Semiconductor device manufacturing method
By forming a semiconductor device with a silicon-nitrogen ratio less than 4/7 and using an N-doped amorphous silicon getter layer, metal atoms are efficiently removed from semiconductor layers, enhancing gettering performance and streamlining the manufacturing process.
Patent Information
- Application Number
- JP2021046203
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-19
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-03-19
AI Technical Summary
Existing methods for forming a getter layer in semiconductor devices are inadequate for effectively removing metal atoms from semiconductor layers.
A method involving the formation of a semiconductor device with a first layer containing silicon and nitrogen atoms, where the ratio of nitrogen to silicon is less than 4/7, and using a getter layer composed of an N-doped amorphous silicon layer to move and remove metal atoms through heat treatment and subsequent etching processes.
This approach effectively reduces the concentration of metal atoms in the semiconductor layer, improving the gettering performance and simplifying the manufacturing process by allowing continuous step execution within a single chamber.
Smart Images

Figure 0007581098000001 
Figure 0007581098000002 
Figure 0007581098000003
Abstract
Description
[Technical field]
[0001] An embodiment of the present invention relates to a method for manufacturing a semiconductor device. [Background technology]
[0002] When removing metal atoms from a semiconductor layer into a layer called a getter layer, it is desirable to form a suitable getter layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 3425392 [Patent Document 2] JP 2001-223219 A [Patent Document 3] JP 2004-128421 A [Patent Document 4] JP 2009-033123 A Summary of the Invention [Problem to be solved by the invention]
[0004] The present invention relates to a method for manufacturing a semiconductor device that is capable of forming a layer suitable for removing metal atoms in a semiconductor layer. [Means for solving the problem]
[0005] According to one embodiment, a method for manufacturing a semiconductor device includes forming a semiconductor layer containing a plurality of metal atoms on a substrate, and forming a first layer containing a plurality of silicon atoms and a plurality of nitrogen atoms on the semiconductor layer. The method further includes transferring at least a portion of the metal atoms in the semiconductor layer into the first layer, and removing the first layer after transferring at least a portion of the metal atoms in the semiconductor layer into the first layer. Furthermore, a ratio of the number of nitrogen atoms to the number of silicon atoms and nitrogen atoms in the first layer is less than 4 / 7. [Brief description of the drawings]
[0006] [Figure 1] 1 is a perspective view showing a structure of a semiconductor device according to a first embodiment; [Diagram 2] 1 is a cross-sectional view showing a structure of a semiconductor device according to a first embodiment. [Diagram 3] 6 is a cross-sectional view (1 / 6) showing the method for manufacturing the semiconductor device according to the first embodiment. [Figure 4] 6 is a cross-sectional view (2 / 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Diagram 5] 6 is a cross-sectional view (3 / 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 6] 4 is a cross-sectional view (4 / 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 7] 5 is a cross-sectional view (5 / 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 8] 6 is a cross-sectional view (6 / 6) illustrating the method for manufacturing the semiconductor device according to the first embodiment. [Figure 9] 11 is a cross-sectional view (1 / 2) showing a method for manufacturing a semiconductor device according to a modified example of the first embodiment. [Figure 10] 11 is a cross-sectional view (2 / 2) showing a method for manufacturing a semiconductor device according to a modified example of the first embodiment. FIG. [Figure 11] 11 is a cross-sectional view (1 / 4) showing a method for manufacturing a semiconductor device according to a second embodiment. [Figure 12] 11 is a cross-sectional view (2 / 4) showing the method for manufacturing the semiconductor device according to the second embodiment. [Figure 13] 11 is a cross-sectional view (3 / 4) illustrating a method for manufacturing a semiconductor device according to a second embodiment. [Figure 14] 11 is a cross-sectional view (4 / 4) illustrating the method for manufacturing the semiconductor device according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In Fig. 1 to Fig. 14, the same components are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0008] (First embodiment) Fig. 1 is a perspective view showing the structure of a semiconductor device according to a first embodiment. The semiconductor device in Fig. 1 is, for example, a three-dimensional semiconductor memory.
[0009] 1 includes a core insulating film 1, a channel semiconductor layer 2, a tunnel insulating film 3, a charge storage layer 4, a block insulating film 5, and an electrode layer 6. The block insulating film 5 includes an insulating film 5a and an insulating film 5b. The electrode layer 6 includes a barrier metal layer 6a and an electrode material layer 6b.
[0010] In the semiconductor device of Fig. 1, a plurality of electrode layers and a plurality of insulating layers are alternately stacked on a substrate, and a plurality of memory holes are provided in these electrode layers and insulating layers. Fig. 1 shows one of these electrode layers, an electrode layer 6, and one of these memory holes, a memory hole MH. These electrode layers function as, for example, word lines or selection lines.
[0011] 1 shows an X direction and a Y direction parallel to the surface of the substrate and perpendicular to each other, and a Z direction perpendicular to the surface of the substrate. In this specification, the +Z direction is treated as an upward direction, and the -Z direction is treated as a downward direction. The -Z direction may or may not coincide with the direction of gravity. In FIG. 1, the electrode layer 6 extends in the X direction and the Y direction, and the memory hole MH extends in the Z direction.
[0012] The core insulating film 1, the channel semiconductor layer 2, the tunnel insulating film 3, the charge storage layer 4, and the insulating film 5a are formed in the memory hole MH, and together with the electrode layers, constitute a memory cell transistor (memory cell) and a select transistor of the three-dimensional semiconductor memory.
[0013] An insulating film 5a is formed on the surfaces of the electrode layer and insulating layer in the memory hole MH, and a charge storage layer 4 is formed on the surface of the insulating film 5a. The charge storage layer 4 is provided to store signal charges in the memory cell transistor. A tunnel insulating film 3 is formed on the surface of the charge storage layer 4, and a channel semiconductor layer 2 is formed on the surface of the tunnel insulating film 3. The channel semiconductor layer 2 functions as a channel of the memory cell transistor and the select transistor. A core insulating film 1 is formed in the channel semiconductor layer 2.
[0014] The insulating film 5a is, for example, a SiO2 film (silicon oxide film). The charge storage layer 4 is, for example, a SiN film (silicon nitride film). The tunnel insulating film 3 is, for example, a SiON film (silicon oxynitride film). The channel semiconductor layer 2 is, for example, a polysilicon layer. The core insulating film 1 is, for example, a SiO2 film.
[0015] The insulating film 5b, the barrier metal layer 6a, and the electrode material layer 6b are formed between the adjacent insulating layers, and are formed in this order on the lower surface of the upper insulating layer, the upper surface of the lower insulating layer, and the side surface of the insulating film 5a. The insulating film 5b is, for example, a metal insulating film such as an Al2O3 film (aluminum oxide film). The barrier metal layer 6a is, for example, a TiN film (titanium nitride film). The electrode material layer 6b is, for example, a W (tungsten) layer.
[0016] 2 is a cross-sectional view showing the structure of the semiconductor device according to the first embodiment, and shows the XZ cross section of the memory hole MH in FIG.
[0017] As shown in Fig. 2, the semiconductor device of this embodiment includes a core insulating film 1, a channel semiconductor layer 2, a tunnel insulating film 3, a charge storage layer 4, a block insulating film 5, a plurality of electrode layers 6, a substrate 11, a stacked film 12, and a plurality of insulating layers 13. In Fig. 2, the block insulating film 5 includes an insulating film 5a and a plurality of insulating films 5b, and each electrode layer 6 includes a barrier metal layer 6a and an electrode material layer 6b. The semiconductor device of this embodiment further includes a memory hole MH and an air gap AG.
[0018] The substrate 11 is, for example, a semiconductor substrate such as a Si (silicon) substrate. Like Fig. 1, Fig. 2 shows the X direction and the Y direction which are parallel to the surface of the substrate 11 and perpendicular to each other, and the Z direction which is perpendicular to the surface of the substrate 11.
[0019] The laminated film 12 includes a plurality of electrode layers 6 and a plurality of insulating layers 13 alternately laminated on the substrate 11. The laminated film 12 may be formed directly on the substrate 11, or may be formed on the substrate 11 via another layer. The insulating layer 13 is, for example, a SiO2 film. The barrier metal layer 6a and the electrode material layer 6b in each electrode layer 6 are formed in order between the insulating layers 13 adjacent to each other in the Z direction, with an insulating film 5b interposed therebetween.
[0020] The insulating film 5a, the charge storage layer 4, the tunnel insulating film 3, the channel semiconductor layer 2, and the core insulating film 1 are formed in this order on the side surface of the laminated film 12 within the memory hole MH. The insulating film 5a, the charge storage layer 4, the tunnel insulating film 3, and the channel semiconductor layer 2 of this embodiment are further formed in this order on the upper surface of the laminated film 12 outside the memory hole MH. Moreover, the core insulating film 1 of this embodiment includes an air gap AG filled with air.
[0021] 3 to 8 are cross-sectional views showing the method for manufacturing the semiconductor device of the first embodiment.
[0022] First, a laminated film 12' is formed on a substrate 11 (FIG. 3). The laminated film 12' is formed by alternately forming a plurality of insulating layers 13 and a plurality of sacrificial layers 15 on the substrate 11. The sacrificial layers 15 are, for example, SiN films. The sacrificial layers 15 are formed to replace the electrode layers 6 in a process described below. In the process shown in FIG. 3, the process of replacing the sacrificial layers 15 with the electrode layers 6 may be omitted by forming the electrode layers 6 instead of the sacrificial layers 15. The insulating layers 13 are an example of a first film, and the sacrificial layers 15 and the electrode layers 6 are examples of a second film.
[0023] Next, a memory hole MH is formed in the laminated film 12' by lithography and RIE (Reactive Ion Etching) (FIG. 4). The memory hole MH is an example of an opening.
[0024] Next, the insulating film 5a, the charge storage layer 4, the tunnel insulating film 3, and the channel semiconductor layer 2 are formed in this order on the entire surface of the substrate 11 (FIG. 5). As a result, the insulating film 5a, the charge storage layer 4, the tunnel insulating film 3, and the channel semiconductor layer 2 are formed in this order on the side surface of the laminated film 12' in the memory hole MH and on the upper surface of the laminated film 12' outside the memory hole MH. The channel semiconductor layer 2 of this embodiment is formed so as to include a plurality of metal atoms 21. FIG. 5 shows a schematic diagram of the metal atoms 21 included in the channel semiconductor layer 2. The metal atoms 21 are, for example, Fe (iron) atoms, Ni (nickel) atoms, or Cu (atoms). The channel semiconductor layer 2 is an example of a semiconductor layer.
[0025] Next, the core insulating film 1 is formed on the entire surface of the substrate 11, so that the core insulating film 1 is formed on the side surface of the channel semiconductor layer 2 in the memory hole MH and on the upper surface of the channel semiconductor layer 2 outside the memory hole MH, and then the core insulating film 1 outside the memory hole MH is removed (FIG. 5). As a result, the core insulating film 1 is buried in the memory hole MH. In this embodiment, the core insulating film 1 is formed so as to include the air gap AG, but it may be formed so as not to include the air gap AG.
[0026] Next, a getter layer 14 is formed on the entire surface of the substrate 11 (FIG. 5). As a result, the getter layer 14 is formed on the channel semiconductor layer 2 and the core insulating film 1 above the stacked film 12 and the memory hole MH. The getter layer 14 of this embodiment is formed only outside the memory hole MH out of inside and outside the memory hole MH. The getter layer 14 is an example of the first layer.
[0027] The getter layer 14 contains, for example, a plurality of Si atoms and a plurality of N (nitrogen) atoms. In this case, it is preferable that the getter layer 14 contains Si atoms and N atoms in a Si-rich form compared to a silicon nitride film represented by the composition formula "Si3N4". The ratio of the number of N atoms to the number of Si atoms and N atoms in the getter layer 14 of this embodiment is, for example, 40% or less. When the number of Si atoms in the getter layer 14 is represented by K1 and the number of N atoms in the getter layer 14 is represented by K2, this condition is expressed by the inequality K2 / (K1+K2)≦0.4. The getter layer 14 of this embodiment is, for example, an amorphous Si layer containing N atoms (N-doped aSi layer), and contains Si atoms and N atoms so as to satisfy this inequality. Furthermore, when the getter layer 14 of the present embodiment contains Si atoms and N atoms in a Si-rich form compared to a silicon nitride film represented by the composition formula "Si3N4", K2 / (K1+K2)<4 / 7 holds.
[0028] The getter layer 14 is formed by, for example, LPCVD (Low Pressure Chemical Vapor Deposition). In this case, it is preferable to form the getter layer 14 by controlling the ratio of the flow rate of the source gas for N atoms to the flow rate of the source gas for Si atoms to 1:5 or less (for example, 1:5 to 1:20) in the chamber of the LPCVD apparatus. This makes it possible to form the getter layer 14 that satisfies the above inequality. The source gas for N atoms is, for example, NH3 (ammonia) gas. The source gas for Si atoms is, for example, SiH4 (monosilane) gas. The getter layer 14 of this embodiment is used to remove the metal atoms 21 in the channel semiconductor layer 2 to the getter layer 14 by gettering.
[0029] Next, a heat treatment is performed to heat the channel semiconductor layer 2 and the like (FIG. 6). This allows at least a part of the metal atoms 21 in the channel semiconductor layer 2 to move into the getter layer 14. As a result, at least a part of the metal atoms 21 in the channel semiconductor layer 2 is removed to the getter layer 14, and the concentration of the metal atoms 21 in the channel semiconductor layer 2 decreases. This heat treatment is also called gettering annealing.
[0030] The heat treatment is performed at a temperature of, for example, 400° C. or higher. This makes it possible to sufficiently reduce the concentration of the metal atoms 21 in the channel semiconductor layer 2.
[0031] The heat treatment may be performed in the same chamber as the one in which the channel semiconductor layer 2 is formed. For example, when the channel semiconductor layer 2 is formed by an LPCVD apparatus, both the formation of the channel semiconductor layer 2 and the heat treatment may be performed in the chamber of the LPCVD apparatus. This makes it possible to continuously perform the steps from the formation of the channel semiconductor layer 2 to the heat treatment in the chamber without carrying the substrate 11 out of the chamber, thereby reducing the number of manufacturing steps of the semiconductor device. In general, the LPCVD apparatus is equipped with a heating means, and the heat treatment can be performed by this heating means.
[0032] The metal atom 21 may be other than an Fe atom, a Ni atom, or a Cu atom. Examples of such metal atoms 21 and 22 include a Co (cobalt) atom, a Sn (tin) atom, a Pb (lead) atom, a Pd (palladium) atom, a Ru (ruthenium) atom, a Rh (rhodium) atom, an Os (osmium) atom, an Ir (iridium) atom, a Pt (platinum) atom, an Au (gold) atom, an Al (aluminum) atom, and an Ag (silver) atom.
[0033] Next, the getter layer 14 is removed (FIG. 7). The getter layer 14 may be removed by wet etching using a chemical solution (e.g., a hot phosphoric acid solution) or by dry etching using a gas (e.g., chlorine). In this embodiment, by removing the getter layer 14, the metal atoms 21 that have migrated into the getter layer 14 are also removed.
[0034] The step (removal step) shown in FIG. 7 may be performed in the same chamber in which the channel semiconductor layer 2 is formed. For example, when the channel semiconductor layer 2 is formed by an LPCVD apparatus, the formation of the channel semiconductor layer 2, the heat treatment, and the removal treatment may be performed in the chamber of the LPCVD apparatus. This makes it possible to continuously perform the steps from the formation of the channel semiconductor layer 2 to the removal treatment in the chamber without carrying the substrate 11 out of the chamber, thereby reducing the number of manufacturing steps of the semiconductor device. For example, the removal treatment can be performed in the LPCVD apparatus by changing the gas supplied into the chamber from a gas for CVD to a gas for etching.
[0035] Next, slits (not shown) are formed in the laminated film 12' by lithography and RIE, and the sacrificial layer 15 is removed by wet etching through the slits (FIG. 8). As a result, a plurality of cavities C are formed between the insulating layers 13 in the laminated film 12'.
[0036] Thereafter, an insulating film 5b, a barrier metal layer 6a, and an electrode material layer 6b are sequentially formed in these cavities C. As a result, a plurality of electrode layers 6 are formed in these cavities C, and a laminated film 12 is formed on the substrate 11 (see FIG. 2). In this manner, the sacrificial layer 15 is replaced with the electrode layer 6, and the semiconductor device of this embodiment is manufactured.
[0037] Hereinafter, still with reference to FIGS. 3 to 8, the method for manufacturing the semiconductor device of this embodiment will be described in further detail.
[0038] Assume that the getter layer 14 contains a plurality of Si atoms and a plurality of B (boron) atoms, a plurality of P (phosphorus) atoms, or a plurality of As (arsenic) atoms. An example of such a getter layer 14 is an amorphous Si layer containing P atoms (P-doped aSi layer). In this case, the etching selectivity between the getter layer 14 and the layer below it becomes small, and there is a risk that the getter layer 14 cannot be removed in the above-mentioned removal step.
[0039] On the other hand, the getter layer 14 of the present embodiment contains, for example, a plurality of Si atoms and a plurality of N atoms. An example of such a getter layer 14 is an amorphous Si layer containing N atoms (N-doped aSi layer). This makes it possible to increase the etching selectivity between the getter layer 14 and the layer below it, and makes it possible to remove the getter layer 14 in the above-mentioned removal step.
[0040] Moreover, according to experiments, when gettering is performed using an N-doped aSi layer, more metal atoms 21 can be removed from the channel semiconductor layer 2 to the getter layer 14 than when gettering is performed using a P-doped aSi layer. Therefore, according to this embodiment, by using an N-doped aSi layer as the getter layer 14, it is possible to improve the gettering performance of the getter layer 14. The reason for this may be, for example, that N atoms are smaller than P atoms, so that N atoms are more likely to enter the Si lattice than P atoms, and that the N concentration is easier to make higher than the P concentration.
[0041] Moreover, the ratio of the number of N atoms to the number of Si atoms and N atoms in the getter layer 14 of this embodiment is, for example, 40% or less, and the heat treatment of this embodiment is performed at a temperature of, for example, 400° C. or more. This makes it possible to realize a suitable getter layer 14 while sufficiently reducing the concentration of metal atoms 21 in the channel semiconductor layer 2.
[0042] 9 and 10 are cross-sectional views showing a method for manufacturing a semiconductor device according to a modification of the first embodiment.
[0043] First, the steps shown in Fig. 3 to Fig. 5 are carried out. However, in the step shown in Fig. 5, a getter layer 16 is formed on the getter layer 14 (Fig. 9). As a result, the structure shown in Fig. 9 is realized. The getter layer 16 contains, for example, a plurality of Si atoms and a plurality of P atoms. An example of such a getter layer 16 is an amorphous Si layer containing P atoms (P-doped aSi layer). The getter layer 16 is an example of the second layer.
[0044] Next, a heat treatment is performed to heat the channel semiconductor layer 2 and the like (FIG. 10). This allows at least a part of the metal atoms 21 in the channel semiconductor layer 2 to move into the getter layers 14 and 16. As a result, at least a part of the metal atoms 21 in the channel semiconductor layer 2 is removed to the getter layers 14 and 16, and the concentration of the metal atoms 21 in the channel semiconductor layer 2 decreases. The heat treatment in FIG. 10 can be performed in the same manner as the heat treatment in FIG. 6.
[0045] Next, the steps shown in Figures 7 and 8 are carried out. However, in the step shown in Figure 7, in addition to the getter layer 14, the getter layer 16 is removed. In this modification, by removing the getter layers 14 and 16, the metal atoms 21 that have migrated into the getter layers 14 and 16 are also removed. Since the getter layer 16 is formed on the getter layer 14, it can be easily removed in the step shown in Figure 7. In this manner, the semiconductor device of this modification is manufactured. The structure of the semiconductor device of this modification is the same as the structure of the semiconductor device of the first embodiment.
[0046] As described above, in this embodiment, the metal atoms 21 in the channel semiconductor layer 2 are removed by using the getter layer 14 containing N atoms (for example, an N-doped aSi layer). Therefore, according to this embodiment, it is possible to remove the metal atoms 21 in the channel semiconductor layer 2 by using a suitable getter layer 14. For example, it is possible to easily remove the getter layer 14 and improve the gettering performance of the getter layer 14.
[0047] Second embodiment 11 to 14 are cross-sectional views showing a method for manufacturing the semiconductor device of the second embodiment.
[0048] First, the steps shown in Figures 3 to 5 are carried out. However, in the step shown in Figure 5, the core insulating film 1 is not formed (Figure 11). As a result, the structure shown in Figure 11 is realized. The getter layer 14 of this embodiment is formed on the side surface of the channel semiconductor layer 2 in the memory hole MH and on the upper surface of the channel semiconductor layer 2 outside the memory hole MH.
[0049] Next, a heat treatment is performed to heat the channel semiconductor layer 2 and the like (FIG. 12). This allows at least a part of the metal atoms 21 in the channel semiconductor layer 2 to move into the getter layer 14. As a result, at least a part of the metal atoms 21 in the channel semiconductor layer 2 is removed to the getter layer 14, and the concentration of the metal atoms 21 in the channel semiconductor layer 2 decreases. The metal atoms 21 in the channel semiconductor layer 2 may be removed to the getter layer 14 in the memory hole MH, or may be removed to the getter layer 14 outside the memory hole MH. The heat treatment in FIG. 12 can be performed in the same manner as the heat treatment in FIG. 6.
[0050] Next, the getter layer 14 is removed (FIG. 13). In this embodiment, by removing the getter layer 14, the metal atoms 21 that have migrated into the getter layer 14 are also removed. The removal process in FIG. 13 can be performed in the same manner as the removal process in FIG. 7.
[0051] Next, the core insulating film 1 is formed on the entire surface of the substrate 11, so that the core insulating film 1 is formed on the side surface of the channel semiconductor layer 2 in the memory hole MH and on the upper surface of the channel semiconductor layer 2 outside the memory hole MH, and then the core insulating film 1 outside the memory hole MH is removed (FIG. 14). As a result, the core insulating film 1 is buried in the memory hole MH. In this embodiment, the core insulating film 1 is formed so as to include the air gap AG, but it may be formed so as not to include the air gap AG.
[0052] Next, slits (not shown) are formed in the laminated film 12' by lithography and RIE, and the sacrificial layer 15 is removed by wet etching through the slits (FIG. 14). As a result, a plurality of cavities C are formed between the insulating layers 13 in the laminated film 12'.
[0053] Thereafter, an insulating film 5b, a barrier metal layer 6a, and an electrode material layer 6b are sequentially formed in these cavities C. As a result, a plurality of electrode layers 6 are formed in these cavities C, and a laminated film 12 is formed on the substrate 11 (see FIG. 2). In this manner, the sacrificial layer 15 is replaced with the electrode layer 6, and the semiconductor device of this embodiment is manufactured. The structure of the semiconductor device of this embodiment is the same as the structure of the semiconductor device of the first embodiment.
[0054] 11 to 14, the method for manufacturing the semiconductor device of this embodiment will be described in further detail below.
[0055] The getter layer 14 of this embodiment is formed not only outside the memory hole MH but also inside the memory hole MH. Therefore, at first glance, it may be considered that the getter layer 14 of this embodiment is more difficult to remove than the getter layer 14 of the first embodiment. However, according to this embodiment, by employing a getter layer 14 containing N atoms (for example, an N-doped aSi layer), it becomes possible to easily remove it.
[0056] As described above, in this embodiment, the metal atoms 21 in the channel semiconductor layer 2 are removed by using a getter layer 14 containing N atoms (for example, an N-doped aSi layer). Therefore, according to this embodiment, similar to the first embodiment, it is possible to remove the metal atoms 21 in the channel semiconductor layer 2 by using a suitable getter layer 14. For example, it is possible to easily remove the getter layer 14 and improve the gettering performance of the getter layer 14.
[0057] The semiconductor device of the first and second embodiments may be a three-dimensional semiconductor memory of a type different from the above-mentioned three-dimensional semiconductor memory, or may be a semiconductor memory other than a three-dimensional semiconductor memory. Furthermore, the semiconductor device of the first and second embodiments may be a semiconductor device other than a semiconductor memory.
[0058] Although some embodiments have been described above, these embodiments are presented only as examples and are not intended to limit the scope of the invention. The novel method described in this specification can be implemented in various other forms. In addition, various omissions, substitutions, and modifications can be made to the form of the method described in this specification without departing from the gist of the invention. The scope of the appended claims and their equivalents are intended to include such forms and modifications that fall within the scope and gist of the invention. [Explanation of symbols]
[0059] 1: core insulating film, 2: channel semiconductor layer, 3: tunnel insulating film, 4: charge storage layer, 5: block insulating film, 5a: insulating film, 5b: insulating film, 6: electrode layer, 6a: barrier metal layer, 6b: electrode material layer, 11: substrate, 12: laminated film, 12': laminated film, 13: insulating layer, 14: getter layer, 15: sacrificial layer, 16: getter layer, 21: Metal atom
Claims
1. forming a semiconductor layer containing a plurality of metal atoms on a substrate; forming a first layer including a plurality of silicon atoms and a plurality of nitrogen atoms on the semiconductor layer by controlling a ratio of a flow rate of a source gas for nitrogen atoms to a flow rate of a source gas for silicon atoms; migrating at least a portion of the metal atoms in the semiconductor layer into the first layer; removing the first layer after at least a portion of the metal atoms in the semiconductor layer are transferred into the first layer; Including, a ratio of the number of nitrogen atoms to the number of silicon atoms and nitrogen atoms in the first layer is smaller than 4 / 7.
2. 2. The method for manufacturing a semiconductor device according to claim 1, wherein the metal atom is an Fe (iron) atom, a Ni (nickel) atom, a Cu (copper) atom, a Co (cobalt) atom, a Sn (tin) atom, a Pb (lead) atom, a Pd (palladium) atom, a Ru (ruthenium) atom, a Rh (rhodium) atom, an Os (osmium) atom, an Ir (iridium) atom, a Pt (platinum) atom, an Au (gold) atom, an Al (aluminum) atom, or an Ag (silver) atom.
3. 3. The method for manufacturing a semiconductor device according to claim 1, wherein the first layer is a silicon layer containing a plurality of nitrogen atoms.
4. 4. The method for manufacturing a semiconductor device according to claim 1, wherein a ratio of the number of nitrogen atoms to the number of silicon atoms and nitrogen atoms in said first layer is 40% or less.
5. 5. The method for manufacturing a semiconductor device according to claim 1, wherein the first layer is formed by controlling a ratio of a flow rate of the source gas for the nitrogen atoms to a flow rate of the source gas for the silicon atoms to be 1:5 or less.
6. forming a plurality of first films and a plurality of second films alternately on the substrate; forming openings in the first and second membranes; forming a charge storage layer in the opening; Further including: The method for manufacturing a semiconductor device according to claim 1 , wherein the semiconductor layer is formed in the opening via the charge storage layer.
7. The method for manufacturing a semiconductor device according to claim 6 , wherein said first layer is formed only outside said opening out of said inside and outside said opening.
8. The method for manufacturing a semiconductor device according to claim 6 , wherein the first layer is formed at least in the opening.
9. The method for manufacturing a semiconductor device according to claim 1 , wherein at least a part of the metal atoms in the semiconductor layer migrate into the first layer by a heat treatment of the semiconductor layer.
10. 10. The method for manufacturing a semiconductor device according to claim 9, wherein the heat treatment is performed at a temperature of 400[deg.] C. or higher.
11. The method for manufacturing a semiconductor device according to claim 1 , wherein the first layer is removed by using a chemical solution or a gas.
12. forming a second layer on the first layer, the second layer being a silicon layer containing a plurality of boron atoms, a plurality of phosphorus atoms, or a plurality of arsenic atoms; migrating at least a portion of the metal atoms in the semiconductor layer into the first and second layers; removing the first and second layers after transferring at least a portion of the metal atoms in the semiconductor layer into the first and second layers; The method for manufacturing a semiconductor device according to claim 1 , further comprising:
13. forming a semiconductor layer containing a plurality of metal atoms on a substrate; forming a first layer containing a plurality of nitrogen atoms on the semiconductor layer; forming a second layer on the first layer, the second layer being a silicon layer containing a plurality of boron atoms, a plurality of phosphorus atoms, or a plurality of arsenic atoms; migrating at least a portion of the metal atoms in the semiconductor layer into the first and second layers; removing the first and second layers after transferring at least a portion of the metal atoms in the semiconductor layer into the first and second layers; A method for manufacturing a semiconductor device comprising the steps of:
14. The method of claim 13 , wherein the first layer includes a plurality of silicon atoms and a plurality of nitrogen atoms.
Citation Information
Patent Citations
Manufacturing method for semiconductor device
JP1998223533A
Production method of semiconductor device
JP1999354448A
Semiconductor wafer and manufacture thereof
JP2000353797A
Manufacturing method of semiconductor device
JP2001223219A
Semiconductor device and its manufacturing method
JP2001250928A