Pellicle, pellicle-attached original plate for exposure, method for manufacturing semiconductor device, method for manufacturing liquid crystal display panel, method for recycling original plate for exposure, and method for reducing peeling residue
The pellicle with an acrylic polymer adhesive layer, irradiated to reduce residue, addresses the issue of dust and adhesive adherence on exposure masters, improving cleaning and recycling efficiency in semiconductor and liquid crystal display manufacturing.
Patent Information
- Application Number
- JP2020133230
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-04-23
- Filing Date
- 2020-08-05
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2040-04-15
AI Technical Summary
The challenge in semiconductor and liquid crystal display manufacturing is the adherence of dust and peeling residue on exposure masters, which affects pattern deformation, cleanliness, and production efficiency, especially with the use of phase shift films and negative type mask patterns, where conventional cleaning methods like functional water struggle to remove adhesive residue effectively.
A pellicle with an adhesive layer made of acrylic polymer containing ether bonds and irradiated with 193 nm ultraviolet rays to reduce peeling residue, allowing for easy recycling and improved cleaning efficiency.
The pellicle effectively minimizes adhesive residue on exposure masters, facilitating easier cleaning and recycling, thereby enhancing production efficiency in semiconductor and liquid crystal display manufacturing.
Smart Images

Figure 0007587936000003 
Figure 0007587936000001 
Figure 0007587936000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a pellicle, an exposed master plate with a pellicle, a method for manufacturing a semiconductor device, a method for manufacturing a liquid crystal display panel, a method for recycling an exposed master plate, and a method for reducing peeling residue. [Background technology]
[0002] In the manufacture of semiconductor devices such as LSI and VLSI, or liquid crystal display panels, a pattern is created by irradiating a semiconductor wafer or a liquid crystal master with light, but if dust is attached to the exposure master used in this case, the dust absorbs or bends the light, causing problems such as deformation of the transferred pattern, rough edges, and black staining of the base, impairing dimensions, quality, appearance, etc. In this invention, "exposure master" is a general term for lithography masks and reticles.
[0003] These operations are usually carried out in a clean room. However, since it is difficult to keep the exposure master clean even in this clean room, a method is used in which a pellicle that allows exposure light to easily pass through is attached to the surface of the exposure master to keep out dirt. In this case, the dust does not adhere directly to the surface of the exposure master, but adheres to the pellicle film. Therefore, if the focus is aligned on the pattern of the exposure master during lithography, the dust on the pellicle film will not affect the transfer.
[0004] The basic structure of a pellicle is a pellicle frame and a pellicle film stretched over it. The pellicle film is made of nitrocellulose, cellulose acetate, fluoropolymer, etc., which transmits light used for exposure (g-line, i-line, 248 nm, 193 nm, 157 nm, etc.) well. The pellicle frame is made of aluminum alloys such as A7075, A6061, A5052, stainless steel, polyethylene, etc., which have been subjected to black anodizing treatment. A good solvent for the pellicle film is applied to the upper part of the pellicle frame, and the pellicle film is air-dried and bonded, or is bonded with an adhesive such as acrylic resin, epoxy resin, or fluororesin. In addition, since the exposure master plate is attached to the lower part of the pellicle frame, an adhesive layer made of polybutene resin, polyvinyl acetate resin, acrylic resin, silicone resin, etc., and a protective liner for protecting the adhesive layer are provided.
[0005] The pellicle is installed so as to surround the pattern area formed on the surface of the exposure master. The pellicle is provided to prevent dust from adhering to the exposure master, and therefore this pattern area is isolated from the outside of the pellicle so that dust outside the pellicle does not adhere to the pattern surface.
[0006] In recent years, LSI design rules have been miniaturized to the sub-quarter micron level, and as a result, exposure light sources are becoming shorter in wavelength, that is, they are shifting from the previously mainstream g-line (436 nm) and i-line (365 nm) from mercury lamps to KrF excimer lasers (248 nm), ArF excimer lasers (193 nm), F2 lasers (157 nm), etc. As a result of miniaturization, the allowable size of foreign matter and haze that may occur on the pattern surface of a mask substrate to which a pellicle is attached is becoming increasingly strict. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Patent No. 5638693 [Patent Document 2] JP 2016-18008 A [Patent Document 3] JP 2006-146085 A [Patent Document 4] JP 2008-21182 A Summary of the Invention [Problem to be solved by the invention]
[0008] In recent years, phase shift films have become the norm for mask substrates in order to keep up with the miniaturization of design rules. However, phase shift films are very delicate, and mask cleaning under excessive conditions can cause damage such as corrosion or scraping. For this reason, there has been a trend in recent years to reconsider the chemicals used for mask cleaning and to weaken the cleaning conditions.
[0009] Furthermore, advanced masks are shifting from the previously mainstream positive type mask patterns to negative type mask patterns, and as a result, there are many cases where there is no light-shielding layer in the area where the pellicle is attached. Without the light-shielding layer, there is a possibility that the exposure light will be irradiated onto the pellicle adhesive through the mask substrate. This may result in more residue of the adhesive layer remaining on the mask substrate when the pellicle is peeled off.
[0010] When a pellicle is attached to a mask for use, if foreign matter or haze occurs or the pellicle film is damaged, the pellicle must be peeled off, the mask regenerated and cleaned, and replaced with a new pellicle (hereinafter, this will be referred to as a "repellicle"). The most important thing about a repellicle is to regenerate and clean the mask to a high degree of cleanliness, but in order to regenerate and clean the mask under recent weak cleaning conditions, it is important to minimize the residue remaining on the mask substrate when the pellicle is peeled off. This regeneration cleaning generally involves cleaning with chemicals such as sulfuric acid / hydrogen peroxide or ammonia / hydrogen peroxide, or physical cleaning using brushes, sponges, etc. However, in order to prevent damage to the photomask and to prevent sulfate ions from remaining on the photomask, regeneration cleaning using functional water has been considered.
[0011] Functional water is generally defined as an aqueous solution that has been given a reproducible and useful function by artificial processing, and the scientific basis of the processing and function has been clarified or is about to be clarified.Specific examples include ozone water, hydrogen water, fine bubble water such as microbubble water and nanobubble water, electrolytic water, supercritical water, and subcritical water, and ozone water and hydrogen water are often used to clean photomasks.In addition, the cleaning power can be improved by adding a small amount of ammonia.
[0012] However, the inventors have found that functional water has a weaker cleaning power than chemicals such as sulfuric acid / hydrogen peroxide, and therefore, when cleaning a photomask after peeling off a pellicle, the residue of the adhesive layer that fixed the pellicle and the photomask is difficult to remove by cleaning with functional water alone. In particular, in the case of a phase shift photomask, damage to the phase shift film leads to changes in transmittance and phase difference, so it is difficult to add physical cleaning in addition to cleaning with functional water.
[0013] Furthermore, when lithography is performed using exposure light such as an ArF excimer laser (193 nm) with a lithography pellicle in which a pellicle film is attached to the upper end surface of the pellicle frame via an adhesive layer for attaching the pellicle film, and an adhesive layer for attaching a mask is provided on the other end surface, the adhesive layer formed on the lower end surface of the pellicle frame is altered by the exposure light, and when it is peeled off from the exposed master, the altered parts of the adhesive layer remain on the exposed master as peeling residue, which is a problem.
[0014] To date, attempts have been made to reduce residue by adding a surface modifier or the like to the adhesive (see Patent Document 1 and Patent Document 2). 2Disclosed are a large pellicle having an adhesive layer having the above structure (Patent Document 3), and a pellicle having an adhesive for a pellicle having a ratio of peel strength to tensile strength of 0.10 or more and 0.33 or less (Patent Document 4).
[0015] The present invention has been made in view of the above circumstances, and aims to provide a pellicle, an exposed master with a pellicle, a method for regenerating an exposed master, and a method for reducing residues left behind after peeling, which can reduce residues that adhere to the exposed master when the pellicle is peeled off from the exposed master after use in lithography, particularly after use in ArF lithography, and thereby to provide a method for manufacturing a semiconductor device and a liquid crystal display panel that can improve production efficiency. [Means for solving the problem]
[0016] The above-mentioned problems of the present invention have been solved by the following means. [1] A pellicle having a pellicle membrane, a pellicle frame having the pellicle membrane provided on one end surface thereof, and an adhesive layer provided on the other end surface of the pellicle frame, After the adhesive layer of the pellicle was attached to the quartz mask substrate, 193 nm ultraviolet light was applied at 10 J / cm from the rear surface of the substrate to the adhesive layer of the pellicle. 2 A pellicle in which, when the pellicle is irradiated with light and then peeled off after the irradiation, the amount of peeling residue of the pressure-sensitive adhesive layer remaining on the substrate is 0.5 mg or less. [2] The pellicle according to [1], wherein the adhesive forming the adhesive layer has an acrylic polymer as a base material. [3] The pellicle according to [2], wherein the acrylic polymer comprises a (meth)acrylic acid ester having an ether bond as a monomer component. [4] The pellicle according to [3], wherein the (meth)acrylic acid ester having an ether bond is a (meth)acrylic acid ester having an alkylene oxide group. [5] The pellicle according to [4], wherein the alkylene oxide group is an ethylene oxide group. [6] The pellicle according to [2], wherein the acrylic polymer has a side chain containing an ether bond. [7] The pellicle described in [6] above, wherein the side chain containing an ether bond has an alkylene oxide group. [8] The pellicle according to [7], wherein the alkylene oxide group is an ethylene oxide group. [9] The pellicle according to any one of the above [1] to [8], wherein the adhesive forming the adhesive layer contains a polyvinyl ether compound.
[10] The pellicle according to any one of [1] to [9], wherein the pressure-sensitive adhesive layer is irradiated with an exposure light beam.
[11] The pellicle according to any one of [1] to [9] above, which is attached to a phase shift photomask.
[12] The pellicle according to any one of [1] to [9] above, which is attached to a negative type exposure master plate.
[13] The pellicle according to any one of [1] to [9] above, which is attached to an exposure master having a non-light-shielding area or a semi-transparent light-shielding area in the area where the pressure-sensitive adhesive layer is attached.
[14] The pellicle according to any one of [1] to [9] above, which is attached to an exposure master having a transparent area in the area where the adhesive layer is attached.
[15] The pellicle according to any one of [1] to [9] above, which is attached to a surface containing silicon oxide as a main component.
[16] The pellicle according to
[15] , wherein the surface mainly composed of silicon oxide is a quartz surface.
[17] The pellicle according to any one of [1] to [9] above, which is adapted for regeneration and cleaning with functional water.
[18] An exposure master with a pellicle, comprising an exposure master having the pellicle described in any one of [1] to
[10] attached thereto.
[19] The exposure master with a pellicle according to the above
[18] , wherein the exposure master is a phase shift photomask.
[20] The exposure master with a pellicle according to
[18] above, wherein the exposure master is of a negative type.
[21] The exposure master with a pellicle according to
[18] , wherein the adhesive layer of the exposure master has an area that is not light-shielded or a semi-transparent light-shielded area in the area to which the adhesive layer is attached.
[22] The exposure master with a pellicle according to
[18] above, wherein the adhesive layer of the exposure master has a transparent area attached thereto.
[23] The exposure master with a pellicle according to
[18] , wherein the exposure master is mainly composed of silicon oxide.
[24] The exposure master with a pellicle according to
[18] , wherein the exposure master is a quartz substrate.
[25] A method for manufacturing a semiconductor device, comprising a step of exposing using an exposure master with a pellicle according to any one of
[18] to
[24] above.
[26] A method for producing a liquid crystal display panel, comprising a step of exposing using an exposure master with a pellicle according to any one of
[18] to
[24] above.
[27] A method for regenerating an exposed master plate, comprising peeling off the pellicle from the pellicle-attached exposed master plate described in any one of
[18] to
[24] above, and washing off any adhesive residue remaining on the exposed master plate with functional water, thereby regenerating the exposed master plate.
[28] A method for reducing the residue of an adhesive layer of a pellicle remaining on an exposure master when the pellicle is peeled off from an exposure master to which the pellicle is affixed, the method using a pellicle described in any one of [1] to
[17] as the pellicle.
[29] An application of a pellicle having a pellicle membrane, a pellicle frame having the pellicle membrane provided on one end surface, and an adhesive layer provided on the other end surface of the pellicle frame, wherein the adhesive layer is exposed to exposure light.
[30] An application of the pellicle having a pellicle film, a pellicle frame having the pellicle film on one end surface, and an adhesive layer on the other end surface of the pellicle frame, wherein the pellicle is attached to a phase shift photomask.
[31] An application of a pellicle having a pellicle film, a pellicle frame having the pellicle film on one end surface, and an adhesive layer on the other end surface of the pellicle frame, wherein the pellicle is attached to a negative-type exposure master.
[32] An application of a pellicle having a pellicle film, a pellicle frame having the pellicle film on one end surface, and an adhesive layer on the other end surface of the pellicle frame, wherein the pellicle is attached to an exposed master having a non-light-shielded area or a translucent light-shielded area in the adhesive layer attachment portion of the exposed master.
[33] An application of a pellicle having a pellicle membrane, a pellicle frame having the pellicle membrane provided on one end surface, and an adhesive layer provided on the other end surface of the pellicle frame, wherein the pellicle is attached to an exposed master having a transparent area at the attachment portion of the adhesive layer on the exposed master.
[34] An application of a pellicle having a pellicle membrane, a pellicle frame having the pellicle membrane provided on one end surface, and an adhesive layer provided on the other end surface of the pellicle frame, wherein the pellicle is attached to a surface primarily composed of silicon oxide (particularly a quartz surface).
[35] An application of a pellicle having a pellicle membrane, a pellicle frame having the pellicle membrane provided on one end surface, and an adhesive layer provided on the other end surface of the pellicle frame, the application of the pellicle being compatible with regeneration and cleaning using functional water.
[36] A peeling residue reducing pellicle having at least a pellicle film, a pellicle frame having the pellicle film attached to one end surface thereof, and an adhesive layer for attaching the pellicle to an exposure master plate on the other end surface of the pellicle frame, After the adhesive layer of the pellicle was attached to the quartz mask substrate, 193 nm ultraviolet light was applied at 10 J / cm from the rear surface of the substrate to the adhesive layer of the pellicle. 2 and when the pellicle is peeled off after the irradiation, the amount of peeling residue of the pressure-sensitive adhesive layer remaining on the substrate is 0.5 mg or less.
[37] The pellicle for reducing peeling residue described in
[36] , wherein the adhesive layer is made of an adhesive containing an acrylic polymer.
[38] The pellicle having reduced peeling residue described in
[37] , wherein 51 mass% or more of all monomer components constituting the acrylic polymer are ethylene oxide group-containing (meth)acrylate monomers.
[39] The pellicle having reduced peeling residue described in
[37] or
[38] above, wherein the adhesive further contains a polyvinyl ether compound.
[40] The pellicle for reducing peeling residue according to any one of
[36] to
[39] , which is a pellicle for reducing peeling residue for ArF lithography.
[41] A method for reducing the peeling residue of an adhesive layer of a pellicle remaining on an exposure master when the pellicle is peeled off from an exposure master to which the pellicle is affixed, the method being characterized in that the pellicle is a pellicle described in any one of
[36] to
[40] above.
[42] A method for selecting a pellicle with reduced peeling residue, comprising the steps of attaching an adhesive layer of a pellicle candidate to a quartz photomask substrate, and applying 193 nm ultraviolet light at 10 J / cm to the adhesive layer attachment portion of the pellicle from the rear surface of the substrate. 2 and selecting a pellicle having a reduced peeling residue when the pellicle is peeled off after the irradiation and the amount of peeling residue of the adhesive layer remaining on the substrate is 0.5 mg or less as a pellicle having a reduced peeling residue. Effect of the Invention
[0017] According to the present invention, when a pellicle is peeled off from an exposed master after lithography, particularly after ArF lithography, a pellicle, a method for regenerating an exposed master, and a method for reducing peeling residues can be provided, which can reduce the peeling residues of the adhesive layer of the pellicle remaining on the exposed master. The pellicle, the exposed master with a pellicle, the method for regenerating an exposed master, and the method for reducing peeling residues of the exposed master of the present invention can peel off the pellicle from the exposed master with very little peeling residues of the adhesive even if the exposure light is irradiated through the exposed master. As a result, the regeneration cleaning of the exposed master from which the pellicle has been peeled off can be carried out well, and the cleaning conditions can be relaxed, which is advantageous in terms of reducing damage to the exposed master surface during cleaning. In addition, the production efficiency can be improved in the manufacture of semiconductor devices and liquid crystal display panels. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is a conceptual diagram showing the basic structure of a pellicle of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] The basic structure of the pellicle of the present invention will first be described with reference to FIG. 1, the pellicle 10 of the present invention comprises a pellicle film 12 stretched over the upper end surface of a pellicle frame 11 via an adhesive layer 13 for attaching the pellicle film, and in this case, an adhesive layer 14 for adhering the pellicle 10 to an exposure master (mask substrate or reticle) 1 is usually formed on the lower end surface of the pellicle frame 11, and a liner (not shown) is releasably attached to the lower end surface of the adhesive layer 14. The pellicle frame 11 may also be provided with an air pressure adjustment hole (vent) 15, and may further be provided with a dust filter 16 for the purpose of removing particles.
[0020] In this case, the size of these pellicle components is similar to that of ordinary pellicles, such as pellicles used in semiconductor lithography and pellicles used in the lithography process of manufacturing large liquid crystal display panels, and the materials thereof can be the well-known materials as described above.
[0021] The type of pellicle film 12 is not particularly limited, and for example, an amorphous fluoropolymer that has been conventionally used for excimer lasers may be used. Examples of amorphous fluoropolymers include Cytop (trade name of Asahi Glass Co., Ltd.), Teflon (registered trademark) AF (trade name of DuPont Co., Ltd.), etc. These polymers may be dissolved in a solvent as necessary when preparing the pellicle film, and can be appropriately dissolved in, for example, a fluorine-based solvent.
[0022] The base material of the pellicle frame 11 may be, for example, a conventionally used aluminum alloy material, preferably JIS A7075, JIS A6061, or JIS A5052 material, but there is no particular restriction on the aluminum alloy material as long as the strength of the pellicle frame is ensured. The surface of the pellicle frame is preferably roughened by sandblasting or chemical polishing, and a polymer coating may be provided after roughening. In the present invention, the method of roughening the frame surface may be a conventionally known method. A method of roughening the surface of an aluminum alloy material by blasting the surface with stainless steel, carborundum, glass beads, or the like, and then chemically polishing the surface with NaOH or the like is preferable.
[0023] The adhesive used to form the adhesive layer 14 can be appropriately selected from various adhesives described later, but an acrylic adhesive is preferred. The shape of the adhesive is preferably flattened to reduce the effect of distortion on the mask substrate to which it is attached and to suppress residual stress caused by attaching the pellicle, so that the adhesive is less likely to deform when the pellicle is attached.
[0024] In the pellicle of the present invention, the thickness of the adhesive layer 14 is usually preferably 150 to 500 μm, more preferably 180 to 350 μm, and particularly preferably 200 to 300 μm. The width of the adhesive layer 14 may be appropriately determined depending on the width of the pellicle frame 11. Usually, the adhesive layer is provided over the entire circumferential direction of the lower end surface of the pellicle frame 11, with a width approximately equal to the width of the pellicle frame.
[0025] The pellicle of the present invention is formed by attaching an adhesive layer of the pellicle to a quartz mask substrate, and then irradiating the adhesive layer of the pellicle with 193 nm ultraviolet light at 10 J / cm from the rear surface of the substrate. 2and when the pellicle is peeled off after the irradiation, the amount of peeling residue of the adhesive layer remaining on the substrate is 0.5 mg or less. Here, the term "peeling residue-reduced pellicle" refers to a pellicle for lithography that can reduce the amount of peeling residue of the adhesive layer remaining on the surface of an exposed master plate when the pellicle is peeled off from the exposed master plate after use in lithography, i.e., a pellicle for lithography that is less likely to generate peeling residue.
[0026] When the adhesive layer of the pellicle is attached to a quartz mask substrate, the quartz mask substrate can be exemplified by a substrate of quartz mask 6025 size (152 mm x 152 mm, t = 6.35 mm). Therefore, the pellicle of the present invention is based on a size that can be attached to a quartz mask 6025 size, and specifically, the outer dimensions are usually in the range of 150 to 145 mm x 124 to 100 mm. The width of the pellicle frame constituting the pellicle of the present invention is usually in the range of 1.7 to 2.1 mm, preferably 1.8 to 2.0 mm, and the thickness of the pellicle frame is usually in the range of 2.0 to 6.2 mm, preferably 2.5 to 6.0 mm.
[0027] When the adhesive layer of the pellicle is attached to the quartz mask substrate, the attachment load is 10 to 250 N, preferably 40 to 100 N, and the load time is 15 to 120 seconds, preferably 20 to 60 seconds. After the adhesive layer of the pellicle is attached to the quartz mask substrate, it is left at room temperature (20±3°C) for 12 to 24 hours, and then ultraviolet rays of the above wavelength are applied to the attached part of the adhesive layer from the back side of the mask substrate so that the ultraviolet rays are irradiated, and the ultraviolet rays are irradiated with 10 J / cm2. 2 Irradiate.
[0028] In the present invention, the irradiation dose is 10 J / cm 2 The reason for this is that it is assumed that 1% of the irradiation dose of 1000 J on the mask (equivalent to approximately 10000 J on the wafer) is irradiated onto the mask adhesive as stray light.
[0029] When peeling off the pellicle after the irradiation, the pellicle is completely peeled off from the mask substrate by gripping the sides of the pellicle with a peeling device or the like at room temperature and pulling it upward (90° direction) relative to the mask surface at a speed of 0.1 mm / sec. After peeling, the mass difference of the mask substrate before and after peeling is measured, and a pellicle having this mass difference (amount of peeling residue) of 0.5 mg or less, preferably 0.2 mg or less is the pellicle of the present invention. Since the amount of peeling residue is small, re-cleaning of the exposed master plate becomes extremely easy.
[0030] In addition, it is preferable that two holes are provided on the outer surface of the long side of the pellicle frame with the distance between the centers of the holes being 104 mm. The pellicle frame has two long sides, and it is preferable that two holes are provided on each long side. It is preferable that these two holes are provided so that the distance from one end of the long side to one hole is the same as the distance from the other end of the long side to the other hole. From the viewpoint of the device, it is preferable that the diameter of the hole is about 1.6 mm, and the depth is 1.0 mm or more and less than 1.8 mm. It is possible to easily peel it off by inserting four pins of a peeling device into these four holes and pulling it up. This pulling speed can be changed in the range of 0.1 mm / sec or less depending on the peel strength. In addition, when pulling up, the two long sides are not pulled up at the same time, but rather, pulling up from one long side can reduce the peeling force applied to the left and right.
[0031] As described above, the pressure-sensitive adhesive layer of the present invention leaves a certain amount of residue on the substrate after peeling. This can be achieved, for example, by the following design guidelines (1) to (5). (1) Increase the hydrophilicity of the adhesive. (2) When the base material contained in the pressure-sensitive adhesive is an acrylic copolymer, an ether bond is introduced into the side chain. (3) When the base material contained in the pressure-sensitive adhesive is a chain polymer, the decomposition property of the side chains upon irradiation with exposure light is made higher than that of the main chain. (4) When the base material contained in the pressure-sensitive adhesive is a chain polymer, the side chains are selectively degraded by irradiation with exposure light. (5) Increases the cohesive strength of the entire adhesive.
[0032] In the above (1), hydrophilicity can be controlled by using the SP value (solubility parameter). For example, when an acrylic polymer is used as the base material of the adhesive, it is preferable to control the SP value to about 10.0 or more and 12.0 or less. This SP value can be calculated by the following formula 1 with reference to Fedors' calculation method [Polymer Engineering and Science, Vol. 14, No. 2 (1974), pp. 148-154].
[0033]
number
[0034] In the above formula 1, δ is the solubility parameter (SP value); Δei is the molar evaporation energy; Δvi is the molar volume. The unit of the solubility parameter is (cal / mol). 1 / 2 The characteristic values of Δei and Δvi given to the main atoms or atomic groups for the above formula 1 are shown in Table 1.
[0035] [Table 1]
[0036] The SP value (solubility parameter) of the acrylic polymer is preferably from 10.0 to 12.0, and more preferably from 10.0 to 11.0. The SP value of an acrylic polymer can be controlled, for example, by changing the polar group concentration in the acrylic polymer. For example, when a relatively highly polar bond such as an ether bond is introduced into the side chain, the SP value increases. On the other hand, when a relatively less polar bond such as a long-chain alkylene bond is introduced into the side chain, the SP value decreases.
[0037] In the above (2), the ether bond introduced into the side chain is preferably an alkylene oxide group, and more preferably an ethylene oxide group. It is presumed that the introduction of the ether bond into the side chain suppresses photodegradation of the main chain.
[0038] In the above (3), the difference in decomposition can be determined, for example, by comparing the decomposition products of the main chain and the decomposition products of the side chain before and after the exposure light irradiation of the adhesive by IR, NMR, etc. More specifically, it can be confirmed by comparing the IR chart of the adhesive before the exposure light irradiation with the IR chart of the adhesive after the exposure light irradiation and observing the change in the spectral intensity. The wave number to be confirmed is, for example, 1125 cm -1 COC (methoxy group), 1160cm -1 COC (ether group), 1727cm -1 C=O (ester group) and the like.
[0039] In the above (4), the presence or absence of deterioration can be judged, for example, by comparing the decomposition products of the main chain and the decomposition products of the side chain before and after the exposure light irradiation of the adhesive by IR, NMR, etc. More specifically, it can be confirmed by comparing the IR chart of the adhesive before the exposure light irradiation with the IR chart of the adhesive after the exposure light irradiation and observing the change in the spectral intensity. The wave number to be confirmed is, for example, 1125 cm -1 COC (methoxy group), 1160cm -1 COC (ether group), 1727cm -1 C=O (ester group) and the like.
[0040] In the above (5), the cohesive strength of the adhesive can be controlled, for example, by adjusting the crosslink density of the polymer or resin used in the base material, or by adding a compound having different physical properties, such as a polyvinyl ether compound, to the base material of the adhesive.
[0041] Examples of adhesives used to form the adhesive layer 14 include adhesives containing acrylic polymers, silicone resins, thermoplastic elastomers, etc. Acrylic polymers can be selected from a variety of monomer components, making it easy to design adhesives that meet the desired adhesive properties. Silicone resins have an excellent balance of light resistance, adhesive properties, peeling properties, etc. Thermoplastic elastomers are highly cost-competitive. Acrylic adhesives are preferred.
[0042] The acrylic polymer is, for example, a polymer containing a (meth)acrylic acid ester as a monomer component, and can be copolymerized with a monomer component copolymerizable with the (meth)acrylic acid ester as necessary. Examples of the (meth)acrylic acid ester include a (meth)acrylic acid ester having an ether bond, a (meth)acrylic acid alkyl ester, and an unsaturated monomer having a carboxyl group or a hydroxyl group. By including a (meth)acrylic acid ester having an ether bond as a monomer component, an ether bond can be introduced into the side chain of the acrylic polymer.
[0043] Examples of the (meth)acrylic acid ester having an ether bond (component (A)) include (meth)acrylic acid esters having an alkylene oxide group such as an ethylene oxide group, a propylene oxide group, and a butylene oxide group. Among these, (meth)acrylic acid esters having an ethylene oxide group (also referred to as (meth)acrylates containing an ethylene oxide group) are preferred, and examples thereof include 2-methoxyethyl (meth)acrylate, 2-ethoxyethyl (meth)acrylate, 2-butoxyethyl (meth)acrylate, phenoxyethylene glycol (meth)acrylate, methoxypolyethylene glycol (meth)acrylate such as methoxydiethylene glycol (meth)acrylate, ethoxypolyethylene glycol (meth)acrylate such as ethoxydiethylene glycol (meth)acrylate, butoxypolyethylene glycol (meth)acrylate such as butoxydiethylene glycol (meth)acrylate, and phenoxypolyethylene glycol (meth)acrylate such as phenoxydiethylene glycol (meth)acrylate. These may be used alone or in combination of two or more.
[0044] Examples of (meth)acrylic acid alkyl esters (component (B)) include (meth)acrylic acid alkyl esters having an alkyl group with 1 to 14 carbon atoms. Specific examples include methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, n-butyl (meth)acrylate, isobutyl (meth)acrylate, isoamyl (meth)acrylate, hexyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, n-octyl (meth)acrylate, isooctyl (meth)acrylate, isononyl (meth)acrylate, and lauryl (meth)acrylate. Among these, (meth)acrylic acid alkyl esters having an alkyl group with 4 or 8 carbon atoms are preferred from the viewpoint of achieving both pressure-sensitive adhesive properties and release properties. These may be used alone or in combination of two or more.
[0045] Examples of unsaturated monomers having a carboxyl group or a hydroxyl group (component (C)) include α,β-unsaturated carboxylic acids such as (meth)acrylic acid, maleic acid, crotonic acid, itaconic acid, and fumaric acid, and hydroxyl group-containing methacrylates such as 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, and 2-hydroxybutyl (meth)acrylate. These may be used alone or in combination of two or more.
[0046] In the acrylic polymer, the proportion of the (A) component used in the total monomer components is preferably 30% by mass or more, more preferably 35% by mass or more, particularly preferably 35 to 98% by mass, and extremely preferably 40 to 95% by mass. By setting the proportion of the (A) component within the above range, it becomes easy to control the peeling residue and light resistance.
[0047] In the acrylic polymer, the proportion of the (B) component used is preferably 0 to 70% by mass, more preferably 3 to 55% by mass, based on the total monomer components. By setting the proportion of the (B) component within the above range, it becomes easy to control the adhesion.
[0048] In the acrylic polymer, the proportion of the (C) component used is preferably 0 to 10% by mass, more preferably 2 to 8% by mass, of the total monomer components. By setting the proportion of the (C) component within the above range, it becomes easy to control the degree of crosslinking caused by the reaction with the peeling residue and the curing agent.
[0049] The acrylic polymer can be produced by appropriately selecting a known production method such as solution polymerization, bulk polymerization, emulsion polymerization, radical polymerization, etc. The obtained acrylic polymer may be any of a random copolymer, a block copolymer, a graft copolymer, etc.
[0050] When the molecular weight of the acrylic polymer is within the range of 700,000 to 2,500,000 as the weight average molecular weight, the pressure-sensitive adhesive layer has an appropriate cohesive strength and adhesive strength, is less likely to leave adhesive residue, and has sufficient adhesive strength and load-bearing capacity, which is preferable.
[0051] The weight average molecular weight is a value measured by gel permeation chromatography (GPC) analysis and is expressed in terms of standard polystyrene. The GPC analysis can be performed using tetrahydrofuran (THF) as a solvent.
[0052] In this embodiment, the adhesive of the adhesive layer preferably contains a reaction product of an acrylic polymer and a curing agent, but may contain an acrylic polymer that does not react with the curing agent in consideration of softness.
[0053] The curing agent is not particularly limited as long as it is a curing material used as a normal adhesive, and examples thereof include metal salts, metal alkoxides, aldehyde compounds, non-amino resin amino compounds, urea compounds, isocyanate compounds, polyfunctional epoxy compounds, metal chelate compounds, melamine compounds, aziridine compounds, etc. Among these, isocyanate compounds and epoxy compounds are preferred from the viewpoint of reactivity with carboxyl groups or hydroxyl groups.
[0054] Examples of the isocyanate compound include xylylene diisocyanate, hexamethylene diisocyanate, tolylene diisocyanate, and multimers, derivatives, polymers, etc. These may be used alone or in combination of two or more.
[0055] Examples of epoxy compounds include compounds having two or more epoxy groups in the molecule, and specific examples thereof include ethylene glycol diglycidyl ether, polyethylene glycol diglycidyl ether, glycerin diglycidyl ether, glycerin triglycidyl ether, 1,6-hexanediol diglycidyl ether, trimethylolpropane triglycidyl ether, diglycidylaniline, diamine glycidylamine, N,N,N',N'-tetraglycidyl-m-xylylenediamine, 1,3-bis(N,N'-diamine glycidylaminomethyl), etc. These may be used alone or in combination of two or more.
[0056] As the silicone resin, for example, a silicone resin known as an adhesive can be suitably used. Specifically, an organopolysiloxane having silanol groups at both ends of the molecular chain and RSiO 0.5 (wherein R represents a substituted or unsubstituted monovalent hydrocarbon group) and an organopolysiloxane having a SiO2 unit, and the like. These are available as silicone adhesives KR-101-10, KR-120, KR-130, and X-40-3068 (all of which are product names manufactured by Shin-Etsu Chemical Co., Ltd.).
[0057] Examples of the thermoplastic elastomer include styrene-based thermoplastic elastomers, (meth)acrylic acid ester-based thermoplastic elastomers, olefin-based thermoplastic elastomers, etc. More specifically, the thermoplastic elastomers described in Japanese Patent No. 5513616 can be used. Among these high molecular weight components, acrylic polymers are preferred because it is easy to control the mixability with the polyvinyl ether compound. These high molecular weight components may be used alone or in combination of two or more. In the present invention, the term "adhesive having an acrylic polymer as a base material" refers to an adhesive containing an acrylic polymer itself, or an adhesive containing a reaction product of an acrylic polymer and a curing agent or the like.
[0058] The content of the acrylic polymer in the total mass of the adhesive forming the adhesive layer 14 is usually 90 to 99 mass %, preferably 92 to 98 mass %, and particularly preferably 94 to 96 mass %, from the viewpoint of reducing peeling residue.
[0059] The adhesive forming the adhesive layer 14 preferably contains a polyvinyl ether compound in addition to the base material such as the acrylic polymer. The use of a polyvinyl ether compound as an adhesive is more effective in reducing the amount of peeling residue. Examples of polyvinyl ether compounds include homopolymers of vinyl ethers such as methyl vinyl ether, ethyl vinyl ether, butyl vinyl ether, isobutyl vinyl ether, and (2-methoxyethyl) vinyl ether, copolymers of two or more vinyl ethers, and copolymers of these vinyl ethers with other monomers. Among these, polyvinyl ether compounds containing methyl vinyl ether as a raw monomer are preferred from the viewpoint of controlling peeling residue.
[0060] In the adhesive forming the adhesive layer 14, the blending ratio of the base material such as the acrylic polymer to the polyvinyl ether compound is 90:10 to 99:1, preferably 92:8 to 98:2, and particularly preferably 94:6 to 96:4, on a mass basis, from the viewpoint of reducing peeling residue.
[0061] In addition, the adhesive forming the adhesive layer of the pellicle may contain other components such as crosslinkers, tackifiers, plasticizers, stabilizers, viscosity regulators, antistatic agents, lubricants, electrical conductivity agents, flame retardant agents, thermal conductivity improvers, heat resistance improvers, weather resistance improvers, thixotropy agents, antioxidants, antibacterial agents, antifungal agents, and colorants, depending on the purpose, within the scope of the present invention.
[0062] The adhesive layer 14 is formed by applying an uncured liquid or paste adhesive to the lower end surface of the pellicle frame 11, and then performing a curing process to form an adhesive layer. The adhesive may be applied once, or may be applied several times in order to obtain a predetermined thickness of the adhesive layer. In this case, it is preferable to leave the adhesive between each application until the shape of the adhesive after application is stabilized. In addition, if the viscosity of the adhesive is high and application is difficult, the adhesive may be diluted with an organic solvent, alcohol, water, etc. as necessary to reduce the viscosity of the adhesive before application. The adhesive can be applied by, for example, dipping, spraying, brushing, or using an application device such as a dispenser, but application using an application device such as a dispenser is preferable in terms of stability, workability, yield, etc.
[0063] In the manufacture of pellicle 10, normally, the adhesive layer 14 is applied and formed first, and then the pellicle film 12 is stretched, but the order may be reversed. The pellicle film 12 is stretched, for example, by applying an adhesive to the upper end surface of pellicle frame 11, then heating pellicle frame 11 to harden the adhesive, and finally attaching the upper end surface of pellicle frame 11 on which the adhesive layer 13 for attaching the pellicle film has been formed, to a pellicle film mounted on an aluminum frame larger than pellicle frame 11, and removing any excess of the pellicle film that protrudes outside pellicle frame 11 to complete the pellicle.
[0064] By using the pellicle of the present invention having the above-described configuration, it is possible to reduce the amount of adhesive residue when the pellicle is peeled off from the exposure master after use in lithography. In addition, according to the present invention, a method for reducing the amount of adhesive residue remaining on the pellicle after peeling off the adhesive layer of the pellicle is provided by using the pellicle of the present invention. Therefore, the pellicle of the present invention is useful as a phase shift photomask having the above-mentioned delicate phase shift film, or as a pellicle that can be attached to a surface mainly composed of silicon oxide, such as quartz.
[0065] It is also useful as a pellicle applied to an exposure master in which the pressure-sensitive adhesive layer is irradiated with exposure light during exposure, such as a negative-type exposure master, an exposure master having a non-light-shielded area or a semi-transparent light-shielded area in the adhesive-attached area, an exposure master having a transparent area in the adhesive-attached area, etc. The pressure-sensitive adhesive layer of the pellicle used in such an exposure master is exposed to exposure light through the exposure master from the side opposite to the side of the exposure master on which the pellicle is provided.
[0066] The pellicle of the present invention may be used not only as a protective member for preventing foreign matter from adhering to an exposed master in an exposure device, but also as a protective member for protecting the exposed master during storage or transportation of the exposed master. An exposed master with a pellicle can be manufactured by attaching the above-mentioned pellicle to an exposed master such as a photomask.
[0067] The manufacturing method of a semiconductor device or liquid crystal display panel according to this embodiment includes a step of exposing a substrate (semiconductor wafer or liquid crystal original plate) using the above-mentioned exposure master with pellicle. For example, in a lithography process, which is one of the manufacturing processes of a semiconductor device or liquid crystal display panel, the above-mentioned exposure master with pellicle is placed on a stepper and exposed to light in order to form a photoresist pattern corresponding to an integrated circuit or the like on the substrate. As a result, even if foreign matter adheres to the pellicle in the lithography process, the foreign matter is not imaged on the wafer coated with photoresist, so that short circuits or breaks in the integrated circuits or the like due to the image of the foreign matter can be prevented. Therefore, the use of the exposure master with pellicle can improve the yield in the lithography process.
[0068] In general, when a desired number of lithography steps are performed, when foreign matter or haze occurs, or when the pellicle film is damaged, the pellicle may be peeled off from the exposure master plate and the exposure master plate may be regenerated and cleaned.By using the pellicle of the present invention, even if the exposure master plate has a surface mainly composed of silicon oxide that is likely to cause peeling residue of the adhesive layer, a negative type exposure master plate in which the adhesive layer is irradiated with more exposure light than before, an exposure master plate having a non-shielded area or a semi-transparent light-shielded area in the adhesive attachment part in which the exposure light is irradiated with more exposure light than before, or an exposure master plate having a transparent area in the adhesive attachment part in which the exposure light is irradiated with more exposure light than before, the exposure master plate in which the adhesive layer is irradiated with more exposure light than before, the exposure master plate in which the adhesive layer is irradiated with more exposure light than before, etc., the peeling residue during repellicle can be reduced. In addition, by using the pellicle of the present invention, the amount of peeled off residue of the adhesive layer is reduced, making it easier to apply cleaning with functional water, and improving the cleaning properties of delicate exposure masters such as phase shift photomasks. In addition, cleaning with functional water can contribute to reducing the environmental load. EXAMPLES
[0069] The present invention will be specifically illustrated and described below with reference to examples. Note that the "mask" in the examples and comparative examples is described as an example of an "exposure master", and it goes without saying that the present invention can also be applied to a reticle in the same manner.
[0070] Example 1 After precision cleaning of an aluminum alloy pellicle frame (outer dimensions: 149 mm x 115 mm x 3 mm, thickness 2 mm, flatness of the end face coated with the adhesive for attaching the mask: 15 um), an acrylic adhesive manufactured by Soken Chemical & Chemical Industries, Ltd. (product name: SK Dyne SN-70A, containing an acrylic polymer in which 95% by mass of the monomer component is an ethylene oxide group-containing (meth)acrylate as a base material, containing 2% by mass (solid content) of a polyvinyl ether compound for 30% by mass (solid content) of the acrylic polymer) was applied to the end face on the 15 um side in the same width as the width of the pellicle frame over the entire circumference of the end face, and left at room temperature for 60 minutes. After that, a separator was placed on an aluminum plate with a flatness of 5 um, and the pellicle frame coated with the adhesive was placed so that the adhesive was facing downward. As a result, the adhesive was flattened by contacting the flat separator. Next, the pellicle on the aluminum plate was placed in a 60°C oven for 60 minutes to harden the adhesive, forming an adhesive layer with a thickness of 240 μm. Then, the pellicle was taken out together with the aluminum plate, and the separator was peeled off.
[0071] Thereafter, an adhesive (product name: Cytop CTX-A) manufactured by Asahi Glass Co., Ltd. was applied to the end face opposite to the adhesive application. The pellicle frame was then heated at 130° C. to harden the adhesive. Finally, the adhesive-coated end face of the pellicle frame was attached to a pellicle film mounted on an aluminum frame larger than the pellicle frame, and the portion outside the pellicle frame was removed to complete the pellicle.
[0072] Next, the mass of the 6025 mask substrate was measured and recorded. The mask substrate whose mass had been measured and the pellicle prepared above were set in the attachment device, and the pellicle was attached to the mask substrate by applying a pressure of 50 N for a loading time of 30 seconds.
[0073] The mask substrate with the pellicle attached was left at room temperature for 24 hours, and then ultraviolet rays were applied at 10 mJ / cm using a 193 nm ultraviolet lamp so that the light was directed at the attached part of the adhesive layer from the back side of the mask. 2 Irradiated. After the ultraviolet irradiation, the mask was left at room temperature for 1 hour, and then the pellicle was slowly peeled upward from the mask substrate at a speed of 0.1 mm / sec.
[0074] When the mask substrate was visually inspected after peeling, a slight faint streak was found at the outline where the pellicle had been attached. The mass of the substrate after peeling was measured and compared with the measured value before attachment, and the difference in mass was +0.08 mg.
[0075] Example 2 A pellicle was completed using the same procedure as in Example 1, except that an acrylic adhesive manufactured by Soken Chemical Industries, Ltd. (product name: SN-25B, containing an acrylic polymer as a base material in which 40% by mass of the monomer component is an ethylene oxide group-containing (meth)acrylate) was used as the mask attachment adhesive, and was attached to a 6025 mask substrate similar to that of Example 1.
[0076] As in Example 1, the mask substrate with the pellicle attached was left at room temperature for 24 hours, and then ultraviolet rays were applied at 10 J / cm using a 193 nm ArF laser so that the light was directed to the attached portion of the adhesive layer from the back side of the mask. 2 Irradiated. After the ultraviolet irradiation, the mask was left at room temperature for 1 hour, and then the pellicle was slowly peeled upward from the mask substrate at a speed of 0.1 mm / sec. When the mask substrate was visually inspected after peeling, a slight faint streak was observed at the outline where the pellicle had been attached. The mass of the substrate after peeling was measured and compared with the measured value before attachment, and the difference in mass was +0.09 mg.
[0077] Example 3 A pellicle was completed using the same procedure as in Example 1, except that an acrylic adhesive manufactured by Soken Chemical Industries, Ltd. (product name: SN-24C, containing an acrylic polymer as a base material in which 90% by mass of the monomer component is an ethylene oxide group-containing (meth)acrylate) was used as the mask attachment adhesive.The pellicle was attached to a 6025 mask substrate similar to that of Example 1.
[0078] As in Example 1, the mask substrate with the pellicle attached was left at room temperature for 24 hours, and then ultraviolet rays were applied at 10 J / cm using a 193 nm ArF laser so that the light was directed to the attached portion of the adhesive layer from the back side of the mask. 2 Irradiated. After the ultraviolet irradiation, the mask was left at room temperature for 1 hour, and then the pellicle was slowly peeled upward from the mask substrate at a speed of 0.1 mm / sec. When the mask substrate was visually inspected after peeling, a slight faint streak was found at the outline where the pellicle had been attached. The mass of the substrate after peeling was measured and compared with the measured value before attachment, and the difference in mass was +0.08 mg.
[0079] Comparative Example 1 A pellicle was completed in the same manner as in Example 1, except that an acrylic adhesive manufactured by Soken Chemical Industries, Ltd. (product name: SK Dyne SK-1425S, 0 mass% ethylene oxide group-containing (meth)acrylate monomer, 100 mass% other (meth)acrylate monomers) was used as the mask attachment adhesive, and was attached to a 6025 mask substrate similar to that of Example 1.
[0080] As in Example 1, the mask substrate with the pellicle attached was left at room temperature for 24 hours, and then ultraviolet rays were applied at 10 J / cm using a 193 nm ArF laser so that the light was directed to the attached portion of the adhesive layer from the back side of the mask. 2 Irradiated. After the ultraviolet irradiation, the mask was left at room temperature for 1 hour, and then the pellicle was slowly peeled upward from the mask substrate at a speed of 0.1 mm / sec. When the mask substrate was visually inspected after peeling, a thin adhesive residue was found in the area where the pellicle had been attached. The mass of the substrate after peeling was measured and compared with the measured value before attachment, and the difference in mass was +0.58 mg.
[0081] Comparative Example 2 A pellicle was completed in the same manner as in Example 1, except that a silicone adhesive (product name: X40-3122) manufactured by Shin-Etsu Chemical Co., Ltd. was used as the mask attachment adhesive, and the pellicle was attached to a 6025 mask substrate similar to that in Example 1.
[0082] As in Example 1, the mask substrate with the pellicle attached was left at room temperature for 24 hours, and then ultraviolet rays were applied at 10 J / cm using a 193 nm ArF laser so that the light was directed to the attached portion of the adhesive layer from the back side of the mask. 2 Irradiated. After the ultraviolet irradiation, the mask was left at room temperature for 1 hour, and then the pellicle was slowly peeled upward from the mask substrate at a speed of 0.1 mm / sec. When the mask substrate was visually inspected after peeling, adhesive residue was found over the entire area where the pellicle had been attached. The mass of the substrate after peeling was measured and compared with the measured value before attachment, and the difference in mass was +3.50 mg. [Explanation of symbols]
[0083] 1 Exposure master 10 Pellicle 11 Pellicle frame 12 Pellicle membrane 13 Adhesive layer for attaching pellicle membrane 14 Adhesive layer 15 Air pressure adjustment hole (vent) 16 Dust removal filter
Claims
1. A pellicle frame with an adhesive layer, comprising: a pellicle frame; and an adhesive layer provided on one end surface of the pellicle frame, After the adhesive layer of the adhesive-layer-attached pellicle frame was attached to the quartz mask substrate, 193 nm ultraviolet light was applied at 10 J / cm from the rear surface of the substrate to the adhesive layer-attached portion of the adhesive-layer-attached pellicle frame. 2 and when the pellicle frame with the adhesive layer is peeled off after the irradiation, the amount of peeled residue of the adhesive layer remaining on the substrate is 0.5 mg or less.
2. A pellicle frame with an adhesive layer as described in claim 1, wherein the adhesive that forms the adhesive layer has an acrylic polymer as a base material.
3. A pellicle frame with an adhesive layer as described in claim 2, wherein the acrylic polymer has a (meth)acrylic acid ester having an ether bond as a monomer component.
4. A pellicle frame with an adhesive layer as described in claim 3, wherein the (meth)acrylic acid ester having an ether bond is a (meth)acrylic acid ester having an alkylene oxide group.
5. A pellicle frame with an adhesive layer as described in claim 4, wherein the alkylene oxide group is an ethylene oxide group.
6. A pellicle frame with an adhesive layer described in any one of claims 1 to 5, wherein the adhesive forming the adhesive layer contains a polyvinyl ether compound.
Citation Information
Patent Citations
Semiconductor differential pressure transmitter
JP1981038693A
Water-soluble tack agent composition, solder masking agent, adhesive tape and production of adhesive tape
JP1993209160A
Processed tacky adhesive product of photosensitive film
JP2005171211A
Large pellicle
JP2006146085A
Hardly contaminating pellicle and method for producing the same
JP2007156397A