Method for etching features using targeted deposition for selective passivation - Patent Application 20070122999
A targeted deposition and etching process with controlled plasma treatment addresses the challenge of uniformity in high aspect ratio feature formation, enabling efficient and cost-effective semiconductor wafer processing.
Patent Information
- Application Number
- JP2021577240
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-07-03
- Filing Date
- 2020-07-01
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-07-01
AI Technical Summary
Existing semiconductor wafer processing methods using silicon oxide (SiO) on patterned organic materials or spin-on carbon (SOC) low temperature ALD for sidewall protection during etching of features are not optimal for forming high aspect ratio features due to non-uniform deposition.
A targeted deposition process involving multiple cycles of precursor layer application, curing, and plasma exposure is used to selectively harden and etch features, with controlled plasma treatment to modify the precursor layer, allowing for non-conformal deposition and etching of high aspect ratio features.
Enables efficient etching of high aspect ratio features with controlled thickness distribution, facilitating faster and cost-effective processing without the need for multiple chamber transfers.
Smart Images

Figure 0007578627000001 
Figure 0007578627000002 
Figure 0007578627000003
Abstract
Description
[Background technology]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of priority to U.S. Patent Application No. 62 / 870,271, filed July 3, 2019, which is incorporated herein by reference for all purposes.
[0002] The description of the background art provided herein is intended to provide a general background to the present disclosure. Anything described in this background art, and any potential aspects of this description, are not admitted, explicitly or implicitly, as prior art with respect to the present application.
[0003] FIELD OF THE DISCLOSURE This disclosure relates to the formation of semiconductor devices. More particularly, this disclosure relates to the formation of semiconductor devices that require etching of features.
[0004] During semiconductor wafer processing, a stack under a mask may be etched. A pattern may be transferred from the mask to one or more layers of the stack. Low temperature ALD (atomic layer deposition) of silicon oxide (SiO2) onto patterned organic materials, photoresist, or spin-on carbon (SOC) is used to provide sidewall protection for etching features. Oxygen (O2) plasma is one method used for oxidation of silicon (Si)-containing precursors. ALD provides uniform deposition, which is not always optimal for forming high aspect ratio features. Summary of the Invention
[0005] To achieve the above, according to the objectives of the present disclosure, a method for patterning a stack with a mask having a plurality of mask features is provided. A targeted deposition is provided, the targeted deposition comprising a plurality of cycles, each cycle comprising flowing a precursor to deposit a precursor layer, and target hardening the precursor layer, the targeted hardening of the precursor layer comprising flowing a hardening gas, flowing a modifying gas, forming a plasma from the hardening gas and the modifying gas, and exposing the precursor layer to the plasma to provide a targeted hardening, the plasma from the hardening gas hardening a first portion of the precursor layer, the plasma from the modifying gas modifying a second portion of the precursor layer, and the modification of the second portion reduces the hardening of the precursor layer in the second portion of the precursor layer. The stack is etched through the targeted deposition.
[0006] In another aspect, a semiconductor device is formed. A targeted deposition is provided, the targeted deposition comprising a plurality of cycles, each cycle comprising flowing a precursor to deposit a precursor layer, and target hardening the precursor layer, the targeted hardening of the precursor layer comprising flowing a hardening gas, flowing a modifying gas, forming a plasma from the hardening gas and the modifying gas, and exposing the precursor layer to the plasma to provide a targeted hardening, the plasma from the hardening gas hardens a first portion of the precursor layer, the plasma from the modifying gas modifies a second portion of the precursor layer, and the modification of the second portion reduces the hardening of the precursor layer in the second portion of the precursor layer. The stack is etched through the targeted deposition.
[0007] In another aspect, an apparatus is provided for etching features in a stack. A plasma chamber is provided. A substrate support is within the plasma chamber. A supply system supplies fluids within the plasma chamber. A fluid source supplies fluids to the supply system. The fluid sources include an etching fluid source, a precursor fluid source, a hardening fluid source, and a modifying fluid source. An electrode supplies RF power within the plasma chamber. At least one RF generator is provided. A controller is controllably connected to the fluid sources and the at least one RF generator. The controller comprises at least one processor and a computer readable medium comprising computer readable code for performing an etch of the stack. The computer readable code includes computer readable code for partially etching the stack; and computer readable code for providing targeted deposition, the targeted deposition comprising a plurality of cycles, each cycle including computer readable code for flowing precursor from a precursor fluid source to deposit a precursor layer, and computer readable code for targeted hardening of the precursor layer, the computer readable code for target hardening of the precursor layer including computer readable code for flowing a hardening gas from a hardening fluid source, computer readable code for flowing a modifying gas from a modifying fluid source, computer readable code for forming a plasma from the hardening gas and the modifying gas, and computer readable code for exposing the precursor layer to the plasma to provide the targeted hardening, wherein the plasma from the hardening gas hardens a first portion of the precursor layer and the plasma from the modifying gas modifies a second portion of the precursor layer, the modification of the second portion reducing hardening of the precursor layer in the second portion of the precursor layer; and computer readable code for etching the stack through targeted deposition.
[0008] The above-mentioned and other features of the present disclosure are set forth in the detailed description of the present disclosure, which proceeds with reference to the accompanying drawings. [Brief description of the drawings]
[0009] The present disclosure is illustrated by way of example, and not by way of limitation, in the accompanying drawings, in which like elements are numbered like elements and in which:
[0010] [Figure 1] 1 is a high level flow chart illustrating a process that can be used in one embodiment.
[0011] [Figure 2A] 1A-1C are schematic cross-sectional views of a stack processed according to one embodiment. [Figure 2B] 1A-1C are schematic cross-sectional views of a stack processed according to one embodiment. [Figure 2C] 1A-1C are schematic cross-sectional views of a stack processed according to one embodiment. [Figure 2D] 1A-1C are schematic cross-sectional views of a stack processed according to one embodiment. [Figure 2E] 1A-1C are schematic cross-sectional views of a stack processed according to one embodiment.
[0012] [Diagram 3] 1 is a schematic diagram illustrating a plasma processing chamber that can be used to practice an embodiment.
[0013] [Figure 4] FIG. 1 illustrates a computer system suitable for implementing a controller used in embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The present disclosure will be described in detail below with reference to some preferred embodiments illustrated in the accompanying drawings. In the following description, numerous specific details are set forth to facilitate a thorough understanding of the present disclosure. However, it will be apparent to those skilled in the art that the present disclosure can be practiced without some or all of these specific details. Additionally, detailed descriptions of well-known process steps and / or structures are omitted to avoid unnecessarily obscuring the present disclosure.
[0015] Low temperature ALD (atomic layer deposition) of silicon oxide (SiO2) onto patterned organic materials, photoresist, or spin-on carbon (SOC) is used to provide sidewall protection for etching features. Oxygen (O2) plasma is one method used for oxidation of silicon (Si)-containing precursors. ALD provides uniform deposition, which is not always optimal for forming high aspect ratio features.
[0016] To facilitate understanding, FIG. 1 shows a high-level flow chart of one embodiment. A stack with a mask having mask features is placed on a substrate support in a plasma chamber (step 104). FIG. 2A shows a cross-sectional view of stack 200 with substrate 205. Substrate 205 is placed under intermediate layer 208. Intermediate layer 208 is placed under mask 212. In this example, mask 212 is a patterned organic mask (such as a photoresist mask) having mask features. One or more layers may be placed between intermediate layer 208 and mask 212. Intermediate layer 208 is partially etched. One or more layers may be placed between intermediate layer 208 and substrate 205. A cyclical process or another process described below may be used to partially etch feature 216. The cyclical process described below is shown with a partially etched feature to more clearly explain the targeted deposition process. The figures are not drawn to scale to better illustrate the various features. For example, in some embodiments, feature 216 may have a height-to-width aspect ratio of at least 100 to 1. However, feature 216 is depicted as much wider to better illustrate subsequently deposited layers.
[0017] To deposit a target deposit, a target deposition is provided (step 108) that includes at least one cycle of precursor delivery (step 112) and targeted curing of the precursor (step 116). A precursor is delivered to the feature 216 (step 112). In this embodiment, a liquid silicon-containing precursor is delivered to the plasma chamber in vapor form to be vaporized and dosed to the feature 216 until saturated, forming a layer of precursor on the feature 216. Once the feature 216 has been dosed with the precursor, the delivery of the precursor vapor is stopped. The precursor then undergoes a target curing (step 116). In one embodiment, the target curing (step 116) is accomplished by subjecting the stack 200 to a target flash process. The target flash process delivers a curing gas of 1000 standard cubic centimeters per minute (sccm) to 2000 sccm of oxygen (O2) and a modifying gas of 10 sccm to 25 sccm of octafluorocyclobutane (C4F8). In this example, the hardening gas and the modifying gas are turned into a plasma by providing radio frequency (RF) power of 13.56 megahertz (MHz) at 2500 watts. A pressure of 20 millitorr (mTorr) to 100 mTorr is provided. A target flash is provided for about 0.5 seconds to about 4 seconds. The target flash forms a silicon oxide monolayer on a first portion of the feature 216. On a second portion of the feature, the formation of a target deposit is reduced or eliminated. Once the target flash operation is completed, the plasma chamber is purged. The cycle may then be repeated. In this embodiment, the precursor delivery (step 112) and the target cure (step 116) are performed sequentially and do not overlap. In this example, purging may be used to prevent overlap of the precursor delivery (step 112) and the target cure (step 116).
[0018] In one embodiment of the precursor delivery, any suitable liquid precursor capable of forming a conformal atomic layer can be utilized. In a non-limiting example, the liquid precursor can have a composition of the general type C(x)H(y)N(z)O(a)Si(b). In some embodiments, the liquid precursor is a silicon-containing polymer with silicon functional groups that can have one of the following compositions: 1-triaminosilylhexane (CH 19 N3Si), bis(t-butylamino)silane (C8H 22 N2Si), 3-aminopropyltriethoxysilane (C9H 23 NO3Si), and tri-t-butoxysilanol (C 12 H 28 In this example, the delivery of the precursor is plasma-less. The precursor has silicon functional groups that form a monolayer on the feature 216 because the precursor does not bond to another precursor.
[0019] 2B is a cross-sectional view of stack 200 after multiple cycles of target deposition (step 108). Target deposits are formed on the sidewalls of feature 216. In this example, the target deposits have a thin top region 220, a thick middle region 224, and a thin bottom region 228. In one example, the target deposits have top region 220 about 1-2 nm thick, middle region 224 about 2-4 nanometers (nm) thick, and bottom region 228 about 1 nm thick. In this example, the first portion is middle region 224 and the second portion is top region 220 and bottom region 228. The thicknesses of the target deposits are not drawn to scale to better illustrate the target deposits.
[0020] The intermediate layer 208 is then etched with respect to the mask 212 (step 120). In this example, the intermediate layer 208 is polysilicon. Figure 2C is a cross-sectional view of the stack 200 after the intermediate layer 208 has been selectively etched with respect to the mask 212. In this example, the feature 216 has been etched deeper and the target deposit has been etched away.
[0021] In this example, target deposition (step 108) and middle layer etching (step 120) are repeated for at least one more cycle (step 124). Target deposition (step 108) deposits another target deposit. Figure 2D is a cross-sectional view of stack 200 after multiple cycles of target deposition (step 108) have deposited another target deposit with another thin top region 232, another thick middle region 236, and another thin bottom region 240.
[0022] Processing continues and the cycle is repeated until feature 216 is completed. Figure 2E is a cross-sectional view of stack 200 after etching of feature 216 is complete. Further processing may be provided. For example, mask 212 may be removed. Stack 200 is then removed from the plasma chamber (step 128).
[0023] Target deposition provides a non-conformal deposit, where the thickness at various locations of the etch feature may be selectively adjusted. Various embodiments provide different controls to determine where thick and thin regions of the target deposit are located. Process parameters such as gas flow rate, pressure, side conditioning gas, process time, temperature, and electrical bias may be used as control means. Various embodiments enable etching of high aspect ratio features. In this specification and claims, a high aspect ratio feature is defined as having a height to width aspect ratio of at least 100 to 1. More specifically, a high aspect ratio feature has an aspect ratio of at least 200 to 1. Various embodiments may provide high aspect ratio features that are channels or holes. In some embodiments, the thickest portion of the target deposit is deposited over the weakest area of the feature (such as the junction area for a drilling process). Various embodiments may be used for drilling processes, shallow trench isolation, and carbon mask openings. In other embodiments, targeted deposition may be used to form lower aspect ratio features.
[0024] The dry etching chemistry and the ALD chemistry are combined into a single step to provide targeted deposition. In various embodiments, the modification gas includes a halogen-containing gas. More specifically, the modification gas includes a fluorocarbon. In various embodiments, the modification gas includes one or more of C4F8, hexafluorobutadiene (C4F6), chlorine (Cl2), hydrogen bromide (HBr), carbon tetrafluoride (CF4), fluoromethane (CH3F), or sulfur hexafluoride (SF6). In other embodiments, a metal oxide may be used for the targeted deposition. In such embodiments, a metal-containing precursor forms a metal-containing layer (such as a metal-containing precursor monolayer). A curing gas and a modification gas are provided and plasma-ignited to provide targeted metal oxide deposition. In other embodiments, silicon nitride or metal nitride may be used for the targeted deposition. In other embodiments, silicon oxynitride or metal oxynitride may be used for the targeted deposition. The precursor layer is nitrided to form a nitride or oxynitride. Thus, in various embodiments, curing the precursor layer at least one of oxidizes or nitrides portions of the precursor layer.
[0025] Without being bound by theory, it is believed that by adding an etchant and using tuning parameters during target curing, the modified gas can be utilized to selectively etch target areas of the precursor layer to reduce deposition at the target areas.
[0026] In various embodiments, the targeted curing of the monolayer may be achieved by applying RF power to a plasma chamber along with the curing gas and the modifying gas to perform a plasma flash process (or oxygen (O2) plasma cure), the plasma flash process being performed for a period of about 0.2 seconds to about 4 seconds, and the RF power being applied at a power level of about 200 watts to about 3,000 watts. The O2 plasma cure converts the Si-containing precursor to SiO2.
[0027] In other embodiments, targeted deposition may deposit thicker deposits on the sidewalls at the bottom of the feature 216. In other embodiments, targeted deposition has minimal deposition on horizontal surfaces. Various embodiments may provide targeted deposition that does not deposit on the bottom of the feature 216. Various embodiments may provide targeted deposition that does not deposit on the top of the feature 216.
[0028] The above embodiments are performed in-situ in the same chamber without moving the chuck or removing the stack from the chuck. Such embodiments provide faster and less expensive processing. Furthermore, in-situ processing allows for a higher number of cycles, so that thinner layers may be formed during each cycle. A higher number of cycles allows for improved feature shapes.
[0029] 3 is a schematic diagram of an example plasma processing system 300. The plasma processing system 300 may be used to perform an embodiment of a process. The system includes a plasma chamber 332 including a chamber body 314, a chuck 316, and a dielectric window 306. The plasma chamber 332 includes a process region, and the dielectric window 306 is disposed above the process region. The chuck 316 may be an electrostatic chuck for supporting the substrate 205, and is disposed within the chamber below the process region. A transformer coupled plasma (TCP) coil 334 is disposed above the dielectric window 306 and is connected to a matching circuit 302. The TCP coil 334 is an electrode for supplying power through the dielectric window 306. The matching circuit 302 is connected to a plasma RF generator 321.
[0030] The system includes a bias RF generator 320. The RF generator 320 may be defined as one or more generators. If multiple generators are provided, different frequencies may be used to achieve various tuning characteristics. A bias matching circuit 318 is connected between the bias RF generator 320 and a conductive plate of an assembly that defines a chuck 316. The chuck 316 also includes an electrostatic electrode to enable chucking and dechucking of the wafer. Generally, a filter and a direct current (DC) clamping power supply may be provided. Other control systems may be provided for lifting the wafer from the chuck 316.
[0031] A first gas injector 304 provides two different flow paths for injecting two separate flows of process gas or liquid precursor (in vapor form) into the plasma chamber 332 from the top of the plasma chamber 332. It should be understood that multiple gas supplies may be provided to supply different gases to the plasma chamber 332 for various types of operations, such as wafer processing operations, waferless automatic cleaning (WAC) operations, and other operations. A second gas injector 310 provides another gas flow that enters the plasma chamber 332 through the side, rather than from the top.
[0032] The supply system 328, in one embodiment, includes an etching gas supply system 327 and a liquid supply system 329. A manifold 322 is utilized to select, switch, and / or mix the output from each supply system. As described in more detail below, the etching gas supply system is configured to output an etchant gas optimized for etching one or more material layers of a substrate. The manifold 322 is further optimized in response to control from the controller 308 to perform targeted deposition. During an operational plasma process, a vacuum pump 330 is connected to the plasma chamber 332 to allow for vacuum pressure control and removal of gas by-products from the plasma chamber 332. A valve 326 is disposed between the exhaust port 324 and the vacuum pump 330 to control the amount of vacuum suction applied to the plasma chamber 332.
[0033] A fluid source 350 may be used to supply various fluids to the supply system 328. The fluids may be gases or liquids. In this embodiment, the fluid source 350 includes a precursor fluid source 354, a hardening fluid source 358, a modifying fluid source 362, and an etching fluid source 366. In various embodiments, the fluid source 350 may be a single unit or two or more separate units. For example, the precursor fluid source 354 supplies a liquid vapor and may thus be separate from the hardening fluid source 358, the modifying fluid source 362, and the etching fluid source 366, which supply gases.
[0034] 4 is a high-level block diagram illustrating a computer system 400 suitable for implementing the controller 308 used in one embodiment. Computer systems may take many physical forms, from integrated circuits, printed circuit boards, and small handheld devices to large supercomputers. The computer system 400 includes one or more processors 402 and may further include an electronic display device 404 (for displaying images, text, and other data), a main memory 406 (e.g., random access memory (RAM)), a storage device 408 (e.g., a hard disk drive), a removable storage device 410 (e.g., an optical disk drive), a user interface device 412 (e.g., a keyboard, touch screen, keypad, mouse, or other pointing device, etc.), and a communication interface 414 (e.g., a wireless network interface). The communication interface 414 allows software and data to be transferred between the computer system 400 and external devices over a link. The system may further comprise a communication infrastructure 416 (eg, a communication bus, crossover bar, or network) to which the above-mentioned devices / modules are connected.
[0035] Information transferred through communications interface 414 may be in the form of signals, such as electronic, electromagnetic, optical, or other signals that may be received by communications interface 414 over a communications link carrying the signals, which may be implemented using wires or cables, fiber optics, telephone lines, cellular phone links, radio frequency links, and / or communications channels. Using such communications interfaces, it is contemplated that one or more processors 402 may receive information from a network or output information to a network when performing the method steps described above. Additionally, method embodiments may be performed solely by the processor or may be performed over a network, such as the Internet, in cooperation with a remote processor that shares some of the processing.
[0036] The term "non-transitory computer-readable medium" is generally used to refer to media such as main memory, secondary memory, removable storage, and storage devices (such as hard disks, flash memory, disk drive memory, CD-ROMs, and other forms of persistent memory), and should not be construed to encompass transitory objects, such as carrier waves or signals. Examples of computer-readable code include machine code, such as code produced by a compiler, and files containing high-level language code that are executed by a computer using an interpreter. The computer-readable medium may also be computer-readable code conveyed by a computer data signal embodied in a carrier wave and representing a sequence of instructions executable by a processor.
[0037] Although the present disclosure has been described with reference to certain preferred embodiments, there are alternatives, permutations, and various substitute equivalents that are within the scope of the present disclosure. It should also be noted that there are many alternative ways of implementing the method and apparatus of the present disclosure. It is therefore intended that the appended claims be interpreted as including all such alternatives, permutations, and various substitute equivalents that fall within the true spirit and scope of the present disclosure. The present invention can be realized, for example, in the following manner. Application example 1: 1. A method for patterning a stack having a mask with a plurality of mask features, comprising: providing a targeted deposition; and etching the stack through the target deposition. The target deposition comprises a plurality of cycles; Each cycle is flowing a precursor to deposit a precursor layer; and target curing the precursor layer; The step of target curing the precursor layer comprises: flowing a hardening gas; flowing the reformed gas; forming a plasma from the hardening gas and the modifying gas; exposing the precursor layer to the plasma to provide a targeted cure, wherein the plasma from the curing gas cures a first portion of the precursor layer and the plasma from the modifying gas modifies a second portion of the precursor layer, the modification of the second portion reducing cure of the precursor layer in the second portion of the precursor layer. method. Application example 2: The method of application example 1, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer. Application example 3: The method of application example 2, wherein hardening the first portion of the precursor layer subjects the first portion of the precursor layer to at least one of oxidation and nitridation. Application example 4: The method of application example 1, wherein the modifying gas includes a halogen-containing gas. Application example 5: In the method according to Application Example 1, the reformed gas is 4 F 8 、C 4 F 6 、Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 , a method comprising at least one of the following: Application example 6: The method of application example 1, wherein the precursor comprises a silicon-containing polymer. Example 7: The method of application example 1, wherein the precursor comprises a polymer having silicon functional groups. Application example 8: The method of application example 1, wherein the precursor flowing step is plasma-free. Example 9: The method of application example 1, wherein the mask is formed of a carbon-containing material. Example 10: The method of application example 1, wherein the step of etching the stack etches a feature having a height-to-width aspect ratio of greater than 100:1. Example 11: The method of Application Example 1, wherein the steps of providing target deposition and etching the stack are provided cyclically during a plurality of cycles. Application example 12: The method of application example 1, wherein the steps of providing target deposition and etching the stack are provided in situ in the same plasma chamber. Application example 13: 1. A semiconductor device formed by a method for patterning a stack having a mask with a plurality of mask features, the method comprising: providing a targeted deposition; and etching the stack through the target deposition, The target deposition comprises a plurality of cycles, each cycle comprising: flowing a precursor to deposit a precursor layer; and target curing the precursor layer; The step of target curing the precursor layer comprises: flowing a hardening gas; flowing the reformed gas; forming a plasma from the hardening gas and the modifying gas; exposing the precursor layer to the plasma to provide a targeted hardening, wherein the plasma from the hardening gas hardens a first portion of the precursor layer and the plasma from the modifying gas modifies a second portion of the precursor layer, the modification of the second portion reducing hardening of the precursor layer in the second portion of the precursor layer. Example 14: 14. The semiconductor device of claim 13, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer. Application example 15: A semiconductor device according to application example 14, wherein hardening the first portion of the precursor layer subjects the first portion of the precursor layer to at least one of oxidation and nitridation. Application example 16: A semiconductor device according to application example 13, wherein the modifying gas includes a halogen-containing gas. Example 17: In the semiconductor device of Application Example 13, the modifying gas is 4 F 8 、C 4 F 6 、Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 A semiconductor device comprising at least one of: Application example 18: 14. The semiconductor device of claim 13, wherein the precursor comprises a silicon-containing polymer. Example 19: 1. An apparatus for etching features in a stack, comprising: A plasma chamber; a substrate support within the plasma chamber; a supply system for supplying a fluid into the plasma chamber; a fluid source for supplying the fluid to the supply system, a source of etching fluid; a precursor fluid source; a source of hardening fluid; a fluid source, the fluid source including a reforming fluid source; an electrode for supplying RF power within the plasma chamber; at least one RF generator; a controller controllably connected to the fluid source and to the at least one RF generator; The controller: At least one processor; a computer readable medium having computer readable code for performing an etch of the stack; Computer readable code for performing an etch of the stack includes: computer readable code for partially etching the stack; computer readable code for providing targeted deposition; and computer readable code for etching the stack through the target deposition, The target deposition comprises a plurality of cycles; Each cycle is computer readable code for flowing a precursor from the precursor fluid source to deposit a precursor layer; and computer readable code for target curing the precursor layer, The computer readable code for target curing the precursor layer comprises: computer readable code for flowing a hardening gas from the hardening fluid source; computer readable code for flowing reformulated gas from the reformulated fluid source; computer readable code for forming a plasma from the hardening gas and the modifying gas; and computer readable code for exposing the precursor layer to the plasma to provide a targeted cure; a plasma from the curing gas curing a first portion of the precursor layer; a plasma from the modifying gas modifies a second portion of the precursor layer; The modification of the second portion reduces hardening of the precursor layer in the second portion of the precursor layer. Example 20: 20. The apparatus of claim 19, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer. Example 21: The apparatus of application example 20, wherein hardening the first portion of the precursor layer at least one of oxidizes or nitrides the first portion of the precursor layer. Example 22: 20. The apparatus of claim 19, wherein the reforming gas includes a halogen-containing gas. Example 23: In the apparatus of application example 19, the reformed gas is 4 F 8 、C 4 F 6 、Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 , an apparatus comprising at least one of: Application 24: 20. The apparatus of claim 19, wherein the precursor comprises a silicon-containing polymer.
Claims
1. 1. A method for patterning a stack having a mask with a plurality of mask features, comprising: providing a targeted deposition; and etching the stack through the target deposition. The target deposition comprises a plurality of cycles; Each cycle is flowing a precursor to deposit a precursor layer; and target curing the precursor layer; The step of target curing the precursor layer comprises: flowing a hardening gas; flowing the reformed gas; forming a plasma from the hardening gas and the modifying gas; exposing the precursor layer to the plasma to provide a targeted cure, wherein the plasma from the curing gas cures a first portion of the precursor layer and the plasma from the modifying gas modifies a second portion of the precursor layer, the modification of the second portion reducing cure of the precursor layer in the second portion of the precursor layer. method.
2. 10. The method of claim 1, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer.
3. 3. The method of claim 2, wherein curing the first portion of the precursor layer at least one of oxidizes or nitrides the first portion of the precursor layer.
4. The method of claim 1 , wherein the modifying gas comprises a halogen-containing gas.
5. 2. The method of claim 1, wherein the reformulated gas is 4 F 8 , C 4 F 6 , Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 , the method comprising at least one of:
6. The method of claim 1 , wherein the precursor comprises a silicon-containing polymer.
7. The method of claim 1 , wherein the precursor comprises a silicon-functionalized polymer.
8. 10. The method of claim 1, wherein the step of flowing the precursor is plasma-less.
9. The method of claim 1 , wherein the mask is formed of a carbon-containing material.
10. 10. The method of claim 1, wherein etching the stack etches features having a height-to-width aspect ratio of greater than 100:
1.
11. 10. The method of claim 1, wherein the steps of providing target deposition and etching the stack are provided cyclically during a plurality of cycles.
12. 10. The method of claim 1, wherein the steps of providing targeted deposition and etching the stack are provided in-situ in the same plasma chamber.
13. 1. A method for producing a semiconductor device comprising patterning a stack with a mask having a plurality of mask features, comprising: providing a targeted deposition; and etching the stack through the target deposition, The target deposition comprises a plurality of cycles, each cycle comprising: flowing a precursor to deposit a precursor layer; and target curing the precursor layer; The step of target curing the precursor layer comprises: flowing a hardening gas; flowing the reformed gas; forming a plasma from the hardening gas and the modifying gas; exposing the precursor layer to the plasma to provide a targeted hardening, wherein the plasma from the hardening gas hardens a first portion of the precursor layer and the plasma from the modifying gas modifies a second portion of the precursor layer, the modification of the second portion reducing hardening of the precursor layer in the second portion of the precursor layer.
14. 14. The method of claim 13, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer.
15. 15. The method of claim 14, wherein hardening the first portion of the precursor layer at least one of oxidizes or nitrides the first portion of the precursor layer.
16. 14. The method of claim 13, wherein the modifying gas comprises a halogen-containing gas.
17. 14. The method for producing a semiconductor device according to claim 13, wherein the modifying gas is C 4 F 8 , C 4 F 6 , Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 13. A method for producing a semiconductor device, comprising:
18. 14. The method of claim 13, wherein the precursor comprises a silicon-containing polymer.
19. 1. An apparatus for etching features in a stack, comprising: A plasma chamber; a substrate support within the plasma chamber; a supply system for supplying a fluid into the plasma chamber; a fluid source for supplying the fluid to the supply system, a source of etching fluid; a precursor fluid source; a source of hardening fluid; a fluid source, the fluid source including a reforming fluid source; an electrode for supplying RF power within the plasma chamber; at least one RF generator; a controller controllably connected to the fluid source and to the at least one RF generator; The controller: At least one processor; a computer readable medium having computer readable code for performing an etch of the stack; Computer readable code for performing an etch of the stack includes: computer readable code for partially etching the stack; computer readable code for providing targeted deposition; and computer readable code for etching the stack through the target deposition, The target deposition comprises a plurality of cycles; Each cycle is computer readable code for flowing a precursor from the precursor fluid source to deposit a precursor layer; and computer readable code for target curing the precursor layer, The computer readable code for target curing the precursor layer comprises: computer readable code for flowing a hardening gas from the hardening fluid source; computer readable code for flowing reformulated gas from the reformulated fluid source; computer readable code for forming a plasma from the hardening gas and the modifying gas; and computer readable code for exposing the precursor layer to the plasma to provide a targeted cure; a plasma from the curing gas curing a first portion of the precursor layer; a plasma from the modifying gas modifies a second portion of the precursor layer; the modification of the second portion reduces hardening of the precursor layer in the second portion of the precursor layer.
20. 20. The apparatus of claim 19, wherein the precursor deposits at least one of a silicon-containing layer or a metal-containing layer.
21. 21. The apparatus of claim 20, wherein curing the first portion of the precursor layer at least one of oxidizes or nitrides the first portion of the precursor layer.
22. 20. The apparatus of claim 19, wherein the modifying gas comprises a halogen-containing gas.
23. 20. The apparatus of claim 19, wherein the reformulated gas is C 4 F 8 , C 4 F 6 , Cl 2 , HBr, CF 4 , C.H. 3 F or SF 6 , an apparatus comprising at least one of:
24. 20. The apparatus of claim 19, wherein the precursor comprises a silicon-containing polymer.
Citation Information
Patent Citations
Hybrid carbon hardmask for lateral hardmask recess reduction
JP2019503082A
Methods for forming pattern using cyclic processing
US20160314981A1
Technique to tune sidewall passivation deposition conformality for high aspect ratio cylinder etch
US20170178920A1
Hybrid carbon hardmask for lateral hardmask recess reduction
US20170207088A1