Variable extraction assembly for wide angle ion beams.

The ion beam processing system with dielectric materials and controlled angular distribution addresses non-uniformity in plasma processing by maintaining consistent ion beam angles and reducing contamination, ensuring uniform semiconductor processing.

JP7580565B2Active Publication Date: 2024-11-11APPLIED MATERIALS INC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023501883
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-07-15
Filing Date
2021-06-09
Publication Date
2024-11-11
Estimated Expiration
2041-06-09

AI Technical Summary

Technical Problem

Existing ion-assisted plasma processes for semiconductor manufacturing face non-uniformity issues due to beam divergence when scanning wafers with ion beams having large angles of incidence, leading to variations in processing across the substrate surface.

Method used

An ion beam processing system with a plasma chamber and extraction assembly using dielectric materials for the plasma plate and beam shield, along with conductive electrodes, facilitates the generation of ion beams with large on-wafer incidence angles and controlled angular distribution, allowing for symmetrical ribbon beamlets to process complex semiconductor structures uniformly.

Benefits of technology

The system achieves uniform processing of semiconductor structures by maintaining consistent ion beam angles and reducing contamination, while minimizing metal contamination and simplifying the design with a compact, low-profile configuration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007580565000008
    Figure 0007580565000008
  • Figure 0007580565000009
    Figure 0007580565000009
  • Figure 0007580565000010
    Figure 0007580565000010
Patent Text Reader

Abstract

An ion beam processing system is provided that includes a plasma chamber, a plasma plate juxtaposed with the plasma chamber and defining a first extraction aperture, a beam shield disposed within the plasma chamber and facing the extraction aperture, a shield electrode disposed on a surface of the beam shield outside the plasma chamber, and an extraction electrode disposed on a surface of the plasma plate outside the plasma chamber.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present embodiments relate to plasma processing apparatus, and more particularly to angled ion beams extracted from a plasma source using a novel ion extraction assembly. [Background technology]

[0002] In the fabrication of complex 3D semiconductor structures, ion-assisted plasma processes are often used. Many such processes use an ion beam with zero or small angles of incidence with respect to the normal of the substrate surface. There are processes such as the controlled etching of trench sidewalls, where an ion beam with an ion angular distribution (IAD) characterized by a large average angle with respect to the normal (>50 degrees) is required. Such a large angle of incidence can be obtained by extracting the beam at zero degrees (with respect to the wafer normal when the wafer is oriented in the default "horizontal orientation") and tilting the wafer to the desired angle. For example, an ion beam with a cross section smaller than the area of ​​the substrate to be processed can be directed to impinge mostly along the normal orientation with respect to the horizontal plane, while the tilted substrate (with respect to the horizontal plane) is scanned along the horizontal direction to sequentially expose the entire substrate to the ion beam. A drawback of this approach is the non-uniformity of the process across the wafer surface, i.e., considering the inherent beam divergence, variations in the ion beam will occur as the wafer (substrate) is scanned in front of the beam.

[0003] It is with respect to these and other considerations that the present disclosure is provided. Summary of the Invention

[0004] This Summary is provided to introduce a selection of concepts in a simplified form that are further described below in the Detailed Description. This Summary is not intended to identify key features or essential features of the claimed subject matter, nor is it intended as an aid in determining the scope of the claimed subject matter.

[0005] An ion beam processing system according to a non-limiting embodiment of the present disclosure may include a plasma chamber, a plasma plate juxtaposed with the plasma chamber, the plasma plate defining a first extraction aperture, a beam shield disposed within the plasma chamber and facing the extraction aperture, a shielding electrode disposed on a surface of the beam shield outside the plasma chamber, and an extraction electrode disposed on a surface of the plasma plate outside the plasma chamber.

[0006] An ion beam processing system according to another non-limiting embodiment of the present disclosure may include a plasma chamber; a plasma plate formed from an electrically insulating material and juxtaposed to the plasma chamber, the plasma plate defining a first extraction aperture; a beam shield formed from an electrically insulating material and disposed within the plasma chamber and facing the extraction aperture; a shielding electrode formed from a conductive material, covered by a first dielectric coating, and disposed on a surface of the beam shield outside the plasma chamber, the shielding electrode being flat and having a thickness measured in a direction perpendicular to a front surface of the beam shield, the shielding electrode being less than one millimeter; an extraction electrode formed from a conductive material, covered by the first dielectric coating, and disposed on a surface of the plasma plate outside the plasma chamber, the shielding electrode being flat and having a thickness measured in a direction perpendicular to a front surface of the plasma plate, the extraction electrode being less than one millimeter; and a pulsed voltage source electrically coupled to the plasma chamber and the extraction electrode to generate a bias voltage between the extraction electrode and the plasma chamber.

[0007] A method of fabricating a plasma plate assembly for an ion beam processing system according to non-limiting embodiments of the present disclosure may include providing a plasma plate formed from an electrically insulating material, the plasma plate defining an elongated extraction aperture; applying a conductive material to a front surface of the plasma plate surrounding the extraction aperture to form an extraction electrode, the extraction electrode being flat and having a thickness of less than 1 millimeter measured in a direction perpendicular to the front surface of the plasma plate; and applying a dielectric coating to the plasma plate and the extraction electrode, the dielectric coating covering the front surface of the plasma plate and the extraction electrode.

[0008] A method of fabricating a shielding assembly for an ion beam processing system according to non-limiting embodiments of the present disclosure may include providing a beam shielding portion formed from an electrically insulating material; applying a conductive material to a front surface of the beam shielding portion to form a shielding electrode, the shielding electrode being flat and having a thickness of less than 1 millimeter measured in a direction perpendicular to the front surface of the beam shielding portion; and applying a dielectric coating to the beam shielding portion and the shielding electrode, the dielectric coating covering the front surface of the beam shielding portion and the shielding electrode. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 illustrates a vertical cross-section of a processing apparatus consistent with an embodiment of the present disclosure. [Figure 2A] 1A-1C are diagrams collectively illustrating the evolution of electron and ion distributions as a function of time, in accordance with an embodiment of the present disclosure. [Figure 2B] 1A-1C are diagrams collectively illustrating the evolution of electron and ion distributions as a function of time, in accordance with an embodiment of the present disclosure. [Figure 2C] 1A-1C are diagrams collectively illustrating the evolution of electron and ion distributions as a function of time, in accordance with an embodiment of the present disclosure. [Figure 2D]1A-1C are diagrams collectively illustrating the evolution of electron and ion distributions as a function of time, in accordance with an embodiment of the present disclosure. [Figure 3A] FIG. 2 illustrates an operating scenario of a processing device arranged according to FIG. 1 and shows beamlets, shapes and electrostatic potential distribution in the extraction region. [Figure 3B] FIG. 2 illustrates an operating scenario of a processing device arranged according to FIG. 1 and shows beamlets, shapes and electrostatic potential distribution in the extraction region. [Figure 3C] FIG. 2 illustrates an operating scenario of a processing device arranged according to FIG. 1 and shows beamlets, shapes and electrostatic potential distribution in the extraction region. [Figure 4] 3A-C are graphs showing ion angular distributions for the scenarios illustrated in FIGS. 3A-C. [Diagram 5] FIG. 2 illustrates a vertical cross-section of a processing apparatus consistent with another embodiment of the present disclosure. [Figure 6] 6A-F illustrate an operating scenario of a processing device arranged according to FIG. 5 and show beamlets, shapes and electrostatic potential distribution in the extraction region. [Figure 7-1] 7 is a graph showing ion angular distribution for the scenario illustrated in FIGS. 6A-C. [Figure 7-2] 7 is a graph showing ion angular distribution for the scenario illustrated in FIGS. 6D-F. [Figure 8] 1A and 1B are perspective and exploded views illustrating a plasma chamber and extraction assembly of a processing apparatus consistent with an embodiment of the present disclosure. [Figure 9] 1A-C are a series of perspective views illustrating a method of fabricating a plasma plate, extraction electrode, and first dielectric coating of a processing apparatus consistent with an embodiment of the present disclosure. [Figure 10] FIG. 10 is a flow diagram illustrating the method described in FIGS. 9A-C. [Figure 11] 1A-C are a series of perspective views illustrating a method of fabricating a beam shield, a shield electrode, and a second dielectric coating of a processing apparatus consistent with an embodiment of the present disclosure. [Figure 12] FIG. 11 is a flow diagram illustrating the method described in FIGS. 11A-C. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The present embodiments will now be described in more detail hereinafter with reference to the accompanying drawings, in which several embodiments are shown. The subject matter of the present disclosure may be embodied in many different forms and should not be construed as being limited to the embodiments set forth herein. These embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the subject matter to those skilled in the art. In the drawings, like numbers refer to like elements throughout.

[0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The embodiments described herein provide systems and methods for controlling the angular distribution of ions directed at a substrate using hidden deflection electrodes. In some embodiments, an apparatus is disclosed that facilitates the generation of an ion beam with a large on-wafer incidence angle in a compact ion beam source. In addition to extracting an ion beam with a large incidence angle, the embodiments also incorporate the use of a chemically reactive plasma (feedstock gas: C x F y , C x H y F z ,SCIENCE FICTION 6 , H 2 , O 2 , Cl 2 , I 2 , Br 2 , and / or mixtures thereof). In particular, ion beams from hundreds of eV to several keV can be extracted with large on-wafer incidence angles (e.g., up to 45 degrees) and beam currents of tens of mA. As an example of device processing, the use of symmetric ribbon beamlet extraction provided by the present embodiment allows for simultaneous processing of vertical trench walls in complex semiconductor structures as the substrate is scanned parallel to the extraction assembly.

[0012] In the following embodiments, the ion beam processing system may include a plasma chamber and an extraction assembly. The extraction assembly may include a plasma plate disposed along a side of the plasma chamber, the plasma plate including an extraction aperture. According to various embodiments of the present disclosure, the plasma plate may be formed from an electrically insulating material. The extraction assembly may include a beam shield formed from an electrically insulating material and disposed in the plasma chamber and facing the extraction aperture. As such, the beam shield may help to divide the extraction aperture into two separate sub-apertures. The extraction assembly may include a shielding electrode including a conductive thin film disposed on a surface of the beam shield outside the plasma chamber, and an extraction electrode including a conductive thin film disposed on a surface of the plasma plate outside the plasma chamber. In certain embodiments, the shielding electrode may be covered by a first dielectric coating covering the shielding electrode and the surface of the beam shield, and the extraction electrode may be covered by a second dielectric coating covering the extraction electrode and the surface of the beam plasma plate. As described in the embodiments below, this arrangement facilitates the generation of high angle ion beams through the secondary apertures, where the high angle ion beams define large angles of incidence, such as 30 degrees or more, with respect to a normal to the plane of the plasma plate.

[0013] The extraction aperture in the plasma plate may have, for example, an elongated shape that facilitates extraction of a pair of ribbon ion beams or ribbon ion beamlets and directs the ribbon ion beamlets at a wide angle relative to a substrate aligned parallel to the plane of the plasma plate. As used herein, the term "wide angle relative to the substrate" may be greater than 30 degrees relative to the normal (perpendicular) to the plane of the substrate.

[0014] Turning now to FIG. 1, a vertical cross-section of a processing apparatus consistent with an embodiment of the present disclosure is shown. The processing system 100 includes a plasma chamber 102, a process chamber 103, and an extraction assembly 130, as described in more detail below. The processing system 100 further includes a pulsed voltage source 124 electrically coupled to generate a bias voltage between the extraction electrode 114 and the plasma chamber 102. As such, the processing system 100 serves as an ion beam processing system for generating an ion beam for processing a substrate 122 disposed proximate to the extraction electrode 114. The plasma chamber 102 may serve as a plasma source for generating a plasma 132 in the plasma chamber 102 by any suitable approach. For example, the plasma chamber 102 may be referenced to ground potential through a conductive wall 134. The ionizable (ion) species of interest may be generated in the plasma 132 by inductively coupling rf power generated by an rf power source (not shown separately) from an rf antenna 136 through a dielectric window 104 to the working gas. Other known means of generating the plasma are possible.

[0015] As shown in FIG. 1, the extraction assembly 130 may include a plasma plate 106 disposed along the side of the plasma chamber 102, where the plasma plate 106 is an Al 2 O 3The plasma plate 106 may be formed from an electrical insulator, such as (alumina), quartz, AlN, or other suitable electrically insulating material. The plasma plate 106 may define an extraction aperture 138 extending along the x-axis of the illustrated Cartesian coordinate system (note that the x-axis generally extends perpendicularly into the plane of the page). As such, the extraction aperture 138 may define a space through which ions from the plasma chamber 102 may pass. The extraction assembly 130 may further include an extraction electrode 114 formed from a thin film of conductive material (e.g., up to 1 millimeter thick) disposed on a face of the plasma plate 106 outside the plasma chamber 102. The extraction electrode 114 may be covered with a first dielectric coating 115 that forms a layer of a chemically inert dielectric material covering the extraction electrode 114 and the face of the plasma plate 106. Collectively, the plasma plate 106, the extraction electrode 114, and the first dielectric coating 115 may be referred to as a "plasma plate assembly."

[0016] The extraction assembly 130 may also include a beam shield 108 formed, for example, from an insulating material. In the arrangement of FIG. 1, when a negative voltage is applied to the substrate 122 (or to the substrate plate 120) relative to the plasma chamber 102 in the presence of the plasma 132, a plasma meniscus is formed at a slit (sub-aperture) formed between the extraction aperture 138 and the beam shield 108. In various embodiments, the beam shield 108 may be symmetrically positioned above the extraction aperture 138 to allow for the formation and extraction of two symmetric ion beamlets 112. Ion beam processing of the substrate 122 is performed by scanning the substrate 122 in the y-direction and may also include rotating the substrate about the z-axis. In various non-limiting embodiments, depending on the electrical conductivity of the substrate 122 (thick or thin oxide), the ion beamlets 112 may be extracted as a pulsed ion beam, where the pulse frequency and duty cycle may be adjusted to target values ​​in the range of 10-50 kHz and 10-100%, respectively, to avoid charging up of the substrate. Advantageously, the use of dielectric materials for the extraction electrode 114 and the beam shield 108 facilitates their use in the highly reactive plasmas used to generate ionic and radical species.

[0017] The extraction assembly 130 may also include a biasable shield electrode 110. As shown in FIG. 1, the shield electrode 110 is formed from a thin film (e.g., up to 1 millimeter thick) of conductive material disposed on the surface of the beam shield 108 outside the plasma chamber 102. The shield electrode 110 may be covered with a second dielectric coating 117 that forms a layer of chemically inert dielectric material covering the shield electrode 110 and the surface of the beam shield 108. Collectively, the beam shield 108, the shield electrode 110, and the second dielectric coating 117 may be referred to as a "shield assembly." As shown mostly in FIG. 1, the beam shield 108 and the plasma plate 106 are not coplanar, but may be considered to define a lower boundary between the inside of the plasma chamber 102 and the outside of the plasma chamber 102. Thus, the shield electrode 110 may be considered to be outside the plasma chamber 102, regardless of whether it is disposed above the plasma plate 106 or not.

[0018] In some non-limiting embodiments, the height of the extraction apertures 138 along the y-direction may vary. In various embodiments of the present disclosure, the plasma plate 106, the extraction electrode 114, and the substrate 122 may be parallel to one another and to the XY plane. Thus, the plane of the plasma plate 106 may be considered to be a plane that is parallel to the XY plane and generally parallel to the scanning direction (y-direction) of the substrate 122.

[0019] The extraction aperture 138 may be symmetrically aligned with respect to the shield electrode 110 and the beam shield 108, thus establishing symmetry of the two ion beamlets 112 extracted from the slit between the beam shield 108 and the plasma plate 106. In some embodiments, the beam shield 108, shield electrode 110, and extraction aperture 138 may be extended to extend 350 mm to 400 mm in the x-direction, allowing for the extraction of a uniform ribbon beamlet 300 mm wide (in the x-direction).

[0020] According to various non-limiting embodiments, biasable elements of the extraction assembly 130, such as the shielding electrode 110 and the extraction electrode 114, may be set to the same potential as the substrate 122. This configuration advantageously means that the substrate 122 is not part of the extraction assembly 130. Notably, because the substrate 122 is at the same potential as the shielding electrode 110 and the extraction electrode 114, there is no potential difference between the substrate 122 and the extraction electrode 114 or the shielding electrode 110, and as a result, there is no electric field.

[0021] Thus, the relative position of the substrate 122 with respect to the extraction assembly 130, such as the extraction electrode 114 and the plasma plate 106, does not affect the ion angular distribution of the ion beam extracted through the extraction assembly 130. Under this condition, the location of the substrate along the Z axis can be varied from 5 mm to 20 mm or more, thereby significantly reducing contamination of the plasma chamber from material sputtered and / or chemically etched from the substrate. In other words, contamination can be reduced by positioning the substrate with a greater separation from the extraction assembly along the Z axis, if desired, because the greater the separation, the smaller the solid angle through which the extraction aperture "sees" the wafer, resulting in less contamination.

[0022] To be electrically biasable, the shielding electrode 110 and the extraction electrode 114 may be constructed of a thin film (e.g., up to 1 millimeter thick in the z-direction) of a conductive material (e.g., in some non-limiting embodiments, metals such as aluminum, titanium, copper, molybdenum, tungsten, doped silicon, etc. may be used for these components), as described above. Metal contamination is reduced because these components are not exposed to ion beam bombardment, as described in more detail below. According to some embodiments, for better protection against contamination, the electrically biasable components may be coated with a thin dielectric film that surrounds the inner body or portion formed from the conductive material. In one non-limiting embodiment, a suitable dielectric coating is made of a mixture of oxides of yttrium, aluminum, and zirconium, and has a thickness of 100 micrometers. Such dielectric materials are known to provide resistance to etching. In other embodiments, Al 2 O 3 , AlFO, yttrium oxide (Y 2 O 3 ), or zirconium oxide (ZrO 2 ), or a combination thereof may be used as the dielectric coating.

[0023] As is known, the shape and location of the plasma meniscus and the mechanism of ion beam extraction depend on the relative plasma density in a plasma such as plasma 132, which in turn depends on the extraction electric field. When non-conductive materials such as dielectrics are used to fabricate the components of the ion extraction assembly, the physics of ion beam extraction change significantly. This occurs because the plasma sheath, which is the interface between the plasma 132 and the walls of the ion extraction assembly (in this embodiment, the beam shield 108 and the plasma plate 106), is a function of the nature of the walls: insulating or conductive. The pulse frequency (f) determines the ion plasma frequency (f pi ) for pulsed plasmas with a higher TIFF0007580565000001.tif25170, where n, ε 0 , and mi are the plasma density, the elementary charge, the dielectric constant of the vacuum, and the ion mass, where the ions are immobile and the electrons are kept away from the wall by the so-called matrix sheath. In this case, the thickness of the sheath is TIFF0007580565000002.tif25170, where V 0 , k B , and T e λ represents the voltage drop across the sheath, the Boltzmann constant, and the electron temperature, respectively. D The quantity denoted by is is the Debye length given in TIFF0007580565000003.tif25170. For a matrix sheath, depending on the value of the voltage at the wall, the thickness of the sheath can range from a few tens to a hundredth of a Debye length. 9 ~5×10 11 cm -3 At typical plasma densities, the ion plasma frequency is 2 MHz to 25 MHz, much higher than the pulse frequency of the extraction voltage (10 to 50 kHz). In this case, the ions have enough time to be accelerated by the electric field in the sheath, and assuming their motion is collisionless, the thickness of the sheath is given by Child's law: TIFF0007580565000004.tif23170Assuming an electron temperature of 3.5 eV, the sheath thickness increases with voltage and with the inverse of the plasma density, varying from a fraction of a millimeter to approximately 20 millimeters for the range of interest.

[0024] According to various embodiments, the ion beam of the present embodiment may be extracted as a pulsed ion beam, as described above. The extraction voltage system may include a pulse component, such as a circuit that pulses the extraction voltage on and off according to the target pulse period and duty cycle. When the ion beam current is small, the pulse duty cycle may be 100%, i.e., ions are continuously extracted. In particular, the pulse period and duty cycle may be determined to facilitate the extraction of an angled ion beam, as discussed below. Because the beam shield 108 and plasma plate 106 components may be formed from dielectric materials, the pulsing of the ion beam may be determined to take into account the time-dependent evolution of the plasma sheath.

[0025] Turning to Figures 2A-D, the evolution of electron and ion distribution as a function of time is shown in ZY space according to an embodiment of the present disclosure. In the simulation shown, the voltage on the substrate (position represented by the vertical line at z=2.5 cm) is pulsed at -1 kV voltage with a pulse frequency of 20 kHz and a duty cycle of 50%. The beam shield and plasma plate components are shown diagrammatically as bright vertically elongated rectangles. The beam shield and plasma plate are modeled as being made of a dielectric material (quartz), which is allowed to electrostatically charge up. Figures 2A and 2B show the electron and ion distributions, respectively, 1 μs after the start of the applied negative voltage pulse. Because quartz allows the transmission of electric field lines, at the start of the pulse (1 μs), a high voltage drop occurs in the sheath, resulting in a fairly thick (~6 mm) sheath. The electric field near the extraction slit is oriented perpendicular (along the z-direction) to the plasma plate and the beam shield, resulting in very few, if any, ions being extracted (see ion distribution in FIG. 2B).

[0026] 2C and 2D, as the plasma sheath evolves over time, ions continue to reach the inner walls of the plasma plate and plasma shield. Without a path to ground, the ions would create an imbalance in the plasma density, a situation that would result in the creation of a bipolar electric field. In this case, an equal flux of electrons and ions would be directed toward the inner walls. TIFF0007580565000005.tif13170In formula, TIFF0007580565000006.tif7170 is the plasma density gradient in the direction perpendicular to the faceplate and shield walls (z direction), and Da is the ambipolar diffusion coefficient as follows: TIFF0007580565000007.tif19170 In formula, μ e,i and D e,i are the mobility and diffusion coefficients of electrons and ions, respectively. As a result of ambipolar diffusion, the sheath thickness decreases (collapses) to the point where a plasma meniscus forms at the extraction slit and the ion beamlets begin to be extracted. This decrease in sheath thickness can be seen in Figures 2C and 2D, where the zy phase space of electrons and ions is shown 4 μs after the start of the negative voltage pulse. In this case, the ion beamlets are easily formed, extracted, and directed to the substrate position, as shown in Figure 2D.

[0027] Thus, according to various embodiments, the duty cycle and frequency of the voltage pulses can be set to provide a given pulse duration that exceeds the time required for the initiation of plasma sheath collapse (plasma sheath collapse period) and extraction of the ion beam. In the above example, assuming a minimum plasma sheath collapse period of 4 μs, a pulse duration of 10 μs or more may be appropriate to ensure proper extraction of the ion beam. At a 50% duty cycle, this pulse duration equates to a pulse period of 20 μs or more, which means that in the scenario of Figures 2A-2D, the voltage pulse frequency can be set to 50 kHz or less to effectively extract ions.

[0028] 3A-3C illustrate an operating scenario of the processing apparatus 100 described above and shown in FIG. 1, and show the beamlets, shape, and electrostatic potential distribution in the extraction region (i.e., the region between the shield electrode 110 and the substrate 122). More specifically, FIGS. 3A-3C illustrate the results of OPERA modeling showing the conductive wall 134 of the plasma chamber 102, the plasma plate 106, the extraction electrode 114, the beam shield 108, the shield electrode 110, and the substrate 122. In the illustrated series of figures, the plasma density and bias voltage remain the same (600 W rf power and −1.5 kV), and the z-distance between the extraction electrode 114 and the substrate 122 increases from 6 mm in FIG. 3A to 10 mm in FIG. 3B to 15 mm in FIG. 3C. As can be seen, the dielectric structures of the extraction assembly 130 pass the electrostatic field potential 140, whereas the metallic structures do not. Thus, electrostatic potential lines 140 extend through the outermost portion of the beam shield 108 that is not covered by the shield electrode 110 (hereinafter "uncovered portion 142"), such uncovered portion 142 having a height (Hh) / 2 in the y-direction as shown in Figure 3B. Similarly, electrostatic potential lines 140 extend through the portion of the plasma plate 106 that is not covered by the extraction electrode 114 (hereinafter "uncovered portion 144"), such uncovered portion 144 having a height r in the y-direction as shown in Figure 3B. Ions extracted through the aperture s (see Figure 3B) at a natural angle (given by the geometry of the extraction assembly 130) will generally diverge as dictated by the ratio of the height of the uncovered portions 142, 144, the bias voltage, and, to a lesser extent, the ion beam current. As a result, and due to the geometric symmetry of the extraction assembly, the ion beamlets 112 have an ion angular distribution characterized by an angle of + / -θ relative to the normal to the plane of the substrate 122 (relative to the Z-axis) (see Figure 3C).

[0029] The ion angular distributions for the arrangements illustrated in Figures 3A-3C are shown in the graphs illustrated in Figures 4A-4C, respectively. When the shield electrode 110, the extraction electrode 114, and the substrate 122 are maintained at the same electrostatic potential, the electric field between the ion source and the substrate 122 is almost entirely concentrated in the extraction slit area (see the distribution of equipotential lines). As a result, the ion angular distributions of the extracted ion beamlets 112 are not affected by the length of the z-gap, their characteristics are quasi-identical and have the same average angle (40 degrees), and due to low space charge effects, there is only a small increase in angular divergence (10 degrees, 11 degrees, and 12 degrees) as the z-distance between the extraction electrode 114 and the substrate 122 increases from 6 mm to 10 mm and from 10 mm to 15 mm. Thus, the substrate 122 can be moved away from the extraction assembly if necessary, such as to minimize contamination of the plasma chamber 102 with material etched from the substrate 122, and the average angle of the ion beamlets 112 relative to the substrate 122 is maintained.

[0030] 5, an alternative embodiment of the processing system 100 is shown implemented with a second pulsed voltage source 150 (in addition to the pulsed voltage source 124 described above, hereafter referred to as the "first pulsed voltage source 124"). The second pulsed voltage source 150 may be coupled to the shielding electrode 110 to differentially bias the shielding electrode 110 with respect to the extraction electrode 114. The second pulsed voltage source 150 may be bipolar to facilitate negative or positive biasing on the extraction electrode 114. A phase controller 152 may be connected between the first pulsed voltage source 124 and the second pulsed voltage source 150 to ensure that the proper phase between them is maintained.

[0031] 6A-6F illustrate an operating scenario of the differentially biased embodiment of the processing system 100 shown in FIG. 5 and show the beamlets, shape, and electrostatic potential distribution in the extraction region. More specifically, FIG. 6A-6F illustrate the results of OPERA modeling showing the conductive wall 134 of the plasma chamber 102, the plasma plate 106, the extraction electrode 114, the beam shield 108, the shield electrode 110, and the substrate 122. In the illustrated series of figures, the plasma density, the bias voltage applied by the first pulsed voltage source 124, and the z-distance between the extraction electrode 114 and the substrate 122 all remain the same (600W rf power, -1.5kV, and 15mm, respectively), and the bias voltage applied to the shield electrode 110 by the second pulsed voltage source 150 decreases in increments of 300V, from 1.8kV in FIG. 6A to 300V in FIG. 6D. As can be seen, as the relative voltage bias increases, the distribution of electrostatic potential lines 140 in the extractor slit region becomes less dense and more parallel (i.e., closer to parallel) toward the substrate, resulting in a reduction in the angular divergence of beamlets 112 and their footprint on the substrate.

[0032] The ion angular distributions of the arrangements illustrated in Figures 6A-6F are shown in the graphs illustrated in Figures 7A-7F, respectively. As a result of the differential bias applied to the shielding electrodes 110, the average angle of the ion beamlets 112 relative to the normal to the plane of the substrate 122 (i.e., relative to the Z-axis) may decrease from 52 degrees in Figure 7A to 8 degrees in Figure 7E, and then the average angle may be -6 degrees beyond the normal in Figure 7F. Thus, the disclosed arrangement facilitates a tuning range of nearly 60 degrees. Additionally, the angular divergence of the beamlets 112 may decrease from 15 degrees at ΔV=-300V (Figures 6A and 7A) to 2.8 degrees at ΔV=1200V (Figures 6F and 7F).

[0033] 8A and 8B show a portion of the processing system 100 including a perspective view and an exploded view, respectively, of the plasma chamber 102 and the extraction assembly 130 described above. The extraction assembly 130 may include a plasma plate 106 and a beam shield 108, which may extend all the way behind the extraction aperture 138 and may be secured to a rear surface of the plasma plate 106, such as by mechanical fasteners (not shown) that extend through respective mounting holes 160a, 160b, and 162a, 162b formed in the beam shield 108 and the plasma plate 106. The plasma plate 106 may cover the front opening of the plasma chamber 102 and may be secured to the front surface of the plasma chamber 102, such as by mechanical fasteners (not shown) that extend through respective mounting holes 164a, 164b and 166a, 166b formed in the plasma plate 106 and the plasma chamber 102. The extraction electrode 114 disposed on the front surface of the plasma plate 106 and surrounding the extraction aperture 138 may be covered by a first dielectric coating 115, and as such is shown by a dashed outline in FIG. 8B. The shield electrode 110 disposed on the front surface of the beam shield 108 is covered by a second dielectric coating 117, and as such is shown by a dashed outline in FIG. 8B.

[0034] 9A-9C are a series of perspective views illustrating a method for fabricating the plasma plate assembly of the extraction assembly 130. FIG. 10 is a flow diagram illustrating the same method. Referring to FIG. 9A and block 200 in FIG. 10, the plasma plate 106 can be manufactured and provided. In various examples, the plasma plate 106 can be made of Al 2 O 3The plasma plate 106 may be machined from a plate of electrically insulating material such as (alumina), quartz, AlN, or other suitable electrical insulator. The disclosure is not limited in this respect. The plasma plate 106 may define an extraction aperture 138 extending along the X-axis of the Cartesian coordinate system shown. Optionally, a recess or pocket 170 may be formed (e.g., machined) in the front surface of the plasma plate 106, the recess 170 having a size and shape adapted to accommodate an extraction electrode 114, described further below. In a non-limiting example, the recess 170 may have a depth in the range of 0.2 millimeters to 0.3 millimeters, as measured along the Z-axis.

[0035] 9B and block 210 in FIG. 10, the extraction electrode 114 may be formed or disposed on the front surface of the plasma plate 106 surrounding the extraction aperture 138. In various examples, the extraction electrode 114 may be formed from a conductive material such as aluminum, nickel, titanium, copper, molybdenum, tungsten, or doped silicon, and may be printed, sprayed, or adhered onto the front surface of the plasma plate 106. In a non-limiting example, the extraction electrode 114 may have a thickness in the range of 0.2 millimeters to 0.3 millimeters, as measured along the Z axis. When the recess 170 is formed in the front surface of the plasma plate 106 as described above (see FIG. 9A), the recess 170 may be filled with a conductive material, such as by spraying a material into the recess 170, to form the extraction electrode 114.

[0036] 9C and block 220 in FIG. 10, a first dielectric coating 115 may be applied to the plasma plate 106 and the extraction electrode 114. The first dielectric coating 115 may cover the front surface of the plasma plate 106 and the extraction electrode 114. In various embodiments, the first dielectric coating 115 may be Al 2 O 3 , Y 2 O 3 , ZrO 2, or a combination thereof, and may be applied using a plasma spray process. The disclosure is not limited in this respect. A small portion of the extraction electrode 114 may be masked during application of the first dielectric coating 115 to provide an exposed connector area 172 not covered by the first dielectric coating 115, for example, to facilitate electrical connection of the extraction electrode 114 to the first pulsed voltage source 124, as described above.

[0037] 11A-11C are a series of perspective views illustrating a method for fabricating the shielding assembly of the extraction assembly 130. FIG. 12 is a flow diagram illustrating the same method. Referring to FIG. 11A and block 300 in FIG. 12, the beam shielding portion 108 can be fabricated and provided. In various examples, the beam shielding portion 108 can be made of Al. 2 O 3 The beam blocking portion 108 may be machined from a plate of electrically insulating material such as (alumina), quartz, AlN, or other suitable electrical insulator. The disclosure is not limited in this respect. The beam blocking portion 108 may extend along the X-axis of the Cartesian coordinate system shown.

[0038] 11B and block 310 in FIG. 10, the shielding electrode 110 may be formed or disposed on the front surface of the beam shielding portion 108. In various examples, the shielding electrode 110 may be formed from a conductive material such as aluminum, nickel, titanium, copper, molybdenum, tungsten, or doped silicon, and may be printed, sprayed, or adhered onto the front surface of the beam shielding portion 108. In a non-limiting example, the shielding electrode 110 may have a thickness in the range of 0.2 millimeters to 0.3 millimeters as measured along the Z-axis.

[0039] 11C and block 320 in FIG. 12, a second dielectric coating 117 may be applied to the beam shield 108 and the shield electrode 110. The second dielectric coating 117 may cover the front surface of the beam shield 108 and the shield electrode 110. In various embodiments, the second dielectric coating 117 may be Al 2 O 3 , Y 2 O 3 , ZrO 2 , or a combination thereof, and may be applied using a plasma spray process. The disclosure is not limited in this respect. A small portion of the shielding electrode 110 may be masked during application of the second dielectric coating 117 to provide an exposed connector area 174 not covered by the second dielectric coating 117, for example, to facilitate electrical connection of the shielding electrode 110 to the pulsed voltage source 124 (or the second pulsed voltage source 150), as described above.

[0040] This embodiment provides numerous advantages in the art. The first advantage is found in an extraction assembly with a novel combination of low profile conductive electrodes that are sufficiently covered by a dielectric material to facilitate the extraction of ion beamlets with large on-wafer incidence angles (>30 degrees average angle) and reduce metal contamination. A further advantage is the ability to control the ion angle distribution in real time. A further advantage is the ability to reduce contamination of the plasma chamber with sputtered and / or chemically etched material from the substrate by preserving the on-wafer incidence angle of the ion beamlets while allowing the substrate to be pulled away from the plasma chamber. Furthermore, in a compact ion beam system, the substrate is removed from the configuration of the extraction assembly while maintaining a simple diode electrostatic extraction process. A further advantage is the simultaneous biasing of the substrate and the biasable electrode using the same power supply, simplifying cost and design complexity. A further example of an advantage of this embodiment is the ability to provide a differential bias to the shielding electrode with respect to the extraction electrode and the substrate using a simple low voltage power supply floating on the high voltage power supply.

[0041] The present disclosure should not be limited in scope by the specific embodiments described herein. Indeed, in addition to those described herein, various other embodiments and modifications of the present disclosure will be apparent to those skilled in the art from the foregoing description and the accompanying drawings. Thus, such other embodiments and modifications are intended to be within the scope of the present disclosure. Furthermore, although the present disclosure is described herein in the context of a particular implementation in a particular environment for a particular purpose, those skilled in the art will recognize that its usefulness is not limited thereto, and the present disclosure may be beneficially implemented in any number of environments for any number of purposes. Thus, the claims set forth below should be construed in light of the full scope and spirit of the present disclosure as described herein.

Claims

1. A plasma chamber; a plasma plate formed from an electrically insulating material and juxtaposed with the plasma chamber, the plasma plate defining an extraction aperture; a beam shield formed from an electrically insulating material and disposed within the plasma chamber and facing the extraction aperture; a shield electrode disposed on a surface of the beam shield outside the plasma chamber; an extraction electrode disposed on a surface of the plasma plate outside the plasma chamber; The ion beam processing system, wherein no electrode is provided within the extraction aperture.

2. 2. The ion beam processing system of claim 1, wherein the shield electrode is formed from a conductive material and is covered by a first dielectric coating, and the extraction electrode is formed from a conductive material and is covered by a second dielectric coating.

3. The ion beam processing system of claim 2 , wherein a portion of the shield electrode is not covered by the first dielectric coating to facilitate electrical connection of the shield electrode to a pulsed voltage source.

4. The ion beam processing system of claim 2 , wherein a portion of the extraction electrode is not covered by the second dielectric coating to facilitate electrical connection of the extraction electrode to a pulsed voltage source.

5. 2. The ion beam processing system of claim 1, wherein the shield electrode is flat and has a thickness measured in a direction perpendicular to a front surface of the beam shield, the thickness being less than 1 millimeter.

6. 2. The ion beam processing system of claim 1, wherein said extraction electrode is flat and has a thickness measured in a direction perpendicular to a front surface of said plasma plate, said thickness being less than 1 millimeter.

7. The ion beam processing system of claim 1 , wherein an outermost end surface of the shield electrode is recessed relative to an outermost end surface of the beam shielding portion in a direction parallel to a front surface of the beam shielding portion.

8. 2. The ion beam processing system of claim 1, wherein an outermost end surface of the extraction electrode is recessed in a direction parallel to a front surface of the plasma plate relative to an end surface of the plasma plate that bounds the extraction aperture.

9. The ion beam processing system of claim 1 , further comprising a pulsed voltage source electrically coupled to the plasma chamber and to the extraction electrode to generate a bias voltage between the extraction electrode and the plasma chamber.

10. The ion beam processing system of claim 9 , wherein the pulsed voltage supply comprises a pulse component for generating a pulsed bias voltage between the extraction electrode and the plasma chamber.

11. 10. The ion beam processing system of claim 9, further comprising a process chamber for housing a substrate, wherein the pulsed voltage source is electrically coupled to the plasma chamber on a first side and electrically coupled to the extraction electrode, the shielding electrode, and the substrate on a second side.

12. 10. The ion beam processing system of claim 9, wherein the pulsed voltage source is a first pulsed voltage source, the ion beam processing system further comprising a second pulsed voltage source electrically coupled to the shield electrode for differentially biasing the shield electrode relative to the extraction electrode.

13. A plasma chamber; a plasma plate formed from an electrically insulating material and juxtaposed with the plasma chamber, the plasma plate defining an extraction aperture; a beam shield formed from an electrically insulating material and disposed within the plasma chamber and facing the extraction aperture; a shielding electrode formed from a conductive material and covered by a first dielectric coating and disposed on a surface of the beam shield outside the plasma chamber, the shielding electrode being flat and having a thickness measured in a direction perpendicular to a front surface of the beam shield, the thickness of the shielding electrode being less than 1 millimeter; an extraction electrode formed from a conductive material and covered by a second dielectric coating and disposed on a surface of the plasma plate outside the plasma chamber, the extraction electrode being flat and having a thickness measured in a direction perpendicular to a front surface of the plasma plate, the thickness of the extraction electrode being less than 1 millimeter; a pulsed voltage source electrically coupled to the plasma chamber and to the extraction electrode to generate a bias voltage between the extraction electrode and the plasma chamber; The ion beam processing system, wherein no electrode is provided within the extraction aperture.

14. 1. A method of fabricating a plasma plate assembly for an ion beam processing system, comprising: providing a plasma plate formed from an electrically insulating material, said plasma plate defining an elongated extraction aperture; applying a conductive material to an outer surface of the plasma plate surrounding the extraction apertures to form an extraction electrode, the extraction electrode being flat and having a thickness measured in a direction perpendicular to the outer surface of the plasma plate of less than 1 millimeter; applying a dielectric coating to the plasma plate and the extraction electrode, the dielectric coating covering the outer surface of the plasma plate and the extraction electrode; The method, wherein no electrodes are provided within the extraction apertures.

15. 15. The method of claim 14, wherein applying a dielectric coating to the plasma plate and the extraction electrode includes masking a portion of the extraction electrode to provide an exposed connector area not covered by the dielectric coating to facilitate electrical connection of the extraction electrode to a pulsed voltage source.

16. 15. The method of claim 14, further comprising forming a recess in the outer surface of the plasma plate to accommodate the extraction electrode prior to applying the conductive material to the outer surface of the plasma plate.

17. 1. A method of fabricating a shield assembly for an ion beam processing system, comprising: providing a beam shield formed from an electrically insulating material; applying a conductive material to a front surface of the beam shield to form a shield electrode, the shield electrode being flat and having a thickness of less than 1 millimeter measured in a direction perpendicular to the front surface of the beam shield, the front surface facing an extraction aperture through which the ion beam is extracted; applying a dielectric coating to the beam shield and the shield electrode, the dielectric coating covering the front surface of the beam shield and the shield electrode; The method, wherein no electrodes are provided within the extraction apertures.

18. 20. The method of claim 17, wherein applying a dielectric coating to the beam shield and the shield electrode includes masking a portion of the shield electrode to provide an exposed connector area not covered by the dielectric coating to facilitate electrical connection of the shield electrode to a pulsed voltage source.

19. The method according to claim 17 , wherein an outermost end surface of the shield electrode is recessed relative to an outermost end surface of the beam shielding portion in a direction parallel to a front surface of the beam shielding portion.

Citation Information

Patent Citations

  • Microwave ion source

    JP1988257166A

  • Fine machining method using charged particle and device thereof

    JP1996222175A

  • Microwave ion source

    JP1998125246A

  • Microwave ion source for oxygen-ion beam

    JP2000340127A

  • Control of Ion Angular Distribution of Ion Beam Using Hidden Deflecting Electrodes

    JP2017533542A