Semiconductor device and its manufacturing method
The semiconductor device addresses the issue of increased cell pitch by embedding gate wiring within substrate grooves, reducing resistance and maintaining integration density, thus enhancing reliability and breakdown voltage.
Patent Information
- Application Number
- JP2020183604
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-11-02
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2040-11-02
AI Technical Summary
Increasing the width of wiring in semiconductor integrated circuits to reduce electrical resistance leads to increased cell pitch, thereby reducing the degree of integration.
A semiconductor device with a substrate featuring intersecting grooves and a gate electrode and wiring configuration that reduces wiring resistance without increasing the cell pitch, achieved by embedding the gate wiring within the substrate grooves.
The solution effectively reduces wiring resistance and suppresses the reduction in integration density while improving the reliability and breakdown voltage of the semiconductor device.
Smart Images

Figure 0007579673000001 
Figure 0007579673000002 
Figure 0007579673000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device having a gate electrode and a method for manufacturing the same. [Background technology]
[0002] Wiring that electrically connects to each region of a transistor is disposed on the surface of a cell region of a semiconductor integrated circuit. For example, gate wiring that connects to a gate electrode is disposed on the main surface of a substrate. In order to reduce the electrical resistance of the wiring (hereinafter also referred to as "wiring resistance"), measures can be taken to widen the width of the wiring. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2013 / 128833 Summary of the Invention [Problem to be solved by the invention]
[0004] However, increasing the width of the wiring increases the cell pitch, which reduces the degree of integration of the semiconductor integrated circuit.
[0005] An object of the present invention is to provide a semiconductor device capable of reducing wiring resistance and suppressing a reduction in the integration density of a semiconductor integrated circuit, and a method for manufacturing the same. [Means for solving the problem]
[0006] A semiconductor device according to one aspect of the present invention includes a substrate having a first groove and a second groove shallower than the first groove formed in a main surface thereof, a gate electrode disposed inside the first groove, and a gate wiring disposed inside the second groove, and the gate electrode and the gate wiring are electrically connected at the intersection of the first groove and the second groove. Effect of the Invention
[0007] According to the present invention, it is possible to provide a semiconductor device capable of reducing wiring resistance and suppressing a reduction in the integration density of a semiconductor integrated circuit, and a method for manufacturing the same. [Brief description of the drawings]
[0008] [Figure 1] 1 is a schematic perspective view showing a configuration of a semiconductor device according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic cross-sectional view taken along the II-II direction in FIG. [Diagram 3] FIG. 2 is a schematic cross-sectional view taken along the line III-III in FIG. [Figure 4] 4 is a schematic cross-sectional view taken along the line IV-IV in FIG. 1. [Diagram 5] FIG. 1 is a schematic perspective view (part 1) for explaining a method for manufacturing a semiconductor device according to a first embodiment of the present invention. [Figure 6] FIG. 2 is a schematic perspective view (part 2) for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention. [Figure 7] FIG. 3 is a schematic perspective view (part 3) for explaining the method for manufacturing the semiconductor device according to the first embodiment of the present invention. [Figure 8] 5 is a schematic cross-sectional view showing a configuration of a semiconductor device according to a modified example of the first embodiment of the present invention. [Figure 9] 11 is a schematic cross-sectional view showing another configuration of a semiconductor device according to a modified example of the first embodiment of the present invention. [Figure 10] 11 is a schematic cross-sectional view showing another configuration of a semiconductor device according to a modified example of the first embodiment of the present invention. [Figure 11] FIG. 11 is a schematic perspective view showing a configuration of a semiconductor device according to a second embodiment of the present invention. [Figure 12] FIG. 11 is a schematic cross-sectional view showing a configuration of a semiconductor device according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, the embodiments will be described with reference to the drawings. In the description of the drawings, the same parts are given the same reference numerals and the description will be omitted. However, the drawings are schematic, and the relationship between thickness and planar dimensions, the thickness ratio of each layer, and the like include parts that differ from the actual ones. In addition, there are parts where the dimensional relationships and ratios differ between the drawings.
[0010] (First embodiment) A semiconductor device according to a first embodiment of the present invention is shown in Fig. 1. The semiconductor device shown in Fig. 1 includes a substrate 10 having a first main surface 101 on which a first groove and a second groove intersecting the first groove are formed, a gate electrode 30 disposed inside the first groove, and a gate wiring 40 disposed inside the second groove. The second groove is formed shallower than the first groove. The gate electrode 30 and the gate wiring 40 are electrically connected at the intersection of the first groove and the second groove. The gate electrode 30 and the gate wiring 40 are, for example, polysilicon films.
[0011] A gate insulating film 31 is disposed on the inner wall surface of the first trench. A gate wiring insulating film 41 is disposed on the inner wall surface of the second trench. The gate insulating film 31 and the gate wiring insulating film 41 are, for example, silicon oxide films.
[0012] The substrate 10 may be a semiconductor substrate, a semi-insulating substrate, or an insulating substrate. Here, an insulating substrate refers to a semiconductor substrate having a resistivity of several kΩ / cm or more. For example, the substrate 10 is an insulating silicon carbide substrate.
[0013] A first conductivity type drift region 11, a second conductivity type well region 12, a first conductivity type source region 13, and a first conductivity type drain region 14 are formed on the upper part of the substrate 10. The upper surfaces of the drift region 11, the well region 12, the source region 13, and the drain region 14 are exposed to a first main surface 101 of the substrate 10.
[0014] The drift region 11 is selectively formed in a portion of the upper part of the substrate 10. The impurity concentration of the substrate 10 is set to be lower than the impurity concentration of the drift region 11. The drift region 11 contacts a portion of the side surface of the first trench.
[0015] The well region 12 is formed in a part of the upper part of the substrate 10 in a region where the drift region 11 is not formed. The well region 12 has a region (hereinafter also referred to as a "channel region") facing the gate electrode 30 via the gate insulating film 31. The channel region faces the gate electrode 30 on the remaining side surfaces except for the side surface of the first trench that contacts the drift region 11. The channel region of the well region 12 contacts the drift region 11. When the semiconductor device is in an on-operation state, an inversion layer is formed in the channel region.
[0016] The source region 13 is formed in a part of the upper part of the well region 12, and is connected to the drift region 11 via the channel region of the well region 12. The source region 13 contacts the first trench at a side surface of the first trench facing the side surface in contact with the drift region 11. In other words, the channel region of the well region 12 faces the gate electrode 30 via the gate insulating film 31 at side surfaces of the first trench adjacent to the side surface in contact with the drift region 11 and the side surface in contact with the source region 13.
[0017] The drain region 14 is connected to the drift region 11 at a position spaced apart from the well region 12. In the semiconductor device shown in FIG.
[0018] The first conductivity type and the second conductivity type are opposite conductivity types. That is, if the first conductivity type is n-type, the second conductivity type is p-type, and if the first conductivity type is p-type, the second conductivity type is n-type. In the following, a case where the first conductivity type is n-type and the second conductivity type is p-type will be described.
[0019] The opening of the first trench in the first main surface 101 of the substrate 10 spans the drift region 11, the well region 12, and the source region 13. The opening of the second trench in the first main surface 101 is formed in the well region 12. However, the second trench may be formed to span the well region 12 and the drift region 11. The gate wiring insulating film 41 electrically insulates the drift region 11, the well region 12, and the source region 13 from the gate wiring 40.
[0020] FIG. 2 shows a cross-sectional view of the semiconductor device along a direction perpendicular to the extension direction of the first trench. FIG. 3 shows a cross-sectional view of the semiconductor device along a direction perpendicular to the extension direction of the second trench. Although not shown in FIG. 1, a source electrode 50 and a drain electrode 60 are disposed on the first main surface 101 of the substrate 10. The source electrode 50 is electrically connected to the source region 13 and the well region 12. The drain electrode 60 is electrically connected to the drain region 14. As shown in FIG. 3, the channel region 121 of the well region 12 is the well region 12 along the side surface of the first trench at a position deeper than the bottom end of the second trench.
[0021] FIG. 4 shows a cross-sectional view of the semiconductor device along the extension direction of the second trench. The first trench, in which the gate electrode 30 is disposed, extends from the surface of the substrate 10 to below the well region 12, penetrating the well region 12. As shown in FIG. 4, a gate insulating film 31 is disposed on the inner wall surface of the first trench, except for the region intersecting with the second trench. A gate wiring insulating film 41 is disposed on the inner wall surface of the second trench, except for the region intersecting with the first trench. As shown in FIG. 4, the gate wiring 40 disposed inside the second trench is connected to the multiple gate electrodes 30 at the intersection of the first trench and the second trench. A predetermined gate voltage is supplied to the gate electrode 30 via the gate wiring 40.
[0022] 2 and 3, when viewed from the surface normal direction of first main surface 101 of substrate 10 (hereinafter also referred to as "planar view"), at least a portion of the second groove is formed in well region 12. Here, the distance from first main surface 101 of substrate 10 to the bottom surface of well region 12 in a region where the second groove is not formed is designated as X, and the depth of the second groove is designated as Y. The distance from first main surface 101 of substrate 10 to the bottom surface of well region 12 directly below the second groove is designated as X+Y. The first groove penetrates well region 12, and the depth T of the first groove is greater than X+Y.
[0023] Well region 12 is formed in substrate 10 deeper in the film thickness direction of substrate 10 than drift region 11. In other words, when the distance from first main surface 101 of substrate 10 to the bottom surface of drift region 11 is Z, X>Z. In this manner, the bottom surface of well region 12 is located lower than the bottom surface of drift region 11.
[0024] The basic operation of the semiconductor device shown in FIG. 1 will now be described.
[0025] In an on-operation, the potential of the gate electrode 30 is controlled with a positive potential applied to the drain electrode 60 with the potential of the source electrode 50 as a reference. This allows the semiconductor device to operate as a transistor. That is, by making the voltage between the gate electrode 30 and the source electrode 50 equal to or higher than a predetermined threshold voltage, an inversion layer is formed in the channel region of the well region 12. As a result, the semiconductor device is turned on, and a main current flows between the source electrode 50 and the drain electrode 60.
[0026] On the other hand, in the off operation, the voltage between the gate electrode 30 and the source electrode 50 is set to a predetermined threshold voltage or less, whereby the inversion layer in the well region 12 disappears and the main current between the source electrode 50 and the drain electrode 60 is cut off.
[0027] In operation of the semiconductor device, the potentials of the multiple gate electrodes 30 are set to the same potential via the gate wiring 40. The channel region of the well region 12 facing the gate electrode 30 via the gate insulating film 31 is formed in a portion of the gate electrode 30 deeper than the lower end of the gate wiring 40. By forming the gate electrode 30 to a deeper position, the width of the channel region is also expanded. This makes it possible to reduce the electrical resistance (channel resistance) of the channel region.
[0028] As described above, the semiconductor device in FIG. 1 has a structure in which the gate wiring 40 is embedded in the substrate 10. In order to reduce the wiring resistance of the gate wiring 40, the second groove may be formed deep along the film thickness direction of the substrate 10. Therefore, in order to reduce the wiring resistance of the gate wiring 40, it is not necessary to increase the width of the gate wiring 40 in a plan view. Therefore, the expansion of the cell pitch is suppressed. As a result, according to the semiconductor device of the first embodiment, the wiring resistance of the gate wiring 40 can be reduced and a reduction in the integration density of the semiconductor integrated circuit can be suppressed.
[0029] Furthermore, according to the semiconductor device of the first embodiment, the gate wiring 40 is embedded in the substrate 10, thereby improving the flatness of the main surface of the substrate 10. This prevents the wiring arranged on the main surface of the substrate 10 from being cut or the width of the wiring from being narrowed due to steps on the main surface of the substrate 10. As a result, the reliability of the semiconductor device is improved.
[0030] Furthermore, since the impurity concentration of the substrate 10 is lower than that of the drift region 11, the impurity concentration is low in the region in contact with the edge of the well region 12. This reduces electric field concentration in the semiconductor device, improving the breakdown voltage.
[0031] Moreover, in the semiconductor device according to the first embodiment, the well region 12 is formed deeper in the film thickness direction of the substrate 10 than the drift region 11. The first trench extends to below the well region 12, and the gate electrode 30 is disposed deeper in the film thickness direction of the substrate 10. This allows the channel region formed on the side surface of the first trench to maintain a wide width in the film thickness direction of the substrate 10. This makes it possible to suppress an increase in channel resistance. As a result, the on-resistance of the semiconductor device can be reduced.
[0032] When at least a portion of the second trench is formed in the well region 12, the depth T of the first trench is larger than the distance X+Y from the first main surface 101 of the substrate 10 directly below the second trench to the bottom surface of the well region 12. Since the semiconductor device shown in FIG. 1 has a structure in which the channel width increases by expanding the channel region, the channel resistance can be reduced by making T>X+Y.
[0033] A semi-insulating substrate or an insulating substrate may be used for the substrate 10. This can prevent leakage current from flowing to the back surface of the substrate 10 opposite the first main surface 101. Furthermore, by using a semi-insulating substrate or an insulating substrate for the substrate 10, the element isolation process can be simplified when integrating multiple semiconductor devices on the same substrate 10.
[0034] A wide band gap semiconductor substrate may be used for the substrate 10. Wide band gap semiconductors include, for example, silicon carbide (SiC), gallium nitride (GaN), diamond, zinc oxide (ZnO), and aluminum gallium nitride (AlGaN). For example, an insulating silicon carbide substrate may be used for the substrate 10. There are several polytypes (crystal polymorphism) of SiC, and a typical 4H SiC substrate may be used for the substrate 10. By making the drift region 11 a wide band gap semiconductor, the breakdown voltage of the semiconductor device can be improved.
[0035] A method for manufacturing a semiconductor device according to a first embodiment of the present invention will be described below with reference to the drawings. Note that the method for manufacturing a semiconductor device described below is one example, and various other manufacturing methods, including modifications thereof, can be used. In the following, a case where a non-doped insulating silicon carbide substrate is used as the substrate 10 will be described.
[0036] First, as shown in Fig. 5, a second groove 400 is formed in the first main surface 101 of the substrate 10. For example, a mask material is formed on the first main surface 101 of the substrate 10. Then, this mask material is patterned to selectively remove the mask material in the region where the second groove 400 is to be formed. Thereafter, the second groove 400 is formed by a dry etching method using the patterned mask material as a mask.
[0037] A typical mask material may be, for example, a silicon oxide film. A thermal CVD method or a plasma CVD method may be used as a method for depositing the mask material. A photolithography method may be used as a patterning method. That is, the mask material is etched using a patterned photoresist film as a mask. A wet etching method using hydrofluoric acid or a dry etching method such as a reactive ion etching method may be used as an etching method. Thereafter, the photoresist film is removed with oxygen plasma, sulfuric acid, or the like. In this way, the mask material is patterned (the same applies below).
[0038] 6, an n-type drift region 11, a p-type well region 12, a high impurity concentration n-type source region 13, and a high impurity concentration n-type drain region 14 are formed in the substrate 10. For example, the drift region 11, the well region 12, the source region 13, and the drain region 14 are formed by an ion implantation method using a mask material patterned on the first main surface 101 of the substrate 10 as a mask. Note that the position of the bottom surface of the well region 12 is lower in the region where the impurity is ion-implanted from the bottom surface of the second groove 400 than in the region where the impurity is ion-implanted from the first main surface 101.
[0039] In the above ion implantation method, for example, nitrogen may be used as the n-type impurity, and aluminum or boron may be used as the p-type impurity. By implanting ions into the substrate 10 while the substrate 10 is heated to a temperature of about 600° C., it is possible to suppress the occurrence of crystal defects in the ion-implanted region. The impurity concentration in the drift region 11 and the well region 12 is, for example, 1E15 cm -3 ~1E19cm -3 The drift region 11 and the well region 12 are formed so that the positions of the bottom surfaces of the drift region 11 and the well region 12 are lower than the lower end of the second trench 400.
[0040] After the ion implantation, the impurities doped in the substrate 10 are activated by heat treatment. For example, the heat treatment is performed at about 1700° C. in an argon or nitrogen atmosphere.
[0041] Next, as shown in FIG. 7, the first groove 300 is formed in the first main surface 101 of the substrate 10. For example, the first groove 300 is formed by a dry etching method using a mask material patterned on the first main surface 101 of the substrate 10 as a mask. An opening of the first groove 300 is formed in a position across the drift region 11, the source region 13, and the well region 12 of the first main surface 101. The first groove 300 is also formed in a position intersecting with the second groove 400. The first groove 300 is formed to a depth penetrating the well region 12.
[0042] Thereafter, a gate insulating film 31 is formed on the inner wall surface of the first groove 300, and a gate wiring insulating film 41 is formed on the inner wall surface of the second groove 400. The thickness of the gate insulating film 31 is, for example, about several tens of nm. Hereinafter, the first groove 300 and the second groove 400 are also collectively referred to as "grooves".
[0043] The gate insulating film 31 and the gate line insulating film 41 may be formed at the same time by thermal oxidation or CVD. When the gate insulating film 31 and the gate line insulating film 41 are formed by thermal oxidation, the substrate 10 is heated to a temperature of about 1100°C in an oxygen atmosphere. This forms a silicon oxide film on all parts of the substrate 10 that are in contact with oxygen. Alternatively, the gate insulating film 31 and the gate line insulating film 41 may be formed by thermal oxidation in a pure NO or NO atmosphere. In this case, the temperature of the thermal oxidation is preferably 1100°C to 1400°C.
[0044] After the gate insulating film 31 and the gate wiring insulating film 41 are formed, in order to reduce the interface state at the interface between the well region 12 and the gate insulating film 31, an annealing treatment may be performed at about 1000° C. in an atmosphere of nitrogen, argon, N2O, or the like.
[0045] Next, the first trench 300 is filled to form the gate electrode 30, and the second trench 400 is filled to form the gate wiring 40. The gate electrode 30 and the gate wiring 40 may be formed at the same time. The gate electrode 30 is generally made of a polysilicon film, and the case where the polysilicon film is used for the gate electrode 30 and the gate wiring 40 will be described here. The polysilicon film may be deposited by low-pressure CVD. For example, the thickness of the polysilicon film to be deposited is set to a value greater than half the width of the trench, and the inside of the trench is filled with the polysilicon film. Since the polysilicon film is formed from the inner wall surface of the trench, the trench can be completely filled with the polysilicon film by setting the thickness of the polysilicon film as described above. For example, when the width of the trench is 2 μm, the polysilicon film is formed so that the film thickness is greater than 1 μm. After the polysilicon film is deposited, an annealing process is performed at 950° C. in phosphorus oxychloride (POCl3) to form an n-type polysilicon film, which can impart conductivity to the gate electrode 30 and the gate wiring 40.
[0046] The polysilicon film is planarized by etching or the like. The etching method may be isotropic etching or anisotropic selective etching. The amount of etching is set so that the polysilicon film remains inside the trench. For example, if a polysilicon film is deposited to a thickness of 1.5 μm for a trench that is 2 μm wide, the amount of etching of the polysilicon film is set to 1.5 μm. However, in controlling the etching, over-etching by a few percent for an etching amount of 1.5 μm is no problem.
[0047] Thereafter, an interlayer insulating film (not shown) is formed so as to cover the entire upper surface of the substrate 10. The interlayer insulating film may be a silicon oxide film or a silicon nitride film. Then, the interlayer insulating film on the upper surface of the region of the source region 13 connected to the source electrode 50 and the interlayer insulating film on the upper surface of the region of the drain region 14 connected to the drain electrode 60 are removed. For example, the interlayer insulating film is selectively removed by a dry etching method using a patterned resist film as a mask using a photolithography technique or the like. In this manner, an opening in the interlayer insulating film is formed. Thereafter, the source electrode 50 connected to the source region 13 through the opening in the interlayer insulating film, and the drain electrode 60 connected to the drain region 14 through the opening in the interlayer insulating film are formed, respectively. Metal materials are generally used as electrode materials for the source electrode 50 and the drain electrode 60. For example, titanium (Ti), nickel (Ni), molybdenum (Mo), etc. may be used as the electrode material. Alternatively, a laminated metal such as Ti / Ni / Ag may be used as the electrode material.
[0048] The above steps complete the semiconductor device shown in Fig. 1. In the above manufacturing method, after the second trench 400 is formed, the drift region 11 and the well region 12 are formed by ion implantation. This allows the drift region 11 and the well region 12 directly below the second trench 400 to be formed in one step, thereby reducing the number of manufacturing steps.
[0049] As described above, by forming the gate electrode 30 and the gate wiring 40 from the same material, it is possible to reduce the contact resistance between the gate electrode 30 and the gate wiring 40. Furthermore, by forming the gate electrode 30 and the gate wiring 40 at the same time, it is possible to reduce the number of manufacturing steps.
[0050] Furthermore, by using polysilicon films for the gate electrode 30 and the gate wiring 40, the gate electrode 30 and the gate wiring 40 can be formed by low pressure CVD, which allows the gate electrode 30 and the gate wiring 40 to be formed with good coverage inside the trench.
[0051] Furthermore, the gate insulating film 31 and the gate wiring insulating film 41 can be formed at the same time by thermal oxidation or CVD, thereby reducing the number of manufacturing steps. The thickness of the gate wiring insulating film 41 may be made thicker than that of the gate insulating film 31. By making the thickness of the gate wiring insulating film 41 thicker, the distance between the end of the gate wiring 40 embedded in the second trench and the drain region 14 becomes wider. This makes it possible to suppress a decrease in the breakdown voltage of the semiconductor device.
[0052] <Modification> 8, at least a part of the second groove may be formed in drift region 11 in plan view. When the distance from the main surface of substrate 10 to the bottom surface of drift region 11 in a region where the second groove is not formed is Z, the distance from the main surface of substrate 10 directly below the second groove to the bottom surface of drift region 11 is Y+Z.
[0053] 8 has a structure in which the drift region 11 is deepened by the depth of the second trench in which the gate wiring 40 is formed. Therefore, even if the cross-sectional area of the gate wiring 40 is increased in order to reduce the resistance of the gate wiring 40, an increase in the resistance of the current flowing through the drift region 11 (drift resistance) can be suppressed.
[0054] 9, a sector-shaped well extension region 120 may be formed in the substrate 10, with the end of the second trench in contact with the well region 12 at its center and the film thickness of the well region 12 as its radius. The well extension region 120 is a region of the second conductivity type with the same impurity concentration as the well region 12. The well extension region 120 is formed in the substrate 10, with a region overlapping with the well region 12.
[0055] The semiconductor device shown in Fig. 9 has a structure in which the channel width is increased by expanding the channel region, thereby reducing the channel resistance.
[0056] The well extension region 120 may be formed by ion implanting the same impurity as the well region 12 after the well region 12 is formed. For example, after forming a second groove by dry etching or the like, the well region 12 is formed by ion implantation using a patterned mask material as a mask. Next, the well extension region 120 is formed by ion implanting additional impurities with the substrate 10 tilted obliquely. The impurity concentration and implantation depth when forming the well extension region 120 are the same as when forming the well region 12. Thereafter, the drift region 11, the source region 13, and the drain region 14 are formed by ion implantation or the like.
[0057] 10, a sector-shaped drift extension region 110 may be formed in the substrate 10, with the end of the second groove at the bottom that contacts the drift region 11 as its center and the film thickness of the drift region 11 as its radius. The drift extension region 110 is a region of the first conductivity type with the same impurity concentration as the drift region 11. The drift extension region 110 is formed in the substrate 10, having a region that overlaps with the drift region 11.
[0058] 10 has a structure in which the width of drift region 11 is increased by expanding drift region 11. This makes it possible to reduce the drift resistance.
[0059] The drift extension region 110 may be formed by ion implanting the same impurities as those in the drift region 11 after the drift region 11 is formed. For example, after the drift region 11 is formed, additional impurities are ion implanted while the substrate 10 is tilted, thereby forming the drift extension region 110. The impurity concentration and implantation depth when forming the drift extension region 110 are the same as when forming the drift region 11.
[0060] Second embodiment In the semiconductor device according to the second embodiment, as shown in FIG. 11, the drain region 14 is arranged so as to be exposed on the second main surface 102 of the substrate 10 facing the first main surface 101. A second groove in which the gate wiring 40 is arranged is formed in the drift region 11 at a position separated from the well region 12. An opening of a first groove in which the gate electrode 30 is arranged is formed in the first main surface 101 across the drift region 11, the well region 12, and the source region 13 exposed on the first main surface 101 of the substrate 10. In the region surrounded by the drift region 11, the gate electrode 30 and the gate wiring 40 are connected. The rest is the same as the first embodiment shown in FIG. 1.
[0061] The basic operation of the semiconductor device shown in FIG. 11 is the same as that of the semiconductor device shown in FIG. 1. In the semiconductor device shown in FIG. 11, the current flowing in the channel region formed in the well region 12 in parallel with the main surface of the substrate 10 flows in the drift region 11 in the film thickness direction of the substrate 10. In the semiconductor device shown in FIG. 11, the gate wiring 40 is disposed in the drift region 11 at a position away from the well region 12. Therefore, according to the semiconductor device shown in FIG. 11, the inhibition of the current path by the gate wiring 40 can be made smaller than that of the semiconductor device shown in FIG. 1. In other words, according to the semiconductor device of the second embodiment, the effect on the electrical resistance of the current path caused by forming the second groove in the substrate 10, in which the gate wiring 40 is disposed, can be made smaller than that of the semiconductor device of the first embodiment.
[0062] An example of a method for manufacturing the semiconductor device according to the second embodiment will be described below.
[0063] First, a drift region 11 is formed by epitaxial growth on a substrate 10. The substrate 10 is, for example, a silicon carbide semiconductor substrate of a first conductivity type with a high impurity concentration. A portion of the silicon carbide semiconductor substrate is a drain region 14.
[0064] Next, by ion implantation using the patterned mask material as a mask, well regions 12 and source regions 13 are selectively formed above drift region 11. The ion implantation and activation steps are similar to those described in the first embodiment.
[0065] Then, a first trench and a second trench are formed using a photolithography technique or the like. Next, a gate insulating film 31 is formed on the inner wall surface of the first trench, and the inside of the first trench is filled with a gate electrode 30. Furthermore, a gate wiring insulating film 41 is formed on the inner wall surface of the second trench, and the inside of the second trench is filled with a gate wiring 40. The method of forming the gate electrode 30 and the gate wiring 40 is the same as in the first embodiment.
[0066] Thereafter, a source electrode 50 electrically connected to the source region 13 is formed on the first main surface 101 of the substrate 10. A drain electrode 60 electrically connected to the drain region 14 is formed on the second main surface 102 of the substrate 10. The drain electrode 60 is made of, for example, a metal material. With the above steps, the semiconductor device shown in FIG. 11 is completed.
[0067] (Other embodiments) As described above, the present invention has been described by the embodiment, but the description and drawings forming a part of this disclosure should not be understood as limiting the present invention. Various alternative embodiments, examples and operating techniques will become apparent to those skilled in the art from this disclosure.
[0068] 12, the width of the second groove may be gradually narrowed from the main surface of the substrate 10 along the film thickness direction of the substrate 10. By tapering the second groove in which the gate wiring 40 is formed, the angle of the end of the gate wiring insulating film 41 becomes gentle. This makes it possible to alleviate electric field concentration.
[0069] In addition, although an example in which an n-type polysilicon film is used for the gate electrode 30 has been described above, a p-type polysilicon film may also be used for the gate electrode 30. In addition, other semiconductor materials may also be used for the gate electrode 30, and other conductive materials such as metal materials may also be used for the gate electrode 30. For example, p-type polysilicon carbide, SiGe, Al, etc. may also be used as the material for the gate electrode 30.
[0070] Moreover, although an example in which a silicon oxide film is used for the gate insulating film 31 has been described, a silicon nitride film may be used for the gate insulating film 31. Alternatively, a laminated film of a silicon oxide film and a silicon nitride film may be used for the gate insulating film 31.
[0071] Thus, it goes without saying that the present invention includes various embodiments that are not described here. [Explanation of symbols]
[0072] 10...Substrate 11…Drift region 12...Well area 13…Source region 14…Drain region 30...Gate electrode 31...Gate insulating film 40…Gate wiring 41...Gate wiring insulating film 50…Source electrode 60...Drain electrode 110…Drift extension area 120…Well extension area 121…Channel region
Claims
1. a substrate having a first groove and a second groove intersecting the first groove and shallower than the first groove formed on a main surface thereof; a gate insulating film disposed on an inner wall surface of the first trench; a gate electrode disposed within the first trench; a drift region of a first conductivity type formed in the substrate and in contact with a part of a side surface of the first trench; a well region of a second conductivity type formed in the substrate, the well region having a channel region facing the gate electrode via the gate insulating film on the remaining side of the first trench except for a side in contact with the drift region; a first conductivity type source region formed in an upper portion of the well region and connected to the drift region via the channel region; a drain region of a first conductivity type formed in the substrate and connected to the drift region at a position spaced apart from the well region; a gate wiring insulating film disposed on an inner wall surface of the second trench; a gate wiring disposed inside the second trench and electrically connected to the gate electrode at an intersection of the first trench and the second trench; A semiconductor device comprising:
2. an impurity concentration of the substrate is lower than an impurity concentration of the drift region; The well region is formed in the substrate deeper in a thickness direction of the substrate than the drift region.
2. The semiconductor device according to claim 1,
3. 3. The semiconductor device according to claim 1, wherein the first trench extends to below the well region.
4. At least a portion of the second trench is formed in the well region in a plan view, a distance from the main surface of the substrate to a bottom surface of the well region in a region where the second trench is not formed is X, and a depth of the second trench is Y, a distance from the main surface of the substrate to the bottom surface of the well region directly below the second trench is X+Y; The depth of the first groove is greater than X+Y.
4. The semiconductor device according to claim 1, wherein the first insulating layer is a conductive layer.
5. At least a portion of the second groove is formed in the drift region in a plan view, When the distance from the main surface of the substrate to the bottom surface of the drift region in a region where the second groove is not formed is Z and the depth of the second groove is Y, the distance from the main surface of the substrate to the bottom surface of the drift region directly below the second groove is Y+Z.
5. The semiconductor device according to claim 1, wherein the first insulating layer is a conductive layer.
6. 6. The semiconductor device according to claim 1, wherein the width of the second groove gradually decreases from the main surface along a thickness direction of the substrate.
7. a well extension region of a second conductivity type having the same impurity concentration as the well region, the well extension region being formed in the substrate and having a region overlapping with the well region and a sector shape having a radius of a film thickness of the well region and a center at an end of a lower end of the second trench that contacts the well region 7. The semiconductor device according to claim 1, wherein the first insulating layer is a conductive layer.
8. a drift extension region of a first conductivity type having the same impurity concentration as the drift region, the drift extension region being formed in the substrate and having a region overlapping with the drift region and a sector shape having a radius equal to the thickness of the drift region and centered at an end of a lower end of the second groove that contacts the drift region, 6. The semiconductor device according to claim 5,
9. 9. The semiconductor device according to claim 1, wherein the substrate is a semi-insulating substrate or an insulating substrate.
10. 10. The semiconductor device according to claim 1, wherein the substrate is a silicon carbide substrate.
11. 11. The semiconductor device according to claim 1, wherein the gate electrode and the gate wiring are made of the same material.
12. 12. The semiconductor device according to claim 1, wherein the material of the gate electrode is a polysilicon film.
13. 13. The semiconductor device according to claim 1, wherein the gate wiring insulating film has a thickness larger than that of the gate insulating film.
14. forming a first groove and a second groove intersecting the first groove and shallower than the first groove in a major surface of a substrate; forming a gate insulating film on an inner wall surface of the first trench; forming a gate electrode within the first trench; forming a drift region of a first conductivity type in the substrate, the drift region being in contact with a portion of a side surface of the first trench; forming a second conductivity type well region in the substrate, the well region having a channel region facing the gate electrode via the gate insulating film on a remaining side surface of the first trench excluding a side surface in contact with the drift region; forming a source region of a first conductivity type in an upper portion of the well region, the source region being connected to the drift region via the channel region; forming a drain region of a first conductivity type in the substrate, the drain region being connected to the drift region at a position spaced from the well region; forming a gate wiring insulating film on an inner wall surface of the second trench; forming a gate wiring inside the second trench, the gate wiring being electrically connected to the gate electrode at an intersection of the first trench and the second trench; Including, a second trench formed in the first region and a second trench formed in the second region;
15. 15. The method for manufacturing a semiconductor device according to claim 14, wherein after the first groove and the second groove are formed, the gate insulating film and the gate wiring insulating film are formed at once by a thermal oxidation method or a CVD method.
16. 16. The method for manufacturing a semiconductor device according to claim 14, wherein after the gate insulating film and the gate wiring insulating film are formed, the gate electrode and the gate wiring are formed at once by low pressure CVD.
Citation Information
Patent Citations
Semiconductor device
CN111373547A
Semiconductor device
JP1999103058A
Lateral semiconductor device utilizing trench structure and its manufacturing method
JP2006049826A
Lateral mosfet and manufacturing method thereof
JP2008210994A
Semiconductor device and manufacturing method therefor
JP2011249422A