Maintenance method and inkjet recording apparatus.

The use of a high-water-content maintenance liquid in the inkjet recording device effectively addresses the cleaning inadequacies of inkjet devices using aggregating agents, enhancing cleaning performance and preventing nozzle wear.

JP7585611B2Active Publication Date: 2024-11-19SEIKO EPSON CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020035591
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-03-03
Publication Date
2024-11-19
Estimated Expiration
2040-03-03

AI Technical Summary

Technical Problem

The cleaning performance of inkjet recording devices using ink compositions and treatment liquids containing aggregating agents is insufficient, leading to ejection failures due to the reaction between ink and treatment liquid on the nozzle forming surface, which forms foreign matter and causes abrasion of the water-repellent film.

Method used

A maintenance method using a maintenance liquid with 80% or more water content for wiping the nozzle forming surface with an absorbent wiping member, which effectively absorbs foreign matter and prevents abrasion of the water-repellent film.

Benefits of technology

The method improves cleaning performance by easily absorbing foreign matter and maintaining the integrity of the water-repellent film, ensuring reliable ejection and high-quality image production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007585611000005
    Figure 0007585611000005
  • Figure 0007585611000006
    Figure 0007585611000006
  • Figure 0007585611000007
    Figure 0007585611000007
Patent Text Reader

Abstract

To provide a maintenance method that has excellent cleaning properties on an inkjet head of a recording device using flocculant, and to provide maintenance liquid.SOLUTION: There is provided a maintenance method for an inkjet recording device that performs recording using an ink composition and treatment liquid containing flocculant. The inkjet recording device includes an inkjet head for discharging the ink composition. The maintenance method includes a wiping step of wiping a nozzle formation surface of the inkjet head using maintenance liquid and an absorptive wiping member. The maintenance liquid includes water by 80 mass% or more based on the total mass of the maintenance liquid.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a maintenance method and a maintenance liquid. [Background technology]

[0002] Inkjet recording methods are capable of recording high-definition images with a relatively simple device, and have made rapid developments in various fields. In the midst of this, various studies have been made on maintenance methods for recording devices. For example, Patent Document 1 discloses a maintenance method having a wiping step of wiping a nozzle formation surface of a recording head with a cleaning liquid and an absorbing member, for the purpose of providing a maintenance method with excellent cleaning properties when recording is performed using an ink composition containing predetermined polymer particles and a treatment liquid. Patent Document 1 discloses that the cleaning liquid contains a penetrating agent and a moisturizing agent as an organic solvent, and the specifically disclosed cleaning liquid contains 60% by mass of 1,3-butanediol and propylene glycol. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-105134 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, it has become apparent that when a cleaning liquid is used to perform maintenance on a nozzle forming surface of an inkjet head of an inkjet recording device that performs recording using a treatment liquid containing an ink composition and a coagulant, the cleaning ability is still not sufficient. [Means for solving the problem]

[0005] The present invention relates to a maintenance method for an inkjet recording device that performs recording using an ink composition and a treatment liquid containing a coagulant, the inkjet recording device having an inkjet head that ejects the ink composition, and a wiping step of wiping a nozzle forming surface of the inkjet head using a maintenance liquid and an absorbent wiping member, the maintenance liquid containing water in an amount of 80% by mass or more relative to the total mass of the maintenance liquid.

[0006] The present invention also provides a maintenance liquid used in the above-mentioned maintenance method, the maintenance liquid containing water in an amount of 80 mass % or more based on the total mass of the maintenance liquid. [Brief description of the drawings]

[0007] [Figure 1] FIG. 4 is a schematic diagram showing an example of a wiping step of the maintenance method of the present embodiment. [Diagram 2] FIG. 1 is a cross-sectional view illustrating an example of an inkjet head according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a plan view illustrating a nozzle formation surface of the inkjet head of the present embodiment. [Figure 4] 4 is a plan view illustrating another example of the nozzle formation surface of the inkjet head of the present embodiment. FIG. [Diagram 5] FIG. 1 is a perspective view illustrating an example of an inkjet recording apparatus according to an embodiment of the present invention. [Figure 6] 2 is a cross-sectional view showing an example of a nozzle formation surface of the inkjet recording apparatus according to the present embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment of the present invention (hereinafter referred to as "the present embodiment") will be described in detail with reference to the drawings as necessary, but the present invention is not limited to this, and various modifications are possible without departing from the gist of the present invention. In the drawings, the same elements are given the same reference numerals, and duplicated explanations will be omitted. Furthermore, positional relationships such as up, down, left, and right are based on the positional relationships shown in the drawings, unless otherwise specified. Furthermore, the dimensional ratios of the drawings are not limited to those shown in the drawings.

[0009] 1. Maintenance Method The maintenance method of the present embodiment is a method for maintaining an inkjet recording apparatus that performs recording using an ink composition and a treatment liquid containing an aggregating agent, and that is equipped with an inkjet head that ejects the ink composition (hereinafter, also simply referred to as "inkjet recording apparatus"). The maintenance method of the present embodiment includes a wiping step of wiping the nozzle formation surface of the inkjet head using a maintenance liquid and an absorbent wiping member, and the maintenance liquid used contains water in an amount of 80% by mass or more based on the total mass of the maintenance liquid.

[0010] By using a recording method in which recording is performed using an ink composition and a treatment liquid containing an aggregating agent, the ink composition can be fixed on the recording medium at an early stage. Therefore, the image quality of the recorded matter obtained by this recording method is excellent. On the other hand, when a treatment liquid that aggregates the ink composition is used, the recording medium to which the treatment liquid is attached may come into contact with the inkjet head that ejects the ink composition, or a mist of the ejected treatment liquid may fly to the inkjet head. In such a case, the ink composition and the treatment liquid may react on the nozzle forming surface of the inkjet head to form foreign matter, which may cause ejection defects.

[0011] In order to eliminate such ejection defects, it is effective to wipe the nozzle formation surface of the inkjet head of the inkjet recording device using a wiping member or the like. In the maintenance method of this embodiment, a maintenance liquid containing a relatively large amount of water is used for this wiping. This further improves the cleanability of the nozzle formation surface. The reason for this is thought to be that, although not limited to the following, the maintenance liquid containing a large amount of water makes it easier for the maintenance liquid to be absorbed by the wiping member, and foreign matter adhering to the nozzle formation surface is more easily absorbed into the wiping member together with the maintenance liquid.

[0012] Furthermore, since the foreign matter formed on the nozzle forming surface by the reaction between the ink composition and the treatment liquid is relatively large, wiping the nozzle forming surface with a wiping member during maintenance can scrape off the water-repellent film formed on the nozzle forming surface, deteriorating the abrasion resistance of the water-repellent film and causing ejection defects. In contrast, by using a maintenance liquid with a relatively high water content, the foreign matter adhering to the nozzle forming surface is more likely to be absorbed into the wiping member together with the maintenance liquid, making it possible to suppress a decrease in the abrasion resistance of the water-repellent film.

[0013] 1.1.Attachment process The maintenance method of this embodiment may include an attachment step of attaching a maintenance liquid to the nozzle forming surface or the wiping member before the wiping step. The method of attaching the maintenance liquid to the nozzle forming surface or the wiping member is not particularly limited, but examples of the method include a method of attaching the maintenance liquid to the nozzle forming surface or the wiping member by spraying, dripping, applying (coating) the maintenance liquid, or a method of impregnating the wiping member with the maintenance liquid. In this way, the nozzle forming surface is wiped by the wiping member in the presence of the maintenance liquid.

[0014] Fig. 1 is a schematic cross-sectional view showing a state in which a wiping member (cloth wiper) is brought into contact with a nozzle forming surface of an inkjet head. Fig. 1 shows a state in which the wiping member 21 is pressed against the nozzle forming surface 12 of an inkjet head 11 in the direction of arrow F1. In this case, the maintenance liquid 31 can be applied by a first injector 24 to a first roll 22 around which the wiping member 21 is wound before use. Alternatively, the maintenance liquid 31 can be applied to the wiping member 21 by applying the first roll 22 around which the wiping member 21 is wound before use to a pool 26 of the maintenance liquid 31.

[0015] The position at which the maintenance liquid is applied to the wiping member 21 before it reaches the nozzle-forming surface 12 is not limited to the position in FIG. 1, and the maintenance liquid 31 may be applied to the wiping member 21 before use, which has been sent out in the direction of arrow F2 from the first roll 22, at any stage before it reaches the nozzle-forming surface 12.

[0016] For example, it may be a position closer to the nozzle forming surface 12. For example, it may be a position immediately before the roller that presses the wiping member 21 in the direction of the arrow F1.

[0017] The maintenance liquid 31 can be applied to the nozzle surface 12 by a second injector 25 .

[0018] The maintenance method does not have to include a deposition step of depositing the maintenance liquid on the nozzle forming surface or the wiping member. In this case, maintenance can be performed using a wiping member to which the maintenance liquid has been deposited in advance.

[0019] The application process for applying the maintenance liquid to the nozzle forming surface or the wiping member is not limited to the application using an application mechanism such as the above-mentioned sprayer or pool (immersion machine), and can be changed as appropriate. For example, a dripper, a coater, or the like can also be used as the application mechanism.

[0020] In the maintenance liquid application process, the amount of the maintenance liquid applied is the amount of the maintenance liquid that has adhered to the wiping member and the nozzle formation surface. The deposition amount is the amount of maintenance liquid used when performing one maintenance operation, and is the amount of maintenance liquid used per nozzle row that ejects one (one type) ink composition.

[0021] The amount of the maintenance liquid adhered is preferably 0.1 g or more, more preferably 0.3 g or more, and even more preferably 0.5 g or more. Meanwhile, the amount of the adhered liquid is preferably 5 g or less, more preferably 3 g or less, and even more preferably 1 g or less. In this case, the cleaning property is more excellent and waste of the maintenance liquid can be reduced, which is preferable.

[0022] 1.2. Wiping process The wiping step is a step of wiping the nozzle forming surface of the inkjet head using the maintenance liquid and an absorbent wiping member. The wiping method is not particularly limited, but for example, wiping can be performed by pressing the wiping member 21 against the nozzle forming surface 12 (arrow F1) and moving the wiping member 21 or the nozzle forming surface 21 so as to move the wiping member 21 relatively in a direction along the nozzle forming surface 12.

[0023] Although the wiping direction is not particularly limited, it is preferable to wipe in the direction along the nozzle row. This makes it possible to prevent the portion of the wiping member that has been in contact with the first nozzle row from contacting the second nozzle row, or the portion that has been in contact with the second nozzle row from contacting the first nozzle row, thereby promoting the formation of foreign matter.

[0024] 1.2.1.Maintenance liquid 1.2.1.1.Water The maintenance liquid contains 80% by mass or more of water relative to the total mass. This improves the permeability of the wiping member, making it easier for foreign matter to be taken into the wiping member, and thus improving the cleaning properties. From the above viewpoints, the water content in the maintenance liquid is preferably 85% by mass or more, more preferably 90% by mass or more, and even more preferably 95% by mass. The water content in the maintenance liquid is 100% by mass or less, preferably 99% by mass or less, more preferably 98.5% by mass or less, and even more preferably 98% by mass or less. When the water content in the maintenance liquid is in the above range or more, foreign matter is more easily taken into the wiping member, and the cleaning properties are more excellent.

[0025] When the water content of the maintenance liquid is within the above range, for example, when the maintenance liquid contains a small amount of organic solvent, the ability to remove foreign matter from the nozzle formation surface tends to be superior and the cleanability tends to be improved compared to a maintenance liquid that is entirely water.

[0026] Organic solvents From this viewpoint, it is preferable that the maintenance liquid contains an organic solvent. The organic solvent is not particularly limited, but examples thereof include water-miscible organic solvents such as glycerin, ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, dipropylene glycol, 1,3-propanediol, 1,2-butanediol, 1,2-pentanediol, 1,2-hexanediol, 1,4-butanediol, 1,5-pentanediol, 1,6-hexanediol, diethylene glycol monoethyl ether, methanol, and ethanol. Examples of the organic solvent include organic solvents that may be contained in the ink or treatment liquid described below.

[0027] By using an organic solvent, there is a tendency for the cleaning properties to be further improved as described below, and the cleaning properties are excellent and therefore preferable.

[0028] Among organic solvents, alkanediols having 5 or more carbon atoms are particularly excellent and preferable in the above respects. The alkanediols having 5 or more carbon atoms more preferably have 5 to 10 carbon atoms, and further preferably have 6 to 8 carbon atoms. Although not limited thereto, 1,2-alkanediols are preferable. The alkanediol having 5 or more carbon atoms is more preferably 1,2-pentanediol or 1,2-hexanediol.

[0029] Among organic solvents, polyols are preferable because of their excellent cleaning properties. Examples of polyols include alkane polyols having 4 or less carbon atoms, and condensates in which hydroxyl groups of alkane polyols having 4 or less carbon atoms are condensed with each other intermolecularly. The number of carbon atoms is preferably 2 to 3. In the case of condensates, the number of condensations is preferably 2 to 4. The number of hydroxyl groups in the molecule of polyols is 2 or more, preferably 2 to 4.

[0030] The content of the organic solvent is, for example, 20% by mass or less, preferably 0.5 to 20% by mass, more preferably 1 to 10% by mass, even more preferably 1 to 5% by mass, and particularly preferably 1 to 3% by mass, relative to the total mass of the maintenance liquid. By including an organic solvent, and particularly by having an organic solvent content of 0.5% by mass or more, the organic solvent penetrates foreign matter adhering to the nozzle formation surface, causing the foreign matter to swell or dissolve, making it easier to remove the foreign matter, and thus tends to improve cleaning properties. In addition, by having an organic solvent content of 20% by mass or less, there is a tendency to suppress a decrease in absorption of the maintenance liquid into the wiping member due to a relative decrease in the water content. Among the organic solvents, polyols and alkanediols having 5 or more carbon atoms are preferable from the above-mentioned viewpoint, and the content of these may be within the above-mentioned range.

[0031] Surfactants The maintenance liquid of the present embodiment may further contain a surfactant. The surfactant is not particularly limited, but examples thereof include acetylene glycol-based surfactants, fluorine-based surfactants, and silicone-based surfactants.

[0032] The acetylene glycol surfactant is not particularly limited, but is preferably one or more selected from 2,4,7,9-tetramethyl-5-decyne-4,7-diol and alkylene oxide adducts of 2,4,7,9-tetramethyl-5-decyne-4,7-diol, and 2,4-dimethyl-5-decyne-4-ol and alkylene oxide adducts of 2,4-dimethyl-5-decyne-4-ol. Commercially available acetylene glycol surfactants are not particularly limited, but include, for example, E series such as Olfin 104 series and Olfin E1010 (trade names, manufactured by Air Products Japan, Inc.), Surfynol 465 and Surfynol 61 (trade names, manufactured by Nissin Chemical Industry CO.,Ltd.). The acetylene glycol surfactant may be used alone or in combination of two or more kinds.

[0033] The fluorosurfactant is not particularly limited, but examples thereof include perfluoroalkyl sulfonate, perfluoroalkyl carboxylate, perfluoroalkyl phosphate, perfluoroalkyl ethylene oxide adduct, perfluoroalkyl betaine, and perfluoroalkyl amine oxide compound. The commercially available fluorosurfactant is not particularly limited, but examples thereof include S-144, S-145 (trade names, manufactured by Asahi Glass Co., Ltd.); FC-170C, FC-430, and Fluorad-FC4430 (trade names, manufactured by Sumitomo 3M Co., Ltd.); FSO, FSO-100, FSN, FSN-100, and FS-300 (trade names, manufactured by Dupont Co., Ltd.); and FT-250 and 251 (trade names, manufactured by Neos Co., Ltd.). The fluorosurfactant may be used alone or in combination of two or more kinds.

[0034] Examples of silicone surfactants include polysiloxane compounds and polyether-modified organosiloxanes. Examples of commercially available silicone surfactants include, but are not limited to, BYK-306, BYK-307, BYK-333, BYK-341, BYK-345, BYK-346, BYK-347, BYK-348, and BYK-349 (all trade names, manufactured by BYK Japan K.K.), KF-351A, KF-352A, KF-353, KF-354L, KF-355A, KF-615A, KF-945, KF-640, KF-642, KF-643, KF-6020, X-22-4515, KF-6011, KF-6012, KF-6015, and KF-6017 (all trade names, manufactured by Shin-Etsu Chemical Co., Ltd.). The silicone surfactant may be used alone or in combination of two or more kinds.

[0035] The content of the surfactant is preferably, for example, 3 mass % or less, based on the total mass of the maintenance liquid. When a surfactant is contained, the content is preferably 0.1 to 3 mass % based on the total mass of the maintenance liquid. The content of the surfactant is more preferably 0.1 to 2 mass %, and even more preferably 0.3 to 1 mass %. It is preferable that the content of the surfactant does not exceed 0.1 mass % based on the total mass of the maintenance liquid.

[0036] On the other hand, since the maintenance liquid contains a surfactant, the contact angle with respect to the nozzle formation surface decreases, and the maintenance liquid containing foreign matter and the like spreads on the nozzle formation surface, which may result in a decrease in cleanability. From this viewpoint, it is preferable that the maintenance liquid does not contain any surfactant, or contains as little surfactant as possible, or contains a small amount of surfactant. In this case, the content of the surfactant is preferably 3% by mass or less, more preferably 2% by mass or less, and even more preferably 1% by mass or less, based on the total mass of the maintenance liquid. Furthermore, it is preferably 0.5% by mass or less, more preferably 0.3% by mass or less, more preferably 0.2% by mass or less, and even more preferably 0.1% by mass or less. It is more preferably less than 0.1% by mass, and particularly preferably 0.05% by mass or less. It is more preferably 0.01% by mass or less. The lower limit is 0% by mass or more. Also, the lower limit is preferably below the detection limit.

[0037] In addition, when the content of a certain component in a composition is XX% by mass or less relative to the total mass of the composition, it is also said that the composition does not contain more than XX% by mass of the component. This means that the composition does not need to contain the component, or may contain the component as long as it does not exceed XX% by mass.

[0038] 1.2.1.4. pH adjusters The maintenance liquid of the present embodiment may further contain a pH adjuster. The pH adjuster can easily adjust the pH value of the ink. The pH adjuster is not particularly limited, but examples thereof include inorganic acids (e.g., sulfuric acid, hydrochloric acid, nitric acid, etc.), inorganic bases (e.g., lithium hydroxide, sodium hydroxide, potassium hydroxide, ammonia, etc.), organic bases (triethanolamine, diethanolamine, monoethanolamine, triisopropanolamine), and organic acids (e.g., adipic acid, citric acid, succinic acid, etc.). Among these, organic bases are preferred, and triethanolamine and triisopropanolamine are more preferred. The pH adjuster may be used alone or in combination of two or more.

[0039] The content of the pH adjuster relative to the total mass of the maintenance liquid is preferably 0.01 to 2 mass %, more preferably 0.05 to 1 mass %, and even more preferably 0.05 to 0.5 mass %.

[0040] 1.2.1.5.Contact angle The contact angle of the maintenance liquid with respect to the nozzle forming surface is preferably 60° or more, more preferably 70° or more, even more preferably 80° or more, and even more preferably 90° or more. Furthermore, 100° or more is preferable, and 105° or more is more preferable. When the contact angle is 60° or more, the maintenance liquid is less likely to spread on the nozzle forming surface and is in the form of droplets. Therefore, foreign matter is taken in the droplet-like maintenance liquid, and the foreign matter is further absorbed by the wiping member, so that the cleaning property tends to be further improved. In addition, the contact angle of the maintenance liquid with respect to the nozzle forming surface is preferably 130° or less, more preferably 120° or less, and even more preferably 110° or less. When the contact angle is 130° or less, the wetted area of ​​the nozzle forming surface per maintenance liquid increases, and the cleaning property tends to be further improved.

[0041] The contact angle of the maintenance liquid with respect to the nozzle forming surface can be adjusted by the amount and type of organic solvent contained in the ink composition, and whether or not a surfactant is used. The contact angle of the maintenance liquid with respect to the nozzle forming surface can be obtained by measuring the contact angle of the maintenance liquid with respect to the water-repellent film on the nozzle forming surface. A detailed measurement method is shown in the examples.

[0042] 1.2.1.6.Surface tension The surface tension of the maintenance liquid is preferably 20 mN / m or more, more preferably 50 mN / m or more, even more preferably 55 mN / m or more, and particularly preferably 60 mN / m or more. When the surface tension of the maintenance liquid is 20 mN / m or more, and particularly preferably 55 mN / m or more, foreign matter is taken into the droplets of the maintenance liquid, and the foreign matter is further absorbed by the wiping member, so that the cleaning property tends to be improved. In addition, the surface tension of the maintenance liquid is preferably 80 mN / m or less, more preferably 75 mN / m or less, and even more preferably 73 mN / m or less. When the surface tension of the maintenance liquid is 80 mN / m or less, the wetted area of ​​the nozzle formation surface per maintenance liquid increases, and the cleaning property tends to be improved.

[0043] The surface tension of the maintenance liquid can be adjusted by the amount and type of organic solvent contained in the ink composition, and whether or not a surfactant is used. The surface tension of the maintenance liquid can be measured by the method described in the examples.

[0044] 1.2.2. Wiping member The wiping member is not particularly limited as long as it is absorbent, and can be a sponge or a cloth such as a woven or nonwoven fabric. Absorbency means that the wiping member can absorb the maintenance liquid, the ink composition, and the like. When the wiping member is a woven or nonwoven fabric, the constituent fibers are not particularly limited, and examples thereof include natural fibers such as cellulose fibers and synthetic fibers such as polyester fibers. Among these, natural fibers are preferred, and cellulose fibers are more preferred. Both polyester fibers and cellulose fibers tend to have excellent cleaning properties. Furthermore, since cellulose fibers swell with water, the fibers become soft with the maintenance liquid, and the wear of the water-repellent film on the nozzle formation surface can be further reduced. In addition, foreign matter enters the gaps of the swollen cellulose fibers, so cleaning properties also tend to be improved.

[0045] 1 is a long piece of fabric, and an unused wiping member 21 is fed from a first roll 22, and a used wiping member 21 is taken up from a second roll 23. This allows a new, unused wiping member 21 to come into contact with the nozzle-forming surface 12. Therefore, re-contact of the used wiping member 21 with the nozzle-forming surface 12 can be prevented, thereby preventing the nozzle-forming surface 12 from being re-contaminated by the treatment liquid or ink composition that has permeated into the used wiping member 21.

[0046] 1.2.3.Inkjet head In order to explain the nozzle forming surface of the inkjet head that is the target of wiping, the configuration of the inkjet head will be explained first. Fig. 2 shows a cross-sectional view of the inkjet head. The inkjet head 11 includes a nozzle plate 112 having a plurality of nozzle holes 111 on a surface facing a recording medium (target of attachment), a plurality of pressure chambers 114 that communicate with each of the plurality of nozzle holes 111 formed in the nozzle plate 112, a pressurizing unit 115 that changes the volume of each of the plurality of pressure chambers 114, and an ink supply chamber 116 that supplies ink to the plurality of pressure chambers 114. In this embodiment, the nozzle forming surface 12 refers to a surface that includes the surface of the nozzle plate 112.

[0047] Examples of the pressurizing unit 115 include a piezoelectric method in which ink is ejected by the driving pressure of a piezoelectric element, and a thermal method in which ink is ejected by bubbles generated by heating the ink. An inkjet head using the piezoelectric method is called a piezoelectric head, and an inkjet head using the thermal method is called a thermal head.

[0048] The nozzle plate 112 is a plate material in which a plurality of nozzle holes 111 for ejecting ink are opened in a row. Figures 3 and 4 show an example of a nozzle formation surface of an inkjet head. In the inkjet head 11 in Figures 3 and 4, a nozzle row 117 is formed in which the nozzles 111 are arranged in a sub-scanning direction (a recording medium transport direction) intersecting the main scanning direction. Here, the surface of the nozzle plate 112 from which the ink is ejected is the nozzle formation surface 12. Note that the nozzle row 117 for ejecting one type of liquid may be a single row, or two or more rows as in Figures 3 and 4.

[0049] In a configuration in which a fixing plate for fixing the inkjet head 11 is disposed around the nozzle plate 112, the surface formed by the nozzle plate 112 and the fixing plate 118 (the surface facing the recording medium during recording operation) functions as the nozzle forming surface 12. As an example, a piezo head tends to have a step between the nozzle plate 112 and the fixing plate 118 at 119, while a thermal head tends not to have a step. The nozzle forming surface 12 having such a step tends to be difficult to clean, and therefore the present invention is particularly useful.

[0050] Fig. 6 is a diagram showing an example of a step that the nozzle forming surface has, and is a cross-sectional view taken along a straight line between the upper and lower arrows in Fig. 3, when the nozzle forming surface is observed from the side with the top facing up in the figure.

[0051] A fixed plate 118 is fixed to the nozzle forming surface of the inkjet head 11. The fixed plate 118 has an opening at the nozzle row 117 and the area around it, and covers the other parts of the nozzle forming surface 112 while not covering the nozzle row 117. In this way, the nozzle row 117 part is lower in height than the part covered by the fixed plate 118. In this way, when the nozzle forming surface 112 rubs against or collides with something, the nozzle row 117 part can be made less likely to be scratched. In this way, the nozzle row 117 can be protected.

[0052] A step 119 is formed on the nozzle forming surface 112 at the boundary between a portion covered by the fixing plate 118 and a portion not covered by the fixing plate 118. The step on the nozzle forming surface is not limited to the step in the above example, but may be any step in the portion of the nozzle forming surface that is wiped by the wiping member. There is no limitation on the purpose of having the step.

[0053] The inkjet head 11 may have a first nozzle row Col for ejecting an ink composition and a second nozzle row OP for ejecting a treatment liquid. A plurality of first nozzle rows Col may be provided depending on the type of ink composition used. The arrangement of the first nozzle row Col and the second nozzle row OP is not particularly limited, but it is preferable that they are arranged on the nozzle forming surface of the inkjet head so that they have an overlapping portion when projected in the main scanning directions S1 and S2 of the inkjet head 11 (FIG. 3). By arranging them in this way, the second nozzle row OP can eject the treatment liquid and the first nozzle row Col can eject the ink composition simultaneously in the same region in one main scan. The same region is a region on the recording medium that faces both the second nozzle row OP and the first nozzle row Co1 when the second nozzle row OP and the first nozzle row Co1 are caused to perform one main scan.

[0054] In addition, the inkjet recording device to which the maintenance method of this embodiment is applied is preferably one that performs recording by performing a main scan multiple times to deposit the ink composition and the treatment liquid on the same area of ​​the recording medium in one main scan. In other words, it is preferable to perform recording in a serial manner, which will be described later, using a main scan that deposits the ink composition and the treatment liquid on the same area of ​​the recording medium in one main scan. In this way, when the treatment liquid and the ink composition are simultaneously ejected in one main scan and performed multiple times, the length of the first nozzle row Co1 in the sub-scanning direction can be made longer and the recording speed can be made faster, which is preferable, compared to an example in which the ink composition and the treatment liquid are not deposited on the same area of ​​the recording medium in one main scan as in FIG. 4. Alternatively, in FIG. 4, when the length of the first nozzle row Co1 in the sub-scanning direction is the same as in FIG. 3 and the recording speed is the same as in FIG. 3, the example in FIG. 3 is preferable because the length of the entire inkjet head 11 in the sub-scanning direction can be made shorter.

[0055] On the other hand, when recording is performed by performing a main scan multiple times in which the ink composition and the treatment liquid are deposited on the same area of ​​the recording medium in one main scan, as shown in Fig. 3, for example, the mist of the treatment liquid and the mist of the ink composition may simultaneously deposit on the nozzle forming surface 12, which may easily result in the generation of foreign matter. In addition, the mist of the treatment liquid floats in the main scanning direction, and the mist of the treatment liquid may easily deposit on the nozzle forming surface 12, which may easily result in the generation of foreign matter. For this reason, the present invention is particularly useful.

[0056] 4, the first nozzle row Col and the second nozzle row OP can also be arranged on the nozzle forming surface of the inkjet head so that they have no overlapping portions when projected in the main scanning directions S1, S2 of the inkjet head 11 (FIG. 4). In other words, when the second nozzle row OP and the first nozzle row Co1 are caused to perform one main scan, there is no identical area on the recording medium that faces both the second nozzle row OP and the first nozzle row Co1.

[0057] "So that there are no overlapping portions" not only means arranging the first nozzle row Col so that it does not exist in the main scanning directions S1, S2 of the second nozzle row OP, but also includes controlling so that the ink composition is not ejected from the first nozzle row Col that exists in the main scanning directions S1, S2 of the second nozzle row OP.

[0058] The method of performing printing by performing main scanning multiple times is called a serial method. In the serial method, in particular, a main scan and a sub-scan, which moves a print medium in a sub-scan direction intersecting the main scan direction, are each performed multiple times. For example, the main scan and the sub-scan are each performed multiple times alternately.

[0059] In particular, a method is preferred in which main scanning is performed to deposit the ink composition and the treatment liquid onto the same area of ​​the recording medium, and such main scanning is performed a plurality of times to perform recording. An inkjet head used in a serial system is also called a serial head.

[0060] In the serial method, the length of the nozzle row ejecting the ink composition in the sub-scanning direction divided by the length of one sub-scan is called the number of passes (number of passes). When the number of passes is 2 or more, the nozzle row faces the recording medium again by another main scan to deposit ink on the area of ​​the recording medium to which the nozzle row faces the recording medium by one main scan. The more passes, the higher the recording resolution can be, and the better the image quality. On the other hand, the more passes, the more main scans are required for recording, and the more mist is produced, so that the cleanability of the nozzle formation surface becomes important. The number of passes is 1 or more, preferably 2 to 20, more preferably 3 to 15, and particularly preferably 4 to 10.

[0061] On the other hand, a recording method in which an inkjet head fixed to an inkjet recording device with a width equal to or greater than the recording width of the recording medium is used to move the recording medium along the longitudinal direction (transport direction) of the recording medium, and ink droplets are ejected from the nozzles of the inkjet head in conjunction with this movement to form an image on the recording medium is called a line method. With the line method, an image can be formed in one pass. The inkjet head used in the line method is also called a line head.

[0062] The maintenance method of the present embodiment can be used for both serial heads and line heads, but is preferably used for serial heads which are prone to foreign matter as described above.

[0063] In the recording performed by the inkjet recording apparatus, the amount of the ink composition applied is preferably 5 mg / inch as the maximum amount of the ink composition applied in the area where the ink composition and the treatment liquid are applied in an overlapping manner. 2 More preferably, it is 10 mg / inch or more. 2 More preferably, it is 12 mg / inch or more. 2 On the other hand, the amount of adhesion is preferably 25 mg / inch 2 More preferably, it is 20 mg / inch or less. 2 and more preferably 15 mg / inch or less. 2 In this case, it is preferable because it is possible to record useful images with excellent color development, and because the amount of ink required for recording is small, contamination of the nozzle formation surface is suppressed, and it is also advantageous in terms of cleanability.

[0064] In the recording performed by the inkjet recording apparatus, the amount of the treatment liquid applied is preferably 0.1 mg / inch in the area where the ink composition and the treatment liquid are applied in a superimposed manner and the amount of the ink composition applied is the maximum. 2 More preferably, it is 0.5 mg / inch or more. 2 More preferably, it is 1.0 mg / inch or more. 2 On the other hand, the amount of adhesion is preferably 10 mg / inch 2More preferably, it is 5 mg / inch or less. 2 More preferably, it is 3 mg / inch or less. 2 It is particularly preferably 2 mg / inch or less. 2 More preferably, it is 1.5 mg / inch or less. 2 This is preferable in that a better image quality can be obtained and that the cleaning properties are superior.

[0065] In recording performed by an inkjet recording apparatus, a primary drying process may be provided in which the ink adhered to the recording medium is immediately dried when the ink is adhered to the recording medium. The primary drying process is performed using a drying mechanism for the primary drying process, and the drying mechanism is, for example, a platen heater, a preheater, a blower fan, an IR heater, etc. The drying of the ink is promoted by heating, blowing air, etc.

[0066] Whether or not a primary drying step is performed, the surface temperature of the recording medium when the ink is attached is preferably 45° C. or lower, more preferably 43° C. or lower, and even more preferably 40° C. or lower, while it is preferably 25° C. or higher, more preferably 30° C. or higher, and even more preferably 35° C. or higher.

[0067] In the recording performed by the inkjet recording device, a post-drying process (secondary drying process) may be provided in which the recording medium to which the ink has been attached is heated to complete the recording. The post-drying process is performed using a drying mechanism for the post-drying process, and the drying mechanism is, for example, a conductive heater, a blower fan, an IR heater, etc. The drying of the ink is promoted by heating, blowing air, etc.

[0068] When a post-drying step is performed, the surface temperature of the recording medium is preferably 120° C. or lower, more preferably 100° C. or lower, and even more preferably 90° C. or lower. On the other hand, it is preferably 60° C. or higher, more preferably 70° C. or higher, and even more preferably 80° C. or higher.

[0069] The maintenance method of this embodiment is preferably carried out in an inkjet recording apparatus in which the above-described recording has been performed.

[0070] The material of the nozzle plate 112 is not particularly limited, but examples thereof include silicon, stainless steel (SUS), etc. Furthermore, these materials may be alloys containing other metals.

[0071] A water-repellent film (not shown) may be formed on the surface of the nozzle plate 112. In the case where the water-repellent film is present, the surface of the water-repellent film becomes the nozzle forming surface 12. The water-repellent film is not particularly limited as long as it is a film having water repellency, and can be formed, for example, by forming a molecular film of a metal alkoxide having water repellency, and then performing a drying process, an annealing process, or the like. The molecular film of the metal alkoxide may be any film having water repellency, but is preferably a monomolecular film of a metal alkoxide having a long-chain polymer group (long-chain RF group) containing fluorine, or a monomolecular film of a metal acid salt having a water-repellent group (for example, a long-chain polymer group containing fluorine). The metal alkoxide is not particularly limited, but examples of the metal species that are commonly used include silicon, titanium, aluminum, and zirconium. The long-chain RF group is not particularly limited, but examples include perfluoroalkyl chains and perfluoropolyether chains. Examples of the alkoxysilane having this long-chain RF group include a silane coupling agent having a long-chain RF group. The water-repellent film is not particularly limited, but for example, a SCA (silane coupling agent) film or one described in Japanese Patent No. 4424954 can be used.

[0072] 1.2.4. Processing solution The treatment liquid contains a flocculant, and may contain water, an organic solvent, an antifoaming agent, a surfactant, and a pH adjuster, as necessary.

[0073] Flocculants The flocculant is not particularly limited, but examples thereof include polyvalent metal salts, organic acids, and cationic polymers. The flocculant is preferably water-soluble. When the flocculant is added to water at room temperature and normal pressure at 1% by mass and thoroughly stirred, if no residual or white turbidity is visually observed, the flocculant is considered to be water-soluble.

[0074] The polyvalent metal salt is not particularly limited, but for example, a polyvalent metal salt of an inorganic acid or a polyvalent metal salt of an organic acid is preferable. Such polyvalent metal salts are not particularly limited, but for example, salts of typical metals of Group 2 of the periodic table (e.g., magnesium, calcium), transition metals of Group 3 of the periodic table (e.g., lanthanum), typical metals from Group 13 of the periodic table (e.g., aluminum), and lanthanides (e.g., neodymium) can be mentioned. As the salts of these polyvalent metals, carboxylates (formic acid, acetic acid, benzoate, etc.), sulfates, nitrates, chlorides, and thiocyanates are suitable. Among them, calcium salts or magnesium salts of carboxylates (formic acid, acetic acid, benzoate, etc.), calcium salts or magnesium salts of sulfates, calcium salts or magnesium salts of nitrates, calcium chloride, magnesium chloride, and calcium salts or magnesium salts of thiocyanates are preferably mentioned.

[0075] The organic acid is not particularly limited, but examples thereof include acids having a carboxyl group, such as succinic acid, oxalic acid, malonic acid, citric acid, and acetic acid.

[0076] The cationic polymer is not particularly limited, and examples thereof include amine resins and cationic urethane resins. Examples of the amine resin include polyamine resins, polyamide resins, and polyallylamine resins. The polyamine resin may be a resin having an amino group in the main skeleton of the resin. The polyamide resin may be a resin having an amide group and an amino group in the main skeleton of the resin. The polyallylamine resin is a resin having a structure derived from allylamine in the main skeleton of the resin, and examples thereof include polyallylamine and polyallylamine derivatives.

[0077] The content of the flocculant is preferably 0.5% by mass or more based on the total mass of the treatment liquid. Also, it is preferably 1 to 15% by mass, more preferably 2 to 10% by mass, and even more preferably 3 to 7% by mass. By keeping the content of the flocculant within the above range, the image quality of the obtained recorded matter tends to be further improved.

[0078] 1.2.4.2.Water The treatment liquid is preferably an aqueous composition. An aqueous composition is a composition that contains at least water as a main solvent component of the composition. The content of water is preferably 40% by mass or more, more preferably 45 to 99.5% by mass, based on the total mass of the treatment liquid. The content is more preferably 50 to 90% by mass, even more preferably 60 to 80% by mass, and still more preferably 65 to 80% by mass.

[0079] Organic Solvents The organic solvent is not particularly limited, but examples thereof include glycerin; ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, 1,3-propanediol, 1,2-butanediol, 1,2-pentanediol, 1,2-hexanediol, 1,4-butanediol, 1,5-pentanediol, 1,6-hexanediol, and the like; glycol-based solvents such as diethylene glycol mono(di)-propyl ether and ethylene glycol mono(di)-butyl ether; alcohols such as methanol, ethanol, propyl alcohol, and butanol; and nitrogen-containing solvents such as 2-pyrrolidone, N-methyl-2-pyrrolidone, and N-ethyl-2-pyrrolidone. Examples of the nitrogen-containing solvent include cyclic amides and non-cyclic amides. Examples of the cyclic amides include the above-mentioned 2-pyrrolidone and pyrrolidone derivatives, such as pyrrolidones. Examples of the non-cyclic amides include N,N-dialkylamides. Examples of the N,N-dialkylamides include alkoxy-N,N-dialkylamides having an alkoxy group, and N,N-dialkylamides not having an alkoxy group. Examples of the N,N-dialkylamides include 3-methoxy-N,N-dimethylpropanamide, 3-butoxy-N,N-dimethylpropanamide, and N,N-dimethylpropanamide.

[0080] Examples of the organic solvent include the organic solvents that may be contained in the maintenance liquid described above, as well as the polyols and alkanediols having 5 or more carbon atoms described above.

[0081] Among the organic solvents, polyols, alkanediols having 5 or more carbon atoms, and nitrogen-containing solvents are preferred, such as propylene glycol, 1,2-hexanediol, and 2-pyrrolidone. The organic solvents may be used alone or in combination of two or more.

[0082] The content of the organic solvent is preferably from 5 to 35% by mass, more preferably from 10 to 30% by mass, and further preferably from 15 to 25% by mass, based on the total mass of the treatment liquid.

[0083] Defoamers The defoaming agent is not particularly limited, but examples thereof include silicone-based defoaming agents, polyether-based defoaming agents, fatty acid ester-based defoaming agents, and acetylene glycol-based defoaming agents. Commercially available defoamers include BYK-011, BYK-012, BYK-017, BYK-018, BYK-019, BYK-020, BYK-021, BYK-022, BYK-023, BYK-024, BYK-025, BYK-028, BYK-038, BYK-044, BYK-080A, BYK-094, BYK-1610, BYK-1615, BYK-1650, BYK-1730, and BYK-1770 (all trade names, manufactured by BYK Japan Co., Ltd.), Surfynol DF37, DF110D, DF58, DF75, DF220, MD-20, and Envirogem AD01 (all trade names, manufactured by Nissin Chemical Industry Co., Ltd.). The antifoaming agent may be used alone or in combination of two or more kinds.

[0084] The content of the antifoaming agent is preferably 0.01 to 2 mass %, more preferably 0.05 to 1 mass %, and even more preferably 0.05 to 0.5 mass %, relative to the total mass of the treatment liquid.

[0085] Surfactants The surfactant may be the same as those exemplified for the maintenance liquid above. The content of the surfactant is preferably 0.1 to 3 mass %, more preferably 0.3 to 2 mass %, and even more preferably 0.5 to 1.5 mass %, relative to the total mass of the treatment liquid.

[0086] 1.2.4.6.pH adjusters Examples of the pH adjuster include the same ones exemplified for the maintenance liquid above. The content of the pH adjuster is preferably 0.01 to 2 mass %, more preferably 0.05 to 1 mass %, and even more preferably 0.05 to 0.5 mass %, relative to the total mass of the treatment liquid.

[0087] 1.2.5. Ink composition An example of the ink composition is a water-based ink. Examples of the components of the water-based ink include coloring materials, water, organic solvents, resins, waxes, defoamers, surfactants, and pH adjusters. Here, "water-based" refers to a composition in which water is one of the main solvent components.

[0088] Colorants Examples of coloring materials include dyes, pigments, etc. In particular, pigments are preferred because of their excellent color development and light resistance.

[0089] Examples of pigments include inorganic pigments such as carbon blacks (CI Pigment Black 7) such as furnace black, lamp black, acetylene black, and channel black, iron oxide, and titanium oxide; and organic pigments such as quinacridone pigments, quinacridonequinone pigments, dioxazine pigments, phthalocyanine pigments, anthrapyrimidine pigments, anthanthrone pigments, indanthrone pigments, flavanthrone pigments, perylene pigments, diketopyrrolopyrrole pigments, perinone pigments, quinophthalone pigments, anthraquinone pigments, thioindigo pigments, benzimidazolone pigments, isoindolinone pigments, azomethine pigments, and azo pigments.

[0090] The content of the coloring material such as a pigment is preferably 0.5% by mass or more, more preferably 2% by mass or more, based on the total mass of the ink composition. Also, it is preferably 2 to 15% by mass, more preferably 2 to 10% by mass, and even more preferably 2 to 7% by mass. When the content of the coloring material such as a pigment is 2% by mass or more, a relatively large amount of foreign matter is likely to be generated, making cleaning difficult. For this reason, the present invention is particularly useful.

[0091] 1.2.5.2.Water The water content is preferably 40% by mass or more, more preferably 45 to 99% by mass, further preferably 55 to 80% by mass, more preferably 60 to 75% by mass, and even more preferably 65 to 70% by mass, based on the total mass of the ink composition.

[0092] Organic Solvents Examples of the organic solvent include the same ones as those exemplified for the treatment liquid and maintenance liquid. The content of the organic solvent is preferably 1% by mass or more, more preferably 5 to 35% by mass, even more preferably 10 to 30% by mass, and even more preferably 15 to 25% by mass, based on the total mass of the ink composition.

[0093] Resins Examples of the resin include those that dissolve in the ink composition, or those that are dispersed in the form of an emulsion (resin particles). By using such a resin, a recorded matter with better abrasion resistance tends to be obtained. In particular, it tends to contribute to improving the binding (abrasion resistance) between the recording medium and the ink coating film, and becomes a component that easily reacts with the coagulant of the treatment liquid described below. Examples of such resins are not particularly limited, but include, for example, acrylic resin, vinyl acetate resin, vinyl chloride resin, butadiene resin, styrene resin, polyester resin, cross-linked acrylic resin, cross-linked styrene resin, benzoguanamine resin, phenol resin, silicone resin, epoxy resin, urethane resin, paraffin resin, fluorine resin, and water-soluble resin, as well as copolymers of monomers that constitute these resins. The acrylic resin is a resin obtained by polymerizing at least an acrylic monomer, and also includes an acrylic copolymer resin of an acrylic monomer and another monomer. The acrylic monomer is a monomer having a (meth)acrylic group, such as (meth)acrylate and (meth)acrylic acid. Examples of other monomers include, for example, vinyl monomers. Examples of vinyl monomers include, for example, styrene. Examples of the acrylic copolymer resin include styrene-acrylic resin. The resin may be a copolymer. The copolymer is not particularly limited, but examples thereof include styrene-butadiene resin and styrene-acrylic resin. In addition, the resin may be a polymer latex containing these resins. Examples thereof include a polymer latex containing fine particles of acrylic resin, styrene-acrylic resin, styrene resin, crosslinked acrylic resin, and crosslinked styrene resin. The resin may be used alone or in combination of two or more kinds. Among the resins, acrylic resin, urethane resin, polyester resin, etc. are preferable.

[0094] The resin content is preferably 0.5% by mass or more, based on the total mass of the ink composition. It is further preferably 1 to 15% by mass, more preferably 2 to 12% by mass, and even more preferably 3 to 10% by mass. When the resin content is 1% by mass or more, the abrasion resistance of the resulting recorded matter tends to be further improved. Furthermore, when the resin content is 15% by mass or less, the viscosity of the ink tends to decrease, resulting in excellent ejection stability and excellent clogging recovery.

[0095] Wax Examples of the wax include those that dissolve in the ink composition or those that disperse in the form of an emulsion. The use of such wax tends to produce a record with better abrasion resistance. In particular, the wax tends to contribute to improving abrasion resistance by being unevenly distributed on the surface of the ink coating film on the recording medium (the interface between the air and the ink coating film). Examples of such wax include, but are not limited to, ester wax of higher fatty acid and higher monohydric alcohol or dihydric alcohol (preferably monohydric alcohol), paraffin wax, olefin wax, or a mixture thereof.

[0096] The content of the wax is preferably 0.1 to 5% by mass, more preferably 0.3 to 3% by mass, and more preferably 0.5 to 2% by mass, based on the total mass of the ink composition. When the content of the wax is 0.1% by mass or more, the abrasion resistance of the resulting recorded matter tends to be improved. Also, when the content of the wax is 5% by mass or less, the viscosity of the ink tends to be reduced, leading to excellent ejection stability and excellent clogging recovery.

[0097] Defoamers The defoaming agent may be the same as those exemplified for the treatment liquid above. The content of the defoaming agent is preferably 0.01 to 2 mass %, more preferably 0.05 to 1 mass %, and even more preferably 0.05 to 0.5 mass %, relative to the total mass of the ink composition.

[0098] Surfactants The surfactant may be the same as those exemplified for the maintenance liquid above. The content of the surfactant is preferably 0.1 to 3 mass %, more preferably 0.3 to 2 mass %, and even more preferably 0.5 to 1.5 mass %, relative to the total mass of the ink composition.

[0099] 1.2.5.8.pH adjusters Examples of the pH adjuster include the same ones exemplified for the maintenance liquid above. The content of the pH adjuster is preferably 0.01 to 2 mass %, more preferably 0.05 to 1 mass %, and even more preferably 0.05 to 0.5 mass %, relative to the total mass of the ink composition.

[0100] 1.3. Recording medium The recording medium used in the present embodiment is not particularly limited, but may be, for example, an absorbent recording medium, or a low-absorbent or non-absorbent recording medium. Among these, it is preferable to use a low-absorbent or non-absorbent recording medium as a recording method using a treatment liquid. In particular, it is preferable to use a non-absorbent recording medium.

[0101] The absorbent recording medium is not particularly limited, but examples thereof include plain paper such as electrophotographic paper having high ink permeability, inkjet paper (paper exclusively for inkjet printers having an ink absorbing layer made of silica particles or alumina particles, or an ink absorbing layer made of hydrophilic polymers such as polyvinyl alcohol (PVA) or polyvinylpyrrolidone (PVP)), and fabrics. Examples of low-absorbency recording media include art paper, coated paper, cast paper, and the like used in general offset printing, which have relatively low ink permeability. These are also called coated papers, and are made by providing a coating layer with relatively low ink permeability on a base material such as paper. The coating layer is a layer made of a resin, an inorganic compound, or the like, which has low water absorbency, and has low ink absorbency.

[0102] Non-absorbent recording media are not particularly limited, but examples include plastic films and plates such as polyvinyl chloride, polyethylene, polypropylene, polyethylene terephthalate (PET), polycarbonate, polystyrene, polyurethane, etc.; metal plates such as iron, silver, copper, aluminum, etc.; or metal plates and plastic films produced by vapor deposition of these various metals, alloy plates such as stainless steel and brass, and recording media in which a plastic film such as polyvinyl chloride, polyethylene, polypropylene, polyethylene terephthalate (PET), polycarbonate, polystyrene, polyurethane, etc. is adhered (coated) to a paper substrate.

[0103] 2. Maintenance fluid The maintenance liquid of this embodiment is a maintenance liquid used in the above-mentioned maintenance method, and contains water in an amount of 80 mass % or more based on the total mass of the maintenance liquid. The composition of the maintenance liquid is as described above.

[0104] 3. Inkjet recording device As an example of an inkjet recording device used in the maintenance method of this embodiment, a perspective view of a serial printer is shown in Fig. 5. As shown in Fig. 5, the serial printer 200 includes a conveying unit 220 and a recording unit 230. The conveying unit 220 conveys the recording medium F fed to the serial printer to the recording unit 230, and ejects the recording medium after recording outside the serial printer. Specifically, the conveying unit 220 has feed rollers and conveys the fed recording medium F in the sub-scanning directions T1 and T2.

[0105] The recording unit 230 also includes an inkjet head 11 that ejects a composition onto the recording medium F sent from the conveying unit 220, a carriage 234 on which it is mounted, and a carriage movement mechanism 235 that moves the carriage 234 in the main scanning directions S1 and S2 of the recording medium F. EXAMPLES

[0106] The present invention will be described in more detail below using examples and comparative examples, but the present invention is not limited to the following examples.

[0107] 1.1. Preparation of ink 1.1.1. Preparation of pigment dispersion 40 parts by mass of St-Ac acid copolymer (copolymerized with a mass ratio of methacrylic acid / butyl acrylate / styrene / hydroxyethyl acrylate = 25 / 50 / 15 / 10. Weight average molecular weight 7000, acid value 150 mgKOH / g) was added to a mixture of 7 parts by mass of potassium hydroxide, 23 parts by mass of water, and 30 parts by mass of triethylene glycol-mono-n-butyl ether, and heated with stirring at 80 ° C to prepare a resin aqueous solution. 20 parts by mass of pigment (pigment blue 15:3), 10 parts by mass of the resin aqueous solution, 10 parts by mass of diethylene glycol, and 60 parts by mass of ion-exchanged water were mixed and dispersed using a zirconia bead mill to obtain a pigment dispersion.

[0108] Each component was placed in a mixing tank so as to obtain the composition shown in Table 1, mixed and stirred, and then filtered through a 5 μm membrane filter to obtain an ink composition of each example. The numerical values ​​of each component shown in each example in the table represent mass % unless otherwise specified. In addition, in the table, the numerical values ​​of the pigment dispersion represent mass % of the pigment solid content, and the numerical values ​​of the resin represent mass % of the resin solid content.

[0109] [Table 1]

[0110] The abbreviations and product ingredients used in Table 1 are as follows: [Organic Solvent] Propylene glycol 2-Pyrrolidone 1,2-Hexanediol [Pigment Dispersion] Cyan Dispersion (Pigment Blue 15:3) 〔resin〕 Joncryl 631 (BASF, styrene acrylic resin emulsion) 〔wax〕 AQUACER531 (polyethylene wax manufactured by BYK Japan) [Antifoaming agent] Surfynol DF110D (manufactured by Nissin Chemical Industry Co., Ltd., acetylene glycol surfactant) [Surfactant] BYK348 (BYK Japan, silicone surfactant) [pH adjuster] Triethanolamine

[0111] 1.2. Preparation of treatment solution The treatment liquid for each example was obtained by placing each component in a mixing tank, mixing and stirring, and filtering through a 5 μm membrane filter so as to obtain the composition shown in Table 2. The numerical values ​​of each component shown in each example in the table represent mass % unless otherwise specified.

[0112] [Table 2]

[0113] The abbreviations and product ingredients used in Table 2 are as follows: [Organic Solvent] Propylene glycol 2-Pyrrolidone 1,2-Hexanediol [Flocculant] Calcium Acetate Monohydrate Malonic Acid Cation Master PD-7 (manufactured by Yokkaichi Chemical Co., Ltd., cationic resin: amine-epichlorohydrin condensation polymer) [Antifoaming agent] Surfynol DF110D (manufactured by Nissin Chemical Industry Co., Ltd., acetylene glycol surfactant) [Surfactant] BYK348 (BYK Japan, silicone surfactant) [pH adjuster] Triethanolamine

[0114] 1.3. Preparation of Maintenance Solution The maintenance liquid for each example was obtained by placing each component in a mixing tank, mixing and stirring, and filtering through a 5 μm membrane filter so as to obtain the composition shown in Table 3. The numerical values ​​for each component shown in each example in the table represent mass % unless otherwise specified.

[0115] [Table 3]

[0116] The abbreviations and product ingredients used in Table 3 are as follows: [Organic Solvent] Propylene glycol 1,2-Hexanediol [Surfactant] BYK348 (BYK Japan, silicone surfactant) [pH adjuster] Triethanolamine

[0117] 1.4.1.Surface tension The surface tensions shown in Tables 1 to 3 were measured by the Wilhelmy method using an automatic surface tensiometer CBVP-Z (manufactured by Kyowa Interface Science Co., Ltd.) Specifically, the force that draws the platinum plate into the ink was measured when the platinum plate was wetted with the ink composition, treatment liquid, or maintenance liquid in an environment of 25°C.

[0118] 1.4.2.Contact angle The contact angles shown in Table 3 were measured using a portable contact angle meter PCA-11 (Kyowa Interface Science Co., Ltd.) to measure the contact angle of the maintenance liquid with the nozzle plate at a liquid volume of 5 μL in an environment of 25° C. for an elapsed time of 100 ms.

[0119] 2. Inkjet recording device The inkjet recording device used was a serial type SC-S40650 (manufactured by Seiko Epson Corporation) that had been modified. A heater was installed downstream of the inkjet head to dry the ink on the recording medium.

[0120] The nozzle plate of the inkjet head was made of single crystal silicon. A silicon oxide film (SiO2 film) was formed on the surface of the nozzle plate by introducing SiC14 and water vapor into a chemical vapor deposition (CVD) reactor. The thickness of the SiO2 film was 50 nm. After that, oxygen plasma treatment was performed and C8F 17 A water-repellent film (10 nm thick) was formed on the SiO2 film by chemical vapor deposition (CVD) using C2H4SiC13, and a silicon nozzle plate with the water-repellent film was fabricated. The resulting nozzle plate was then used in an inkjet head.

[0121] In addition, as the inkjet head, one was prepared in which the first nozzle row Col and the second nozzle row OP were arranged on the nozzle forming surface so that they had overlapping portions when projected in the scanning directions S1, S2, as shown in Fig. 3 (head configuration A), and one was prepared in which the first nozzle row Col and the second nozzle row OP were arranged on the nozzle forming surface so that they had no overlapping portions when projected in the scanning directions S1, S2, as shown in Fig. 4 (head configuration B). Both head configurations A and B used piezo heads.

[0122] In head configurations A and B, the fixed plate was fixed, and a step was generated between the nozzle plate and the fixed plate on the nozzle formation surface as shown in Figure 6, resulting in a nozzle formation surface with a step.

[0123] In addition, head configuration A' was also prepared. Head configuration A' did not have a fixing plate, and the nozzle formation surface did not have the above-mentioned step. Other than this, head configuration A' was the same as head configuration A. In any of the head configurations, the treatment liquid was discharged from nozzle row number 1 in Figure 2 or 3, and the ink composition was discharged from nozzle row number 2. The nozzle rows used for recording were one each for the ink composition and the treatment liquid.

[0124] The inkjet recording device had a wiping mechanism as shown in Fig. 1. As wiping members for the wiping mechanism, one using a cloth made of cellulose fiber (manufactured by Asahi Kasei Corporation, product name "Bemliese") (wiper type W1) and one using a cloth made of polyester fiber (manufactured by Toray Industries, product name "Traysee MK") (wiper type W2) were prepared.

[0125] The following tests were performed by combining the above inkjet head and wiping member. The recording conditions for solid image quality were as follows: recording resolution: 720 x 1440 dpi, print pattern: solid image (cyan monochromatic), number of ink scans: 8 times, printing temperature: 40°C, secondary drying temperature by drying heater: 90°C, recording medium: Orajet-3169G (model number, PVC film, ORAFOL JAPAN Co., Ltd.). The adhesion amount is shown in Table 4. The printing temperature and secondary drying temperature were obtained by measuring the temperature of the recording medium with a thermocouple.

[0126] The printing temperature is the surface temperature of the recording medium in the portion facing the head. The secondary drying temperature is the surface temperature of the recording medium in the portion receiving heat from the drying heater. Both were taken as the maximum temperature.

[0127] 3. Evaluation method 3.1. Cleanability The ink jet recording device was filled with the ink composition and the treatment liquid, and a solid image was printed continuously for two hours under the above recording conditions. After printing, the nozzle forming surface of the ink jet head was wiped in the sub-scanning direction T1 using a wiper sprayed with the maintenance liquid. The type and amount of the maintenance liquid used are as shown in Table 4. Here, the amount of adhesion is the amount per ink (per nozzle row).

[0128] After the wiping, whether or not the ink and foreign matter on the nozzle surface had been wiped off was visually confirmed, and the cleanability was evaluated according to the following criteria. (Evaluation Criteria) AA: Sufficient wiping with one wipe, no ink is found on the nozzle surface A: After one wipe, some areas remain unwiped, but after two wipes, it is completely wiped off. B: The ink was not completely wiped off even after two wipes, and a small amount of ink was found on the nozzle surface. C: Ink was not wiped off sufficiently even after two wipes, and ink was clearly visible on the nozzle surface.

[0129] 3.2.Abrasion resistance of nozzle forming surface The ink jet recording device was filled with the ink composition and the treatment liquid, and a solid image was printed continuously for 1 hour under the above recording conditions. Then, the nozzle forming surface of the ink jet head after printing was wiped in the sub-scanning direction T1 using a wiper sprayed with the maintenance liquid. This cycle of printing and wiping was repeated 60,000 times, and then the state of the water-repellent film near the nozzle was measured using an optical microscope (Union Optical Co., Ltd.'s high-precision non-contact step measuring instrument "Hisomet II" DH2). In addition, the occurrence of flight deflection of the ink jet head after the test was also confirmed.

[0130] Based on these results, the effect of the maintenance method on the wear resistance of the nozzle forming surface was evaluated. The evaluation criteria are as follows: (Evaluation Criteria) AA: No peeling of the water-repellent film was observed. A: Some peeling of the water-repellent film was observed, but there was no flight deflection after the test. B: Some peeling of the water-repellent film was observed, and flight deflection was confirmed after the test. C: Considerable peeling of the water-repellent film was observed.

[0131] 3.3. Solid Image Quality The ink composition and the treatment liquid were filled into the inkjet recording device, and a solid image was printed continuously for 2 hours under the above recording conditions. The obtained solid image was visually observed, and the image quality was evaluated according to the following evaluation criteria. (Evaluation Criteria) A: There are no areas in the solid image where the ink composition is not uniform and appears to be light and dark. B: There are some areas in the solid image where the ink composition is not uniform and appears to be light and dark, but this does not pose a problem in practical use. C: There are many areas in a solid image where the ink composition is not uniform and appears to be light and dark.

[0132] [Table 4]

[0133] 4. Evaluation Results Table 4 shows the configuration of the inkjet recording device used in each example, the conditions of the ink composition, the treatment liquid, and the maintenance liquid, and the evaluation results. Recording was performed using ink and a treatment liquid, and all of the examples in which a maintenance liquid with a water content of 80% by mass or more was used showed excellent cleansing properties and excellent image quality. In contrast, all of the comparative examples that did not have this feature were inferior in either cleaning ability or image quality.

[0134] Comparing Examples 1 and 3, it is clear that maintenance liquids containing an organic solvent have higher cleanability, while comparing Examples 1 and 4, it is clear that maintenance liquids containing a lower amount of organic solvent have better cleanability and nozzle surface abrasion resistance. This is thought to be because, in the absence of organic solvent, it is difficult to wipe off foreign matter that has adhered to the nozzle formation surface, while too much organic solvent actually reduces the water content, resulting in a relative decrease in cleanability and nozzle surface abrasion resistance.

[0135] Comparing Examples 1 and 5, it can be seen that the one that does not contain a surfactant and has a larger surface tension and contact angle has better cleaning properties.

[0136] A comparison between Examples 7 and 9 revealed that, as an organic solvent contained in the maintenance liquid, an alkanediol having 5 or more carbon atoms had superior cleaning properties.

[0137] Comparing Examples 1 with 6 to 8, 10, 12, 13, and 17, it can be seen that the cleanability and nozzle surface abrasion resistance are affected by the type and amount of aggregating agent and the amount of pigment, in other words, the strength of the aggregating action, and by the aggregates formed by the aggregation of ink components. This shows that improving the cleanability and nozzle surface abrasion resistance is an issue that arises from the use of a treatment liquid, and that this issue is resolved by these Examples.

[0138] Comparing Examples 7 and 11, it can be seen that in head configuration B, the first nozzle row Col and the second nozzle row OP do not overlap in the main scanning direction, so the first nozzle row Col is less affected by the ejection of the treatment liquid, resulting in excellent cleanability and nozzle surface abrasion resistance, as well as excellent solid image quality.

[0139] Comparing Examples 1 and 15, it can be seen that using wiper W2 made of cellulose fiber as the wiping member provides excellent cleaning properties and nozzle surface abrasion resistance. Furthermore, comparing Examples 7 and 16, it can be seen that a nozzle surface without steps provides excellent cleaning properties and nozzle surface abrasion resistance.

[0140] Comparing Examples 7 and 16, the head without a step on the nozzle formation surface was superior in terms of cleaning properties. Furthermore, in the head with a step, the nozzle row part of the nozzle formation surface was less likely to rub or collide with other objects and was more easily protected. This maintenance method was useful in that it was possible to obtain excellent cleaning properties even with a head with such a step.

[0141] In Comparative Examples 1 and 2, the water content was less than 80% by mass, and the cleaning ability was poor. Furthermore, ink aggregates that could not be absorbed by the wiping member tended to remain on the nozzle surface, and the wear resistance of the nozzle surface was also poor. In Comparative Examples 3 to 5, when no treatment liquid was used, the image quality obtained was inferior. When Comparative Example 5 is compared with Example 4, when no treatment liquid was used, the cleaning properties and nozzle surface wear resistance were better than when a treatment liquid was used. The ink components were aggregated by the treatment liquid, and the aggregates formed were detrimental to the cleaning properties and It was found that this reduced the wear resistance of the nozzle surface. [Explanation of symbols]

[0142] Reference Signs List 11...inkjet head, 12...nozzle formation surface, 21...wiping member, 22...first roll, 23...second roll, 24...first ejector, 25...second ejector, 26...pool, 31...maintenance liquid, 111...nozzle hole, 112...nozzle plate, 114...pressure chamber, 115...pressurizing section, 116...ink supply chamber, 117...nozzle row, 118...fixed plate, 119...gap, 200...serial printer, 220...transport section, 230...recording section, 234...carriage, 235...carriage movement mechanism

Claims

1. An ink jet recording apparatus for recording using an ink composition and a treatment liquid containing an aggregating agent A maintenance method for The ink composition is a water-based ink, The inkjet recording apparatus includes an inkjet head for ejecting the ink composition. Preparation, The inkjet head includes a first nozzle row for ejecting the ink composition, and a second nozzle row for ejecting the ink composition. a second nozzle row that ejects liquid; The first nozzle row and the second nozzle row project ink in a main scanning direction of the inkjet head. and arranged on the nozzle forming surface of the inkjet head, the nozzle forming surface being overlapped when the inkjet head is shaded. And, The ink jet recording device is configured to apply the ink composition and the treatment liquid to the same area of ​​the recording medium. The recording is performed by main scanning in which the toner is applied to the toner in the same main scanning direction. The nozzle forming surface of the inkjet head is wiped with a maintenance liquid and an absorbent wiping member. A wiping step of wiping using The maintenance liquid contains water and an organic solvent, The water content is 90% by mass or more based on the total mass of the maintenance liquid, The content of the organic solvent is 5% by mass or less with respect to the total mass of the maintenance liquid. 、 Maintenance methods.

2. The maintenance liquid contains an organic solvent in an amount of 0.5 to 1.0% by weight based on the total weight of the maintenance liquid. Contains 5% by mass, The maintenance method according to claim 1 .

3. The organic solvent contains an alkanediol having 5 or more carbon atoms. The maintenance method according to claim 2.

4. The nozzle forming surface has a step. The maintenance method according to any one of claims 1 to 3.

5. a contact angle of the maintenance liquid with respect to the nozzle forming surface is 60° or more; The maintenance method according to any one of claims 1 to 4.

6. The surface tension of the maintenance liquid is 20 mN / m or more. The maintenance method according to any one of claims 1 to 5.

7. The wiping member includes cellulose fibers. The maintenance method according to any one of claims 1 to 6.

8. The flocculant contains any one of a polyvalent metal salt, an organic acid, or a cationic polymer; The maintenance method according to any one of claims 1 to 7.

9. The maintenance liquid contains water in an amount of 95% by mass or more based on the total mass of the maintenance liquid. Contains The maintenance method according to any one of claims 1 to 8.

10. The ink jet recording device is configured to apply the ink composition and the treatment liquid to the same area of ​​the recording medium. The recording is performed by performing the same main scanning operation multiple times. 、 The maintenance method according to claim 9.

11. Before the wiping step, the maintenance liquid is The method includes the step of: The maintenance method according to any one of claims 1 to 10.

12. The ink composition contains a pigment in an amount of 2 mass % or more based on the total mass of the ink composition. 、 The maintenance method according to any one of claims 1 to 11.

13. The maintenance liquid contains a surfactant in an amount of 0.1% by mass based on the total mass of the maintenance liquid. Does not contain more than The maintenance method according to any one of claims 1 to 12.

14. An ink jet recording apparatus which performs the maintenance method according to any one of claims 1 to 13. The position is The maintenance liquid, the treatment liquid, the ink composition, and the inkjet head and a wiping member that performs the wiping step.

Citation Information

Patent Citations

  • Ink set for inkjet recording and image forming method

    JP2011194744A

  • Maintenance method for recording device

    JP2017105134A

  • Liquid jetting device and method for controlling ionizer in liquid jetting device

    JP2017124582A

  • Inkjet recording method, inkjet recording device and inkjet head

    JP2020019180A

  • Assembly of a print head and a maintenance unit and method for the use of said assembly

    US20150298475A1