Pin-disk type friction-corrosion multi-environment coupling experiment device and method

The pin-disk type friction-corrosion multi-environment coupled experimental device simplifies the structure and operation of existing devices, enabling simultaneous evaluation of wear and corrosion resistance performance, thereby addressing the complexity of current testing methods and providing comprehensive material performance data.

JP7577389B2Active Publication Date: 2024-11-05HENAN UNIV OF SCI & TECH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023579626
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-11-28
Filing Date
2022-12-01
Publication Date
2024-11-05
Estimated Expiration
2042-12-01

AI Technical Summary

Technical Problem

Current experimental devices for simultaneously testing wear resistance and corrosion resistance of copper-based materials under friction-corrosion coupling conditions have complex structures and are difficult to operate, making it challenging to accurately evaluate the comprehensive material performance.

Method used

A pin-disk type friction-corrosion multi-environment coupled experimental device comprising a corrosive environment unit, electrochemical unit, and friction wear unit, which allows for adjustable loading force and rate, temperature control, and simultaneous measurement of electrochemical and frictional data, enabling synchronous detection of wear and corrosion performance.

Benefits of technology

The device simplifies the structure and operation, allowing for simultaneous evaluation of wear and corrosion resistance performance, providing comprehensive data for material development under varying conditions, and clarifying the combined damage mechanism.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007577389000001
    Figure 0007577389000001
Patent Text Reader

Abstract

Pin-disk type friction-corrosion multi-environment coupling experimental device and method [Solution] The device includes a corrosive environment unit including a box (11) and a corrosive medium located within the box (11); an electrochemical unit including an electrochemical workstation, a working electrode (3) located within the box (11), and an auxiliary electrode (8) and a reference electrode (9) one end of which are inserted into the box (11), where the working electrode (3), the auxiliary electrode (8) and the reference electrode (9) are all connected to the electrochemical workstation; and a friction and wear unit including a rotation unit and a normal force loading unit, where a sample (5) is connected to one end of the rotation unit and one end of the rotation unit extends to one side of the box (11), where a friction pair (6) is connected to one end of the normal force loading unit and one end of the normal force loading unit extends to the other side of the box (11), and where the friction and wear process is realized by contact motion between the sample (5) and the friction pair (6). The device has a simple structure, convenient operation, high measurement accuracy and comprehensive functions, and can obtain electrochemical data and friction and wear data under different corrosion and friction conditions.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the technical field of material performance testing, and more particularly to a pin-disk type friction-corrosion multiple environment coupling test device and method. [Background technology]

[0002] Metallic materials are widely used as key components in the national economy, such as electronic information, machinery manufacturing, rail transportation, and marine engineering. With the different application scenarios of various components, the requirements for the comprehensive performance of materials and the service efficiency in the service process are also different. Take copper-based materials as an example, because of their excellent conductive performance and mechanical performance, excellent cold / hot processing performance, and wear resistance and corrosion resistance, they have always been widely used as functional and structural integrated materials. With the development of science and technology and the emergence of new application scenarios, the requirements for the single wear resistance or single corrosion performance of copper-based materials in the past do not meet the actual usage requirements. For example, the application of copper-based materials to various oil drilling tools such as oil drilling guide rods, electric pump modules, drilling probes, deep sea explosion-proofing, and separable connecting valves requires high temperature, high pressure, high load, high corrosion and other severe service conditions, so copper alloy materials need to meet basic mechanical performance and also have high wear resistance and high corrosion performance.

[0003] However, for a long time, the tests and evaluations of the wear resistance and corrosion resistance of copper-based materials belong to different specialties, and each uses a single experimental device to detect a single wear resistance or a single corrosion resistance, and lacks synchronous test devices and methods for wear resistance and corrosion resistance under friction-corrosion combined conditions. For example, the test of wear resistance is mainly performed by a line-slider type or pin-disk type wear tester to perform friction and wear tests under certain load, speed and current conditions to obtain quantitative evaluation indicators such as wear rate. The test of corrosion resistance is mainly performed by static full immersion experiments, dynamic flashing experiments and electrochemical experiments in various types of corrosion media to obtain polarization curves, AC impedance spectrum curves and corrosion rates. Therefore, the single wear resistance or single corrosion resistance obtained by the above single experimental platform is difficult to accurately evaluate the comprehensive indicators of materials in the application scene of friction and corrosion. At present, the conventional experimental device that can perform friction and corrosion simultaneously has a complex structure and is difficult to operate.

[0004] Therefore, there is a need to provide an improved technical solution to address the shortcomings of the prior art. Summary of the Invention [Problem to be solved by the invention]

[0005] The objective of the present invention is to provide a friction-corrosion multi-environment coupling experimental apparatus and method, which at least solves the problem that the current experimental apparatus for synchronously detecting friction and corrosion on materials has a complicated structure and is difficult to operate. [Means for solving the problem]

[0006] In order to achieve the above object, the present invention provides the following technical means.

[0007] a corrosive environment unit including a box and a corrosive medium disposed within the box; an electrochemical unit including an electrochemical workstation, a working electrode located within a box, and an auxiliary electrode and a reference electrode, one end of which is inserted into the box, wherein the working electrode, the auxiliary electrode and the reference electrode are all in contact with a corrosive medium, and the working electrode, the auxiliary electrode and the reference electrode are all connected to the electrochemical workstation; a friction-wear unit including a rotation unit and a normal force loading unit, one end of the rotation unit is connected with a sample and extends to one side of the box, one end of the normal force loading unit is connected with a friction pair and extends to the other side of the box, the rotation unit provides a rotational motion, the normal force loading unit provides a normal loading force, and the friction-wear process is realized by the contact motion between the sample and the friction pair; A pin-disk type friction-corrosion multi-environment coupling experimental device including:

[0008] Step 1: fixing a specimen to a rotation unit, fixing a friction pair to a normal force loading unit, and putting a corrosive medium into a box so that the liquid level of the corrosive medium covers the specimen and the friction pair; Step 2: open the temperature control system to set the heating temperature, and after the temperature reaches the required level, open the first driving mechanism to rotate the sample, and open the second driving mechanism to perform a friction and wear test on the friction pair and the sample, and load the friction pair according to the set normal force and loading speed, and collect and process data during the friction and wear process to obtain electrochemical data and friction force data during the corrosion process; Step 3: changing one or more of the corrosive medium, temperature, normal load force, and loading rate and measuring again to obtain electrochemical data and frictional force data under different conditions; Step 4: closing the first driving mechanism, the second driving mechanism and the temperature control system, processing the obtained electrochemical data and friction force data, and evaluating the wear resistance and corrosion resistance performance of the material; A method for operating a pin-disk type friction-corrosion multiple environment coupling experimental device, comprising:

[0009] The experimental equipment of the present invention includes a corrosive environment unit, an electrochemical unit and a friction and wear unit, which has a simple structure and is convenient to operate, and can adjust the loading force and loading speed in the loading process, adjust and control the temperature of the corrosive medium in the friction process, and obtain electrochemical data and friction and wear data under different corrosion and friction conditions. In addition, the experimental parameters such as electrochemical curves, corrosion rate, and wear rate can be obtained synchronously, and the wear resistance and corrosion resistance performance of the material can be simultaneously detected, which is helpful to reveal the composite damage mechanism of the material under different conditions of friction, wear and corrosion coupling, and further provide guidance for the development of high wear resistance and high corrosion resistance materials. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic diagram of the structure of a pin-disk type friction-corrosion multiple environment coupling experimental device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] As shown in Fig. 1, according to the embodiment of the present invention, a pin-disk type friction-corrosion multiple environment coupling experimental device is provided, which can carry out friction-corrosion tests under various conditions by changing parameters such as corrosive medium, temperature, normal load force, load speed, sample material, etc., and measure the electrochemical curve, corrosion rate, wear rate, friction coefficient and other data of materials, and at the same time, can realize automatic loading, off-loading, infinitely variable speed, and online collection of load, rotation speed, and temperature in the test process, and synchronously evaluate the wear resistance and corrosion resistance of materials. At the same time, it is helpful to reveal the composite damage mechanism of materials under friction wear and corrosion coupling conditions, and further provide guidance for the development of high wear resistance and high corrosion resistance materials.

[0012] The apparatus includes a corrosive environment unit, an electrochemical unit, and a friction and wear unit.

[0013] The corrosive environment unit includes a box 11 and a corrosive medium located within the box 11 .

[0014] In a specific embodiment of the present invention, the material of the box 11 is a high-strength corrosion-resistant polymer material or other corrosion-resistant materials. The corrosive medium may be a standard static full immersion corrosion solution containing 3.5 wt.% NaCl, an acidic corrosion solution containing 0.1-5 wt.% hydrogen sulfide (H2S), or a corrosion solution containing 1-10 wt.% sand according to the requirements of the experimental conditions.

[0015] The electrochemical unit includes an electrochemical workstation, a working electrode 3 located in a box 11, an auxiliary electrode 8 and a reference electrode 9 one end of which are inserted into the box 11, the working electrode 3, the auxiliary electrode 8 and the reference electrode 9 are all in contact with the corrosive medium, and the working electrode 3, the auxiliary electrode 8 and the reference electrode 9 are all connected to the electrochemical workstation.

[0016] The electrochemical unit includes an electrochemical workstation, a working electrode 3 positioned in a box 11, an auxiliary electrode 8 and a reference electrode 9 each having one end inserted into the box 11, the working electrode 3, the auxiliary electrode 8 and the reference electrode 9 all being in contact with a corrosive medium, and the working electrode 3, the auxiliary electrode 8 and the reference electrode 9 all being connected to the electrochemical workstation.

[0017] In a specific embodiment of the present invention, the electrochemical workstation performs data collection and processing, and its main function is to collect electrochemical data during the corrosion process of the sample 5, and subsequently obtain important characteristic curves (e.g., AC impedance spectrum and polarization curve) for evaluating the corrosion performance of the material.

[0018] The friction-wear unit includes a rotation unit and a normal force loading unit, one end of which is connected to the sample 5 and extends to one side of the box 11, one end of which is connected to the friction pair 6 and extends to the other side of the box 11, the rotation unit provides the rotational motion, the normal force loading unit provides the normal loading force, and the friction-wear process is realized by the contact motion between the sample 5 and the friction pair 6.

[0019] In a specific embodiment of the present invention, the rotating unit includes a first driving mechanism and a friction disk 4, the propeller shaft 101 of the first driving mechanism extends into the box 11, one end of the propeller shaft 101 is connected to the working electrode 3, the friction disk 4 and the sample 5 in order, and the working electrode 3 and the sample 5 are connected by a wire. The connection point between the propeller shaft 101 of the first driving motor and the box 11 is provided with a movable seal 2 used to seal the inside and outside of the box 11 and prevent the overflow of the corrosive medium. The working electrode 3 and the friction disk 4 are removably connected with a pin or a screw, and the friction disk 4 and the sample 5 are also removably connected with a pin or a screw, the working electrode 3 is connected to the sample 5 with a wire through a through hole provided in the friction disk 4, and the connection point between the wire and the sample 5 is adopted an insulating seal treatment. Specifically, the first driving mechanism is a rotating electric machine 1, which rotates the working electrode 3 and the friction disk 4 by the rotation of a propeller shaft 101, and thus rotates the sample 5. The rotation speed of the rotating electric machine 1 is 5 to 1000 revolutions per minute. Of course, in other embodiments, the working electrode 3, the friction disk 4, and the sample 5 can be fixed to each other by other methods such as caulking or welding, and the present invention is not limited thereto.

[0020] In a specific embodiment of the present invention, the normal force loading unit includes a second driving mechanism, a fixed disk 7, and a data acquisition and processing system, the propeller shaft of the second driving mechanism extends into the box 11, and the fixed disk 7 is connected to the propeller shaft of the second driving mechanism, and the friction pair 6 is movably connected to the outside of the fixed disk 7. Specifically, the second driving mechanism is a normal force loading servo motor 12, and the contact point between the propeller shaft and the box 11 is provided with a movable seal 2, which is used to prevent the corrosive medium in the box 11 from overflowing. Preferably, the friction pair 6 is a pin shaft, the number of pin shafts is two or more, and the pin shafts are uniformly arranged along the circumferential direction on the wall surface of the fixed disk 7, and the free end portion of the pin shaft is a hemispherical or flat structure, and different friction modes are realized by replacing different types of pin shafts, so that the friction contact mode between the friction pair 6 and the sample 5 is a ball-surface or surface-surface contact.

[0021] The data collection and processing system is connected to the second driving mechanism and is used for collecting the normal load force in the friction and wear process and performing data processing to obtain the friction force data.

[0022] In a specific embodiment of the present invention, the material of the specimen 5 can be any corrosion-resistant metal material, such as aluminum alloy, copper alloy, titanium alloy, etc., and the material of the friction pair 6 can be a wear-resistant ceramic material.

[0023] In a specific embodiment of the present invention, the second driving mechanism is a normal force load servo motor 12, which provides a normal load force without rotating, and can adjust the load speed, achieve non-polarity speed change, and achieve high normal load force control accuracy. Specifically, the normal load force is 0-150N, and the normal load accuracy is 0.2%FS (FULL SCALE, full range, that is, the normal load repeat error does not exceed 0.2% of the full range).

[0024] In a specific embodiment of the present invention, the data collection and processing system includes a stress sensor, a processor, and a display, the stress sensor is built into the second drive mechanism, and the processor is electrically connected to the stress sensor and the display, and is used for processing the normal load force data collected by the stress sensor and displaying the obtained friction force data on the display.

[0025] In a specific embodiment of the present invention, the apparatus further includes a temperature control system, which includes a heater 14, a temperature sensor 10, and a control unit, where the heater 14 and the temperature sensor 10 are electrically connected to the control unit, and the control unit is used to set the temperature and control the opening and closing of the heater 14.

[0026] The heater 14 is used to heat the inside of the box 11, and one end of the temperature sensor 10 extends into the box 11 and is used to measure the temperature inside the box 11. By providing a temperature control system, the adjustment of the corrosive medium temperature can be realized to change the friction wear environment and make the function of the friction-corrosion bond test device of the present invention more comprehensive and abundant. Specifically, the operating temperature can be set to 0-80°C, and the corrosion time can be 24-720h.

[0027] In a specific embodiment of the present invention, the device further includes a separator 15, which is disposed in the lower part of the box 11 and is used to separate the box 11 into two sealed cabins, a liquid cabin and an empty cabin, the liquid cabin is used for friction and wear testing under corrosive conditions, and the heater end of the heater 14 is disposed in the empty cabin. The separator 15 is preferably made of glass.

[0028] In a specific embodiment of the present invention, all parts in the liquid cabin of the box 11 are made of high-strength insulating materials such as polymer plastics and ceramics. The propeller shaft 101 through which the first driving mechanism and the second driving mechanism extend into the box 11 is also made of polymer material. This can ensure that there is no interference of metal materials in the corrosion state, and improve the accuracy and precision of the electrochemical test.

[0029] In a specific embodiment of the present invention, the device further includes a stirring device 13 extending through the separator 15 into the liquid cabin of the box 11, and a movable seal 2 is provided at the portion of the stirring device 13 that contacts the separator 15. The stirring device 13 can improve the uniformity of the heating of the corrosive medium in the liquid cabin and realize the uniformity of the medium environment; in addition, when the corrosive medium is a solution containing sediment, the corrosive medium can be stirred to make it more uniform and avoid the settling of sediment, which is more suitable for the actual application situation.

[0030] The present invention further provides a method for operating a pin-disk type friction-corrosion multiple environment coupling experimental apparatus, the method comprising: Step 1: fixing a specimen 5 to a rotating unit, fixing the specimen 5 to a friction disc 4 with a screw, fixing the specimen 5 to a fixed disc 7 with a pin by inserting or screwing, and putting a corrosive medium into a box 11 so that the liquid level of the corrosive medium covers the specimen 5 and the friction pair 6; Step 2: open the heater 14 in the temperature control system to set the heating temperature, and after the temperature reaches the required temperature, open the rotating machine 1 to rotate the specimen 5, open the normal force loading servo motor 12 to perform a friction and wear test on the pin shaft and the specimen 5, and load according to the set normal force and loading speed, and collect and process data during the friction and wear process to obtain electrochemical data and friction force data during the corrosion process; Step 3: changing one or more of the corrosive medium, temperature, normal load force, and loading rate and measuring again to obtain electrochemical data and frictional force data under different conditions; Step 4: closing the first driving mechanism, the second driving mechanism and the temperature control system, processing the obtained electrochemical data and friction force data, and evaluating the wear resistance and corrosion resistance performance of the material; Includes.

[0031] Example 1 In this embodiment, an experimental method of simultaneously measuring the wear resistance and corrosion resistance of materials using a friction-corrosion multiple environment coupling experimental device is adopted, and the specific steps are as follows:

[0032] (1) The material of the corrosive environment unit of the pin-disk type friction-corrosion multiple environment coupling experimental apparatus and the box 11 is glass, and the corrosive medium is a standard static complete immersion corrosive aqueous solution containing 3.5 wt.% NaCl.

[0033] (2) The friction pair 6 of the pin-disk type friction-corrosion multiple environment coupling experimental device is made of ceramic material, and the material of the sample 5 is pure copper. The outer diameter of the sample is φ130 mm, the end face of the friction pair 6 is a hemisphere with a diameter of φ5 mm, and the contact method between the sample 5 and the friction pair 6 is a spherical surface. The working electrode 3 is fixed to the friction disk 4 by a screw and a pin, and is also fixed to the propeller shaft 101 of the rotating electric machine 1 and moves therewith.

[0034] (3) The normal force load servo motor 12 has a built-in mechanical sensor that realizes normal force load to measure the load force in real time. Before starting the friction and wear experiment in the corrosive medium, the original mass of the sample 5 is measured as the calculation basis for the corrosion rate and wear rate after the subsequent corrosive wear. The set normal load force is 10 N, the loading method is constant force load, the rotation speed is 10 rpm, and the rotation radius is 20 mm.

[0035] (4) In the friction and wear experiment process in a corrosive medium, the rotating machine 1 drives the movement of the sample 5, while the working electrode 4 cooperates with the auxiliary electrode 8 and the reference electrode 9 to collect electrochemical test data. After a corrosion time of 720 hours, the sample 5 is taken out and its mass is measured and compared with the mass before corrosion to calculate the corrosion rate and wear rate, and a polarization curve and an AC impedance spectrum curve are plotted.

[0036] Example 2 In this embodiment, an experimental method of simultaneously measuring the wear resistance and corrosion resistance of materials using a friction-corrosion multiple environment coupling experimental device is adopted, and the specific steps are as follows:

[0037] (1) The material of the corrosive environment unit of the pin-disk type friction-corrosion multiple environment coupling experimental device and the box 11 is glass, and the corrosive medium is an acidic corrosive aqueous solution containing 0.5 wt.% hydrogen sulfide (H2S). The heater 14 is opened and the temperature is set to 30°C.

[0038] (2) The friction pair of the pin-disk type friction-corrosion multiple environment coupling experimental device is made of ceramic material, and the material of the sample 5 is Cu-15Ni-8Sn alloy. The outer diameter of the sample 5 is φ130mm, the end face of the friction pair 6 is a hemisphere with a diameter of φ6mm, and the contact manner between the sample 5 and the friction pair 6 is a spherical surface. The working electrode 3 is fixed to the friction disk 4 by a screw and a pin, and is also fixed to the propeller shaft 101 of the rotating electric machine 1 and moves therewith.

[0039] (3) Normal Force Loading The servo motor 12 has a built-in mechanical sensor that realizes normal force loading to measure the loading force in real time. Before starting the friction and wear experiment in the corrosive medium, the original mass of the sample 5 is measured as the calculation basis for the corrosion rate and wear rate after the subsequent corrosive wear. The normal load force set is 130N, the loading method is step loading, the initial load force is 10N, and after 30 rotations it is loaded to 50N, after another 30 rotations it is loaded to 100N, after another 30 rotations it is loaded to 130N, and kept constant until the end of the experiment, the rotation speed is 20rpm, and the rotation radius is 15mm.

[0040] (4) In the friction and wear experiment process in a corrosive medium, the rotating machine 1 drives the movement of the sample 5, and at the same time, the working electrode 4 cooperates with the auxiliary electrode 8 and the reference electrode 9 to collect electrochemical test data. After a corrosion time of 240 hours, the sample 5 is taken out, its mass is measured, and compared with the mass before corrosion to calculate the corrosion rate and wear rate, and a polarization curve and an AC impedance spectrum curve are plotted.

[0041] Example 3 In this embodiment, an experimental method of simultaneously measuring the wear resistance and corrosion resistance of materials using a friction-corrosion multiple environment coupling experimental device is adopted, and the specific steps are as follows:

[0042] (1) The material of the corrosive environment unit of the pin-disk type friction-corrosion multiple environment coupling experimental device and the box 11 is glass, and the corrosive medium is a corrosive aqueous solution containing 5 wt.% soil and sand + 3.5 wt.% NaCl. The heater is opened, the heating temperature is set to 40°C, and the stirring device 13 is opened to stir the corrosive medium.

[0043] (2) The friction pair of the pin-disk type friction-corrosion multiple environment coupling experimental device is made of ceramic material, and the material of the sample 5 is a wear-resistant chromium bronze alloy. The outer diameter of the sample 5 is φ130 mm, the end face of the friction pair 6 is a flat surface with a diameter of φ5 mm, and the contact mode between the sample 5 and the friction pair 6 is face-to-face. The working electrode 3 is fixed to the friction disk 4 by a screw and a pin, and is also fixed to the propeller shaft 101 of the rotating electric machine 1 and moves therewith.

[0044] (3) Normal Force Loading The servo motor 12 has a built-in mechanical sensor that realizes normal force loading to measure the loading force in real time. Before starting the friction and wear experiment in the corrosive medium, the original mass of the sample 5 is measured as the calculation basis for the corrosion rate and wear rate after the subsequent corrosive wear. The set normal loading force is 100N, the loading method is linear loading, the loading force increases by 10N every 100 revolutions to perform linear loading, the rotation speed is 20rpm, and the rotation radius is 20mm.

[0045] (4) In the friction and wear experiment process in a corrosive medium, the rotating machine 1 drives the movement of the sample 5, while the working electrode 4 cooperates with the auxiliary electrode 8 and the reference electrode 9 to collect electrochemical test data. After a corrosion time of 300 hours, the sample 5 is taken out and its mass is measured and compared with the mass before corrosion to calculate the corrosion rate and wear rate, and a polarization curve and an AC impedance spectrum curve are plotted. [Explanation of symbols]

[0046] 1 Rotating Electric Machine 101 Propeller shaft 2 Movable seal 3 Working electrode 4 Friction Discs 5. Sample 6 Friction Pair 7 Fixed Disks 8 Auxiliary electrode 9 Reference electrode 10 Temperature Sensor 11 Box body 12 Normal force load servo motor 13 Mixing device 14 Heater 15 Separator

Claims

1. A pin-disk type friction-corrosion multiple environment coupling experimental device, The pin-disk type friction-corrosion multiple environment coupling experimental device includes a corrosive environment unit including a box and a corrosive medium disposed in the box; an electrochemical unit including an electrochemical workstation, a working electrode located within a box, and an auxiliary electrode and a reference electrode, one end of which is inserted into the box, wherein the working electrode, the auxiliary electrode and the reference electrode are all in contact with a corrosive medium, and the working electrode, the auxiliary electrode and the reference electrode are all connected to the electrochemical workstation; a friction-wear unit including a rotation unit and a normal force loading unit, one end of the rotation unit is connected with a sample and extends to one side of the box, one end of the normal force loading unit is connected with a friction pair and extends to the other side of the box, the rotation unit provides a rotational motion, the normal force loading unit provides a normal loading force, and the friction-wear process is realized by the contact motion between the sample and the friction pair; Including, the rotating unit includes a first driving mechanism and a friction disk, a propeller shaft of the first driving mechanism extends into the box, a working electrode, a friction disk, and a sample are connected to one end of the propeller shaft in this order, and the working electrode and the sample are connected by a wire; The normal force loading unit includes a second driving mechanism, a fixed disk, and a data collection and processing system, the propeller shaft of the second driving mechanism extends into the box body, and a fixed disk is connected to the propeller shaft of the second driving mechanism, the friction pair is movably connected to the outside of the fixed disk, and the data collection and processing system is connected to the second driving mechanism, and is used to collect normal load forces in the friction and wear process and process data. used to obtain friction data by The device further includes a temperature control system, the temperature control system including a heater, a temperature sensor, and a control unit, the heater and the temperature sensor are electrically connected to the control unit, the control unit is used to set a temperature and control opening and closing of the heater, the heater is used to heat the inside of the box, and one end of the temperature sensor extends into the box and is used to measure the temperature inside the box. A pin-disk type friction-corrosion multiple environment coupling experimental device.

2. The data collection and processing system includes a stress sensor, a processor, and a display, the stress sensor being built into the second drive mechanism, the processor being electrically connected to the stress sensor and the display, and being used to process the normal load force data collected by the stress sensor and to display the resulting friction force data on the display. The pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 1.

3. The apparatus further includes a separator, the separator is provided in a lower portion of the box and is used to separate the box into two sealed cabins, a liquid cabin and an empty cabin, the liquid cabin is used for friction and wear testing under a corrosive condition, and a heater end of the heater is provided in the empty cabin. The pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 1.

4. The separator is made of glass. The pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 3.

5. The apparatus further includes an agitator extending through the separator into the liquid cabin of the box; A movable seal is provided at a portion of the stirring device that comes into contact with the separator. The pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 3.

6. The propeller shaft through which the first drive mechanism and / or the second drive mechanism extend inside the box is made of a polymer material. The pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 1.

7. Step 1: fixing a sample to a rotation unit, fixing a friction pair to a normal force loading unit, and putting a corrosive medium into a box so that the liquid level of the corrosive medium covers the sample and the friction pair; Step 2: open the temperature control system to set the heating temperature, and after the temperature reaches the required level, open the first driving mechanism to rotate the sample, and open the second driving mechanism to perform a friction and wear test on the friction pair and the sample, and load the friction pair according to the set normal force and loading speed, and collect and process data during the friction and wear process to obtain electrochemical data and friction force data during the corrosion process; Step 3: changing one or more of the corrosive medium, temperature, normal load force, and loading rate and measuring again to obtain electrochemical data and frictional force data under different conditions; Step 4: closing the first driving mechanism, the second driving mechanism and the temperature control system, processing the obtained electrochemical data and friction force data, and evaluating the wear resistance and corrosion resistance performance of the material; Including, 7. A method for operating the pin-disk type friction-corrosion multiple environment coupling experimental device according to claim 1.

Citation Information

Patent Citations

  • Pin-disc type corrosive abrasion test device

    CN110006818A

  • Pin-disc-type corrosion wear testing device

    CN204286967U

  • Friction abrasion testing device

    JP2010256195A

  • Corrosion speed measurement method and corrosion speed measurement probe

    JP2011196737A

  • Electrochemical testing cell

    KR100783967B1