Repair structure and repair method for electric furnace taphole bricks
The use of a castable construction body with coarse particles between taphole bricks and an iron pipe addresses the peeling issue, forming a dense structure that prolongs the lifespan of taphole bricks in electric furnaces.
Patent Information
- Application Number
- JP2021047637
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-22
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-03-22
AI Technical Summary
Existing repair materials for taphole bricks in electric furnaces peel off due to friction and heat from molten steel during tapping, necessitating frequent replacement.
A repair structure and method using a castable construction body with coarse particles, such as alumina-magnesia, between the taphole brick and an iron pipe, ensuring a gap of 30 mm or more, which is less prone to peeling and cracking.
The castable construction body with coarse particles forms a dense structure, reducing peeling and cracking, allowing extended use of taphole bricks without frequent replacement.
Smart Images

Figure 0007575318000002 
Figure 0007575318000003 
Figure 0007575318000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a repair structure and a repair method for a taphole brick arranged on the inner periphery of a taphole at the bottom of an electric furnace. [Background technology]
[0002] When molten steel is transferred from an electric furnace to a ladle, it is tapped from a taphole at the bottom of the electric furnace. Taphole bricks are installed on the inner circumference of the taphole, and they melt when they come into contact with molten steel. For this reason, it was necessary to replace the taphole bricks after each specified number of uses. Since replacing taphole bricks takes time, Patent Document 1 proposes repairing the taphole bricks using mortar as a repair material to extend their lifespan. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2001-215084 A Summary of the Invention [Problem to be solved by the invention]
[0004] When taphole bricks are repaired using mortar as a repair material as in Patent Document 1, there is a problem in that the repair material peels off due to the effects of friction and heat caused by molten steel when tapping. An object of the present invention is to provide a repair structure and a repair method for electric furnace taphole bricks, in which a repair material for the taphole bricks is less likely to peel off. [Means for solving the problem]
[0005] According to the present invention, there are provided the following repair structure and repair method for an electric furnace taphole brick. 1. A repair structure for a taphole brick arranged on the inner periphery of a taphole at the bottom of an electric furnace, an iron pipe arranged to face an inner peripheral wall of the taphole brick; A castable construction body is provided between the outer peripheral surface of the iron pipe and the inner peripheral wall of the taphole brick, The castable construction contains coarse grains and has a thickness of 30 mm or more, and is a repair structure for electric furnace taphole bricks. 2. 2. The repair structure for electric furnace taphole bricks according to claim 1, wherein the castable body contains coarse particles of alumina and fine particles of magnesia, and the maximum particle size of the coarse particles of alumina is 5 mm or more. 3. A method for repairing a taphole brick disposed on an inner periphery of a taphole at the bottom of an electric furnace, comprising the steps of: A first step of installing a receiving tool at a lower end of the tap hole; a second step of inserting an iron pipe into the inner peripheral side of the taphole brick from the upper end side of the taphole brick, and placing the iron pipe on the jig with a gap of 30 mm or more between the inner peripheral wall of the taphole brick and the outer peripheral surface of the iron pipe; A third step of pouring a castable material containing coarse particles into a gap between an inner peripheral wall of the taphole brick and an outer peripheral surface of the iron pipe; A fourth step of removing the jig after the castable material has hardened. How to repair electric furnace taphole bricks. 4. The receiving tool has a positioning portion, The second step of the method for repairing an electric furnace taphole brick described in item 3 above comprises inserting the positioning part into the inside of the iron pipe and placing the iron pipe on the jig, thereby forming the gap between the inner wall of the taphole brick and the outer circumferential surface of the iron pipe. 5. 5. The method for repairing an electric furnace taphole brick according to claim 3 or 4, further comprising, prior to the first step, a step of cutting the inner wall of the taphole brick so as to leave a gap of 30 mm or more between the inner wall of the taphole brick and the outer circumferential surface of the iron pipe. 6. A fifth step of cutting obliquely from the lower part of the castable body, which is a castable material body, toward the inner periphery of the taphole so that the inclination angle θ is between 30° and 60° after the molten steel is tapped from the taphole; A sixth step of installing a jig at the lower end of the tap hole; A seventh step of inserting an iron pipe into the inner peripheral side of the castable refractory body from the upper end side of the castable refractory body, and placing the iron pipe on the jig with a gap of 30 mm or more between the inner peripheral wall of the castable refractory body and the outer peripheral surface of the iron pipe; An eighth step of pouring a castable material containing coarse particles into a gap between the inner peripheral wall of the castable construction body and the outer peripheral surface of the iron pipe; and a ninth step of removing the jig after the castable material has hardened. 6. The method for repairing an electric furnace taphole brick according to any one of 3 to 5. Effect of the Invention
[0006] According to the present invention, a castable construction body with repaired taphole bricks is less likely to peel off. [Brief description of the drawings]
[0007] [Figure 1] Schematic cross-sectional view showing the bottom of an electric furnace. [Diagram 2] FIG. 2 is a conceptual cross-sectional view of a repair structure for an electric furnace taphole brick according to one embodiment of the present invention. [Diagram 3] Schematic cross-section showing an electric furnace taphole brick before repair. [Figure 4] FIG. 4 is a conceptual cross-sectional view showing a first step and a second step of a repair method for an electric furnace taphole brick according to another embodiment of the present invention. [Diagram 5] FIG. [Figure 6] FIG. 13 is a conceptual cross-sectional view showing the third step of the method for repairing electric furnace taphole bricks. [Figure 7]FIG. 13 is a conceptual cross-sectional view showing the fifth step of the method for repairing an electric furnace taphole brick. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] FIG. 1 shows a conceptual cross-section of the bottom of an electric furnace. A bottom electrode 12 is installed in the center of the bottom 11 of the electric furnace 1. A taphole 13 is provided at one end of the bottom 11 as a tap hole. A taphole brick 14 is arranged in a cylindrical shape around the inner periphery of the taphole 13. A taphole opening and closing cover 15 is installed at the lower end of the taphole 13. The taphole opening and closing cover 15 is movable in the horizontal and vertical directions. FIG. 1 shows the state in which the taphole opening and closing cover 15 closes the lower end of the taphole 13. In FIG. 1, reference numeral 16 denotes a hearth refractory material, and reference numeral 17 denotes an iron shell. When transferring molten steel from the electric furnace 1 to the ladle, the electric furnace 1 is tilted toward one end where the taphole 13 is located. The taphole opening and closing cover 15 is moved vertically downward and then moved horizontally. The molten steel in the electric furnace 1 is then tapped out of the taphole 13. At this time, the taphole brick 14 melts due to contact with the molten steel. As the taphole brick 14 melts, the taphole 13 expands. This makes it necessary to repair the taphole 13.
[0009] FIG. 2 conceptually shows a cross section of a repair structure for an electric furnace taphole brick (hereinafter simply referred to as a "repair structure") according to one embodiment of the present invention. The repair structure 2 comprises an iron pipe 21 arranged to face the inner peripheral wall of the taphole brick 14, and a castable construction body 22 arranged between the outer peripheral surface of the iron pipe 21 and the inner peripheral wall of the taphole brick 14. The castable construction body 22 is obtained by pouring a castable material, and the castable material and the castable construction body 22 contain coarse particles. In this respect, it differs from the mortar used in Comparative Examples 4 and 5 described below. Here, the mortar does not contain coarse particles, and is made by kneading fine powder in which 60 to 80% of the particles constituting the aggregate are 75 μm or less by mass and the maximum particle size is adjusted to a range of 0.3 to 0.5 mm, a binder, and a solvent such as water. In the present specification, "coarse particles" refers to particles having a particle size of 3 mm or more. The upper limit of the particle size of coarse particles is not particularly limited and is based on common technical knowledge, but is generally 8 mm or less.
[0010] Since the castable material contains coarse grains, it is easy to fill the material with air when poured. In addition, gas is easily released from the castable material during drying, so the structure of the castable material 22 tends to become dense. Therefore, peeling is unlikely to occur. In contrast, mortar does not contain coarse particles, so air is easily trapped in it when it is poured in. Moreover, gas does not easily escape from the mortar during drying, so the structure of the mortar is not easily dense.
[0011] The castable material and the castable construction body 22 are preferably made of alumina-magnesia. Specifically, the castable material and the castable construction body 22 preferably contain coarse alumina particles and fine magnesia particles, and the maximum particle diameter of the coarse alumina particles is 5 mm or more. In this way, by containing coarse alumina particles and fine magnesia particles as main components, spinel is generated during drying or tapping, and the castable construction body 22 expands. Therefore, during drying or tapping, the castable construction body 22 is less likely to crack due to shrinkage, and peeling is less likely to occur. For example, the porosity of the alumina-magnesia castable construction body 22 after drying at 1000°C is 18 to 20%, and the structure is more dense, so peeling is less likely to occur. Here, in this specification, "fine particles" refers to particles with a particle diameter of less than 1 mm. In contrast, as mentioned above, the structure of a mortar-based body is difficult to make dense. Moreover, the mortar-based body shrinks when drying or tapping steel. Therefore, the mortar-based body is prone to cracks due to shrinkage during drying or tapping steel, and peeling occurs easily. In addition, the porosity of the mortar-based body after drying at 1000°C is 25-30%, and the structure is coarse, so peeling occurs easily.
[0012] The castable material and castable construction body 22 are not limited to alumina-magnesia, and may be, for example, alumina-silica or magnesia. In addition, in addition to the refractory raw material powder, any of the materials may appropriately contain a binder such as alumina cement, and may also contain fibrous materials such as organic fibers and metal fibers.
[0013] The castable construction body 22 has a thickness of 30 mm or more. The thickness of the castable construction body 22 corresponds to the gap between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21, which corresponds to the construction width when the castable material is poured in and construction. In other words, when at least a part of the castable construction body 22 has a thickness of 50 mm or more, it means that there is a construction width of 30 mm or more between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21. By pouring the castable material while ensuring a construction width of 30 mm or more in this way, the castable material is easily filled between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21. From this point of view, the castable construction body 22 is likely to have a dense structure. Therefore, peeling is unlikely to occur.
[0014] The average construction width of the castable material, i.e., the average thickness of the castable construction body 22, is preferably 30 mm or more. This is because, if the average thickness of the castable construction body 22 is less than 30 mm, the strength of the castable construction body 22 is insufficient and peeling is likely to occur. Here, in this specification, the average thickness of the castable construction body 22 refers to a value calculated from the total volume V of the gap between the inner wall of the taphole brick 14 and the outer circumferential surface of the iron pipe 21. Specifically, in a virtual cylinder having the outer diameter r of the iron pipe 21 and the construction height h, the outer diameter R is obtained when the volume of the cylinder is the total volume V of the gap. Then, (Rr) / 2 is defined as the average thickness of the castable construction body 22. Since the castable body 22 contains coarse particles, it is normal for unevenness to occur near the surface, and it is permissible for some of the unevenness to be less than 30 mm in some places. Generally, the outer diameter of the iron pipe 21 is set to the initial diameter of the tap hole 13. The initial diameter of the tap hole 13 is, for example, about 180 mm.
[0015] Next, a method for repairing an electric furnace taphole brick (hereinafter simply referred to as the "repair method") according to another embodiment of the present invention will be described. FIG. 3 conceptually shows a cross section of an electric furnace taphole brick before repair. In FIG. 3, the position of the initial diameter of the taphole 13 is virtually indicated by a dashed line. As shown in the figure, the taphole brick 14 arranged on the inner circumference of the taphole 13 is melted down by contact with molten steel. The melting is particularly large near the tap hole at the lower end of the taphole brick 14. As the taphole brick 14 melts down, the taphole 13 expands. In this embodiment, repair is performed when the taphole 13 becomes larger than the initial diameter by about 100 mm. Each step of the repair method of this embodiment will be described below.
[0016] <1st process> A receiving tool is installed at the lower end of the tap hole 13. Specifically, as conceptually shown in Fig. 4, the receiving tool 3 is sandwiched and supported between the tap hole opening / closing cover 15 and the lower end of the tap hole 13.
[0017] <Second process> The iron pipe 21 is inserted into the inner periphery of the taphole brick 14 from the upper end side of the taphole brick 14. At this time, as conceptually shown in Figure 4, the iron pipe 21 is placed on the receiving fixture 3 so that a gap of 30 mm or more is provided between the inner periphery wall of the taphole brick 14 and the outer periphery of the iron pipe 21. 5, the receiving tool 3 in this embodiment has a base portion 31, a positioning portion 32, and a side wall portion 33. The positioning portion 32 is provided in a circular convex shape in the center of the base portion 31. The outer diameter of the lower end of the circular convex positioning portion 32 is approximately the same as the inner diameter of the iron pipe 21. In the second step of this embodiment, the positioning portion 32 is inserted inside the iron pipe 21, and the iron pipe 21 is placed on the receiving fixture 3. This allows the iron pipe 21 to be positioned in the center of the tapping hole 13, and also allows a gap of 30 mm or more to be formed between the inner circumferential wall of the tapping hole brick 14 and the outer circumferential surface of the iron pipe 21. At this time, the inner circumferential surface of the side wall portion 33 is brought into contact with the outer circumferential surface of the iron shell 17 of the tapping hole 13, thereby allowing the receiving fixture 3 to be positioned relative to the tapping hole 13. The side wall portion 33 has three notches 331 provided at equal intervals in the circumferential direction. These notches 331 are provided to check whether there is a gap between the receiving fixture 3 and the iron shell 17. In this embodiment, if simply inserting the iron pipe 21 into the inner side of the taphole brick 14 does not provide a gap of 30 mm or more between the inner wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21, then prior to the first step, the inner wall of the taphole brick 14 is cut so as to provide a gap of 30 mm or more between the inner wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21.
[0018] <3rd process> A castable material containing coarse particles is poured into the gap between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21. In this embodiment, since there is a gap of 30 mm or more between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21, the castable material can be easily filled between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21. In addition, since the castable material contains coarse particles, it is less likely to contain air during pouring, making it easier to fill. Furthermore, in this embodiment, since there is a gap of 30 mm or more between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21, for example, as shown in Fig. 6, the tip of the vibrator 4 can be inserted into the gap between the inner peripheral wall of the taphole brick 14 and the outer peripheral surface of the iron pipe 21. By inserting the tip of the vibrator 4 in this way and pouring the castable material C while applying vibration, the castable material C can be filled more easily. During pouring, the upper end of the iron pipe 21 can be covered with a cap 5 as shown in FIG.
[0019] <4th process> After the castable material C has hardened, the receiving jig 3 and the cap 5 are removed. This provides the repair structure 2 as shown in Fig. 2. That is, the first repair is completed up to the fourth step.
[0020] <5th process> After the first repair is completed, molten steel is tapped from the taphole 13. When molten steel is tapped from the taphole 13 after repair, the iron pipe 21 in the repair structure 2 melts and disappears, and the castable construction body 22 then comes into contact with the molten steel. The castable construction body 22 then melts and is damaged by contact with the molten steel. Therefore, in this embodiment, a second repair is performed. In the second repair, the lower part of the castable body 22 is cut as the fifth step, as shown in Fig. 7. Specifically, the castable body 22, located about 10 mm away from the originally placed taphole brick 14, is cut obliquely from the lower end toward the inner periphery of the taphole 13. The appropriate inclination angle θ when cutting obliquely is about 30 to 60°.
[0021] <6th process> In the sixth step, the receiving jig 3 is placed at the lower end of the tap hole 13 in the same manner as in the first step described above.
[0022] <7th process> In the seventh step, similarly to the above-mentioned second step, the iron pipe 21 is inserted into the inner peripheral side of the castable body 22 from the upper end side of the castable body 22, and the iron pipe 21 is placed on the receiving jig 5 with a gap of 30 mm or more between the inner peripheral wall of the castable body 22 and the outer peripheral surface of the iron pipe 21. When this seventh step is performed, the castable body 22 from the first repair remains on at least a part of the inner peripheral side of the taphole brick 14, so the iron pipe 21 is inserted into the inner peripheral side of the castable body 22.
[0023] <8th process> In the eighth step, similarly to the above-mentioned third step, a castable material containing second coarse particles is poured into the gap between the inner peripheral wall of the castable construction body 22 and the outer peripheral surface of the iron pipe 21. The second castable material used in this eighth step can be made of the same material as the castable material used in the above-mentioned third step.
[0024] <9th process> In the ninth step, similarly to the fourth step described above, the receiving jig 3 and the cap 5 are removed after the second castable material has hardened. This completes the second repair. The third and subsequent repairs can be performed by repeating the fifth to ninth steps described above. By repeating the fifth to ninth steps in this manner, the electric furnace can be used continuously without replacing the taphole brick 14.
[0025] In this embodiment, in the second and subsequent repairs, the lower part of the castable body 22 is cut as the fifth step. If the lower part of the castable body 22 is not cut as the second and subsequent repairs, the phenomenon of peeling off of the lower end part of the castable body newly constructed in the eighth step is likely to occur. In other words, by cutting the lower part of the castable body 22 as the fifth step, peeling off of the lower end part of the castable body newly constructed in the eighth step can be suppressed. This is because by cutting the lower part of the castable body 22 as the fifth step, the thickness of the lower end part of the castable body newly constructed in the eighth step can be increased. EXAMPLES
[0026] Table 1 shows examples of the present invention and comparative examples. In each of the examples and comparative examples, a gap equivalent to the "average thickness of the workpiece" in Table 1 was provided between the inner peripheral wall of the taphole brick and the outer peripheral surface of the iron pipe, and a material in which moisture equivalent to the "amount of moisture added" in Table 1 was added to the "refractory raw material" was poured in to perform the first repair. After the first repair, 50 to 60 taps were performed, and the middle and bottom ends of the taphole were visually observed after the 50 to 60 taps to evaluate the degree of peeling of the workpiece. Specifically, the absence of peeling was rated as ⊚ (good), the presence of small peeling was rated as ◯ (passable), and the presence of large peeling was rated × (unacceptable).
[0027] [Table 1]
[0028] In all of Examples 1 to 5, a castable material containing coarse particles was used, and the average thickness of the castable body was 30 mm or more. The degree of peeling of the castable body after 50 to 60 tappings was excellent, being rated as ◎ (good) or ◯ (fair). Of these, Examples 1 to 3 used a castable material containing coarse alumina particles and fine magnesia particles, with the maximum particle size of the coarse alumina particles being 5 mm or more, and the degree of peeling of the castable body after 50 to 60 tappings was especially excellent, being rated as ◎ (good).
[0029] In Comparative Examples 1 to 3, castable materials containing coarse particles were used, and the average thickness of the castable bodies was 10 to 20 mm. The degree of peeling of the bodies after 50 to 60 tappings was × (unacceptable). Mortar not containing coarse particles was used in Comparative Examples 4 and 5. The average thickness of the applied body was 50 to 60 mm, but the degree of peeling of the applied body after 50 to 60 tappings was × (unacceptable). [Explanation of symbols]
[0030] 1 Electric furnace 11 Hearth bottom 12 Hearth electrode 13 Taphole 14 Taphole brick 15 Taphole opening and closing cover 16 Hearth refractories 17 Ironhide 2 Repair structure 21 Iron Pipe 22 Castable construction body 3 Fixture 31 Circuit Board Section 32 Positioning part 33 Side wall 331 Notch 4. Vibrator 5 Cap C Castable material
Claims
1. A repair structure for a taphole brick arranged on the inner periphery of a taphole at the bottom of an electric furnace, an iron pipe arranged to face an inner peripheral wall of the taphole brick; A castable construction body is provided between the outer peripheral surface of the iron pipe and the inner peripheral wall of the taphole brick, The castable construction contains coarse grains and has a thickness of 30 mm or more.
2. 2. The repair structure for an electric furnace taphole brick according to claim 1, wherein the castable body contains coarse particles of alumina and fine particles of magnesia, and the maximum particle size of the coarse particles of alumina is 5 mm or more.
3. A method for repairing a taphole brick disposed on an inner periphery of a taphole at the bottom of an electric furnace, comprising the steps of: A first step of installing a receiving tool at a lower end of the tap hole; a second step of inserting an iron pipe into the inner peripheral side of the taphole brick from the upper end side of the taphole brick, and placing the iron pipe on the jig with a gap of 30 mm or more between the inner peripheral wall of the taphole brick and the outer peripheral surface of the iron pipe; a third step of pouring a castable material containing coarse particles into a gap between an inner peripheral wall of the taphole brick and an outer peripheral surface of the iron pipe; A fourth step of removing the jig after the castable material has hardened. How to repair electric furnace taphole bricks.
4. The receiving tool has a positioning portion, 4. The electric furnace taphole brick repair method according to claim 3, wherein in the second step, the positioning part is inserted inside the iron pipe and the iron pipe is placed on the jig, thereby forming the gap between an inner wall of the taphole brick and an outer circumferential surface of the iron pipe.
5. 5. The electric furnace taphole brick repair method according to claim 3, further comprising, prior to the first step, a step of cutting an inner peripheral wall of the taphole brick so as to provide a gap of 50 mm or more in at least a part between the inner peripheral wall of the taphole brick and the outer peripheral surface of the iron pipe.
6. A fifth step of cutting obliquely from a lower part of the castable body, which is a body of the castable material, toward an inner peripheral side of the taphole so that an inclination angle θ is between 30° and 60° after the molten steel is tapped from the taphole; A sixth step of installing a jig at a lower end of the tap hole; A seventh step of inserting an iron pipe into the inner peripheral side of the castable refractory body from the upper end side of the castable refractory body, and placing the iron pipe on the jig with a gap of 30 mm or more between the inner peripheral wall of the castable refractory body and the outer peripheral surface of the iron pipe; An eighth step of pouring a castable material containing coarse particles into a gap between the inner peripheral wall of the castable construction body and the outer peripheral surface of the iron pipe; and a ninth step of removing the jig after the castable material has hardened. The method for repairing an electric furnace taphole brick according to any one of claims 3 to 5.
Citation Information
Patent Citations
Method of repairing cylindrical lining refractory material
JP1987019684A
Method for prolonging lifetime of electric furnace tap hole
JP2001215084A
Low elastic modulus alumina-magnesia castable refractory, pre-cast block, and molten metal vessel
JP2004142957A
Method of extending service life of electric furnace tap hole
JP2011191043A
Baking repairing material
JP2011207702A