Optical devices and laser devices

The optical device addresses heat-related reliability issues by using a slant-type FBG and roughened cladding to scatter and absorb cladding mode light, enhancing performance and reducing parts.

JP7579159B2Active Publication Date: 2024-11-07FUJIKURA LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021010504
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-26
Publication Date
2024-11-07
Estimated Expiration
2041-01-26

AI Technical Summary

Technical Problem

Existing optical devices using fiber lasers face reliability issues due to heat generation caused by cladding mode light, which is absorbed by a high refractive index resin, leading to decreased performance.

Method used

An optical device with a slant-type FBG formed on the core and a roughened outer surface of the cladding to reflect and scatter cladding mode light, preventing heat generation without using resin, and a housing to accommodate and absorb the scattered light.

Benefits of technology

Prevents reliability degradation by effectively removing cladding mode light, maintaining device performance and reducing part count by integrating FBG and roughened surface functionality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007579159000001
    Figure 0007579159000001
  • Figure 0007579159000002
    Figure 0007579159000002
  • Figure 0007579159000003
    Figure 0007579159000003
Patent Text Reader

Abstract

To provide an optical device and a laser device, which can prevent reliability from being deteriorated by heat generation due to clad mode light.SOLUTION: An optical device 1 includes: a core 10a; a clad 10b that covers the core 10a and has a refractive index lower than that of the core 10a; a protective coating 10c that covers the clad 10b; a slant type FBG 11 that is formed in the core 10a in a removed portion RP obtained by removing the protective coating 10c and couples SRS light propagating the core 10a to the clad 10b. At least a part of an outer peripheral surface of the clad 10b in the removed portion RP is a roughened surface portion 12 obtained by roughening a surface.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to optical devices and laser apparatus. [Background technology]

[0002] Currently, laser devices are used in various fields such as processing, automobiles, and medicine. In recent years, for example, in the processing field, fiber laser devices that have superior beam quality and focusing ability compared to conventional laser devices (e.g., carbon dioxide gas laser devices) have been attracting attention. The maximum output of such fiber laser devices is limited by stimulated Raman scattering (SRS), which occurs nonlinearly with respect to the laser output.

[0003] The following Patent Document 1 discloses an optical device that removes SRS light generated in a fiber laser device or the like. This optical device has a slant-type Fiber Bragg Grating (FBG) formed in the core of an optical fiber, and the outer peripheral surface of the cladding is covered with a high refractive index resin. With this optical device, SRS light is selectively removed from the light propagating within the core, and cladding mode light including the removed SRS light is emitted to the outside via the high refractive index resin. This makes it possible to stabilize the signal light propagating within the core and prevent damage to the pump light source. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2020 / 171152 Summary of the Invention [Problem to be solved by the invention]

[0005] Incidentally, in the optical device disclosed in the above-mentioned Patent Document 1, the outer peripheral surface of the cladding is covered with a high refractive index resin, and therefore the cladding mode light including the SRS light coupled from the core to the cladding by the slant FBG can be efficiently emitted to the outside. However, depending on the power of the cladding mode light and the NA (Numerical Aperture), the high refractive index resin covering the outer peripheral surface of the cladding and the protective coating (protective coating of the optical fiber) may generate heat, which may reduce reliability.

[0006] The present invention has been made in view of the above circumstances, and an object of the present invention is to provide an optical device and a laser apparatus that can prevent a decrease in reliability due to heat generation caused by cladding mode light. [Means for solving the problem]

[0007] In order to solve the above problems, an optical device (1) according to one embodiment of the present invention comprises a core (10a), a cladding (10b) covering the core and having a lower refractive index than the core, a protective coating (10c) covering the cladding, and a slant-type FBG (11) formed in the core in a removed portion (RP) where the protective coating has been removed, and coupling SRS light propagating through the core to the cladding, and at least a portion of the outer circumferential surface of the cladding in the removed portion is roughened to form a roughened portion (12).

[0008] In an optical device according to one aspect of the present invention, a slant FBG is formed in the core in the removed portion where the protective coating has been removed, and a roughened portion is formed on at least a part of the outer circumferential surface of the cladding in the removed portion. Then, the SRS light propagating through the core is reflected by the slant FBG and coupled to the cladding, and the cladding mode light including the SRS light coupled to the cladding is scattered by the roughened portion formed on the outer circumferential surface of the cladding and removed. In this way, the cladding mode light including the SRS light coupled from the core to the cladding is scattered by the roughened portion formed on the cladding and removed without using resin, which has the effect of preventing a decrease in reliability due to heat generation caused by the cladding mode light.

[0009] In the optical device according to one aspect of the present invention, the roughened portion is not in contact with the protective coating.

[0010] In an optical device according to an aspect of the present invention, the slanted FBG is a chirped FBG in which the grating period changes so that the reflection position of light differs depending on the wavelength of the light.

[0011] Moreover, an optical device according to one embodiment of the present invention further comprises a housing (20) having a storage section (21) that stores at least the removed portion, and a resin (30) that fixes the portion having the protective coating on both sides of the removed portion stored in the storage section to the housing, and the surface of the housing facing the removed portion is a light absorbing section (22) that absorbs at least the SRS light.

[0012] A laser device (40) according to one aspect of the present invention includes an excitation light source (41a, 41b) that emits excitation light, a resonator (43) that generates signal light, which is laser light, using the excitation light emitted from the excitation light source, and any of the optical devices described above (1) that are arranged between the resonator and an output end of the signal light. Effect of the Invention

[0013] According to the present invention, it is possible to prevent a decrease in reliability due to heat generation caused by cladding mode light. [Brief description of the drawings]

[0014] [Figure 1] 1 is a cross-sectional view showing a configuration of a main part of an optical device according to a first embodiment of the present invention. [Diagram 2] 1 is a cross-sectional view of an optical fiber included in an optical device according to a first embodiment of the present invention. [Diagram 3] 1 is a diagram showing a configuration of a main part of a laser device according to a first embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an optical device and a laser apparatus according to an embodiment of the present invention will be described in detail with reference to the drawings. Note that the drawings used in the following description may show characteristic parts in an enlarged scale for the sake of convenience in order to make the characteristics easier to understand, and the dimensional ratios of each component may not necessarily be the same as in reality. Furthermore, the present invention is not limited to the following embodiments.

[0016] [First embodiment] Optical Devices Fig. 1 is a cross-sectional view showing a main configuration of an optical device according to a first embodiment of the present invention. As shown in Fig. 1, the optical device 1 of this embodiment includes an optical fiber 10, a housing 20, and a fiber fixing resin 30 (resin), and removes cladding mode light (including SRS light) propagating through the optical fiber 10. Such an optical device 1 is also called a cladding mode stripper. In the following, the longitudinal direction of the optical fiber 10 (left-right direction on the paper) is referred to as the "X direction", the right side on the paper is referred to as the "+X side", and the left side on the paper is referred to as the "-X side".

[0017] Fig. 2 is a cross-sectional view of an optical fiber included in the optical device according to the first embodiment of the present invention. As shown in Fig. 2, the optical fiber 10 includes a core 10a in which a slant FBG 11 is formed, a clad 10b, and a protective coating 10c. That is, the optical fiber 10 is a single-clad fiber having a core 10a in which a slant FBG 11 is formed. Note that the clad 10b of the optical fiber 10 may be formed of two clads or three clads. That is, the optical fiber 10 may be a double-clad fiber or a triple-clad fiber having a core 10a in which a slant FBG 11 is formed.

[0018] The core 10a of the optical fiber 10 is a long member formed in a cylindrical shape, and propagates light of a predetermined wavelength (hereinafter, referred to as signal light) along the longitudinal direction of the optical fiber 10. For example, silica glass or the like can be used for this core 10a. The cladding 10b covers the core 10a and has a lower refractive index than the core 10a. For example, silica glass or the like can be used for this cladding 10b, just like the core 10a. The protective coating 10c covers the cladding 10b and protects the optical fiber 10 from external forces such as lateral pressure. For example, a resin material such as an acrylic resin or a silicone resin can be used for the protective coating 10c. These resin materials used for the protective coating 10c generally absorb light and generate heat.

[0019] The slant FBG 11 is formed in the core 10a of the optical fiber 10, and is intended to couple (mode-couple) the SRS light propagating through the core 10a to the cladding 10b. The slant FBG 11 is formed by partially irradiating the core 10a of the optical fiber 10 with a processing light beam (ultraviolet laser light or the like) and modulating the refractive index of the core 10a in the longitudinal direction. In this embodiment, in order to form the slant FBG 11, the protective coating 10c is partially removed, and the processing light beam is irradiated onto the core 10a through the portion (removed portion RP) from which the protective coating 10c has been removed. Therefore, the slant FBG 11 is formed in the core 10a at the removed portion RP from which the protective coating 10c has been removed.

[0020] The slant FBG 11 is configured to transmit light in the wavelength band of the signal light (e.g., 1070 nm) and to allow light in the wavelength band of the SRS light (e.g., 1125 nm) to escape from the core 10a to the cladding 10b. Here, the slant FBG 11 transmits most of the signal light propagating through the core 10a, but reflects a portion of the signal light. The signal light reflected by the slant FBG 11 is coupled to the cladding 10b.

[0021] In the slant FBG 11, it is desirable that the intervals between the refractive index modulation parts in the longitudinal direction are not uniform. For example, it is desirable that the slant FBG 11 is a chirp FBG in which the grating period changes so that the reflection position of the light propagating through the core 10a varies depending on the wavelength of the light. This increases the wavelength band of the light removed from the core 10a by the slant FBG 11. This makes it possible to more reliably allow the SRS light to escape toward the cladding 10b. In this way, by selectively removing the SRS light from the core 10a and coupling it to the cladding 10b, it is possible to stabilize the quality of the signal light and prevent problems caused by the SRS light propagating through the core 10a.

[0022] At least a part of the outer circumferential surface of the cladding 10b in the removed portion RP from which the protective coating 10c has been removed is formed with a roughened surface 12, which is obtained by roughening the outer circumferential surface of the cladding 10b. This roughened surface 12 is for scattering cladding mode light, including SRS light, which is coupled from the core 10a of the optical fiber 10 to the cladding 10b, and removing it from the cladding 10b. In other words, the roughened surface 12 is a portion that functions as a so-called cladding mode stripper. The cladding mode light is scattered by the roughened surface 12, so that the energy density of the cladding mode light is reduced, and therefore heat generation caused by the cladding mode light (for example, heat generation caused by irradiation of the protective coating 10c with the cladding mode light) can be suppressed.

[0023] The roughened portion 12 is formed over the entire outer circumferential surface of the cladding 10b in the removed portion RP, except for a region R1 in the vicinity of the protective coating 10c, as shown in FIG. 2. Here, the region R1 in the vicinity of the protective coating 10c is, for example, a region from the end E1 of the protective coating 10c to a position at least about 5 mm away on the +X side, and a region from the end E2 of the protective coating 10c to a position at least about 5 mm away on the -X side. That is, the roughened portion 12 is not in contact with the protective coating 10c. This is because, by keeping the roughened portion 12 away from the protective coating 10c, the cladding mode light scattered by the roughened portion 12 is prevented from entering the protective coating 10c and generating heat in the protective coating 10c.

[0024] The roughened portion 12 may be formed in the whole or part of a region R21, which is a region on the -X side from the center position P0 of the slant FBG 11 in the removed portion RP, excluding the region R1 in the vicinity of the protective coating 10c. The roughened portion 12 may be formed in the whole or part of a region R22, which is a region on the +X side from the center position P0 of the slant FBG 11 in the removed portion RP, excluding the region R1 in the vicinity of the protective coating 10c. Alternatively, the roughened portion 12 may be formed in the above-mentioned regions R21 and R22 so as to sandwich the slant FBG 11 in the longitudinal direction of the optical fiber 10.

[0025] When the roughened portion 12 is formed in the region R21, it is possible to remove cladding mode light including SRS light reflected by the slant FBG 11 by propagating through the core 10a of the optical fiber 10 from the -X side to the +X side. When the roughened portion 12 is formed in the region R22, it is possible to remove cladding mode light including SRS light reflected by the slant FBG 11 by propagating through the core 10a of the optical fiber 10 from the +X side to the -X side.

[0026] The surface roughness of the roughened portion 12 (the surface roughness of the outer peripheral surface of the cladding 10b) is set, for example, taking into consideration the reflection angle of the slant FBG 11, the energy density of the cladding mode light, etc. The surface roughness of the roughened portion 12 may be uniform or may vary depending on the location. For example, the surface roughness of the roughened portion 12 may increase with increasing distance from the center position P0 of the slant FBG 11. In such a configuration, the surface roughness of the roughened portion 12 may increase stepwise or gradually. With such a configuration, the heat generation in the longitudinal direction of the optical fiber 10 can be made closer to uniform.

[0027] The surface roughness of the roughened portion 12 may be different depending on whether or not the portion is prone to heat generation. For example, when the slant FBG 11 is a chirped FBG, the reflected wavelength differs depending on the position of the slant FBG 11 in the longitudinal direction of the optical fiber 10. For this reason, for example, the portion where the central wavelength of the SRS light is reflected is prone to heat generation, and the portion where a wavelength shifted from the central wavelength of the SRS light is reflected is unlikely to heat generation. In such a situation, for example, the surface roughness of the roughened portion 12 in the portion where heat generation is likely to occur may be made small, and the surface roughness of the roughened portion 12 in the portion where heat generation is unlikely to occur may be made large. In this way, heat generation in the longitudinal direction of the optical fiber 10 can be made closer to uniform.

[0028] The roughened portion 12 is formed, for example, by etching the outer peripheral surface of the cladding 10b or by laser processing using a pulsed laser. The method for etching the outer peripheral surface of the cladding 10b may be chemical etching using an etching solution or physical etching by sandblasting. When the optical fiber 10 is a double-clad fiber or a triple-clad fiber, the roughened portion 12 is formed on the outer peripheral surface of the cladding located at the outermost layer.

[0029] The removed portion RP from which the protective coating 10c has been removed is not recoated with resin, so that the outer peripheral surface of the cladding 10b (including the portion where the roughened portion 12 is formed and the portion where the roughened portion 12 is not formed) is exposed to the outside in the removed portion RP from which the protective coating 10c has been removed.

[0030] The housing 20 includes a housing section 21 that houses at least a portion (removed portion RP) of the optical fiber 10 from which the protective coating 10c has been removed. The housing 20 is provided to reinforce the optical fiber 10 from which the protective coating 10c has been removed, to prevent heat generation due to adhesion of foreign matter (e.g., dust, dirt, etc.) to the cladding 10b, and to absorb cladding mode light removed from the optical fiber 10.

[0031] That is, the strength of the removed portion RP of the optical fiber 10 is reduced because the protective coating 10c has been removed. By accommodating the removed portion RP of the optical fiber 10, which has such reduced strength, in the accommodating portion 21 of the housing 20, the optical fiber 10 from which the protective coating 10c has been removed is reinforced.

[0032] Furthermore, if a foreign object adheres to the roughened portion 12 formed on the outer peripheral surface of the cladding 10b, the cladding mode light scattered by the roughened portion 12 is absorbed by the foreign object, generating heat. By accommodating the removed portion RP of the optical fiber 10 in the accommodating portion 21 of the housing 20, heat generation due to the adhesion of the foreign object to the cladding 10b is prevented.

[0033] Furthermore, if the cladding mode light removed from the optical fiber 10 is emitted outside the optical device 1, the light may be incident on members other than the optical device 1, possibly causing unintended heat generation. The removed portion RP of the optical fiber 10 is accommodated in the accommodation portion 21 of the housing 20, and the cladding mode light scattered by the roughened portion 12 is absorbed by the housing 20, thereby preventing the cladding mode light from being emitted outside the optical device 1.

[0034] The housing 20 is, for example, a member having a rectangular or cylindrical shape, and is arranged so as to surround the periphery of the removed portion RP of the optical fiber 10 housed in the housing portion 21. The inner surface of the housing 20 (the surface facing the removed portion RP of the optical fiber 10) is made to be a light absorbing portion 22. Specifically, the inner surface of the housing 20 is formed of a metal such as aluminum that has been black anodized, Raydent (registered trademark), or low-temperature black-plated. The reason that the inner surface of the housing 20 is black anodized or the like is to absorb cladding mode light, including SRS light, that is incident on the inner surface while preventing its reflection. Note that, as a material for the housing 20, for example, a metal having an emissivity (a measure representing the efficiency of radiation of an object) of 0.7 or more can be used.

[0035] The housing 20 may be formed from a plurality of (e.g., two) members so that the removed portion RP of the optical fiber 10 can be easily accommodated in the accommodation portion 21. For example, the housing 20 may be formed from a first housing having a rectangular cylindrical shape with one side open, and a second housing having a flat plate shape covering the open side of the first housing. Even when the housing 20 is made of a plurality of members, the surface (inner surface) facing the removed portion RP of the optical fiber 10 accommodated therein needs to be the light absorbing portion 22.

[0036] The fiber fixing resin 30 is for fixing the optical fiber 10, whose removed portion RP is accommodated in the accommodation portion 21 of the housing 20, to the housing 20. The fiber fixing resin 30 is filled into both ends (the end on the -X side and the end on the +X side) of the housing 20, and fixes the portion having the protective coating 10c on both sides of the removed portion RP accommodated in the accommodation portion 21 of the housing 20 to the housing 20. For example, a silicone resin can be used as the fiber fixing resin 30. The silicone resin constituting the fiber fixing resin 30 may or may not be optically transparent.

[0037] Now, consider a case where signal light including SRS light propagates from the -X side to the +X side through the core 10a of the optical fiber 10. When the signal light including SRS light propagating through the core 10a of the optical fiber 10 is incident on the slant FBG 11, most of the signal light passes through the slant FBG 11, while a part of the signal light and the SRS light are reflected by the slant FBG 11 and coupled to the cladding 10b to become cladding mode light.

[0038] If the roughened portion 12b is not formed on the outer peripheral surface of the cladding 10b, this cladding mode light will travel within the cladding 10b from the +X side to the -X side while being reflected by the outer peripheral surface of the cladding 10b. However, in this embodiment, since the roughened portion 12b is formed on the outer peripheral surface of the cladding 10b, when the cladding mode light is incident on the outer peripheral surface of the cladding 10b, it is scattered by the roughened portion 12 formed on the outer peripheral surface of the cladding 10b and is removed from the optical fiber 10.

[0039] Most of the cladding mode light removed from the optical fiber 10 is absorbed by the housing 20. This makes it possible to suppress heat generation caused by the cladding mode light being irradiated onto the protective coating 10c of the optical fiber 10 and the fiber fixing resin 30. In this way, it is possible to prevent a decrease in reliability due to heat generation caused by the cladding mode light.

[0040] Here, the description has been given of a case where the signal light including SRS light propagates from the -X side to the +X side of the core 10a of the optical fiber 10. Similarly, when the signal light including SRS light propagates from the +X side to the -X side of the core 10a of the optical fiber 10, the cladding mode light can be removed without heat generation in the protective coating 10c of the optical fiber 10 or the fiber fixing resin 30.

[0041] Laser Device Fig. 3 is a diagram showing a configuration of a main part of a laser device according to a first embodiment of the present invention. As shown in Fig. 3, a laser device 40 of this embodiment includes a pumping light source 41a, a pumping light source 41b, a first combiner 42a, a second combiner 42b, a resonator 43, an optical device 1, and an output end 44. Such a laser device 40 is a bidirectional pumping type fiber laser device including the pumping light source 41a and the pumping light source 41b.

[0042] In the following description, the pumping light source 41a side may be referred to as the "front" and the pumping light source 41b side may be referred to as the "rear" when viewed from the amplification fiber 43a of the resonator 43. In addition, in Fig. 3, the fusion spliced ​​parts of the various fibers are indicated by crosses. In reality, the fusion spliced ​​parts are disposed inside a reinforcing part (not shown) for protection. The reinforcing part includes, for example, a fiber housing body having a groove capable of housing an optical fiber, and a resin for fixing the various fibers to the fiber housing body with the fusion spliced ​​parts housed in the groove of the fiber housing body.

[0043] 3, a plurality of pumping light sources 41a and a plurality of pumping light sources 41b are arranged on either side of the resonator 43. The pumping light source 41a emits pumping light (forward pumping light) toward the resonator 43, and the pumping light source 41b emits pumping light (backward pumping light) toward the resonator 43. For example, laser diodes can be used as the pumping light source 41a and the pumping light source 41b.

[0044] The first combiner 42a and the second combiner 42b are disposed on either side of the resonator 43. The first combiner 42a couples the excitation light emitted by each of the excitation light sources 41a into one optical fiber and directs the excitation light toward the resonator 43. The second combiner 42b couples the excitation light emitted by each of the excitation light sources 41b into one optical fiber and directs the excitation light toward the resonator 43.

[0045] The resonator 43 includes an amplification fiber 43a, a high reflectivity-fiber Bragg grating (HR-FBG) 43b, and an output coupler-fiber Bragg grating (OC-FBG) 43c. The resonator 43 generates signal light, which is a laser light, by pumping light emitted from the pumping light source 41a and the pumping light source 41b.

[0046] The amplification fiber 43a has a core doped with one or more types of active elements, a first cladding covering the core, a second cladding covering the first cladding, and a protective coating covering the second cladding. In other words, the amplification fiber 43a is a double-clad fiber. As the active element doped in the core, for example, a rare earth element such as erbium (Er), ytterbium (Yb), or neodymium (Nd) is used. These active elements emit light in an excited state. Silica glass or the like can be used for the core and the first cladding. A resin such as a polymer can be used for the second cladding. A resin material such as an acrylic resin or a silicone resin can be used for the protective coating.

[0047] The HR-FBG 43b is formed in the core of an optical fiber fusion-spliced ​​to the front end of the amplification fiber 43a. The HR-FBG 43b is adjusted to reflect light of the signal light wavelength emitted by the active element of the amplification fiber 43a in an excited state with a reflectance of almost 100%. The HR-FBG 43b has a structure in which high refractive index portions are repeated at a constant interval along its longitudinal direction.

[0048] The OC-FBG 43c is formed in the core of an optical fiber fused to the rear end of the amplification fiber 43a. The OC-FBG 43c has a structure similar to that of the HR-FBG 43b, but is adjusted to reflect light with a lower reflectance than the HR-FBG 43b. For example, the OC-FBG 43c is adjusted to have a reflectance of about 10 to 20% for light of the signal light wavelength.

[0049] In the amplification fiber 43a, the signal light reflected by the HR-FBG 43b and the OC-FBG 43c travels back and forth in the longitudinal direction of the amplification fiber 43a. The signal light is amplified as it travels back and forth, becoming laser light. In this way, light is amplified in the resonator 43 to generate laser light. A part of the laser light passes through the OC-FBG 43c, passes through the optical device 1, reaches the output end 44, and is output to the outside.

[0050] Here, even if SRS light is contained in the laser light (signal light) generated in the amplification fiber 43a and transmitted through the OC-FBG 43c, the SRS light is removed by the optical device 1 when the signal light containing the SRS light passes through the optical device 1. For this reason, signal light of stable quality is output from the output end 44 of the laser device 40. Note that SRS light may also be generated due to return light of the signal light output from the laser device 40 (light input from the output end 44 and traveling toward the resonator 43). Such SRS light is also removed by the optical device 1 when the return light passes through the optical device 1.

[0051] As described above, in this embodiment, the slant FBG 11 is formed in the core 10a in the removed portion RP where the protective coating 10c has been removed, and the roughened portion 12 is formed on at least a part of the outer circumferential surface of the cladding 10b in the removed portion RP. Then, the SRS light propagating through the core 10a is reflected by the slant FBG 11 and coupled to the cladding 10b, and the cladding mode light including the SRS light coupled to the cladding 10b is scattered by the roughened portion 12 formed on the outer circumferential surface of the cladding 10b and removed.

[0052] In this manner, in this embodiment, the cladding mode light including the SRS light coupled from the core to the cladding is scattered and removed by the roughened surface 12 formed on the cladding 10b without using resin. This makes it possible to prevent a decrease in reliability due to heat generation caused by the cladding mode light. In addition, in this embodiment, the slant type FBG 11 and the roughened surface 12 functioning as a so-called cladding mode stripper are formed on the device 1, so that the number of parts can be reduced compared to a configuration in which these are provided separately.

[0053] Second Embodiment Next, a laser device according to a second embodiment of the present invention will be described. The laser device of this embodiment has a different pumping method for the amplification fiber 43a. The laser device 40 according to the first embodiment described above is a bidirectional pumping type laser device that includes a pumping light source 41a and a pumping light source 41b, and performs pumping using the pumping light output from the pumping light source 41a and the pumping light output from the pumping light source 41b.

[0054] In contrast, the laser device of this embodiment is a one-side pumping type laser device that includes either the pumping light source 41a or the pumping light source 41b and performs pumping using either the pumping light output from the pumping light source 41a or the pumping light output from the pumping light source 41b. Specifically, the pumping light source 41b and the second combiner 42b shown in Fig. 3 are omitted, and the laser device is a forward pumping type laser device that performs pumping using the pumping light output from the pumping light source 41a. Alternatively, the laser device is a backward pumping type laser device that does not include the pumping light source 41a and the first combiner 42a shown in Fig. 3 and performs pumping using the pumping light output from the pumping light source 41b.

[0055] The laser device of this embodiment differs from the laser device 40 of the first embodiment only in the excitation method, and like the laser device 40 of the first embodiment, includes an optical device 1 disposed between a resonator 43 and an output end 44. Therefore, like the laser device 40 of the first embodiment, the laser device of this embodiment can prevent a decrease in reliability due to heat generation caused by cladding mode light, and can reduce the number of parts.

[0056] Third Embodiment Next, a laser device according to a third embodiment of the present invention will be described. The laser device of this embodiment differs in the method of supplying pumping light to the amplification fiber 43a. In the laser device 40 according to the first embodiment described above, the pumping light output from the pumping light source 41a is supplied by the first combiner 42a, and the pumping light output from the pumping light source 41b is supplied by the second combiner 42b.

[0057] In contrast, the laser device of this embodiment supplies pumping light by side pumping. Here, side pumping refers to a method in which the clad of a supplying fiber to which pumping light is supplied and the clad of a receiving fiber to which the pumping light is to be supplied are partially brought into contact with each other or partially fusion spliced, and the pumping light supplied to the supplying fiber is supplied to the receiving fiber via the contact portion.

[0058] Specifically, the laser device of this embodiment does not include the first combiner 42a and the second combiner 42b shown in Fig. 3. Then, the pumping light output from the pumping light source 41a is supplied by a side pump between, for example, the HR-FBG 43b and the fusion splice located behind the HR-FBG 43b. The pumping light output from the pumping light source 41b is supplied by a side pump between, for example, the OC-FBG 43c and the fusion splice located in front of the OC-FBG 43c.

[0059] The laser device of this embodiment differs from the laser device 40 of the first embodiment only in the method of supplying pumping light to the amplification fiber 43a, and like the laser device 40 of the first embodiment, includes an optical device 1 disposed between a resonator 43 and an output end 44. Therefore, like the laser device 40 of the first embodiment, the laser device of this embodiment can prevent a decrease in reliability due to heat generation caused by cladding mode light, and can reduce the number of parts.

[0060] Although the embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and can be freely modified within the scope of the present invention. For example, the laser device of the above embodiment has one output end 44, but an optical fiber or the like may be further connected to the end of the output end 44. Also, a beam combiner may be connected to the end of the output end 44 to bundle laser light from a plurality of laser devices.

[0061] The optical device 1 may be used in a MOPA (Master Oscillator Power Amplifier) ​​type laser device. The optical device 1 may also be applied to a laser device in which the resonator is configured by something other than an optical fiber, such as a semiconductor laser (DDL: Direct Diode Laser) or a disk laser, and the laser light emitted from the resonator is focused on an optical fiber. [Explanation of symbols]

[0062] 1...optical device, 10a...core, 10b...cladding, 10c...protective coating, 11...slant-type FBG, 12...roughened portion, 20...housing, 21...accommodation portion, 22...light absorbing portion, 30...fiber fixing resin, 40...laser device, 41a, 41b...excitation light source, 43...resonator, 44...output end, RP...removed portion

Claims

1. A core, a cladding covering the core and having a lower refractive index than the core; a protective coating covering the cladding; a slant FBG formed in the core at a portion where the protective coating is removed, the FBG coupling an SRS light propagating through the core to the cladding; Equipped with At least a part of the outer circumferential surface of the cladding in the removed portion is a roughened portion, the roughened portion is formed to cover the slant-type FBG; Optical devices.

2. The optical device of claim 1 , wherein the roughened portion is not in contact with the protective coating.

3. 3. The optical device according to claim 1, wherein the slant FBG is a chirped FBG in which a grating period changes so that a reflection position of light differs depending on a wavelength of the light.

4. A housing having a housing portion that houses at least the removed portion; a resin that fixes the portion having the protective coating on both sides of the removed portion accommodated in the accommodation portion to the housing; Further comprising: A surface of the housing facing the removed portion is a light absorbing portion that absorbs at least the SRS light. An optical device according to any one of claims 1 to 3.

5. an excitation light source that emits excitation light; a resonator for generating signal light, which is a laser beam, using the excitation light emitted from the excitation light source; an optical device according to any one of claims 1 to 4, which is disposed between the resonator and an output end of the signal light; A laser device comprising:

Citation Information

Patent Citations

  • A manufacture method of a stimulated Raman scattering filter in a kilowatt-level fiber laser

    CN109149329A

  • Optical fiber

    JP1982089706A

  • Waveguide type optical filter

    JP1997304622A

  • Optical loss filter

    JP2002131550A

  • Slant type short period optical fiber grating, optical amplifier module and optical communication system