Method and apparatus for enhancing titanium and titanium silicide selectivity during chemical vapor deposition - Patents.com
The method of using titanium tetrachloride, hydrogen, and argon in a controlled plasma environment addresses the selectivity issue in titanium deposition, achieving high selectivity and uniformity on silicon surfaces, reducing contact resistance and enhancing feature fill.
Patent Information
- Application Number
- JP2023031713
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-12-05
- Filing Date
- 2023-03-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-12-19
AI Technical Summary
The challenge of poor selectivity in titanium deposition between silicon and dielectrics such as silicon nitride and silicon oxide leads to non-uniform substrate deposition and limited feature fill in high aspect ratio features, hindering the formation of ohmic contacts and increasing contact resistance.
A method involving the use of titanium tetrachloride, hydrogen, and argon in a controlled plasma environment within a processing chamber, with a lid heater and showerhead configuration, to selectively deposit titanium or titanium silicide on silicon surfaces while minimizing deposition on dielectric surfaces, enhanced by pretreatment with silane and post-treatment with hydrogen radicals to form robust titanium silicide.
Enhances selectivity of titanium deposition on silicon surfaces, improving substrate uniformity and reducing contact resistance, with selectivity ratios greater than 40:1 for titanium and 60:1 for titanium silicide, and minimizing titanium nitride memory effects to less than 3 angstroms.
Smart Images

Figure 0007575507000001 
Figure 0007575507000002 
Figure 0007575507000003
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure relate generally to substrate processing equipment and techniques, and more particularly to methods and apparatus for selectively depositing materials by chemical vapor deposition. [Background technology]
[0002] Selective deposition processes can advantageously reduce the number of steps and costs associated with traditional lithography while keeping up with the pace of shrinking device dimensions. Selective deposition of titanium and / or titanium silicide dielectric patterns has high potential value because titanium and titanium silicide (TiSix) are important materials widely used to form ohmic contacts and reduce contact resistance in transistor connections. The inventors have recognized that the poor selectivity of titanium material between silicon and dielectrics such as silicon nitride and silicon oxide poses a significant challenge in maximizing metallic feature fill. For example, poor selectivity can result in titanium material being deposited on the sidewalls and bottom of high aspect ratio features, limiting the ability to fill the features with the desired metallic material. Poor selectivity can promote substrate non-uniformity, which necessitates highly selective deposition of titanium material to silicon in order to reduce contact resistance and maximize the volume of feature fill material. Summary of the Invention [Problem to be solved by the invention]
[0003] In response, the present inventors have developed an improved method for selectively depositing titanium materials onto silicon or exposed silicon (hereinafter exposed silicon) over dielectrics such as silicon oxide and silicon nitride. [Means for solving the problem]
[0004] Provided herein are methods and apparatus for selective deposition. In some embodiments, a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface includes forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature between 200-800 degrees Celsius in a region between a lid heater and a showerhead of a processing chamber, and flowing the reaction products into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate.
[0005] In some embodiments, a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface includes forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) between a lid heater and a showerhead in a processing chamber to selectively deposit a titanium material layer on the substrate in the processing chamber, the dielectric surface inhibiting deposition of the titanium material layer on the dielectric surface, the remote plasma reaction reacting titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature between 200 and 800 degrees Celsius.
[0006] In some embodiments, a method for depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface may include optionally forming a first direct plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) between a showerhead and the substrate in a processing chamber for 0.1 to 200 seconds; forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) between a lid heater and the showerhead in the processing chamber to selectively deposit a titanium material layer on the silicon surface of the substrate; forming a titanium material layer on the plate, where a dielectric surface inhibits deposition of the titanium material layer on the dielectric surface, forming a remote plasma reaction at a first temperature of 200-800 degrees Celsius by reacting titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) to cause the titanium material to pass through a showerhead; and forming a direct plasma reaction between nitrogen (N2), hydrogen (H2) and argon (Ar) between the showerhead and the substrate in a processing chamber to form a capping titanium nitride layer for the titanium material layer on a silicon surface of the substrate.
[0007] In some embodiments, the present disclosure relates to a processing chamber comprising a lid heater, a showerhead, and a substrate support disposed within the processing chamber, the processing chamber configured to remotely ignite a plasma in a region between the lid heater and the showerhead and directly ignite a plasma between the showerhead and the substrate support.
[0008] In some embodiments, the present disclosure relates to a processing chamber including a lid heater, a showerhead, and a substrate support disposed within the processing chamber, the processing chamber configured to remotely ignite a plasma in the processing chamber between the lid heater and the showerhead and directly ignite a plasma between the showerhead and the substrate support.
[0009] In some embodiments, the present disclosure relates to a non-transitory computer readable medium having instructions stored thereon that, when executed, cause a method of selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface, the method including forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) in a region between a lid heater and a showerhead of a processing chamber at a first temperature between 200 and 800 degrees Celsius, and flowing reaction products into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate.
[0010] Other additional embodiments of the present disclosure are described below.
[0011] Embodiments of the present disclosure, briefly outlined above and discussed in more detail below, can be understood by reference to exemplary embodiments of the present disclosure illustrated in the accompanying drawings, which, however, depict only typical embodiments of the present disclosure and are therefore not to be considered as limiting the scope, as the present disclosure may embrace other embodiments that are equally effective. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram of an apparatus suitable for carrying out the methods of the present disclosure. [Diagram 2] 1 is a flow diagram of a method of selective deposition according to some embodiments of the present disclosure. [Figure 3A] 3A-3C are illustrative cross-sectional views of a substrate during different stages of the processing sequence of FIG. 2 according to some embodiments of the present disclosure. [Figure 3B] 3A-3C are illustrative cross-sectional views of a substrate during different stages of the processing sequence of FIG. 2 according to some embodiments of the present disclosure. [Figure 4] 1 is a flow diagram of a method of selective deposition according to some embodiments of the present disclosure. [Figure 5A]5A-5C are illustrative cross-sectional views of a substrate during different stages of the processing sequence of FIG. 4 according to some embodiments of the present disclosure. [Figure 5B] 5A-5C are illustrative cross-sectional views of a substrate during different stages of the processing sequence of FIG. 4 according to some embodiments of the present disclosure. [Figure 5C] 5A-5C are illustrative cross-sectional views of a substrate during different stages of the processing sequence of FIG. 4 according to some embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] For ease of understanding, the same reference numerals have been used, where possible, to designate identical elements common to the figures. The figures are not drawn to scale and may be simplified for clarity. Elements and features of one embodiment may be beneficially incorporated in other embodiments without specific mention.
[0014] Provided herein are methods and apparatus for selective deposition. In some embodiments, a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface includes forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature between 200-800 degrees Celsius in a region between a lid heater and a showerhead of a processing chamber, and flowing the reaction products into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate. In some embodiments, the methods described herein advantageously enhance and promote selectivity of titanium material over silicon and reduce selectivity over dielectrics such as silicon nitride and silicon oxide. The methods facilitate and promote maximizing metal feature fill. For example, it increases selectivity over the bottom of silicon-containing features and reduces titanium material deposition on the sidewalls of high aspect ratio features that include dielectrics to increase the volume within the feature that is filled with the desired metal material. The high selectivity over silicon promotes uniformity of the substrate, thereby advantageously reducing contact resistance and advantageously maximizing the volume of feature fill material. In some embodiments, the showerhead traps reaction products, such as titanium material ions, within the showerhead to facilitate selective deposition. In some embodiments, a pretreatment including heating the substrate in the presence of silane further enhances the selectivity to silicon over silicon nitride. In some embodiments, such as those in which the titanium material is titanium, the pretreatment enhances the selectivity to silicon to greater than 40:1. In some embodiments, such as those in which the titanium material is titanium silicide, the pretreatment enhances the selectivity to silicon to greater than 60:1. In some embodiments, a post-deposition treatment including contacting the showerhead and substrate with silane and / or remote plasma hydrogen, such as hydrogen radicals, can reduce the memory effect of titanium nitride depositing films on both silicon and silicon nitride (SiN) above the substrate to less than 3 angstroms, further enhancing the selectivity to silicon over silicon nitride.
[0015] 1 is a schematic diagram of an apparatus, such as a wafer processing system 10, suitable for carrying out the methods of the present disclosure. In an embodiment, the wafer processing system 10 includes a processing chamber 100, a gas panel 130, a control unit 110, and other hardware components, such as power supplies and vacuum pumps. An exemplary processing chamber can include any of several processing chambers available from Applied Materials, Inc. of Santa Clara, Calif., configured for remote chemical vapor deposition (CVD) and direct CVD reactions as described herein. Other suitable processing chambers from other manufacturers can be similarly used and modified in accordance with the present disclosure.
[0016] In an embodiment, the processing chamber 100 generally includes a lid heater 131, which is used to heat the processing volume 101, including a region within the processing chamber 100, such as a plenum space between the lid heater 131 and the showerhead 165. Prior to and during processing according to the present disclosure, the region of the processing volume 101 between the lid heater 131 and the showerhead 165 can be heated to a desired temperature depending on the particular process. In an embodiment, the lid heater 131 is heated by an embedded heating element, such as heating element 171. For example, the lid heater 131 can be resistively heated by passing an electric current through the heating element 171 from an AC power source (not shown). The lid heater 131 then heats the area of the process volume 101 between the lid heater 131 and the showerhead 165, which can be maintained within a process temperature range, for example, 200-800 degrees Celsius, or can be maintained at a first temperature of about 550 degrees Celsius. In some embodiments, the area of the process chamber between the lid heater and the showerhead is maintained at a first temperature of 200-800 degrees Celsius. In some embodiments, the area between the lid heater and the showerhead can be heated to a temperature of 200-800 degrees Celsius, or in some embodiments, about 550 degrees Celsius, by providing a lid heater at a temperature of 200-800 degrees Celsius, or in some embodiments, about 550 degrees Celsius, a showerhead (heated by radiant heat from the lid heater) at about 500 degrees Celsius, a wafer temperature of about 425 degrees Celsius, and a pedestal heated to about 450 degrees Celsius. In an embodiment, the area between the lid heater and the showerhead is described as the plenum space.
[0017] In an embodiment, a temperature sensor (not shown), such as a thermocouple, may be embedded in the lid heater 131 to monitor the temperature of the lid heater 131 in a conventional manner. For example, the measured temperature may be used in a feedback loop to control the power supply to the lid heater 131 in such a manner that the temperature of the region of the process volume 101 between the lid heater 131 and the showerhead 165 may be maintained or controlled at a desired temperature appropriate for a particular process application. In an embodiment, the lid heater 131 is configured to provide sufficient heat to promote remote plasma formation between the lid heater 131 and the showerhead 165 or within the showerhead 165 in the process volume 101 and prevent condensation in or on the showerhead 165. For example, the control unit 110 may communicate with the lid heater 131 to enable a user to adjust the heat of the lid heater 131 and maintain sufficient heat to form a remote plasma. In an embodiment, depending on the process needs, the lid heater 131 is configured not to heat up or promote remote plasma formation in the region between the lid heater 131 and the showerhead 165 in the process volume 101. For example, depending on the user needs, the lid heater 131 can be switched off via the control unit 110.
[0018] In an embodiment, the lid heater 131 may be configured to provide sufficient RF to form a plasma in the vicinity of the lid heater 131 by embedding a radio frequency electrode 181 therein. In an embodiment, the lid heater 131 may be configured to provide sufficient RF to promote remote plasma formation in the area between the lid heater 131 and the showerhead 165 and / or within the showerhead 165 in the process volume 101. For example, the control unit 110 may communicate with the lid heater 131 to allow a user to adjust the RF emitted from the lid heater 131 and to maintain a sufficient RF signal to form a plasma. In an embodiment, depending on the process needs, the lid heater 131 may be configured not to emit an RF signal or to not promote plasma formation between the lid heater 131 and the showerhead 165 in the process volume 101. For example, depending on the user needs to eliminate RF emanating from the lid heater 131, the lid heater 131 may be switched off via the control unit 110.
[0019] In an embodiment, the processing chamber 100 generally includes a support pedestal 150 that is used to support a substrate, such as a semiconductor substrate 190, within the processing chamber 100. The support pedestal 150 can be moved vertically within the processing chamber 100 using a displacement mechanism (not shown). Prior to processing, the semiconductor substrate 190 can be heated to a desired temperature depending on the particular process. In an embodiment, the support pedestal 150 is heated by an embedded heating element, such as heating element 170. For example, the support pedestal 150 can be resistively heated by passing an electric current through the heating element 170 from an AC power source 106. The support pedestal 150 then heats the semiconductor substrate 190, and the semiconductor substrate 190 can be maintained within a processing temperature range, such as 200-800 degrees Celsius or 300-700 degrees Celsius. In an embodiment, a temperature sensor 172, such as a thermocouple, may be embedded in the support pedestal 150 to monitor the temperature of the support pedestal 150 in a conventional manner. For example, the measured temperature may be used in a feedback loop to control a power source, such as the AC power source 106, for the heating element 170 in such a manner that the temperature of the semiconductor substrate 190 may be maintained or controlled at a desired temperature appropriate for a particular processing application. In an embodiment, the support pedestal includes a ground at 182.
[0020] In an embodiment, a controller unit 110, such as mass flow controllers (not shown) and a computer, provides proper control and regulation of gas flow through the processing chamber 100 and the gas panel 130. The showerhead 165 allows process gases from the gas panel 130 to be evenly distributed and introduced into the processing chamber 100. In an embodiment, the showerhead 165 is configured to flow reaction products (such as reaction products suitable for forming a titanium material layer, such as titanium or titanium silicide, as described herein) into the processing chamber to selectively form a titanium material layer on a silicon surface of a substrate.
[0021] By way of example, control unit 110 includes a central processing unit (CPU) 112, support circuits 114, and memory, which includes associated control software 116. Control unit 110 is responsible for the automated control of the numerous steps required for processing semiconductor substrates 190, such as wafer transport, gas flow control, temperature control, chamber evacuation, etc. Bidirectional communication between control unit 110 and the various components of wafer processing system 10 is handled through a number of signal cables collectively referred to as signal bus 118, some of which are shown in FIG.
[0022] In some embodiments, the present disclosure relates to a non-transitory computer readable medium, such as a memory, having instructions stored thereon that, when executed, cause a method of selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface, the method including forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) in a region between a lid heater and a showerhead of a processing chamber at a first temperature between 200 and 800 degrees Celsius, and flowing reaction products into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate.
[0023] In some embodiments, the showerhead 165 can be configured to provide a sufficient amount of RF energy to form a plasma in the vicinity of the showerhead 165 by embedding a radio frequency electrode 181 in the showerhead 165. In embodiments, the showerhead 165 can be configured to provide sufficient RF to promote plasma formation in the process volume 101. For example, the control unit 110 can communicate with the showerhead 165 to allow a user to adjust the RF emitted from the showerhead 165 and maintain a sufficient RF signal to form a plasma. In embodiments, the showerhead 165 can be grounded by a ground 183 depending on the user needs to place a plasma in the process volume 101. In embodiments where the showerhead 165 is grounded, a remote plasma can be formed in the process volume 101 in a region between the lid heater 131 and the showerhead 165. In embodiments where the showerhead is not grounded, a plasma is formed directly in the process volume 101 in a region between the showerhead 165 and the semiconductor substrate 190. The switch 184 can be in communication with the ground 183, the RF electrode 180, and the showerhead, and can be configured to control remote and direct plasma formation according to user needs in accordance with the present disclosure. In an embodiment, the switch 184 and the showerhead 165 are in communication with each other, and the switch 184 and the showerhead 165 are configured to control remote and direct plasma formation according to user needs in accordance with the present disclosure. In some embodiments, when the switch is placed in a first position, a power source, such as an RF power source or a VHF power source, is electrically coupled to the chamber lid via the switch 184. When the switch is placed in a second position (not shown), the power source is electrically coupled to the showerhead 165. When the switch 184 is in the first position, the power source is used to ignite and maintain a first plasma remote from the substrate, such as a remote plasma located directly in a plenum space or region between the lid heater and the showerhead. In some embodiments, the remote plasma consists of process gas flowed into the plenum and maintained as a plasma by capacitive coupling of power from the power source.In some embodiments, when the switch 184 is in the second position, the power supply is used to ignite and maintain a second plasma (not shown) between the showerhead 165 in the process volume 101 and a substrate 190 disposed on a substrate support.
[0024] In an embodiment, the processing chamber 100 includes a vacuum pump 102 for evacuating the processing chamber 100 and for maintaining proper gas flow and pressure within the processing chamber 100. A showerhead 165 is located above the support pedestal 150 through which processing gases are introduced into the processing chamber 100. In an embodiment, the showerhead 165 can be configured as a multi-gas showerhead with two or more separate paths that allow two or more gases to be introduced separately into the processing chamber 100 without premixing. In some embodiments, the showerhead 165 is connected to a gas panel 130 that controls and supplies various gases used in different steps of the processing sequence by mass flow controllers (not shown). Additionally, a purge gas source 104 supplies a purge gas, e.g., an inert gas, around the bottom of the support pedestal 150 during wafer processing to minimize undesirable deposits formed on the support pedestal 150.
[0025] In an embodiment, the control unit 110 is responsible for controlling the gas flow from the gas panel 130 to the process volume 101, such as the region between the lid heater 131 and the showerhead 165, via a first gas flow line 162, or from the gas panel 130 into the showerhead 165 via a second gas flow line 163. In some embodiments, the process chamber 100 is configured such that the gas panel 130 provides titanium tetrachloride (TiCl4), hydrogen (H2) and / or argon (Ar) or a noble gas into the process chamber 100 and the process volume 101. For example, in an embodiment, the process volume 101 is configured to receive about 1-100 sccm or about 25 sccm of titanium tetrachloride (TiCl4). In an embodiment, the process volume 101 is configured to receive about 50-10000 sccm or about 500 sccm of hydrogen (H2). In an embodiment, the process volume 101 is configured to receive about 3.5 liters of argon. In some embodiments, one or more desired gases may be directed from the gas panel 130 to the process volume 101 via the second gas flow line 163. For example, in embodiments, the second gas flow line 163 may add to the process volume 101 a silane such as SiH4, a disilane such as Si2H6, a silane compound, or a noble gas such as hydrogen (H2) or argon (Ar) gas. In some embodiments, such as those in which the process chamber 100 is configured for remote plasma applications, e.g., where a plasma is ignited in the region between the lid heater 131 and the showerhead 165 or within the showerhead 165, one or more desired gases, such as titanium tetrachloride (TiCl4), hydrogen (H2) and / or argon (Ar), can be directed from the gas panel 130 to the process volume 101 via a first gas flow line 162, and one or more desired gases, such as a silane, such as SiH4, or hydrogen (H2), or argon (Ar) gas, can be directed to the process volume 101 by a second gas flow line 163. In some embodiments, the inclusion of silane during deposition of titanium material results in the formation of titanium silicide or TiSix. In some embodiments, TiSix refers to titanium silicide, where x is a number between 0.4 and 2.2.In some embodiments, TiSix refers to one or more of Ti5Si3, TiSi2, TiSi, or combinations thereof.
[0026] In embodiments, the flow rates, temperatures, and pressures of the throughput can be adjusted to values sufficient for the desired reactions according to the present disclosure. In some embodiments, such as those in which the processing chamber 100 is configured for direct plasma applications, e.g., direct plasma applications in which a plasma is ignited in a region between the showerhead 165 and the semiconductor substrate 190, one or more desired gases, such as nitrogen (N2), hydrogen (H2), and argon (Ar), can be directed from the gas panel 130 to the throughput 101 via a first gas flow line 162, and one or more desired gases, such as argon (Ar), can be directed to the throughput 101 by a second gas flow line 163. In embodiments, the flow rates, temperatures, and pressures of the throughput can be adjusted to values sufficient for the desired reactions according to the present disclosure.
[0027] In an embodiment, the process chamber 100 includes an RF electrode 180 sufficient to ignite a plasma in the process volume 101 according to the present disclosure. In an embodiment, the RF electrode 180 can be coupled to one or more power sources (one power source not shown) through one or more corresponding respective matching networks (matching networks shown). The one or more power sources can be capable of producing up to 3000 watts of RF energy at a frequency between about 350 kHz and about 60 MHz, such as about 350 kHz or about 13.56 MHz or about 60 Mhz. In an embodiment, about 65 watts to 150 watts of RF energy is provided to the remote plasma reaction in the process volume 101. In some embodiments, the RF energy is about 120 watts to 140 watts, or about 130 watts. In some embodiments, pulsed RF energy or continuous wave mode RF is provided. In some embodiments, the RF power is about 130 watts, the pulse frequency is about 1 kHz, and the duty cycle is about 50%. In some embodiments, the process chamber 100 can utilize capacitively coupled RF energy for the plasma process. For example, the processing chamber 100 can have a ceiling made of a dielectric material and a showerhead 165 that is at least partially conductive to provide an RF electrode (or can be provided with a separate RF electrode). The showerhead 165 (or other RF electrode) can be coupled to one or more RF power sources (one RF power source not shown) through one or more corresponding respective matching networks (matching networks not shown). The one or more plasma sources can be capable of producing RF energy of up to about 3,000 watts, or in some embodiments up to about 5,000 watts.
[0028] Figure 2 is a flow diagram of a method 200 of selective deposition according to some embodiments of the present disclosure. Figures 3A-3B are exemplary cross-sectional views of a substrate, such as semiconductor substrate 190, during different stages of a processing sequence of Figure 2 according to some embodiments of the present disclosure. The method of the present disclosure can be performed in a processing chamber configured for thermal deposition techniques, such as chemical vapor deposition (CVD), or in a processing chamber discussed above with respect to Figure 1.
[0029] In an embodiment, the method 200 is performed on a semiconductor substrate 190, shown in FIG. 3A, having one or more dielectric surfaces, such as a silicon surface 302 and a dielectric surface 304, extending across the bottom of the feature 351. In an embodiment, the semiconductor substrate 190 is made of crystalline silicon (e.g., Si <100> or Si <111> ), silicon germanium, doped or undoped polycrystalline silicon, doped or undoped silicon wafers, patterned or unpatterned wafers, silicon on insulator (SOI), and combinations thereof. In an embodiment, the silicon material 301 can be crystalline silicon (e.g., Si <100> or Si <111> The semiconductor substrate 190 may include or consist of materials such as silicon, pure silicon, substantially pure silicon (with less than 1% or less than 0.5% impurities), or bare silicon. The exposed silicon may be, for example, pre-processed silicon from which the native oxide layer has been removed. In embodiments, the semiconductor substrate 190 may have a variety of dimensions, such as, for example, 200 mm, 300 mm, 450 mm, or other diameters for a circular substrate. The semiconductor substrate 190 may also be any polygonal, square, rectangular, curved, or other non-circular workpiece, such as a polygonal glass substrate used in the manufacture of flat panel displays. Unless otherwise specified, the embodiments and examples described herein are performed on a substrate such as the semiconductor substrate 190, for example, a substrate having a diameter of 200 mm, 300 mm, or 450 mm.
[0030] In some embodiments, the silicon material 301 is deposited by any suitable atomic layer deposition process or chemical layer deposition process. In some embodiments, the silicon material 301 can include any suitable silicon material for semiconductor device manufacturing. With reference to FIG. 3A, there may be a silicon oxide layer (not shown) on the silicon surface 302. This silicon oxide layer may be a native oxide layer or may be formed when the silicon surface 302 comes into contact with oxygen, for example, oxygen in air or water. The silicon oxide layer may be problematic in some embodiments because it may have a lower selectivity to titanium material than the exposed silicon surface. In some embodiments, the method 200 may include pretreating the silicon surface 302 to form an exposed silicon surface. In some embodiments, the method includes contacting the silicon surface 302 with one or more etchants to form the exposed silicon surface 302. In some embodiments, the silicon oxide layer is removed to form the exposed silicon surface before depositing the titanium material on or directly on the silicon surface 302. Non-limiting examples of exposed silicon surface materials include substantially pure silicon, such as silicon that is substantially free of oxides.
[0031] In embodiments, the dielectric layer 305 including the dielectric surface 304 is not the same as the silicon material 301 including the silicon surface 302. In some embodiments, the dielectric layer 305 is deposited by any suitable atomic layer deposition process or chemical layer deposition process. In some embodiments, the dielectric layer 305 can include a low-k dielectric layer deposited on the silicon material 301. In some embodiments, the dielectric layer 305 can include any low-k dielectric material suitable for semiconductor device fabrication, and combinations of materials. Non-limiting materials suitable as low-k dielectric materials can include silicon-containing materials, such as, for example, silicon oxide (SiO2), silicon nitride or silicon oxynitride (SiON), or combinations of these materials, or combinations of layers of these materials. In embodiments, the low-k dielectric material can have a low-k value of less than about 3.9 (e.g., about 2.5 to about 3.5). In some embodiments, the dielectric layer 305 can be formed of HfO x In an embodiment, the dielectric layer 305 and the dielectric surface 304 include or consist of silicon oxide (SiO2), silicon nitride, silicon oxynitride (SiON), or a combination thereof.
[0032] In some embodiments, the substrate is optionally pretreated as shown in the process sequence 201 of the method 200. In some embodiments, the dielectric layer 305 is pretreated by contacting the dielectric layer 305 with silane, either alone or in combination with a noble gas, such as argon. In some embodiments, the dielectric layer 305 includes a nitrogenous material, such as silicon nitride, and the substrate can be preheated prior to depositing the titanium material layer. In some embodiments, during a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface, such as silicon nitride, the substrate is preheated to a temperature of 200-800 degrees Celsius by contacting the substrate and the dielectric surface with a heated gas, such as heated argon or hydrogen, prior to forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature of 200-800 degrees Celsius in a region between a lid heater and a showerhead of the process chamber. Referring to FIG. 1, in some embodiments, argon and hydrogen can be flowed and heated through the first gas flow line 162 to preheat the substrate. In some embodiments, silane and argon can be flowed through the second gas flow line 163 while the substrate is preheated. In some embodiments, about 500 sccm to 3000 sccm of silane is flowed through the second gas flow line 163 to react with and / or cover the dielectric surface 304. In some embodiments, the dielectric surface is silicon nitride (SiN) and a sufficient amount of silane is contacted with the dielectric surface to saturate the exposed surface of the dielectric surface 304. In some embodiments, the silane bonds to silicon in the silicon nitride layer of the dielectric surface 304, which further enhances the selectivity of the titanium material over silicon. In some embodiments, a pretreatment including heating the substrate in the presence of silane further enhances the selectivity for silicon over silicon nitride. In some embodiments, such as those in which the titanium material is titanium, the pretreatment enhances the selectivity to silicon to greater than 40:1, such as up to 45:1.In some embodiments, such as those in which the titanium material is titanium silicide, the pretreatment enhances the selectivity to silicon to greater than 60:1, for example, up to 68:1.
[0033] In some embodiments, method 200 may begin at 201 where a substrate is pretreated. For example, the substrate is pretreated by preheating the substrate to a temperature greater than 200 degrees Celsius or between 200 degrees Celsius and 800 degrees Celsius, as described above. In some embodiments, such as those in which the dielectric surface is silicon nitride, the substrate may be further contacted with a silane during pretreatment, as described above.
[0034] In some embodiments, the present disclosure relates to a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface including silicon nitride, the method including preheating the substrate by contacting the substrate with hydrogen and argon at a temperature above room temperature (such as a temperature between 200-800 degrees Celsius) while contacting the substrate with argon and silane, followed by forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature between 200-800 degrees Celsius in a region between a lid heater and a showerhead of a processing chamber, and flowing the reaction products into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate. In some embodiments, silane and argon are provided through a second gas flow line 163 to form a titanium material layer including or consisting of titanium silicide (TiSix). In an embodiment, a silane (SiH4) pre-soak enhances selectivity for a remote plasma enhanced chemical vapor deposition (CVD) titanium deposition process and a remote plasma enhanced CVD titanium silicide (TiSix) deposition process. In an embodiment, the pre-treatment shown in process sequence 201 includes pre-heating the substrate by contacting the substrate with hydrogen and argon at a temperature above room temperature (such as a temperature between 200 and 800 degrees Celsius) while contacting the substrate with argon and silane.
[0035] In embodiments, the dielectric layer 305 may include one or more features 351, such as vias or trenches, formed in the dielectric layer 305. The one or more features 351 may be formed by etching the dielectric layer 305 using any suitable etching process. In some embodiments, the one or more features 351 are defined by one or more sidewalls 314, openings 322, and top corners 321. In some embodiments, the one or more features 351 may have a high aspect ratio, for example, an aspect ratio between about 5:1 and about 20:1. As used herein, aspect ratio is the ratio of the depth of the feature to the width of the feature. In embodiments, the one or more features 351 have a width 309 of 20 nanometers or less, 10 nanometers or less, or a width 309 between 5 and 10 nanometers.
[0036] 2, in some embodiments, the method 200 may begin at 202 by forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) in a region between a lid heater and a showerhead of a processing chamber at a first temperature between 200 and 800 degrees Celsius. In some embodiments, the method 200 proceeds to 204 by flowing reaction products, such as reaction products from the remote plasma reaction, into the processing chamber to selectively form a layer of titanium material on a silicon surface of a substrate. In some embodiments, the method includes forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) in a region between a lid heater (such as the lid heater 131 of FIG. 1) and a showerhead (such as the showerhead 165 shown in FIG. 1) in a process chamber (such as the process chamber 100 of FIG. 1) to selectively deposit a titanium material layer 350 on a silicon surface 302 of the substrate to form a reaction product suitable for forming a titanium material layer 350 on a substrate, such as a semiconductor substrate 190, in the process chamber. In embodiments, the dielectric surface 304 inhibits deposition of the titanium material layer 350 on the dielectric surface 304. In embodiments, the remote plasma reaction reacts titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) at a first temperature between 200 and 800 degrees Celsius. In some embodiments, a substrate, such as semiconductor substrate 190, includes a feature, such as a high aspect ratio feature, with a silicon surface 302 disposed at a bottom 307 of the high aspect ratio feature, and a dielectric surface 304 disposed at one or more sidewalls 314 of the high aspect ratio feature, such as one or more features 351. In some embodiments, the first temperature is about 550 degrees Celsius, or less than 500 degrees Celsius. In some embodiments, about 65 watts of RF energy is provided to the remote plasma reaction. In embodiments, the titanium material layer is deposited to a predetermined thickness, such as about 10 Angstroms to about 100 Angstroms, or about 100 to about 500 Angstroms. In some embodiments, the titanium material layer 350 includes titanium, titanium silicide, or substantially pure titanium.
[0037] In some embodiments, the method 200 further includes adding a silane compound, such as silane, hydrogen, and argon to a showerhead (such as the showerhead 165 of FIG. 1) for contacting with the remote plasma reaction. In embodiments, the titanium material layer 350 includes or consists of titanium silicide. In some embodiments, titanium silicide is designated TiSix, where x is a number in the range of 0.4 to 2.2.
[0038] 2, in processing sequence 205, some embodiments of method 200 may include post-deposition processing of the titanium material layer to further enhance selectivity and facilitate robust formation of semiconductor devices. Accordingly, the present disclosure includes post-processing of the titanium material layer. In some embodiments, the post-deposition processing of the titanium material layer includes a pre-selected processing sequence depending on the composition of the deposited titanium material layer, for example, whether the titanium material layer is the result of remote plasma enhanced chemical vapor deposition (CVD) deposition of titanium or remote plasma enhanced chemical vapor deposition (CVD) deposition of titanium silicide.
[0039] The inventors have found that it is advantageous to post-treat the titanium material layer following deposition of the titanium material layer. For example, the inventors have found that residues or reaction by-products such as titanium chlorides (TiClx or TiClx, where x is a number ranging from 1 to 3, or x=3) on the showerhead contribute to the formation of titanium nitride (TiN), depositing problematic TiN films on both silicon or exposed silicon surfaces and dielectric surfaces, such as silicon nitride dielectric surfaces, which reduces selectivity. The inventors have found that post-treating after deposition of remote plasma CVD titanium or remote plasma CVD titanium silicide, but before any downstream nitridation, passivates by-products such as titanium chlorides deposited or attached to the showerhead and reduces problematic memory effects to less than 3 angstroms.
[0040] In some embodiments, a post-deposition treatment may be performed following the remote plasma CVD deposition of titanium. The inventors have recognized that when a remote plasma reaction involves titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) supplied through the first gas flow line 162, and argon (Ar) supplied through the second gas flow line 163 at a first temperature of 200-800 degrees Celsius, titanium chloride (TiClx) and hydrogen radicals may collect between the showerhead and the substrate, resulting in titanium chloride (TiClx) depositing on the showerhead surface and / or the top surface of the substrate, which can be problematic. Following the formation of titanium chloride (TiClx), the titanium chloride (TiClx) can be contacted with silane provided through second gas flow line 163, which coats the titanium chloride (TiClx) and forms titanium silicide (TiSix) on the showerhead at a temperature greater than 400 degrees Celsius, such as 450-500 degrees Celsius, or between 200-800 degrees Celsius. In some embodiments, the temperature of the showerhead is between 200-800 degrees Celsius or about 500 degrees Celsius, heated by radiant energy from a lid heater at a temperature of 200-800 degrees Celsius or about 550 degrees Celsius. In embodiments, 0.5 liters to 3 liters of a silane compound, such as silane, is added. In embodiments, 500-3000 sccm of the silane compound or silane flows through second gas flow line 163. In some embodiments of the post-treatment, following the formation of titanium silicide (TiSix), a hydrogen soak and / or a remote plasma soak are performed to purge the silane compound or silane from the processing chamber. In these soaks, hydrogen radicals react with titanium silicide (TiSix) to form a robust titanium silicide (TiSix) composition that does not flake off from the showerhead and / or on the substrate. In embodiments, titanium silicide (TiSix) has superior adhesion and strong bonding compared to titanium chloride (TiClx). In some embodiments, a remote plasma is performed by flowing hydrogen and argon through the first gas flow line 162 while flowing argon through the second gas flow line 163.In embodiments, the process chamber is grounded in such a manner that a remote plasma is formed between the lid heater and the showerhead. In some embodiments, after flowing the reaction products into the process chamber to selectively form a titanium material layer on the silicon surface of the substrate, the titanium material layer is post-treated at a temperature greater than 200 degrees Celsius, or between 200 and 800 degrees Celsius. In some embodiments where the titanium material layer comprises or consists of titanium, the post-treating or post-treatment includes contacting the titanium with one or more of silane and hydrogen or hydrogen radicals.
[0041] In some embodiments, a post-deposition treatment may be performed following the remote plasma CVD deposition of titanium silicide. The inventors have observed that when a remote plasma reaction involves titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) supplied through the first gas flow line 162, and argon (Ar) and silane supplied through the second gas flow line 163 at a first temperature between 200 and 800 degrees Celsius, titanium chloride (TiClx), hydrogen radicals and silane compounds such as silane react between the showerhead and the substrate to form titanium silicide (TiSix) on the showerhead surface and / or the top surface of the substrate. Including silane compounds such as silane in the deposition reactants results in the formation of problematic titanium silicide (TiSix). Following the formation of titanium silicide (TiSix), silane is purged from the process chamber by performing a hydrogen soak and / or a remote plasma soak. In these soaks, hydrogen radicals react with titanium silicide (TiSix) to form a robust titanium silicide (TiSix) composition that does not flake off on the substrate or from the showerhead. In embodiments, the titanium silicide (TiSix) has excellent adhesion and strong bonding. In some remote plasma CVD deposition of titanium silicide embodiments, a silane soak process sequence is not performed because in embodiments, the deposition chemistry includes silane. In some embodiments, a remote plasma is performed by flowing hydrogen and argon through the first gas flow line 162 while flowing argon through the second gas flow line 163. In embodiments, the process chamber is grounded in such a manner that a remote plasma is formed between the heater lid and the showerhead. In some embodiments, the post-treated titanium material layer includes or consists of titanium silicide, and the post-treatment includes contacting the titanium silicide with one or more of hydrogen or hydrogen radicals, e.g., contacting the titanium silicide with one or more of hydrogen or hydrogen radicals in an amount sufficient to render the titanium silicide robust.
[0042] In some embodiments, the method 200 may further include forming a direct plasma reaction between nitrogen (N2), hydrogen (H2), and argon (Ar) in a processing chamber (such as the processing chamber 100 of FIG. 1) between a showerhead (such as the showerhead 165 of FIG. 1) and a substrate to form a titanium nitride capping layer 370 on or within the titanium material layer 350 on the silicon surface 302 of the semiconductor substrate 190. In some embodiments, a direct plasma nitrogen and hydrogen reaction is provided to form the titanium nitride capping layer 370. In some embodiments, the direct plasma reaction is performed after post-treating the titanium material layer 350 as described above. In some embodiments, the direct plasma reaction includes nitrogen in an amount of 4-8 standard liters per minute (slpm) or about 6 slpm. In some embodiments, hydrogen is provided in an amount of 0.5-2 slpm or about 1 slpm to the direct plasma reaction. In embodiments, argon is provided in an amount of 2-5 slpm, such as 3.75 slpm to the direct plasma reaction. In embodiments, the process chamber during the direct plasma reaction has a pressure of about 1-8 Torr, such as 4 Torr. In embodiments, about 500 Watts of RF power is provided during the direct plasma reaction. In some embodiments, the wafer temperature is maintained at a temperature of 200-800 degrees Celsius, such as about 425 degrees Celsius, during the direct plasma reaction. In some embodiments, the lid heater is heated to a temperature of 200-800 degrees Celsius, such as about 550 degrees Celsius, during the direct plasma reaction. In some embodiments, the pedestal temperature is maintained at a temperature of 200-800 degrees Celsius, or about 450 degrees Celsius, during the direct plasma reaction.
[0043] In some embodiments, the nitridation process sequence or direct plasma reaction provides nitrogen at a flow rate of about 0.1 slpm to 6 slpm and hydrogen in an amount of about 0.1 slpm to 6 slpm. In embodiments, the process chamber pressure is maintained at 1 Torr to 15 Torr during the direct plasma reaction. In embodiments, RF power of about 100 Watts to 1000 Watts is provided during the direct plasma reaction.
[0044] Figure 4 is a flow diagram of a method 400 of selective deposition according to some embodiments of the present disclosure. Figures 5A-5C are exemplary cross-sectional views of a substrate during different stages of the processing sequence of Figure 4 according to some embodiments of the present disclosure. The method of the present disclosure can be performed in a processing chamber configured for thermal deposition techniques such as chemical vapor deposition (CVD) or in a processing chamber discussed above with respect to Figure 1.
[0045] In an embodiment, the method 400 is performed on a semiconductor substrate 590, shown in Figure 5A, having a silicon surface 502 and one or more dielectric surfaces, such as a dielectric surface 504. In an embodiment, the semiconductor substrate 590 may include a silicon material 501, such as the silicon material 301 described above.
[0046] In some embodiments, the silicon material 501 is deposited by any suitable atomic layer deposition process or chemical layer deposition process. In some embodiments, the silicon material 501 can include any suitable silicon material for semiconductor device fabrication. With reference to FIG. 5A, there may be a silicon oxide layer (not shown) on the silicon surface 502. This silicon oxide layer may be a native oxide layer 510 (shown in dashed lines in FIG. 5A) or may be formed when the silicon surface 502 comes into contact with oxygen, for example, oxygen in air or water. The silicon oxide layer may be problematic in some embodiments because it may have a lower selectivity to titanium material than the exposed silicon surface. In some embodiments, the method 400 may include pretreating the silicon surface 502 to form an exposed silicon surface. In some embodiments, the method includes contacting the silicon surface 502 with one or more etchants to form the exposed silicon surface 502. In some embodiments, the silicon oxide layer is removed to form the exposed silicon surface before depositing the titanium material on or directly on the silicon surface 502. Non-limiting examples of exposed silicon surface materials include substantially pure silicon, such as silicon that is substantially free of oxide. In some embodiments, the semiconductor substrate 590 may be pre-treated and post-treated as described above. In some embodiments, the remote plasma CVD deposition of titanium silicide may be followed by a post-deposition treatment as described above. In some embodiments, the remote plasma CVD deposition of titanium may be followed by a post-deposition treatment as described above.
[0047] In embodiments, the dielectric layer 505 including the dielectric surface 504 is not the same as the silicon material 501 including the silicon surface 502. In some embodiments, the dielectric layer 505 is deposited by any suitable atomic layer deposition process or chemical layer deposition process. In embodiments, the dielectric layer 505 and the dielectric surface 504 include or consist of silicon oxide (SiO2), silicon nitride, silicon oxynitride (SiON), or combinations thereof.
[0048] In embodiments, the dielectric layer 505 may include one or more features 551, such as vias or trenches, formed in the dielectric layer 505. The one or more features 551 may be formed by etching the dielectric layer 505 using any suitable etching process. In some embodiments, the one or more features 551 are defined by one or more sidewalls 514, openings 522, and top corners 521. In some embodiments, the one or more features 551 may have a high aspect ratio, for example, an aspect ratio between about 5:1 and about 20:1. As used herein, aspect ratio is the ratio of the depth of the feature to the width of the feature. In embodiments, the one or more features 551 have a width 509 of 20 nanometers or less, 10 nanometers or less, or a width 509 between 5 and 10 nanometers.
[0049] In an embodiment, the method 400 begins at 402 (shown in dashed lines) where a first direct plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) is optionally formed in a region between the showerhead and the substrate in a processing chamber for 0.1-200 seconds. In an embodiment, a layer, such as a monolayer, of titanium material 511 (shown in FIG. 5B) may be deposited on the silicon surface 502 to prepare the silicon surface 502 for further deposition. In an embodiment, the first direct plasma reaction is performed for a very short time, such as 0.1-200 seconds. In an embodiment, the first direct plasma reaction is performed at a temperature of 200-800 degrees Celsius or 300-700 degrees Celsius. In an embodiment, the processing chamber is provided with sufficient amounts of titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) to prepare the silicon surface 502 for further deposition. In an embodiment, the process chamber is provided with titanium tetrachloride (TiCl 4 ), hydrogen (H 2 ), and argon (Ar) in amounts sufficient to deposit a monolayer of a titanium material 511, such as titanium, on the silicon surface 502.
[0050] In an embodiment, the method 400 may begin with a process sequence 404 in which a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) is formed in a process chamber, such as in a region between a lid heater and a showerhead, to selectively deposit a titanium material layer 550 on a silicon surface 502 of a semiconductor substrate 590 to form a titanium material layer 550 (shown in FIG. 5B) on the semiconductor substrate 590 in the process chamber. The dielectric surface 504 inhibits the titanium material layer 550 from depositing on the dielectric surface 504. In an embodiment, the remote plasma reaction reacts titanium tetrachloride (TiCl4), hydrogen (H2) and argon (Ar) at a first temperature between 200 and 800 degrees Celsius.
[0051] In some embodiments, this remote plasma reaction can form titanium silicide as titanium material layer 550. For example, in embodiments, forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2), and argon (Ar) in the process chamber between the lid heater and the showerhead further includes adding silane, hydrogen, and argon to the showerhead in contact with the remote plasma reaction. In some embodiments, the silane, hydrogen, and argon can be provided via the second flow line 163 shown in FIG. 1.
[0052] As shown in processing sequence 405 of method 400, in some embodiments, method 400 may include post-processing the titanium material layer over the substrate. In embodiments, this post-processing includes the embodiments described above with respect to processing sequence 205 of method 200.
[0053] In an embodiment, the method 400 includes forming 406 a direct plasma reaction between nitrogen (N2), hydrogen (H2) and argon (Ar) in a region between the showerhead and the substrate in the processing chamber to form a titanium nitride layer 559 on or within the silicon surface 502 of the substrate on a titanium material layer 550 (shown in FIG. 5C). In some embodiments, the titanium nitride layer 559 is formed within the titanium material layer 550.
[0054] In an embodiment, as shown in Figure 5C, the silicon surface 502 is at the bottom of the feature 551. In an embodiment, the method of the present disclosure further includes filling the feature from the bottom to the top 525 with a metal fill 523, such as cobalt or tungsten.
[0055] In an embodiment, the present disclosure relates to a processing chamber comprising a lid heater, a showerhead, and a substrate support disposed within the processing chamber, the processing chamber configured to remotely ignite a plasma in a region between the lid heater and the showerhead, and directly ignite a plasma in a region between the showerhead and the substrate support. In some embodiments, the lid heater comprises an RF electrode for emitting RF energy into the processing chamber. In some embodiments, the showerhead comprises an RF electrode for emitting RF energy into the processing chamber. In some embodiments, the showerhead may be connected to a ground. For example, the showerhead may be grounded or not grounded depending on the user needs and the desired placement of the plasma in the processing chamber. In an embodiment, the showerhead is connected to a ground to remotely ignite a plasma between the lid heater and the showerhead in the processing chamber. In some embodiments, the showerhead is not connected to a ground to directly ignite a plasma between the showerhead and the substrate in the processing chamber. In an embodiment, the substrate support is connected to a ground. In some embodiments, the process chamber includes a switch 184 in communication with the ground 183 and the RF electrode 180, the switch 184 configured to control remote and direct plasma formation according to user needs according to the present disclosure. In an embodiment, the switch 184 and the showerhead 165 are in communication and configured to control remote and direct plasma formation according to user needs according to the present disclosure. In some embodiments, the RF energy provided to the remote plasma reaction in the process volume 101 is about 65 Watts to 150 Watts. In some embodiments, the RF energy provided to the remote plasma reaction in the process volume 101 is about 120 Watts to 140 Watts, or about 130 Watts. In some embodiments, the RF energy provided to the remote plasma reaction in the process volume 101 is pulsed RF energy or continuous wave mode RF. In some embodiments, the RF power in the remote plasma reaction in the process volume 101 is about 130 Watts, the pulse frequency is about 1 kHz, and the duty cycle is about 50%.
[0056] In some embodiments, the present disclosure relates to a method for selectively depositing a titanium material layer on a substrate having a silicon surface and a dielectric surface, the method including forming a remote plasma reaction between titanium tetrachloride (TiCl4), hydrogen (H2) and a noble gas, such as argon (Ar), in a region between a lid heater and a showerhead of a process chamber at a first temperature between 200-800 degrees Celsius to form one or more reaction products, and flowing the one or more reaction products into the process chamber to selectively form a titanium material layer on the silicon surface of the substrate. In some embodiments, the method includes adding one or more silane compounds, hydrogen and a noble gas, such as argon, to the showerhead for contact with the remote plasma reaction. In some embodiments, the one or more silane compounds are silane (SiH4), disilane (Si2H6), trisilane (Si3H8) and tetrasilane (Si4H 10 ) or a combination thereof. In an embodiment, one or more silane compounds are added in an amount sufficient to form TiSix in accordance with the present disclosure.
[0057] The present disclosure can also be practiced using other semiconductor substrate processing systems in which process parameters can be adjusted by one of ordinary skill in the art to achieve acceptable characteristics using the teachings disclosed herein without departing from the spirit of the present disclosure.
[0058] While the forgoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof.
Claims
1. A processing chamber comprising: Lid heater; a shower head disposed below the lid heater; a substrate support disposed within the processing chamber below the showerhead, the processing chamber configured to remotely ignite a plasma in a region between the lid heater and the showerhead and directly ignite a plasma between the showerhead and the substrate support; a gas panel coupled to the process chamber and configured to supply titanium tetrachloride (TiCl 4 ), hydrogen (H 2 ), and a noble gas; a processing chamber comprising:
2. 10. The processing chamber of claim 1, wherein the showerhead is connected to ground to remotely ignite a plasma in the process chamber between a lid heater and the showerhead.
3. The processing chamber of claim 1 , wherein the gas panel is further configured to supply silane and disilane.
4. 10. The processing chamber of claim 1, wherein the lid heater is configured to heat an area between the lid heater and the showerhead to a temperature between 200 and 800 degrees Celsius.
5. The processing chamber of claim 1 , further comprising: a radio frequency electrode embedded in the lid heater; and a radio frequency electrode embedded in the showerhead.
6. further comprising a switch in communication with the ground, the RF electrode, and the showerhead; 10. The processing chamber of claim 1, wherein the switch is configured to selectively couple RF energy to the chamber lid when the switch is placed in a first position and to selectively couple RF energy to the showerhead when the switch is placed in a second position.
7. The processing chamber of claim 1 , further comprising a heating element embedded in the substrate support.
8. 10. The processing chamber of claim 1, wherein the showerhead is a multi-gas showerhead having two or more separate paths allowing two or more gases to be introduced separately into the processing chamber without premixing.
9. 10. The processing chamber of claim 8, further comprising: a first gas flow line configured to provide a gas flow to a region between the lid heater and the showerhead; and a second gas flow line configured to provide a gas flow into the showerhead.
10. a control unit configured to control operation of the processing chamber to selectively deposit a layer of titanium material on a substrate having a silicon surface and a dielectric surface, the control unit comprising: In the region between the lid heater and the showerhead of the processing chamber, titanium tetrachloride (TiCl 4 ), hydrogen (H 2 forming a remote plasma reaction between hydrogen (H2O) and argon (Ar) at a first temperature between 200 and 800 degrees Celsius; 10. The processing chamber of claim 1, further comprising a control unit that causes a reaction product to flow into the processing chamber to selectively form a titanium material layer on the silicon surface of the substrate.
11. 11. The processing chamber of claim 10, wherein the control unit is further configured to control operation of the processing chamber by pre-heating the substrate to a temperature between 200 and 800 degrees Celsius and contacting the substrate and a dielectric surface with argon, hydrogen, silane, and combinations thereof prior to selectively forming a titanium material layer on a silicon surface of the substrate.
12. A processing chamber comprising: Lid heater; a showerhead disposed below the lid heater, the showerhead being a multi-gas showerhead having two or more separate paths allowing two or more gases to be introduced separately into the processing chamber without premixing; a plenum defined in a region between the lid heater and the showerhead; a gas panel configured to provide one or more gases to the plenum via a first gas flow line and one or more gases into the showerhead via a second gas flow line; a substrate support disposed within the processing chamber below the showerhead, the processing chamber configured to remotely ignite a plasma in the pronum and directly ignite a plasma between the showerhead and the substrate support; Including, The process chamber, wherein the gas panel is configured to supply titanium tetrachloride (TiCl 4 ), hydrogen (H 2 ), and a noble gas.
13. 13. The processing chamber of claim 12, wherein the showerhead is connected to ground to remotely ignite a plasma in the process chamber between a lid heater and the showerhead.
14. The processing chamber of claim 12 , wherein the gas panel is further configured to supply silane and disilane.
15. The processing chamber of claim 12, wherein the lid heater is configured to heat an area between the lid heater and the showerhead to a temperature between 200 and 800 degrees Celsius.
16. The processing chamber of claim 12 , further comprising a radio frequency electrode embedded in the lid heater and a radio frequency electrode embedded in the showerhead.
17. further comprising a switch in communication with the ground, the RF electrode, and the showerhead; 13. The processing chamber of claim 12, wherein the switch is configured to selectively couple RF energy to the chamber lid when the switch is placed in a first position and to selectively couple RF energy to the showerhead when the switch is placed in a second position.
18. The processing chamber of claim 12 further comprising a heating element embedded in the substrate support.
Citation Information
Patent Citations
Method of forming salicide
JP1999507770A
Apparatus and method for minimizing parasitic chemical vapor deposition during atomic layer deposition
JP2003517731A
Dual-chamber plasma processing apparatus
JP2006041539A
Apparatus and processes for fluid dielectrics
JP2011525299A
Dual delivery chamber design
JP2013541848A