Structure, manufacturing method, and gel for manufacturing microstructure

A triblock copolymer with alternating hydrophobic and hydrophilic segments addresses the distortion issue in ImpFab methods, ensuring precise pattern retention and reduced deformation in micro and nanostructures.

JP7584619B2Active Publication Date: 2024-11-15FUJIKURA LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023500583
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-02-19
Filing Date
2021-12-21
Publication Date
2024-11-15
Estimated Expiration
2041-12-21

AI Technical Summary

Technical Problem

Conventional implosion fabrication (ImpFab) methods using radical polymerization result in hydrogels with irregular mesh structures, leading to distortion during dehydration and contraction, especially in micro and nanostructures.

Method used

Employing a multi-block copolymer with alternating hydrophobic and hydrophilic segments, specifically a triblock copolymer with a total of 3 segments, to form a structure that suppresses distortion by precise control of polymer matrix uniformity and crosslinking.

Benefits of technology

The method maintains structural integrity during dehydration, reducing distortion in micro and nanostructures, enabling precise pattern retention and enhanced resolution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007584619000001
    Figure 0007584619000001
  • Figure 0007584619000002
    Figure 0007584619000002
  • Figure 0007584619000003
    Figure 0007584619000003
Patent Text Reader

Abstract

The purpose of the present invention is to provide a structure which has reduced distortion compared with structures produced employing the conventional InpFab method. A structure (10) has a micro-structure or a nano-structure, and contains a polymeric block copolymer, in which the polymeric block copolymer is composed of a first segment (111) and a second segment (112), each of which is composed of one or more block polymers and which respectively have hydrophobicity and hydrophilicity, bonded alternately, and the total number of the segments is 3 or more.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a structure including a microstructure or nanostructure and a manufacturing method thereof. [Background technology]

[0002] Implosion Fabrication (hereinafter referred to as IFA) is a method for producing a structure having a microstructure, which is a micrometer-scale structure, or a nanostructure, which is a nanometer-scale structure. m The pFab) method is known (see Patent Document 1 and Non-Patent Document 1).

[0003] I m In the pFab method, a hydrogel that is swollen with a lot of water is exposed to light to pattern the hydrogel, and the patterned hydrogel is then shrunk by dehydration. If the shrinkage rate of the hydrogel due to dehydration is, for example, 1 / 10, then shrinking the patterned hydrogel theoretically achieves a resolution 10 times higher than that obtained during patterning. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] US Patent Application Publication No. 2017 / 0081489 [Non-patent literature]

[0005] [Non-Patent Document 1] Daniel Oran et. al.,Science 362, 1281-1285 (2018) 14 December 2018 Summary of the Invention [Problem to be solved by the invention]

[0006] In FIGS. 1A and 1B of Patent Document 1, the polymer matrix of the hydrogel is depicted as having a regular mesh structure. However, the structure of the actual polymer matrix of the hydrogel is irregular, as depicted in (A), (C), and (E) of Fig. 1 of Non-Patent Document 1. This irregular structure is caused by the fact that the hydrogel polymer matrix used in Patent Document 1 and Non-Patent Document 1 is produced by a radical polymerization method. In general, hydrogels are synthesized using this radical polymerization method and have a non-uniform mesh structure.

[0007] When the patterned hydrogel is dehydrated and shrunk, the pattern of the resulting structure is distorted due to the irregular mesh structure of the polymer matrix (see Fig. 4 (A) and (C) in Non-Patent Document 1). This distortion becomes more pronounced the smaller the structures contained in the structure. This is clear when comparing the structure in Fig. 4 (A), which is an example of a microstructure, with Fig. 4 (C), which is an example of a nanostructure.

[0008] One aspect of the present invention has been made in view of the above-mentioned problems, and its object is to provide a method for manufacturing a semiconductor device using a conventional I m The object of the present invention is to provide a structure in which distortion is suppressed compared to structures produced using the pFab method, and a method for producing the same. [Means for solving the problem]

[0009] In order to solve the above problems, a structure according to one embodiment of the present invention has a microstructure or nanostructure, and contains a multi-block copolymer in which first and second segments, each of which is composed of one or more block polymers, are alternately bonded to each other, each of which has hydrophobic and hydrophilic properties, and the total number of segments is 3 or more.

[0010] In order to solve the above problems, a manufacturing method according to one embodiment of the present invention is a method for manufacturing a structure having a microstructure or a nanostructure, the method comprising: a first step of dispersing a dye in a multiblock copolymer that has been gelled by containing a solvent, the multiblock copolymer including first and second segments each composed of one or more block polymers, the first and second segments each having hydrophobicity and hydrophilicity being alternately bonded to each other, and the total number of segments being 3 or more; a second step of exposing the multiblock copolymer in which the dye has been dispersed to light to pattern it; a third step of removing the dye from the patterned multiblock copolymer; and a fourth step of shrinking the multiblock copolymer by removing the solvent from the multiblock copolymer from which the dye has been removed.

[0011] In order to solve the above problems, a gel for manufacturing a microstructure according to one embodiment of the present invention is a gel for manufacturing a microstructure for manufacturing a structure including a microstructure or a nanostructure, and contains a multi-block copolymer in which first and second segments, each of which is composed of one or more block polymers, are alternately bonded to each other, and the first and second segments, each of which has hydrophobicity and hydrophilicity, are bonded together, and the total number of segments is 3 or more. Effect of the Invention

[0012] According to one aspect of the present invention, the conventional I m It is possible to provide a structure with reduced distortion as compared to structures produced using the pFab method, and a method for producing the same. [Brief description of the drawings]

[0013] [Figure 1] FIG. 1A is a perspective view of a structure according to a first embodiment of the present invention, FIG. 1B is a schematic enlarged view of a portion of the structure shown in FIG. 1A, and FIG. 1C is a schematic view of two triblock copolymers contained in the structure shown in FIG. [Diagram 2](a) is the structural formula of the triblock copolymer shown in (b) and (c) of Figure 1. (b) is the structural formula of the dye shown in (b) and (c) of Figure 1. (c) is the structural formula of the cross-linking agent shown in (b) and (c) of Figure 1. [Diagram 3] FIG. 2 is a perspective view of a modified example of the structure shown in FIG. [Figure 4] FIG. 2 is a schematic diagram of a gel according to a second embodiment of the present invention. [Diagram 5] 10 is a flowchart of a manufacturing method according to a third embodiment of the present invention. [Figure 6] 6(a) to (e) are schematic diagrams of the gel or structure in each step included in the production method shown in FIG. [Figure 7] 5 is a flowchart of a modified example of the manufacturing method shown in FIG. [Figure 8] 8(a) to 8(c) are schematic diagrams of the gel or structure in each step included in the production method shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] [First embodiment] A structure 10 according to a first embodiment of the present invention will be described with reference to Fig. 1 and Fig. 2. Fig. 1(a) is a perspective view of the structure 10, Fig. 1(b) is a schematic diagram of an enlarged portion of the structure 10, and Fig. 1(c) is a schematic diagram of two triblock copolymers 11 contained in the structure 10. Fig. 2(a) is a structural formula of a specific example of the triblock copolymer 11, Fig. 2(b) is a structural formula of a specific example of the dye 12 contained in the structure 10, and Fig. 2(c) is a structural formula of a specific example of the cross-linking material 13 contained in the structure 10.

[0015] <Structure> In this embodiment, the shape of the structure 10 is a cube (see FIG. 1(a)). However, the shape of the structure 10 is not limited to this. The shape of the structure 10 can be appropriately determined according to the pattern of exposure performed in the exposure step (see FIG. 4 and FIG. 5(b)) included in the manufacturing method described later in the third embodiment. Furthermore, the structure 10 is not limited to a three-dimensional structure as shown in FIG. 1(a) and may be a two-dimensional structure.

[0016] In the structure 10 of this embodiment, 500 nm is adopted as the length L of one side. Therefore, the structure 10 has a nanostructure, which is a nanometer-scale structure. However, the structure of the structure 10 is not limited to a nanostructure, and may be a microstructure, which is a microscale structure. However, when manufacturing a structure using the existing ImpFab method, the smaller the size of the structure, the more likely it is that the shape will be distorted due to shrinkage that occurs in the dehydration and sintering process. Therefore, the effect obtained by the structure 10 and the manufacturing methods M10 and M20 (see Figs. 4 to 7) described later becomes more prominent as the size of the structure 10 becomes smaller. Specifically, the structure 10 and the manufacturing methods 10 and 20 can be suitably used when the minimum width of the pattern is less than 10 μm, and can be more suitably used when the minimum width of the pattern is less than 1 μm. Note that the nanometer-scale structure refers to a structure in which the minimum width of the pattern is less than 1 μm, and the micrometer-scale structure refers to a structure in which the minimum width of the pattern is less than 1 mm.

[0017] The structure 10 contains a triblock copolymer 11, a dye 12, and a cross-linking agent 13 (see FIG. 1(b)). In FIG. 1(c), two triblock copolymers 11 contained in the structure 10 are enlarged and diagrammatically illustrated.

[0018] (Triblock copolymer) Triblock copolymer 11, which is an example of a multiblock copolymer, is composed of hydrophobic segments 111 and hydrophilic segments 112 bonded alternately (see FIG. 1(c)). Segment 111 is an example of a first segment, and segment 112 is an example of a second segment.

[0019] In this embodiment, each of the segment 111 and the segment 112 is composed of one block polymer. However, the block polymer constituting the segment 111 has hydrophobic properties, and the block polymer constituting the segment 112 has hydrophilic properties. An example of the segment 111 and the segment 112 will be described later with reference to (a) of FIG. However, the segment 111 may be composed of a plurality of block polymers having hydrophobic properties, and the segment 112 may be composed of a plurality of block polymers having hydrophilic properties.

[0020] In addition, in the present embodiment, in the triblock copolymer 11, the segment 111, the segment 112, and the segment 111 are bonded in this order. In other words, the triblock copolymer 11 is composed of two segments 111 and a segment 112 interposed between these two segments 111. Therefore, the total number of segments in the triblock copolymer 11 is 3. However, the total number of segments is not limited to 3, and can be appropriately determined as long as it is 3 or more. In this way, the structure 10 may be a multi-block copolymer instead of a triblock copolymer. The total number of segments is preferably an odd number, and more preferably 3.

[0021] In the manufacturing methods M10 and M20 described later, a polymer gel (hydrogel in the manufacturing methods M10 and M20) obtained by swelling the triblock copolymer 11 in a solvent (water in the manufacturing methods M10 and M20) is used as an intermediate for manufacturing the structure 10 (hereinafter also referred to as a gel for manufacturing a microstructure). Since the total number of segments is an odd number, block polymers having the same polarity are located at both ends of the triblock copolymer 11. Therefore, when forming a polymer gel, the ends of the multiple triblock copolymers 11 can be easily aggregated together. In addition, since the total number of segments is 3, it is possible to prevent the portions other than the ends of the multiple triblock copolymers 11 from aggregating. Therefore, it is easy to make the pitch of the polymer matrix constituting the polymer gel uniform.

[0022] In the present embodiment, the triblock copolymer 11 is designed to use water, which is an example of a hydrophilic solvent, as a solvent when preparing a gel for producing a microstructure. Therefore, a triblock copolymer having segments 111 at both ends is used as the triblock copolymer 11. However, if a hydrophobic solvent is used when preparing a gel for producing a microstructure, a triblock copolymer having segments 112 at both ends may be used as the triblock copolymer 11.

[0023] (Pigments and crosslinking agents) 1(b) and (c), in at least one of the plurality of triblock copolymers 11, a dye 12 is bonded to a segment 112 interposed between two segments 111 at both ends. In addition, the dyes 12 are crosslinked to each other by a crosslinking agent 13. Therefore, at least some of the plurality of triblock copolymers 11 are crosslinked to each other via the dye 12.

[0024] When a triblock copolymer having segments 112 at both ends is used as the triblock copolymer 11, the dye 12 may be bonded to the segment 111 interposed between the two segments 112.

[0025] (Specific examples of block polymers, dyes, and crosslinkers) Examples of block polymers constituting the segments 111 and 112 constituting the triblock copolymer 11 include poly(butyl methacrylate) (PBMA) and poly(methacrylic acid) (PMMA), respectively. In the specific example shown in FIG. 2(a), the degree of polymerization n of the left-hand segment 111 is n=134, the degree of polymerization m of the segment 112 is m=273, and the degree of polymerization k of the right-hand segment 111 is k=192.

[0026] However, the block polymers constituting the segments 111 and 112 are not limited to PBMA and PMMA, respectively. As other block polymers constituting the segment 111, methacrylates and acrylates having an alkyl chain, such as poly(hexyl methacrylate) and poly(octyl methacrylate), are preferably used, but are not limited thereto, and polymers having a hydrophobic side chain, such as an alicyclic functional group or an alkyl fluoride, can be preferably used. As other block polymers constituting the segment 112, methacrylates and acrylates having a carboxylic acid group, such as poly(acrylic acid), are preferably used, but are not limited thereto, and can be polymers containing a functional group capable of reacting with a desired dye.

[0027] The segment 112 to which the dye 12 is bonded has a number average molecular weight (M n ) and polystyrene equivalent weight average molecular weight (M W ) ratio (M W / M n) is preferably 3 or less, more preferably 2 or less, and most preferably 1.2 or less. The narrower the molecular weight dispersion, the narrower the chain length distribution of the block polymer, so that a hydrogel with a more uniform knit structure can be formed. The molecular weight dispersion of the segment 112 may be appropriately determined according to the minimum width of the pattern in the microstructure or nanostructure of the structure 10 to be manufactured. The smaller the minimum width of the pattern, the smaller the molecular weight dispersion of the segment 112 is. It is preferable that the molecular weight dispersion of the segment 111 is also small, like the segment 112. The segment 111 and the segment 112 can be manufactured using a precision polymerization method such as living radical polymerization, so that the molecular weight dispersion can be reduced.

[0028] Moreover, the ratio of block components in the segment 112 is preferably 80% or more and 100% or less, more preferably 90% or more, when measured by 13C-NMR. The ratio of block components can be calculated from the sequence information in the triad in the 13C-NMR measurement. Here, the ratio of block components is defined as follows. (Ratio of block components) = (fractions that are all the same unit) / (total fractions) x 100 (%)

[0029] In addition, even if a block polymer is composed of multiple monomers, it will be counted in the above formula as long as all the triad components are the same. For example, in the case of a block copolymer composed of two types of monomers, A and B, it will be counted as an "AAA" fraction and a "BBB" fraction molecule, but other fractions containing different units such as "BAB" and "ABA" will not be counted in the above formula. By having the proportion of block components be 80% or more, it is possible to construct a gel with a more controlled structure and a knitted structure.

[0030] An example of the dye 12 is fluorescein, which is a fluorescent dye, or fluorescein in which the carboxyl group is replaced with a substituent R (see FIG. 2(b)). A cross-linking agent 13, which will be described later, is used as the substituent R. When the triblock copolymers 11 are not cross-linked to each other, as in a modified example of the structure 10, which will be described later, an amino group (NH2), a thiol group (SH), biotin, or the like can be used as the substituent R.

[0031] The cross-linking agent 13 is a cross-linking agent for aqueous resins, and an example thereof is 1,11-diazide-3,6,9-trioxaundecane, which is a diazide having a water-soluble skeleton (see FIG. 2(c)). When diazides or the like are used as cross-linking agents in a cross-linking reaction, it is preferable that the substituent introduced into the dye 12 is a functional group having an unsaturated double bond or triple bond.

[0032] <Modification of structure> A structural body 10A, which is a modified example of the structural body 10 shown in Fig. 1, will be described with reference to Fig. 3. Fig. 3 is a perspective view of the structural body 10A.

[0033] The structure 10A has a nanostructure, similar to the structure 10. In addition, similar to the structure 10, the structure 10A contains a triblock copolymer in which a first segment 111 having hydrophobicity and a second segment 112 having hydrophilicity are alternately bonded, and the total number of segments is three.

[0034] However, the triblock copolymer contained in the structure 10A is different from the triblock copolymer 11 contained in the structure 10 (FIGS. 1(b) and (c)) in that nanoparticles are bonded to the dye 12 instead of the crosslinker 13. In this modification, the nanoparticles and the high refractive index portion 102 will be described. The high refractive index portion 102 is a part of the triblock copolymer and is a region where the nanoparticles are bonded to the dye 12.

[0035] As described above, in the triblock copolymer contained in structure 10A, one of segments 111 and 112, i.e., segment 112 interposed between the two segments 111 at both ends, has dye 12 and nanoparticles bonded to it in this order.

[0036] The nanoparticles are configured so that the refractive index is greater than the refractive index of the polymer matrix including the segments 111 and 112. In this modification, gold nanoparticles, which are an example of metal, are used as the nanoparticles. However, the metal constituting the nanoparticles is not limited to gold, and may be, for example, silver, copper, or platinum. Further metal may be grown on the surface of the nanoparticles. Furthermore, the material constituting the nanoparticles is not limited to metal, and may be a semiconductor or an insulator, for example, carbon nanotubes, fullerene, titanium oxide, silica, and diamond. Furthermore, it is not necessary to use these alone, and they may be blends or alloys of these.

[0037] As a result, the refractive index of the region of the triblock copolymer where the dye 12 and the nanoparticles are bonded to the segment 112 is higher than the refractive index of the region where the dye 12 and the nanoparticles are not bonded to the segment 112. Hereinafter, the region where the dye 12 and the nanoparticles are not bonded to the segment 112 is referred to as a low refractive index section 101, and the region where the refractive index is higher than that of the low refractive index section 101 due to the nanoparticles is referred to as a high refractive index section 102.

[0038] In this modification, the shape of the low refractive index portion 101 is a rectangular parallelepiped block. The size of the low refractive index portion 101 is such that the length of each side of the pair of bottom walls is 4.5 μm, and the thickness is 1.5 μm.

[0039] In this modification, the shape of the high refractive index portion 102 is a columnar pillar. The size of the high refractive index portion 102 is such that the length L of each side of a pair of bottom surfaces is 500 nm, and the thickness is 1.5 μm. The high refractive index portion 102 is formed inside the low refractive index portion 101 so as to penetrate a pair of bottom walls of the low refractive index portion 101. The high refractive index portion 102 configured in this manner is an example of a nanostructure. In this modification, 16 high refractive index portions 102 are arranged in a matrix shape inside the low refractive index portion 101. In addition, in FIG. 3, only one of the 16 high refractive index portions 102 is marked with a reference symbol.

[0040] The shapes and sizes of the low refractive index portion 101 and the high refractive index portion 102 are not limited to those in this modified example and can be appropriately determined. The high refractive index portion 102 may be partially exposed from the low refractive index portion 101 as in this modified example, or may be embedded inside the low refractive index portion 101.

[0041] Second Embodiment A gel 10G according to a second embodiment of the present invention will be described with reference to Fig. 4. Fig. 4 is a schematic diagram of the gel 10G. For ease of explanation, the same reference numerals are given to members having the same functions as those described in the above embodiment, and the explanations thereof will not be repeated.

[0042] The gel 10G is an example of a gel for producing a microstructure for producing the above-mentioned structure 10 or structure 10A. The gel 10G contains water and a triblock copolymer in which the first segments 111 and the second segments 112, each of which is composed of one or more block polymers, are alternately bonded to each other, and the total number of segments is three. Note that the triblock copolymer may be a multi-block copolymer as described above.

[0043] The gel 10G is obtained by dispersing a triblock copolymer 11, which includes a segment 111 and a segment 112 and in which a dye 12 is not bound to the segment 112, in water, which is an example of a hydrophilic solvent, thereby causing it to swell.

[0044] The triblock copolymer 11 is configured to be composed of segments 111 having hydrophobic properties at both ends, and a hydrophilic segment 112 is interposed between the segments 111. By dispersing such a triblock copolymer 11 in water, a polymer matrix 14 as shown in FIG. 4 is formed. The polymer matrix 14 is composed of water as a solvent, pseudo crosslinking points 141 formed by aggregation of the segments 111, and segments 112 interposed between the two crosslinking points 141. Note that in FIG. 4, the polymer matrix 14 is illustrated as a two-dimensional structure to make the structure of the polymer matrix easier to understand, but the actual polymer matrix 14 has a three-dimensional structure.

[0045] As described above, the segment 111 and the segment 112 constituting the triblock copolymer 11 can be produced by using a precision polymerization method. Therefore, the block polymers constituting the segment 111 and the segment 112 have a small molecular weight dispersion. The molecular weight dispersion of the block polymers of the segment 111 and the segment 112 is, for example, preferably 2 or less, and more preferably 1.2 or less. In this way, by precisely controlling the degree of polymerization of each of the segment 111 and the segment 112, it is possible to suppress the variation that may occur in the pitch p between the crosslinking points 141 in the polymer matrix 14.

[0046] In this embodiment, the polymer matrix 14 is formed using a triblock copolymer in which the segments 111 are located at both ends and the segments 112 are interposed between the segments 111, so water, which is an example of a hydrophilic solvent, is used as the solvent. Examples of hydrophilic solvents other than water include dimethyl sulfoxide (DMSO) and dimethylformamide (DMF).

[0047] Furthermore, when the polymer matrix 14 is formed using a triblock copolymer in which the segments 112 are located at both ends and the segments 111 are interposed between the segments 112, a hydrophobic solvent may be used as the solvent. Examples of the hydrophobic solvent include normal hexane and cyclohexane.

[0048] Third embodiment A manufacturing method M10 according to a third embodiment of the present invention, which is suitable for manufacturing the structure 10A shown in FIG. 3, will be described with reference to FIG. 5 and FIG. 6. FIG. 5 is a flow chart of the manufacturing method M10. FIG. 6 is a schematic diagram of the gel 10G or the structure 10A in each step included in the manufacturing method M10. FIG. 6(a) is a schematic diagram of the gel 10G after the dye dispersion step S12, FIG. 6(b) is a schematic diagram of the gel 10G in the exposure step S13, FIG. 6(c) is a schematic diagram of the gel 10G after the nanoparticle addition step S15, FIG. 6(d) is a schematic diagram of the gel 10G after the nanoparticle growth step S17, and FIG. 6(e) is a schematic diagram of the structure 10A obtained by carrying out the dehydration and sintering step S18. For convenience of explanation, the same reference numerals are attached to members having the same functions as the members described in the above embodiment, and the explanations thereof will not be repeated. The manufacturing method M10 is described in Non-Patent Document 1. m It is based on the pFab method and uses gel 10G containing triblock copolymer 11.

[0049] As shown in FIG. 5, the manufacturing method M10 includes a gelling step S11, a dye dispersion step S12, an exposure step S13, a dye washing step S14, a nanoparticle adding step S15, a nanoparticle washing step S16, a nanoparticle growing step S17, and a dehydration / sintering step S18.

[0050] The gelation step S11 is a step for obtaining a gel 10G in which a triblock copolymer 11, in which first segments 111 and second segments 112 are alternately bonded and the total number of segments is 3, is swollen in water. Note that in the gelation step S11 of the present embodiment, the gel 10G is prepared using the triblock copolymer 11, but a multiblock copolymer in which the total number of segments is 4 or more may be used instead of the triblock copolymer 11.

[0051] The triblock copolymer 11 (see, for example, FIG. 2(a)) including the segment 111 and the segment 112 can be appropriately purchased from among commercially available products, taking into consideration the degrees of polymerization of the segment 111 and the segment 112. Alternatively, the segment 111 and the segment 112 having the desired degrees of polymerization may be produced by a precision polymerization method, and then the triblock copolymer 11 may be produced using these.

[0052] First, a solution of the triblock copolymer 11 in N,N-dimethylformamide (DMF) is prepared. The concentration of the triblock copolymer 11 is not particularly limited, but is, for example, 20% by weight. The solution is filled into a mold having a predetermined shape (rectangular in this embodiment). Next, a weak gel of the triblock copolymer 11 is obtained by exposing the surface of the solution to water vapor for several minutes. Next, the weak gel is immersed in water for three days to obtain a gel 10G.

[0053] If gel 10G containing the desired triblock copolymer 11 is commercially available, it may be purchased and the gelling step S11 may be omitted.

[0054] The dye dispersion step S12 is one aspect of the first step, and is a step of dispersing the dye 12 in the gel 10G (see FIG. 6(a)). In FIG. 6, the segment 111 constituting the triblock copolymer 11 is shown by double lines, and the segment 112 is shown by solid lines. Also, the reference numerals 111 and 112 are omitted from the illustration. The dye 12 used in this embodiment is fluorescein shown in FIG. 2(b) in which the carboxyl group has been replaced with an aminomethyl group.

[0055] The exposure step S13 is one aspect of the second step, and is a step of patterning by exposing a predetermined region of the triblock copolymer 11 constituting the gel 10G in which the dye 12 is dispersed (see FIG. 6(b)). The two-dot chain line shown in FIG. 6(b) shows a schematic representation of the region to be exposed. By absorbing the energy of the light irradiated by this exposure, the dye 12 bonds to the block polymer constituting the segment 112 (see FIG. 2(b)). In the gel 10G, which is a rectangular parallelepiped, an exposure process using a two-photon absorption method is suitable for exposing a desired region three-dimensionally. The exposure step S13, the nanoparticle addition step S15, the nanoparticle washing step S16, the nanoparticle growth step S17, and the dehydration and sintering step S18, which will be described later, are the same as those described above. m These steps are known as the pFab method, and therefore, in this embodiment, only a brief explanation of these steps will be given.

[0056] The dye washing step S14 is one aspect of the third step, and is a step of washing the gel 10G after patterning to remove the unreacted dye 12 remaining in the gel 10G. By carrying out this step, only the dye 12 bound to the segment 112 in the exposed area remains inside the structure 10. In other words, the dye 12 remains only in the area patterned by exposure.

[0057] The nanoparticle addition step S15 is a step of modifying the dye 12 with nanoparticles 15 (eg, made of gold) (see FIG. 6(c)).

[0058] The nanoparticle washing step S16 is a step of washing the gel 10G after the dye 12 has been modified with the nanoparticles 15 to remove the nanoparticles that are not bound to the dye 12 and remain in the gel 10G.

[0059] The nanoparticle growth step S17 is a step of increasing the content of the high refractive index material in the gel 10G by further growing the nanoparticles 15 modified with the dye 12 (see FIG. 6(d)). In FIG. 6(d), the nanoparticles 15 are shown by dashed lines, and the particles 16 after growth are shown by solid lines.

[0060] The dehydration and sintering step S18 is an embodiment of the fourth step, and is a step of removing water from the triblock copolymer 11 from which the dye 12 has been removed, thereby shrinking the triblock copolymer 11 and obtaining the structure 10A (see FIG. 6(e)). By carrying out this step, the gel 10G is reduced in size while maintaining a shape similar to that of the gel 10G before dehydration. In FIG. 6(e), the reduction ratio is set for convenience so that the size of the gel 10G is reduced to 1 / 2 by dehydration. However, the reduction ratio of the actual gel 10G due to dehydration is determined depending on the structure of the triblock copolymer 11 and the water content in the gel 10G (in other words, the degree of swelling). For example, in the triblock copolymer 11 of this embodiment (see FIG. 2(a)), when the water content in the gel 10G is about 83%, the reduction ratio due to dehydration is about 1 / 10.

[0061] At this time, as shown in FIG. 4, since there is little variation in the pitch p between the crosslinking points 141 in the polymer matrix 14 constituting the gel 10G, it is possible to suppress distortion that may occur with the contraction of the gel 10G. As a result, the region patterned in the exposure step S13 (the region shown by the two-dot chain line in FIG. 6(e)) is also reduced in size while maintaining a shape similar to that of the patterned region before dehydration. Therefore, in the structure 10A manufactured using the manufacturing method M10, the conventional I m Compared to structures fabricated using the pFab method, distortion can be suppressed.

[0062] The dehydration and sintering step S18 is carried out by heating the gel 10G after the nanoparticle growth step S17 in an oven. The temperature of the dehydration step is preferably set lower than the heat resistance temperature of the polymer used or the boiling point of the solvent in order to maintain a good shape. For example, in the case of a hydrogel based on water and acrylic acid, it is preferable to dry it at a temperature of 60°C to 95°C for about 30 to 120 minutes. It is also efficient to dry it in a vacuum after drying and shrinkage have progressed to a certain extent. The sintering temperature is preferably a temperature slightly lower than the melting point of the nanoparticles, and it is preferable to heat it as quickly as possible so as to melt only the surface of the nanoparticles. Exposure to high heat for a long period of time is likely to cause problems such as damage to the gel and oxidation of the metal nanoparticles. To prevent oxidation of the metal nanoparticles, sintering in an inert atmosphere or in a vacuum is preferable. Furthermore, the dehydration and sintering process may be a combination of a plurality of heating conditions. For example, in the first half of the dehydration process, the heating temperature of the oven is set to 90° C. and the heating time is set to 1 hour under atmospheric pressure to remove most of the water from the triblock copolymer 11, and then the mixture is dried for another 30 minutes while evacuating with a vacuum pump at the same temperature setting. In the subsequent sintering process, the particles 16 contained in the triblock copolymer 11 are sintered together by switching the heating temperature of the oven to 400° C. and the heating time to 3 minutes while continuing to evacuate. As a result, the particles 16 contained in the triblock copolymer 11 are fixed together, so that the strength of the high refractive index portion 102 (see FIG. 3) in the structure 10A can be increased. In addition, the sintering process is not limited to melting the nanoparticles by a heating method, and an instantaneous sintering method using irradiation with a laser or a flash xenon lamp may be adopted.

[0063] <Modification of manufacturing method> A manufacturing method M20, which is a modification of manufacturing method M10, will be described with reference to Figs. 7 and 8. Fig. 7 is a flowchart of manufacturing method M20. Fig. 8 is a schematic diagram of a gel or structure in each step included in manufacturing method M20. Fig. 8(a) is a schematic diagram of a gel after performing crosslinking step S25, Fig. 8(b) is a schematic diagram of a gel obtained by performing gel removal step S26, and Fig. 8(c) is a schematic diagram of structure 10 obtained by dehydration step S28.

[0064] 7, the manufacturing method M20 includes a gelation step S11, a pigment dispersion step S22, an exposure step S13, a pigment washing step S14, a crosslinking step S25, a gel removal step S26, and a dehydration step S28. The gelation step S11, the exposure step S13, and the pigment washing step S14 included in the manufacturing method M20 are the same as the gelation step S11, the exposure step S13, and the pigment washing step S14 included in the manufacturing method M10. Therefore, in this modification, the description of these steps will be omitted, and only the pigment dispersion step S22, the crosslinking step S25, the gel removal step S26, and the dehydration step S28 will be described.

[0065] The pigment dispersion step S22 is a step of dispersing the pigment 12 in the gel 10G, similar to the pigment dispersion step S12 included in the manufacturing method M10, but the pigment 12 used is different from that used in the pigment dispersion step S12. In this modification, the pigment 12 used is the fluorescein shown in Fig. 2(b) in which the carboxyl group has been replaced with a cross-linking agent 13 (Fig. 2(c)).

[0066] The crosslinking step S25 is an embodiment of the fifth step. The crosslinking step S25 is a step of irradiating ultraviolet light onto the gel 10G in which the dye 12 and the crosslinking agent 13 are bonded to the segments 112 in this order, thereby bonding the crosslinking agents 13 bonded to different segments 112. By this step, the triblock copolymers 11 are crosslinked to each other via the dye 12 and the crosslinking agent 13 (see FIG. 8(a)).

[0067] The gel removal step S26 is a step of decomposing the gel 10G in the region that is not cross-linked via the dye 12 and the cross-linking material 13 by immersing the gel 10G in a hydrophobic solvent or exposing the gel 10G to the vapor of the hydrophobic solvent. By this step, a gel 10G' that is cross-linked via the dye 12 and the cross-linking material 13 is obtained (see FIG. 8(b)).

[0068] The dehydration step S28 is one embodiment of the fourth step, similar to the dehydration / sintering step S18 of the manufacturing method M10, and is a step in which water is removed from the triblock copolymer 11 from which the dye 12 has been removed, thereby shrinking the triblock copolymer 11 and obtaining the structure 10 (see (e) of FIG. 6).

[0069] In the manufacturing method M20, the gel 10G containing the triblock copolymer 11 is used as in the manufacturing method M10. Therefore, in the structure 10 manufactured by the manufacturing method M20, the conventional I m Compared to structures fabricated using the pFab method, distortion can be suppressed.

[0070] Furthermore, in the manufacturing method M20, by carrying out the gel removal step S26, it is possible to decompose the gel 10G in the region of the gel 10G that has not been cross-linked via the dye 12 and the cross-linking agent 13. As a result, only the region of the gel 10G that has been patterned in the exposure step S13 can be obtained as the structure 10. Therefore, the manufacturing method M20 is different from the conventional I m It is possible to produce a structure 10 that could not be produced by the pFab method.

[0071] The structure according to the first aspect of the present invention has a microstructure or nanostructure, and contains a multi-block copolymer in which first and second segments, each of which is composed of one or more block polymers, are alternately bonded to each other, each of which has hydrophobic and hydrophilic properties, and the total number of segments is 3 or more.

[0072] The structure according to the first embodiment is a structure according to the I m The block polymer can be manufactured by applying the pFab method. The block polymer has a linear form, but since hydrophobic and hydrophilic segments are alternately bonded and the total number of segments is 3 or more, when the block polymer is dispersed in a hydrophilic or hydrophobic solvent, the segments having the opposite polarity to the solvent aggregate in the solvent, and this site becomes a physical crosslinking point, and a swollen gel form can be obtained. For example, when a block polymer consisting of three segments, a hydrophobic segment / hydrophilic segment / hydrophobic segment, is dispersed in water, the hydrophobic segments at both ends of the multiple block polymers aggregate together and become a physical crosslinking point, thereby forming a gel form. By the way, the block polymer constituting the first segment and the block polymer constituting the second segment can be manufactured by using a precision polymerization method, so that the polymerization degree of each block polymer can be precisely controlled. Therefore, in a gel obtained by swelling a multi-block copolymer with a solvent, the variation that may occur in the pitch between crosslinking points in the polymer matrix can be suppressed. Therefore, the present structure 10 has a structure different from the conventional I m Compared to structures fabricated using the pFab method, distortion can be suppressed.

[0073] In addition, in the structure according to the second aspect of the present invention, in addition to the configuration of the structure according to the first aspect described above, the multi-block copolymer is a triblock copolymer having a total number of segments of 3, and is composed of two of the first segments and a second segment interposed between the two first segments.

[0074] According to the above arrangement, a hydrophilic solvent (for example, water) can be used as the solvent for swelling the multi-block copolymer.

[0075] Furthermore, in a structure according to a third aspect of the present invention, in addition to the configuration of the structure according to the first or second aspect described above, a configuration is adopted in which, in each multi-block copolymer, a dye and a nanoparticle are bonded to the first segment or the second segment in this order, and the refractive index of the nanoparticle is greater than the refractive index of a polymer matrix including the first segment and the second segment.

[0076] According to the above configuration, it is possible to arbitrarily create within the structure a region that does not contain nanoparticles and has a low refractive index, and a region that contains nanoparticles and has a high refractive index.

[0077] Furthermore, in the structure according to the fourth aspect of the present invention, in addition to the configuration of the structure according to any one of the first to third aspects described above, a dye is bonded to the first segment or the second segment in each multi-block copolymer, and at least some of the multi-block copolymers are crosslinked with each other via the dye.

[0078] According to the above-mentioned configuration, in the process of producing the present structure, the gel obtained by swelling the multi-block copolymer can be decomposed in the region that is not cross-linked via the dye, and as a result, only the region of the gel that is cross-linked via the dye (i.e., the patterned region) can be obtained as the structure.

[0079] Furthermore, in the structure according to the fifth aspect of the present invention, in addition to the configuration of the structure according to any one of the first to fourth aspects described above, a configuration is adopted in which, in each multi-block copolymer, a dye is bonded to the first segment or the second segment, and the first segment or the second segment to which the dye is bonded has a molecular weight dispersity of 2 or less.

[0080] According to the above-mentioned configuration, in a gel obtained by swelling the multi-block copolymer with a solvent, it is possible to further suppress the variation that may occur in the pitch between crosslinking points in the polymer matrix. Therefore, the present structure is more advantageous than the conventional I m Compared to structures fabricated using the pFab method, distortion can be further suppressed.

[0081] Furthermore, in the structure according to the sixth aspect of the present invention, in addition to the configuration of the structure according to any one of the first to fifth aspects described above, a configuration is adopted in which, in each multi-block copolymer, a dye is bonded to the first segment or the second segment, and the proportion of block components constituting the first segment or the second segment to which the dye is bonded satisfies 80% or more and 100% or less when measured by 13C-NMR.

[0082] According to the above-mentioned configuration, since the ratio of the block component is 80% or more, a gel having a more controlled mesh structure can be constructed.

[0083] A manufacturing method according to a seventh aspect of the present invention is a method for manufacturing a structure having a microstructure or a nanostructure, the method comprising: a first step of dispersing a dye in a multiblock copolymer that has been gelled by containing a solvent, the multiblock copolymer comprising first and second segments, each of which is composed of one or more block polymers, the first and second segments each having hydrophobicity and hydrophilicity, which are alternately bonded to each other, and the total number of segments being 3 or more; a second step of exposing the multiblock copolymer in which the dye has been dispersed to light, thereby patterning the multiblock copolymer; a third step of removing the dye from the patterned multiblock copolymer; and a fourth step of shrinking the multiblock copolymer by removing the solvent from the multiblock copolymer from which the dye has been removed.

[0084] The block polymer constituting the first segment and the block polymer constituting the second segment can be produced by a precision polymerization method, which allows precise control of the degree of polymerization of each block polymer. Therefore, in a gel obtained by swelling a multi-block copolymer with a solvent, it is possible to suppress variations that may occur in the pitch between crosslinking points in the polymer matrix. Therefore, this production method is different from the conventional I m Compared to the pFab method, distortion that may occur in the structure can be suppressed.

[0085] Furthermore, the production method according to an eighth aspect of the present invention employs, in addition to the configuration of the production method according to the seventh aspect described above, a fifth step in which a crosslinking agent is bonded to the dye and at least some of the multi-block copolymers are crosslinked together using the crosslinking agent, the sixth step being carried out after the third step.

[0086] According to the above configuration, the same effects as those of the structure according to the fourth aspect of the present invention are achieved.

[0087] A gel for producing a microstructure according to a ninth aspect of the present invention is a gel for producing a microstructure including a microstructure or a nanostructure, and contains a multi-block copolymer in which first and second segments, each of which is composed of one or more block polymers, are alternately bonded to each other, each of which has hydrophobic and hydrophilic properties, and the total number of segments is 3 or more.

[0088] This gel for microstructure production is I m The pFab method can be suitably used to manufacture structures having a microstructure or nanostructure.

[0089] [Additional Notes] The present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present invention. [Explanation of symbols]

[0090] 10,10A Structure 10G gel (an example of gel for manufacturing microstructures) 101, 102 Low refractive index section, high refractive index section 11 Triblock copolymer (an example of a multi-block copolymer) 111, 112 segments (examples of the first and second segments) 12 Dye 13 Crosslinking material 14 Polymer Matrix 141 Crosslinking point

Claims

1. having a microstructure or nanostructure, The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multi-block copolymer, a dye is chemically bonded to the first segment or the second segment. A structure characterized by:

2. The multi-block copolymer is a triblock copolymer having a total number of segments of 3, and is composed of two of the first segments and a second segment interposed between the two first segments.

2. The structure of claim 1.

3. having a microstructure or nanostructure, The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multiblock copolymer, a dye and a nanoparticle are bound to the first segment or the second segment in this order; the refractive index of the nanoparticles is greater than the refractive index of a polymer matrix comprising the first segment and the second segment; A structure characterized by:

4. having a microstructure or nanostructure, The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multi-block copolymer, a dye is bonded to the first segment or the second segment, At least some of the multi-block copolymers are crosslinked via the dye. A structure characterized by:

5. having a microstructure or nanostructure, The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multi-block copolymer, a dye is bonded to the first segment or the second segment, the first segment or the second segment to which the dye is bonded has a molecular weight distribution of 2 or less; A structure characterized by:

6. having a microstructure or nanostructure, The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multi-block copolymer, a dye is bonded to the first segment or the second segment, a ratio of a block component constituting the first segment or the second segment to which the dye is bonded satisfies 80% or more and 100% or less when measured by 13C-NMR; A structure characterized by:

7. A method for producing a structure having a microstructure or nanostructure, comprising the steps of: a first step of dispersing a dye in a multi-block copolymer that is gelled by containing a solvent, the multi-block copolymer comprising first and second segments each composed of one or more block polymers, the first segments having hydrophobicity and the second segments having hydrophilicity being alternately bonded to each other, and the total number of segments being 3 or more; a second step of patterning the dye-dispersed multiblock copolymer by exposure to light; a third step of removing dye that is not bonded to the multi-block copolymer from the patterned multi-block copolymer; and a fourth step of removing the solvent from the multi-block copolymer from which the dye not bound to the multi-block copolymer has been removed, thereby shrinking the multi-block copolymer. A manufacturing method comprising the steps of:

8. The dye has a crosslinker attached thereto, a fifth step of crosslinking at least some of the multi-block copolymers with the crosslinking agent; The fifth step is carried out after the third step. The method according to claim 7 .

9. A gel for producing a microstructure for producing a structure including a microstructure or a nanostructure, comprising: The present invention includes a multi-block copolymer in which first and second segments each are composed of one or more block polymers, the first segments having hydrophobic properties and the second segments having hydrophilic properties are alternately bonded, and the total number of segments is 3 or more; In each multi-block copolymer, a dye is chemically bonded to the first segment or the second segment. A gel for producing a microstructure, comprising:

Citation Information

Patent Citations

  • Block polymer processing method for mesostructured inorganic oxide materials

    JP2003531083A

  • Block copolymer nanostructures formed by disturbed self-assembly and uses thereof

    US20160332869A1

  • Three-dimensional nanofabrication by patterning of hydrogels

    US20170081489A1

  • Three-dimensional printing with supramolecular templated hydrogels

    US20200131383A1

  • Block of copolymer phases as templates for structured organic-inorganic hybrid materials