Electrode assembly and battery cell including the same
The electrode assembly with a separation membrane and minimal binder content addresses resistance and manufacturing limitations, enhancing productivity and discharge capacity by ensuring direct contact between active material layers and current collectors.
Patent Information
- Application Number
- JP2023523637
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-10-15
- Filing Date
- 2021-10-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-10-20
AI Technical Summary
Existing secondary battery electrodes manufactured using a dry method face issues with resistance due to the binder acting as a barrier to electron transfer and require separate manufacturing of positive and negative electrodes, leading to reduced productivity.
An electrode assembly is designed with a separation membrane where positive and negative active material layers are attached to its surfaces, using a minimal binder content and omitting separate adhesive layers between current collectors, allowing direct contact for improved electron transfer and simplified manufacturing.
The solution enhances productivity and reduces resistance, resulting in improved discharge capacity, especially in high-rate regions, by minimizing binder content and ensuring direct contact between active material layers and current collectors.
Smart Images

Figure 0007581507000003 
Figure 0007581507000004 
Figure 0007581507000005
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of priority based on Korean Patent Application No. 10-2020-0143427 filed on October 30, 2020, and Korean Patent Application No. 10-2021-0137514 filed on October 15, 2021, and all contents disclosed in the documents of said Korean patent applications are incorporated herein by reference.
[0002] The present invention relates to an electrode assembly and a battery cell including the same, and more particularly, to an electrode assembly having improved productivity and resistance reduction effect and a battery cell including the same. [Background technology]
[0003] Along with technological development and increasing demand for mobile devices, the demand for secondary batteries as an energy source is rapidly increasing. Among such secondary batteries, lithium secondary batteries, which have high energy density and voltage, long cycle life, and low self-discharge rate, have been commercialized and are widely used.
[0004] In particular, secondary batteries have attracted great attention as energy sources for power plants such as electric bicycles, electric vehicles, and hybrid electric vehicles, as well as for mobile devices such as mobile phones, digital cameras, notebook computers, and wearable devices.
[0005] In addition, with the growing interest in environmental issues, much research is being conducted on electric vehicles and hybrid electric vehicles that can replace vehicles that use fossil fuels such as gasoline vehicles and diesel vehicles, which are one of the main causes of air pollution. Nickel metal hydride secondary batteries are mainly used as the power source for such electric vehicles and hybrid electric vehicles, but active research is being conducted on the use of lithium secondary batteries with high energy density and discharge voltage, and some of them are already in the commercialization stage.
[0006] Existing secondary battery electrodes have generally been manufactured using a wet process. However, when manufacturing electrodes using the wet process, a heat treatment process at high temperatures is required, which may damage the metal oxide. Therefore, electrodes manufactured using a dry process have recently been developed.
[0007] 1 is a diagram showing a conventional electrode assembly. Referring to Fig. 1, the conventional electrode assembly includes a positive electrode 10, a negative electrode 20, and a separator 30 interposed between the positive electrode 10 and the negative electrode 20. Here, the positive electrode 10 has a positive electrode active material layer 11 located on a positive electrode current collector 15, and the negative electrode 20 has a negative electrode active material layer 21 located on a negative electrode current collector 25.
[0008] Fig. 2 is a diagram showing a manufacturing process of the electrodes included in the electrode assembly of Fig. 1. Referring to Fig. 2, the positive electrode active material layer 11 is formed in the form of a free-standing film by dry mixing an electrode composition including polytetrafluoroethylene (PTFE) as a binder. At this time, the positive electrode 10 is formed by attaching the positive electrode active material layer 11 to the positive electrode current collector 15 by roll pressing. The same can be said for the negative electrode 20.
[0009] However, when the positive electrode 10 and the negative electrode 20 are manufactured in a dry manner as shown in Fig. 2, due to the characteristics of polytetrafluoroethylene (PTFE), the electrode composition is manufactured in a bonding manner that surrounds the active material through fiberization due to shear force, rather than a chemical bonding method due to high temperature and pressure. In particular, in order to attach the electrode composition to the current collectors 15 and 25 in the form of a free-standing film, a separate binder needs to be additionally applied or coated between the free-standing film and the current collector.
[0010] For example, conventionally, in addition to polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVDF), acrylic binder, etc. have been added to the electrode composition to increase the adhesive strength of the freestanding film, or the adhesive binder has been coated on the current collectors 15, 25 in advance to increase the adhesive strength of the current collectors 15, 25. In this case, the adhesive binder has been coated on the current collectors 15, 25 using a slurry coating method such as general bar coating or gravure coating, or a pattern coating method.
[0011] However, the adhesive layer formed between the free-standing film and the current collectors 15, 25 has a problem of restricting electron movement by preventing contact between the free-standing film and the current collectors 15, 25. In the past, an attempt was made to solve this problem by mixing a conductive material with the adhesive layer. However, the conventional method still has a problem in that the binder acts as a resistor in the high rate region and the discharge capacity is reduced because the binder is located between the free-standing film and the current collectors 15, 25.
[0012] Figure 3 is an exploded view of the electrode assembly of Figure 1. Referring to Figures 1 to 3, the conventional electrode assembly has a structure in which a separator 30 is interposed between a positive electrode 10 and a negative electrode 20, which are respectively manufactured as shown in Figure 2. Therefore, in the conventional electrode assembly, the positive electrode 10 and the negative electrode 20 are limited to a film form in order to ensure a certain strength, and there is a problem in that the productivity is reduced by separately manufacturing the positive electrode 10 and the negative electrode 20.
[0013] Therefore, unlike the conventional technique, there is a growing need to develop an electrode assembly that includes an electrode manufactured by a dry method, but has an improved resistance reduction effect and improved productivity by minimizing the binder content. Summary of the Invention [Problem to be solved by the invention]
[0014] An object of the present invention is to provide an electrode assembly having improved productivity and resistance reduction effect, and a battery cell including the same.
[0015] The problems to be solved by the present invention are not limited to the problems described above, and problems not mentioned will be clearly understood by a person having ordinary skill in the art to which the present invention pertains from this specification and the accompanying drawings. [Means for solving the problem]
[0016] An electrode assembly according to an embodiment of the present invention includes a separator; a positive electrode active material layer attached to a first surface of the separator; and a negative electrode active material layer attached to a second surface of the separator, the positive electrode active material layer being formed of a first dry mixed electrode composition including a positive electrode active material, a conductive material, and a binder, and the negative electrode active material layer being formed of a second dry mixed electrode composition including a negative electrode active material, a conductive material, and a binder.
[0017] The positive electrode active material layer may be disposed such that a positive electrode current collector is laminated on a surface opposite to a surface in contact with the separator, and the negative electrode active material layer may be disposed such that a negative electrode current collector is laminated on a surface opposite to a surface in contact with the separator.
[0018] At least one of the positive electrode current collector and the negative electrode current collector may be formed from a planar sheet.
[0019] At least one of the positive electrode current collector and the negative electrode current collector may be formed from two or more linear sheets, and the two or more linear sheets may be spaced apart from each other.
[0020] The two or more linear sheets may have the same pattern as each other.
[0021] At least one of the positive and negative current collectors may be formed from a fibrous sheet having a random orientation.
[0022] The first electrode composition and the second electrode composition each contain a binder, and the content of the binder in the first electrode composition may be 1 wt % or more and 5 wt % or less based on the total weight of the first electrode composition, and the content of the binder in the second electrode composition may be 1 wt % or more and 5 wt % or less based on the total weight of the second electrode composition.
[0023] The binder can include polytetrafluoroethylene (PTFE).
[0024] The content of the positive electrode active material in the first electrode composition may be 90 wt % or more and 98 wt % or less based on the total weight of the first electrode composition.
[0025] The positive electrode active material is lithium cobalt oxide (LiCoO 2 ), lithium nickel oxide (LiNiO 2 ), lithium copper oxide (Li 2 CuO 2 ), vanadium oxide, Ni-site type lithium nickel oxide, lithium manganese composite oxide, lithium manganese composite oxide with spinel structure, LiMn in which part of the Li is replaced by alkaline earth metal ions 2 O 4 , disulfide compounds, Fe 2 (MoO 4 ) 3 , lithium manganese oxide (LMO).
[0026] The content of the negative electrode active material in the second electrode composition may be 90 wt % or more and 98 wt % or less based on the total weight of the second electrode composition.
[0027] The negative electrode active material may include at least one of lithium metal, lithium alloy, petroleum coke, activated carbon, graphite, silicon, tin, and metal oxides.
[0028] The positive electrode active material layer and the negative electrode active material layer may each be a free-standing film.
[0029] An adhesive layer may be formed between the separator and the positive electrode active material layer and between the separator and the negative electrode active material layer, and the adhesive layer may have a porous structure.
[0030] A battery cell according to another embodiment of the present invention may include the above-described electrode assembly.
[0031] The battery cell may include at least two of the electrode assemblies stacked together, and the at least two electrode assemblies may be arranged such that the positive electrode active material layers included in each electrode assembly face each other or the negative electrode active material layers included in each electrode assembly face each other.
[0032] The at least two electrode assemblies may be arranged such that a positive electrode current collector is stacked between the respective positive electrode active material layers, and a negative electrode current collector is stacked between the respective negative electrode active material layers.
[0033] According to another embodiment of the present invention, a method for manufacturing an electrode assembly includes the steps of: preparing a positive electrode active material layer formed from a first electrode composition in which a positive electrode active material, a conductive material, and a binder are dry-mixed; preparing a negative electrode active material layer formed from a second electrode composition in which a negative electrode active material, a conductive material, and a binder are dry-mixed; and attaching the positive electrode active material layer to a first surface of a separator and attaching the negative electrode active material layer to a second surface of a separator.
[0034] The positive electrode active material layer and the negative electrode active material layer may be formed as free-standing films.
[0035] The positive electrode active material layer may be disposed such that a positive electrode current collector is stacked on a surface opposite to the surface in contact with the separator, and the negative electrode active material layer may be disposed such that a negative electrode current collector is stacked on a surface opposite to the surface in contact with the separator. Effect of the Invention
[0036] According to an embodiment of the present invention, by providing an electrode assembly in which a free-standing film manufactured by a dry method is attached to a separator, and a battery cell including the same, it is possible to improve productivity and a resistance reduction effect.
[0037] The effects of the present invention are not limited to the effects described above, and effects not mentioned will be clearly understood by those having ordinary skill in the art to which the present invention pertains from this specification and the accompanying drawings. [Brief description of the drawings]
[0038] [Figure 1] 1 is a diagram showing a conventional electrode assembly. [Diagram 2] 2 is a diagram showing a manufacturing process of an electrode included in the electrode assembly of FIG. 1. [Diagram 3] FIG. 2 is an exploded view of the electrode assembly of FIG. [Figure 4] 1 is a view showing an electrode assembly according to an embodiment of the present invention; [Diagram 5] 5 is a diagram showing a current collector included in the electrode assembly of FIG. 4. [Figure 6] 5 is a flowchart showing a process for manufacturing the electrode assembly of FIG. 4. [Figure 7] 7 is a diagram showing a manufacturing step of the electrode assembly of FIG. 6. [Figure 8] 7 is an exploded view of the electrode assembly manufactured at the electrode assembly manufacturing stage of FIG. 6. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0039] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will now be described in detail with reference to exemplary embodiments thereof, so that those skilled in the art can easily practice the present invention. However, the present invention may be embodied in many different forms and is not limited to the embodiments set forth herein.
[0040] Hereinafter, an electrode assembly according to an embodiment of the present invention will be described.
[0041] FIG. 4 is a view showing an electrode assembly according to an embodiment of the present invention.
[0042] 4, an electrode assembly according to an embodiment of the present invention includes a positive electrode active material layer 110, a negative electrode active material layer 210, and a separator 300. In the separator 300, the positive electrode active material layer 110 is attached to a first surface of the separator 300, and the negative electrode active material layer 210 is attached to a second surface of the separator 300.
[0043] For example, the positive electrode active material layer 110 may be laminated on a first surface of the separator 300, and the negative electrode active material layer 210 may be laminated on a second surface of the separator 300. The positive electrode active material layer 110, the negative electrode active material layer 210, and the separator 300 may then be attached to each other by roll pressing.
[0044] Here, the separator 300 can be used without any particular limitation as long as it is generally used as a separator in a lithium secondary battery, and it is particularly preferable that the separator 300 has low resistance to ion migration of the electrolyte, excellent electrolyte humectancy, and surface adhesiveness. As an example, the separator 300 may be a porous polymer film made of a polyolefin (PO)-based polymer such as an ethylene homopolymer, a propylene homopolymer, an ethylene / butene copolymer, an ethylene / hexene copolymer, and an ethylene / methacrylate copolymer. Alternatively, a safety reinforced separator (SRS) may be used. Alternatively, a general porous nonwoven fabric made of a high-melting glass fiber, a polyethylene terephthalate fiber, or the like may be used.
[0045] Therefore, the separator 300 can separate the positive electrode active material layer 110 and the negative electrode active material layer 210 to serve as a lithium ion passage, and can also serve as a support for the positive electrode active material layer 110 and the negative electrode active material layer 210 attached to each side. In addition, the surface adhesive force of the separator 300 can minimize the content of the binder included in the electrode assembly, thereby improving the resistance reduction effect.
[0046] In an electrode assembly according to another embodiment of the present invention, the separator 300 may include an adhesive layer (not shown) between the separator 300 and the positive electrode active material layer 110, and may include an adhesive layer (not shown) between the separator 300 and the negative electrode active material layer 210.
[0047] The adhesive layer (not shown) is attached to the separator 300 and may have a porous structure that does not impede the movement of lithium ions through the separator 300. As an example, the adhesive layer (not shown) may be formed on the separator 300 by a vapor-induced phase separation method. In addition, the adhesive layer (not shown) may be formed by any coating technique that does not block pores formed in the separator 300, and methods such as binder pattern coating, mixed composition coating of an inorganic material and a binder, etc. may be used.
[0048] In addition, the adhesive layer may be formed of a coating slurry containing an adhesive binder such as polyvinylidene fluoride (PVDF), an acrylic binder, etc. However, the material constituting the adhesive layer is not limited thereto, and any material that can be coated on the surface of the separator 300 and has adhesive properties can be used without limitation.
[0049] Therefore, the separator 300 can have improved adhesive strength to each of the positive electrode active material layer 110 and the negative electrode active material layer 210. In addition, even if the adhesive layer is formed, the separator 300 is not limited in its role as a passage for lithium ions. In addition, due to the surface adhesive strength of the separator 300, the content of the binder contained in the adhesive layer formed on the separator 300 can be reduced compared to the conventional case, and the resistance reduction effect can be improved. In addition, the increase in resistance due to the adhesive layer does not need to be large, and the discharge capacity can be improved in a high rate region.
[0050] In addition, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be 13 gf / 15 mm or more and 100 gf / 15 mm or less. More specifically, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be 15 gf / 15 mm or more and 95 gf / 15 mm or less. As an example, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be 20 gf / 15 mm or more and 90 gf / 15 mm or less.
[0051] Therefore, in the electrode assembly of the present embodiment, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be within the above-mentioned range, and the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be stably fixed to each other. On the other hand, if the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 is too low and deviates from the above-mentioned range, the separator 300 may not be stably fixed to the positive electrode active material layer 110 or the negative electrode active material layer 210. Also, if the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 is too high and deviates from the above-mentioned range, problems such as increased manufacturing costs and difficulty in implementing the manufacturing process may occur.
[0052] In addition, the positive electrode active material layer 110 is formed from a first electrode composition in which a positive electrode active material is dry-mixed. The negative electrode active material layer 210 is formed from a second electrode composition in which a negative electrode active material is dry-mixed. As an example, the positive electrode active material layer 110 and the negative electrode active material layer 210 may each be manufactured as a free-standing film. Therefore, the positive electrode active material layer 110 and the negative electrode active material layer 210 may each be stored in a roll form as a free-standing film before being manufactured into an electrode assembly, thereby improving productivity.
[0053] The positive electrode active material contained in the first electrode composition is, for example, lithium cobalt oxide (LiCoO 2 ), lithium nickel oxide (LiNiO 2 );Lithium manganese oxide;Lithium copper oxide (Li 2 CuO 2 );Vanadium oxide;Ni-site type lithium nickel oxide;Lithium manganese composite oxide;Lithium manganese composite oxide with spinel structure;Chemical formula Li is partially replaced by alkaline earth metal ions, LiMn 2 O 4 ;Disulfide compounds;Fe 2 (MoO 4 ) 3 For example, the positive electrode active material may include lithium manganese oxide (LMO).
[0054] Here, the positive electrode active material may be included in an amount of 88 wt% to 99 wt% based on the total weight of the first electrode composition. More preferably, the positive electrode active material may be included in an amount of 89 wt% to 98.5 wt% based on the total weight of the first electrode composition. For example, the positive electrode active material may be included in an amount of 90 wt% to 98 wt% based on the total weight of the first electrode composition.
[0055] The negative electrode active material contained in the second electrode composition may be a negative electrode active material for lithium secondary batteries commonly used in the art, such as lithium metal, lithium alloy, petroleum coke, activated carbon, graphite, silicon, tin, metal oxides, or other carbons.
[0056] Here, the negative electrode active material may be included in an amount of 88 wt% to 99 wt% based on the total weight of the second electrode composition. More preferably, the negative electrode active material may be included in an amount of 89 wt% to 98.5 wt% based on the total weight of the second electrode composition. For example, the negative electrode active material may be included in an amount of 90 wt% to 98 wt% based on the total weight of the second electrode composition.
[0057] In addition, the first electrode composition and the second electrode composition may each contain a binder. The binder plays a role of improving the adhesion between active material particles and the adhesive strength between the active material and the current collector. Specific examples include polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVDF), vinylidene fluoride-hexafluoropropylene copolymer (PVDF-co-HFP), polyvinyl alcohol, polyacrylonitrile, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene polymer (EPDM), sulfonated EPDM, styrene butadiene rubber (SBR), fluororubber, or various copolymers thereof, and one or more of these may be used alone or in combination.
[0058] As an example, each of the binders may include polytetrafluoroethylene (PTFE). Here, polytetrafluoroethylene (PTFE) has a characteristic that fibers are pulled out from particles by application of shear force. That is, in one embodiment of the present invention, the first electrode composition and the second electrode composition each include polytetrafluoroethylene (PTFE) as a binder, and the first electrode composition and the second electrode composition may be mixed by a physical mixing method in which polytetrafluoroethylene (PTFE) is fiberized by application of strong shear force.
[0059] Therefore, in one embodiment of the present invention, the first electrode composition and the second electrode composition may be mixed in a dry manner without a separate solvent or additive, which is very effective in bridging between active material particles or between the active material particles and a current collector, and also prevents damage to the active material that may occur during a heat treatment at high temperatures in a conventional mixing method.
[0060] In addition, the content of the binder contained in the first electrode composition may be 1 wt % or more and 5 wt % or less based on the total weight of the first electrode composition, and the content of the binder contained in the second electrode composition may be 1 wt % or more and 5 wt % or less based on the total weight of the second electrode composition. More preferably, the content of the binder contained in the first electrode composition may be 2 wt % or more and 4 wt % or less based on the total weight of the first electrode composition, and the content of the binder contained in the second electrode composition may be 2 wt % or more and 4 wt % or less based on the total weight of the second electrode composition.
[0061] Therefore, the first electrode composition and the second electrode composition may have sufficient tensile strength and discharge capacity to form the positive electrode active material layer 110 and the negative electrode active material layer 210. In contrast, if the binder content is less than 1 wt %, the tensile strength of the positive electrode active material layer 110 and the negative electrode active material layer 210 may decrease. In addition, if the binder content exceeds 5 wt %, the binder acts as a resistor in the positive electrode active material layer 110 and the negative electrode active material layer 210, and the discharge capacity may decrease.
[0062] Furthermore, the first electrode composition and the second electrode composition may each contain a conductive material. The conductive material is used to impart electrical conductivity to the electrode, and may be used without any particular restrictions as long as it does not cause chemical changes in the battery that is constructed, but has electronic conductivity. Specific examples include carbon-based materials such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, thermal black, graphene, and carbon fiber; graphite such as natural graphite and artificial graphite; metal powder or metal fiber such as copper, nickel, aluminum, and silver; conductive whiskers such as zinc oxide and potassium titanate; conductive metal oxides such as titanium oxide; or conductive polymers such as polyphenylene derivatives, and the like. One or a mixture of two or more of these may be used. Here, the conductive material may be contained in an amount of 1% by weight to 10% by weight based on the total weight of the electrode.
[0063] Hereinafter, the current collectors 150 and 250 included in the electrode assembly according to the present embodiment will be described in detail.
[0064] FIG. 5 is a view showing a current collector included in the electrode assembly of FIG.
[0065] 4 and 5, in an electrode assembly according to an embodiment of the present invention, a positive electrode current collector 150 is laminated on a surface of a positive electrode active material layer 110 opposite to a surface in contact with a separator 300. In addition, a negative electrode current collector 250 is laminated on a surface of a negative electrode active material layer 210 opposite to a surface in contact with the separator 300.
[0066] Therefore, the electrode assembly according to the present embodiment is laminated without a separate adhesive layer between the positive electrode active material layer 110 and the positive electrode current collector 150, so that the contact area between the positive electrode active material layer 100 and the positive electrode current collector 150 can be increased, and the electron transfer between the positive electrode active material layer 100 and the positive electrode current collector 150 is not restricted, so that the discharge capacity can be improved. This can be similarly explained for the negative electrode active material layer 210 and the negative electrode current collector 250.
[0067] Here, the positive electrode current collector 150 and the negative electrode current collector 250 are not particularly limited as long as they do not induce chemical changes in the battery and have high conductivity. For example, copper, stainless steel, aluminum, nickel, titanium, calcined carbon, copper or stainless steel surface-treated with carbon, nickel, titanium, silver, or the like, aluminum-cadmium alloy, or the like can be used.
[0068] In addition, there may be almost no adhesive force between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210. Even if there is adhesive force between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210, the adhesive force may be the adhesive force between the current collectors 150, 250 and the active material layers 210, 250 themselves.
[0069] In this case, the adhesive strength between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210 may be 0 gf / 15 mm or more and 5 gf / 15 mm or less. More specifically, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be 0.05 gf / 15 mm or more and 4.5 gf / 15 mm or less. As an example, the adhesive strength between the separator 300 and the positive electrode active material layer 110 or the negative electrode active material layer 210 may be 0.1 gf / 15 mm or more and 4 gf / 15 mm or less.
[0070] Therefore, in the electrode assembly of the present embodiment, the adhesive strength between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210 may be within the above-mentioned range, and there may be almost no adhesive strength between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210. In other words, since no separate adhesive layer is formed between the positive electrode current collector 150 and the positive electrode active material layer 110 or between the negative electrode current collector 250 and the negative electrode active material layer 210, the hindrance of electron transfer is reduced, and the discharge capacity may be improved.
[0071] On the other hand, if the adhesive strength between the positive electrode collector 150 and the positive electrode active material layer 110 or between the negative electrode collector 250 and the negative electrode active material layer 210 is excessively large beyond the above-mentioned range, it may be considered that a separate adhesive layer is formed between the positive electrode collector 150 and the positive electrode active material layer 110 or between the negative electrode collector 250 and the negative electrode active material layer 210. In this case, the adhesive layer located between the positive electrode collector 150 and the positive electrode active material layer 110 or between the negative electrode collector 250 and the negative electrode active material layer 210 may hinder the electron transfer between the positive electrode collector 150 and the positive electrode active material layer 110 or between the negative electrode collector 250 and the negative electrode active material layer 210, and the discharge capacity in the high rate region may also be reduced.
[0072] Also, referring to FIGS. 4 and 5, in the electrode assembly according to the present embodiment, the positive electrode active material layer 110 and the negative electrode active material layer 210 are attached to a separator 300, and the positive electrode current collector 150 and the negative electrode current collector 250 are not limited to the conventional film type and can be used in various forms.
[0073] 5(a), at least one of the positive electrode current collector 150 and the negative electrode current collector 250 may be formed from a flat sheet. For example, when the positive electrode current collector 150 is formed from a flat sheet, the positive electrode current collector 150 may have a size equal to or smaller than one surface of the positive electrode active material layer 110. Furthermore, unlike the conventional case, the positive electrode current collector 150 does not need to serve as a support for the positive electrode active material layer 110, and may have a smaller thickness than the conventional case. This can be similarly explained for the negative electrode current collector 250.
[0074] 5(b) and (c), at least one of the positive electrode current collector 150 and the negative electrode current collector 250 may be formed of two or more linear sheets, and the linear sheets may be spaced apart from each other. Here, the linear sheets may be formed in various shapes, such as a fiber shape, a rod shape, a thin plate shape, etc. Also, the linear sheets may have the same pattern. For example, the pattern may be a curved line type, a straight line type, a dotted line type, or the like.
[0075] Referring to FIG. 5(d), at least one of the positive electrode current collector 150 and the negative electrode current collector 250 may be formed from a fibrous sheet having a random orientation.
[0076] Therefore, the electrode assembly according to the present embodiment may include various types of current collectors 150, 250, and may fully function as an electron transfer path while reducing the total area of the current collectors 150, 250. In addition, the total weight during assembly of the battery cell may be reduced, and the manufacturing form may be simplified, leading to improved productivity. In addition, the active material layers 110, 210 may be included in greater numbers than in the past, leading to an increased discharge capacity.
[0077] Furthermore, in the electrode assembly according to the present embodiment, a notching process for forming an electrode tab at one end of the current collectors 150 and 250 can be performed during the manufacture of the current collectors 150 and 250 of the above-described configuration, thereby further improving productivity.
[0078] Hereinafter, a method for manufacturing an electrode assembly according to another embodiment of the present invention will be described in detail.
[0079] Fig. 6 is a flow chart showing a process for manufacturing the electrode assembly of Fig. 4. Fig. 7 is a diagram showing a manufacturing step of the electrode assembly of Fig. 6. Fig. 8 is an exploded view of the electrode assembly manufactured by the manufacturing step of the electrode assembly of Fig. 6.
[0080] Referring to FIG. 6, the method for manufacturing an electrode assembly according to the present embodiment includes a premixing step (S10) of dry-mixing an active material, a conductive material, and a binder, a mixing step (S20) of preparing an electrode composition by applying high shear force, a step (S30) of preparing a free-standing film using the electrode composition, and a step (S50) of attaching the free-standing film onto a separator, performing a lamination process, and laminating a current collector on the free-standing film to prepare an electrode assembly.
[0081] 6 and 7, in the electrode assembly manufacturing step (S50), the positive electrode active material layer 110 manufactured in the freestanding step (S30) is attached to one side of the separator 300, and the negative electrode active material layer 210 manufactured in the freestanding step (S30) is attached to the other side of the separator 300. As an example, the positive electrode active material layer 110 and the negative electrode active material layer 210 are laminated on the upper and lower sides of the separator 300, respectively, and bonded by flat pressing to form an electrode assembly having a positive electrode active material layer 110-separator 300-negative electrode active material layer 210 structure.
[0082] 6 to 8, in the electrode assembly preparation step (S50), a positive electrode current collector 150 and a negative electrode current collector 250 may be additionally stacked on an electrode assembly having a structure of a positive electrode active material layer 110-separator 300-negative electrode active material layer 210. As an example, at least two electrode assemblies are stacked, and the at least two electrode assemblies may be arranged such that the positive electrode active material layers 110 included in each electrode assembly face each other or the negative electrode active material layers 210 included in each electrode assembly face each other. Also, the at least two electrode assemblies may have a positive electrode current collector 150 stacked between each positive electrode active material layer 110, and a negative electrode current collector 250 stacked between each negative electrode active material layer 210.
[0083] Therefore, the method for manufacturing an electrode assembly according to the present embodiment manufactures an electrode assembly having a structure of the positive electrode active material layer 110-separator 300-negative electrode active material layer 210, and therefore the manufacturing process can be simplified compared to the conventional process in which the positive electrode and the negative electrode must be manufactured separately. In addition, the electrode assembly having the structure of the positive electrode active material layer 110-separator 300-negative electrode active material layer 210 does not include a separate adhesive layer between the positive electrode active material layer 110 and the positive electrode current collector 150 or between the negative electrode active material layer 210 and the negative electrode current collector 250, and thus is not restricted in electron movement, and therefore the discharge capacity can be improved.
[0084] A battery cell according to another embodiment of the present invention may include the above-described electrode assembly. Also, a battery cell according to another embodiment of the present invention may include the above-described electrode assembly and an electrolyte.
[0085] The electrolyte used in the present invention includes, but is not limited to, organic liquid electrolytes, inorganic liquid electrolytes, solid polymer electrolytes, gel polymer electrolytes, solid inorganic electrolytes, molten inorganic electrolytes, and the like that can be used in the production of lithium secondary batteries.
[0086] Specifically, the electrolyte may include an organic solvent and a lithium salt. The organic solvent may be any organic solvent that can act as a medium through which ions involved in the electrochemical reaction of the battery can move. The lithium salt may be any lithium salt that can provide lithium ions used in the lithium secondary battery.
[0087] In addition to the above-mentioned components, the electrolyte may further contain one or more additives such as haloalkylene carbonate compounds such as difluoroethylene carbonate, pyridine, triethyl phosphate, triethanolamine, cyclic ethers, ethylenediamine, n-glyme, hexaphosphoric acid triamide, nitrobenzene derivatives, sulfur, quinoneimine dyes, N-substituted oxazolidinones, N,N-substituted imidazolidines, ethylene glycol dialkyl ethers, ammonium salts, pyrrole, 2-methoxyethanol, or aluminum trichloride, for the purpose of improving the life characteristics of the battery, suppressing the decrease in the battery capacity, improving the discharge capacity of the battery, etc. In this case, the additives may be contained in an amount of 0.1 wt % to 5 wt % based on the total weight of the electrolyte.
[0088] The present invention will be described in detail with reference to the following examples. However, the following examples are provided for illustrative purposes only and are not intended to limit the scope of the present invention.
[0089] <Example> In this embodiment, a premixing step is performed to prepare a mixture by dry mixing a positive electrode active material, a conductive material, and a binder using a blender manufactured by Waring Co. Here, the positive electrode active material is 94 wt% lithium manganese oxide (LMO), and the conductive material is 3 wt% Super C65. The binder contains 3 wt% polytetrafluoroethylene (PTFE). At this time, the premixing step (S10) is performed at room temperature and 5000 rpm for 1 minute. Then, a mixing step (S20) is performed to prepare a first electrode composition by applying a shear force to the mixture prepared in the premixing step (S10) using a PBV-0.1L machine manufactured by Irie Shokai Co. At this time, the mixing step (S20) is performed at room temperature and 30 rpm for 5 minutes. Then, using an Inoue Two Roll Mill MR-3, the first electrode composition prepared in the mixing step (S20) was used to prepare a free-standing film-type positive electrode active material layer 110. The negative electrode active material layer 210 was prepared in the same manner, except that a negative electrode active material, graphite, was used instead of the positive electrode active material.
[0090] Then, PVDF-HFP (Mw. 500,000) resin was added to acetone to prepare a polymer solution (solid content 5 wt% concentration). 2 O 3 (Nippon Light Metal Co., Ltd., LS235) was added and dispersed using a ball mill to prepare a slurry for the porous coating layer. The prepared slurry for the porous coating layer was coated on a separator 300 made of polyolefin (PO) with a thickness of 15 um by dip coating. Here, the thickness of the adhesive layer coated with the slurry for the porous coating layer was 2 um. This was done at a temperature of 23 degrees Celsius and a relative humidity (RH) of 40%.
[0091] Thereafter, the positive electrode active material layer 110 and the negative electrode active material layer 210 were laminated on the separator 300 coated with the slurry for the porous coating layer, and then roll pressing was performed to manufacture an electrode assembly having a positive electrode active material layer 110-separator 300-negative electrode active material layer 210 structure.
[0092] Thereafter, a battery cell was manufactured by laminating at least two of the electrode assemblies, a positive electrode current collector 150 made of 20 um aluminum foil on the positive electrode active material layer 110, and a negative electrode current collector 250 made of 20 um copper foil on the negative electrode active material layer 210, and packaging the resulting battery cell in a pouch together with an electrolyte. The electrolyte was a 1.0 M LiPF4 solution in a mixed solvent of ethylene carbonate (EC) / ethyl methyl carbonate (EMC) (volume ratio of 20 / 80). 6 A solution was used.
[0093] <Comparative Example 1> In Comparative Example 1, the separator 30 in the above-mentioned Example does not include a separate adhesive layer, and an adhesive layer in which an adhesive slurry containing PVDF and carbon is mixed and coated to a thickness of 0.5 um is included between the positive electrode active material layer 11 and the positive electrode current collector 15, and the positive electrode 10 is manufactured by roll pressing the positive electrode active material layer 11 and the positive electrode current collector 15. In addition, an adhesive layer in which an adhesive slurry containing PVDF and carbon is mixed and coated to a thickness of 0.5 um is included between the negative electrode active material layer 21 and the negative electrode current collector 25, and the negative electrode 10 is manufactured by roll pressing the negative electrode active material layer 21 and the negative electrode current collector 25. In addition, the separator 30 is laminated between the positive electrode 10 and the negative electrode 20 to manufacture an electrode assembly having a positive electrode 10-separator 30-negative electrode 20 structure, and the electrode assembly is packaged in a pouch together with an electrolyte to manufacture a battery cell, except that the comparative example is manufactured in the same manner as the examples.
[0094] <Comparative Example 2> In Comparative Example 2, the separator 30 in the above-mentioned Example does not include a separate adhesive layer, and an adhesive layer in which an adhesive slurry containing PVDF and carbon is coated to a thickness of 1.5 um is included between the positive electrode active material layer 11 and the positive electrode current collector 15, and the positive electrode active material layer 11 and the positive electrode current collector 15 are roll-pressed to manufacture the positive electrode 10. In addition, an adhesive layer in which an adhesive slurry containing PVDF and carbon is coated to a thickness of 1.5 um is included between the negative electrode active material layer 21 and the negative electrode current collector 25, and the negative electrode active material layer 21 and the negative electrode current collector 25 are roll-pressed to manufacture the negative electrode 10. In addition, the separator 30 is laminated between the positive electrode 10 and the negative electrode 20 to manufacture an electrode assembly having a positive electrode 10-separator 30-negative electrode 20 structure, and the separator 30 is laminated between the positive electrode 10 and the negative electrode 20 to manufacture a battery cell, and the battery cell is manufactured in the same manner as in the Example.
[0095] <Experimental Example 1 (Adhesive Strength Measurement)> The adhesive strength between the positive electrode active material layers 11, 110 and the negative electrode active materials 21, 210 in the form of freestanding films prepared in Example, Comparative Example 1, and Comparative Example 2 and other substrates was measured. At this time, the adhesive strength was measured by peel strength at an angle of 90 degrees at a speed of 300 mm / min using a UTM device from Instron after sampling with a width of 15 mm. Here, the adhesive strength was measured by the adhesive strength between the current collector and the active material layer and the adhesive strength between the separator and the active material layer, and the results are shown in Table 1.
[0096] [Table 1]
[0097] Referring to Table 1, it can be seen that, unlike Comparative Examples 1 and 2, when an adhesive layer is formed between the active material layer and the separator as in the Example, the adhesive strength between the active material layer and the separator is very excellent.
[0098] In contrast, when an adhesive layer is formed between the current collector and the active material layer as in Comparative Examples 1 and 2, it can be seen that the adhesive strength between the current collector and the active material layer is better than in the Examples, but is much lower than the adhesive strength between the separator and the active material layer in the Examples. Furthermore, in the cases of Comparative Examples 1 and 2, it can be seen that there is no adhesive strength between the separator and the active material layer, unlike the Examples.
[0099] Therefore, even if the positive electrode active material layer 110 and the negative electrode active material layer 210 according to this embodiment are manufactured in the form of a free-standing film as in the comparative example, the adhesive strength between the active material layers 110, 210 and the separator 300 is excellent, and the active material layers 110, 210 and the separator 300 are stably fixed to each other, thereby improving the stability of the battery cell during the charge and discharge process of the battery cell and extending its lifespan.
[0100] <Experimental Example 2 (Measurement of Discharge Capacity)> The battery cells manufactured in the examples and comparative examples were charged and discharged in a voltage range of 3.0 to 4.3 V under conditions of 0.1 C / 0.1 C, 1 C / 1 C, and 2 C / 2 C, and the discharge capacity value of the first cycle was calculated. The results are shown in Table 2.
[0101] [Table 2]
[0102] Referring to Table 2, it can be seen that, unlike Comparative Example 1 and Comparative Example 2, the Examples are generally superior in discharge capacity. In particular, it can be seen that, unlike Comparative Example 1 and Comparative Example 2, the Examples are improved in discharge capacity in the high rate region. Furthermore, in the case of Comparative Example 1 and Comparative Example 2, the adhesive layer located between the current collectors 15, 25 and the active material layers 11, 21 contains a mixture of a binder and a conductive material, and it can be seen that the binder contained in the adhesive layer interferes with electron transfer between the current collectors 15, 25 and the active material layers 11, 21, and therefore is inferior in the high rate region. In particular, when comparing Comparative Example 1 and Comparative Example 2, it can be seen that the degree of inferiority becomes greater as the thickness of the adhesive layer located between the current collectors 15, 25 and the active material layers 11, 21 becomes thicker.
[0103] In contrast, in the case of the embodiment, no separate adhesive layer is formed between the current collectors 150, 250 and the active material layers 110, 210, and they are in complete contact with each other. Therefore, the adhesive layer does not interfere with the transfer of electrons between the current collectors 150, 250 and the active material layers 110, 210, and it can be seen that the discharge capacity is superior to that of the comparative example even in the high rate region.
[0104] Therefore, when an electrode assembly having a structure of a positive electrode active material layer 110-separator 300-negative electrode active material layer 210 is included as in the embodiment, the content of the binder contained in the electrode assembly is minimized, thereby improving the resistance and reducing the interference with electron transfer caused by the adhesive layer, thereby generally improving the discharge capacity.
[0105] Although the preferred embodiments of the present invention have been described in detail above, the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present invention defined in the claims also fall within the scope of the present invention.
Claims
1. separation membrane, a positive electrode active material layer attached to a first surface of the separator; and a negative electrode active material layer attached to a second surface of the separator, The positive electrode active material layer is formed from a first dry mixed electrode composition including a positive electrode active material, a binder, and a conductive material; the negative electrode active material layer is formed from a second dry mixed electrode composition of a negative electrode active material, a binder, and a conductive material; the positive electrode active material layer is disposed such that a positive electrode current collector is laminated on a surface opposite to a surface in contact with the separator without an adhesive layer; the negative electrode active material layer is disposed such that a negative electrode current collector is laminated on a surface opposite to a surface in contact with the separator without an adhesive layer; an adhesive layer is formed between the separator and the positive electrode active material layer, and between the separator and the negative electrode active material layer, The adhesive layer has a porous structure.
2. The electrode assembly of claim 1 , wherein at least one of the positive and negative current collectors is formed from a planar sheet.
3. At least one of the positive electrode current collector and the negative electrode current collector is formed from two or more linear sheets, The electrode assembly of claim 1 , wherein the two or more linear sheets are spaced apart from each other.
4. The electrode assembly according to claim 3 , wherein the two or more linear sheets have the same pattern as each other.
5. 2. The electrode assembly of claim 1, wherein at least one of the positive and negative current collectors is formed from a fibrous sheet having a random orientation.
6. The content of the binder contained in the first dry mixed electrode composition is 1 wt % or more and 5 wt % or less based on the total weight of the first dry mixed electrode composition; The electrode assembly of claim 1 , wherein the content of the binder in the second dry mixed electrode composition is from 1 wt % to 5 wt % based on a total weight of the second dry mixed electrode composition.
7. The electrode assembly of claim 6 , wherein the binder comprises polytetrafluoroethylene (PTFE).
8. 2 . The electrode assembly of claim 1 , wherein the content of the positive electrode active material contained in the first dry mixed electrode composition is from 90% by weight to 98% by weight based on the total weight of the first dry mixed electrode composition.
9. The positive electrode active material is lithium cobalt oxide (LiCoO 2 ), lithium nickel oxide (LiNiO 2 ), lithium copper oxide (Li 2 CuO 2 ), vanadium oxide, Ni-site type lithium nickel oxide, lithium manganese composite oxide, lithium manganese composite oxide with spinel structure, LiMn 2 O 4 , disulfide compound, Fe 2 (MoO 4 ) 3 9. The electrode assembly of claim 8, comprising at least one of the following: lithium manganese oxide (LMO).
10. 2 . The electrode assembly of claim 1 , wherein the content of the negative active material contained in the second dry mixed electrode composition is from 90% by weight to 98% by weight based on the total weight of the second dry mixed electrode composition.
11. 11. The electrode assembly of claim 10, wherein the negative electrode active material comprises at least one of lithium metal, lithium alloy, petroleum coke, activated carbon, graphite, silicon, tin, and metal oxides.
12. The electrode assembly according to claim 1 , wherein the positive electrode active material layer and the negative electrode active material layer are each a free-standing film.
13. A battery cell comprising the electrode assembly according to claim 1.
14. The battery cells are arranged such that at least two of the electrode assemblies are stacked, The battery cell according to claim 13 , wherein the at least two electrode assemblies are arranged such that the positive electrode active material layers included in each electrode assembly face each other or the negative electrode active material layers included in each electrode assembly face each other.
15. 15. The battery cell according to claim 14, wherein the at least two electrode assemblies are arranged such that a positive electrode current collector is stacked between the respective positive electrode active material layers and a negative electrode current collector is stacked between the respective negative electrode active material layers.
16. preparing a positive electrode active material layer formed of a first electrode composition in which a positive electrode active material, a conductive material, and a binder are dry-mixed; preparing a negative electrode active material layer formed of a second electrode composition in which a negative electrode active material, a conductive material, and a binder are dry-mixed; and attaching the positive electrode active material layer to a first surface of a separator and attaching the negative electrode active material layer to a second surface of the separator; The method further includes the steps of: arranging the positive electrode active material layer such that a positive electrode current collector is laminated on a surface opposite to the surface in contact with the separator without an adhesive layer; and arranging the negative electrode active material layer such that a negative electrode current collector is laminated on a surface opposite to the surface in contact with the separator without an adhesive layer, an adhesive layer is formed between the separator and the positive electrode active material layer, and between the separator and the negative electrode active material layer, The adhesive layer has a porous structure.
17. The method of claim 16, wherein the positive electrode active material layer and the negative electrode active material layer are formed as free-standing films.
Citation Information
Patent Citations
Lithium ion secondary battery and its manufacture
JP1998172606A
Electrode, its manufacturing method, and battery using the same
JP2016519841A
Method for manufacturing positive electrode for nonaqueous electrolyte coin-type battery
JP2017157337A
Dry electrode for energy storage device and its manufacturing method
JP2017517862A
Electrode for energy storage device and method for manufacturing dry electrode film for energy storage device
JP2019512872A