Secondary battery control method

By estimating vibration intensity and temperature, calculating adhesive force limits, and cooling the battery when necessary, the method maintains adhesive force between the current collector and active material layer, addressing issues of thermal and vibration-induced separation in secondary batteries.

JP7586133B2Active Publication Date: 2024-11-19TOYOTA JIDOSHA KK
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2022080219
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-05-16
Publication Date
2024-11-19
Estimated Expiration
2042-05-16

AI Technical Summary

Technical Problem

The adhesive force between the current collector and the active material layer in secondary batteries decreases due to thermal and vibration loads, leading to increased contact resistance and unexpected input and output issues.

Method used

A method for controlling secondary batteries that includes estimating vibration intensity and temperature, calculating the lower limit of adhesive force and temperature to prevent peeling, and cooling the battery when the measured temperature exceeds the calculated limit to maintain adhesive force.

Benefits of technology

The method effectively suppresses the decrease in adhesive force between the current collector and active material layer, preventing separation and maintaining battery performance under thermal and vibration loads.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586133000001
    Figure 0007586133000001
  • Figure 0007586133000002
    Figure 0007586133000002
  • Figure 0007586133000003
    Figure 0007586133000003
Patent Text Reader

Abstract

To provide a control method for a secondary battery that can suppress a decrease in adhesive force between a current collector and an active material layer due to an adhesive layer.SOLUTION: A control method for a secondary battery 31 includes a step (S40) of estimating the vibration intensity applied to a secondary battery 31, a step (S50) of measuring the temperature of the secondary battery 31, and a step (S41) of calculating a lower limit value Plim1 of the adhesive force of an adhesive layer (312, 316) that can prevent separation between a current collector (311, 317) and an active material layer (313, 315) for the estimated vibration intensity. The control method further includes a step (S42) of calculating a lower limit value Tlim1 of the temperature of the secondary battery 31 at which the adhesive force of the adhesive layer (312, 316) may decrease with respect to the lower limit value Plim1. The control method further includes a step (S70) of cooling the secondary battery 31 when the measured temperature of the secondary battery 31 is equal to or higher than the calculated lower limit value Tlim1.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a control method for a secondary battery. [Background technology]

[0002] JP 2017-204377 A (Patent Document 1) discloses an all-solid-state battery in which a positive electrode collector, a positive electrode active material layer, a solid electrolyte layer, a negative electrode active material layer, a negative electrode collector, a negative electrode active material layer, a solid electrolyte layer, a positive electrode active material layer, and a positive electrode collector are laminated in this order. Although not described in the above Patent Document 1, the positive electrode collector and the positive electrode active material layer (the negative electrode collector and the negative electrode active material layer) may be bonded together by an adhesive layer. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2017-204377 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, when the current collector and the active material layer are bonded by an adhesive layer as described above, the adhesive strength of the adhesive layer is reduced due to thermal load and vibration load in the battery. This increases the contact resistance between the current collector and the active material layer, which may result in an unexpected decrease in input / output, etc. Therefore, it is desirable to suppress the decrease in the adhesive strength between the current collector and the active material layer by the adhesive layer.

[0005] The present disclosure has been made to solve the above-mentioned problems, and its purpose is to provide a method for controlling a secondary battery that can suppress a decrease in the adhesive strength between a current collector and an active material layer due to an adhesive layer. [Means for solving the problem]

[0006] A control method for a secondary battery according to one aspect of the present disclosure is a control method for a secondary battery including a current collector, an active material layer, and an adhesive layer that bonds the current collector and the active material layer, and includes a vibration intensity estimation step of estimating the intensity of vibration applied to the secondary battery, a temperature measurement step of measuring the temperature of the secondary battery, an adhesion strength calculation step of calculating a lower limit value of the adhesion strength of the adhesive layer that can prevent peeling between the current collector and the active material layer, based on the vibration intensity estimated in the vibration intensity estimation step, a temperature calculation step of calculating a lower limit value of the temperature of the secondary battery at which the adhesion strength of the adhesive layer may decrease, based on the lower limit value of the adhesion strength calculated in the adhesion strength calculation step, and a cooling step of cooling the secondary battery if the temperature of the secondary battery measured in the temperature measurement step is equal to or greater than the lower limit value of the temperature calculated in the temperature calculation step.

[0007] In the control method for a secondary battery according to one aspect of the present disclosure, as described above, a lower limit of the adhesive strength of the adhesive layer capable of preventing the peeling between the current collector and the active material layer is calculated for an estimated value of vibration strength applied to the secondary battery, and a lower limit of the temperature of the secondary battery at which the adhesive strength of the adhesive layer may decrease is calculated for the lower limit of the adhesive strength. Then, when the measured temperature of the secondary battery is equal to or higher than the lower limit of the temperature, the secondary battery is cooled. This allows the secondary battery to be cooled so that the decrease in the adhesive strength of the adhesive layer is suppressed even if a thermal load or a vibration load is applied to the secondary battery. As a result, the thermal expansion of the adhesive layer is suppressed, and therefore the mechanical deterioration of the adhesive layer is suppressed. In addition, chemical deterioration caused by the thermal load of the adhesive layer is suppressed. As a result, the decrease in the adhesive strength between the current collector and the active material layer due to the adhesive layer can be suppressed. Effect of the Invention

[0008] According to the present disclosure, it is possible to suppress a decrease in the adhesive strength between the current collector and the active material layer due to the adhesive layer. [Brief description of the drawings]

[0009] [Figure 1] 1 is a diagram showing a configuration of an electric vehicle according to an embodiment; [Diagram 2]1 is a schematic cross-sectional view showing a configuration of a battery cell of a secondary battery according to an embodiment; [Diagram 3] FIG. 2 is a flow diagram illustrating a method for controlling the adhesive strength of an adhesive layer according to one embodiment. [Figure 4] FIG. 13 is a graph showing the relationship between the amount of moisture and oxygen that penetrates into a battery and the adhesive strength of a positive electrode current collector. [Diagram 5] FIG. 11 is a diagram showing the relationship between the amount of moisture and the amount of oxygen that have penetrated into a battery and the elapsed time. [Figure 6] FIG. 13 is a graph showing the relationship between the adhesive strength of a positive electrode current collector and the elapsed time. [Figure 7] FIG. 1 is a diagram showing a state in which a LIDAR of an electric vehicle detects a bump on a road surface. [Figure 8] FIG. 13 is a diagram showing an inclination angle of a convex portion. [Figure 9] 13 is a diagram showing the relationship between the inclination angle of a convex portion and a vibration intensity prediction value. FIG. [Figure 10] FIG. 13 is a diagram showing the relationship between the predicted vibration strength value and the lower limit of adhesive strength capable of preventing peeling of the positive electrode current collector. [Figure 11] FIG. 11 is a diagram showing the relationship between the adhesive strength of a positive electrode current collector and the lower limit value of the temperature of a secondary battery at which the adhesive strength of a positive electrode-side adhesive layer can decrease. [Figure 12] FIG. 13 is a diagram showing the relationship between the predicted vibration strength value and the lower limit value of the temperature of the secondary battery at which the adhesive strength of the positive electrode side adhesive layer may decrease. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. In the drawings, the same or corresponding parts are designated by the same reference characters and the description thereof will not be repeated.

[0011] 1 is a diagram showing a configuration of an electric vehicle 10 equipped with a secondary battery 31. The electric vehicle 10 includes a battery ECU (Electrical Control Unit) 20, a battery unit 30, and a LIDAR (Light Detection And Ranging) 40. The battery ECU 20 controls the battery unit 30.

[0012] The battery ECU 20 includes a processor 21 and a memory 22. The memory 22 stores programs executed by the processor 21 as well as information used in the programs (for example, maps, formulas, and various parameters).

[0013] The battery unit 30 includes a secondary battery 31, a cooling device 32, and a thermistor 33. The secondary battery 31 is, for example, an all-solid-state battery. The thermistor 33 measures the temperature of the secondary battery 31 (battery cell 310).

[0014] The cooling device 32 is provided to cool the secondary battery 31 (battery cells 310). The cooling device 32 includes, for example, an air-cooling fan. The cooling device 32 may cool the secondary battery 31 (battery cells 310) with a refrigerant such as cooling water.

[0015] FIG. 2 is a diagram showing the configuration of one of the battery cells 310 included in the secondary battery 31. In the secondary battery 31, a positive electrode collector 311, a positive electrode side adhesive layer 312, a positive electrode active material layer 313, a solid electrolyte layer 314, a negative electrode active material layer 315, a negative electrode side adhesive layer 316, and a negative electrode collector 317 are laminated in this order. Note that the configuration of the secondary battery 31 (battery cell 310) is not limited to this. Also, the positive electrode collector 311 and the negative electrode collector 317 are an example of a "collector" in the present disclosure. Also, the positive electrode active material layer 313 and the negative electrode active material layer 315 are an example of an "active material layer" in the present disclosure. Also, the positive electrode side adhesive layer 312 and the negative electrode side adhesive layer 316 are an example of an "adhesive layer" in the present disclosure.

[0016] The positive electrode side adhesive layer 312 is provided so as to be sandwiched between the positive electrode collector 311 and the positive electrode active material layer 313, and bonds the positive electrode collector 311 and the positive electrode active material layer 313. The negative electrode side adhesive layer 316 is provided so as to be sandwiched between the negative electrode collector 317 and the negative electrode active material layer 315, and bonds the negative electrode collector 317 and the negative electrode active material layer 315. Each of the positive electrode side adhesive layer 312 and the negative electrode active material layer 315 is conductive. Each of the positive electrode side adhesive layer 312 and the negative electrode active material layer 315 includes, for example, a carbon layer.

[0017] (Method of controlling secondary batteries) 3 is a control flow showing a method of controlling the secondary battery 31 (battery cell 310) by the processor 21 of the battery ECU 20. For simplification, in this embodiment, only the control of the adhesive strength between the positive electrode collector 311 and the positive electrode active material layer 313 by the positive electrode side adhesive layer 312 will be described. The control of the adhesive strength between the positive electrode collector 311 and the positive electrode active material layer 313 by the negative electrode side adhesive layer 316 is similar (or the same) to the positive electrode side, so a detailed description will not be repeated.

[0018] First, in step S10, the processor 21 detects that the electric vehicle 10 has started. The processor 21 detects that the electric vehicle 10 has started by receiving information indicating that the electric vehicle 10 has started, for example, from an EV-ECU (not shown) or the like.

[0019] Next, in step S20, the processor 21 estimates the adhesive strength of the positive electrode current collector 311. The processor 21 estimates the adhesive strength of the positive electrode current collector 311 based on various information stored in the memory 22. Specifically, the adhesive strength is estimated based on the relationship shown in Fig. 4 and the relationship shown in Fig. 5, which will be described later.

[0020] In detail, the memory 22 stores the relationship (see the solid line in FIG. 4) between the adhesive strength of the positive electrode current collector 311 at 25° C. and the amount of moisture and oxygen that penetrate into the secondary battery 31 (battery cell 310). It is known that the adhesive strength of the positive electrode side adhesive layer 312 (carbon layer) decreases due to oxidation caused by moisture and oxygen. Therefore, the memory 22 stores in advance the test results that derive the adhesive strength of the positive electrode side adhesive layer 312 when the oxygen concentration and humidity are changed at 25° C.

[0021] The memory 22 also stores the relationship (see the solid line in Fig. 5) between the amount of water and oxygen that penetrates into the secondary battery 31 (battery cell 310) and the elapsed time (the elapsed time since the manufacture of the battery cell 310). The relationship shown in Fig. 5 is determined by the permeability coefficient (a preset experimental value) of the members used in the secondary battery 31, the temperature history of the members used in the secondary battery 31, and the elapsed time.

[0022] Then, the processor 21 derives the relationship between the adhesive strength of the positive electrode current collector 311 at 25° C. and the elapsed time (see the solid line in FIG. 6) based on the relationship shown in FIG. 4 and the relationship shown in FIG. 5. As a result, it is estimated that the adhesive strength at the current elapsed time (here, Y1) is P1.

[0023] 3 again, in step S30, the processor 21 detects that the electric vehicle 10 is running (has started running). The processor 21 detects that the electric vehicle 10 is running (has started running) by receiving information indicating that the electric vehicle 10 is running, for example, from an EV-ECU (not shown) or the like.

[0024] Next, in step S40, the processor 21 estimates the intensity of vibration applied to the battery cell 310. For example, the processor 21 detects the presence of a convex portion 90 (see FIG. 7) on the road surface ahead of the electric vehicle 10 by acquiring a signal from the LIDAR 40. Then, the processor 21 acquires information on the height h (see FIG. 8) and the inclination length d (see FIG. 8) of the convex portion 90 from the LIDAR 40, and calculates the inclination angle θ (see FIG. 8) of the convex portion 90. Note that the processor 21 may utilize connected systems such as VICS (Vehicle Information and Communication System) (registered trademark) and vehicle-to-vehicle communication when calculating the inclination angle θ.

[0025] The processor 21 also acquires information on the vehicle speed of the electric vehicle 10 from an EV-ECU (not shown) or the like. The processor 21 then calculates a predicted value of vibration strength g applied to the battery cell 310 based on the inclination angle θ of the convex portion 90 and the vehicle speed of the electric vehicle 10. The vibration strength g means the maximum value of the vibration strength that the battery cell 310 receives in a certain prediction target period.

[0026] Here, the electric vehicle 10 is equipped with a control system (map) (see FIG. 9) in which the relationship between various inclination angles θ and vibration intensity g for each vehicle speed is learned in advance. The processor 21 calculates the vibration intensity g from the calculated inclination angle θ based on the above control system. The above control system may be stored in the memory 22. The processor 21 may use the above control system (map) learned in a vehicle of the same model as the electric vehicle 10 and stored in a server.

[0027] Although the above is an example of calculating the vibration intensity g corresponding to the convex portion 90, the present disclosure is not limited to this, and for example, the vibration intensity g corresponding to the concave portion may be calculated. Also, in Fig. 9, data for vehicle speeds of 50km / h, 65km / h, and 80km / h are shown, but vibration intensity g corresponding to vehicle speeds other than the above three may be learned in advance. In this embodiment, it is assumed that the vibration intensity g of the battery cell 310 is predicted to be G1 (see Fig. 10).

[0028] Next, in step S41, the processor 21 calculates a lower limit (minimum value) of the adhesive strength of the positive electrode side adhesive layer 312 that can prevent peeling between the positive electrode current collector 311 and the positive electrode active material layer 313, for the vibration strength g calculated (predicted) in step S40.

[0029] Here, the memory 22 stores the relationship between the vibration intensity g and the lower limit value of the adhesive strength for each elapsed time Y. The relationship for each elapsed time Y is experimentally derived by an adhesive strength measurement test and is stored in the memory 22 in advance.

[0030] Therefore, the processor 21 calculates the lower limit Plim1 of the adhesive strength corresponding to the vibration intensity G1 based on the above relationship (see FIG. 10) corresponding to the elapsed time Y1. The hatched area in FIG. 10 indicates an area where the positive electrode current collector 311 and the positive electrode active material layer 313 may peel off. The vibration intensity G2 in FIG. 10 indicates the vibration intensity at which the positive electrode side adhesive layer 312 peels off regardless of the temperature of the battery cell 310.

[0031] Next, in step S42, the processor 21 calculates a lower limit value of the temperature of the secondary battery 31 (battery cell 310) at which the adhesive strength of the positive electrode side adhesive layer 312 may decrease, relative to the lower limit value of the adhesive strength calculated in step S41.

[0032] Here, it is known that the positive electrode side adhesive layer 312 (carbon layer) softens and loses mechanical strength above a certain temperature. Therefore, the memory 22 stores in advance the relationship between the temperature of the secondary battery 31 (battery cell 310) and the adhesive strength of the positive electrode side adhesive layer 312. The relationship is experimentally derived in advance and stored in the memory 22.

[0033] In detail, the memory 22 stores a rate of change (the slope of the solid line in FIG. 11) of the adhesive strength of the positive electrode-side adhesive layer 312 with respect to the temperature of the secondary battery 31 (battery cell 310). In step S42, the processor 21 derives a relationship (see the solid line in FIG. 11) between the temperature of the secondary battery 31 (battery cell 310) and the adhesive strength of the positive electrode-side adhesive layer 312 based on the adhesive strength (P1) of the positive electrode-side adhesive layer 312 at 25° C. at elapsed time Y1 and the rate of change. Then, the processor 21 calculates a lower limit value Tlim1 of the temperature corresponding to a lower limit value Plim1 of the adhesive strength estimated in step S41 based on the relationship.

[0034] Fig. 12 is a diagram showing the relationship between the predicted value of vibration intensity g, calculated based on Fig. 10 and Fig. 11, and the lower limit value of the temperature of the secondary battery 31 (battery cell 310) at which the adhesive strength of the positive electrode-side adhesive layer 312 may decrease. The hatched area in Fig. 12 indicates an area where the positive electrode current collector 311 and the positive electrode active material layer 313 may peel off from each other.

[0035] Furthermore, in step S50, the temperature of the secondary battery 31 (battery cell 310) is measured. Specifically, the processor 21 acquires temperature information of the secondary battery 31 (battery cell 310) measured by the thermistor 33.

[0036] Next, in step S60, the processor 21 determines whether the temperature of the secondary battery 31 (battery cell 310) measured in step S50 is equal to or higher than the temperature lower limit value Tlim1 calculated in step S42. If the measured temperature of the secondary battery 31 (battery cell 310) is equal to or higher than the temperature lower limit value Tlim1 (Yes in S60), the process proceeds to step S70. Note that if the result is Yes in S60, the processor 21 may perform control to notify (warn) the user that a decrease in adhesive strength of the adhesive layers (312, 316) is predicted. If the measured temperature of the secondary battery 31 (battery cell 310) is lower than the temperature lower limit value Tlim1 (No in S60), the process returns to a step between steps S30 and S40 (S50).

[0037] Then, in step S70, the secondary battery 31 (battery cells 310) is cooled. Specifically, the processor 21 cools the secondary battery 31 (battery cells 310) by controlling the cooling device 32. Thereafter, the process returns to step S60, and the above cooling control is repeated until the temperature of the secondary battery 31 (battery cells 310) becomes less than the lower limit temperature Tlim1. Note that the above cooling control may be ended when the traveling of the electric vehicle 10 is stopped (or the electric vehicle 10 is powered off).

[0038] As described above, the control method for the secondary battery 31 of this embodiment includes a cooling step of cooling the secondary battery 31 (battery cell 310) when the temperature of the secondary battery 31 (battery cell 310) measured (acquired) in the temperature measurement step (S50) is equal to or higher than the lower limit Tlim1 calculated in the temperature calculation step (S42). This adjusts the temperature of the secondary battery 31 (battery cell 310) so that the adhesive strength of the adhesive layers (312, 316) of the secondary battery 31 is maintained. As a result, peeling of the current collectors (311, 317) in the secondary battery 31 can be easily prevented.

[0039] In the above embodiment, the cooling device 32 is used to cool the secondary battery 31, but the present disclosure is not limited to this. For example, the temperature of the secondary battery 31 (battery cell 310) may be lowered by performing control to suppress heat generation from the secondary battery 31 (for example, electrically disconnecting the secondary battery 31 from other electric devices). Specifically, the secondary battery 31 (battery cell 310) may be cooled by natural heat dissipation while the use of the secondary battery 31 (battery cell 310) is temporarily stopped.

[0040] In the above embodiment, the process of steps S40 to S42 and the process of step S50 are performed in parallel, but the present disclosure is not limited to this. The process of steps S40 to S42 and the process of step S50 may be performed in series.

[0041] The configurations described in the above embodiment and the above modified examples may be implemented in any combination.

[0042] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present disclosure is defined by the claims, not by the description of the embodiments described above, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0043] 31 secondary battery, 311 positive electrode current collector (current collector), 312 positive electrode side adhesive layer (adhesive layer), 313 positive electrode active material layer (active material layer), 315 negative electrode active material layer (active material layer), 316 negative electrode side adhesive layer (adhesive layer), 317 negative electrode current collector (current collector).

Claims

[Claim 1] A method for controlling a secondary battery including a current collector, an active material layer, and an adhesive layer that bonds the current collector and the active material layer, comprising the steps of: a vibration intensity estimating step of estimating the intensity of vibration applied to the secondary battery; a temperature measuring step of measuring a temperature of the secondary battery; an adhesive strength calculation step of calculating a lower limit of the adhesive strength of the adhesive layer capable of preventing peeling between the current collector and the active material layer with respect to the vibration intensity estimated in the vibration intensity estimation step; a temperature calculation step of calculating a lower limit of a temperature of the secondary battery at which the adhesive strength of the adhesive layer may decrease, with respect to the lower limit of the adhesive strength calculated in the adhesive strength calculation step; A method for controlling a secondary battery, comprising: a cooling step of cooling the secondary battery when the temperature of the secondary battery measured in the temperature measurement step is equal to or higher than a lower limit value of the temperature calculated in the temperature calculation step.

Citation Information

Patent Citations

  • Thin secondary battery

    JP1991024256U

  • Power supply device, and vehicle and power storage device comprising the same

    JP2015111493A

  • All-solid battery

    JP2017204377A

  • battery module

    JP2018522373A

  • Electrode plate for all-solid battery

    JP2020098745A