Semiconductor manufacturing apparatus, semiconductor device, and method for manufacturing the semiconductor device
The semiconductor manufacturing apparatus addresses the challenge of forming impurity diffusion layers with reduced defects and increased throughput by separating and alternating the implantation of ionic and neutral components, resulting in improved efficiency and reduced leakage current.
Patent Information
- Application Number
- JP2021138315
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-08-26
- Publication Date
- 2024-11-07
- Estimated Expiration
- 2041-08-26
AI Technical Summary
Existing semiconductor manufacturing processes face challenges in forming impurity diffusion layers with few crystal defects and low throughput due to the need for multiple ion implantation steps under different conditions, which can lead to increased leakage current and decreased efficiency.
A semiconductor manufacturing apparatus that separates impurity beams into ionic and neutral components, allowing for alternating modes of implantation using a control unit to introduce these components at different depths and angles on the substrate, forming multiple impurity layers with controlled concentrations and reduced defects.
The apparatus enables the formation of impurity diffusion layers with fewer crystal defects and improved throughput by simultaneously implanting ion and neutral components, reducing leakage current and production costs while enhancing the accuracy of concentration profiles.
Smart Images

Figure 0007579221000001 
Figure 0007579221000002 
Figure 0007579221000003
Abstract
Description
[Technical field]
[0001] The present embodiment relates to a semiconductor manufacturing apparatus, a semiconductor device, and a method for manufacturing a semiconductor device. [Background technology]
[0002] As semiconductor devices become finer, there is a demand for highly accurate control of impurity diffusion layers. For example, if the source or drain layer of a transistor is made of a single impurity diffusion layer, crystal defects are likely to remain in the impurity diffusion layer, increasing leakage current. If the source or drain layer is made of multiple impurity diffusion layers, it is necessary to repeatedly perform multiple ion implantation processes under different conditions. This leads to a decrease in throughput. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2014-049620 A [Patent Document 2] JP 2003-115277 A [Patent Document 3] Patent No. 3356629 (U.S. Patent No. 6071781) [Patent Document 4] Patent No. 4901094 (U.S. Patent No. 7351987) Summary of the Invention [Problem to be solved by the invention]
[0004] Provided are a semiconductor manufacturing apparatus, a semiconductor device, and a method for manufacturing a semiconductor device, which are capable of forming an impurity diffusion layer with few crystal defects in a short process. [Means for solving the problem]
[0005] The semiconductor manufacturing apparatus according to the present embodiment includes a stage on which a substrate can be mounted. The separation unit separates an impurity beam to be introduced into the substrate into ion components and neutral components. The control unit switches between a first mode in which the ion components are introduced into the substrate and a second mode in which the neutral components are introduced into the substrate. [Brief description of the drawings]
[0006] [Figure 1] 1 is a schematic diagram showing an example of the configuration of an ion implantation apparatus according to an embodiment of the present invention; [Figure 2A] 4 is a graph showing an example of a power supply voltage in the ion implantation method according to the present embodiment. [Figure 2B] 4 is a graph showing an example of a power supply voltage in the ion implantation method according to the present embodiment. [Figure 2C] 4 is a graph showing an example of a power supply voltage in the ion implantation method according to the present embodiment. [Diagram 3] FIG. 4 is a conceptual diagram showing ion components and neutral components in an energy filter. [Figure 4] A conceptual diagram showing the operation of a stage. [Diagram 5] 4 is a graph showing an example of acceleration energies of ion components and neutral components. [Figure 6] 6 is a graph showing the impurity concentration and depth of the diffusion layer formed in the first and second modes. [Figure 7] FIG. 2 is a cross-sectional view showing a configuration example of a transistor according to the present embodiment. [Figure 8] 4 is a graph showing the concentrations of boron, interstitial silicon, and vacancies generated in a semiconductor substrate W by implantation of ion components in a first mode. [Figure 9] 2 is a graph showing boron, interstitial silicon and vacancy concentrations induced in a semiconductor substrate by implantation of a first mode ionic component and a second mode neutral component; [Figure 10] 6 is a graph showing the boron concentrations in a semiconductor substrate after annealing processes performed in the first and second modes. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The present invention is not limited to this embodiment. The drawings are schematic or conceptual, and the ratio of each part is not necessarily the same as the actual one. In the specification and drawings, elements similar to those described above with respect to the previous drawings are given the same reference numerals, and detailed descriptions are omitted as appropriate.
[0008] 1 is a schematic diagram showing an example of the configuration of an ion implantation apparatus 1 according to the present embodiment. The ion implantation apparatus 1 includes a chamber 3, a stage 5, an ion source 10, an analyzer 20, a Q lens 30, a scanner 40, a parallel lens 50, an acceleration / deceleration electrode 60, and an energy filter 70. The ion implantation apparatus 1 is an apparatus for doping impurities into a semiconductor substrate W, and implants, for example, boron (B), phosphorus (P), arsenic (As), or the like as the impurity. In the present embodiment, the ion implantation apparatus 1 will be described as implanting boron into the semiconductor substrate W as an example.
[0009] The chamber 3 houses the stage 5, the ion source 10, the analyzer 20, the Q lens 30, the scanner 40, the parallel lens 50, the acceleration / deceleration electrode 60, and the energy filter 70. The chamber 3 is connected to a vacuum pump (not shown) and is configured to be able to reduce the pressure inside the chamber 3. The chamber 3 has a transfer port for the semiconductor substrate W, and the semiconductor substrate W is transferred into the chamber 3 through the transfer port and mounted on the stage 5. Alternatively, the semiconductor substrate W is transferred out of the chamber 3 through the transfer port.
[0010] The stage 5 is capable of mounting a semiconductor substrate W. The stage 5 is configured to be capable of moving the position of the semiconductor substrate W or changing the inclination angle of the semiconductor substrate W with respect to the ion beam 12. Driving units 80 and 90 are connected to the stage 5. The driving unit 80 is configured to be capable of moving the stage 5 in a direction substantially parallel to the mounting surface of the stage 5. The driving unit 90 is configured to be capable of tilting the mounting surface of the stage 5 with respect to the incidence angle of the ion beam 12. This allows the stage 5 to move the semiconductor substrate W within the chamber 3 and adjust the angle with respect to the ion beam 12.
[0011] The ion source 10 is, for example, a source of generating ions of the impurity BF3.
[0012] The aperture 15 is an opening that shapes the impurity beam from the ion source 10 .
[0013] The analyzer 20 removes unnecessary ions contained in the impurity beam and extracts the desired ion beam 12. For example, in order to extract the ion beam 12 of B+ ions from the impurity beam (B+, F+, BF+, BF2+) generated from a BF3 ion source, the analyzer 20 removes the other F+, BF+, and BF2+ ions.
[0014] The Q lens 30 is an electromagnetic lens that electromagnetically shapes the desired ion beam (eg, B+ ions) 12 extracted by the analyzer 20.
[0015] The scanner 40 controls the direction of the ion beam 12 to scan the B+ ions onto the semiconductor substrate W.
[0016] The parallelizing lens 50 is an electromagnetic lens that contracts or diverges the ion beam 12 .
[0017] The acceleration / deceleration electrodes 60 accelerate or decelerate the velocity of the ion beam 12 .
[0018] The ion beam 12 that passes through such beamlines (15, 20, 30, 40, 50, 60) may be neutralized by gas remaining in the chamber 3. Therefore, the ion beam 12 includes not only an ion beam (ion components) but also a neutralized neutral beam (neutral components). Hereinafter, the components of the ion beam 12 that are maintained as ions are referred to as ion components, and the components that are neutralized ions are also referred to as neutral components.
[0019] The energy filter 70 separates the ion components from the neutral components by controlling the ion components of the ion beam 12. At this time, the energy filter 70 applies acceleration or deceleration energy to the ion components to make the injection energy of the ion components different from that of the neutral components. This allows the energy filter 70 to introduce the ion components and the neutral components separately into the semiconductor substrate W. Moreover, the energy filter 70 can introduce the ion components to a first depth into the semiconductor substrate W with a certain energy, and introduce the neutral components to a second depth into the semiconductor substrate W with another energy. For example, the energy filter 70 can decelerate boron ions (B+) and inject them into the semiconductor substrate W with a relatively low energy, and inject the neutralized boron (B) directly into the semiconductor substrate W with a relatively high energy. This allows the semiconductor substrate W to have a boron diffusion layer that is introduced to a deep position and a boron diffusion layer that is introduced only to a relatively shallow position. That is, a plurality of impurity layers having different depths can be formed in the semiconductor substrate W. At this time, by changing the position and inclination of the semiconductor substrate W by the stage 5, the deep boron diffusion layer and the shallow boron diffusion layer can be formed at the same position in a plan view seen from above the surface of the semiconductor substrate W.
[0020] The control unit 100 controls each component of the ion implantation apparatus 1 and the power supplies 110 to 130. The power supply 110 supplies power to the energy filter 70 to control the ion components from the ion beam 12. The power supply 120 supplies power to the drive unit 80, enabling the movement of the stage 5. The power supply 130 supplies power to the drive unit 90, enabling the change of the tilt angle of the stage 5. The control unit 100 controls the operation of the other components of the ion implantation apparatus 1.
[0021] Next, an ion implantation method using the ion implantation apparatus 1 will be described.
[0022] 2A to 2C are graphs showing an example of the voltages of the power supplies 110 to 130 in the ion implantation method according to the present embodiment. The vertical axis indicates the power supply voltage of each of the power supplies 110 to 130. The horizontal axis indicates time t. Fig. 3 is a conceptual diagram showing ion components 12I and neutral components 12N in the energy filter 70. Fig. 4 is a conceptual diagram showing the operation of the stage 5.
[0023] First, an ion source 10 in Fig. 1 generates ions of, for example, an impurity BF3 to generate an impurity beam. An aperture 15 shapes and accelerates the impurity beam. An analyzer 20 removes unwanted ions (for example, F+, BF+, BF2+) contained in the impurity beam and extracts a desired ion beam 12 (for example, B+).
[0024] A Q lens 30 then electromagnetically shapes the ion beam 12, and a scanner 40 controls the direction of the ion beam.
[0025] Next, the parallel lens 50 contracts or disperses the ion beam 12 , and the acceleration / deceleration electrodes 60 accelerate or decelerate the velocity of the ion beam 12 .
[0026] The ion beam 12 that has passed through such beamlines (15, 20, 30, 40, 50, 60) may be neutralized by the gas remaining in the chamber 3. Therefore, the ion beam 12 contains not only ion components but also neutral components.
[0027] 2A, after t1, the power supply 110 applies a negative voltage to the energy filter 70. This enables the energy filter 70 to extract ion components from the ion beam 12 and separate them from neutral components.
[0028] 3, the traveling direction of boron ions (B+) as ion components is bent by the electric field from the energy filter 70. On the other hand, the traveling direction of boron particles (B) as neutral components is hardly changed by the electric field from the energy filter 70. In this way, the energy filter 70 separates the ion components 12I and the neutral components 12N.
[0029] Here, as shown in FIG. 2B, in a period t1 to t2, the power supply 120 applies a positive voltage to the driving unit 80, and as shown in FIG. 2C, the power supply 130 applies a positive voltage to the driving unit 90. As a result, as shown in FIG. 4, the driving unit 80 moves the stage 5 in the -Z direction so as to irradiate the semiconductor substrate W with the ion component 12I, and places the semiconductor substrate W at a position Zi. In addition, the driving unit 90 tilts the stage 5 by an angle θ to introduce the ion component 12I from a direction tilted by the angle θ from a direction perpendicular to the surface of the semiconductor substrate W. The angle θ is the tilt angle of the stage 5 based on a plane that is approximately perpendicular to the traveling direction of the ion component 12I.
[0030] At this time, the scanner 40 controls the direction of the ion beam 12 to scan the beam of the ion component 12I and the neutral component 12N over the entire semiconductor substrate W. The process of implanting the ion component 12I into the semiconductor substrate W at the position Zi is referred to as a first mode here.
[0031] Next, as shown in FIG. 2B, in a period t3 to t4, the power supply 120 stops supplying the positive voltage, and as shown in FIG. 2C, the power supply 130 stops supplying the positive voltage. As a result, as shown in FIG. 4, the driving unit 80 moves the stage 5 in the +Z direction to return it to its original position, places the semiconductor substrate W at the position Zn, and irradiates the neutral component 12N onto the semiconductor substrate W. The driving unit 90 also returns the inclination of the stage 5 to its original position so that the neutral component 12N is incident on the surface of the semiconductor substrate W from a direction approximately perpendicular to the surface of the semiconductor substrate W. The driving unit 90 inclines the stage 5 so that the neutral component 12N is incident on the surface of the semiconductor substrate W from a direction approximately perpendicular to the surface of the semiconductor substrate W. The driving unit 90 may incline the stage 5 by an angle φ (not shown) different from the angle θ, and introduce the neutral component 12N from a direction inclined by the angle φ from the direction perpendicular to the surface of the semiconductor substrate W. The angle φ is the inclination angle of the stage 5 based on a plane approximately perpendicular to the traveling direction of the neutral component 12N. The process of implanting the neutral component 12N into the semiconductor substrate W at the position Zn is referred to here as the second mode.
[0032] At this time, the scanner 40 controls the direction of the ion beam 12, so that the beam of the ion component 12I and the neutral component 12N is scanned over the entire semiconductor substrate W.
[0033] The control unit 100 switches between the first mode and the second mode between t2 and t3, between t4 and t5, and between t6 and t7. This allows the driving unit 80 to move the stage 5 between the position Zi where the ion component 12I is introduced in the first mode and the position Zn where the neutral component 12N is introduced in the second mode. The driving unit 90 can adjust the inclination of the stage 5 in the first mode and the second mode. The driving units 80 and 90 synchronously execute the movement of the stage 5 between the position Zi and the position Zn, and the adjustment of the stage between the inclination angle θ of the stage 5 at the position Zi and the inclination angle φ of the stage 5 at the position Zn.
[0034] The first and second modes are successively performed in the same chamber 3. Therefore, a plurality of impurity layers having different depths and concentrations can be formed.
[0035] During the transition period between the first mode and the second mode (for example, from t2 to t3, from t4 to t5), the ion implantation apparatus 1 may continuously irradiate the stage 5 with the ion beam 12. Alternatively, the ion implantation apparatus 1 may temporarily suspend irradiation of the ion beam 12 after the first mode ends, and resume it at the start of the second mode. Furthermore, the order of execution of the first mode and the second mode is not particularly limited, and either may be executed first.
[0036] Next, the stage 5 rotates the semiconductor substrate W, for example, by 90°, and performs the operations from t1 to t4 at t5 to t8. After that, the semiconductor substrate W is rotated by 180° and 270°, and the operations from t1 to t4 are repeatedly performed. This causes the ion components 12I and neutral components 12N to be introduced into the entire surface of the semiconductor substrate W.
[0037] Here, the acceleration energy (keV) of the ion component 12I and the neutral component 12N will be described.
[0038] 5 is a graph showing an example of the acceleration energy of the ion component 12I and the neutral component 12N. The vertical axis indicates the acceleration energy (keV), and the horizontal axis indicates the position of the ion beam 12, the ion component 12I, or the neutral component 12N.
[0039] In this embodiment, for example, about +1.0 keV is applied to the ion source 10. The ion beam 12 is extracted from the ion source 10 and accelerated at the aperture 15 at, for example, about -2.0 keV. Therefore, the acceleration energy of the ion beam 12 is the difference between the potential of the ion source 10 and the potential of the aperture 15, and is, for example, about -3.0 keV.
[0040] When the ion beam 12 passes through the beamline (20 to 60), the ion beam 12 becomes a mixture of ion components 12I and neutral components 12N due to the gas in the chamber 3, as described above.
[0041] Next, the energy filter 70 separates the ion component 12I and the neutral component 12N of the ion beam 12. At this time, the energy filter 70 receives power from the power source 110 to apply an electric field to the ion beam 12, changing the traveling direction of only the ion component 12I. Since the neutral component 12N is electrically neutral, it is not affected by the electric field and its traveling direction does not change.
[0042] Furthermore, the energy filter 70 makes the acceleration energies of the ion component 12I and the neutral component 12N different. For example, the energy filter 70 reduces the acceleration energy of the ion component 12I by, for example, about -2.0 keV. As a result, the acceleration energy of the ion component 12I becomes about -1.0 keV with respect to the potential of the ion source 10. On the other hand, the neutral component 12N is electrically neutral and is not affected by the electric field from the energy filter 70, and maintains, for example, an acceleration energy of about -3.0 keV.
[0043] In this way, the energy filter 70 separates the ion component 12I and the neutral component 12N of the ion beam 12 and makes their acceleration energies different from each other. As a result, the ion component 12I travels to a lower position Zi in Fig. 4 with an acceleration energy of about -1.0 keV. The neutral component 12N travels to an upper position Zn in Fig. 4 with an acceleration energy of about -3.0 keV.
[0044] (First mode) In the first mode, the stage 5 positions the semiconductor substrate W at a position Zi, and tilts the stage 5 by an angle θ. The ion component 12I is introduced from a direction tilted by an angle θ from a direction substantially perpendicular to the surface of the semiconductor substrate W. The acceleration energy of the ion component 12I is, for example, about −1 keV.
[0045] (Second mode) In the second mode, the stage 5 positions the semiconductor substrate W at a position Zn, and tilts the stage 5 by an angle φ. The neutral component 12N is introduced from a direction tilted by the angle φ from a direction substantially perpendicular to the surface of the semiconductor substrate W. In this embodiment, the angle φ is approximately 0°. Therefore, the neutral component 12N is introduced from a direction substantially perpendicular to the surface of the semiconductor substrate W. The acceleration energy of the neutral component 12N is, for example, approximately -3 keV.
[0046] FIG. 6 is a graph showing the impurity concentration and depth of the diffusion layer formed by the first and second modes. The vertical axis indicates the concentration of the impurity (e.g., boron). The horizontal axis indicates the depth from the surface of the semiconductor substrate W. In the first mode, the acceleration energy of the ion component 12I is, for example, about -1 keV. Therefore, the ion component (e.g., B+) 12I is introduced to a relatively shallow position from the surface of the semiconductor substrate W. On the other hand, in the second mode, the acceleration energy of the neutral component 12N is, for example, about -3 keV. Therefore, the neutral component 12N (e.g., B) is introduced to a relatively deep position from the surface of the semiconductor substrate W.
[0047] The concentrations of the ion component 12I and neutral component 12N in the ion beam 12 vary depending on the pressure in the chamber 3. For example, when the pressure in the chamber 3 is very low and close to a vacuum, the ion beam 12 does not collide much with other gases in the chamber 3. Since the ion beam 12 is neutralized to become the neutral component 12N by colliding with other gases, when the pressure in the chamber 3 is very low, most of the ion beam 12 remains as the ion component 12I and does not change much to the neutral component 12N. In this case, the concentration of the ion component 12I is relatively high, and the concentration of the neutral component 12N is relatively low.
[0048] On the other hand, when the pressure in the chamber 3 is relatively high, most of the ion beam 12 collides with other gases in the chamber 3. In this case, most of the ion beam 12 is neutralized to neutral components 12N. Therefore, the concentration of the neutral components 12N becomes relatively high, and the concentration of the ion components 12I becomes relatively low.
[0049] The control unit 100 may control the concentrations of the ion components 12I and the neutral components 12N by controlling the pressure in the chamber 3. This allows the ion implantation device 1 according to the present embodiment to control the concentrations of each of the impurity layers introduced in the first mode and the second mode to be desired.
[0050] As described above, the ion implantation device 1 according to the present embodiment continuously switches between the first mode in which the ion component 12I is introduced into the semiconductor substrate W and the second mode in which the neutral component 12N is introduced into the semiconductor substrate W in the same ion implantation process. The first and second modes can implant the ion component 12I and the neutral component 12N having different acceleration energies into the semiconductor substrate W under the same ion implantation conditions. The energy filter 70 separates the ion component 12I and the neutral component 12N and implants them into the semiconductor substrate W with different acceleration energies. The stage 5 moves the semiconductor substrate W and changes the inclination angle from a plane perpendicular to the traveling direction of the ion component 12I and the neutral component 12N. This allows a diffusion layer consisting of a plurality of impurity layers having different depths and concentrations to be formed in the semiconductor substrate W in a single ion implantation process.
[0051] 7 is a cross-sectional view showing an example of the configuration of a transistor Tr according to this embodiment. The transistor Tr may be, for example, a transistor of a CMOS (Complementary Metal Oxide Semiconductor) circuit used in a controller of a NAND type flash memory or the like. The transistor Tr is formed on a semiconductor substrate W.
[0052] The transistor Tr includes a semiconductor substrate W, source diffusion layers 211 and 212, drain diffusion layers 213 and 214, a gate insulating film 230, a gate electrode 240, a cap film 250, a protective film 260, a spacer 270, a liner layer 280, an interlayer insulating film 290, and a contact 295. Hereinafter, the transistor Tr will be described as a P-type MOSFET (MOS Field Effect Transistor), but may be an N-type MOSFET.
[0053] The semiconductor substrate W may be, for example, a silicon substrate. A gate electrode 240 is provided on the surface of the semiconductor substrate W via a gate insulating film 230. The gate electrode 240 is made of, for example, a conductive material such as doped polysilicon or a metal. The gate insulating film 230 is made of, for example, a silicon oxide film or a high dielectric material having a higher dielectric constant than a silicon oxide film.
[0054] The source diffusion layers 211 and 212 are provided on one side of the gate electrode 240. The source diffusion layers 211 and 212 include a plurality of impurity layers 211 and 212 having different depths. The impurity layer 211 is an impurity layer formed by an ion component 12I implanted in a first mode. The impurity layer 212 is an impurity layer formed by a neutral component 12N implanted in a second mode. Therefore, the impurity layer 212 is formed deeper than the impurity layer 211. The impurity layers 211 and 212 may be impurity layers formed by implanting boron, for example.
[0055] The impurity layer 211 is formed by injecting ion components 12I from a direction inclined to the surface of the semiconductor substrate W. On the other hand, the impurity layer 212 is formed by injecting neutral components 12N from a direction perpendicular to the surface of the semiconductor substrate W. For this reason, the impurity layer 211 extends from the impurity layer 212 toward the channel region CH below the gate electrode 240, and is provided closer to the channel region CH than the impurity layer 212.
[0056] The drain diffusion layers 213 and 214 are provided on the other side of the gate electrode 240. The drain diffusion layers 213 and 214 include a plurality of impurity layers 213 and 214 having different depths. The impurity layer 213 is an impurity layer formed simultaneously or continuously with the impurity layer 211 by the ion component 12I implanted in the first mode. The impurity layer 214 is an impurity layer formed simultaneously or continuously with the impurity layer 212 by the neutral component 12N implanted in the second mode. Therefore, the impurity layer 214 is formed deeper than the impurity layer 213. The impurity layers 213 and 214 may be impurity layers formed by implanting boron, for example.
[0057] The impurity layer 213 is formed by injecting ion components 12I from a direction inclined to the surface of the semiconductor substrate W. On the other hand, the impurity layer 214 is formed by injecting neutral components 12N from a direction perpendicular to the surface of the semiconductor substrate W. For this reason, the impurity layer 213 extends from the impurity layer 214 toward the channel region CH below the gate electrode 240, and is provided closer to the channel region CH than the impurity layer 214.
[0058] The source diffusion layers 211, 212 and the drain diffusion layers 213, 214 may further be provided with an LDD (Lightly Doped Drain) 220 on the channel region CH side. In this embodiment, the source diffusion layer and the drain diffusion layer each include two impurity layers, but may include three or more impurity layers.
[0059] A cap film 250 is provided on the gate electrode 240. The cap film 250 is used as a hard mask when processing the gate electrode 240. The cap film 250 is made of an insulating material such as a silicon nitride film.
[0060] A protective film 60 is provided so as to cover the gate electrode 240 and the cap film 250. The protective film 260 is made of an insulating material such as a silicon oxide film.
[0061] Spacers 270 are provided on both sides of the gate electrode 240 via protective films 260. The spacers 270 are made of an insulating material such as a silicon oxide film.
[0062] A liner layer 280 is provided so as to cover the spacer 270 and the protective film 260. The liner layer 280 is made of an insulating material such as a silicon nitride film. The liner layer 280 prevents harmful substances such as hydrogen from entering from the outside.
[0063] An interlayer insulating film 290 is provided on the liner layer 280. The interlayer insulating film 290 is made of an insulating material such as a silicon oxide film.
[0064] The contact 295 penetrates the interlayer insulating film 290 and the liner layer 280, etc., and is connected to the source diffusion layers 211, 212 or the drain diffusion layers 213, 214. The contact 295 is made of a low resistance metal, such as tungsten or copper.
[0065] With this configuration, the transistor Tr electrically connects or disconnects the source diffusion layers 211, 212 and the drain diffusion layers 213, 214 via the channel region CH in accordance with the potential of the gate electrode 240.
[0066] FIG. 8 is a graph showing the concentrations of boron B1, interstitial silicon Si_int1, and vacancies V1 in the semiconductor substrate W caused by the implantation of the ion component 12I in the first mode. FIG. 9 is a graph showing the concentrations of boron B1, B2, interstitial silicon Si_int1, Si_int2, and vacancies V1, V2 in the semiconductor substrate W caused by the implantation of the ion component 12I in the first mode and the neutral component 12N in the second mode. FIG. 10 is a graph showing the concentrations of boron B1, B2 in the semiconductor substrate W after the annealing process by performing the first and second modes. The vertical axis of these graphs indicates the concentration, and the horizontal axis indicates the depth Xj from the surface of the semiconductor substrate W.
[0067] As shown in FIG. 8, in the first mode, boron B1 is implanted into the semiconductor substrate W from the surface to a depth position XB1 by implanting the ion component 12I. At this time, due to the influence of the implantation of the ion component 12I, vacancy V1 and interstitial silicon Si_int1 are generated. The interstitial silicon Si_int1 is a silicon atom that has been cut off from the crystal bond when boron B1 collides with the silicon crystal of the semiconductor substrate W. The vacancy V1 is the space remaining after the silicon atom cut off from the crystal bond. The vacancy V1 is generated at a depth position XV1 from the surface of the semiconductor substrate W. The interstitial silicon Si_int1 is generated at a depth position XSi1 from the surface of the semiconductor substrate W.
[0068] Since the vacancy V1 and the interstitial silicon Si_int1 are generated when boron B1 collides with the silicon crystal, XV1 < XB1 < XSi1. Since the vacancy V1 is a crystal defect, it is preferably less. Note that the depth positions XB1, XV1, and XSi1 indicate the positions of the concentration peaks of boron B1, vacancy V1, and interstitial silicon Si_int1, respectively.
[0069] As shown in FIG. 9, in the second mode, boron B2 is implanted into the semiconductor substrate W from the surface to a depth position XB2 by implanting the neutral component 12N. At this time, due to the influence of the implantation of the neutral component 12N, vacancy V2 and interstitial silicon Si_int2 are generated. The interstitial silicon Si_int2 is a silicon atom that has been cut off from the crystal bond when boron B2 collides with the silicon crystal of the semiconductor substrate W. The vacancy V2 is the space remaining after the silicon atom cut off from the crystal bond. For example, the vacancy V2 is generated at a depth position XV2 from the surface of the semiconductor substrate W. The interstitial silicon Si_int2 is generated at a depth position XSi2 from the surface of the semiconductor substrate W.
[0070] The empty lattice V2 and the interstitial silicon Si_int2 are generated by the collision of boron B2 with the silicon crystal, so XV2 < XB2 < XSi2. Since the empty lattice V2 is a crystal defect, it is preferably less. Note that the depth positions XB2, XV2, and XSi2 indicate the positions of the concentration peaks of boron B2, the empty lattice V2, and the interstitial silicon Si_int2, respectively.
[0071] Here, the depth position XV2 of the empty lattice V2 is close to or substantially equal to the depth position XSi1 of the interstitial silicon Si_int1. As a result, after the annealing process, the interstitial silicon Si_int1 is rearranged into the empty lattice V2, and the concentrations of the empty lattice V2 and the interstitial silicon Si_int1 can be reduced. Thereby, crystal defects (EOR (End-Of-Range) defects) in the source diffusion layers 211, 212 and the drain diffusion layers 213, 214 can be reduced. Also, since the implantation energy of the neutral component 12N is high in the second mode, the interstitial silicon Si_int2 is widely scattered and its density becomes low. Thereby, crystal defects in the source diffusion layers 211, 212 and the drain diffusion layers 213, 214 can be further reduced.
[0072] After the execution of the first and second modes, an annealing process is executed. As a result, as shown in FIG. 10, the empty lattices V1, V2 and the interstitial silicons Si_int1, Si_int2 are reduced as described above, and the borons B1, B2 form the source diffusion layers 211, 212 and the drain diffusion layers 213, 214. At this time, the empty lattices V1, V2 and the interstitial silicons Si_int1, Si_int2 are reduced, and the borons B1, B2 form the source diffusion layers 211, 212 and the drain diffusion layers 213, 214.
[0073] In this way, the ion implantation apparatus 1 and the ion implantation method according to the present embodiment can form a source diffusion layer (or a drain diffusion layer) consisting of the multiple impurity layers 211, 212 (or the multiple impurity layers 213, 214) with few crystal defects in one short ion implantation process sequence. The drain diffusion layer consisting of the multiple impurity layers 213, 214 with few crystal defects can relax the electric field near the drain, and can suppress the generation of leakage current and hot carriers.
[0074] Moreover, the ion implantation apparatus 1 and the ion implantation method can form a diffusion layer having a plurality of concentration profiles in one sequence of impurity implantation steps, thereby improving throughput and reducing production costs.
[0075] The concentrations of the ion components 12I and neutral components 12N in the ion beam 12 can be controlled by adjusting the pressure in the chamber 3. Therefore, the control unit 100 may control the concentrations of the ion components 12I and neutral components 12N by adjusting the pressure in the chamber 3. For example, when the pressure in the chamber 3 is set to 1×10 -3 (Pa) ~ 1 × 10 -2 (Pa), the probability of collision between the ion beam 12 and the increased number of particles increases accordingly. Therefore, the amount of neutral components 12N increases by 10 times. As a result, in this embodiment, the concentration profile of the diffusion layer can be formed with high accuracy by controlling the concentration of the neutral components 12N.
[0076] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope of the invention and its equivalents described in the claims, as well as in the scope and spirit of the invention. [Explanation of symbols]
[0077] 1 ion implantation device, 3 chamber, 5 stage, 10 ion source, 20 analyzer, 30 Q lens, 40 scanner, 50 parallel lens, 60 acceleration / deceleration electrode, 70 energy filter, 80, 90 drive unit, 100 control unit, 110 to 130 power supply, W semiconductor substrate
Claims
1. a stage on which a substrate can be mounted; a separation unit that separates the impurity beam to be introduced into the substrate into an ion component and a neutral component; a control unit that switches between a first mode in which the ion component is introduced into the substrate and a second mode in which the neutral component is introduced into the substrate.
2. The semiconductor manufacturing apparatus according to claim 1 , further comprising a drive unit that moves the stage to a first position where the ion component is introduced and a second position where the neutral component is introduced.
3. 3. The semiconductor manufacturing apparatus of claim 2, wherein the driving unit adjusts the inclination of the stage so that the ion component is introduced from a direction inclined at a first angle from a direction perpendicular to the surface of the substrate, and adjusts the inclination of the stage so that the neutral component is introduced from a direction inclined at a second angle from a direction perpendicular to the surface of the substrate.
4. 4. The semiconductor manufacturing apparatus of claim 3, wherein the control unit synchronously executes the movement of the stage between the first position and the second position and the adjustment of the stage between the first angle and the second angle.
5. Further comprising a chamber capable of accommodating the substrate; 5. The semiconductor manufacturing apparatus according to claim 1, wherein the control unit controls the concentrations of the ionic components and the neutral components by a pressure in the chamber.
6. 6. The semiconductor manufacturing apparatus according to claim 1, wherein the separation section differentiates energies of the ionic components and the neutral components, introduces the ionic components into the substrate with a first energy, and introduces the neutral components into the substrate with a second energy.
7. A method for manufacturing a semiconductor device using a semiconductor manufacturing apparatus having a separation unit that separates an impurity beam to be introduced into a substrate into an ion component and a neutral component and differentiates the energies of the ion component and the neutral component, comprising: Separating the impurity beam into ionic and neutral components; performing a first mode of introducing the ionic constituents to the substrate at a first energy; and performing a second mode in which the neutral component is introduced into the substrate at a second energy.
Citation Information
Patent Citations
JP1974001094A
Semiconductor device and manufacture of semiconductor device
JP1994045350A
Ion implanting method and device therefor
JP1995258846A
Method and device for implanting ion
JP1997115850A
Ion implantation device and ion implantation method
JP2002008579A