Semiconductor device and its manufacturing method
The semiconductor device addresses mechanical stress issues during wire bonding by incorporating a robust laminate or columnar structure under the metal pad, enhancing durability and design flexibility while maintaining efficient manufacturing processes.
Patent Information
- Application Number
- JP2020150749
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-08
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2040-09-08
AI Technical Summary
Mechanical stress during wire bonding can damage semiconductor elements or wiring in hybrid bonding technology for CMOS image sensors and nonvolatile semiconductor memories.
A semiconductor device design that includes a structure with a robust laminate or columnar portion under the metal pad to alleviate mechanical stress during wire bonding, formed simultaneously with the memory cell array to enhance strength and reduce the impact of stress on the semiconductor device.
The design effectively suppresses mechanical stress during wire bonding, improving the durability of semiconductor elements and allowing for more design freedom without increasing the number of manufacturing steps.
Smart Images

Figure 0007583561000001 
Figure 0007583561000002 
Figure 0007583561000003
Abstract
Description
[Technical field]
[0001] The present embodiment relates to a semiconductor device and a manufacturing method thereof. [Background technology]
[0002] In recent years, hybrid bonding technology, which bonds two wafers on which semiconductor elements are formed, has been introduced into CMOS (Complementary Metal Oxide Semiconductor) image sensors and non-volatile semiconductor memories. In this case, electrode pads for wire bonding to connect to the outside are formed so as to be exposed on the top surface of the chip, for example, after the substrate is thinned.
[0003] However, there is a possibility that the semiconductor element or the wiring may be destroyed due to mechanical stress during wire bonding. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 11-354562 [Patent Document 2] JP 2018-73967 A Summary of the Invention [Problem to be solved by the invention]
[0005] A semiconductor device capable of suppressing the influence of stress due to wire bonding and a manufacturing method thereof are provided. [Means for solving the problem]
[0006] The semiconductor device according to the present embodiment includes a first chip on which a memory cell array is provided, and a second chip bonded to the first chip on which a control circuit for controlling the memory cell array is provided. The first chip has a substrate, a pad, a first structure, and a second structure. The substrate is disposed on the opposite side to a bonding surface with the second chip, and includes a first surface on which the memory cell array is provided between the opposing bonding surface, a second surface opposite to the first surface, and an opening in the first region that reaches from the second surface to the first surface. The pad is provided within the opening. The first structure is provided between the first surface and the bonding surface, and is electrically connected to the pad. The second structure is provided in the first region between the first surface and the bonding surface. [Brief description of the drawings]
[0007] [Figure 1] 1 is a cross-sectional view showing an example of a structure of a semiconductor device. [Diagram 2] FIG. 4 is a cross-sectional view showing an example of the structure of a columnar portion. [Diagram 3] 1A to 1C are cross-sectional views showing an example of a manufacturing method of a semiconductor device. [Figure 4] 1A to 1C are cross-sectional views showing an example of a manufacturing method of a semiconductor device. [Diagram 5] 1 is a cross-sectional view showing a configuration of a semiconductor device according to a first embodiment. [Figure 6] FIG. 3 is an overhead view showing the arrangement of structures and via plugs according to the first embodiment. [Figure 7] 1A to 1C are cross-sectional views showing a method for manufacturing the semiconductor device according to the first embodiment. [Figure 8] 8 is a cross-sectional view showing the method for manufacturing the semiconductor device, subsequent to FIG. 7. [Figure 9] 9 is a cross-sectional view showing the method for manufacturing the semiconductor device subsequent to FIG. 8. [Figure 10] 10 is a cross-sectional view showing the method for manufacturing the semiconductor device subsequent to FIG. 9. [Figure 11] 11 is a cross-sectional view showing the method for manufacturing the semiconductor device, subsequent to FIG. 10. [Figure 12] 12 is a cross-sectional view showing the method for manufacturing the semiconductor device subsequent to FIG. 11. [Figure 13]13 is a cross-sectional view showing the method for manufacturing the semiconductor device subsequent to FIG. 12. [Figure 14] 14 is a cross-sectional view showing the method for manufacturing the semiconductor device subsequent to FIG. 13. [Figure 15] FIG. 11 is a cross-sectional view showing a configuration of a semiconductor device according to a comparative example. [Figure 16] FIG. 11 is a cross-sectional view showing the configuration of a semiconductor device according to a second embodiment. [Figure 17] FIG. 11 is an overhead view showing an arrangement of structures and via plugs according to a second embodiment. [Figure 18] FIG. 11 is a cross-sectional view showing the configuration of a semiconductor device according to a third embodiment. [Figure 19] FIG. 11 is an overhead view showing an arrangement of structures and via plugs according to a third embodiment. [Figure 20] FIG. 13 is a cross-sectional view showing the configuration of a semiconductor device according to a fourth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. The present embodiment does not limit the present invention. In the following embodiments, the up-down direction of the semiconductor substrate indicates the relative direction when the surface on which the semiconductor element is provided is the upper side, and may differ from the up-down direction according to the gravitational acceleration. The drawings are schematic or conceptual, and the ratio of each part is not necessarily the same as the actual one. In the specification and drawings, the same reference numerals are used for elements similar to those described above with respect to the previously mentioned drawings, and detailed explanations are omitted as appropriate.
[0009] (First embodiment) Fig. 1 is a cross-sectional view showing an example of the structure of a semiconductor device. The semiconductor device in Fig. 1 is a three-dimensional memory in which an array chip 1 and a circuit chip 2 are bonded together. The array chip 1 is an example of a first chip, and the circuit chip 2 is an example of a second chip.
[0010] The array chip 1 includes a memory cell array 11 including a plurality of memory cells, an insulating film 12 on the memory cell array 11, and an interlayer insulating film 13 below the memory cell array 11. The insulating film 12 is, for example, a silicon oxide film or a silicon nitride film. The interlayer insulating film 13 is, for example, a silicon oxide film or a laminated film including a silicon oxide film and another insulating film.
[0011] The circuit chip 2 is provided under the array chip 1. The reference character S indicates the bonding surface between the array chip 1 and the circuit chip 2. The bonding surface S is an example of a first bonding surface. The circuit chip 2 includes an interlayer insulating film 14 and a substrate 15 under the interlayer insulating film 14. The interlayer insulating film 14 is, for example, a silicon oxide film, or a laminated film including a silicon oxide film and another insulating film. The substrate 15 is, for example, a semiconductor substrate such as a silicon substrate.
[0012] 1 shows an X direction and a Y direction parallel to and perpendicular to the surface of the substrate 15, and a Z direction perpendicular to the surface of the substrate 15. In this specification, the +Z direction is treated as the upward direction, and the -Z direction is treated as the downward direction. The -Z direction may or may not coincide with the direction of gravity.
[0013] The array chip 1 includes a plurality of word lines WL and source lines SL as electrode layers in a memory cell array 11. FIG. 1 shows a staircase structure portion 21 of the memory cell array 11. Each word line WL is electrically connected to a word wiring layer 23 via a contact plug 22. Each columnar portion CL penetrating the plurality of word lines WL is electrically connected to a bit line BL via a via plug 24, and is also electrically connected to a source line SL. The source line SL includes a first layer SL1 which is a semiconductor layer, and a second layer SL2 which is a metal layer.
[0014] The circuit chip 2 includes a plurality of transistors 31. Each of the transistors 31 includes a gate electrode 32 provided on the substrate 15 via a gate insulating film, and a source diffusion layer and a drain diffusion layer (not shown) provided in the substrate 15. The circuit chip 2 also includes a plurality of contact plugs 33 provided on the gate electrodes 32, the source diffusion layer, or the drain diffusion layer of each of the transistors 31, a wiring layer 34 provided on the contact plugs 33 and including a plurality of wirings, and a wiring layer 35 provided on the wiring layer 34 and including a plurality of wirings.
[0015] The circuit chip 2 further includes a wiring layer 36 provided on the wiring layer 35 and including a plurality of wirings, a plurality of via plugs 37 provided on the wiring layer 36, and a plurality of metal pads 38 provided on these via plugs 37. The metal pads 38 are, for example, a Cu (copper) layer or an Al (aluminum) layer. The circuit chip 2 functions as a control circuit (logic circuit) that controls the operation of the array chip 1. This control circuit is composed of transistors 31 and the like, and is electrically connected to the metal pads 38.
[0016] The array chip 1 includes a plurality of metal pads 41 provided on the metal pads 38, and a plurality of via plugs 42 provided on the metal pads 41. The array chip 1 also includes a wiring layer 43 including a plurality of wires provided on the via plugs 42, and a wiring layer 44 including a plurality of wires provided on the wiring layer 43. The metal pads 41 are, for example, a Cu layer or an Al layer.
[0017] The array chip 1 further includes a plurality of via plugs 45 provided on the wiring layer 44, metal pads 46 provided on the via plugs 45 and on the insulating film 12, and a passivation film 47 provided on the metal pads 46 and on the insulating film 12. The metal pads 46 are, for example, a Cu layer or an Al layer, and function as external connection pads (bonding pads) of the semiconductor device of FIG. 1. The passivation film 47 is, for example, an insulating film such as a silicon oxide film, and has an opening P that exposes the upper surface of the metal pad 46. The metal pads 46 can be connected to a mounting board or other devices via the opening P by a bonding wire, a solder ball, a metal bump, or the like.
[0018] FIG. 2 is a cross-sectional view showing an example of the structure of the columnar portion CL.
[0019] 2, the memory cell array 11 includes a plurality of word lines WL and a plurality of insulating layers 51 alternately stacked on the interlayer insulating film 13 (FIG. 1). The word lines WL are, for example, W (tungsten) layers. The insulating layers 51 are, for example, silicon oxide films.
[0020] The columnar portion CL includes a block insulating film 52, a charge storage layer 53, a tunnel insulating film 54, a channel semiconductor layer 55, and a core insulating film 56, in that order. The charge storage layer 53 is, for example, a silicon nitride film, and is formed on the side surface of the word line WL and the insulating layer 51 via the block insulating film 52. The charge storage layer 53 may be a semiconductor layer such as a polysilicon layer. The channel semiconductor layer 55 is, for example, a polysilicon layer, and is formed on the side surface of the charge storage layer 53 via the tunnel insulating film 54. The block insulating film 52, the tunnel insulating film 54, and the core insulating film 56 are, for example, a silicon oxide film or a metal insulating film.
[0021] 3 and 4 are cross-sectional views showing an example of a method for manufacturing a semiconductor device.
[0022] 3 shows an array wafer W1 including a plurality of array chips 1 and a circuit wafer W2 including a plurality of circuit chips 2. The array wafer W1 is also called a "memory wafer" and the circuit wafer W2 is also called a "CMOS wafer." The array wafer W1 is an example of a first wafer and the circuit wafer W2 is an example of a second wafer.
[0023] It should be noted that the orientation of the array wafer W1 in Fig. 3 is opposite to that of the array chip 1 in Fig. 1. In this embodiment, a semiconductor device is manufactured by bonding the array wafer W1 and the circuit wafer W2 together. Fig. 3 shows the array wafer W1 before it is inverted for bonding, and Fig. 1 shows the array chip 1 after it has been inverted for bonding, bonded, and diced.
[0024] 3, reference symbol S1 indicates the upper surface of the array wafer W1, and reference symbol S2 indicates the upper surface of the circuit wafer W2. It should be noted that the array wafer W1 includes a substrate 16 provided under an insulating film 12. The substrate 16 is, for example, a semiconductor substrate such as a silicon substrate.
[0025] In this embodiment, first, as shown in FIG. 3, the memory cell array 11, the insulating film 12, the interlayer insulating film 13, the staircase structure 21, the metal pad 41, etc. are formed on the substrate 16 of the array wafer W1, and the interlayer insulating film 14, the transistor 31, the metal pad 38, etc. are formed on the substrate 15 of the circuit wafer W2. For example, the via plug 45, the wiring layer 44, the wiring layer 43, the via plug 42, and the metal pad 41 are formed in this order on the substrate 16. In addition, the contact plug 33, the wiring layer 34, the wiring layer 35, the wiring layer 36, the via plug 37, and the metal pad 38 are formed in this order on the substrate 15. Next, as shown in FIG. 4, the array wafer W1 and the circuit wafer W2 are bonded together by mechanical pressure. As a result, the interlayer insulating film 13 and the interlayer insulating film 14 are bonded. Next, the array wafer W1 and the circuit wafer W2 are annealed at 400° C. As a result, the metal pad 41 and the metal pad 38 are bonded.
[0026] Thereafter, the substrate 15 is thinned by CMP (Chemical Mechanical Polishing), the substrate 16 is removed by CMP, and the array wafer W1 and the circuit wafer W2 are cut into a plurality of chips. In this manner, the semiconductor device of Fig. 1 is manufactured. Fig. 1 shows a circuit chip 2 including a metal pad 38, and an array chip 1 including a metal pad 41 disposed on the metal pad 38. Note that the metal pad 46 and the passivation film 47 are formed on the insulating film 12, for example, after the substrate 15 is thinned and the substrate 16 is removed.
[0027] In this embodiment, the array wafer W1 and the circuit wafer W2 are bonded together, but instead, array wafers W1 may be bonded together. The contents described above with reference to Figures 1 to 4 and the contents described below with reference to Figures 5 to 20 are also applicable to bonding array wafers W1 together.
[0028] 1 shows the boundary surface between the interlayer insulating film 13 and the interlayer insulating film 14 and the boundary surface between the metal pad 41 and the metal pad 38, but these boundaries generally cannot be observed after the above-mentioned annealing. However, the positions of these boundaries can be estimated by detecting, for example, the inclination of the side surface of the metal pad 41 or the side surface of the metal pad 38, or the positional deviation between the side surface of the metal pad 41 and the metal pad 38.
[0029] The semiconductor device of this embodiment may be traded in the state shown in FIG. 1 after being cut into a plurality of chips, or in the state shown in FIG. 4 before being cut into a plurality of chips. FIG. 1 shows the semiconductor device in the form of a chip, and FIG. 4 shows the semiconductor device in the form of a wafer. In this embodiment, a plurality of chip-shaped semiconductor devices (FIG. 1) are manufactured from one wafer-shaped semiconductor device (FIG. 4).
[0030] 5 to 20, the array chip 1 of this embodiment will be described in detail, specifically, the metal pads 46 and the structure around them will be described in detail. The following description also applies to the circuit wafer W2 of this embodiment.
[0031] FIG. 5 is a cross-sectional view showing the configuration of the semiconductor device according to the first embodiment.
[0032] 5, compared to the configuration shown in Fig. 1, the substrate 16 shown in Fig. 4 is not completely removed and is made thinner. The insulating film 12 and the source line SL shown in Fig. 1 are not shown in Fig. 5. A structure 18 and insulating layers 61 and 62 are further provided in Fig. 5. Reference numeral 111 denotes a stack of the memory cell array 11, and reference numeral 112 denotes a columnar portion of the memory cell array 11.
[0033] As shown in FIG. 5, the array chip 1 includes a substrate 16, metal pads 46, via plugs 45, a structure 18, and insulating layers 61 and 62.
[0034] The substrate 16 is disposed on the opposite side to the bonding surface (joint surface) S with the circuit chip 2. The substrate 16 also includes a surface F1 and a surface F2 opposite to the surface F1. The surface F1 faces the bonding surface S, and the memory cell array 11 is provided between the surface F1 and the bonding surface S. The substrate 16 also includes an opening 16a in the region A1 that extends from the surface F2 to the surface F1. The region A1 is a region where wiring is formed by wire bonding WB, as will be described later.
[0035] The metal pads 46 are provided in the openings 16a. The metal pads 46 are electrically connected in the region A1 by wire bonding WB. In the example shown in Fig. 5, two metal pads 46 are provided. However, the number of metal pads 46 is not limited to this. The material of the metal pads 46 is, for example, aluminum (Al).
[0036] The via plug 45 is provided between the surface F1 and the bonding surface S, and is electrically connected to the metal pad 46. As shown in FIG. 5, the via plug 45 is connected to the transistor 31, which is a part of the control circuit. That is, the via plug 45 is electrically connected to the control circuit provided in the circuit chip 2. The via plug 45 is formed, for example, at approximately the same time as the columnar portion 112 (for example, the contact plug 22 in FIG. 1) of the memory cell array 11. Therefore, the material of the via plug 45 is the same as the material of the contact plug 22, and is, for example, tungsten. The via plug 45 is not limited to a columnar portion, and may be a structure having another shape. This structure may include a wiring layer connected to the via plug 45.
[0037] The structural body 18 is provided between the face F1 and the bonding face S in the region A1.
[0038] As described above, as one method for connecting a semiconductor device to an external mounting board or device, it is known to form wiring on the metal pad 46 by wire bonding WB. In the wire bonding WB, a weight is applied to the metal pad 46 for a certain period of time by a bonding tool such as a capillary. Therefore, stress is applied to the semiconductor device during wire bonding. Here, the metal pad 46 electrically connected to the transistor 31 is provided by removing the substrate 16 as shown in the region A1. Therefore, the strength of the region A1 may be reduced. For example, the memory cell array 11, the transistor 31, the via plug 45, or the wiring layer, which are arranged directly under or around the opening 16a, may be mechanically destroyed by the stress.
[0039] Therefore, in the first embodiment, a structure 18 that functions as a film for countering stress during wire bonding is provided directly under the opening 16a. The structure 18 has, for example, a highly rigid or robust structure. This can improve the load resistance and impact resistance. As a result, the effect of the stress applied to the semiconductor device during wire bonding can be mitigated.
[0040] In the example shown in FIG. 5, the structure 18 is a laminated body that is laminated so as to correspond to the laminated body 111 of the memory cell array 11. As described in FIG. 2, the memory cell array 11 has a laminated body 111 including a plurality of word lines WL (conductive layers) and a plurality of insulating layers 51 that are alternately laminated in the Z direction perpendicular to the face F1. Therefore, the structure 18 has a laminated body 181 including two types of insulating layers 181a and 181b that are alternately laminated so as to correspond to the laminated body 111. This is because the structure 18 (laminate 181) is formed at approximately the same time as the memory cell array 11 in the process of forming the memory cell array 11. Therefore, the insulating layer 181a has approximately the same position and thickness from the face F1 as the word lines WL. Moreover, the insulating layer 181b has approximately the same position and thickness from the face F1 as the insulating layer 51.
[0041] Moreover, one of the two types of insulating layers 181a, 181b of the laminate 181 is the same as the insulating layer 51 of the laminate 111. In the example shown in FIG. 5, the insulating layer 181b is, for example, a silicon oxide film. Therefore, the material of the insulating layer 181b is the same as the material of the insulating layer 51. On the other hand, the insulating layer 181a is, for example, a silicon nitride film. Silicon nitride (SiN) has a higher strength than silicon oxide (SiO2) of the interlayer insulating film 13. This provides the structure 18 with a high strength.
[0042] Here, as a method for forming the stack 111 of the memory cell array 11, for example, a method is known in which the sacrificial layer is selectively removed from a stack including the sacrificial layer and the insulating layer 51, and the resulting cavity is filled with a metal such as tungsten. This sacrificial layer corresponds to the insulating layer 181a. Therefore, in the process of forming the memory cell array 11 up to the point where the sacrificial layer is replaced with the word line WL, the stack 181 is formed substantially simultaneously with the memory cell array 11.
[0043] Fig. 6 is a bird's-eye view showing the arrangement of the structures 18 and the via plugs 45 according to the first embodiment. Fig. 6 is a view of the opening 16a as viewed from the Z direction in Fig. 5. In the example shown in Fig. 6, the via plugs 45 are arranged in two rows and two columns for one metal pad 46.
[0044] 6, the structure 18 is disposed so as not to come into contact with the via plug 45. That is, the interlayer insulating film 13 is provided between the insulating layers 181a, 181b of the structure 18 and the via plug 45. The structure 18 is formed so as to open the periphery of the via plug 45, for example.
[0045] 6, the structures 18 are provided within the range of the metal pads 46. However, this is not limiting, and the structures 18 may be provided outside the range of the metal pads 46. From the viewpoint of strength, it is preferable that the structures 18 are arranged more widely, but this may be changed depending on the arrangement of other components in the array chip 1.
[0046] 5, the insulating layer 61 is provided in the opening 16a so that in the region A1, at least a portion of the metal pad 46 is exposed on the surface F2 side of the substrate 16. The insulating layer 61 is, for example, a silicon oxide film.
[0047] The insulating layer 62 is provided on the side surfaces of the array chip 1 and the circuit chip 2 so as to cover the connection between the array chip 1 and the circuit chip 2. In the example shown in FIG. 5, the metal pads 38, 41 used for bonding the array chip 1 and the circuit chip 2 are exposed from the interlayer insulating films 13, 14. By covering the metal pads 38, 41 with the insulating layer 62, contamination of the metal pads 38, 41 due to impurity mixing during the manufacturing process can be suppressed. The insulating layer 61 is, for example, a silicon oxide film. More specifically, the material of the insulating layer 62 is the same as the material of the insulating layer 61. This is because the insulating layers 61, 62 are formed collectively, as will be described later. In FIG. 5, the side surfaces of the array chip 1 and the circuit chip 2 on which the insulating layer 62 is provided correspond to the peripheral side surfaces of the wafer. On the other hand, in FIG. 5, the side surface opposite to the side surface on which the insulating layer 62 is provided is a continuous arbitrary cross section.
[0048] Next, a method for manufacturing a semiconductor device will be described.
[0049] 7 to 14 are cross-sectional views showing the method for manufacturing the semiconductor device according to the first embodiment.
[0050] First, as shown in Fig. 7, the memory cell array 11 and via plugs 45 are formed on the surface F1 of the substrate 16 including the surface F1 and the surface F2 opposite to the surface F1, and the structures 18 are formed in the area A1 on the surface F1. Note that the orientation of the array wafer W1 in Fig. 7 is opposite to that of the array chip 1 in Fig. 5. More specifically, the structures 18 are formed in parallel with the formation of the memory cell array 11, as described above.
[0051] As described with reference to FIG. 3, the transistor 31, wiring, and the like are formed on the substrate 15.
[0052] Next, as shown in FIG. 8, the array wafer W1 and the circuit wafer W2 are bonded together. That is, the array wafer W1 having the substrate 16 is bonded to the circuit wafer W2 on which a control circuit for controlling the memory cell array 11 is formed. The substrate 16 is ground by back grinding. The side surfaces Ws of the array wafer W1 and the circuit wafer W2 are polished by, for example, trimming. The side surfaces Ws refer to the outer peripheral side surfaces of the wafers. In the example shown in FIG. 8, the metal pads 38 and 41 at the bonding interface are exposed by polishing the side surfaces Ws.
[0053] 9, an opening 16a is formed in region A1, extending from face F2 to face F1 of substrate 16. For example, a silicon oxide film is formed on face F2 of substrate 16, and RIE (Reactive Ion Etching) is performed using a resist mask to form opening 16a. At the bottom of opening 16a, via plug 45 is exposed from interlayer insulating film 13.
[0054] 10, an aluminum film 46a is formed on the face F2 and the opening 16a. The aluminum film 46a is formed so as to extend along the bottom of the opening 16a, as well as along the side surfaces and face F2 of the substrate 16.
[0055] Next, as shown in FIG. 11, the aluminum film 46a is processed using a resist mask to form a metal pad 46 electrically connected to the via plug 45 within the opening 16a.
[0056] 12, an insulating layer 63 is formed to cover the surface F2, the opening 16a, the metal pad 46, and the side surface Ws of the substrate 16. This allows the metal pads 38, 41 at the bonding interface exposed from the side surface Ws and the upper surface and side surface of the substrate 16 to be substantially simultaneously covered with the insulating layer 63. The insulating layer 63 is, for example, a silicon oxide film. The insulating layer 63 is formed using, for example, TEOS (Tetra-ethoxy silane) or the like.
[0057] Next, as shown in Fig. 13, the upper surface of the insulating layer 63 is polished by CMP until the surface F2 of the substrate 16 is exposed. As a result, the insulating layer 63 is separated into the insulating layer 61 and the insulating layer 62. That is, the insulating layer 61 provided in the opening 16a and the insulating layer 62 provided on the side surface Ws are formed in parallel. The insulating layer 62 is provided on the side surface Ws so as to cover the connection portion between the array wafer W1 and the circuit wafer W2. That is, the metal pads 38, 41 remain covered by the insulating layer 62 even after polishing by CMP.
[0058] 14, a passivation film 47 is formed on face F2 and the upper surface of the insulating layer 61. For example, a thick-film resist such as PI (Polyimide) is applied, and exposed, developed, and processed by RIE. This makes it possible to form an opening P that exposes the metal pad 46. Thereafter, the semiconductor device of FIG. 5 is completed by being singulated.
[0059] As described above, according to the first embodiment, the metal pad 46 is provided in the opening 16a of the substrate 16 in the region A1 where wire bonding is performed. Furthermore, the structure 18 is provided between the face F1 and the bonding face S in the region A1. The structure 18 has high strength and can suppress the influence of mechanical stress applied to the semiconductor device during wire bonding. As a result, even if wire bonding is performed on the metal pad 46 directly above the via plug 45, the influence of mechanical stress on the via plug 45 and the like can be suppressed. Furthermore, since it is no longer necessary to consider the stress during wire bonding, the design freedom of the semiconductor element, wiring, and the like can be improved.
[0060] Moreover, the structures 18 are formed substantially simultaneously with the memory cell array 11 in the process of forming the memory cell array 11. Therefore, it is possible to suppress an increase in the number of processes for forming the structures 18. Note that the structures 18 do not necessarily have to be formed by utilizing the process for forming the memory cell array 11. The stacked body 181 may be formed separately from the memory cell array 11, for example, as a robust stacked body or the like.
[0061] FIG. 15 is a cross-sectional view showing the configuration of a semiconductor device according to a comparative example.
[0062] As a method for suppressing the influence of stress when the structure 18 is not provided, it is possible to arrange the metal pad 46 so that it is drawn out in the lateral direction (horizontal direction) of FIG. 15, as shown in FIG. 15. In this case, wire bonding WB is performed in an opening P that is arranged away from the opening 16a directly above the via plug 45. However, it is necessary to ensure the distance L from the opening 16a to the opening P. In other words, an extra arrangement space is required to draw out the metal pad 46, which hinders the reduction of the chip size.
[0063] In contrast to this, in the first embodiment, wiring can be formed directly in the opening P in the region A1 by wire bonding WB without drawing out the metal pad 46 in the lateral direction. As a result, the chip area can be reduced.
[0064] In the comparative example shown in FIG. 15, the metal pad 46 near the sidewall of the opening 16a is formed with a high aspect ratio. Therefore, there is a possibility that a disconnection (step) occurs in the metal pad 46 at the edge of the opening 16a, resulting in a connection failure. In addition, in order to extract the metal pad 46, it is necessary to form a multilayer film of the metal pad 46 and insulating layers 61a, 61b, etc. on the step caused by the substrate 16, which complicates the process. The insulating layers 61a, 61b are, for example, silicon oxide films. In addition, in the structure shown in FIG. 6, it is difficult to form the insulating layer 62 as a protective film on the side of the chip.
[0065] In contrast, in the first embodiment, the metal pad 46 can be provided along the surface F1 (flat surface) in the opening 16a. The metal pad 46 is provided between the surface F1 and the surface F2 because it is not necessary to pull it out laterally. This makes it possible to suppress step disconnection of the metal pad 46 due to the high aspect ratio. In addition, the insulating layer 61 is provided from the surface F1 to the surface F2 in the opening 16a. That is, the lower surface and the upper surface of the insulating layer 61 are provided flush with the surfaces F1 and F2 of the substrate 16, respectively. Therefore, the metal pad 46 and the insulating layer 61 can be formed more easily without using a complex multilayer film. In addition, the insulating layer 62 can be formed collectively with the insulating layer 61, and the process can be shared. As a result, the insulating layer 62 can be formed more easily.
[0066] Second embodiment 16 is a cross-sectional view showing the configuration of a semiconductor device according to the second embodiment. The second embodiment differs from the first embodiment in that a structure 18 is disposed so as to be in contact with a via plug 45.
[0067] 16, the structures 18 are provided continuously across the region A1, as compared to the first embodiment of FIG 5. Also, the via plugs 45 are provided so as to penetrate the structures 18.
[0068] FIG. 17 is a perspective view showing the arrangement of the structures 18 and the via plugs 45 according to the second embodiment.
[0069] As shown in FIG. 17, the laminate 181 is provided so as to come into contact with the via plug 45. Since the insulating layers 181a and 182b are insulators, even if they come into contact with the via plug 45, a short circuit between the via plugs 45 does not occur. Therefore, the operation of the control circuit including the transistor 31 is not affected. In addition, the layout area of the structure 18 can be increased, and the robustness of the structure 18 can be improved. In addition, the structure 18 can directly support the via plug 45, and the effect of stress on the via plug 45 can be further suppressed. As a result, the effect of stress during wire bonding can be further suppressed.
[0070] In the second embodiment, an opening of the structure 18 around the via plug 45 as shown in Fig. 6 of the first embodiment is not provided. Therefore, the stack 181 can be formed approximately uniformly, similar to the stack 111 of the memory cell array 11. As a result, the structure 18 can be formed more easily than in the first embodiment.
[0071] Other configurations of the semiconductor device according to the second embodiment are similar to the corresponding configurations of the semiconductor device according to the first embodiment, and therefore detailed description thereof will be omitted. The semiconductor device according to the second embodiment can obtain the same effects as the second embodiment.
[0072] Third embodiment 18 is a cross-sectional view showing the configuration of a semiconductor device according to the third embodiment. The third embodiment differs from the first embodiment in that a metal layer is included in the laminate of the structure 18.
[0073] The structural body 18 has a laminate 182 including a plurality of metal layers 182a and a plurality of insulating layers 182b that are alternately laminated to correspond to the laminate 111 and are electrically disconnected from the via plugs 45. This is because the structural body 18 (laminate 182) is formed substantially simultaneously with the memory cell array 11 in the process of forming the memory cell array 11. Therefore, the position and thickness of the metal layers 182a from the face F1 are substantially the same as those of the word lines WL. Moreover, the position and thickness of the insulating layers 182b from the face F1 are substantially the same as those of the insulating layer 51.
[0074] The material of the metal layer 182a is the same as the material of the word lines WL of the laminate 111, for example, tungsten. The tungsten of the metal layer 182a has a strength higher than that of the silicon oxide of the interlayer insulating film 13. This provides the structure 18 with high strength. The material of the insulating layer 182b is the same as the material of the insulating layer 51 of the laminate 111. The insulating layer 182b is, for example, a silicon oxide film.
[0075] In the third embodiment, the insulating layer 181a, which is the sacrificial layer in the first embodiment, is replaced with a metal layer 182a. Therefore, in the process of forming the memory cell array 11, including the replacement process, the stacked body 182 is formed substantially simultaneously with the memory cell array 11.
[0076] FIG. 19 is a perspective view showing the arrangement of the structures 18 and the via plugs 45 according to the third embodiment.
[0077] 19, the structure 18 is disposed so as not to come into contact with the via plug 45. That is, an interlayer insulating film 13 is provided between the metal layer 182a of the structure 18 and the via plug 45. This makes it possible to suppress short circuits between the via plugs 45. The metal layer 182a is, for example, in an electrically floating state. The structure 18 is formed so as to open the periphery of the via plug 45, for example.
[0078] Other configurations of the semiconductor device according to the third embodiment are similar to the corresponding configurations of the semiconductor device according to the first embodiment, and therefore detailed description thereof will be omitted. The semiconductor device according to the third embodiment can obtain the same effects as the first embodiment.
[0079] (Fourth embodiment) 20 is a cross-sectional view showing the configuration of a semiconductor device according to the fourth embodiment. The fourth embodiment differs from the first embodiment in that the structure 18 is not a laminate.
[0080] In the example shown in FIG. 20, the structure 18 is a columnar portion 183 provided to correspond to the columnar portion 112 of the memory cell array 11. The memory cell array 11 has the columnar portion 112 provided along the Z direction so as to be connected to the stacked body 111. The columnar portion 112 is, for example, the contact plug 22 shown in FIG. 1. However, the present invention is not limited to this, and the columnar portion 112 may be another contact plug in the memory cell array 11. The structure 18 has a plurality of columnar portions 183 provided along the Z direction. That is, the columnar portion 183 is provided to be approximately parallel to the columnar portion 112. As shown in FIG. 19, the columnar portion 183 is not connected to the wiring layer 44, unlike the via plug 45. Therefore, the columnar portion 183 is in an electrically floating state.
[0081] The columnar portion 183 is not limited to a metal, and may be an insulator. In this case, the material of the columnar portion 112 formed substantially simultaneously with the columnar portion 183 may be the same as the material of the columnar portion CL shown in FIG. 1 or the material of a columnar portion provided to support the staircase structure portion 21 during replacement. The structure 18 does not necessarily have to be formed using a process for forming the memory cell array 11. The columnar portion 183 may be formed separately from the memory cell array 11, for example, as a robust columnar portion.
[0082] Other configurations of the semiconductor device according to the fourth embodiment are similar to the corresponding configurations of the semiconductor device according to the first embodiment, so detailed description thereof will be omitted. The semiconductor device according to the fourth embodiment can obtain the same effects as the first embodiment. The semiconductor device according to the fourth embodiment may be combined with the first to third embodiments. In this case, the structure 18 may have both the stacked bodies 181, 182 and the columnar portion 183.
[0083] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope of the invention and its equivalents described in the claims, as well as in the scope and spirit of the invention.
[0084] (Additional Note) The following will addendum to the contents of the above-described embodiment. (Appendix 1) The pad is provided along the first surface within the opening. (Appendix 2) The pad is provided between the first surface and the second surface. (Appendix 3) The third stack is provided so as to be in contact with the first structure. (Appendix 4) A semiconductor device, wherein the material of one of the two types of insulating layers of the third stack is the same as the material of the insulating layer of the first stack. (Appendix 5) the material of the metal layer of the second stack is the same as the material of the conductive layer of the first stack, A semiconductor device, wherein the material of the insulating layer of the second stack is the same as the material of the insulating layer of the first stack. (Appendix 6) the semiconductor device further comprising a first insulating layer provided in the opening such that at least a portion of the pad is exposed on the second surface side of the substrate in the first region. (Appendix 7) 7. The semiconductor device according to claim 6, wherein the first insulating layer is provided from the first surface to the second surface within the opening. (Appendix 8) the semiconductor device further comprising a second insulating layer provided on a side surface of the first chip and the second chip so as to cover a connection portion between the first chip and the second chip. (Appendix 9) The semiconductor device described in Appendix 8, wherein the material of the second insulating layer is the same as the material of the first insulating layer provided in the opening so that at least a portion of the pad in the first region is exposed on the second surface side of the substrate. (Appendix 10) The first structure is electrically connected to the control circuit provided in the second chip. (Appendix 11) polishing the side surfaces of the first wafer and the second wafer; The method for manufacturing a semiconductor device further comprises forming in parallel a first insulating layer provided within the opening so that at least a portion of the pad in the first region is exposed on the second surface side of the substrate, and a second insulating layer provided on the side so as to cover a connection portion between the first wafer and the second wafer. (Appendix 12) 12. The method for manufacturing a semiconductor device described in appendix 11, further comprising forming a third insulating layer covering the second surface, the opening, and the side surface of the substrate, and polishing the third insulating layer until the second surface of the substrate is exposed, thereby forming the first insulating layer provided in the opening and the second insulating layer provided on the side surface in parallel. (Appendix 13) The method for manufacturing a semiconductor device further comprises forming the second structure in parallel with forming the memory cell array. [Explanation of symbols]
[0085] 1 array chip, 2 circuit chip, 11 memory cell array, 111 stack, 112 columnar portion, 16 substrate, 16a opening, 18 structure, 181 stack, 181a insulating layer, 181b insulating layer, 182 stack, 182a metal layer, 182b insulating layer, 183 columnar portion, 31 transistor, 45 via plug, 46 metal pad, 51 insulating layer, 61 insulating layer, 62 insulating layer, 63 insulating layer, A1 region, F1 surface, F2 surface, W1 array wafer, W2 circuit wafer, WL word line
Claims
1. a first chip having a memory cell array provided thereon; and a second chip connected to the first chip and having a control circuit for controlling the memory cell array provided thereon; The first chip includes: a first insulating layer including a first surface disposed on an opposite side to a bonding surface with the second chip, the memory cell array being provided between the first surface and the bonding surface, a second surface opposite to the first surface, and a connection terminal region in a first region; a connection terminal provided so as to be at least partially exposed in the connection terminal area; a first structure provided between the first surface and the bonding surface and electrically connected to the connection terminal; a second structure provided between the first surface and the joining surface in the first region; an interlayer insulating film provided between a first stacked body included in the memory cell array and the first structure; the connection terminal and the second structure have an overlapping portion in a top view, the second structure and the interlayer insulating film have different materials; the connection terminal electrically connects the first chip to an outside; A plurality of the first structures are provided below the connection terminal, and the second structure is provided between the plurality of the first structures, the memory cell array has a first stack including a plurality of conductive layers and a plurality of insulating layers alternately stacked in a first direction perpendicular to the first surface; The second structure has a third stack including a plurality of metal layers and a plurality of insulating layers alternately stacked to correspond to the first stack and insulated from the first structure; The semiconductor device further comprises a bonding wire connected to the connection terminal in the first region.
2. 2. The semiconductor device according to claim 1, wherein the first chip has a first bonding pad located on the bonding surface, the second chip has a second bonding pad located on the bonding surface, and the first bonding pad and the second bonding pad are electrically connected.
3. The semiconductor device according to claim 2 , wherein the first structure is provided at a position overlapping the connection terminal and the second bonding pad in a top view.
4. 2. The semiconductor device according to claim 1, wherein the first chip further includes a substrate arranged on the opposite side of the bonding surface with the second chip, the substrate including a third surface on which the memory cell array is provided between the opposing bonding surfaces, a fourth surface opposite the third surface, and an opening extending from the fourth surface to the third surface in the first region, the first insulating layer being provided therein.
5. the material of the metal layer of the third stack is the same as the material of the conductive layer of the first stack, The semiconductor device according to claim 1 , wherein a material of the insulating layer of said third stack is the same as a material of the insulating layer of said first stack.
6. The semiconductor device according to claim 4 , wherein said first insulating layer is provided from said third surface to said fourth surface within said opening.
7. the first chip is provided in a first wafer, the second chip is provided in a second wafer, and a second insulating layer is provided on a side surface of the first wafer and the second wafer so as to cover a connection portion between the first wafer and the second wafer; 5. The semiconductor device according to claim 4, wherein the material of the second insulating layer is the same as the material of the first insulating layer provided in the opening so that at least a portion of the connection terminal in the first region is exposed on the fourth surface side of the substrate.
8. The semiconductor device according to claim 4 , wherein the connection terminal is provided along the third surface within the opening.
9. The semiconductor device according to claim 4 , wherein the connection terminal is provided between the third surface and the fourth surface.
10. forming a first stacked body in a memory cell array region on a third surface of a substrate including a third surface and a fourth surface opposite to the third surface, and forming a first structure and a second structure as a second stacked body in a first region on the third surface; bonding a first wafer having the substrate to a second wafer having a control circuit for controlling the memory cell array formed thereon; forming an opening extending from the fourth surface to the third surface of the substrate in the first region; forming a connection terminal in the opening, the connection terminal being electrically connected to the first structure; forming a third insulating layer covering the fourth surface of the substrate, the opening, and side surfaces of the first wafer and the second wafer, and polishing the third insulating layer until the fourth surface of the substrate is exposed, thereby forming a first insulating layer and a second insulating layer in the opening and on the side surfaces, respectively; forming the second structure simultaneously with a first stack of the memory cell array; The method for manufacturing a semiconductor device further comprises forming a bonding wire in the first region, the bonding wire being connected to the connection terminal.
11. polishing the side surfaces of the first wafer and the second wafer before forming the third insulating layer; 11. The method for manufacturing a semiconductor device according to claim 10, further comprising forming the first insulating layer and the second insulating layer in the opening and on a side surface of a connection portion between the first wafer and the second wafer, respectively, to cover the connection portion between the first wafer and the second wafer.
Citation Information
Patent Citations
Semiconductor device and package
JP1999354562A
Pad structure of semiconductor device
JP2011109055A
Semiconductor storage device and manufacturing method of the same
JP2016062901A
Semiconductor device, solid-state image pickup device and manufacturing method
JP2018073967A
Storage device
JP2018148071A