Placement table

The mounting table design with removable sleeves and O-rings effectively seals the adhesive layer from plasma radicals, preventing degradation and reducing maintenance costs by allowing easy replacement of worn components.

JP7586617B2Active Publication Date: 2024-11-19TOKYO ELECTRON LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023134840
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-08-22
Publication Date
2024-11-19
Estimated Expiration
2039-08-09

AI Technical Summary

Technical Problem

The adhesive layer used in the mounting table of plasma processing apparatuses is consumed due to exposure to plasma or radicals, leading to degradation.

Method used

A mounting table design featuring a wafer placement part with a first through hole, a base with a larger second through hole, and a cylindrical sleeve with a sealing member that includes a protrusion to prevent plasma radicals from reaching the adhesive layer, using removable inner and outer sleeves with O-rings to enhance sealing.

Benefits of technology

Prevents adhesive layer consumption by sealing the adhesive layer from plasma exposure, allowing for easy replacement of worn sealing components and reducing maintenance costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586617000001
    Figure 0007586617000001
  • Figure 0007586617000002
    Figure 0007586617000002
  • Figure 0007586617000003
    Figure 0007586617000003
Patent Text Reader

Abstract

To prevent consumption of an adhesive layer used in a placement stage.SOLUTION: A placement stage includes: a wafer placement part which has a placement surface where a wafer is placed, and in which a first through hole is formed; a base which is bonded to a rear surface of the wafer placement part by a first adhesive layer, and in which a second through hole having a hole diameter larger than the first through hole and communicating with the first through hole is formed; a cylindrical sleeve which is provided inside the second through hole so as to be detachable from the base with a sealing member; and the sealing member which is provided between the rear surface of the wafer placement part and the sleeve to be spaced apart from the first adhesive layer so as to seal the first adhesive layer. A convex portion is formed circumferentially to extend on an outer circumference or an inner circumference of a tip end of the sleeve, and the sealing member is pressed against the tip end of the sleeve so as to be extended / contracted.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a mounting table. [Background technology]

[0002] 2. Description of the Related Art There is known a plasma processing apparatus that includes a vacuum processing vessel, a mounting table that holds a target object in the processing vessel and also serves as a lower electrode, and an upper electrode facing the mounting table (see, for example, Patent Document 1).

[0003] The mounting table of the plasma processing apparatus includes an electrostatic chuck, a base, and a cylindrical sleeve. A first through hole is formed in the electrostatic chuck. The base is bonded to the back surface of the electrostatic chuck by a first adhesive layer, and a second through hole communicating with the first through hole is formed in the base. The sleeve is bonded to the back surface of the electrostatic chuck by the second adhesive layer in a state where the sleeve communicates with the first through hole. In this way, the cylindrical sleeve is bonded to the back surface of the electrostatic chuck in a state where the second through hole formed in the base communicates with the first through hole. Since the plasma or radicals flowing in from the first through hole or the second through hole are blocked by the sleeve, it is possible to prevent the first adhesive layer, i.e., the adhesive used for adhesive bonding of the electrostatic chuck, from being directly exposed to the plasma or radicals and being consumed. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2016-28448 A Summary of the Invention [Problem to be solved by the invention]

[0005] The present disclosure provides a mounting table and a substrate processing apparatus that can prevent wear of an adhesive layer used on the mounting table. [Means for solving the problem]

[0006] According to one aspect of the present disclosure, there is provided a mounting table having a mounting surface for mounting a wafer, the mounting table comprising: a wafer mounting section having a mounting surface on which a wafer is to be mounted and in which a first through hole is formed; a base bonded to a rear surface of the wafer mounting section by a first adhesive layer, the base having a second through hole formed therein and having a hole diameter larger than that of the first through hole and communicating with the first through hole; a sealing member for sealing the first adhesive layer; and a cylindrical sleeve provided inside the second through hole together with the sealing member so as to be detachable from the base, the sleeve having a protrusion formed on at least one of an outer periphery or an inner periphery of a tip thereof extending in the circumferential direction, the sealing member being positioned in engagement with the protrusion between a tip surface defined by the protrusion of the sleeve and the rear surface of the wafer mounting section. Effect of the Invention

[0007] According to one aspect, it is possible to prevent the adhesive layer used for the mounting table from being worn away. [Brief description of the drawings]

[0008] [Figure 1] 1 is a schematic cross-sectional view showing an example of a substrate processing apparatus according to an embodiment; [Diagram 2] FIG. 2 is a diagram illustrating an example of a mounting table according to an embodiment. [Diagram 3] FIG. 13 is a diagram showing an example of a mounting table according to a modified example of the embodiment. [Figure 4] FIG. 13 is a diagram showing an example of a mounting table according to a modified example of the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings. In the drawings, the same components are denoted by the same reference numerals, and duplicated descriptions may be omitted.

[0010] [Substrate processing equipment] 1 is a schematic cross-sectional view showing the configuration of a substrate processing apparatus 100 according to this embodiment. The substrate processing apparatus 100 has a processing vessel 1 that is airtight and electrically grounded. The processing vessel 1 is cylindrical and made of, for example, aluminum. A mounting table 2 on which a wafer W is placed is provided within the processing vessel 1. The mounting table 2 has a base 2a and an electrostatic chuck 6. The base 2a is made of a conductive metal, for example, aluminum. A support table 4 supports the mounting table 2.

[0011] An edge ring 5 made of, for example, silicon is provided around the wafer W. The edge ring 5 is also called a focus ring. A cylindrical inner wall member 3a made of, for example, quartz is provided around the edge ring 5, the base 2a, and the support table 4. The mounting table 2 is disposed at the bottom of the processing vessel 1 via the inner wall member 3a and the support member 3 made of, for example, quartz.

[0012] An electrode 6a in the electrostatic chuck 6 is sandwiched between dielectric bodies 6b and connected to a power source 12. When a voltage is applied from the power source 12 to the electrode 6a, the wafer W is electrostatically attracted to the electrostatic chuck 6 by Coulomb force.

[0013] The mounting table 2 has a flow path 2d therein. A heat medium, for example, water, supplied from a chiller unit circulates through the inlet pipe 2b, the flow path 2d, and the outlet pipe 2c. A heat transfer gas, such as helium gas, is supplied to the rear surface of the wafer W via the gas through holes 30 and the gas through holes 30a that penetrate the mounting table 2. With this configuration, the wafer W is controlled to a predetermined temperature.

[0014] The mounting table 2 is provided with pin through holes 200 for a plurality of, for example, three, lifter pins 61. Note that only one lifter pin 61 is shown in Fig. 1. The lifter pin 61 inserted through the pin through hole 200 is connected to a lifting mechanism 62 and moves up and down by driving the lifting mechanism 62. The structure around the pin through hole 200 and the lifting mechanism 62 that raises and lowers the lifter pin 61 will be described later.

[0015] A first RF power supply 10a is connected to the base 2a via a first matching box 11a, and a second RF power supply 10b is connected to the base 2a via a second matching box 11b. The first RF power supply 10a applies high frequency power for plasma generation at a predetermined frequency to the base 2a. The second RF power supply 10b applies high frequency power for bias voltage for attracting ions, which has a frequency lower than that of the high frequency power for plasma generation, to the base 2a. However, the high frequency power supplied from the second RF power supply 10b may be used for plasma generation. A shower head 16 facing the base 2 is provided above the base 2. The shower head 16 and the base 2 function as a pair of electrodes (upper electrode and lower electrode).

[0016] The showerhead 16 has an electrode plate 16b and a top plate 16a. An insulating annular member 95 that supports the showerhead 16 is provided around the showerhead 16, and the upper opening of the processing vessel 1 is closed by the showerhead 16 and the annular member 95. The top plate 16a is made of a conductive material, for example, aluminum whose surface is anodized, and detachably supports the electrode plate 16b at its lower portion.

[0017] The top plate 16a is formed with a gas diffusion chamber 16c and a gas inlet 16g for introducing a process gas into the gas diffusion chamber 16c. A gas supply pipe 15a is connected to the gas inlet 16g. A gas supply unit 15, a mass flow controller (MFC) 15b, and an on-off valve V2 are connected to the gas supply pipe 15a in this order, and a process gas is supplied from the gas supply unit 15 to the inside of the top plate 16a via the gas supply pipe 15a. The on-off valve V2 and the mass flow controller (MFC) 15b control the on / off and flow rate of the gas.

[0018] A number of gas flow holes 16d are formed in the lower part of the gas diffusion chamber 16c toward the inside of the processing vessel 1 and penetrate the electrode plate 16b. The tip of the gas flow hole 16d is a gas introduction hole 16e. The processing gas is supplied in a shower-like manner from the gas introduction hole 16e through the gas diffusion chamber 16c and the gas flow holes 16d into the processing vessel 1.

[0019] A variable DC power supply 72 is connected to the shower head 16 via a low pass filter (LPF) 71, and a switch 73 turns on and off the supply of a DC voltage output from the variable DC power supply 72. The DC voltage from the variable DC power supply 72 and the on and off of the switch 73 are controlled by a control unit 90. When high frequency power is applied from the first RF power supply 10a and the second RF power supply 10b to the mounting table 2 to convert the processing gas into plasma, the control unit 90 turns on the switch 73 as necessary, and a predetermined DC voltage is applied to the shower head 16.

[0020] A cylindrical ground conductor 1a is provided so as to extend from the side wall of the processing vessel 1 to a position above the height position of the shower head 16. This cylindrical ground conductor 1a has a ceiling wall on its upper portion.

[0021] An exhaust port 81 is formed at the bottom of the processing vessel 1, and an exhaust device 83 is connected to the exhaust port 81 via an exhaust pipe 82. The exhaust device 83 has a vacuum pump, and operates the vacuum pump to reduce the pressure inside the processing vessel 1 to a predetermined vacuum level. A load / unload port 84 for the wafer W is provided on a side wall inside the processing vessel 1, and the load / unload port 84 can be opened and closed by a gate valve 85.

[0022] A deposit shield 86 is provided along the inner wall surface on the inside of the side of the processing vessel 1. In addition, a deposit shield 87 is detachably provided along the inner wall member 3a. The deposit shields 86, 87 prevent etching by-products (deposits) from adhering to the inner wall of the processing vessel 1 and the inner wall member 3a. A conductive member (GND block) 89 connected to a ground potential in a controllable manner is provided at a height position of the deposit shield 86 approximately at the same height as the wafer W, thereby preventing abnormal discharge.

[0023] The substrate processing apparatus 100 is generally controlled by a control unit 90. The control unit 90 includes a process controller 91 that controls each unit of the substrate processing apparatus 100, a user interface 92, and a storage unit 93.

[0024] The user interface 92 includes a keyboard through which a process manager inputs commands for managing the substrate processing apparatus 100, a display for visualizing and displaying the operating status of the substrate processing apparatus 100, and the like.

[0025] The storage unit 93 stores recipes, which include control programs (software) for causing the process controller 91 to execute various processes performed in the substrate processing apparatus 100, processing condition data, and the like. Then, as necessary, an arbitrary recipe is called from the storage unit 93 by an instruction from the user interface 92, and executed by the process controller 91, whereby a desired process is performed in the substrate processing apparatus 100 under the control of the process controller 91. In addition, recipes such as control programs and processing condition data can be used in a state stored in a computer-readable computer storage medium, or can be used online by transmitting them from another device as needed via, for example, a dedicated line. Examples of storage media include a hard disk, a CD, a flexible disk, and a semiconductor memory.

[0026] [Configuration of the mounting table] Next, the configuration of the mounting table 2 will be described with reference to Fig. 2. Fig. 2 is a schematic enlarged cross-sectional view showing the mounting table 2 in the substrate processing apparatus 100 of Fig. 1. Fig. 2 shows a case where the lifter pins 61 are raised to support the wafer W.

[0027] The electrostatic chuck 6 is disk-shaped and has a mounting surface 21 on which the wafer W is placed and a back surface 22 opposite to the mounting surface 21. The mounting surface 21 has a circular shape and supports the wafer W by contacting the back surface of the wafer W. The adhesive layer 7 is disposed between the base 2a and the electrostatic chuck 6 and adheres the base 2a to the back surface 22 of the electrostatic chuck 6.

[0028] The electrostatic chuck 6 has a pin through hole 200a, and the base 2a has a pin through hole 200b. The inner wall of the pin through hole 200a is formed by the electrostatic chuck 6. The inner wall of the pin through hole 200b is formed by the base 2a.

[0029] The pin through hole 200a is an example of a first through hole formed in the electrostatic chuck. The pin through hole 200b is an example of a second through hole formed in the base 2a. The pin through hole 200 is formed by communicating the pin through hole 200a and the pin through hole 200b, and accommodates the lifter pin 61 therein.

[0030] At least a portion of the lifter pin 61 is made of sapphire. The lifter pin 61 has a cylindrical shape and an outer diameter of, for example, about several mm. An upper end 61a of the lifter pin 61 has a spherical surface.

[0031] The lifter pins 61 are moved up and down within the pin through holes 200 by the lifting mechanism 62, and are operable to freely appear and disappear from the mounting surface 21 of the mounting table 2. The lifting mechanism 62 adjusts the height of the stop position of the lifter pins 61 so that the upper ends 61a of the lifter pins 61 are positioned directly below the back surface of the wafer W when the lifter pins 61 are accommodated.

[0032] 2, when the lifter pins 61 are raised, the lifter pins 61 protrude from the mounting surface 21 of the mounting table 2 and support the wafer W on the upper part of the mounting table 2. With the lifter pins 61 supporting the wafer W, the lifting mechanism 62 lowers the lifter pins 61 to the mounting surface 21. When the lifter pins 61 are lowered, the lifter pins 61 are housed in the pin through holes 200 and the wafer W is placed on the mounting surface 21. In this manner, the lifter pins 61 transport the wafer W in the vertical direction. After the wafer W is placed on the mounting surface 21, a predetermined process is performed on the wafer W, and the lifter pins 61 lift up the processed wafer W and transfer it to the transport arm.

[0033] The pin through hole 200a has a hole diameter that matches the outer diameter of the lifter pin 61, that is, a hole diameter that is slightly larger than the outer diameter of the lifter pin 61 (for example, about 0.1 to 0.5 mm larger), and moves the lifter pin 61 up and down inside. The hole diameter of the pin through hole 200b is larger than the hole diameter of the pin through hole 200a. An inner sleeve 201 and an outer sleeve 202 are disposed between the inner wall of the pin through hole 200b and the lifter pin 61, and the inner sleeve 201 and the outer sleeve 202 form a part of the pin through hole 200. The inner sleeve 201 and the outer sleeve 202 are formed of an insulating material such as ceramics. The inner sleeve 201 and the outer sleeve 202 may be made of the same material or different materials as long as they are insulating materials.

[0034] The inner sleeve 201 is a cylindrical member having a hole diameter substantially equal to that of the pin through hole 200a. The outer sleeve 202 has a hole diameter that matches the outer diameter of the inner sleeve 201, i.e., a hole diameter that is slightly larger than the outer diameter of the inner sleeve 201, and the inner sleeve 201 is detachably disposed inside the outer sleeve 202.

[0035] The outer sleeve 202 is inserted into the pin through hole 200b, and the outer side and the upper part of the outer sleeve 202 are bonded by the adhesive layer 8, and fixed to the base 2a. The inner sleeve 201 is inserted into the pin through hole 200b to which the outer sleeve 202 is fixed. At the tip of the inner sleeve 201, a convex part 209a is formed in the circumferential direction, extending to the outer periphery. The O-ring 203 is provided on the tip surface 201a inside the convex part 209a of the inner sleeve 201. The tip surface 201a of the inner sleeve 201 is a flat surface surrounded by the convex part 209a. The inner sleeve 201 is provided detachably from the pin through hole 200b together with the O-ring 203. The lower ends of the inner sleeve 201 and the outer sleeve 202 protrude at the bottom so that the cross section is L-shaped, and the protruding parts of the inner sleeve 201 and the outer sleeve 202 fit into the step of the base 2a. This positions the inner sleeve 201 and the outer sleeve 202. In this state, the inner sleeve 201 presses the O-ring 203 from below, bringing it into contact with the back surface 22 of the electrostatic chuck 6. With this configuration, the O-ring 203 is provided between the inner sleeve 201 and the electrostatic chuck 6. An O-ring 207 is provided in a recess in the side wall of the inner sleeve 201 that fits into the step of the base 2a. The O-ring 207 mainly functions to prevent the inner sleeve 201 from falling and to separate the atmospheric space from the vacuum space.

[0036] The adhesive layer 8 is provided from the protruding portion of the outer sleeve 202 to the side portion of the adhesive layer 7 and the upper end of the outer sleeve 202. The adhesive layer 7 and the adhesive layer 8 may be formed from different materials.

[0037] The O-ring 203 contacts the front end surface 201a of the inner sleeve 201 and the back surface 22 of the electrostatic chuck 6, and is pressed against the front end surface 201a of the inner sleeve 201, and expands and contracts to seal the plasma space so that the adhesive layers 7, 8 are not exposed to the plasma space. This makes it possible to prevent plasma radicals from entering the adhesive layers 7, 8 side of the O-ring 203 in the pin through hole 200. This makes it possible to prevent the adhesive layers 7, 8 from being consumed.

[0038] The O-ring 203 is preferably made of a material having plasma resistance. For example, the O-ring 203 may be made of a fluorine-based material. Examples of fluorine-based materials include fluorine vinylidene fluoride (FKM) and polytetrafluoroethylene (PTFE). Other examples of fluorine-based materials include fluorine-based materials such as tetrafluoroethylene-purple vinyl ether (FFKM).

[0039] The O-ring 203 is not fixed by an adhesive layer. The inner sleeve 201 is provided in the pin through hole 200b together with the O-ring 203 so as to be detachable from the base 2a. This allows the inner sleeve 201 to be detachable together with the O-ring 203, thereby making it possible to replace the O-ring 203. This allows the O-ring 203 to be easily replaced when the O-ring 203 is deteriorated by plasma radicals or the like and the sealing effect is reduced, thereby improving maintainability. In addition, since it is not necessary to replace the mounting table 2 itself according to the deterioration of the O-ring 203, costs can be reduced.

[0040] Moreover, the O-ring 203 is disposed apart from the outer sleeve 202 in a space surrounded by the inner sleeve 201 and the rear surface 22 of the electrostatic chuck 6. This provides a distance between the O-ring 203 and the surface of the base 2a, and further provides an insulating member of the outer sleeve 202 therebetween, thereby making it possible to prevent plasma from entering the pin through hole 200 and causing creeping discharge between the O-ring 203 and the surface of the base 2a.

[0041] The O-ring 203 is a ring-shaped member, and is pressed against the tip surface 201a of the inner sleeve 201 and expands and contracts. The O-ring 203 may be elongated such that the vertical length of the cross section is greater than the horizontal length. This increases the vertical compression rate of the O-ring 203, enhances the sealing effect of the O-ring 203, and reliably prevents the adhesive layers 7 and 8 from being exposed to plasma and consumed. Furthermore, by making the O-ring 203 elongated, the distance between the O-ring 203 and the outer sleeve 202 can be increased. This ensures a space for the O-ring 203 to expand due to heat input from the plasma, etc. Furthermore, by cutting the corners of the upper end of the inner sleeve 201 to make it round, the space for the O-ring 203 to expand due to heat input from the plasma, etc. can be increased.

[0042] In this embodiment, the outer sleeve 202 is fixed, but may be provided detachably from the base 2a. That is, the inner sleeve 201 and the outer sleeve 202 are provided such that at least the inner sleeve 201 together with the O-ring 203 is detachable from the base 2a.

[0043] The O-ring 203 is an example of a sealing member provided between the back surface of the wafer placement portion and the sleeve, and is spaced from the adhesive layer to seal the first adhesive layer. The adhesive layer 7 is an example of a first adhesive layer. The inner sleeve 201 is an example of a first sleeve, and the outer sleeve 202 is an example of a second sleeve provided on the outside of the first sleeve. The outer sleeve 202 is fixed to the base 2a inside the pin through hole 200b by the second adhesive layer. The adhesive layer 8 is an example of a second adhesive layer.

[0044] The inner sleeve 201 and the outer sleeve 202 are an example of a cylindrical sleeve, and may be formed as one piece without being divided into two. In this case, the one piece sleeve is provided detachably from the base 2a together with the O-ring 203.

[0045] However, it is preferable to divide the sleeve into an inner sleeve 201 and an outer sleeve 202 as in this embodiment. This allows an insulating member of the outer sleeve 202 to be provided between the O-ring 203 and the adhesive layers 7, 8, and increases the distance between the ring 203 and the adhesive layers 7, 8. This ensures a withstand voltage and suppresses creeping discharge occurring between the O-ring 203 and the surface of the base 2a. It is also preferable to divide the sleeve into an inner sleeve 204 and an outer sleeve 205. The adhesive 8 on the upper surfaces of the outer sleeves 202, 205 may be as thin as possible.

[0046] In consideration of radical resistance, the adhesive layer 7 may be formed of, for example, an epoxy resin, and the adhesive layer 8 may be formed of, for example, a silicone resin. However, in this embodiment, since the sealing effect of the O-ring 203 can be enhanced, the adhesive layers 7 and 8 may be formed of either a silicone resin or an epoxy resin without considering radical resistance. In addition, the adhesives used for the adhesive layers 7 and 8 may be the same material or different materials.

[0047] Further, the electrostatic chuck 6 has a gas through hole 30a, and the base 2a has a gas through hole 30b. An inner wall of the gas through hole 30a is formed by the electrostatic chuck 6. An inner wall of the gas through hole 30b is formed by the base 2a. The gas through hole 30a and the gas through hole 30b are in communication with each other, thereby forming a gas through hole 30 in the mounting table 2. The gas through hole 30 supplies helium gas for heat transfer from below the base 2a to the back surface of the wafer W mounted on the mounting surface 21 of the electrostatic chuck 6.

[0048] The hole diameter of the gas through hole 30b is larger than the hole diameter of the gas through hole 30a. An inner sleeve 204 and an outer sleeve 205 are disposed on the inner wall of the gas through hole 30b, and the inner sleeve 204 and the outer sleeve 205 form a part of the gas through hole 30. A convex portion 210a is formed in the circumferential direction at the tip of the inner sleeve 204, extending to the outer periphery. The O-ring 206 is provided on the tip surface 204a inside the convex portion 210a of the inner sleeve 204. The tip surface 204a of the inner sleeve 201 is a plane surrounded by the convex portion 210a. The O-ring 206 is provided between the inner sleeve 204 and the electrostatic chuck 6. An O-ring 208 is provided in a recess in the side wall of the inner sleeve 204 that fits into the step of the base 2a. The O-ring 208 mainly functions to separate the atmosphere space from the vacuum space. Other configurations of the inner sleeve 204, the outer sleeve 205 and the O-ring 206 are similar to other configurations of the inner sleeve 201, the outer sleeve 202 and the O-ring 203, respectively, and therefore will not be described here.

[0049] The outer sleeve 205 is inserted into the gas through hole 30b before the inner sleeve 204 is inserted, and the side and top parts are bonded with an adhesive layer 8 to be fixed to the base 2a. The inner sleeve 204 is detachable from the gas through hole 30b together with an O-ring 206 provided on its upper part.

[0050] The O-ring 206 is a ring-shaped member, and is pressed against the tip surface 204a of the inner sleeve 204 and expands and contracts. The O-ring 206 may have a vertically elongated shape in which the vertical length of the cross section is greater than the horizontal length. The O-ring 206 seals the adhesive layers 7, 8 from the plasma space by contacting the inner sleeve 204 and the back surface 22 of the electrostatic chuck 6. This prevents the adhesive layers 7, 8 from deteriorating due to the plasma radicals entering the inside of the gas through hole 30b. In addition, an insulating member of the outer sleeve 205 is provided between the O-ring 206 and the adhesive layers 7, 8, widening the distance between the O-ring 206 and the adhesive layers 7, 8 to provide a space. Therefore, in addition to the sealing effect of the O-ring 206, a withstand voltage is ensured, and creeping discharge occurring between the O-ring 206 and the surface of the base 2a can be suppressed. The O-ring 206 may have the same shape and material as the O-ring 203.

[0051] The electrostatic chuck 6 has a mounting surface 21 on which the wafer W is mounted, and is an example of a wafer mounting portion in which a first through hole is formed. The pin through holes 200 and the gas through holes 30 are also examples of first through holes formed in the wafer mounting portion. The wafer mounting portion may have at least one of the pin through holes 200 and the gas through holes 30.

[0052] In other words, the hole formed by the first through hole and the second through hole of the mounting table 2 is at least one of a hole (pin through hole 200) through which the lifter pin 61 that holds the wafer W passes and a hole (gas through hole 30) through which a heat transfer gas is supplied.

[0053] Furthermore, a through hole similar to the pin through hole 200 may be provided in the mounting table 2 on the lower surface of the edge ring 5, and a pin that can move up and down through the through hole and a drive mechanism for moving the pin up and down may be provided. In this case, an O-ring, an inner sleeve, and an outer sleeve having the above structure may be assembled and set in the through hole into which the pin is inserted. This also makes it possible to prevent the adhesive layer from deteriorating due to the plasma radicals entering the inside of the through hole by the installed O-ring.

[0054] As described above, in the mounting table 2 according to this embodiment, the O-rings 203, 206 come into contact with the inner sleeves 201, 204 and the rear surface 22 of the electrostatic chuck 6, and seal the adhesive layers 7, 8 from the plasma space. This makes it possible to prevent radicals of plasma from entering the inside of the pin through hole 200 and the gas through hole 30, which would deteriorate the adhesive layers 7, 8, or prevent abnormal discharge from occurring due to the entry of plasma.

[0055] The electrostatic chuck 6 is an example of a wafer mounting portion, and the mounting table 2 does not necessarily have to have the electrostatic chuck 6. In this case, the wafer mounting portion does not have the function of the electrostatic chuck 6 that electrostatically attracts the wafer W.

[0056] [Variations] A mounting table 2 according to a modified example of the embodiment will be described with reference to Fig. 3 and Fig. 4. Figs. 3(a)-(c) and Fig. 4(a) and (b) are diagrams showing an example of the mounting table 2 according to a modified example of the embodiment. Note that, although modified examples of the inner sleeve 201, the outer sleeve 202, and the O-ring 203 will be described below, similar modified examples are also possible for the inner sleeve 204, the outer sleeve 205, and the O-ring 206.

[0057] In the first modification shown in FIG. 3(a), a protruding portion 209b is formed in the circumferential direction at the tip of the inner sleeve 201, extending to the outer periphery of the inner sleeve 201. The O-ring 203 is provided on the tip surface 201a inside the protruding portion 209b of the inner sleeve 201. The tip surface 201a of the inner sleeve 201 is a flat surface surrounded by the protruding portion 209b. The inner surface of the protruding portion 209b has a groove 209b1 that is inclined so that the upper portion is located more inward than the lower portion. As a result, the O-ring 203 is pressed against the tip of the inner sleeve 201, and when it expands or contracts, it enters the groove 209b1, and the inner sleeve 201 and the O-ring 203 engage with each other to prevent them from coming off.

[0058] 3(b), a protrusion 209c is formed in the circumferential direction at the tip of the inner sleeve 201, extending along the inner circumference of the inner sleeve 201. An upper portion of the protrusion 209c protrudes vertically outward, so that the tip of the inner sleeve 201 has a groove 209c1 and is L-shaped.

[0059] The O-ring 203 is provided on the outer tip surface 201a of the convex portion 209c of the inner sleeve 201. The O-ring 203 has a cross section that is U-shaped in the opposite direction to the groove 209c1, and is configured such that, when pressed against the tip of the inner sleeve 201 and expands and contracts, the O-ring 203 enters into the groove 209c1 and between the back surface 22 of the electrostatic chuck 6 and the upper surface of the convex portion 209c, and the inner sleeve 201 and the O-ring 203 engage with each other so as not to come off.

[0060] In the third modification shown in Fig. 3(c), a protrusion 209d is formed in the circumferential direction at the tip of the inner sleeve 201, extending along the inner circumference of the inner sleeve 201. An upper portion of the protrusion 209d protrudes vertically outward, so that the tip of the inner sleeve 201 has a groove 209d1 and is L-shaped.

[0061] O-ring 203 is provided on the outer tip surface 201a of convex portion 209d of inner sleeve 201. O-ring 203 has an L-shape with a lower portion protruding toward the inner circumference to fit into groove 209d1. When O-ring 203 is pressed against the tip of inner sleeve 201 and expands or contracts, inner sleeve 201 and O-ring 203 engage with each other in groove 209d1 to prevent them from coming off.

[0062] According to the mounting table 2 according to the first to third modifications shown in FIGS. 3(a) to 3(c) described above, the inner sleeve 201 and the O-ring 203 can be integrated together.

[0063] 4(a), a protrusion 209a is formed at the tip of the inner sleeve 201 in the circumferential direction, extending to the outer periphery of the inner sleeve 201, and a protrusion 209e is formed at the tip of the inner sleeve 201 in the circumferential direction, extending to the inner periphery of the inner sleeve 201. A groove 209e1 is formed between the protrusions 209a and 209e. An upper portion of the protrusion 209a is grounded to the rear surface 22 of the electrostatic chuck 6 to fix the position of the inner sleeve 201.

[0064] A small gap D is provided between the upper part of the protrusion 209e and the back surface 22 of the electrostatic chuck 6. The O-ring 203 is a ring-shaped member divided in half, and is arranged so that the divided surface contacts the bottom surface of the groove 209e1. Thus, the O-ring 203 has a half-ring shape and is arranged in the groove 209e1. When the O-ring 203 is pressed against the tip of the inner sleeve 201 and expands and contracts, the inner sleeve 201 and the O-ring 203 engage with each other in the groove 209e1 and do not come off.

[0065] As shown in the modified example 5 of FIG. 4(b), the radial width of the convex portion 209e may be made wider than that of the modified example 4 of FIG. 4(a), and the radial length of the groove 209e1 may be made narrower. The O-ring 203 is disposed in the groove 209e1 of the inner sleeve 201. The O-ring 203 is disposed by dividing a ring-shaped member in half so that the divided surface is in contact with the inner peripheral surface of the convex portion 209a. This allows the O-ring 203 to have a half-ring shape and to fit into the groove 209e1. When the O-ring 203 is pressed against the tip of the inner sleeve 201 and expands and contracts, the inner sleeve 201 and the O-ring 203 engage with each other in the groove 209e1 so as not to come off.

[0066] According to the mounting table 2 according to the fourth and fifth modified examples shown in FIGS. 4(a) and 4(b) described above, the inner sleeve 201 and the O-ring 203 can be integrated together.

[0067] The mounting table and the substrate processing apparatus according to the embodiment disclosed herein should be considered as illustrative in all respects and not restrictive. The above-described embodiment can be modified and improved in various forms without departing from the scope and spirit of the appended claims. The matters described in the above-described embodiments can be configured in other ways without contradiction, and can be combined without contradiction.

[0068] In this specification, the wafer W has been described as an example of a substrate, but the substrate is not limited to this and may be various substrates used in FPDs (Flat Panel Displays), printed circuit boards, etc.

[0069] The substrate processing apparatus 100 can be applied to any type of substrate processing apparatus, such as Capacitively Coupled Plasma (CCP), Inductively Coupled Plasma (ICP), Radial Line Slot Antenna (RLSA), Electron Cyclotron Resonance Plasma (ECR), and Helicon Wave Plasma (HWP). The substrate processing apparatus 100 may be an apparatus that uses plasma or an apparatus that does not use plasma.

[0070] The following is added: [Appendix 1] a wafer placement section having a placement surface for placing a wafer thereon and in which a first through hole is formed; a base that is bonded to a rear surface of the wafer placement portion by a first adhesive layer, the base having a second through hole that has a hole diameter larger than a hole diameter of the first through hole and communicates with the first through hole; a cylindrical sleeve provided inside the second through hole together with a sealing member so as to be detachable from the base; the sealing member is provided between the rear surface of the wafer placement portion and the sleeve and spaced apart from the first adhesive layer, and seals the first adhesive layer; A protrusion is formed in a circumferential direction extending on at least one of the outer periphery and the inner periphery of the tip of the sleeve, The sealing member is pressed against the tip surface of the sleeve and expands and contracts. Mounting stand. [Appendix 2] The sealing member is not fixed by an adhesive layer. 2. The mounting table according to claim 1. [Appendix 3] The sleeve is A first sleeve and a second sleeve provided on the outside of the first sleeve, At least the first sleeve is provided detachably from the base together with the sealing member. 3. The mounting table according to claim 1 or 2. [Appendix 4] the sealing member is disposed in a space surrounded by the first sleeve, the second sleeve, and a rear surface of the wafer placement portion, and spaced apart from the second sleeve. 4. A mounting table as described in appendix 3. [Appendix 5] The second sleeve is adhered to the base by a second adhesive layer inside the second through hole. Attachment 4. A mounting table as described in appendix 4. [Appendix 6] the first adhesive layer bonding the rear surface of the wafer placement portion to the front base and the second adhesive layer bonding the second sleeve to the base are formed from different materials. The mounting table according to any one of claims 1 to 5. [Appendix 7] a hole formed by the first through hole and the second through hole is at least one of a hole through which a lifter pin for holding a wafer passes and a hole through which a heat transfer gas is supplied; The mounting table according to any one of claims 1 to 6. [Appendix 8] The sealing member is an O-ring. The mounting table according to any one of claims 1 to 7. [Appendix 9] A processing vessel; a mounting table provided in the processing vessel, The mounting table is a wafer placement section having a placement surface for placing a wafer thereon and in which a first through hole is formed; a base that is bonded to a rear surface of the wafer placement portion by a first adhesive layer, the base having a second through hole that has a hole diameter larger than a hole diameter of the first through hole and communicates with the first through hole; a cylindrical sleeve provided inside the second through hole together with a sealing member so as to be detachable from the base; the sealing member is provided between the rear surface of the wafer placement portion and the sleeve and spaced apart from the first adhesive layer, and seals the first adhesive layer; A protrusion is formed in a circumferential direction extending on at least one of the outer periphery and the inner periphery of the tip of the sleeve, The sealing member is pressed against the tip surface of the sleeve and expands and contracts. Substrate processing equipment. [Explanation of symbols]

[0071] 1 Processing vessel 2. Placement table 2a base 5 Edge Ring 6 Electrostatic Chuck 7, 8 Adhesive layer 15 Gas supply section 16. Shower Head 21 Placement surface 30a, 30b Gas through holes 61 Lifter pin 62 Lifting mechanism 100 Substrate processing apparatus 200a, 200b Pin through holes 201, 204 Inner sleeve 202, 205 Outer sleeve 203, 206 O-ring

Claims

1. a wafer placement portion having a placement surface for placing a wafer thereon and in which a first through hole is formed; a base that is bonded to a rear surface of the wafer placement portion by a first adhesive layer, the base having a second through hole that has a hole diameter larger than a hole diameter of the first through hole and communicates with the first through hole; a sealing member that seals the first adhesive layer; a cylindrical sleeve provided inside the second through hole and detachably provided from the base together with the sealing member, A protrusion is formed on at least one of the outer periphery and the inner periphery of the tip of the sleeve, the protrusion extending in the circumferential direction; the sealing member is disposed between a tip surface defined by the protrusion of the sleeve and a rear surface of the wafer placement portion, the sealing member being engaged with the protrusion. Mounting stand.

2. The protrusion is formed in a circumferential direction and extends on an inner circumference of a tip end of the sleeve, The convex portion has a horizontal portion at an upper portion thereof that protrudes toward the outer periphery, and the horizontal portion and the sealing member are disposed in engagement with each other. The mounting table according to claim 1 .

3. The sleeve is a first sleeve and a second sleeve provided to surround the first sleeve, The protrusion is formed on the first sleeve. The mounting table according to claim 1 or 2.

4. the second sleeve is bonded to at least one of the wafer placement portion and the base by a second adhesive layer; The mounting table according to claim 3 .

5. the second sleeve is adhered to the wafer placement portion and the base by a second adhesive layer; The mounting table according to claim 4 .

6. The sealing member is provided spaced apart from the first adhesive layer. The mounting table according to any one of claims 1 to 5.

7. The protrusion has an L-shape. The mounting table according to any one of claims 1 to 6.

8. The sealing member has a U-shape. The mounting table according to any one of claims 1 to 7.

9. The sealing member has an L-shape. The mounting table according to any one of claims 1 to 7.

10. a wafer placement portion having a placement surface for placing a wafer thereon and in which a first through hole is formed; a base that is bonded to a rear surface of the wafer placement portion by a first adhesive layer, the base having a second through hole that has a hole diameter larger than a hole diameter of the first through hole and communicates with the first through hole; a sealing member having a half-ring shape and sealing the first adhesive layer; a cylindrical sleeve provided inside the second through hole and detachably provided from the base together with the sealing member, A first protrusion is formed on the inner periphery of the tip of the sleeve and extends in a circumferential direction. A second protrusion is formed on the outer periphery of the tip of the sleeve, the second protrusion being extended in the circumferential direction. the sealing member is disposed in a groove formed between the first convex portion and the second convex portion; Mounting stand.

11. a gap is formed between the wafer placement portion and an upper surface of the first protrusion. The mounting table according to claim 10.

12. The height of an upper surface of the first protrusion is lower than the height of an upper surface of the second protrusion. The mounting table according to claim 10 or 11.

13. an upper surface of the second protrusion contacts a lower surface of the wafer placement portion; The mounting table according to any one of claims 10 to 12.

14. The sleeve is a first sleeve and a second sleeve provided to surround the first sleeve, the first protrusion and the second protrusion are formed on the first sleeve; The mounting table according to any one of claims 10 to 13.

15. the second sleeve is bonded to at least one of the wafer placement portion and the base by a second adhesive layer; The mounting table according to claim 14 .

16. the second sleeve is adhered to the wafer placement portion and the base by a second adhesive layer; The mounting table according to claim 15 .

Citation Information

Patent Citations

  • Depressurized chamber

    JP1995273095A

  • Electrostatic clamp with lip seal for substrate clamping

    JP2000502837A

  • Seal structure and joining device

    JP2013071297A

  • Installation table, plasma processing device and method for manufacturing installation table

    JP2016028448A

  • Device for holding a planar substrate

    US20140191478A1