By employing an isotropic SmCo sintered magnet and controlling the heating and cooling process, the method achieves uniform magnetization characteristics, addressing non-uniformity issues in existing technologies and improving magnetic sensor accuracy.

JP7576505B2Active Publication Date: 2024-10-31MINEBEAMITSUMI INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2021070163
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-04-19
Publication Date
2024-10-31
Estimated Expiration
2041-04-19

AI Technical Summary

Technical Problem

Existing magnetization technologies for permanent magnets result in non-uniform magnetization characteristics due to misalignment during manufacturing, leading to variations in surface magnetic flux density, which affects the accuracy of magnetic sensors like magnetic encoders.

Method used

A method involving the use of an isotropic SmCo sintered magnet with a predetermined shape, applied in the vicinity of the magnetized object, where the object is heated above its Curie point and then cooled while maintaining a magnetizing magnetic field, ensuring uniform magnetization characteristics.

Benefits of technology

This approach improves the uniformity of magnetization characteristics on the surface of the magnetized object, enhancing the accuracy and consistency of magnetic sensors by minimizing variations in magnetic properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576505000003
    Figure 0007576505000003
  • Figure 0007576505000004
    Figure 0007576505000004
  • Figure 0007576505000005
    Figure 0007576505000005
Patent Text Reader

Abstract

To provide a manufacturing method of a permanent magnet and a magnetizing device in which the uniformity of magnetization characteristics of a magnetic pattern magnetized with multiple poles on the surface of a magnetized object is improved.SOLUTION: A manufacturing method of a permanent magnet by a magnetizing device 1 includes a heating step of arranging a magnetic field portion 6 in which a plurality of magnetizing permanent magnets for applying a magnetic field for magnetization to an object 100 to be magnetized are arranged at predetermined intervals in the vicinity of the object 100 to be magnetized, and raising the temperature of the object 100 to a temperature equal to or higher than the Curie point of the object to be magnetized, and a magnetizing step of lowering the temperature of the object 100 to be magnetized, which has reached the Curie point or above, to a temperature below the Curie point, and continuing to apply a magnetizing magnetic field to the object 100 to be magnetized by the magnetic field portion 6, and the magnetizing permanent magnet is an isotropic SmCo sintered magnet with a predetermined shape.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a permanent magnet and a magnetizing device. [Background technology]

[0002] Conventionally, techniques for multi-pole magnetization with a narrow magnetization pitch have been known (see, for example, Patent Document 1 and Non-Patent Document 1). In such magnetization techniques, the object to be magnetized is heated by a heating unit, rapidly heated to a temperature above the Curie temperature of the magnetic powder that constitutes the object to be magnetized, and then cooled from that temperature to a temperature below the Curie temperature while continuously generating a magnetic field by a permanent magnet in a field magnet unit, thereby performing multi-pole magnetization with a narrow magnetization pitch.

[0003] The magnetization device using the above magnetization technology has a heating section and a magnetizing section arranged in the axial direction as separate structures, and a field space is formed by arranging the desired number of poles of SmCo sintered magnets as a field source, and the object to be magnetized is rapidly heated to a temperature above its Curie temperature, and then cooled in the field space. During this time, the magnetizing magnetic field is continuously applied to the object to be magnetized by the SmCo sintered magnet, thereby providing high magnetization characteristics.

[0004] The permanent magnet used as the field source in the magnetization technology described above is an SmCo sintered magnet. Here, Non-Patent Document 1 states with regard to the SmCo sintered magnet that is the field source, "The magnetic field generated by the SmCo sintered magnet was calculated to be 160 kA / m or more even at 320°C at the outer peripheral portion of the magnet where magnetization is performed. Therefore, it is clear that it has a sufficient field magnetic field to magnetize an Nd-Fe-B magnet." From this description, it can be seen that the SmCo sintered magnet used as the field source is an anisotropic sintered magnet. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2006-295122 A [Non-patent literature]

[0006] [Non-Patent Document 1] "Powder and Powder Metallurgy" Vol. 57 (2010) No. 1 P19-P26 Summary of the Invention [Problem to be solved by the invention]

[0007] The anisotropic sintered magnet that constitutes the field magnet portion of a magnetization device using the above magnetization technology is generally manufactured by applying an aligning magnetic field and applying a prescribed pressure to mold the magnet in order to align the magnetization easy axes of the crystal grains in a certain direction, and then sintering the magnetized magnet at a prescribed temperature.

[0008] Sintered magnets are manufactured by applying an aligning magnetic field, applying a predetermined pressure to form the magnet, and then sintering it at a predetermined temperature. During this process, the orientation direction can sometimes deviate (become disturbed) from the specified direction. As a result, the magnetic properties of some parts of the sintered magnet block can deteriorate due to the deviation in orientation.

[0009] Usually, a block of sintered magnets manufactured by sintering is cut into a desired shape by cutting, and then magnetized. Magnetization is performed in a direction that matches the direction of the aligning magnetic field, but the magnetizing magnetic field follows the oriented direction. For this reason, sintered magnets cut from a part where the orientation has shifted have lower magnetic properties than sintered magnets cut from other parts, and the magnetic properties vary depending on the part cut out of the block.

[0010] When a magnetizing device using the above magnetizing technology is used to magnetize a magnetic sensor, for example, a permanent magnet for a magnetic encoder, the magnetic pattern (alternate N and S poles) formed in the circumferential direction of the magnet surface will have partially different magnetization characteristics, resulting in variations in the surface magnetic flux density. A magnetic encoder recognizes information related to the position by detecting the magnetic pattern formed on the magnet surface, but variations in the surface magnetic flux density of the magnetic pattern can reduce the signal accuracy of the encoder.

[0011] In view of the above problems, the present invention provides a method for manufacturing a permanent magnet and a magnetizing device that can improve the uniformity of the magnetization characteristics of a magnetic pattern magnetized in multiple poles on the surface of an object to be magnetized. [Means for solving the problem]

[0012] In order to solve the above-mentioned problems and achieve the object, a manufacturing method of a permanent magnet according to one aspect of the present invention includes a heating step of arranging a field magnet section in which a plurality of magnetizing permanent magnets are arranged at predetermined intervals near an object to be magnetized, and raising the temperature of the object to be magnetized to a temperature equal to or higher than the Curie point of the object to be magnetized, and a magnetization step of cooling the object to be magnetized that has reached a temperature equal to or higher than the Curie point to a temperature below the Curie point, while continuing to apply a magnetizing magnetic field to the object to be magnetized by the field magnet section, wherein the magnetizing permanent magnets are isotropic SmCo sintered magnets having a predetermined shape. Effect of the Invention

[0013] According to one aspect of the present invention, it is possible to improve the uniformity of the magnetization characteristics of a magnetic pattern magnetized in multiple poles on the surface of an object to be magnetized. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 is a diagram showing an example of the schematic configuration of a magnetization device used in a method for producing a permanent magnet according to an embodiment. [Diagram 2] FIG. 2 is a perspective view showing a field magnet portion of the magnetizing device shown in FIG. [Diagram 3] FIG. 3 is a cross-sectional view showing the object to be magnetized after magnetization. [Figure 4] FIG. 4 is an explanatory diagram of the operation of the magnetizing device shown in FIG. [Diagram 5] FIG. 5 is an explanatory diagram of the operation of the magnetizing device shown in FIG. [Figure 6] FIG. 6 is an explanatory diagram of the operation of the magnetizing device shown in FIG. [Figure 7] FIG. 7 is a diagram for explaining the evaluation method of the examples. [Figure 8] FIG. 8 is a diagram showing the measurement results in the example. [Figure 9] FIG. 9 is a diagram for explaining the magnetic field generated by the isotropic sintered SmCo magnet shown in FIG. [Figure 10] FIG. 10 is a diagram for explaining the magnetic field generated by the anisotropic sintered SmCo magnet shown in FIG. [Figure 11] FIG. 11 is a graph showing the uniformity of the generated magnetic field of the evaluation sample in terms of standard deviation. [Figure 12] FIG. 12 is a diagram showing a schematic configuration example of a magnetizing device according to a first modified example. [Figure 13] FIG. 13 is a diagram showing a schematic configuration example of a magnetizing device according to a first modified example. [Figure 14] FIG. 14 is a perspective view showing a field magnet portion of the magnetizing device shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, a permanent magnet manufacturing method and a magnetizing device according to an embodiment will be described with reference to the drawings. Note that the present invention is not limited to the embodiment. In addition, the dimensional relationships of each element in the drawings, the ratios of each element, etc. may differ from the reality. The drawings may also include parts with different dimensional relationships and ratios. In principle, the contents described in one embodiment or modified example are similarly applied to other embodiments or modified examples.

[0016] [Embodiment] First, an example of a magnetizing device used in the manufacturing method of a permanent magnet according to the embodiment will be described. FIG. 1 is a diagram showing a schematic configuration example of a magnetizing device used in the manufacturing method of a permanent magnet according to the embodiment. FIG. 2 is a perspective view showing a field magnet part of the magnetizing device shown in FIG. 1. FIG. 3 is a cross-sectional view showing an object to be magnetized after magnetization. FIGS. 4 to 6 are explanatory views of the operation of the magnetizing device shown in FIG. 1. FIG. 3 is a cross-sectional view in a plane including the axial direction of the object to be magnetized. Here, the X direction in each diagram is the radial direction of the object to be magnetized in this embodiment. The Z direction is the axial direction of the object to be magnetized, and is the up-down direction, with the Z1 direction being the upward direction and the Z2 direction being the downward direction.

[0017] 1 to 3, a magnetization device 1 used in the manufacturing method of a permanent magnet according to the embodiment magnetizes an object 100 to be magnetized and manufactures an object 100′ to be magnetized. The magnetization device 1 includes a stand unit 2, a moving unit 3, a heating unit 4, a preheating unit 5, a field magnet unit 6, a positioning pin 7, a cooling unit 8, and a control unit 10.

[0018] The base unit 2 is a base of the magnetization device 1, and at least a moving unit 3, a heating unit 4, a preheating unit 5, a field magnet unit 6, a positioning pin 7, a cooling unit 8, and a control unit 10 are mounted on the base unit 2.

[0019] The moving unit 3 moves the magnetized object 100 and the heating unit 4 between a non-heating position and a heating position in the axial direction. The moving unit 3 shown in FIG. 1 has a ceiling plate 31, an actuator 32, and a heating unit mounting base 33. The ceiling plate 31 is disposed apart from the base unit 2 in the axial direction, and the actuator 32 and the heating unit mounting base 33 are fixed thereto. The actuator 32 moves the ceiling plate 31 relative to the base unit 2 in the axial direction. The actuator 32 is, for example, a linear motion mechanism such as a hydraulic cylinder, and is supplied with power from an external power source (not shown), and is driven and controlled by the control unit 10. A plurality of actuators 32 are disposed between the base unit 2 and the ceiling plate 31, for example, two or four actuators are disposed. The heating unit mounting base 33 is, to which the heating unit 4 is fixed, and is fixed to the lower side surface of the ceiling plate 31.

[0020] The heating unit 4 applies heating for magnetization to the object 100 to be magnetized. The heating unit 4 is made of a non-magnetic metal material, such as non-magnetic stainless steel, and heats the object 100 to a temperature equal to or higher than the Curie point of the magnetic powder constituting the object 100 to be magnetized. The heating unit 4 in this embodiment is formed in a disk shape, and of the two surfaces in the vertical direction, the upper side surface is fixed to the heating unit mounting base 33 of the moving unit 3, and the lower side surface is the heating surface 4a. The heating surface 4a is formed to have an outer diameter larger than the outer diameter of the object 100 to be magnetized, and faces a later-described mounting surface 6a of the field magnet unit 6 in the axial direction. That is, the heating surface 4a faces the object 100 to be magnetized placed on the mounting surface 6a in the axial direction. The heating surface 4a also comes into contact with the object 100 to be magnetized at the heating position. The heating unit 4 has one or more heaters, is supplied with power from an external power source (not shown), and has its temperature controlled by the control unit 10.

[0021] The preheating section 5 performs preliminary heating on the object 100 to be magnetized. The preheating section 5 is made of a non-magnetic metal material, and heats the object 100 to a temperature lower than the Curie point of the magnetic powder constituting the object 100 to be magnetized (a temperature higher than room temperature) before the object 100 reaches the heating position. The preheating section 5 in this embodiment is formed in a cylindrical shape, and the field magnet section 6 and the positioning pin 7 are fixed thereto. Here, the preheating section 5 heats the object 100 to be magnetized placed on the field magnet section 6 via the field magnet section 6 and the positioning pin 7. The preheating section 5 has two sides in the vertical direction, the lower side is fixed to the stand section 2, and the upper side is the mounting heating surface 5a. The mounting heating surface 5a is formed larger than the outer diameter of the field magnet section 6, and contacts the field magnet section 6 and the positioning pin 7. The preheating section 5 is supplied with power from an external power source (not shown), has one or more heaters, and is temperature controlled by the control section 10.

[0022] The field magnet section 6 generates a magnetic field for the object 100 to be magnetized. The field magnet section 6 in this embodiment magnetizes the object 100 to be magnetized in the axial direction, and includes a main body section 61, a flange section 62, and a permanent magnet 63 that is a permanent magnet for magnetization. The main body section 61 is made of a non-magnetic metal material and formed in a cylindrical shape. Of the two sides in the vertical direction, the lower side surface is fixed to the mounting and heating surface 5a of the preheating section 5, and the upper side surface is the mounting surface 6a on which the object 100 to be magnetized is placed. The main body section 61 is formed with an insertion hole 6b into which the positioning pin 7 is inserted. The flange section 62 is formed to protrude radially outward from the lower end of the main body section 61. The flange portion 62 is configured to fix the field magnet portion 6 to the preheating portion 5 by inserting a fastener, for example, a fastening screw, into a through hole (not shown) and fixing the fastener to the preheating portion 5 with the field magnet portion 6 placed on the placement heating surface 5a of the preheating portion 5. The permanent magnet 63 is embedded in the upper end of the main body portion 61 and generates a magnetic field for the magnetized object 100, and is, for example, a rectangular SmCo sintered magnet. When viewed from the top and bottom, the permanent magnets 63 are arranged at equal intervals in the circumferential direction of a concentric circle centered on the center of the main body portion 61. The field magnet portion 6 has a plurality of recesses formed radially at predetermined intervals along the circumferential direction, and each of the plurality of permanent magnets 63 is disposed in each of the plurality of recesses. The permanent magnet 63 has two magnetic poles (S pole, N pole) on the upper side and the lower side, and is embedded in the main body portion 61 so that the magnetic poles are alternately different in the circumferential direction. Here, the permanent magnet 63 has a magnetic pole (e.g., S pole) on the upper side that is different from the magnetic pole (e.g., N pole) of the permanent magnets 63, 64 adjacent thereto in the circumferential direction on the upper side, and a magnetic pole (e.g., N pole) on the lower side that is different from the magnetic pole (e.g., S pole) of the permanent magnet 63 adjacent thereto in the circumferential direction on the lower side. Note that, in Fig. 2, the permanent magnet 63 is embedded in the main body 61 in a state where it is exposed to the mounting surface 6a, but it may be embedded inside the main body 61 without being exposed to the mounting surface 6a.

[0023] Furthermore, the shape of the permanent magnet 63 is not limited to a rectangle, and may be any shape as long as it can be embedded in the main body 61. For example, the shape of the permanent magnet 63 may be a sector shape when viewed from above. Furthermore, FIG. 2 illustrates the field magnet section 6 in which the permanent magnets 63 are arranged on concentric circles centered on the center of the main body 61, but this embodiment is not limited to this. For example, this embodiment may use a field magnet section 6 in which the permanent magnets 63 are arranged on two concentric circles with different diameters.

[0024] The positioning pin 7 determines the position of the object 100 to be magnetized with respect to the field magnet portion 6 in the radial direction, and is inserted into a through hole 100c (described later) of the object 100 to be magnetized. The positioning pin 7 is fixed to the preheating portion 5 by being inserted into the insertion hole 6b of the field magnet portion 6 with the field magnet portion 6 fixed to the preheating portion 5.

[0025] The cooling section 8 cools the object 100 to be magnetized heated by the heating section 4. The cooling section 8 in this embodiment is fixed to the stand section 2 by a fixing member (not shown), and outputs air toward the object 100 to be magnetized placed on the field magnet section 6. The cooling section 8 is, for example, an air-cooling fan or a compressor that supplies compressed air, and cools the object 100 to be magnetized after heating by forced air cooling, which has high cooling efficiency, rather than natural air cooling. The cooling section 8 is supplied with power from an external power source (not shown), and the air supply is controlled by the control section 10.

[0026] The control unit 10 controls the magnetization device 1 to magnetize the object 100 to be magnetized. The control unit 10 controls the moving unit 3, the heating unit 4, the preheating unit 5, and the cooling unit 8. The control unit 10 drives and controls the moving unit 3 to move the heating unit 4 relative to the object 100 to be magnetized placed on the field magnet unit 6 between a non-heating position and a heating position. Here, the non-heating position is a position where the heating surface 4a is separated (non-contact) from the object 100 to be magnetized in the axial direction, and where the heating unit 4 does not heat the object 100 to be magnetized (see FIG. 4). On the other hand, the heating position is a position where the heating surface 4a is close to the object 100 to be magnetized in the axial direction (in this embodiment, the heating surface 4a is in contact with the object 100 to be magnetized), and where the heating unit 4 heats the object 100 to be magnetized (see FIG. 5). The control unit 10 controls the temperature of the heating unit 4 to heat the heating unit 4 to a heating temperature equal to or higher than the Curie point of the magnetic powder constituting the magnetized object 100. In this embodiment, the control unit 10 heats the heating unit 4 to a temperature 30°C higher than the Curie point and equal to or lower than 350°C before the heating position. The heating temperature is a temperature that can suppress the occurrence of deterioration of the magnetic properties of the magnetic powder constituting the magnetized object 100 and deterioration of the thermosetting resin described later. The heating temperature is a temperature lower than the Curie point of the magnetizing permanent magnet. Here, the control unit 10 controls the pressing force of the heating unit 4 against the magnetized object 100 when the heating surface 4a contacts the magnetized object 100. The control unit 10 drives and controls the moving unit 3 to a pressing force that can suppress damage to the magnetized object 100 when the heating surface 4a contacts the magnetized object 100. This makes it possible to suppress damage to the object 100 to be magnetized and to make the contact state between the object 100 to be magnetized and the heating unit 4 uniform. The control unit 10 controls the temperature of the preheating unit 5, thereby heating the preheating unit 5 to a preheat temperature lower than the Curie point of the magnetic powder constituting the object 100 to be magnetized before it reaches the heating position. In this embodiment, the control unit 10 heats the preheating unit 5 to a temperature that is 30°C below the Curie point and 150°C above before it reaches the heating position. In other words, the preferable range of the preheating temperature T is T <T c , the more preferable range of preliminary temperature T is T≦T c More specifically, 150°C≦T <T cMore specifically, 150°C≦T≦T c The temperature is −30. The control unit 10 controls the temperature of the cooling unit 8, thereby cooling the heated object 100 to be magnetized after it has been moved from the heated position to the non-heated position (see FIG. 6).

[0027] Here, the object 100 to be magnetized and the object 100' to be magnetized after magnetization are formed in a ring shape as shown in Fig. 1 and Fig. 3, and have a lower side surface 100a, an upper side surface 100b, a through hole 100c, and an outer circumferential surface 100d, which are both sides in the axial direction. The object 100 to be magnetized is a rare earth iron-based magnet before magnetization, and in this embodiment, for example, is formed by mixing magnetic powder containing neodymium (Nd-Fe-B), which is a magnetically isotropic rare earth iron-based magnet, and a thermosetting resin, for example, an epoxy resin, in a predetermined ratio. The object 100 to be magnetized is not a small object to be magnetized, but a so-called large object to be magnetized, and is formed in a ring shape with an outer diameter of 10 mm or more, preferably an outer diameter of 15 mm to 50 mm.

[0028] The object to be magnetized 100 is preferably an anisotropic rare earth iron-based magnet having an average crystal grain size of 10 nm to 10,000 nm, more preferably an anisotropic rare earth iron-based magnet having an average crystal grain size of 10 nm to 6,600 nm. When such an anisotropic rare earth iron-based magnet is used, it can be strongly magnetized by the magnetizing device 1 described above.

[0029] Next, a magnetization method for the object 100 to be magnetized by the magnetization device 1 in this embodiment will be described. The magnetization device 1 is in a non-heating position. The object 100 to be magnetized is previously formed into a ring shape according to the number of objects to be manufactured. First, the control unit 10 starts heating the heating unit 4 and the preheating unit 5 as shown in FIG. 1. Here, the control unit 10 heats the heating unit 4 to a heating temperature and heats the preheating unit 5 to a preheating temperature. Next, the worker moves the object 100 to be magnetized downward in the axial direction (arrow A in the figure) with the through hole 100c of the object 100 to be magnetized facing the positioning pin 7. As a result, the object 100 to be magnetized is placed on the placement surface 6a of the field magnet unit 6 as shown in FIG. 4. At this time, the worker inserts the upper end of the positioning pin protruding from the mounting surface 6a of the field magnet unit 6 into the through hole 100c of the object 100 to be magnetized, thereby positioning the object 100 to be magnetized with respect to the magnetization device 1. Note that the upper side surface 100b of the object 100 to be magnetized faces the heating surface 4a of the heating unit 4 in the axial direction.

[0030] Next, the control unit 10 moves the heating unit 4 from the non-heating position to the heating position with respect to the magnetized object 100 by the moving unit 3 after a first predetermined time T1 has elapsed since the magnetized object 100 was placed on the placement surface 6a (arrow B in the figure). Here, the first predetermined time T1 refers to a sufficient time for the heating unit 4 to maintain the heating temperature and for the magnetized object 100 placed on the placement surface 6a to receive heat from the preheating unit 5 via the field magnet unit 6 so that the temperature of the magnetized object 100 can be lowered to a temperature lower than the Curie point, which is higher than room temperature. In other words, after the heating unit 4 reaches the heating temperature at the non-heating position and the object 100 reaches the preheating temperature, the control unit 10 moves the heating unit 4 to the heating position with respect to the magnetized object 100, and starts heating the preheated object 100 with the heating surface 4a in contact with the magnetized object 100. When the heating unit 4 is moved from the non-heated position to the heated position by the moving unit 3 with respect to the object 100 to be magnetized, the control unit 10 ends heating of the preheating unit 5, i.e., turns off the temperature control. Next, as shown in FIG. 5, the control unit 10 heats the object 100 to be magnetized until the Curie point or higher while the heating surface 4a is in contact with the object 100 to be magnetized. Next, the control unit 10 moves the heating unit 4 from the heated position to the non-heated position with respect to the object 100 to be magnetized (arrow C in the figure) after a second predetermined time T2 has elapsed since the start of heating of the object 100 to be magnetized at the heating position. Here, the second predetermined time T2 refers to a time sufficient for the object 100 to be magnetized to reach the Curie point or higher.

[0031] 6, the control unit 10 causes the cooling unit 8 to cool the object 100 to be magnetized at the non-heated position. Next, the control unit 10 ends the cooling by the cooling unit 8 at the non-heated position after a third predetermined time T3 has elapsed since the cooling by the cooling unit 8 was started. Here, the third predetermined time T3 refers to a sufficient time for the object 100 to cool from a temperature equal to or higher than the Curie point to a temperature lower than the Curie point, preferably to a temperature 50° C. below the Curie point.

[0032] Next, the worker takes out the magnetized object 100'. When the magnetizing device 1 is to newly magnetize the object 100 to be magnetized, the control unit 10 starts heating the preheating unit 5 since the heating unit 4 has already been heated.

[0033] As described above, the magnetization device 1 in this embodiment magnetizes the object 100 to be magnetized by raising the temperature of the object 100 to be magnetized from below the Curie point to above the Curie point, and then lowering the temperature from above the Curie point to below the Curie point while the magnetizing magnetic field is applied by the field unit 6. In this way, the magnetization device 1 produces an object 100' to be magnetized after magnetization from the object 100 to be magnetized, as shown in FIG. 3. In the object 100' to be magnetized after magnetization, the areas corresponding to the permanent magnets 63 of the field unit 6 are magnetized. In this embodiment, the object 100' to be magnetized after magnetization is a permanent magnet in which magnetized areas 101 corresponding to the permanent magnets 63 are formed, and the permanent magnet is magnetized with multiple poles in a ring shape in at least the lower side surface 100a. Here, since the heating unit 4 heats the object 100 to be magnetized in the axial direction, i.e., the heating surface 4a and the upper side surface 100b of the object 100 to be magnetized are opposed to each other, the upper side surface 100b of the object 100 to be magnetized after magnetization has a thicker oxide film than the outer peripheral surface 100d in the radial direction. As a result, it was confirmed that the amount of Nd in the object 100' to be magnetized after magnetization is greater on the upper side surface 100b than on the outer peripheral surface 100d, and more Nd segregation occurs.

[0034] In the magnetization device 1 of this embodiment, the heating surface 4a of the heating unit 4 is closer to the object 100 to be magnetized in the axial direction at the heating position than at the non-heating position, so that the heating unit 4 heats the object 100 to be magnetized in the axial direction. Therefore, compared with the case where the object 100 to be magnetized is heated in the radial direction by the heating unit 4, i.e., with the heating surface 4a facing the outer peripheral surface 100d of the object 100 to be magnetized, the case where the object 100 to be magnetized is heated in the axial direction, i.e., with the heating surface 4a facing the upper side surface 100b of the object 100 to be magnetized, can suppress uneven heating of the object 100 to be magnetized and can suppress non-uniform heating of the object 100 to be magnetized. In particular, a large object 100 to be magnetized has a larger heat capacity than a small object 100 to be magnetized. Since the small object 100 to be magnetized heats up and cools down easily, the temperature distribution in the object 100 to be magnetized is unlikely to be biased. However, when the object to be magnetized is large, for example, has a large diameter, the object 100 to be magnetized is likely to be heated non-uniformly. In the case of a large object 100 to be magnetized, it is possible to further increase the heating temperature or lengthen the second predetermined time T2 in order to suppress the occurrence of non-uniform heating, but there is a risk of the magnetic properties of the magnetic powder constituting the object 100 to be magnetized and the thermosetting resin being deteriorated. However, the magnetization device 1 of this embodiment heats the object 100 to be magnetized in the axial direction, i.e., by facing the heating surface 4a and the upper side surface 100b of the object 100 to be magnetized, even if the object 100 to be magnetized is large, and therefore the non-uniform heating of the object 100 to be magnetized can be suppressed even if the heating temperature is not high and the second predetermined time T2 is not long. This makes it possible to suppress unevenness in the temperature of the object 100 to be magnetized in a state in which the magnetizing magnetic field is applied by the field portion 6, and therefore makes it possible to achieve uniformity in the magnetization characteristics of the object 100 to be magnetized.

[0035] As described above, the manufacturing method of the permanent magnet according to the present embodiment includes a heating step of arranging a field magnet section 6 in which a plurality of permanent magnets 63, which are magnetizing permanent magnets for applying a magnetizing magnetic field to the magnetized object 100, are arranged at a predetermined interval (for example, at equal intervals) near the magnetized object 100, and raising the temperature of the magnetized object 100 to a temperature equal to or higher than the Curie point of the magnetized object 100, and a magnetization step of lowering the temperature of the magnetized object 100 that has reached a temperature equal to or higher than the Curie point to a temperature lower than the Curie point, while continuing to apply a magnetizing magnetic field to the magnetized object by the field magnet section 6. In the manufacturing method of the permanent magnet according to the present embodiment, the permanent magnets 63, which are magnetizing permanent magnets, are isotropic SmCo sintered magnets having a predetermined shape (for example, a rectangular shape). As a result, in the present embodiment, it is possible to improve the uniformity of the magnetic properties of the magnetic pattern magnetized into multiple poles on the surface of the magnetized object 100' after magnetization. This point will be described below.

[0036] The SmCo sintered magnet used as the magnetizing permanent magnet in this embodiment is isotropic, so it is molded under a predetermined pressure without applying an aligning magnetic field during molding, and then sintered at a predetermined temperature. The block sintered at the predetermined temperature is cut into a predetermined shape by machining to obtain a rectangular magnet. The cut-out rectangular magnet is then magnetized in a predetermined direction and then placed, for example, in the field magnet section 6 of the magnetization device 1.

[0037] On the other hand, since the SmCo sintered magnets used as magnetized permanent magnets are usually anisotropic magnets, they are molded by applying a predetermined pressure while applying an aligning magnetic field in a predetermined direction during molding, and then sintered at a predetermined temperature. During this process, the orientation direction may deviate from the predetermined direction, resulting in variations in magnetic properties due to the deviation in orientation depending on the location of the sintered magnet block. In this regard, since an isotropic SmCo sintered magnet is used in this embodiment, there is no deviation in the orientation direction and there is almost no variation in magnetic properties, so the desired magnetization can be achieved.

[0038] In addition, since an isotropic SmCo sintered magnet has lower magnetic properties (low surface magnetic flux density) than an anisotropic SmCo sintered magnet, the magnetization properties of the magnetized object 100 are low. For example, the magnetic field generated by an anisotropic SmCo sintered magnet, which is a field source, is calculated to be 160 kA / m or more at a position 0.3 mm away from the magnet's outer periphery where magnetization is performed at 320°C. In contrast, the magnetic field generated by an isotropic SmCo sintered magnet is 40 kA / m or more and less than 160 kA / m, which is a lower value than that of an anisotropic SmCo sintered magnet. However, in the case of a permanent magnet for a magnetic encoder, the magnitude of the magnetization magnetic field of an isotropic SmCo sintered magnet does not pose a practical problem. Rather, for accurate sensing, it is important to minimize the distribution variation of the generated magnetic field of a permanent magnet used to magnetize a permanent magnet for a magnetic encoder. In this regard, since an isotropic SmCo sintered magnet does not suffer from variations in magnetic properties due to misalignment, when an object to be magnetized 100' magnetized by an isotropic SmCo sintered magnet is used as a magnetic sensor component, the uniformity of the magnetic properties is improved, thereby improving the sensing accuracy.

[0039] [Example] An anisotropic sintered SmCo (2-17 type) magnet processed into a rectangular shape and an isotropic sintered SmCo (2-17 type) magnet processed into a rectangular shape were prepared, and each was magnetized in the axial direction to prepare an evaluation sample. Fig. 7 is a diagram for explaining the evaluation method in the example.

[0040] Then, as shown in Fig. 7, 15 pre-magnetized anisotropic sintered SmCo (2-17 system) magnets (hereinafter, anisotropic SmCo sintered magnets) and 15 pre-magnetized isotropic sintered SmCo (2-17 system) magnets (hereinafter, isotropic SmCo sintered magnets) were embedded in the recesses of the field magnet section 6 of the magnetization device 1. The anisotropic sintered magnets and the isotropic sintered magnets were arranged so that their magnetic poles were alternately different in the circumferential direction. Next, a pin-shaped measuring tool with a measuring probe at its tip was brought close to each sintered magnet and held at a position a predetermined distance away from the magnet, and the field magnet section 6 was rotated to measure the surface magnetic flux density as the magnetic field generated by each magnet.

[0041] Fig. 8 is a diagram showing the measurement results in the example. Fig. 8 shows the results of measuring the surface magnetic flux density (mT) as the magnetic field generated by the magnet. In Fig. 8, the vertical axis shows the surface magnetic flux density (mT) and the horizontal axis shows the angle by which the field magnet portion 6 was rotated, i.e., the position of each sintered magnet. As shown in Fig. 8, it can be seen that the magnetic field generated by the magnet is greater for anisotropic SmCo sintered magnets than for isotropic SmCo sintered magnets.

[0042] FIG. 9 is a diagram for explaining the magnetic field generated by the isotropic SmCo sintered magnet shown in FIG. 8. FIG. 9(A) is an enlarged view of the data of the magnetic field generated by the isotropic SmCo sintered magnet among the data shown in FIG. 8. FIG. 9(B) is a diagram showing the magnetic field generated by the isotropic SmCo sintered magnet shown in FIG. 8, normalized with the maximum magnetic field generated on the S pole side as 1, excluding the magnetic fields generated by the magnets at both ends. FIG. 9(C) is a diagram showing the magnetic field generated by the isotropic SmCo sintered magnet shown in FIG. 8, normalized with the maximum magnetic field generated on the N pole side as 1, excluding the magnetic fields generated by the magnets at both ends. That is, FIG. 9(A) shows the actual measured values ​​of each isotropic SmCo sintered magnet, FIG. 9(B) shows the standardized values ​​obtained by standardizing the peak value of each isotropic SmCo sintered magnet with the maximum value on the S pole side, and FIG. 9(C) shows the standardized values ​​obtained by standardizing the peak value of each isotropic SmCo sintered magnet with the maximum value on the N pole side. Table 1 below shows the numerical values ​​in Fig. 9. Note that N (actual value) and S (actual value) in Table 1 show the absolute values ​​of the peak value of the actual measurement on the N pole side and the peak value of the actual measurement on the S pole side. Furthermore, the Nmax normalization in Table 1 shows the standard value of the peak value (absolute value) of each actual measurement on the N pole side when the maximum peak value (maximum absolute value) of the actual measurement on the N pole side is set to 1, and the Smax normalization in Table 1 shows the standard value of the peak value (absolute value) of each actual measurement on the S pole side when the maximum peak value (maximum absolute value) of the actual measurement on the S pole side is set to 1.

[0043] [Table 1]

[0044] FIG. 10 is a diagram for explaining the magnetic field generated by the anisotropic SmCo sintered magnet shown in FIG. 8. FIG. 10(A) is an enlarged view of the data of the magnetic field generated by the anisotropic SmCo sintered magnet among the data shown in FIG. 8. FIG. 10(B) is a diagram showing the magnetic field generated by the anisotropic SmCo sintered magnet shown in FIG. 8, normalized with the maximum magnetic field generated on the S pole side being 1, excluding the magnetic fields generated by the magnets at both ends. FIG. 10(C) is a diagram showing the magnetic field generated by the anisotropic SmCo sintered magnet shown in FIG. 8, normalized with the maximum magnetic field generated on the N pole side being 1, excluding the magnetic fields generated by the magnets at both ends. That is, FIG. 10(A) shows the actual measured values ​​of each anisotropic SmCo sintered magnet, FIG. 10(B) shows the normalized values ​​obtained by normalizing the peak value of each anisotropic SmCo sintered magnet with the maximum value on the S pole side, and FIG. 10(C) shows the normalized values ​​obtained by normalizing the peak value of each anisotropic SmCo sintered magnet with the maximum value on the N pole side. The values ​​in Fig. 10 are summarized in Table 2 below. N (actual measurement value), S (actual measurement value), and Nmax normalization in Table 2 are the same as in Table 1, so the explanation will be omitted.

[0045] [Table 2]

[0046] Fig. 11 is a diagram showing the uniformity of the generated magnetic field of the evaluation sample in standard deviation. In Fig. 11, isotropic SmCo_N is the standard deviation of the standardized value of Nmax normalization in Table 1, isotropic SmCo_S is the standard deviation of the standardized value of Smax normalization in Table 1, anisotropic SmCo_N is the standard deviation of the standardized value of Nmax normalization in Table 2, and anisotropic SmCo_S is the standard deviation of the standardized value of Smax normalization in Table 2. When calculating the standard deviation shown in Fig. 11, the peak values ​​of the magnets at both ends, which have no magnets at both ends, tend to generate a larger magnetic field due to the magnetic path, so the peak values ​​of the magnets at both ends are removed.

[0047] As shown in FIG. 11, the standard deviation of the isotropic SmCo sintered magnet is "0.0405" at the N pole and "0.0400" at the S pole. On the other hand, the standard deviation of the anisotropic SmCo sintered magnet is "0.0475" at the N pole and "0.0447" at the S pole. That is, FIG. 5 shows that the isotropic SmCo sintered magnet has a smaller standard deviation value than the anisotropic SmCo sintered magnet, and the variation in the magnetic field generated by the isotropic SmCo sintered magnet is smaller than the variation in the magnetic field generated by the anisotropic SmCo sintered magnet. Also, FIG. 5 shows that when comparing the variation on the N pole side and the S pole side of the isotropic SmCo sintered magnet, the standard deviation values ​​of both are approximately the same, so there is almost no variation between the poles.

[0048] In contrast, for anisotropic SmCo sintered magnets, the standard deviation on the south pole side (0.0447) is larger than the standard deviation on the north pole side (0.0475), indicating a large variation between poles.

[0049] From the above evaluation results, it is found that the magnetic field generated by an isotropic SmCo sintered magnet has less variation than that generated by an anisotropic SmCo sintered magnet, and the magnetic field generated by an isotropic SmCo sintered magnet has almost no variation between poles. Therefore, by using an isotropic SmCo sintered magnet as the magnetizing permanent magnet of the magnetizing device 1, it is possible to improve the uniformity of the magnetization characteristics of the magnetic pattern magnetized on the surface of the object to be magnetized.

[0050] Furthermore, the following points can be considered as advantages of using an isotropic SmCo sintered magnet as a permanent magnet for magnetization. First, since an isotropic magnet is unoriented, it is unrelated to the orientation disorder that may occur in anisotropic magnets, and high-precision magnetization is possible by precisely controlling only the magnetization direction during the manufacturing process of the isotropic magnet used for magnetization. In other words, when using an object to be magnetized in an actuator or motor, strong magnetization characteristics are required for the purpose of increasing torque and design freedom, so it was important to generate a large field magnetic field using an anisotropic SmCo sintered magnet and stably obtain strong magnetization characteristics at the saturation level. However, when using an object to be magnetized in a sensing device (magnetic encoder), precise sensing is important, and strong magnetization characteristics at the saturation level are not an essential condition, so it is sufficient to precisely control only the magnetization direction of the permanent magnet for magnetization.

[0051] In addition, if the magnetizing permanent magnet is isotropic, the magnetization direction is arbitrary, so fine adjustment is possible, which is advantageous for industrial use. In other words, since the object to be magnetized is magnetized following the orientation direction of the magnetizing permanent magnet, if the orientation direction is misaligned, it is difficult to correct the direction of the magnetic field generated by magnetization. However, with an isotropic magnet, if the magnetization direction is strictly controlled, it is possible to achieve high precision in the orientation direction, and it is also possible to finely adjust the orientation direction by intentionally shifting the magnetization direction. In addition, when the object to be magnetized is used for a magnetic encoder, a saturation level magnetization strength is not necessary, and it is sufficient to obtain a constant magnetization strength that can operate as a magnetic encoder, so it is possible to finely adjust the magnitude of the magnetization strength and achieve high precision. In addition, since the fine adjustment is possible, it is possible to improve the yield, which is advantageous for industrial use. In addition, since an isotropic magnet is easier to manufacture than an anisotropic magnet, it is possible to keep the cost required for magnetizing the object to be magnetized low.

[0052] [Modification of magnetizing device] The magnetizing device used in the above-mentioned manufacturing method of a permanent magnet is not limited to the magnetizing device 1 shown in Fig. 1. Modifications of the magnetizing device will be described below with reference to Figs. 12 to 14. Fig. 12 is a diagram showing a schematic configuration example of the magnetizing device according to the first modification. Fig. 13 is a diagram showing a schematic configuration example of the magnetizing device according to the first modification, and Fig. 14 is a perspective view showing a field magnet part of the magnetizing device shown in Fig. 13.

[0053] (First modified example of magnetizing device) First, the magnetizing device 1 according to the first modified example shown in Fig. 12 will be described. Note that the basic configuration of the magnetizing device 1 shown in Fig. 12 is the same as the basic configuration of the magnetizing device 1 shown in Fig. 1, so the configurations with the same reference numerals will be omitted or simplified in the description. The X direction shown in Fig. 12 is the radial direction of the object to be magnetized, and the Z direction is the axial direction of the object to be magnetized, which are the up-down direction. The Z1 direction shown in Fig. 12 is the up-down direction, and the Z2 direction is the down-down direction.

[0054] The magnetization device 1 according to the first modified example shown in Fig. 12 differs from the magnetization device 1 according to the embodiment shown in Fig. 1 in that a spacer 11 made of a nonmagnetic material is placed on the field magnet part 6 and the spacer 11 is interposed between the field magnet part 6 and the object 100 to be magnetized. Another difference is that the object 100 to be magnetized is magnetized by the field magnet part 6 via the spacer 11.

[0055] The spacer 11 is a member placed on the mounting surface 6a of the field magnet part 6 and interposed between the field magnet part 6 and the object 100 to be magnetized. The spacer 11 is formed, for example, in a ring shape from a nonmagnetic metal material. Examples of nonmagnetic metal materials that can be thinned include nonmagnetic stainless steel, titanium alloy, brass, etc., and it is preferable that the spacer 11 is made of these. Since it is heated, the material is not limited to nonmagnetic metal materials as long as it has heat resistance of 350°C or more. For example, nonmagnetic Secramix may be used.

[0056] The outer diameter of this spacer 11 is the same as the mounting surface 6a of the field magnet part 6. The axial thickness of the spacer 11 is preferably 0.7 mm or less, more preferably 0.3 mm or less. If the spacer thickness is greater than 0.7 mm, it may be difficult to magnetize (magnetize) the object to be magnetized. By interposing this spacer 11 made of a nonmagnetic metal material between the field magnet part 6 and the object to be magnetized 100, the force of attraction between the magnetized object 100' and the field magnet part 6 after magnetizing the object to be magnetized 100 can be reduced. As a result, the object to be magnetized 100' can be easily removed from the field magnet part 6. Furthermore, when removing the object to be magnetized 100' from the field magnet part 6, it is possible to prevent chipping of a part of the object to be magnetized 100' and damage to the isotropic SmCo sintered magnet, which is the permanent magnet for magnetization exposed on the mounting surface 6a of the field magnet part 6, by the edge of the object to be magnetized 100'.

[0057] The operation of the magnetizing method for the object 100 to be magnetized by the magnetizing device 1 according to the first modified example is similar to that of the first modified example except that the object 100 to be magnetized is placed on the field magnet portion 6 via the spacer 11, and therefore a description thereof will be omitted.

[0058] (Second modified example of magnetizing device) Next, the magnetizing device 1 according to the second modified example shown in Fig. 13 will be described. In Figs. 1 and 2, the manufacturing method of a permanent magnet according to this embodiment using an isotropic SmCo sintered magnet as a magnetizing magnet has been described as being applied to the magnetizing device 1 which magnetizes the object 100 to be magnetized in the axial direction, but the present invention is not limited thereto. The manufacturing method of a permanent magnet according to this embodiment can also be applied to a magnetizing device which magnetizes the object 100 to be magnetized in the radial direction. Note that the basic configuration of the magnetizing device 1 shown in Fig. 13 is the same as the basic configuration of the magnetizing device 1 shown in Fig. 1, and therefore the configurations with the same reference numerals will be omitted or simplified in the description.

[0059] The heating unit 4 has a main body 41 and a protrusion 42. The main body 41 is formed in a disk shape, and of the two surfaces in the vertical direction, the upper side surface is fixed to the heating unit mounting base 33 of the moving unit 3, and the protrusion 42 is formed protruding downward from the lower side surface. The lower side surface of the protrusion 42 in the vertical direction is the heating surface 4a. The heating surface 4a is configured to have a diameter smaller than the diameter of the insertion hole 9b of the field magnet unit 9.

[0060] The preheating unit 5 has an upper side surface serving as a mounting and heating surface 5a, which is formed in two stages. On the first stage on the upper side of the mounting and heating surface 5a, the object 100 to be magnetized is placed and heated, and on the second stage on the lower side, the field magnet unit 9 is placed and heated.

[0061] The field magnet section 9 shown in Figs. 13 and 14 generates a magnetic field for the object 100 to be magnetized. The field magnet section 9 in the second modified example magnetizes the object 100 to be magnetized in the radial direction, and includes a main body section 91, a flange section 92, and a permanent magnet 93 that is a permanent magnet for magnetization. The main body section 91 is made of a non-magnetic metal material and formed in a cylindrical shape. Of the two sides in the up-down direction, the lower side surface is fixed to the second step of the mounting and heating surface 5a of the preheating section 5, and the upper side surface 9a faces the ceiling plate 31 in the axial direction. The main body section 91 is formed with an insertion hole 9b into which the object 100 to be magnetized is inserted. The flange section 92 is formed to protrude radially outward from the lower end of the main body section 91. The flange portion 92 is configured to fix the field magnet portion 9 to the preheating portion 5 by inserting a fixing device, such as a fastening screw, into a through hole not shown in the figure when the field magnet portion 9 is placed on the second stage of the mounting heating surface 5a of the preheating portion 5, and fixing the fixing device to the preheating portion 5.

[0062] The permanent magnet 93, which is a permanent magnet for magnetization, is, for example, a rectangular isotropic SmCo magnet, embedded radially on the insertion hole 9b side of the main body 91, and generates a magnetic field for the object 100 to be magnetized. When viewed from above and below, a plurality of permanent magnets 93 are arranged at equal intervals along the circumferential direction of a concentric circle centered on the center of the main body 91. The permanent magnets 93 have two magnetic poles (S pole, N pole) on the radially inner side and the radially outer side, and are embedded in the main body 91 so that the magnetic poles are alternately different in the circumferential direction. Here, the magnetic pole (e.g., S pole) on the radially inner side of the permanent magnet 93 is different from the magnetic pole on the radially inner side of the permanent magnet 93 adjacent in the circumferential direction (e.g., N pole), and the magnetic pole (e.g., N pole) on the radially outer side is different from the magnetic pole on the radially outer side of the permanent magnet 93 adjacent in the circumferential direction (e.g., S pole). Although the permanent magnet 93 is embedded in the main body 91 in a state where it is exposed to the insertion hole 9b, it may be embedded inside the main body 91 without being exposed to the insertion hole 9b.

[0063] Next, a magnetization method for the object 100 to be magnetized by the magnetization device 1 in the second modified example will be described. Note that the same parts as those in the magnetization method by the magnetization device 1 according to the embodiment will be omitted or simplified in the description. First, the control unit 10 starts heating the heating unit 4 and the preheating unit 5. Next, the worker moves the object 100 to be magnetized downward in a state in which the object 100 to be magnetized faces the insertion hole 9b of the field magnet unit 9 in the axial direction, inserts the object 100 to be magnetized into the insertion hole 9b of the field magnet unit 9, and places it on the first stage of the heating placement surface 5a of the preheating unit 5. At this time, the worker positions the object 100 to be magnetized with respect to the magnetization device 1 by inserting the object 100 to be magnetized into the insertion hole 9b. The object 100 to be magnetized has an outer circumferential surface 100d facing the field magnet portion 9 in the radial direction, and an upper side surface 100b facing the heating surface 4a of the heating portion 4 in the axial direction.

[0064] Next, the control unit 10 moves the heating unit 4 from the non-heating position to the heating position with respect to the magnetized object 100 by the moving unit 3 after a first predetermined time T1 has elapsed since the magnetized object 100 was placed on the heating placement surface 5a, and starts heating the preheated magnetized object 100, and after a second predetermined time T2 has elapsed since the heating of the magnetized object 100 was started at the heating position, the control unit 10 moves the heating unit 4 from the heating position to the non-heating position with respect to the magnetized object 100 by the moving unit 3. The control unit 10 cools the magnetized object 100 by the cooling unit 8 at the non-heating position, and ends the cooling by the cooling unit 8 at the non-heating position after a third predetermined time T3 has elapsed since the cooling by the cooling unit 8 was started at the non-heating position. Next, the operator takes out the magnetized object 100'.

[0065] As described above, the magnetization device 1 in the second modified example magnetizes the object 100 to be magnetized by increasing the temperature of the object 100 to be magnetized from below the Curie point to above the Curie point, and decreasing the temperature from above the Curie point to below the Curie point while the magnetizing magnetic field is applied by the field magnetization unit 9. In this way, the magnetization device 1 produces an object to be magnetized after magnetization from the object 100 to be magnetized. After magnetization, the object to be magnetized is magnetized in areas corresponding to the permanent magnets 93 of the field magnetization unit 9. After magnetization, the object to be magnetized in the modified example is a permanent magnet in which magnetization areas corresponding to each permanent magnet 93 are formed, that is, magnetized with multiple poles in one row at least on the outer circumferential surface 100d. After magnetization, the object to be magnetized 100' in the second modified example is a permanent magnet in which magnetization areas corresponding to each permanent magnet 93 are formed, and magnetized with multiple poles in one row at least on the outer circumferential surface 100d.

[0066] Furthermore, the magnetization device 1 in the second modified example is configured to manufacture a permanent magnet magnetized with multiple poles in one row on the outer circumferential surface 100d of the object 100 to be magnetized, but is not limited to this. The permanent magnets 93 provided in the field magnet portion 9 may be arranged coaxially in multiple rows (e.g., two rows) spaced apart in the axial direction. In this case, the outer circumferential surface 100d of the object 100 to be magnetized can be magnetized with multiple poles in multiple rows (e.g., two rows) in the axial direction.

[0067] In the above embodiment and modified examples, the heating temperature is reached before the heating section 4 reaches the heating position, but this is not limited to the above. The heating section 4 may be heated to a standby temperature lower than the heating temperature in the non-heating position, and then the temperature may be increased from the standby temperature to the heating temperature in the heating position with the heating surface 4a in contact with the magnetized object 100.

[0068] Furthermore, the present invention is not limited to the above-mentioned embodiment. The present invention also includes a configuration in which the above-mentioned components are appropriately combined. Further effects and modifications can be easily derived by those skilled in the art. Therefore, the broader aspects of the present invention are not limited to the above-mentioned embodiment, and various modifications are possible. [Explanation of symbols]

[0069] 1 magnetization device, 2 stand section, 3 moving section, 4 heating section, 4a heating surface, 5 preheating section, 6 field section, 63 permanent magnet (permanent magnet for magnetization), 7 positioning pin, 8 cooling section, 9 field section, 10 control section, 11 spacer, 100 object to be magnetized, 100' object to be magnetized after magnetization

Claims

1. a heating step of arranging a field magnet portion in the vicinity of an object to be magnetized, the field magnet portion including a plurality of magnetizing permanent magnets arranged at predetermined intervals to apply a magnetizing magnetic field to the object to be magnetized, and heating the object to be magnetized to a temperature equal to or higher than the Curie point of the object to be magnetized; a magnetizing step of lowering the temperature of the object to be magnetized, which has reached a temperature equal to or higher than the Curie point, to a temperature lower than the Curie point, and continuously applying a magnetizing magnetic field to the object to be magnetized by the field magnet portion; Including, The magnetizing permanent magnet is an isotropic SmCo sintered magnet having a predetermined shape. How permanent magnets are manufactured.

2. 2. The method for producing a permanent magnet according to claim 1, wherein the permanent magnet for magnetization is a rectangular isotropic SmCo sintered magnet.

3. a field magnet portion in which a plurality of magnetizing permanent magnets are arranged at equal intervals in the circumferential direction to generate a magnetizing magnetic field for a disk-shaped object to be magnetized; a heating unit having a heating surface facing the object to be magnetized in the axial direction of the object to be magnetized and heating the object to a temperature equal to or higher than the Curie point of magnetic powder constituting the object to be magnetized; a moving section that moves the object to be magnetized and the heating section relatively between a non-heating position and a heating position in an axial direction of the object to be magnetized; A control unit that controls at least the heating unit and the moving unit; Equipped with The magnetizing permanent magnet is an isotropic SmCo sintered magnet having a predetermined shape, the non-heating position is a position where the heating surface is separated from the object to be magnetized in the axial direction and the object to be magnetized is not heated by the heating unit, the heating position is a position where the heating surface is close to the object to be magnetized in the axial direction and where the object to be magnetized is heated by the heating unit.

Citation Information

Patent Citations

  • Polarizing method of permanent magnet

    JP2006203173A

  • Device of magnetizing permanent magnet

    JP2006295122A

  • Rare earth magnet powder, rare earth bonded magnet, and method of manufacturing rare earth bonded magnet

    JP2019102583A