Sensors and Sensing Devices

A flexible sensor design with conductive linear bodies and an electrolyte layer generates high voltage for wireless communication, improving upon previous moisture sensors.

JP7588020B2Active Publication Date: 2024-11-21LINTEC CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021055627
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-29
Publication Date
2024-11-21
Estimated Expiration
2041-03-29

AI Technical Summary

Technical Problem

Existing moisture sensors using sheet members as electrodes lack flexibility and do not generate sufficient electromotive force for wireless transmission.

Method used

A sensor design featuring a pair of conductive linear bodies with different ionization tendencies, connected in series through an electrolyte layer, and covered partially to allow contact with moisture, generating high voltage.

Benefits of technology

The sensor achieves high flexibility and generates sufficient electromotive force for wireless communication, addressing the limitations of previous designs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007588020000002
    Figure 0007588020000002
  • Figure 0007588020000003
    Figure 0007588020000003
  • Figure 0007588020000004
    Figure 0007588020000004
Patent Text Reader

Abstract

To provide a sensor that is excellent in flexibility and can generate a high voltage.SOLUTION: A sensor 100 comprises: two or more pairs of wiring including first wiring 11 including a conductivity linear body, and second wiring 12 including the conductivity linear body and made of a material in ionization tendency from the first wiring 11; a wiring fixation member 3 that fixes the pair of wiring; and a coated material 4 that covers more than at least one of the pair of wiring, and does not let water pass. One of the pair of wiring is not coated with the covered material 4. Aside from the pair of wiring not coated with the coated material 4, an electrolyte layer 2 is provided between the first wiring 11 and second wiring 12, and the pair of wiring themselves is electrically connected in series.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to sensors and sensing devices. [Background technology]

[0002] As a moisture sensor for detecting moisture, one that utilizes an electromotive force generated when moisture comes into contact with a pair of electrodes has been proposed. For example, Patent Document 1 describes an electromotive module provided in a worn article having an absorbent body that receives excrement. This electromotive module has a pair of electrodes made of materials with different ionization tendencies, and at least one of the pair of electrodes has a skeleton structure having a skeleton portion and a void portion provided between the skeleton portions. An electromotive force is generated when the pair of electrodes come into contact with urine excreted in the absorbent body. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2015-229003 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, in the electromotive module described in Patent Document 1, sheet members such as carbon printed sheets and aluminum sheets are used as electrodes. Therefore, when the sheet members are thick, there is a problem that they lack flexibility and the wearer feels uncomfortable wearing them. In addition, the electromotive force at the electrodes is not necessarily sufficient, and it is not possible to supply enough power to drive the wireless transmission module.

[0005] An object of the present invention is to provide a sensor and a sensing device that are highly flexible and capable of generating a high voltage. [Means for solving the problem]

[0006] According to one aspect of the present invention, a sensor is provided comprising: two or more pairs of wiring including a first wiring including a conductive linear body and a second wiring including a conductive linear body and made of a material having a different ionization tendency from the first wiring; a wiring fixing material for fixing the pair of wiring; and a water-impermeable coating for covering at least one or more of the pair of wiring, wherein one of the pair of wirings is not covered by the coating, an electrolyte layer is provided between the first wiring and the second wiring except for the pair of wirings that is not covered by the coating, and the pair of wirings are electrically connected in series.

[0007] In the sensor according to the aspect of the present invention, it is preferable that the conductive linear body has a diameter of not less than 2 μm and not more than 500 μm.

[0008] In the sensor according to the aspect of the present invention, the electrolyte layer preferably has a thickness of not less than 2 μm and not more than 1 cm.

[0009] In the sensor according to the aspect of the present invention, it is preferable that the conductive linear body has a wave shape in a plan view of the sensor.

[0010] In the sensor according to the aspect of the present invention, it is preferable that the wiring fixing material has elasticity.

[0011] In the sensor according to the aspect of the present invention, it is preferable that a coating containing a metal salt is provided on the pair of wires that are not covered with the coating.

[0012] In a sensor according to one embodiment of the present invention, the combination of materials for the first wiring and the second wiring is preferably any one of a combination of copper and zinc, a combination of copper and aluminum, a combination of aluminum and carbon, a combination of titanium and carbon, a combination of titanium and copper, a combination of zinc and carbon, a combination of zinc and silver, and a combination of zinc and gold.

[0013] According to one aspect of the present invention, there is provided a sensing device comprising a sensor according to the aspect of the present invention, a sensing module that senses the potential difference between the wirings, and a wireless transmission module that transmits a wireless signal. Effect of the Invention

[0014] According to one aspect of the present invention, a sensor and a sensing device that are highly flexible and capable of generating a high voltage can be provided. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a schematic diagram illustrating a sensor according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view showing the II-II cross section of FIG. [Diagram 3] FIG. 2 is a cross-sectional view showing the cross section III-III of FIG. [Figure 4] 5A to 5C are diagrams for explaining a method for manufacturing a sensor according to an embodiment of the present invention. [Diagram 5] 1 is a schematic diagram showing a state in which a sensor according to an embodiment of the present invention is attached to an adherend. [Figure 6] 1 is a schematic diagram illustrating a sensing device according to a first embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, the present invention will be described with reference to the drawings, taking an embodiment as an example. The present invention is not limited to the contents of the embodiment. In the drawings, some parts are illustrated enlarged or reduced in size for ease of explanation.

[0017] (Sensor) 1, 2, and 3, the sensor 100 according to this embodiment includes two or more pairs of wiring including a first wiring 11 and a second wiring 12, a wiring fixing material 3 that fixes the pair of wiring, and a water-impermeable coating 4. The first wiring 11 and the second wiring 12 each include a conductive linear body. The second wiring 12 is made of a material having a different ionization tendency from that of the first wiring 11. One of the pair of wires is not covered by the coating 4. Since the pair of wires is not covered by the coating 4, the pair of wires can directly come into contact with water and can detect moisture. Hereinafter, this part may be referred to as a detection section. In addition, as shown in FIG. 2, an electrolyte layer 2 is provided between the first wiring 11 and the second wiring 12 of the other pair of wires, and the pair of wires is configured like a battery. Hereinafter, this part may be referred to as a battery section. Furthermore, in the two or more pairs of wires, the first wiring 11 of one pair of wires and the second wiring 12 of the other pair of wires are in contact with each other in a portion where there is no electrolyte layer 2, as shown in FIG. 3, and are electrically connected in series.

[0018] In the pair of wirings that are not covered with the coating 4, the first wiring 11 and the second wiring 12 are configured not to come into contact with each other. When an object to be detected comes into contact between the first wiring 11 and the second wiring 12, the object to be detected can be sensed by the sensor 100. Furthermore, the pair of wirings covered with the coating 4 has an electrolyte layer 2 provided between the first wiring 11 and the second wiring 12, and this combination constitutes a type of battery, with multiple sets of such batteries being connected in series. Furthermore, when moisture comes into contact between the first wiring 11 and the second wiring 12 in the detection unit, an electromotive force is also generated in the detection unit. Since the battery unit and the detection unit are electrically connected in series, a high electromotive force is generated in the sensor 100 when the object to be detected comes into contact with the detection unit. The object to be detected is not particularly limited as long as it is a fluid that can pass electricity. Specific examples include liquids and gel-like fluids. More specific examples include water, urine, and blood. Particularly preferred objects to be detected include substances that contain moisture. The sensor 100 is preferably a moisture sensor, and more preferably a urine sensor.

[0019] (Pair of wires) The pair of wirings used in this embodiment includes a first wiring 11 including a conductive linear body and a second wiring 12 including a conductive linear body. Here, the material of the second wiring 12 needs to have a different ionization tendency from the material of the first wiring 11. With this configuration, when a detection object comes into contact between the first wiring 11 and the second wiring 12, an electromotive force is generated, and the detection object can be sensed by the sensor 100.

[0020] A metal may be plated or vapor-deposited on the surface of each of the first wiring 11 and the second wiring 12. When a metal is plated or vapor-deposited on the surface, the material of the surface of the second wiring 12 needs to have a different ionization tendency from the material of the surface of the first wiring 11. The surface materials of the first wiring 11 and the second wiring 12 are, for example, aluminum (-1.676 V), titanium (-1.63 V), zinc (-0.7626 V), chromium (-0.74 V), iron (-0.44 V), nickel (-0.257 V), tin (-0.1375 V), copper (0.340 V), silver (0.7991 V), gold (1.52 V), and carbon. The values ​​in parentheses above are the values ​​of standard electrode potential. In this specification, conductive materials that are not ionically conductive, such as carbon, are treated as 0 V for convenience.

[0021] From the viewpoint of the electromotive force required for sensing or wireless communication, the difference in ionization tendency between the materials of the surfaces of the first wiring 11 and the second wiring 12 is preferably 0.5 V or more, more preferably 0.8 V or more, and even more preferably 1.1 V or more. Preferred combinations of the surface materials of the first wiring 11 and the second wiring 12 include a combination of copper and zinc, a combination of copper and aluminum, a combination of aluminum and carbon, a combination of titanium and carbon, a combination of titanium and copper, a combination of zinc and carbon, a combination of zinc and silver, and a combination of zinc and gold.

[0022] (Conductive wire) The conductive linear body used for the first wiring 11 and the second wiring 12 is not particularly limited as long as it has conductivity, and examples of the conductive linear body include a linear body including a metal wire and a linear body including a conductive thread, etc. The conductive linear body may be a linear body including a metal wire and a conductive thread (such as a linear body in which a metal wire and a conductive thread are twisted together). In this specification, the term "linear body" refers to a linear member. The length of the linear body is, for example, 1 cm or more. The shape of the linear body is not particularly limited, and may be a single linear member or an assembly of multiple linear members. The cross-sectional shape of the linear body may be various shapes depending on the shape of the linear body.

[0023] The conductive linear body preferably has a wave shape in a plan view of the sensor 100. Examples of the wave shape include a sine wave, a rectangular wave, a triangular wave, and a sawtooth wave. If the conductive linear body has such a structure, breakage of the conductive linear body can be suppressed when the sensor 100 is stretched in the axial direction of the conductive linear body. Furthermore, if the conductive linear body has such a structure, in one part of the wave shape, the first wiring 11 and the second wiring 12 of the pair of wirings can be prevented from contacting each other, as shown in Fig. 2, and in another part of the wave shape, the first wiring 11 of one pair of wirings can be in contact with the second wiring 12 of the other pair of wirings, as shown in Fig. 3. Therefore, the pair of wirings can be electrically connected in series.

[0024] Both the linear body including a metal wire and the linear body including a conductive thread have high electrical conductivity, and therefore, when used as a conductive linear body, it becomes easy to reduce the resistance of the first wiring 11 and the second wiring 12.

[0025] Examples of the metal wire include wires containing metals such as copper, aluminum, tungsten, iron, molybdenum, nickel, titanium, silver, and gold, or alloys containing two or more metals (steels such as stainless steel and carbon steel, brass, phosphor bronze, zirconium-copper alloys, beryllium copper, iron-nickel, nichrome, nickel-titanium, Kanthal, Hastelloy, and rhenium-tungsten, etc.). The metal wire may be plated with tin, zinc, silver, nickel, chromium, nickel-chromium alloys, solder, etc., or may be surface-coated with a carbon material described later.

[0026] The metal wire may be a metal wire coated with a carbon material, which can inhibit metal corrosion.

[0027] Examples of the carbon material that coats the metal wire include amorphous carbon (carbon black, activated carbon, hard carbon, soft carbon, mesoporous carbon, carbon fiber, etc.), graphite, fullerene, graphene, and carbon nanotubes.

[0028] The linear body including the conductive thread may be a linear body made of one conductive thread, or may be a linear body made of twisted conductive threads. It may also be a linear body made of twisted conductive thread and insulating thread. The linear body including the conductive thread has an advantage that it is more flexible and less likely to break than a linear body including a metal wire. Examples of conductive yarns include yarns containing conductive fibers (such as metal fibers, carbon fibers, and fibers of ion-conductive polymers), yarns containing conductive microparticles (such as carbon nanoparticles), yarns whose surfaces are plated or vapor-deposited with metals (such as copper, silver, and nickel), and yarns impregnated with metal oxides.

[0029] A particularly suitable example of a linear body containing a conductive thread is a linear body containing a thread (carbon nanotube thread) containing carbon nanotubes as carbon nanoparticles (hereinafter also referred to as a "carbon nanotube linear body").

[0030] The carbon nanotube linear body can be obtained, for example, by drawing carbon nanotubes into a sheet shape from the end of a carbon nanotube forest (a growth body in which multiple carbon nanotubes are grown on a substrate so as to be aligned in a direction perpendicular to the substrate, and sometimes referred to as an "array"), bundling the drawn carbon nanotube sheets, and twisting the bundle of carbon nanotubes. In such a manufacturing method, if no twist is applied during twisting, a ribbon-shaped carbon nanotube linear body is obtained, and if twist is applied, a thread-shaped linear body is obtained. The ribbon-shaped carbon nanotube linear body is a linear body that does not have a structure in which a collection of multiple carbon nanotubes is twisted. In addition, the carbon nanotube linear body can be obtained by spinning a dispersion of carbon nanotubes. The carbon nanotube linear body can be manufactured by spinning, for example, by the method disclosed in U.S. Patent Publication US 2013 / 0251619 (JP Patent Publication 2012-126635). From the viewpoint of obtaining uniformity in the diameter of the carbon nanotube linear body, it is preferable to use a thread-like carbon nanotube linear body, and from the viewpoint of obtaining a high-purity carbon nanotube linear body, it is preferable to obtain a thread-like carbon nanotube linear body by twisting a carbon nanotube sheet. The carbon nanotube linear body may be a linear body in which two or more carbon nanotube linear bodies are twisted together.

[0031] The carbon nanotube linear body may be a linear body including a carbon nanotube and a conductive material other than the carbon nanotube, such as a metal, a conductive polymer, graphene, etc. (hereinafter, also referred to as a "composite linear body.") The composite linear body tends to improve the conductivity of the linear body while maintaining the above-mentioned characteristics of the carbon nanotube linear body.

[0032] Examples of the composite linear body include linear bodies containing carbon nanotubes and metals, such as (1) a composite linear body in which a metal element or a metal alloy is supported on the surface of a forest, sheet or bundle of carbon nanotubes, or a twisted linear body, by vapor deposition, ion plating, sputtering, spray coating, wet plating, or the like, in a process of obtaining a carbon nanotube linear body by drawing out carbon nanotubes from an end of a carbon nanotube forest into a sheet shape, bundling the drawn carbon nanotube sheet, and twisting the bundles of carbon nanotubes, (2) a composite linear body in which a bundle of carbon nanotubes is twisted together with a linear body of a metal element or a linear body of a metal alloy, or a composite linear body, and (3) a composite linear body in which a linear body of a metal element or a linear body of a metal alloy, or a composite linear body, is twisted with a carbon nanotube linear body or a composite linear body, etc. In the composite linear body of (2), a metal may be supported on the carbon nanotubes when twisting the bundles of carbon nanotubes, as in the composite linear body of (1). In addition, the composite linear body of (3) is a composite linear body in which two linear bodies are woven together, but as long as it contains at least one linear body of a simple metal or a linear body of a metal alloy, or a composite linear body, it may be a composite linear body in which three or more carbon nanotube linear bodies, or linear bodies of a simple metal or a linear body of a metal alloy, or a composite linear body are woven together. Examples of metals for the composite linear body include elemental metals (gold, silver, copper, iron, aluminum, nickel, chromium, tin, zinc, etc.) and alloys containing at least one of these elemental metals (copper-nickel-phosphorus alloy, copper-iron-phosphorus-zinc alloy, etc.).

[0033] Among these conductive linear bodies, conductive linear bodies containing carbon nanotube yarns (particularly, conductive linear bodies containing only carbon nanotube yarns and conductive linear bodies containing carbon nanotube yarns and a non-metallic conductive material) are preferred. For example, threads whose surfaces are plated or vapor-deposited with metals (copper, silver, nickel, etc.) or threads impregnated with metal oxides are prone to cracking in the metal or metal oxide when stretched repeatedly, and have low durability. In this regard, carbon nanotube linear bodies are highly resistant to bending, and their resistance value is less likely to change even when stretched repeatedly. Carbon nanotube linear bodies also have the advantage of being highly corrosion-resistant.

[0034] Here, the linear resistance (resistivity) of the conductive linear body is 5.0×10 -3 Ω / cm or more 1.0×10 3 It is preferable that the resistance is 1.0×10 -2 Ω / cm or more 5.0×10 2 It is more preferable that the linear resistance of the conductive linear body is Ω / cm or less. If the conductive linear body is made of a metal with high conductivity, the linear resistance of the conductive linear body can be set to the lower limit or more. On the other hand, if the linear resistance of the conductive linear body is equal to or less than the upper limit, the resistance can be kept low even if the wiring path is long, and the problem that the wiring itself becomes a resistor and puts a load on the measuring instrument can be suppressed.

[0035] The linear resistance of the conductive linear body is measured as follows. First, silver paste is applied to both ends of the conductive linear body, and the resistance between the silver pastes is measured to obtain the resistance value (unit: Ω) of the conductive linear body. The obtained resistance value is then divided by the distance (cm) between the silver pastes to calculate the linear resistance of the conductive linear body.

[0036] The cross-sectional shape of the conductive linear body is not particularly limited and may be polygonal, flat, elliptical, circular, etc., but is preferably elliptical or circular. When the cross section of the conductive linear body is circular, the diameter of the conductive linear body is more preferably 2 μm to 500 μm, and from the viewpoints of flexibility and durability, the diameter of the conductive linear body is more preferably 5 μm to 300 μm, and further preferably 10 μm to 100 μm. When the cross section of the conductive linear body is elliptical, the major axis is preferably in the same range as the above diameter, and when the cross section of the conductive linear body is polygonal, the diameter of the circumferential circle of the polygon is preferably in the same range as the above diameter.

[0037] The diameter of the conductive linear body is determined by observing the cross section of the conductive linear body using a digital microscope, measuring the diameter of the conductive linear body, and averaging the measured diameters.

[0038] (electrolyte layer) The electrolyte layer 2 is formed in a band shape in a plan view of the sensor 100, as shown in Fig. 1. The electrolyte layer 2 is formed in a film shape having a predetermined thickness, as shown in Fig. 2. In the pair of wirings covered with the coating 4, the electrolyte layer 2 is provided between the first wiring 11 and the second wiring 12, as shown in Fig. 2. The component constituting the electrolyte layer 2 is preferably a polymer solid electrolyte consisting of a solid solution of a polymer compound and an electrolyte. The electrolyte is preferably a metal salt. The polymer compound contained in the electrolyte layer 2 preferably has a mass average molecular weight of 100,000 or more, and more preferably has a mass average molecular weight of 100,000 or more and 1,000,000 or less. Examples of the polymer compound include ion-conductive polymers such as polyethylene oxide, polyethylene carbonate, polyacrylonitrile, polyvinylidene fluoride, polymethyl methacrylate, polyhexafluoropropylene, and polyethylene oxide. Known metal salts can be used, including alkali metal salts such as lithium salts and sodium salts, and alkaline earth metal salts such as magnesium salts and calcium salts.

[0039] From the viewpoint of the effect of increasing the electromotive force, the thickness of the electrolyte layer 2 is preferably 2 μm to 1 cm, more preferably 5 μm to 1 mm, and further preferably 10 μm to 100 μm.

[0040] (Wiring fixing material) Examples of the wiring fixing material 3 include an adhesive sheet having an adhesive layer and a heat seal made of a thermoplastic resin. The first wiring 11 and the second wiring 12 can be supported and fixed by this wiring fixing material 3. Furthermore, when the first wiring 11 or the second wiring 12 is formed on the wiring fixing material 3, the adhesive layer or heat seal makes it easy to attach the first wiring 11 or the second wiring 12 to the wiring fixing material 3. Furthermore, it is preferable that the wiring fixing material 3 has elasticity. In such a case, the elasticity and flexibility of the sensor 100 can be ensured.

[0041] The adhesive layer constituting the adhesive sheet is preferably formed from an adhesive composition containing an adhesive resin from the viewpoints of processability, wiring retention, stretchability and handling. The form of the adhesive composition is not particularly limited, and may be, for example, any of a solvent-type adhesive composition, an emulsion-type adhesive composition, a hot melt-type adhesive composition and a heat-sensitive adhesive composition. Here, the hot melt-type adhesive refers to an adhesive that melts when heated and becomes spreadable and coatable, and develops adhesion and cohesive force when cooled. The heat-sensitive adhesive refers to an adhesive that has a relatively low adhesive strength at room temperature (25°C) and becomes highly adhesive when heated to a temperature above room temperature (25°C) (for example, 60°C to 80°C).

[0042] Examples of the adhesive resin include acrylic resin, urethane resin, rubber resin, olefin resin, silicone resin, and energy ray curable resin having a polymerizable functional group in these resins. In addition, when the adhesive layer is formed from a heat-sensitive adhesive composition, examples of the adhesive resin contained in the heat-sensitive adhesive composition include polyester urethane resin, polyester resin, acrylic resin, vinyl acetate resin, polyurethane resin, and rubber resin. These adhesive resins may be used alone or in combination of two or more. The adhesive composition that is the material for forming the adhesive layer may contain an additive for adhesives depending on the type of adhesive resin or the application of the adhesive sheet. Examples of additives for pressure-sensitive adhesives include crosslinking agents, tackifiers, fillers, antioxidants, heat stabilizers, UV absorbers, light stabilizers, colorants, flame retardants, thickeners, antistatic agents, polymerization initiators, and curing aids.

[0043] For example, when the pressure-sensitive adhesive layer is formed from a hot-melt pressure-sensitive adhesive composition, the hot-melt pressure-sensitive adhesive composition can be a mixture of a block copolymer, a tackifier, and a plasticizer in a predetermined ratio.

[0044] Examples of block copolymers include AB type diblock copolymers and ABA type triblock copolymers. Examples of AB type diblock copolymers include styrene-isobutylene block copolymers (SIB), styrene-butadiene block copolymers (SB), and styrene-isoprene block copolymers (SI). Examples of ABA type triblock copolymers include styrene-isobutylene-styrene block copolymers (SIBS), styrene-butadiene-styrene block copolymers (SBS), and styrene-isoprene-styrene block copolymers (SIS). These can be used alone or in combination of two or more. The tackifier and plasticizer are not particularly limited, and conventionally known tackifiers and plasticizers can be used.

[0045] The adhesive layer is also preferably a pseudo-adhesive layer. The pseudo-adhesive layer has the function of putting the adhesive sheet and the adherend into a pseudo-adhesive state. Here, the pseudo-adhesive state means that the adhesive sheet and the adherend are adhered to each other under normal use conditions, but when the adhesive sheet is peeled off from the adherend, it can be peeled off by simply pulling it by hand without using any tools or the like, and cannot be re-adhered by simply overlapping and pressing it. In this "state in which it cannot be re-adhered by simply overlapping and pressing it", the pseudo-adhesive state is different from adhesion by a normal adhesive. An example of the pseudo adhesive layer is a heat seal layer made of a thermoplastic resin.

[0046] The heat seal layer of a thermoplastic resin is a layer having heat sealability and containing a thermoplastic resin as a main component. The main component means the component having the highest content (mass%) in the heat seal layer. Examples of the thermoplastic resin used to form the heat seal layer include polyethylene, polystyrene, acrylic resin, natural rubber resin, vinyl chloride-vinyl acetate copolymer, ethylene-vinyl acetate copolymer, ultraviolet curing varnish, etc. Among them, polyethylene is preferred as the thermoplastic resin used to form the heat seal layer. A pressure-sensitive adhesive sheet using a "heat seal layer made of a thermoplastic resin" as a pressure-sensitive adhesive layer can be produced, for example, as follows. A composition containing a thermoplastic resin for forming a heat seal layer is heated and melted by an extruder and extruded into a film, and one surface of this film is brought into contact with the surface of a flexible substrate.

[0047] The thickness of the pressure-sensitive adhesive layer is selected depending on the application, but is preferably from 1 μm to 500 μm, more preferably from 5 μm to 300 μm, and even more preferably from 10 μm to 100 μm.

[0048] (covering) The covering 4 covers at least one of the pair of wires and is impermeable to water. One of the pair of wires is not covered by the covering 4. Examples of the covering 4 include a synthetic resin film and a glass film. The covering 4 is preferably stretchable. When the covering 4 is stretchable, the stretchability of the sensor 100 can be ensured even when the pair of wires is covered with the covering 4. As the stretchable covering 4, a synthetic resin film or the like can be used.

[0049] Examples of synthetic resin films include polyethylene films, polypropylene films, polybutene films, polybutadiene films, polymethylpentene films, polyvinyl chloride films, vinyl chloride copolymer films, polyethylene terephthalate films, polyethylene naphthalate films, polybutylene terephthalate films, polyurethane films, ethylene-vinyl acetate copolymer films, ionomer resin films, ethylene-(meth)acrylic acid copolymer films, ethylene-(meth)acrylic acid ester copolymer films, polystyrene films, polycarbonate films, and polyimide films. Other examples of the stretchable covering 4 include crosslinked films and laminated films of these.

[0050] There is no particular limitation on the thickness of the coating 4. The thickness of the coating 4 is preferably 10 μm or more and 10 mm or less, more preferably 15 μm or more and 3 mm or less, and even more preferably 30 μm or more and 1 mm or less.

[0051] (Sensor manufacturing method) There is no particular limitation on the method for manufacturing the sensor 100 according to this embodiment. The sensor 100 can be manufactured, for example, by the following steps. First, a composition for forming the wire fixing material 3 is applied onto the covering 4 to form a coating film as shown in Fig. 4(A). Next, the coating film is dried to prepare the wire fixing material 3. 4(B), a plurality of second wirings 12 are arranged in an array on the wiring fixing material 3, and one first wiring 11 is further arranged to create a lower sheet. Note that the second wiring 12 and the first wiring 11 are each made to have a wave shape when the sensor 100 is viewed in a plan view. Here, in the same manner as described above, a plurality of first wirings 11 are arranged and disposed on the wiring fixing material 3 to create an upper sheet. Note that the first wirings 11 are each made to have a wave shape when the sensor 100 is viewed in a plan view. 4(C), a plurality of strip-shaped electrolyte layers 2 are formed on the lower sheet so as to cover a portion of the second wiring 12 and to extend along the axial direction of the second wiring 12. However, the electrolyte layers 2 are not in contact with the first wiring 11 on the lower sheet and the second wiring 12 adjacent to the first wiring 11 when the sensor 100 is viewed in plan. Next, as shown in FIG. 4(D), an upper sheet is placed on the electrolyte layer 2 to prepare the sensor 100. At this time, the coating 4 is made not to cover at least a part of the first wiring 11 of one pair of wirings and the second wiring 12 of the other adjacent pair of wirings. In addition, in the area covered by the coating 4, as shown in FIG. 2, the electrolyte layer 2 is provided between the pair of first wirings 11 and second wirings 12. Furthermore, as shown in FIG. 3, in the area without the electrolyte layer 2, the first wiring 11 of one pair of wirings and the second wiring 12 of the other pair of wirings are in contact with each other and are electrically connected in series.

[0052] (Sensing device) Next, the sensing device according to this embodiment will be described. 5, the sensing device according to this embodiment includes a sensor 100, a sensing module 5 that senses the potential difference between wirings, and a wireless transmission module 6 that transmits a wireless signal. Furthermore, since the sensor 100 generates an electromotive force upon contact with a detected object, the sensor 100 may be used as a battery to drive the wireless transmission module 6. Furthermore, the sensor 100 can be used, for example, by being attached to an adherend. The adherend is a target to which the sensor 100 is attached, and is not particularly limited. The adherend may be deformable and may have an uneven or curved surface. The adherend may be a woven fabric, a knitted fabric, or the like, and specific examples thereof include a diaper, a sanitary napkin, or an incontinence pad.

[0053] The sensing module 5 includes a first electrode 51 and a second electrode 52. The first electrode 51 is electrically connected to the first wiring 11 constituting the detection unit, and the second electrode 52 is electrically connected to the second wiring 12 constituting at least one battery unit. When an object to be detected comes into contact between the first wiring 11 and the second wiring 12 of the sensor 100 attached to the adherend, an electromotive force is generated, and the object to be detected can be detected by the sensor 100.

[0054] When the sensing module 5 senses contact with an object to be sensed, the wireless transmitting module 6 transmits a wireless signal to a wireless relay station 7 shown in FIG. The wireless relay station 7 receives the wireless signal transmitted from the wireless transmitting module 6, and transmits a signal indicating that the wireless signal has been transmitted to the sensing server 8. Upon receiving the signal from the wireless relay station 7, the sensing server 8 senses that an object to be detected is in contact with the sensor 100 based on the signal, and records this in an information processing terminal (not shown) as necessary.

[0055] (Effects of this embodiment) According to this embodiment, the following advantageous effects can be obtained. (1) In the present embodiment, the first wiring 11 and the second wiring 12 include conductive linear bodies, so that the sensor 100 has excellent flexibility. (2) In this embodiment, the first wiring 11 and the second wiring 12 are made of different materials, and the ionization tendencies of these materials are different. Therefore, when an object to be detected comes into contact with the first wiring 11 and the second wiring 12 that are not covered with the coating 4, an electromotive force is generated, and the object to be detected can be detected by the sensor 100. (3) The pair of wirings covered with the coating 4 has an electrolyte layer 2 provided between the first wiring 11 and the second wiring 12, and these pairs of wirings are electrically connected in series, thereby acting as a battery. When an object to be detected comes into contact between the first wiring 11 and the second wiring 12 of a pair of wirings that are not covered with the coating 4, the electromotive force is increased, and a high voltage can be generated. (4) The conductive linear body has a wave shape in a plan view of the sensor 100. With such a structure, in a part of the wave shape, the first wiring 11 and the second wiring 12 can be prevented from contacting each other as shown in Fig. 2, and in another part of the wave shape, the first wiring 11 and the second wiring 12 can be in contact with each other as shown in Fig. 3. Therefore, the pair of wirings can be electrically connected in series.

[0056] [Modifications of the embodiment] The present invention is not limited to the above-described embodiment, and includes modifications and improvements within the scope of the present invention that can achieve the object of the present invention. For example, in the above embodiment, one of the pair of wirings (the first wiring 11 and the second wiring 12) is not covered with the coating 4, and nothing is provided thereon, but this is not limited thereto. For example, a coating containing an electrolyte may be provided on the first wiring 11 and the second wiring 12 that are not covered with the coating 4. The coating containing an electrolyte may be a water-soluble polymer compound film containing an electrolyte such as a metal salt, etc. Examples of the metal salt include sodium chloride and potassium chloride.

[0057] In the above embodiment, the sensing device includes a wireless transmission module 6 for transmitting a wireless signal, but is not limited thereto. For example, when the sensing module 5 detects contact with a detection object, a signal may be sent using a wired signal module. In addition, this signal may be sent directly to an information processing terminal and recorded by the information processing terminal. EXAMPLES

[0058] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples in any way.

[0059] [Example 1] (Preparation of adhesive sheet with wiring (lower sheet)) An acrylic adhesive ("PK" manufactured by Lintec Corporation) was applied to a thickness of 20 μm on a 50 μm thick urethane film, and the film was cut into a 100 mm x 75 mm rectangle to prepare an adhesive sheet. As the second wiring, a copper wire (diameter 150 μm, "C1100-H AuP" manufactured by Tokusai Co., Ltd.) was prepared. Next, an adhesive sheet was wound around a drum member whose outer circumferential surface was made of rubber so that there were no wrinkles. Both ends of the adhesive sheet in the circumferential direction were fixed with double-sided tape. The copper wire wound around the bobbin was attached to the surface of the adhesive layer located near the end of the drum member, and the copper wire was wound around the drum member while being unwound, and the drum member was moved little by little in a direction parallel to the drum axis so that the copper wire was wound around the drum member while drawing a spiral at equal intervals. At this time, the drum member was rotated while vibrating in the drum axis direction so that the wound copper wire drew a wave shape. In this way, 11 copper wires were provided on the surface of the adhesive sheet and placed at equal intervals. The interval between the copper wires was 8 mm. In addition, the amplitude of the wave shape was 2 mm, and the wavelength was 8 mm. Furthermore, a zinc wire (diameter 150 μm, "Zinc Wire" manufactured by Japan Fine Steel Co., Ltd.) was prepared as the first wiring, and the zinc wire wound around a bobbin was attached to the surface of the adhesive layer so that the copper wire was spaced 8 mm apart from the other wires. The zinc wire was then unwound and wound around the drum member, and the drum member was gradually moved in a direction parallel to the drum axis so that the zinc wire was wound around the drum member while drawing a spiral at equal intervals. At this time, the drum member was rotated while vibrating in the drum axis direction so that the wound zinc wire drew a wavy shape. In this way, one zinc wire was placed on the surface of the adhesive sheet. The amplitude of the wavy shape was 2 mm, and the wavelength was 8 mm. The adhesive sheet with the copper and zinc wires was then cut parallel to the drum axis. The adhesive sheet with the copper and zinc wires was cut into a rectangle of 75 mm x 100 mm with the direction in which the copper and zinc wires extended as the short side direction, to produce an adhesive sheet with wiring (lower sheet) with 11 copper wires and 1 zinc wire.

[0060] (Formation of a strip-shaped electrolyte layer and a coating containing metal salt) The following composition A was applied onto a release film (product name: SP-382150 (manufactured by Lintec Corporation)) so that coated areas (5 mm) and uncoated areas (3 mm) were alternately arranged, forming a strip-shaped electrolyte layer with a thickness of 20 μm. A release film ("SP-PET381130" manufactured by Lintec Corporation) was attached to the formed strip-shaped electrolyte layer. At this time, the strip-shaped electrolyte layer was cut into a rectangle of 75 mm x 83 mm with the extension direction as the short side direction. Thereafter, ultraviolet light with a wavelength of 365 nm was applied at an illuminance of 130 mW / cm. 2 , Light amount: 540mJ / cm 2 A sheet with composition A was prepared by irradiating under the above conditions. Composition A A hydrogel containing 100 parts by mass of monomer aqueous solution ("SMU-4005" manufactured by Yusiro Chemical Industry Co., Ltd.), 0.24 parts by mass of photopolymerization initiator ("PKU-8001" manufactured by Yusiro Chemical Industry Co., Ltd.), 138 parts by mass of anti-drying liquid ("SW-9002" manufactured by Yusiro Chemical Industry Co., Ltd.), and 1.4 parts by mass of sodium chloride (manufactured by Kanto Chemical Co., Ltd.). Next, the following composition B was applied onto another release film ("SP-382150" manufactured by Lintec Corporation) to form a metal salt-containing resin having a thickness of 20 μm. A release film ("SP-PET381130" manufactured by Lintec Corporation) was attached to the formed metal salt-containing resin. At this time, it was cut into a rectangle of 75 mm × 10 mm. ·Composition B A water-soluble thermoplastic resin made by blending 100 parts by mass of polyethylene oxide (manufactured by Meisei Chemical Industry Co., Ltd., product name "Alcox EP1010N") with 17 parts by mass of copper sulfate pentahydrate (manufactured by Kanto Chemical Co., Ltd.). Next, the release film (manufactured by Lintec Corporation, product name "SP-PET381130") of the sheet with composition A was peeled off, and the sheet was attached to the lower sheet. At this time, the sheet with composition A was attached at a position 3 mm away from the end of the side where the copper wire was installed of the lower sheet. Then, the release film (manufactured by Lintec Corporation, "SP-PET381130") was peeled off. Furthermore, the release film (manufactured by Lintec Corporation, product name "SP-PET381130") of the sheet with composition B was peeled off, and composition B was attached to the end of the lower sheet on the side where the zinc wire was installed. Thereafter, the release film (manufactured by Lintec Corporation, "SP-PET382150") was peeled off. In this manner, a coating containing a strip-shaped electrolyte and a metal salt was formed on the lower sheet.

[0061] (Preparation of adhesive sheet with wiring (upper sheet)) As the first wiring, a zinc wire (diameter 150 μm, "Zinc Wire" manufactured by Japan Fine Steel Co., Ltd.) was prepared. Next, the adhesive sheet was wound around a drum member whose outer circumferential surface was made of rubber so as not to wrinkle. Both ends of the adhesive sheet in the circumferential direction were fixed with double-sided tape. The zinc wire wound around the bobbin was attached to the surface of the adhesive layer located near the end of the drum member, and the zinc wire was wound around the drum member while being unwound, and the drum member was moved little by little in a direction parallel to the drum axis so that the zinc wire was wound around the drum member while drawing a spiral at equal intervals. At this time, the drum member was rotated while vibrating in the drum axis direction so that the wound zinc wire drew a wave shape. In this way, 10 zinc wires were installed on the surface of the adhesive sheet. In addition, the amplitude of the wave shape was 2 mm, and the wavelength was 8 mm. The adhesive sheet with the zinc wires was then cut parallel to the drum axis. The adhesive sheet with the zinc wires was cut into a rectangle of 75 mm x 86 mm with the direction in which the zinc wires extended as the short side direction, to produce an adhesive sheet with wiring (upper sheet) with 10 zinc wires installed.

[0062] (Sensor creation) The upper sheet was attached to the lower sheet on which the strip-shaped electrolyte layer and the coating containing metal salt were formed. At this time, the copper wire on the lower sheet and the zinc wire on the upper sheet were adjacent to each other with a 1 mm interval, and the composition B was attached so as to be exposed, thereby obtaining a sensor.

[0063] [Comparative Example 1] As the first wiring, a zinc wire (diameter 150 μm, "Lead Wire" manufactured by Japan Fine Steel Co., Ltd.) was prepared, and the zinc wire wound around a bobbin was attached to the surface of the adhesive layer so that the end copper wires on the lower sheet prepared in Example 1 were spaced 5 mm apart. Then, the zinc wire was wound around the drum member while being unwound, and the drum member was gradually moved in a direction parallel to the drum axis so that the zinc wire was wound around the drum member while drawing a spiral at equal intervals. At this time, the drum member was rotated while being vibrated in the drum axis direction so that the wound zinc wire drew a wave shape. In this way, 10 zinc wires were placed on the surface of the lower sheet prepared in Example 1. In addition, the amplitude of the wave shape was 2 mm, and the wavelength was 8 mm. Then, the adhesive sheet on which the copper wire and zinc wire were placed was cut parallel to the drum axis. The adhesive sheet with the copper wire and zinc wire attached was cut into a rectangle of 75 mm x 100 mm, with the direction in which the copper wire and zinc wire extended as the short side direction, and a sensor was produced in which 11 copper wires and 11 zinc wires were attached, but composition A (strip-shaped electrolyte layer), composition B, and the coating in Example 1 were omitted.

[0064] [Comparative Example 2] The release film (manufactured by Lintec Corporation, product name "SP-PET381130") of the sheet with composition B produced in Example 1 was peeled off from the sensor obtained in Comparative Example 1, and composition B was attached to the end of the sensor on the side where the zinc wire was installed. Thereafter, the release film (manufactured by Lintec Corporation, "SP-PET382150") was peeled off. In this manner, a coating containing a metal salt was formed on the sensor in Example 1 from which composition A (strip-shaped electrolyte layer) and the coating were omitted.

[0065] [Voltage Rating] The sensor was immersed in saline (0.9% NaCl) and the voltage was measured for 60 seconds using a tester, and the average voltage was taken as the voltage value. The results are shown in Table 1.

[0066] [Table 1] [Explanation of symbols]

[0067] 11...first wiring, 12...second wiring, 2...electrolyte layer, 3...wiring fixing material, 4...coating, 5...sensing module, 51...first electrode, 52...second electrode, 6...wireless transmitting module, 7...wireless relay station, 8...sensing server, 100...sensor.

Claims

1. The device comprises two or more pairs of wirings each including a first wiring including a conductive linear body and a second wiring including a conductive linear body and made of a material having an ionization tendency different from that of the first wiring, a wiring fixing material for fixing the pair of wirings, and a water-impermeable covering material for covering at least one of the pair of wirings, The conductive linear body has a diameter of 5 μm or more and 300 μm or less, The wire fixing material has elasticity, The covering has elasticity, one of the pair of wires is not covered with the coating, an electrolyte layer is provided between the first wiring and the second wiring, except for the pair of wirings that are not covered with the coating; The pair of wirings are electrically connected in series. Sensor.

2. 2. The sensor according to claim 1, The conductive linear body has a diameter of 10 μm or more and 100 μm or less. Sensor.

3. The sensor according to claim 1 or 2, The thickness of the electrolyte layer is 2 μm or more and 1 cm or less. Sensor.

4. The sensor according to any one of claims 1 to 3, The conductive linear body has a wave shape in a plan view of the sensor. Sensor.

5. The sensor according to any one of claims 1 to 4, the wiring fixing material is a pressure-sensitive adhesive sheet having a pressure-sensitive adhesive layer, the pressure-sensitive adhesive layer being formed from a pressure-sensitive adhesive composition containing a pressure-sensitive adhesive resin, The coating is a synthetic resin film. Sensor.

6. The sensor according to any one of claims 1 to 5, a coating containing a metal salt is provided on the pair of wirings that is not covered with the coating; Sensor.

7. The sensor according to any one of claims 1 to 6, The combination of materials of the first wiring and the second wiring is any one of a combination of copper and zinc, a combination of copper and aluminum, a combination of aluminum and carbon, a combination of titanium and carbon, a combination of titanium and copper, a combination of zinc and carbon, a combination of zinc and silver, and a combination of zinc and gold. Sensor.

8. A sensor according to any one of claims 1 to 7; a sensing module for sensing a potential difference between the wirings; A wireless transmission module for transmitting a wireless signal. Sensing device.

Citation Information

Patent Citations

  • Sealing sheet, liquid discharge head using the same and ink jet device

    JP2013068420A

  • Liquid leakage detection device

    JP2014190722A

  • Electromotive module and clothing article

    JP2015229003A

  • Cable and liquid detection member for cable

    JP2017072454A

  • Detection system, detector and detection method

    JP2020139856A