[0009] As a result of intensive research into achieving the above-mentioned object, the present inventors have found that the above technical problems can be solved by a production apparatus for a non-aqueous electrolyte, the production apparatus having an ion exchange section containing a weakly basic anion exchange resin for obtaining a non-aqueous electrolyte by passing an alkali metal salt electrolyte-containing liquid in which an alkali metal salt electrolyte is dispersed in a carbonate ester through the apparatus, the weakly basic anion exchange resin having a styrene-based resin as a base and a specific tertiary amino group as a weakly basic anion exchange group. Based on this finding, the present invention has been completed.
[0010] That is, the present invention provides (1) Carbonated an ion exchange section containing a weakly basic anion exchange resin for passing an alkali metal salt electrolyte-containing liquid in which an alkali metal salt electrolyte capable of being decomposed into an ester to generate an acid is dissolved, to obtain a nonaqueous electrolyte; The weakly basic anion exchange resin has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): TIFF0007573356000001.tif30148 (However, R1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bonding site with the substrate or a bonding group for bonding to the substrate.) having a tertiary amino group represented by An apparatus for producing a non-aqueous electrolyte, (2) The apparatus for producing a non-aqueous electrolyte according to (1) above, wherein the styrene-based resin is a styrene-divinylbenzene copolymer. (3) The weakly basic anion exchange group is represented by the following general formula (II): TIFF0007573356000002.tif30150 (However, R 1 Groups and R 2 R 3 The group is a hydrocarbon group having 1 to 3 carbon atoms, and * indicates the bonding site with the substrate. The apparatus for producing a non-aqueous electrolyte solution according to the above (1) or (2), (4) The apparatus for producing a nonaqueous electrolyte according to any one of (1) to (3) above, wherein the weakly basic anion exchange group represented by the general formula (I) or the general formula (II) is a dimethylaminomethyl group. (5) The apparatus for producing a non-aqueous electrolyte according to any one of (1) to (4) above, wherein the non-aqueous electrolyte is an electrolyte for a lithium ion battery. (6) A method for producing a nonaqueous electrolyte, comprising the steps of: Carbonated an acid adsorption step of passing an alkali metal salt electrolyte-containing solution, in which an alkali metal salt electrolyte capable of being decomposed into an ester to generate an acid, through an ion exchange section containing a weakly basic anion exchange resin to obtain a non-aqueous electrolyte; The weakly basic anion exchange resin has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): TIFF0007573356000003.tif29130 (However, R 1 Groups and R 2The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bond to the substrate or a bonding group for bonding to the substrate.) having a tertiary amino group represented by A method for producing a non-aqueous electrolyte solution, (7) The method for producing a nonaqueous electrolyte according to (6) above, wherein the styrene-based resin is a styrene-divinylbenzene copolymer. (8) The weakly basic anion exchange group is represented by the following general formula (II): TIFF0007573356000004.tif30137 (However, R 1 Groups and R 2 R 3 The group is a hydrocarbon group having 1 to 3 carbon atoms, and * indicates the bonding site with the substrate. The method for producing a nonaqueous electrolyte solution according to the above (6) or (7), wherein the tertiary amino group is represented by the following formula: (9) The method for producing a nonaqueous electrolyte solution according to any one of the above (6) to (8), wherein the weakly basic anion exchange group represented by the general formula (I) or the general formula (II) is a dimethylaminomethyl group. (10) The method for producing a non-aqueous electrolyte solution according to any one of (6) to (9), wherein the non-aqueous electrolyte solution is an electrolyte solution for a lithium ion battery. This provides: Effect of the Invention
[0011] According to the present invention, there is provided an apparatus for producing a nonaqueous electrolyte solution that can easily prepare a nonaqueous electrolyte solution having a reduced content of acidic impurities such as hydrofluoric acid by effectively adsorbing the acidic impurities, and there is also provided a method for producing a nonaqueous electrolyte solution. [Brief description of the drawings]
[0012] [Figure 1] FIG. 2 is a diagram illustrating a configuration of an apparatus for producing a nonaqueous electrolyte according to the present invention. [Diagram 2] 1 is a diagram showing an example of an apparatus for producing a nonaqueous electrolyte according to the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The apparatus for producing a non-aqueous electrolyte according to the present invention includes an ion exchange unit containing a weakly basic anion exchange resin, and configured to pass an alkali metal salt electrolyte-containing liquid in which an alkali metal salt electrolyte is dispersed in a carbonate ester to obtain a non-aqueous electrolyte, The weakly basic anion exchange resin has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): [ka] (However, R 1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bonding site with the substrate or a bonding group for bonding to the substrate.) having a tertiary amino group represented by It is characterized by the above.
[0014] FIG. 1 shows an example of the configuration of a non-aqueous electrolyte manufacturing apparatus according to the present invention.
[0015] As shown in FIG. 1, a nonaqueous electrolyte manufacturing apparatus 1 according to the present invention has an ion exchange unit 2 containing a weakly basic anion exchange resin, for obtaining a nonaqueous electrolyte by passing an alkali metal salt electrolyte-containing solution S in which an alkali metal salt electrolyte such as a lithium-based electrolyte is dispersed in a carbonate ester.
[0016] In the apparatus for producing a non-aqueous electrolyte according to the present invention, the carbonate ester may be at least one selected from cyclic carbonate esters and chain carbonate esters.
[0017] Examples of the cyclic carbonate ester include one or more selected from ethylene carbonate, propylene carbonate, and the like. Examples of the chain carbonate ester include one or more selected from dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, and the like.
[0018] In the nonaqueous electrolyte manufacturing apparatus according to the present invention, the alkali metal salt electrolyte may be a lithium-based electrolyte, and the lithium-based electrolyte may be one or more selected from LiPF, LiClO, LiBF, LiAsF, LiSbF, LiAlCl, LiCFSO, etc., with LiPF being preferred in terms of battery performance. In the non-aqueous electrolyte production apparatus according to the present invention, the non-aqueous electrolyte is preferably an electrolyte for lithium ion batteries.
[0019] In the nonaqueous electrolyte manufacturing apparatus according to the present invention, the alkali metal salt electrolyte concentration in the alkali metal salt electrolyte-containing solution is preferably 0.5 to 2.0 mol / L, more preferably 0.5 to 1.2 mol / L, and even more preferably 0.8 to 1.2 mol / L.
[0020] The method for preparing the alkali metal salt electrolyte-containing liquid is not particularly limited. For example, the liquid can be prepared by adding and dissolving an alkali metal salt electrolyte in a carbonate ester under an inert gas atmosphere.
[0021] The apparatus for producing a non-aqueous electrolyte according to the present invention has an ion exchange section containing a weakly basic anion exchange resin, through which an alkali metal salt electrolyte-containing liquid (unrefined non-aqueous electrolyte) passes.
[0022] In the apparatus for producing a non-aqueous electrolyte according to the present invention, the weakly basic anion exchange resin used in the ion exchange section has a styrene-based resin as a base.
[0023] In the present application, the styrene-based resin means a resin in which styrene or a styrene derivative is homopolymerized or copolymerized, and which contains 50 mass % or more of structural units derived from styrene or a styrene derivative.
[0024] Examples of the styrene derivative include α-methylstyrene, vinyltoluene, chlorostyrene, ethylstyrene, i-propylstyrene, dimethylstyrene, and bromostyrene.
[0025] The styrene-based resin may be a copolymer with other copolymerizable vinyl monomers, so long as it is mainly composed of a homopolymer or copolymer of styrene or a styrene derivative. Examples of such vinyl monomers include one or more selected from polyfunctional monomers such as divinylbenzenes, such as o-divinylbenzene, m-divinylbenzene, and p-divinylbenzene, alkylene glycol di(meth)acrylates, such as ethylene glycol di(meth)acrylate and polyethylene glycol di(meth)acrylate, (meth)acrylonitrile, methyl (meth)acrylate, and the like.
[0026] The other copolymerizable vinyl monomers are preferably ethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate having an ethylene polymerization number of 4 to 16, and divinylbenzene, more preferably divinylbenzene and ethylene glycol di(meth)acrylate, and even more preferably divinylbenzene.
[0027] In the apparatus for producing a non-aqueous electrolyte according to the present invention, the weakly basic anion exchange resin used in the ion exchange section has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): [ka] (However, R 1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bonding site with the substrate or a bonding group for bonding to the substrate.) The tertiary amino group is represented by the following formula:
[0028] In the weakly basic anion exchange group represented by the above general formula (I), R 1 Groups and R 2 The group is a hydrocarbon group having 1 to 3 carbon atoms. R 1 Group or R 2 The group may be one or more selected from an alkyl group and an alkenyl group, and is preferably an alkyl group. R 1 Group or R 2 Specific examples of the group include one or more groups selected from a methyl group, an ethyl group, a propyl group, and a propylene group, with a methyl group being preferred. In the weakly basic anion exchange group represented by the above general formula (I), R 1 Groups and R 2 The groups may be the same or different.
[0029] Examples of the weakly basic anion exchange group represented by the above general formula (I) include a dimethylamino group, a diethylamino group, and a dipropylamino group, with the dimethylamino group being preferred.
[0030] In the above general formula (I), * indicates the binding site between the weakly basic anion exchange group represented by the above general formula (I) and the substrate or a binding group for binding to the substrate.
[0031] The weakly basic anion exchange group represented by the above general formula (I) is appropriately bonded to a substrate made of a styrene-based resin by bonding with a bonding group R 3 It is preferable that the bond is via a group. [ka] (However, R 1 Groups and R 2 R 3The group is a hydrocarbon group having 1 to 3 carbon atoms, and * indicates the bonding site with the substrate.
[0032] Above R 1 Groups and R 2 Examples of the group include the same as those mentioned above. Above R 3 The group is a hydrocarbon group having 1 to 3 carbon atoms, and R 3 The group may be at least one selected from an alkylene group and an alkenylene group, and is preferably an alkylene group. R 3 Specific examples of the group include one or more selected from a methylene group (-CH2-), an ethylene group (-CH2CH2CH2-), a propylene group (-CH2CH2CH2-), etc., with a methylene group being preferred.
[0033] The weakly basic anion exchange group represented by the above general formula (I) can be introduced into a styrene-based resin by introducing it as a substituent into styrene or a styrene derivative.
[0034] The weakly basic anion exchange resin contained in the ion exchange section may have any of a gel type structure, a macroporous (MR) type structure, and a porous type structure, and is preferably one having a macroporous type structure.
[0035] The size of the weakly basic anion exchange resin is not particularly limited, but the harmonic mean diameter is preferably from 300 to 1000 μm, more preferably from 400 to 800 μm, and even more preferably from 500 to 700 μm.
[0036] Furthermore, the weakly basic anion exchange resin preferably has a total ion exchange capacity in a wet state of 0.1 to 3.0 (eq / LR), more preferably 0.5 to 2.5 (eq / LR), and even more preferably 1.0 to 2.0 (eq / LR).
[0037] Such a weakly basic anion exchange resin may be a commercially available product, and examples thereof include one or more types selected from Diaion WA30 manufactured by Mitsubishi Chemical Corporation and ORLITE DS-6 manufactured by Organo Corporation.
[0038] In the non-aqueous electrolyte manufacturing apparatus according to the present invention, the form of the weakly basic anion exchange resin contained in the ion exchange unit is not particularly limited as long as it allows contact between the alkali metal salt electrolyte-containing liquid and the weakly basic anion exchange resin. For example, the ion exchange unit may be a column or tank packed with a weakly basic anion exchange resin through which the alkali metal salt electrolyte-containing liquid can pass. The ion exchange unit may also be provided with a pump for passing the alkali metal salt electrolyte-containing liquid.
[0039] In the nonaqueous electrolyte manufacturing apparatus according to the present invention, the liquid passing speed (liquid hourly space velocity) at which the alkali metal salt electrolyte-containing liquid is passed through the weakly basic anion exchange device in the ion exchange unit may be appropriately selected from the speeds at which acidic impurities in the alkali metal salt electrolyte-containing liquid can be removed.
[0040] In the treatment with the weakly basic anion exchange resin, for example, first, the weakly basic anion exchange resin is washed in advance with the carbonate ester solvent constituting the alkali metal salt electrolyte-containing liquid to be treated, and then dried under reduced pressure at about 40 to 80°C. Next, the weakly basic anion exchange resin is swollen again with the carbonate ester solvent constituting the alkali metal salt electrolyte-containing liquid to be treated, and then packed into a column. After that, backwashing, pushing out, etc. are performed according to a conventional method, and the electrolyte to be treated is swelled at SV (flow rate / ion exchange resin volume ratio) of 1 to 100 hr. -1 , more preferably SV2 to 50hr -1 , and more preferably SV5 to 20 hr -1 This can be done by passing the solution through the column.
[0041] In the nonaqueous electrolyte manufacturing apparatus according to the present invention, the content of acidic impurities such as hydrofluoric acid in the acid adsorption treatment solution obtained from the ion exchange unit is preferably 20 ppm by mass or less, more preferably 10 ppm by mass or less, and even more preferably 5 ppm by mass or less. In the present application, the amount of acidic impurities refers to a value measured by neutralization titration.
[0042] According to the present invention, by employing a weakly basic anion exchange resin contained in the ion exchange section that has a styrene-based resin as a base and a specific weakly basic anion exchange group having a tertiary amine structure, acidic impurities in the electrolyte can be effectively adsorbed and removed.
[0043] Therefore, according to the present invention, it is possible to provide an apparatus for producing a nonaqueous electrolyte that can easily prepare a nonaqueous electrolyte having a reduced content of acidic impurities such as hydrofluoric acid by effectively adsorbing them.
[0044] Next, a method for producing the nonaqueous electrolyte according to the present invention will be described. The method for producing a non-aqueous electrolyte according to the present invention includes an acid adsorption step of passing an alkali metal salt electrolyte-containing solution, in which an alkali metal salt electrolyte is dispersed in a carbonate ester, through an ion exchange unit containing a weakly basic anion exchange resin to obtain a non-aqueous electrolyte, the weakly basic anion exchange resin having a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): [ka] (However, R 1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bond to the substrate or a bonding group for bonding to the substrate.) The compound is characterized in that it has a tertiary amino group represented by the following formula:
[0045] The method for producing a non-aqueous electrolyte solution according to the present invention is essentially a method for producing a non-aqueous electrolyte solution using the production apparatus according to the present invention, and therefore the details of the production method are the same as those described above in relation to the use of the production apparatus according to the present invention.
[0046] According to the present invention, it is possible to provide a method for producing a non-aqueous electrolyte solution which can easily prepare a non-aqueous electrolyte solution in which the content of acidic impurities such as hydrofluoric acid is effectively reduced. EXAMPLES
[0047] The present invention will now be described in more detail with reference to examples, but these are merely illustrative and do not limit the present invention.
[0048] Example 1 An electrolyte solution was prepared using an apparatus for producing an electrolyte solution for lithium ion batteries as the nonaqueous electrolyte solution producing apparatus 1 shown in FIG. That is, first, as shown in FIG. 2, a column packed with a weakly basic anion exchange resin (macroporous type) having a styrene-divinylbenzene base and dimethylamino groups as weakly basic anion exchange groups was prepared as an ion exchange section 2 constituting a nonaqueous electrolyte production apparatus (an apparatus for producing an electrolyte solution for lithium ion batteries) 1. Next, an electrolyte S, which was prepared by dissolving LiPF6 at 1 mol / L in a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of 1:1, was pumped into the column at 40 hr -1 The electrolyte was passed through the tank at a rate of 1000 rpm, and the electrolyte after passing through the tank was stored in the tank T. The hydrofluoric acid concentration in the electrolyte was measured before and after the passage of the electrolyte by the following method. The results are shown in Table 1.
[0049] <Method for measuring hydrofluoric acid concentration> The hydrogen ion concentrations calculated from the neutralization titration with sodium hydroxide were all converted into hydrofluoric acid concentrations to obtain hydrofluoric acid concentrations.
[0050] Comparative Example 1 As the weakly basic anion exchange resin, an acrylic resin-based weakly basic anion exchange resin having a dimethylamino group as a weakly basic anion exchange group (gel type) was used. In the same manner as in Example 1, the electrolytic solution S was passed through a column packed with the weakly basic anion exchange resin, and the hydrofluoric acid concentration in the electrolytic solution was measured before and after passing the electrolytic solution. The results are shown in Table 1.
[0051] Comparative Example 2 As the weakly basic anion exchange resin, a styrene-divinylbenzene-based weakly basic anion exchange resin having a polyamine group as a weakly basic anion exchange group (macroporous type) was used. In the same manner as in Example 1, the electrolytic solution S was passed through a column packed with the weakly basic anion exchange resin, and the hydrofluoric acid concentration in the electrolytic solution was measured before and after passing the electrolytic solution. The results are shown in Table 1.
[0052] Comparative Example 3 As the weakly basic anion exchange resin, an acrylic resin-based resin having a polyamine group as a weakly basic anion exchange group (macroporous type) was used. In the same manner as in Example 1, the electrolytic solution S was passed through a column packed with the weakly basic anion exchange resin, and the hydrofluoric acid concentration in the electrolytic solution was measured before and after passing the electrolytic solution. The results are shown in Table 1.
[0053] [Table 1]
[0054] (Reference example 1) The aqueous solution was passed through a column packed with a weakly basic anion exchange resin in the same manner as in Example 1, except that instead of the electrolyte solution in which LiPF6 was dissolved in a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of 1:1 to give a concentration of 1 mol / L, water in which hydrofluoric acid was dissolved to give a concentration of 100 mass ppm was passed through the column, and the hydrofluoric acid concentration in the electrolyte solution was measured before and after passing the aqueous solution through the column. The results are shown in Table 2.
[0055] (Reference example 2) The aqueous solution was passed through a column packed with a weakly basic anion exchange resin in the same manner as in Comparative Example 1, except that instead of the electrolyte solution in which LiPF6 was dissolved in a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of 1:1 to give a concentration of 1 mol / L, water in which hydrofluoric acid was dissolved to give a concentration of 100 mass ppm was passed through the column, and the hydrofluoric acid concentration in the electrolyte solution was measured before and after passing the aqueous solution through the column. The results are shown in Table 2.
[0056] (Reference example 3) The aqueous solution was passed through a column packed with a weakly basic anion exchange resin in the same manner as in Comparative Example 2, except that instead of the electrolyte solution in which LiPF6 was dissolved in a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of 1:1 to give a concentration of 1 mol / L, water in which hydrofluoric acid was dissolved to give a concentration of 100 mass ppm was passed through the column, and the hydrofluoric acid concentration in the electrolyte solution was measured before and after passing the aqueous solution through the column. The results are shown in Table 2.
[0057] (Reference example 4) The aqueous solution was passed through a column packed with a weakly basic anion exchange resin in the same manner as in Comparative Example 3, except that instead of the electrolyte solution in which LiPF6 was dissolved in a mixed solvent of ethylene carbonate (EC) and dimethyl carbonate (DMC) in a volume ratio of 1:1 to give a concentration of 1 mol / L, water in which hydrofluoric acid was dissolved to give a concentration of 100 mass ppm was passed through the column, and the hydrofluoric acid concentration in the electrolyte solution was measured before and after passing the aqueous solution through the column. The results are shown in Table 2.
[0058] [Table 2]
[0059] From Table 1, it can be seen that in Example 1, the treatment for removing acidic impurities from the lithium-based electrolyte-containing solution in which the lithium-based electrolyte is dispersed in the carbonate ester is carried out using a specific weakly basic anion exchange resin based on a styrene-based resin, and therefore the acidic impurities can be effectively removed.
[0060] On the other hand, from Table 1, it can be seen that in Comparative Examples 1 to 3, the treatment for removing acidic impurities from the lithium-based electrolyte-containing liquid in which the lithium-based electrolyte is dispersed in the carbonate ester is not performed using the specific weakly basic anion exchange resin, and therefore it is difficult to effectively remove the acidic impurities.
[0061] Moreover, from the results of Reference Examples 1 to 4 shown in Table 2, it is understood that when acidic impurities in water are removed, the acidic impurities can be effectively removed regardless of the type of ion exchange resin. [Industrial Applicability]
[0062] According to the present invention, there is provided an apparatus for producing a nonaqueous electrolyte solution that can easily prepare a nonaqueous electrolyte solution having a reduced content of acidic impurities such as hydrofluoric acid by effectively adsorbing the acidic impurities, and there is also provided a method for producing a nonaqueous electrolyte solution. [Explanation of symbols]
[0063] 1. Nonaqueous electrolyte manufacturing equipment 2. Acid Absorber
Claims
1. An electrolytic solution comprising an ion exchange section containing a weakly basic anion exchange resin for passing an alkali metal salt electrolyte-containing liquid in which an alkali metal salt electrolyte capable of decomposing into a carbonate ester to generate an acid is dissolved, to obtain a nonaqueous electrolyte solution; The weakly basic anion exchange resin has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): (However, R 1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bonding site with the substrate or a bonding group for bonding to the substrate. having a tertiary amino group represented by The apparatus for producing a non-aqueous electrolyte solution is characterized in that
2. 2. The apparatus for producing a non-aqueous electrolyte according to claim 1, wherein the styrene-based resin is a styrene-divinylbenzene copolymer.
3. The weakly basic anion exchange group is represented by the following general formula (II): (However, R 1 Groups and R 2 R 3 The group is a hydrocarbon group having 1 to 3 carbon atoms, and * indicates the bonding site with the substrate.
3. The apparatus for producing a non-aqueous electrolyte solution according to claim 1, wherein the tertiary amino group is represented by the following formula:
4. 4. The apparatus for producing a non-aqueous electrolyte according to claim 1, wherein the weakly basic anion exchange group represented by the general formula (I) or the general formula (II) is a dimethylaminomethyl group.
5. The apparatus for producing a non-aqueous electrolyte according to any one of claims 1 to 4, wherein the non-aqueous electrolyte is an electrolyte for a lithium ion battery.
6. A method for producing a non-aqueous electrolyte solution, comprising the steps of: an acid adsorption step of passing an alkali metal salt electrolyte-containing solution, in which an alkali metal salt electrolyte capable of being decomposed into a carbonate ester to generate an acid, through an ion exchange unit containing a weakly basic anion exchange resin to obtain a non-aqueous electrolyte; The weakly basic anion exchange resin has a styrene-based resin as a base and a weakly basic anion exchange group represented by the following general formula (I): (However, R 1 Groups and R 2 The groups are hydrocarbon groups having 1 to 3 carbon atoms and may be the same or different, and * indicates a bond to the substrate or a bonding group for bonding to the substrate.) having a tertiary amino group represented by The present invention relates to a method for producing a non-aqueous electrolyte solution.
7. 7. The method for producing a non-aqueous electrolyte according to claim 6, wherein the styrene-based resin is a styrene-divinylbenzene copolymer.
8. The weakly basic anion exchange group is represented by the following general formula (II): (However, R 1 Groups and R 2 R 3 The group is a hydrocarbon group having 1 to 3 carbon atoms, and * indicates the bonding site with the substrate. The method for producing a non-aqueous electrolyte solution according to claim 6 or 7, wherein the tertiary amino group is represented by the following formula:
9. 9. The method for producing a non-aqueous electrolyte solution according to claim 6, wherein the weakly basic anion exchange group represented by the general formula (I) or the general formula (II) is a dimethylaminomethyl group.
10. The method for producing a non-aqueous electrolyte according to any one of claims 6 to 9, wherein the non-aqueous electrolyte is an electrolyte for a lithium ion battery.
Citation Information
Patent Citations
Production of sulfide group-containing thiol compound
JP1998029971A
Method for removing acid from lithium salt solution
JP2000505042A
Higher Purification Methods for Hydrogen Peroxide Solutions
JP2003535007A
Zeolite for processing nonaqueous electrolyte and method for processing nonaqueous electrolyte
JP2011071111A