Atomic Layer Deposition of Electrochemical Catalysis
By functionalizing substrates and using atomic layer deposition with passivation, the method addresses PGM instability in PEM fuel cells, achieving stable, low-loading catalyst films with enhanced activity and scalability, reducing degradation and cost.
Patent Information
- Application Number
- JP2021202557
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-09-08
- Filing Date
- 2021-12-14
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2037-09-07
AI Technical Summary
State-of-the-art polymer electrolyte membrane (PEM) fuel cells face challenges due to the high cost and instability of platinum group metals (PGMs) used as catalysts, which are prone to degradation processes such as dissolution, corrosion, and agglomeration, necessitating excessive amounts to ensure longevity, and current synthesis methods lack scalability and control over catalyst shape and size.
The method involves functionalizing a substrate through treatments like plasma, ozone, or acid, followed by atomic layer deposition (ALD) to form a thin, conformal catalyst film, which can be directly applied to supports without specialized structures, using passivation to enhance uniformity and stability, reducing PGM loading and minimizing degradation.
This approach results in highly stable, low-loading catalyst films with increased mass activity and scalability, overcoming degradation issues and enabling efficient use of PGMs, even on complex substrates, while maintaining high surface exposure and uniform coverage.
Smart Images

Figure 0007573511000001 
Figure 0007573511000002 
Figure 0007573511000003
Abstract
Description
[Technical field]
[0001] CITED RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Application No. 62 / 385,135, filed September 8, 2016, the contents of which are incorporated herein by reference in their entirety. [Background technology]
[0002] background Polymer electrolyte membrane (PEM) fuel cells have great potential as a power source for applications such as zero-emission vehicles. However, state-of-the-art PEM fuel cells have several drawbacks. One of the most troublesome is the amount of expensive platinum group metals (PGMs), in the form of nano-sized particles (i.e., nanoparticles), that serve as electrochemical catalysts in the fuel cell's membrane electrode assembly (MEA). The amount of PGM catalyst is typically determined by the power specification per cell in the fuel cell stack. However, to allow for several decomposition processes and ensure reliable operation over the life of the fuel cell, a significant additional amount of PGM catalyst is typically included. Typical decomposition processes are associated with loss of PGM material or loss of catalytically active surface area and include dissolution and corrosion of PGM particles, PGM particle growth by Ostwald ripening, PGM particle agglomeration, PGM particle detachment from the carbonaceous support, and corrosion of the carbonaceous support.
[0003] Small PGM nanoparticles are often unstable under fuel cell conditions and may have a tendency to dissolve due to their high surface-to-volume ratio. Therefore, small PGM nanoparticles (e.g., less than about 2-3 nm) are often avoided. However, utilizing larger particles results in higher PGM loads, which increases costs. Proposed solutions to reduce the amount of PGM include alloying PGM with non-precious metals, core-shell structures of a non-precious metal core material coated with a PGM shell, or the formation of nanostructured thin films (NSTFs). Although alloyed catalysts initially exhibit enhanced catalytic activity, dissolution of the non-precious metal components can cause severe degradation of the alloyed catalyst. Furthermore, state-of-the-art synthesis techniques for PGM and PGM alloy catalysts typically rely on wet-chemistry type batch synthesis, which typically results in the growth of nanoparticles that are poorly scalable, typically have complex control over shape and size, and are vulnerable to corrosion, dissolution, and other decomposition processes. The proposed core-shell structure suffers from similar decomposition processes as PGM alloy catalysts, as the non-precious metal core material may tend to diffuse to the surface of the shell and dissolve under harsh PEM fuel cell conditions. Although NSTFs can provide high activity and high stability at low PGM loadings, the formation of NSTFs also involves specially structured supports. In the case of NSTFs, the PGMs are typically applied by physical vapor deposition (PVD), a non-conformal coating technique, so the support structure is limited to a unique "zigzag" configuration. Furthermore, NSTFs have severe water management issues due to their whisker-like structure, making them impractical to operate in low-temperature PEM fuel cells.
[0004] It is against this background that a need arose to develop the embodiments of the present disclosure. Summary of the Invention [Means for solving the problem]
[0005] Abstract In some embodiments, a method includes: (1) functionalizing a substrate to obtain a functionalized substrate; and (2) depositing a catalyst onto the functionalized substrate by atomic layer deposition to form a thin film of catalyst coating the functionalized substrate.
[0006] In some embodiments of the method, the substrate is a catalyst support.
[0007] In some embodiments of the method, the substrate is a porous conductive material.
[0008] In some embodiments of the method, the step of functionalizing the substrate comprises applying a plasma treatment, an ozone treatment, an acid treatment, or a peroxide treatment to the substrate.
[0009] In some embodiments of the method, applying a plasma treatment includes applying a hydrogen plasma, an oxygen plasma, or a nitrogen plasma.
[0010] In some embodiments of the method, depositing the catalyst comprises: a) introducing a precursor into a deposition chamber housing the functionalized substrate to deposit a catalytic material onto the functionalized substrate; and Injecting a passivating gas into the deposition chamber to passivate the surface of the material. performing an atomic layer deposition cycle, comprising: b) repeating a) multiple times to form a thin film of the catalyst.
[0011] In some embodiments of the method, depositing the catalyst comprises: a) introducing a first precursor into a deposition chamber containing a functionalized substrate such that the first precursor is adsorbed onto the functionalized substrate; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the functionalized substrate to obtain a catalytic material deposited on the functionalized substrate and to passivate the surface of the material; performing an atomic layer deposition cycle, comprising: b) repeating a) multiple times to form a thin film of the catalyst.
[0012] In a further embodiment, the method includes the steps of: (1) depositing a tie layer on a substrate to obtain a tie layer-coated substrate; and (2) depositing a catalyst on the tie layer-coated substrate by atomic layer deposition to form a thin film of catalyst coating the tie layer-coated substrate.
[0013] In some embodiments of the method, the substrate is a catalyst support.
[0014] In some embodiments of the method, the substrate is a porous conductive material.
[0015] In some embodiments of the method, the step of depositing the bonding layer is performed by atomic layer deposition.
[0016] In some embodiments of the method, the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide.
[0017] In some embodiments of the method, depositing the catalyst comprises: a) introducing a precursor into a deposition chamber containing the tie layer coated substrate to deposit a catalytic material onto the tie layer coated substrate; and introducing a passivating gas into the deposition chamber to passivate the surface of the material; performing an atomic layer deposition cycle, comprising: b) repeating a) multiple times to form a thin film of the catalyst.
[0018] In some embodiments of the method, depositing the catalyst comprises: a) introducing a first precursor into a deposition chamber containing the tie layer coated substrate; is adsorbed onto the tie layer coated substrate; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the tie layer coated substrate to obtain a catalytic material deposited on the tie layer coated substrate and to passivate the surface of the material; performing an atomic layer deposition cycle, comprising: b) repeating a) multiple times to form a thin film of the catalyst.
[0019] Additional embodiments are directed to structures obtained by the method of any of the preceding embodiments.
[0020] In some embodiments, the supported catalyst comprises: (1) a catalyst support; and (2) a thin film of catalyst coating the catalyst support, wherein the surface coverage of the catalyst support by the thin film is at least 80%, and the thin film has an average thickness in the range of 1 atomic layer to 5 atomic layers.
[0021] In some embodiments of the supported catalyst, the average thickness of the thin film ranges from 1 atomic layer to 3 atomic layers.
[0022] In some embodiments of the supported catalyst, the catalyst support is a carbonaceous support.
[0023] In some embodiments, the supported catalyst further comprises a tie layer disposed between the thin film and the catalyst support.
[0024] In some embodiments of the supported catalyst, the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide.
[0025] In some embodiments of the supported catalyst, the catalyst comprises a platinum group metal.
[0026] In a further embodiment, a fuel cell comprises: (a) a cathode electrocatalyst layer; (b) an anode electrocatalyst layer; and (c) a polymeric ion conducting membrane disposed between the cathode electrocatalyst layer and the anode electrocatalyst layer, wherein at least one of the cathode electrocatalyst layer or the anode electrocatalyst layer comprises the supported catalyst of any of the preceding embodiments.
[0027] In a further embodiment, a fuel cell comprises: (a) a first gas diffusion layer; (b) a second gas diffusion layer; and (c) a polymeric ion conductive membrane disposed between the first gas diffusion layer and the second gas diffusion layer, wherein at least one of the first gas diffusion layer or the second gas diffusion layer comprises the supported catalyst of any of the preceding embodiments.
[0028] In a further embodiment, the gas diffusion layer comprises: (1) a porous conductive material; and (2) a thin film of catalyst coating the porous conductive material.
[0029] In some embodiments of the gas diffusion layer, the porous conductive material comprises carbon cloth or carbon paper.
[0030] In some embodiments, the gas diffusion layer further comprises a tie layer disposed between the thin film and the porous conductive material.
[0031] In some embodiments of the gas diffusion layer, the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide.
[0032] In some embodiments of the gas diffusion layer, the catalyst comprises a platinum group metal.
[0033] Further embodiments are directed to a fuel cell including the gas diffusion layer of any of the preceding embodiments.
[0034] Other aspects and embodiments of the present disclosure are contemplated. The foregoing summary and the following detailed description are not intended to limit the disclosure to any specific embodiment, but are merely intended to describe some embodiments of the present disclosure.
[0035] For a better understanding of the nature and objectives of certain embodiments of the present disclosure, reference should be made to the following detailed description taken in conjunction with the accompanying drawings. [Brief description of the drawings]
[0036] [Figure 1] Figure 1. Schematic process flow for forming thin films of catalyst on a substrate, where the substrate is functionalized prior to catalyst deposition in the left panel, and a tie layer is deposited on the substrate prior to catalyst deposition in the right panel.
[0037] [Diagram 2] Figure 2. Schematic process flows for atomic layer deposition without passivation in the left panel, atomic layer deposition incorporating the use of a passivating precursor in the center panel, and atomic layer deposition incorporating the use of a passivating process gas in the right panel.
[0038] [Diagram 3] Figure 3. Schematic process flows for atomic layer deposition without passivation in the left panel, atomic layer deposition incorporating the use of a passivating precursor in the center panel, and atomic layer deposition incorporating the use of a passivating process gas in the right panel.
[0039] [Figure 4] Figure 4. Schematic of the supported catalyst architecture where in the left panel a thin film of catalyst coats a functionalized catalyst support, and in the right panel a thin film of catalyst coats a tie-layer coated catalyst support.
[0040] [Diagram 5] Figure 5. Schematic of the structure of a thin film of catalyst coating a porous conductive material that can be used as a gas diffusion layer.
[0041] [Figure 6] Figure 6. Schematic of the structure of a gas diffusion layer containing a supported catalyst.
[0042] [Figure 7] FIG. 7. Schematic of a PEM fuel cell incorporating the supported catalysts disclosed herein.
[0043] [Figure 8] FIG. 8 is a schematic diagram of a PEM fuel cell incorporating the catalytic structures disclosed herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0044] explanation The embodiments of the present disclosure are directed to an improved process for forming a substantially continuous thin film of PGM (or alloy or other multi-element material containing PGM) for highly stable and extremely low loading catalysts for fuel cells, including PEM fuel cells, and the resulting structure of the thin film coating a substrate. The formation of a substantially continuous thin film of catalyst provides high stability compared to nanoparticle morphology of catalysts, as a result of the substantial absence of noticeable surface defects, such as corners and edges, which are highly susceptible to decomposition and corrosion, and the thin film being substantially free of decomposition processes, such as Ostwald ripening and particle agglomeration, which affect nanoparticles. By using atomic layer deposition, the thin film of catalyst can be deposited in a highly conformal manner with reduced thickness. The reduced thickness of the thin film allows efficient use of the catalyst at lower loadings, and also increases the exposure of the surface atoms of the catalyst in the thin film. This results in higher mass activity. Additionally, atomic layer deposition provides greater scalability and conformal coatings, even on high surface area or high aspect ratio substrates, compared to wet chemistry type batch synthesis. Additionally, by functionalizing the substrate prior to catalyst deposition and / or depositing a tie layer on the substrate, thin films of catalyst can be formed on a variety of substrates without the need for specially structured supports. In some embodiments, thin films of catalyst can be formed on carbonaceous supports or other catalyst supports, and in other embodiments, thin films of catalyst can be formed directly on gas diffusion layers without the need for additional catalyst supports.
[0045] 1 is a schematic process flow for forming a thin film of a catalyst on a substrate, where in the left panel the substrate is functionalized before depositing the catalyst, and in the right panel a tie layer is deposited on the substrate before depositing the catalyst. In some embodiments, the substrate is a catalyst support, such as a carbon-containing support or a carbonaceous support, such as carbon nanotubes, carbon nanohorns, carbon nanofibers, carbon nanoribbons, graphite, graphene sheets, carbon black, conductive carbon black, graphitized carbon, activated carbon, etc., or other carbonaceous nanoparticles, or for example another non-carbon-based support, such as a metal oxide support, a metal nitride support, a metal carbide support, or other ceramic support. In other embodiments, the substrate is a porous conductive material that can be used as a gas diffusion layer, such as carbon cloth, carbon paper, or other carbonaceous or non-carbonaceous fibrous material. Other types of substrates can be used with appropriate selection or functionalization of the tie layer.
[0046] Referring to the left panel of FIG. 1, the process flow includes functionalizing a substrate to obtain a functionalized substrate, followed by depositing a catalyst on the functionalized substrate. Substrate functionalization is performed to introduce anchoring or functional groups to the surface of the substrate to enhance or promote chemical bonding with the precursor of the catalyst to be deposited on the substrate. In some embodiments, the substrate may be substantially devoid of anchoring groups and substantially inert to catalyst deposition prior to functionalization. For example, the basal surface of a pure graphene sheet may be substantially inert to atomic layer deposition of a PGM, such as platinum (Pt), and performing atomic layer deposition of Pt on a pure graphene sheet may result in the formation of Pt nanoparticles on the edges of the sheet. Functionalization of the graphene sheet may include, for example, sp , which promotes chemical bonding with the precursor of the catalyst. 3 -hybridized carbon (sp 2-hybridized carbon instead of the anchoring group. In other embodiments, the substrate contains some anchoring groups before functionalization, and functionalization of the substrate introduces additional anchoring groups to provide a higher density and uniformity of the anchoring groups across the surface of the substrate, facilitating the subsequent formation of a substantially continuous thin film of catalyst. Substrate functionalization may be performed by applying a plasma treatment, such as a hydrogen plasma, an oxygen plasma, or a nitrogen plasma, which may result in the formation of, for example, hydrogen-containing anchoring groups (e.g., hydrogenation to introduce -CH groups), oxygen-containing anchoring groups (e.g., groups containing -CO- or carbonyl moieties), nitrogen-containing anchoring groups, or combinations of such groups. Instead of or in combination with plasma treatment, substrate functionalization may be performed by ozone treatment, for example, acid (e.g., oxidizing acid treatment using boiling nitric acid), wet chemical treatment using base, peroxide treatment, or other reactive compounds, or by thermal treatment.
[0047] With further reference to the left panel of Figure 1, the step of depositing the catalyst onto the functionalized substrate is performed by chemical vapor deposition, in particular atomic layer deposition, which in some embodiments may be performed without a passivation treatment and in other embodiments with a passivation treatment.
[0048] 2 is a schematic process flow for atomic layer deposition of a catalyst using atomic layer deposition without passivation in the left panel, a passivating precursor in the center panel, and a passivating gas in the right panel. Although FIG. 2 illustrates deposition of the catalyst as a single element material, e.g., a single PGM, deposition of binary, ternary, or other multi-element materials is also contemplated by the present disclosure. and is further described below. The atomic layer deposition process flow includes performing a first atomic layer deposition cycle to deposit material on a substrate held in a deposition chamber, followed by a second atomic layer deposition cycle to deposit material on the substrate, followed by a third atomic layer deposition cycle to deposit material on the substrate, etc., until the required amount of material is deposited.
[0049] Referring to the process flow in the left panel of FIG. 2, performing each atomic layer deposition cycle includes sequentially exposing a substrate, or a portion of a substrate, to a deposition gas that includes a first precursor containing the material to be deposited, and a deposition gas that includes a second oxidizing precursor. In the case of a single element material, for example, the first precursor may be a precursor containing a PGM, such as an organometallic compound in which the PGM is coordinated with an organic ligand, and the second oxidizing precursor may be oxygen, ozone, or oxygen plasma. For example, in the specific case of Pt, the first precursor may be (methylcyclopentadienyl)trimethylplatinum or another organometallic compound containing Pt. In addition to Pt, deposition may also be performed with other PGMs, such as ruthenium (Ru), rhodium (Rh), palladium (Pd), osmium (Os), and iridium (Ir), as well as other precious metals, such as silver (Ag) and gold (Au). During the first atomic layer deposition cycle, the first precursor is introduced into the chamber, where it is adsorbed on the substrate in the form of molecules of the first precursor, residues of molecules of the first precursor, or a combination of both, and the second oxidized precursor is introduced into the chamber, whereby a reaction between the adsorbed first precursor and the second oxidized precursor occurs, liberating the ligands contained in the adsorbed first precursor, thereby leaving the material deposited on the substrate. The anchoring groups on the substrate (introduced by functionalization) promote a higher density and more uniform adsorption of the first precursor to the substrate. In some embodiments, the anchoring groups on the substrate may react with the adsorbed first precursor to form bonds or links between carbon atoms of the substrate and metal atoms contained in the adsorbed first precursor, either directly or indirectly through one or more intervening atoms such as oxygen or nitrogen atoms. A second reduced precursor, such as hydrogen or hydrogen plasma, may be used instead of or in combination with the second oxidized precursor. The introduction of each precursor may be followed by a removal operation to remove reaction products and any unreacted precursor, for example by evacuation or purging with an inert carrier gas.
[0050] Referring to the process flow in the right panel of FIG. 2, after the introduction of the precursor in each atomic layer deposition cycle, including the first atomic layer deposition cycle, and before the introduction of the precursor in a subsequent atomic layer deposition cycle, a passivation gas is introduced into the chamber. The passivation gas acts to adjust or change the adsorption energy between the first precursor and the already deposited material, making this adsorption energy less favorable, so that the adsorption of the subsequent first precursor is preferential or promoted to cover the open areas of the substrate rather than the already deposited material. In this way, the use of the passivation gas enhances the distribution of the first precursor along the substrate, and enhances, more uniform, and allows for control over the coverage of the deposited material along the substrate. In some embodiments, the criteria for the passivating gas include one or more of the following: 1) the adsorption ability in the deposited material; 2) exhibit a higher adsorption tendency or stronger adsorption to the deposited material compared to the substrate; 3) form an intermediate species after the passivating gas is adsorbed to the deposited material; and 4) the adsorption energy of the first precursor to the intermediate species is greater than about -10 kJ / mol (e.g., less negative or more positive) (or greater than about -0.104 eV), such as about -5 kJ / mol or more (or about -0.052 eV or more), about 0 kJ / mol or more (or about 0 eV or more), or about 10 kJ / mol or more (or about 0.104 eV or more), or the adsorption energy of the first precursor to the intermediate species is greater than the adsorption energy of the first precursor to the substrate. For example, in the case of Pt or another single element material, the passivating gas may be carbon monoxide (CO). In addition to CO, other non-cancerous substances that meet the above criteria Passivating gases such as ammonia (NH3), nitric oxide (NO), and methane (CH4) can be used. The process temperature can be controlled to inhibit desorption of the passivating gas. For example, in the case of CO, or another passivating gas, the temperature of the substrate can be controlled to be in the range of about 50°C to about 250°C, about 80°C to about 200°C, or about 100°C to about 150°C.
[0051] Referring now to the process flow in the center panel of FIG. 2, the step of performing each atomic layer deposition cycle includes sequentially exposing the substrate, or a portion of the substrate, to a deposition gas that includes a first precursor containing the material to be deposited, and a deposition gas that includes a second passivating precursor. Certain aspects of the process flow in the center panel may be performed similarly to those described above for the right panel, and such aspects will not be repeated. Here, the passivating precursor serves two functions: reacting with the first precursor adsorbed on the substrate to liberate ligands contained in the adsorbed first precursor, and adjusting or changing the adsorption energy between the first precursor and the already deposited material, making this adsorption energy less favorable, so that the adsorption of the subsequent first precursor is preferential or promoted for the coverage of the open areas of the substrate rather than the already deposited material. In this way, the use of the passivating precursor enhances the distribution of the first precursor along the substrate, and enhances, more uniform, and allows for control over the coverage of the deposited material along the substrate. In some embodiments, the criteria for the passivating precursor include one or more of the following: 1) the ability to react with the first precursor to form an intermediate species; and 2) the adsorption energy of the first precursor to the intermediate species is greater than about -10 kJ / mol (e.g., less negative or more positive) (or greater than about -0.104 eV), such as about -5 kJ / mol or greater (or about -0.052 eV or greater), about 0 kJ / mol or greater (or about 0 eV or greater), or about 10 kJ / mol or greater (or about 0.104 eV or greater), or the adsorption energy of the first precursor to the intermediate species is greater than the adsorption energy of the first precursor to the substrate. In some embodiments, the passivating precursor comprises a passivating ligand or another passivating chemical moiety that remains adsorbed on the first precursor after reaction of the passivating precursor with the first precursor. For example, the passivating moiety may have a chemical structure that corresponds to or is similar to that of the passivating gas described above.
[0052] In addition to the deposition of single elemental materials described above, atomic layer deposition may also be applied to the deposition of multi-elemental materials. FIG. 3 is a schematic process flow of atomic layer deposition of a catalyst using atomic layer deposition without passivation in the left panel, passivation precursor in the center panel, and passivation gas in the right panel. Although FIG. 3 illustrates the deposition of a catalyst as a binary elemental material as an example, deposition of ternary elemental materials or other multi-elemental materials is also encompassed in the present disclosure. The process flow of atomic layer deposition includes performing a first atomic layer deposition cycle to deposit material on a substrate held in a deposition chamber, followed by a second atomic layer deposition cycle to deposit material on the substrate, followed by a third atomic layer deposition cycle to deposit material on the substrate, and so on until the required amount of material is deposited. Certain aspects of the process flow in FIG. 3 may be performed similarly to those described above for FIG. 2, and such aspects will not be repeated.
[0053] Referring to the process flow in the left panel of FIG. 3, performing each atomic layer deposition cycle includes sequentially exposing the substrate, or a portion of the substrate, to a deposition gas including a first precursor containing a first element of the material to be deposited, a deposition gas including a second precursor containing a second element of the material to be deposited, and a deposition gas including a third oxidizing precursor. In the case of a binary element material, for example, the first precursor and the second precursor may be precursors containing different metals, e.g., different organometallic compounds in which each metal is coordinated with an organic ligand. The first element may be a PGM and the second element may be a different PGM, or other noble metal. The precursor may be a metal, or other transition metal, such as scandium (Sc), titanium (Ti), vanadium (V), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), copper (Cu) or zinc (Zn). During the first atomic layer deposition cycle, the first precursor is introduced into the chamber, causing the first precursor to be adsorbed on the substrate, the second precursor is introduced into the chamber, causing the second precursor to be adsorbed on the substrate, and the third oxidizing precursor is introduced into the chamber, causing a reaction between the adsorbed first precursor, the adsorbed second precursor and the third oxidizing precursor to liberate ligands contained in the adsorbed first precursor and the adsorbed second precursor, thereby leaving the material deposited on the substrate. A third reducing precursor, such as hydrogen or hydrogen plasma, can be used instead of or in combination with the third oxidizing precursor. Also, the second precursor can perform an oxidizing or reducing action on the first precursor, such that a separate oxidizing or reducing precursor can be omitted. The introduction of each precursor may be followed by a removal operation to remove reaction products and any unreacted precursor, for example by evacuation or purging with an inert carrier gas.
[0054] Referring to the process flow in the right panel of FIG. 3, after the introduction of precursors in each atomic layer deposition cycle and before the introduction of precursors in the subsequent atomic layer deposition cycle, a passivation gas is introduced into the chamber. The passivation gas acts to adjust or change the adsorption energy between the first precursor and the already deposited material and between the second precursor and the already deposited material to make such adsorption energy less favorable, so that the adsorption of the subsequent first and second precursors is preferential or promoted to cover the open areas of the substrate rather than the already deposited material. In this way, the use of the passivation gas enhances the distribution of the first and second precursors along the substrate, which enhances, more uniform, and allows for control over the coverage of the deposited material along the substrate. It is also contemplated that two or more different passivation gases may be used, e.g., a first passivation gas that preferentially adsorbs to a first element of the deposited material, adjusting or changing the adsorption energy for the first element, and a second passivation gas that preferentially adsorbs to a second element of the deposited material, adjusting or changing the adsorption energy for the second element.
[0055] Referring now to the process flow in the center panel of Figure 3, performing each atomic layer deposition cycle involves sequentially exposing the substrate, or a portion of the substrate, to a deposition gas including a first precursor containing a first element of the material to be deposited, a deposition gas including a second precursor containing a second element of the material to be deposited, and a deposition gas including a third passivating precursor, where the passivating precursor serves two functions: reacting with the first and second precursors adsorbed on the substrate to liberate ligands contained in the adsorbed first and second precursors, and adjusting or changing the adsorption energies between the first and second precursors and previously deposited materials, making such adsorption energies less favorable, such that subsequent adsorption of the first and second precursors is preferentially or favored towards coverage of open areas of the substrate rather than previously deposited materials. In this manner, the use of a passivating precursor enhances the dispersion of the first and second precursors along the substrate, providing enhanced, more uniform, and controlled coverage of the deposited material along the substrate. It is also envisioned that two or more different passivating precursors can be used, for example, a first passivating precursor that reacts preferentially with a first precursor adsorbed on the substrate to adjust or change the adsorption energy for a first element, and a second passivating precursor that reacts preferentially with a second precursor adsorbed on the substrate to adjust or change the adsorption energy for a second element.
[0056] Referring again to FIG. 1, and in particular to the right panel of FIG. 1, the process flow includes depositing a tie layer on a substrate to obtain a tie layer coated substrate, followed by depositing a catalyst on the tie layer coated substrate. The tie layer provides a high thermal conductivity for both the substrate and the catalyst to improve stability. The bonding layer may include a material that strongly bonds to the substrate. In some embodiments, the bonding layer may include an anchoring group or a functional group on the surface of the bonding layer to enhance or promote chemical bonding with the precursor of the catalyst to be deposited on the substrate. The bonding layer may provide additional benefits, such as increased catalytic activity, due to structural effects (e.g., lattice distortion) and electronic effects (e.g., d-band center shift). Examples of bonding layer materials include metal oxides, metalloid oxides, metal nitrides, metalloid nitrides, metal carbides, metalloid carbides, and other ceramics. The step of depositing the bonding layer is performed by chemical vapor deposition, particularly atomic layer deposition. In the case of a binary element material, for example, the step of performing each atomic layer deposition cycle includes sequentially exposing the substrate, or a portion of the substrate, to a deposition gas that includes a first precursor containing a first element of the material to be deposited, a deposition gas that includes a second precursor containing a second element of the material to be deposited, and a deposition gas that includes a third oxide precursor. For example, the first element may be a metal or metalloid, and the second element may be oxygen, nitrogen, or carbon. A third reduced precursor may be used in place of or in combination with a third oxidized precursor. Also, the second precursor may perform an oxidizing or reducing action on the first precursor, such that a separate oxidizing or reducing precursor may be omitted. Certain aspects of the atomic layer deposition of the bonding layer may be performed similarly to those described above with respect to FIG. 3, and such aspects will not be repeated. The average thickness of the bonding layer may range from about 1 nm to about 100 nm or more, for example, from about 1 nm to about 50 nm, from about 1 nm to about 40 nm, from about 1 nm to about 30 nm, from about 1 nm to about 20 nm, or from about 1 nm to about 10 nm.
[0057] Following the step of depositing the tie layer, the step of depositing the catalyst on the tie layer coated substrate is performed by chemical vapor deposition, in particular atomic layer deposition. The atomic layer deposition of the catalyst may be performed without passivation treatment in some embodiments and with passivation treatment in other embodiments. Certain aspects of the atomic layer deposition of the catalyst may be performed similarly to those described above with respect to Figures 2 and 3, and such aspects will not be repeated. Although Figure 1 illustrates functionalization of the substrate and alternatively deposition of a tie layer, in other embodiments, either treatment may be performed. For example, the substrate may be functionalized to obtain a functionalized substrate, followed by deposition of a tie layer on the functionalized substrate, followed by deposition of the catalyst.
[0058] Referring to both the left and right panels of FIG. 1, deposition of catalyst with atomic layer deposition forms a substantially continuous thin film of catalyst with high stability and very low catalyst loading. Compared to atomic layer deposition without passivation, atomic layer deposition incorporating passivation allows greater control over deposition to achieve enhanced coverage of deposited catalyst down to a thickness of a single atomic layer or a few atomic layers. By incorporating passivation, the process flow exhibits self-limiting monolayer (or near monolayer) deposition of catalyst, overcoming nucleation tendencies that may otherwise constrain the required minimum coverage thickness of the substrate (typically a few atomic layers). Moreover, the process flow incorporating passivation still retains the advantages of atomic layer deposition, including self-saturation for greater thickness control, and the ability to conformally deposit materials on high surface area or high aspect ratio surfaces.
[0059] In some embodiments, the resulting catalyst thin film exhibits a surface coverage of the substrate of at least about 30%, e.g., at least about 40%, at least about 50%, at least about 60%, at least about 70%, at least about 80%, at least about 90%, at least about 95%, at least about 98%, at least about 98.5%, or at least about 99%, and up to about 100%, an average thickness in the range of about 1 to about 5 atomic layers, about 1 to about 4 atomic layers, about 1 to about 3 atomic layers, about 1 to about 2 atomic layers, or about 1 to about 1.5 atomic layers, and a surface roughness (root mean square) of about 80% or less of the average thickness, e.g., about 70% or less, about 60% or less, about 50% or less, about 40% or less, about 30% or less, about 20% or less, about 15% or less, or about 10% or less. The surface coverage of the thin film can be measured using imaging techniques, e.g., transmission electron microscopy ( The thickness of the atomic layer can be evaluated using TEM (transmission electron microscope) or scanning electron microscope (TEM) images, backscattering spectroscopy, X-ray photoelectron spectroscopy (XPS), or inductively coupled plasma mass spectrometry (ICP-MS). In the case of single element materials, one atomic layer can correspond to the thickness of a monolayer of atoms of the element. In the case of a binary element material with a molar composition of a% of the first element and b% of the second element, one atomic layer can correspond to the thickness of a monolayer of atoms with effective size given by (a / 100) x (atomic size of the first element) + (b / 100) x (atomic size of the second element). For ternary or other multi-element materials, a similar weighted average according to the molar composition can be used to determine the thickness of one atomic layer.
[0060] FIG. 4 is a schematic diagram of the structure of supported catalysts, where in the left panel a thin film of catalyst 400 covers a functionalized catalyst support 402, and in the right panel a thin film of catalyst 404 covers a catalyst support 406 coated with a bonding layer 408. Here, the catalyst support 402 or 406 is in the form of nanoparticles, e.g., carbonaceous nanoparticles, having a size ranging from about 5 nm to about 500 nm or more, e.g., from about 10 nm to about 400 nm, from about 10 nm to about 300 nm, from about 10 nm to about 200 nm, from about 10 nm to about 150 nm, or from about 10 nm to about 100 nm, and having an aspect ratio of about 3 or less, or about 2 or less. Other types of catalyst supports, e.g., carbon nanohorns, carbon nanofibers, carbon nanoribbons, graphite, and graphene sheets, as well as non-carbon-based supports, may be used. Referring to the left panel of FIG. 4, the catalyst support 402 is functionalized to facilitate bonding with the catalyst 400 deposited on the functionalized catalyst support 402. Referring to the right panel of FIG. 4, a tie layer 408 coats the catalyst support 406 and is disposed between the thin film of catalyst 404 and the catalyst support 406 .
[0061] 5 is a schematic diagram of the structure of a thin film of catalyst coating a porous conductive material that can be used as a gas diffusion layer. Here, the porous conductive material is in the form of a carbonaceous fibrous material, such as carbon cloth or carbon paper, although other carbonaceous or non-carbonaceous fibrous materials may be used. With reference to FIG. 5, individual fibers 500 of the carbonaceous fibrous material are conformally coated with a thin film of catalyst 502; in some embodiments, the fibers 500 can be functionalized to promote bonding with the catalyst 502, and in other embodiments, a bonding layer can be deposited to conformally coat the fibers 500 and can be disposed between the thin film of catalyst 502 and the fibers 500.
[0062] 6 is a schematic diagram of the structure of a gas diffusion layer that includes a carbonaceous fibrous layer 600, such as carbon cloth or carbon paper, although other carbonaceous or non-carbonaceous fibrous materials can be used. The gas diffusion layer also includes a mesoporous layer 602. The carbonaceous fibrous layer 600 is coated by the mesoporous layer 602. The mesoporous layer 602 includes a supported catalyst 604 with a polymeric binder and a fluorinated polymer to control water transport. The supported catalyst 604 can be implemented as described in connection with FIG. 4.
[0063] A variety of fuel cell applications can benefit from the catalyst structures disclosed herein. Examples include:
[0064] 1) Fuel cell vehicles, such as cars, buses, trucks, and motorcycles;
[0065] 2) Stationary fuel cell applications; and
[0066] 3) Including fuel cells in home appliances.
[0067] Various types of fuel cells can benefit from the catalyst structures disclosed herein. Examples include H2-PEM fuel cells, methanol fuel, and ethanol fuel cells, among others.
[0068] FIG. 7 is a schematic diagram of a PEM fuel cell incorporating the supported catalysts disclosed herein. The fuel cell includes a polymeric ion conducting membrane 700 disposed between a cathode electrocatalyst layer 702 and an anode electrocatalyst layer 704, which together constitute the membrane electrode assembly of the fuel cell. The fuel cell also includes electrically conducting flow field plates 706 and 708, which may be bipolar or unipolar plates. Gas diffusion layers 710 and 712 are also interposed between the flow field plates 706 and 708 and the electrocatalyst layers 702 and 704. Either the cathode electrocatalyst layer 702 or the anode electrocatalyst layer 704, or both, may include the supported catalysts disclosed herein. For example, the supported catalysts may be incorporated in the cathode electrocatalyst layer 702 to promote oxygen reduction reaction on the cathode side, and may be incorporated in the anode electrocatalyst layer 704 to promote hydrogen oxidation reaction on the anode side.
[0069] FIG. 8 is a schematic diagram of another PEM fuel cell incorporating the catalyst structure disclosed herein. The fuel cell includes a polymeric ion conducting membrane 800 disposed between gas diffusion layers 802 and 804, which in turn are disposed between electrically conductive flow field plates 806 and 808, which may be bipolar or unipolar plates. Either the gas diffusion layer 802 on the cathode side or the gas diffusion layer 804 on the anode side, or both, may include a catalyst coating a porous conductive material or a thin film of a supported catalyst. For example, a catalyst may be incorporated in the gas diffusion layer 802 to promote an oxygen reduction reaction on the cathode side, and may also be incorporated in the gas diffusion layer 804 to promote a hydrogen oxidation reaction on the anode side. By forming the catalyst directly in the gas diffusion layer 802 or 804 or by incorporating the catalyst, an additional layer including a catalyst support may be omitted.
[0070] As used herein, the singular terms "a," "an," and "the" may include plural referents unless the context clearly dictates otherwise. Thus, for example, a reference to an object may include a plurality of objects unless the context clearly dictates otherwise.
[0071] As used herein, the terms "substantially", "substantial" and "about" are used to describe and explain small differences. When used with an event or situation, these terms can refer to the exact occurrence of the event or situation, and the approximate occurrence of the event or situation. For example, when used with a numerical value, this term can include a difference of less than or equal to ±10% of the numerical value, such as less than or equal to ±5%, less than or equal to ±4%, less than or equal to ±3%, less than or equal to ±2%, less than or equal to ±1%, less than or equal to ±0.5%, less than or equal to ±0.1%, or less than or equal to ±0.05%.
[0072] As used herein, the term "size" refers to a characteristic dimension of an object. Thus, for example, the size of an object that is spherical may refer to the diameter of the object. In the case of an object that is non-spherical, the size of the object may refer to the diameter of a corresponding spherical object, which exhibits or has a specific inducible or measurable set of properties that are substantially the same as those of the non-spherical object. When a set of objects is referred to as having a particular size, it is assumed that the objects may have a size distribution around the particular size. Thus, as used herein, the size of a set of objects may refer to a typical size of the size distribution, such as an average size, a median size, or a peak size.
[0073] In the description of some embodiments, an object is "on" another object means that the former object is directly on (e.g., in physical contact with) the latter object, and also means that the former object is directly on (e.g., in physical contact with) the latter object, and that the latter object is in contact with (e.g., in contact with) one or more other objects. This may include cases where multiple intervening objects are located between the former object and the latter object.
[0074] Furthermore, amounts, ratios and other numerical values may be presented in range format herein. It should be understood that such range format is used for convenience and brevity, and includes numerical values expressly defined as the limits of the range, but should be understood to be flexible to include all individual numerical values or subranges contained within the range as if each numerical value and subrange were expressly defined. For example, the range of about 1 to about 200 should be understood to include the limits of about 1 and about 200 expressly stated, and also include individual values such as about 2, about 3, and about 4, and subranges such as about 10 to about 50, about 20 to about 100, etc.
[0075] Although the present disclosure has been described with respect to its specific embodiments, it should be understood by those skilled in the art that various modifications may be made and equivalents may be substituted without departing from the true spirit and scope of the present disclosure as defined in the appended claims. Furthermore, many modifications may be made to adapt a particular situation, material, composition of matter, method, operation(s) to the objective, spirit and scope of the present disclosure. All such modifications are intended to be within the scope of the claims appended hereto. In particular, although a particular method may be described with specific operations performed in a specific order, it is understood that these operations may be combined, sub-divided, or reordered to form equivalent methods without departing from the teachings of the present disclosure. Thus, unless specifically indicated herein, the order and grouping of operations are not limitations of the present disclosure.
[0076] According to a preferred embodiment of the present invention, for example, the following is provided: (Section 1) functionalizing the substrate to obtain a functionalized substrate; and depositing a catalyst onto the functionalized substrate by atomic layer deposition to form a thin film of the catalyst coating the functionalized substrate. A method comprising: (Section 2) 2. The method according to claim 1, wherein the substrate is a catalyst support. (Section 3) 2. The method according to claim 1, wherein the substrate is a porous conductive material. (Section 4) 2. The method of claim 1, wherein the step of functionalizing the substrate comprises applying a plasma treatment, an ozone treatment, an acid treatment, or a peroxide treatment to the substrate. (Section 5) 5. The method according to claim 4, wherein the applying of the plasma treatment comprises applying a hydrogen plasma, an oxygen plasma, or a nitrogen plasma. (Section 6) The step of depositing the catalyst comprises: 1) introducing a precursor into a deposition chamber containing the functionalized substrate to deposit the catalytic material onto the functionalized substrate; and introducing a passivating gas into the deposition chamber to passivate the surface of the material; performing an atomic layer deposition cycle comprising: 2) repeating step 1) multiple times to form the thin film of the catalyst. The method according to claim 1, comprising: (Section 7) The step of depositing the catalyst further comprises: 1) introducing a first precursor into a deposition chamber containing the functionalized substrate such that the first precursor is adsorbed onto the functionalized substrate; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the functionalized substrate to obtain the catalytic material deposited on the functionalized substrate and to passivate the surface of the material; performing an atomic layer deposition cycle comprising: 2) repeating step 1) multiple times to form the thin film of the catalyst. The method according to claim 1, comprising: (Section 8) depositing a tie layer on the substrate to obtain a tie layer coated substrate; and depositing a catalyst onto the tie layer coated substrate by atomic layer deposition to form a thin film of the catalyst covering the tie layer coated substrate. A method comprising: (Section 9) 9. The method according to item 8, wherein the substrate is a catalyst support. (Section 10) 9. The method according to claim 8, wherein the substrate is a porous conductive material. (Section 11) 9. The method according to claim 8, wherein the step of depositing the bonding layer is performed by atomic layer deposition. (Section 12) 9. The method of claim 8, wherein the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide. (Section 13) The step of depositing the catalyst further comprises: 1) introducing a precursor into a deposition chamber containing the tie layer coated substrate to deposit the catalytic material onto the tie layer coated substrate; and introducing a passivating gas into the deposition chamber to passivate the surface of the material; performing an atomic layer deposition cycle comprising: 2) repeating step 1) multiple times to form the thin film of the catalyst. 9. The method according to claim 8, comprising: (Section 14) The step of depositing the catalyst further comprises: 1) introducing a first precursor into a deposition chamber containing the tie layer coated substrate such that the first precursor is adsorbed onto the tie layer coated substrate; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the tie layer coated substrate to obtain the catalytic material deposited on the tie layer coated substrate and to passivate the surface of the material; performing an atomic layer deposition cycle comprising: 2) repeating step 1) multiple times to form the thin film of the catalyst. 9. The method according to claim 8, comprising: (Section 15) 15. A structure obtainable by the method according to any one of items 1 to 14 above. (Section 16) A catalyst support, and A thin film of catalyst covering the catalyst support wherein a surface coverage of the catalyst support with the thin film is at least 80%, and the thin film has an average thickness in the range of 1 atomic layer to 5 atomic layers. (Section 17) Item 17. The supported catalyst according to item 16, wherein the average thickness of the thin film is in the range of one atomic layer to three atomic layers. (Section 18) 17. The supported catalyst according to item 16, wherein the catalyst support is a carbonaceous support. (Section 19) 17. The supported catalyst of claim 16, further comprising a bonding layer disposed between the thin film and the catalyst support. (Section 20) 20. The supported catalyst of claim 19, wherein the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide. (Section 21) 17. The supported catalyst of claim 16, wherein the catalyst comprises a platinum group metal. (Section 22) A cathode electrocatalyst layer; an anode electrocatalyst layer; and a polymeric ion-conducting membrane disposed between the cathode electrocatalyst layer and the anode electrocatalyst layer; 22. A fuel cell comprising: at least one of the cathode electrocatalyst layer or the anode electrocatalyst layer comprising the supported catalyst of any one of claims 16 to 21 above. (Section 23) A first gas diffusion layer; A second gas diffusion layer, and a polymeric ion conductive membrane disposed between the first gas diffusion layer and the second gas diffusion layer; 22. A fuel cell comprising: at least one of the first gas diffusion layer or the second gas diffusion layer comprising the supported catalyst according to any one of claims 16 to 21. (Section 24) a porous conductive material, and A thin film of catalyst coating the porous conductive material. A gas diffusion layer comprising: (Section 25) 25. The gas diffusion layer according to item 24, wherein the porous conductive material comprises carbon cloth or carbon paper. (Section 26) 25. The gas diffusion layer according to claim 24, further comprising a bonding layer disposed between the thin film and the porous conductive material. (Section 27) 27. The gas diffusion layer according to claim 26, wherein the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide. (Section 28) 25. The gas diffusion layer according to item 24, wherein the catalyst comprises a platinum group metal. (Section 29) 29. A fuel cell comprising the gas diffusion layer according to any one of items 24 to 28.
Claims
1. Catalyst carrier, a thin film of catalyst coating the catalyst support; and a bonding layer disposed between the thin film and the catalyst support, wherein the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide. A supported catalyst comprising: wherein the catalyst support is a carbonaceous catalyst support, wherein the catalyst comprises a platinum group metal; wherein the surface coverage of the catalyst support by the thin film is at least 80%, and the thin film has an average thickness in the range of 1 atomic layer to 5 atomic layers; and below: A1-a) introducing a precursor into a deposition chamber containing the catalyst support to deposit the catalyst material onto the catalyst support; and introducing a passivating gas into the deposition chamber to passivate the surface of the material; or performing an atomic layer deposition cycle comprising: A1-b) introducing a first precursor into a deposition chamber containing the catalyst support such that the first precursor is adsorbed onto the catalyst support; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the catalyst support to obtain a material of the catalyst deposited on the catalyst support and to passivate the surface of the material; performing an atomic layer deposition cycle comprising: A2) Repeating A1-a) or A1-b) multiple times to form the thin film of the catalyst. The thin film of the catalyst is deposited on the catalyst support by a method comprising: Supported catalyst.
2. 2. The supported catalyst of claim 1, wherein the average thickness of the thin film is in the range of 1 atomic layer to 3 atomic layers.
3. a cathode electrocatalyst layer; an anode electrocatalyst layer; and a polymeric ion-conducting membrane disposed between the cathode electrocatalyst layer and the anode electrocatalyst layer; 3. A fuel cell comprising: at least one of the cathode electrocatalyst layer or the anode electrocatalyst layer comprising the supported catalyst of claim 1 or 2.
4. A first gas diffusion layer; A second gas diffusion layer, and a polymeric ion conductive membrane disposed between the first gas diffusion layer and the second gas diffusion layer; 3. A fuel cell comprising: at least one of the first gas diffusion layer or the second gas diffusion layer comprising the supported catalyst of claim 1 or 2.
5. a porous conductive material, and A thin film of catalyst coating the porous conductive material. A gas diffusion layer comprising: wherein the porous conductive material is a carbonaceous material; wherein the catalyst comprises a platinum group metal; where: A1-a) introducing a precursor into a deposition chamber containing the porous conductive material to deposit the catalyst material onto the porous conductive material; and introducing a passivating gas into the deposition chamber to passivate a surface of the material of the catalyst; or performing an atomic layer deposition cycle comprising: A1-b) introducing a first precursor into a deposition chamber containing the porous conductive material such that the first precursor is adsorbed onto the catalyst support; and introducing a second passivating precursor into the deposition chamber to react with the first precursor adsorbed on the porous conductive material to obtain the catalytic material deposited on the porous conductive material and to passivate the surface of the catalytic material; performing an atomic layer deposition cycle comprising: A2) Repeating A1-a) or A1-b) multiple times to form the thin film of the catalyst. the thin film of the catalyst is deposited on the porous conductive material by a method comprising: Here, the surface coverage of the porous conductive material by the thin film is at least 80%, and the thin film has an average thickness in the range of 1 atomic layer to 5 atomic layers. Gas diffusion layer.
6. The gas diffusion layer of claim 5 , wherein the porous conductive material comprises carbon cloth or carbon paper.
7. The gas diffusion layer of claim 5 further comprising a tie layer disposed between the thin film and the porous conductive material.
8. 8. The gas diffusion layer of claim 7, wherein the bonding layer comprises at least one of a metal oxide, a metalloid oxide, a metal nitride, a metalloid nitride, a metal carbide, or a metalloid carbide.
9. A fuel cell comprising a gas diffusion layer according to any one of claims 5 to 8.
Citation Information
Patent Citations
Porous fuel cell electrode structure having a conformal conductive layer on its surface
JP2005530307A
Pt-HIGH DISPERSION SUPPORTED CATALYST AND MANUFACTURING METHOD OF THE SAME
JP2013046883A
Thin-film catalyst materials for use in fuel cells
JP2015512782A
Core-shell structured nanosheet
JP2017127799A
Nucleation of Ultrathin, Continuous, Conformal Metal Films Using Atomic Layer Deposition And Application As Fuel Cell Catalysts
US20120100301A1