Stator core, rotating electric machine, and method for designing stator core

By adjusting tooth widths in stator cores based on magnetic properties, the design addresses flux density variations and iron loss in rotating electrical machines, improving efficiency.

JP7588600B2Active Publication Date: 2024-11-22NIPPON STEEL CORPORATION
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021556185
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-11-15
Filing Date
2020-11-13
Publication Date
2024-11-22
Estimated Expiration
2040-11-13

AI Technical Summary

Technical Problem

Existing stator cores in rotating electrical machines exhibit variations in magnetic flux density due to anisotropic magnetic properties of electromagnetic steel sheets, leading to increased iron loss.

Method used

The stator core design involves adjusting the width of teeth along directions with superior and inferior magnetic properties to ensure that the product of tooth width and magnetic flux density remains approximately constant for each tooth, using specific chemical compositions and angles relative to the rolling direction.

Benefits of technology

This approach reduces variations in magnetic flux density and suppresses iron loss, enhancing the efficiency of rotating electrical machines.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007588600000005
    Figure 0007588600000005
  • Figure 0007588600000006
    Figure 0007588600000006
  • Figure 0007588600000007
    Figure 0007588600000007
Patent Text Reader

Abstract

This stator core has a plurality of laminated electromagnetic steel sheets. Among a plurality of teeth (121a-121p) of the stator core, the width of teeth arranged along the direction in which magnetic characteristics are superior is narrower than the width of teeth arranged along the direction in which magnetic characteristics are inferior.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a stator core, a rotating electric machine, and a method for designing a stator core, and is particularly suitable for use in a stator core having a plurality of laminated electromagnetic steel sheets. This application claims priority based on Japanese Patent Application No. 2019-206649, filed on November 15, 2019, the contents of which are incorporated herein by reference. [Background technology]

[0002] Electromagnetic steel sheets are mainly used as the stator core (iron core) of rotating electrical machines. Electromagnetic steel sheets are broadly divided into oriented electromagnetic steel sheets and non-oriented electromagnetic steel sheets. The magnetic properties of electromagnetic steel sheets generally have anisotropy within the sheet surface. In particular, oriented electromagnetic steel sheets have large anisotropy in their magnetic properties, and the magnetic properties in the rolling direction are extremely better than in other directions. On the other hand, even non-oriented electromagnetic steel sheets have anisotropy in their magnetic properties, although it is smaller than that of oriented electromagnetic steel sheets. When a stator core is constructed by stacking electromagnetic steel sheets with such anisotropic magnetic properties, there are parts with good magnetic properties and parts with bad magnetic properties, and the distribution of the magnetic properties of the stator core varies. Specifically, the magnetic flux density in the stator core varies, resulting in large iron loss.

[0003] Patent Document 1 discloses a rotating electric machine technology in which the path dimension of the magnetic flux between the groove bottom and the outer periphery of the stator core (i.e., the radial length of the yoke of the stator core) is made smaller in areas with good magnetic properties and made larger in areas with poor magnetic properties. In the rotating electric machine technology disclosed in Patent Document 1, the cross-sectional area of ​​the yoke of the stator core is made different depending on the magnetic properties, so that for the same magnetic flux, the magnetic flux density becomes lower in areas with poorer magnetic properties. Patent Document 2 discloses a three-pole core technology in which the surface area of ​​the magnetic pole teeth in the direction along the rolling direction or the direction perpendicular to the rolling direction is narrower than the surface area of ​​the other magnetic pole teeth. The three-pole core disclosed in Patent Document 2 is inexpensive and can eliminate the imbalance of magnetic flux by making the surface area of ​​the magnetic pole teeth in the direction along the rolling direction or the direction perpendicular to the rolling direction narrower than the surface area of ​​the other magnetic pole teeth. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Publication No. 59-10142 [Patent Document 2] Japanese Patent Application Publication No. 8-214476 Summary of the Invention [Problem to be solved by the invention]

[0005] However, in the technology disclosed in Patent Document 1, the magnetic flux flows from the teeth into the yoke while bending, so it is not easy to specify which part in the circumferential direction of the yoke should have a larger or smaller passage dimension. In other words, with the technology in Patent Document 1, it is difficult to determine the shape of the stator core, and there is a risk that the variation in magnetic flux density cannot be reduced. In addition, the technology disclosed in Patent Document 2 is premised on the premise that magnetic flux in the direction along the rolling direction or the direction perpendicular to the rolling direction passes more easily than magnetic flux in other directions, but there are cases in which magnetic flux in the direction along the rolling direction or the direction perpendicular to the rolling direction does not pass easily. In other words, even if the shape of the three-pole core is determined based on the rolling direction as in the technology of Patent Document 2, there is a risk that it will not be possible to reduce the variation in magnetic flux density.

[0006] The present invention has been made in consideration of the above problems, and has an object to reduce the variation in magnetic flux density and suppress iron loss. [Means for solving the problem]

[0007] In order to solve the above problems, the present invention employs the following configuration. (1) A stator core according to one aspect of the present invention is a stator core having a plurality of laminated electromagnetic steel sheets, and among a plurality of teeth of the stator core, a width of the teeth along a direction having superior magnetic properties is narrower than a width of the teeth along a direction having inferior magnetic properties. The stator core is formed by laminating rolled electromagnetic steel sheets, and the electromagnetic steel sheets contain, by mass%, C: 0.0100% or less, Si: 1.50% to 4.00%, sol.Al: 0.0001% to 1.0%, S: 0.0100% or less, N: 0.0100% or less, and one or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, and Au: a total of 2. 50% to 5.00%, Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%, and one or more selected from the group consisting of Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd: 0.0000% to 0.0100% in total, and the Mn content (mass%) is [Mn], and the Ni content is The alloy has a chemical composition that satisfies the following formula (1) when the B50 content (mass%) is [Ni], the Co content (mass%) is [Co], the Pt content (mass%) is [Pt], the Pb content (mass%) is [Pb], the Cu content (mass%) is [Cu], the Au content (mass%) is [Au], the Si content (mass%) is [Si], and the sol.Al content (mass%) is [sol.Al], with the balance consisting of Fe and impurities, and satisfies the following formulas (2) and (3) when the B50 value in the rolling direction is B50L, the B50 value in the direction tilted at 45° from the rolling direction is B50D1, the B50 value in the direction tilted at 90° from the rolling direction is B50C, and the B50 value in the direction tilted at 135° from the rolling direction is B50D2, <011> The X-ray random intensity ratio is 5 or more and less than 30, the plate thickness is 0.50 mm or less, the direction in which the magnetic properties are superior is a direction at an angle of 45° from the rolling direction, and the directions in which the magnetic properties are inferior are directions at angles of 0° and 90° from the rolling direction, and the width of the teeth along the direction at an angle of 45° from the rolling direction is narrower than both the width of the teeth along the direction at an angle of 0° from the rolling direction and the width of the teeth along the direction at an angle of 90° from the rolling direction. ([Mn]+[Ni]+[Co]+[Pt]+[Pb]+[Cu]+[Au])-([Si]+[sol.Al])>0% ···(1) (B50D1+B50D2) / 2>1.7T ···(2) (B50D1+B50D2) / 2>1.1×(B50L+B50C) / 2...(3) (2) A stator core according to one aspect of the present invention is a stator core having a plurality of laminated electromagnetic steel sheets, wherein among a plurality of teeth of the stator core, a width of the teeth along a direction having superior magnetic properties is narrower than a width of the teeth along a direction having inferior magnetic properties, and the stator core is formed by laminating rolled electromagnetic steel sheets, and the electromagnetic steel sheets contain, by mass%, C: 0.0100% or less and Si: 1.50% to 4.00%. , sol.Al: 0.0001% to 1.0%, S: 0.0100% or less, N: 0.0100% or less, one or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, and Au: 2.50% to 5.00% in total, Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%, and Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd. One or more selected from the group consisting of: a total content of 0.0000% to 0.0100%, a Mn content (mass%) of [Mn], a Ni content (mass%) of [Ni], a Co content (mass%) of [Co], a Pt content (mass%) of [Pt], a Pb content (mass%) of [Pb], a Cu content (mass%) of [Cu], a Au content (mass%) of [Au], a Si content (mass%) of [Si], a sol.Al content (mass%) of [sol and has a chemical composition consisting of the balance Fe and impurities, and satisfies the following formula (1) when the B50 value in the rolling direction is B50L, the B50 value in the direction tilted at 45° from the rolling direction is B50D1, the B50 value in the direction tilted at 90° from the rolling direction is B50C, and the B50 value in the direction tilted at 135° from the rolling direction is B50D2, and satisfies the following formulas (4) and (5), <011> The X-ray random intensity ratio is 5 or more and less than 30, the plate thickness is 0.50 mm or less, the direction in which the magnetic properties are superior is a direction at an angle of 45° from the rolling direction, and the directions in which the magnetic properties are inferior are directions at angles of 0° and 90° from the rolling direction, and the width of the teeth along the direction at an angle of 45° from the rolling direction is narrower than both the width of the teeth along the direction at an angle of 0° from the rolling direction and the width of the teeth along the direction at an angle of 90° from the rolling direction. ([Mn]+[Ni]+[Co]+[Pt]+[Pb]+[Cu]+[Au])-([Si]+[sol.Al])>0% ···(1) (B50D1+B50D2) / 2>1.8T ···(4) (B50D1+B50D2) / 2>(B50L+B50C) / 2···(5). ( 3 )(1) above or (2 In the stator core described in the above, the product of the width of the teeth of the stator core and the magnetic flux density of the teeth when excited with a predetermined magnetic field strength may be approximately constant for each tooth. ( 4 )the above( 1 The stator core according to any one of claims 1 to 3, The following formula (6) may be satisfied. (B50D1+B50D2) / 2>1.2×(B50L+B50C) / 2...(6) ( 5 )the above( 1 In the stator core according to any one of claims 1 to 4, The electrical steel sheet may contain, by mass %, 0.020% to 0.400% of the Sn or 0.020% to 0.400% of the Sb. ( 6 A rotating electric machine according to one aspect of the present invention comprises the above items (1) to ( 5 The stator core according to any one of claims 1 to 4 is provided. ( 7 ) A method for designing a stator core according to one aspect of the present invention is a method for designing a stator core having laminated electromagnetic steel sheets, the method including: a teeth magnetic flux density acquisition process for acquiring information on the magnetic flux density of the teeth when excited with a predetermined magnetic field strength; a determining step of determining a width of the teeth of the stator core such that a product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquiring step is substantially constant for each tooth; the step of acquiring operation data of a rotating electric machine having the stator core when the rotating electric machine is operated; the step of identifying a ratio of operation time for each of a plurality of operation conditions based on the operation data acquired by the step of acquiring operation data; the step of acquiring information on an average magnetic flux density of the teeth corresponding to each of the plurality of operation conditions; and the step of calculating an average magnetic field strength of the teeth for each of the plurality of operation conditions from the information on the average magnetic flux density of the teeth corresponding to each of the plurality of operation conditions acquired by the step of acquiring the average magnetic flux density, In the density acquisition step, information on the magnetic flux density of the teeth for each of the plurality of operating conditions when excited with the average magnetic field strength of the teeth for each of the plurality of operating conditions calculated in the average magnetic field strength calculation step is acquired, and in the determination step, a width of the teeth is calculated for each of the plurality of operating conditions so that the product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquisition step is approximately constant for each tooth, and the calculated width of the teeth for each of the plurality of operating conditions is weighted based on the ratio of the operating time specified in the specification step to determine the weighted width of the teeth. . (8) A method for designing a stator core according to one aspect of the present invention is a method for designing a stator core having laminated electromagnetic steel sheets, the method including: acquiring information on the magnetic flux density of the teeth when excited with a predetermined magnetic field strength; a determining step of determining a width of the teeth of the stator core such that a product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquiring step is substantially constant for each tooth; an operating data acquiring step of acquiring operating data of the rotating electric machine having the stator core when the rotating electric machine is operated; a specifying step of specifying a ratio of operating time for each of a plurality of operating conditions based on the operating data acquired in the operating data acquiring step; an average magnetic flux density acquiring step of acquiring information on an average magnetic flux density of the teeth corresponding to each of the plurality of operating conditions; The method includes an evaluated magnetic flux density calculation process for calculating an evaluated magnetic flux density of the teeth weighted based on the ratio of operating times specified in the specification process from information on the average magnetic flux density of the teeth corresponding to each of the multiple operating conditions acquired in the average magnetic flux density acquisition process, and an average magnetic field strength calculation process for calculating an average magnetic field strength of the teeth from the evaluated magnetic flux density of the teeth calculated in the evaluated magnetic flux density calculation process, wherein the teeth magnetic flux density acquisition process acquires information on the magnetic flux density of the teeth when excited with the average magnetic field strength of the teeth calculated in the average magnetic field strength calculation process. ( 9 )the above( 7 ) or ( 8 In the method for designing a stator core described in the above, the operation data acquisition step may acquire at least any one of planned data and actual data of a rotating electric machine including the stator core. Effect of the Invention

[0008] According to the above aspect of the present invention, it is possible to reduce the variation in magnetic flux density and suppress iron loss. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a diagram illustrating an example of a configuration of a rotating electric machine. [Diagram 2] 1 is a graph showing the relationship between the angle from the rolling direction and the magnetic properties. [Diagram 3] FIG. 4 is a diagram for explaining the width of the teeth. [Figure 4] FIG. 2 is a diagram illustrating an example of a configuration of a motor. [Diagram 5] FIG. 4 is a diagram showing angles of 0° to 90° from the rolling direction of the stator core. [Figure 6] 11 is a table showing the relationship between the torque ratio and the average magnetic flux density of the teeth. [Figure 7] 1 is a table showing the relationship between the torque ratio and the magnetic flux density of the teeth for each angle from the rolling direction (material A). [Figure 8] 1 is a table showing the relationship between the torque ratio and the optimum width of the teeth for each angle from the rolling direction (material A). [Figure 9]1 is a table showing iron loss ratios of comparative examples and invention examples (material A). [Figure 10] 4 is a table showing an example of operation data. [Figure 11] This is a table showing the width of teeth weighted based on the ratio of operating time for each angle from the rolling direction (Material A). [Figure 12] 13 is a table showing the relationship between the torque ratio and the magnetic flux density of the teeth for each angle from the rolling direction (material B). [Figure 13] 13 is a table showing the relationship between the torque ratio and the optimum width of the teeth for each angle from the rolling direction (material B). [Figure 14] 1 is a table showing iron loss ratios of comparative examples and invention examples (material B). [Figure 15] This is a table showing the width of teeth weighted based on the ratio of operating time for each angle from the rolling direction (Material B). [Figure 16] FIG. 2 is a diagram illustrating an example of a configuration of a motor. [Figure 17] FIG. 4 is a diagram showing angles of 0° to 90° from the rolling direction of the stator core. [Figure 18] 11 is a table showing the relationship between the torque ratio and the average magnetic flux density of the teeth. [Figure 19] 1 is a table showing the relationship between the torque ratio and the magnetic flux density of the teeth for each angle from the rolling direction (material A). [Figure 20] 1 is a table showing the relationship between the torque ratio and the optimum width of the teeth for each angle from the rolling direction (material A). [Figure 21] 1 is a table showing iron loss ratios of comparative examples and invention examples (material A). [Figure 22] This is a table showing the width of teeth weighted based on the ratio of operating time for each angle from the rolling direction (Material A). [Figure 23] 13 is a table showing the relationship between the torque ratio and the magnetic flux density of the teeth for each angle from the rolling direction (material B). [Figure 24] 13 is a table showing the relationship between the torque ratio and the optimum width of the teeth for each angle from the rolling direction (material B). [Diagram 25]1 is a table showing iron loss ratios of comparative examples and invention examples (material B). [Figure 26] This is a table showing the width of teeth weighted based on the ratio of operating time for each angle from the rolling direction (Material B). [Figure 27] FIG. 2 is a diagram illustrating an example of a functional configuration of a design device for a stator core. [Figure 28] 4 is a flowchart illustrating an example of a process of a stator core design device. [Figure 29] 4 is a flowchart illustrating an example of a process of a stator core design device. [Diagram 30] 4 is a flowchart illustrating an example of a process of a stator core design device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Note that the XYZ coordinates shown in each drawing indicate the relationship of the directions in each drawing, and the origin of the XYZ coordinates is not limited to the position shown in each drawing. In addition, in the following description, the same length, shape, direction, size, interval, and other physical quantities are not limited to being completely the same, and also include cases where they are different within the range where the function of the target part is not impaired.

[0011] <Configuration of rotating electric machine> Fig. 1 is a diagram showing an example of the configuration of a rotating electric machine 100. Specifically, Fig. 1 is a diagram showing a cross section of the rotating electric machine 100 cut perpendicularly to its axis O. In the following description, the circumferential direction (direction around the axis O of the rotating electric machine 100), radial direction (direction extending radially from the axis O of the rotating electric machine 100), and height direction (direction parallel to the axis O (Z-axis direction)) of the rotating electric machine 100 will be abbreviated as the circumferential direction, radial direction, and height direction, respectively, as necessary. Furthermore, the axis O of the rotating electric machine 100 will be abbreviated as the axis O, as necessary.

[0012] In FIG. 1, a rotating electric machine 100 includes a rotor 110 and a stator 120 . The rotor 110 is attached to the rotating shaft 130 (axis O) directly or via a member so as to be coaxial with the rotating shaft 130. The rotor 110 has, for example, a rotor core (iron core), a permanent magnet, and a rotating shaft (shaft). The rotor 110 can be realized by known technology, and therefore detailed description thereof will be omitted here.

[0013] The stator 120 is disposed outside the rotor 110 so as to be coaxial with the rotating shaft 130 (axis O). The stator 120 has a stator core and a coil. For convenience of notation, the coil is not shown in FIG. 1. The stator core has a plurality of teeth 121a-121p and a yoke 122. The yoke 122 has a generally hollow cylindrical shape. The teeth 121a-121p extend radially from the inner peripheral surface of the yoke 122 toward the axis O. The teeth 121a-121p are disposed at equal intervals in the circumferential direction. The teeth 121a-121p and the yoke 122 are integral. That is, there is no boundary line between the teeth and the yoke. Furthermore, there is no boundary line that exists in the yoke in the case of a so-called split core.

[0014] The rotor 110 and the stator 120 are positioned so that the tip surfaces of the teeth 121a-121p face the outer circumferential surface of the rotor core of the rotor 110 with a gap (air gap) therebetween. A coil (winding) is arranged for each of the teeth 121a-121p while being electrically insulated from the teeth 121a-121p. The coil may be wound in a distributed or concentrated manner. A rotating magnetic field is generated by passing an excitation current through the coil of the stator 120, and the rotor 110 rotates due to the rotating magnetic field.

[0015] Here, an example will be described in which the rotating electric machine 100 is an inner rotor type motor (electric motor). Applications of the motor include, for example, electric vehicles, hybrid electric vehicles, and compressors, but the applications of the motor are not particularly limited.

[0016] In the present embodiment, the stator core is formed using a non-oriented electromagnetic steel sheet as an example of an electromagnetic steel sheet. For example, the non-oriented electromagnetic steel sheet conforms to the "non-oriented electromagnetic steel strip" defined in JIS C 2552 (2014). The stator core is constructed by stacking and fixing a plurality of non-oriented electromagnetic steel sheets having the same shape and size as the non-oriented electromagnetic steel sheets cut to match the overall planar shape of the stator core (the shape shown in FIG. 1). The stator core is fixed, for example, by crimping. The method of cutting out the non-oriented electromagnetic steel sheets is not particularly limited. For example, the non-oriented electromagnetic steel sheets can be cut out by punching with a die, wire electric discharge machining, or the like.

[0017] In Fig. 1, for the convenience of the description that will be given later, angles are expressed in two types. The angles (0°, 22.5°, 45°, 67.5°, 90°) shown without parentheses in Fig. 1 indicate angles that are 90° or less between the rolling direction of the non-oriented electrical steel sheet and the radial direction of the teeth 121a to 121p when the rolling direction of the non-oriented electrical steel sheet is used as the reference. The angles shown in parentheses in Fig. 1 (0°, 22.5°, 45°, 67.5°, 90°, 112.5°, 135°, 157.5°, 180°, 202.5°, 225°, 247.5°, 270°, 292.5°, 315°, 337.5°, 360°) indicate angles expressed with the positive direction of the X-axis among the rolling directions of the non-oriented electrical steel sheet as the reference (0°), and with the counterclockwise direction as viewed into the paper of Fig. 1 as the positive direction. Thus, in Fig. 1, angles shown without parentheses and angles shown with parentheses thereafter are expressed in different ways but have the same meaning.

[0018] Here, the radial direction of the teeth 121a-121p is a virtual line that passes through the circumferential center of the teeth 121a-121p and the axis O, and is parallel to the extension direction of a virtual line (a straight line shown by a dashed line in FIG. 1) that is parallel to a plane (XY plane) perpendicular to the axis O (axis of the stator core). FIG. 1 shows an example in which the rolling direction of a non-oriented electrical steel sheet is the X-axis direction. In the following description, the angle between the rolling direction of the non-oriented electrical steel sheet and the radial direction of the teeth 121a-121p when the rolling direction of the non-oriented electrical steel sheet is used as a reference will be referred to as the angle from the rolling direction as necessary. Note that in the following description, for convenience of explanation, the angle from the rolling direction will be described as an angle defined as the angle shown without parentheses in Fig. 1 in some cases and as an angle shown with parentheses in other cases. However, as described above, the angle shown without parentheses and the angle shown with parentheses thereafter are different notations and have the same meaning.

[0019] In this embodiment, the multiple non-oriented electrical steel sheets cut out as described above are laminated with the same angle from the rolling direction. That is, among the regions of the multiple non-oriented electrical steel sheets cut out as described above, the regions belonging to the same tooth have the same angle from the rolling direction (when expressed as an angle defined as the angle shown without parentheses in FIG. 1).

[0020] In this embodiment, we will explain the case where a stator core is constructed using two types of non-oriented electromagnetic steel sheets, a first non-oriented electromagnetic steel sheet (referred to as material A) and a second non-oriented electromagnetic steel sheet (referred to as material B), whose magnetic properties differ depending on the angle from the rolling direction. Material A is a steel sheet with relatively small anisotropy and with the best magnetic properties at an angle of 0° from the rolling direction. Material B is a steel sheet with relatively large anisotropy and with the best magnetic properties at an angle of 45° from the rolling direction.

[0021] Figure 2 is a graph showing the relationship between the angle from the rolling direction and the magnetic properties of each of Material A and Material B. One example of the magnetic property is the magnitude of magnetic flux density, which in this case is the magnitude of magnetic flux density (B50) when excited with a magnetic field strength of 5000 [A / m]. Graph 201 shows the normalized magnetic flux density B50 of material A, and graph 502 shows the normalized magnetic flux density B50 of material B. The normalized magnetic flux density B50 in graphs 201 and 202 is shown as a ratio when the average B50 for each angle from the rolling direction in material A is standardized to 1.000. Also, in Fig. 2, for convenience of notation, the notation of the angle from the rolling direction is the same as the angle shown in parentheses in Fig. 1.

[0022] The magnetic flux density of the material A is the highest at an angle of 0° from the rolling direction, and the magnetic flux density increases at intervals of 90° from the angle of 0°. The magnetic flux density is also low near an angle of 45° from the rolling direction, and the magnetic flux density decreases at intervals of 90° from the angle of 45°. That is, the magnetic properties of the material A are excellent at angles of 0°, 90°, 180°, and 270° from the rolling direction, and the magnetic properties are inferior at angles of 45°, 135°, 225°, and 315° from the rolling direction. Hereinafter, the magnetic properties of the material A are represented by angles of 45°, 135°, 225°, and 315° from the rolling direction. The magnetic flux density of the material A in the range of angles of 0° to 90° and the magnetic flux density in the range of angles of 90° to 180° are approximately symmetrical with respect to the angle of 90°. Furthermore, for material A, the magnetic flux density in the angle range of 0° to 180° and the magnetic flux density in the angle range of 180° to 360° are substantially symmetrical with respect to the angle of 180°. On the other hand, the magnetic flux density of the material B is the highest at an angle of 45° from the rolling direction, and the magnetic flux density increases at intervals of 90° from the angle of 45°. The magnetic flux density is also low near an angle of 0° from the rolling direction, and the magnetic flux density decreases at intervals of 90° from the angle of 0°. That is, the directions in which the magnetic properties of the material B are excellent are at angles of 45°, 135°, 225°, and 315° from the rolling direction, and the directions in which the magnetic properties are poor are near angles of 0°, 90°, 180°, and 270° from the rolling direction. Hereinafter, the angles of 0°, 90°, 180°, and 270° from the rolling direction are described as representative values ​​of the directions in which the magnetic properties of the material B are poor. In addition, the magnetic flux density of the material B in the range of angles from 0° to 90° and the magnetic flux density in the range of angles from 90° to 180° are approximately symmetrical with respect to the angle of 90°. Furthermore, for material B, the magnetic flux density in the angle range of 0° to 180° and the magnetic flux density in the angle range of 180° to 360° are substantially symmetrical with respect to the angle of 180°.

[0023] As shown in Fig. 2, when a stator core is made of material A or material B, whose magnetic flux density varies depending on the angle from the rolling direction, the radial direction of each tooth of the stator core is at a different angle from the rolling direction, so that the magnetic flux density of each tooth is different when a certain magnetic field strength is excited. This causes variation in the magnetic flux density in the stator core, resulting in large iron loss. If a rotating electric machine is made using such a stator core, the efficiency of the rotating electric machine will decrease.

[0024] The inventors came up with the idea that the width of each tooth can be adjusted to reduce the variation in magnetic flux density in the stator core. Specifically, the inventors came up with the idea that the width of the teeth along the direction with superior magnetic properties should be narrower than the width of the teeth along the direction with inferior magnetic properties, or the width of the teeth along the direction with inferior magnetic properties should be wider than the width of the teeth along the direction with superior magnetic properties. Furthermore, the inventors came up with the idea that the variation in magnetic flux density can be further reduced by determining the width of the teeth so that the product of "teeth width" and "magnetic flux density of teeth" is approximately constant for each tooth.

[0025] When a stator core is constructed based on the above-described idea, the width of the teeth 121a to 121p shown in FIG. 1 along the direction having superior magnetic properties is narrower than the width of the teeth along the direction having inferior magnetic properties. Specifically, when the stator core shown in FIG. 1 is constructed using material A, the direction in which the magnetic properties are excellent in material A is a direction at an angle of 0° from the rolling direction. Here, in material A, the direction in which the magnetic properties are excellent in material A is a direction at an angle of 0° from the rolling direction, in addition to the angle of 0°, and also the directions at angles of 90°, 180°, and 270° from the rolling direction. Also, in material A, the direction in which the magnetic properties are poor is a direction at an angle of 45° from the rolling direction. Here, in material A, the direction in which the magnetic properties are poor is a direction at an angle of 45° from the rolling direction, in addition to the angle of 45°, and also the directions at angles of 135°, 225°, and 315° from the rolling direction. That is, in material A, the angles of 0°, 90°, 180°, and 270° from the rolling direction are the directions in which the magnetic properties are excellent, and the angles of 45°, 135°, 225°, and 315° are the directions in which the magnetic properties are poor. Therefore, by making the width of each of the teeth 121a, 121e, 121i, and 121m narrower than the width of each of the teeth 121c, 121g, 121k, and 121o, it is possible to reduce variations in magnetic flux density within the stator core. On the other hand, when the stator core shown in FIG. 1 is constructed using material B, the direction in which the magnetic properties are excellent in material B is a direction at an angle of 45° from the rolling direction. Here, in material B, the direction in which the magnetic properties are excellent at an angle of 45° from the rolling direction refers to the directions at angles of 135°, 225°, and 315° from the rolling direction in addition to the angle of 45°. Also, in material B, the direction in which the magnetic properties are poor is a direction at an angle of 0° and 90° from the rolling direction. Here, in material B, the direction in which the magnetic properties are poor is a direction at an angle of 0° and 90° from the rolling direction refers to the directions at angles of 180° and 270° from the rolling direction in addition to the angles of 0° and 90°. That is, in material B, the angles of 45°, 135°, 225°, and 315° from the rolling direction are the directions in which the magnetic properties are excellent, and the angles of 0°, 90°, 180°, and 270° are the directions in which the magnetic properties are poor. Therefore, by making the width of each of the teeth 121c, 121g, 121k, and 121o narrower than the width of each of the teeth 121a, 121e, 121i, and 121m, it is possible to reduce variations in the magnetic flux density within the stator core.

[0026] Here, the width of the teeth will be described with reference to Fig. 3. Fig. 3 is a diagram for explaining the width of the teeth. Fig. 3(a) is an example of teeth that are parallel along the radial direction. In this example, the teeth themselves are parallel along the radial direction. Fig. 3(b) is an example of teeth in which the slots are parallel along the radial direction. In this example, the slots located between circumferentially adjacent teeth are parallel along the radial direction. In this embodiment, the width of the teeth is the length of the stator core in the circumferential direction at the center of the straight line area of ​​the teeth. The straight line area of ​​the teeth is the area of ​​the longest straight line among the straight lines constituting the ends of the teeth in the circumferential direction of the stator core in a cross section of the stator core cut in a direction perpendicular to the axis of the stator core, which is determined for each of the two ends of the teeth in the circumferential direction of the stator core. In the example shown in Fig. 3(a), the straight line connecting positions 311 and 312 and the straight line connecting positions 313 and 314 form the teeth straight line region. In the example shown in Fig. 3(a), the center positions of the teeth straight line region are positions 321 and 322. Therefore, the width of the teeth shown in Fig. 3(a) is the distance TW between positions 321 and 322. In the example shown in Fig. 3(b), the straight line connecting positions 315 and 316 and the straight line connecting positions 317 and 318 form the teeth straight line region. In the example shown in Fig. 3(b), the center positions of the teeth straight line region are positions 323 and 324. Therefore, the width of the teeth shown in Fig. 3(b) is the distance TW between positions 323 and 324.

[0027] FIG. 3(a) shows an example of teeth that are parallel along the radial direction, so the width of the teeth is constant regardless of the radial position in the straight line region of the teeth. On the other hand, in FIG. 3(b), since the slot is an example of a tooth that is parallel along the radial direction, the actual width of the tooth varies depending on the radial location in the straight tooth region, and therefore the width of the tooth is taken as a representative value to be the distance TW between the above-mentioned positions 323 and 324.

[0028] <Example of tooth width determination (slots parallel to the radial direction (material A))> Next, when designing a stator core for an embedded permanent magnet synchronous motor using electromagnetic steel sheet as material A, an example of determining the width of the teeth so that the above-mentioned "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth will be described. In the example of an embedded permanent magnet synchronous motor shown here, the slots of the teeth of the stator core are parallel along the radial direction as shown in Figure 3(b). 4 is a diagram showing an example of the configuration of a motor 400 before the width of the teeth is determined, i.e., when the width of each tooth is constant over the entire circumference. Fig. 4 shows a cross section of the motor 400 taken perpendicular to its axis O. In FIG. 4, motor 400 is an interior permanent magnet synchronous motor (IPMSM) and has a rotor 410 and a stator 420. The rotor 410 is attached to the rotating shaft 430 (axis O) so as to be coaxial with the rotating shaft 430. The rotor 410 has a plurality of permanent magnets 411. The permanent magnets 411 are embedded in a rotor core 415. As shown in FIG. 4, the motor 400 has eight poles. The outer diameter of the rotor 410 is 133 mm. Stator 420 has stator core 421 and coil 422. Stator 420 has an outer diameter of 207 mm, and an inner diameter of 135 mm. Stator core 421 has 48 slots. Coil 422 has a distributed winding.

[0029] Fig. 5 is an enlarged view of a portion of stator core 421 in Fig. 4 that is at an angle of 0° to 90° from the rolling direction. Here, among teeth 501a to 501m of stator core 421, tooth 501a is positioned at an angle of 0° from the rolling direction, and half of the tooth width is omitted in the drawing. Also, among teeth 501a to 501m, tooth 501m is positioned at an angle of 90° from the rolling direction, and half of the tooth width is omitted in the drawing. Also, each tooth has a slot that is parallel to the radial direction, as shown in Fig. 3(b). As shown in Fig. 5, the width TW1 of the base of the tooth is 6.56 mm, and the width TW2 of the tip is 5.16 mm. Therefore, the width of the tooth (TW shown in Fig. 3(b)) is 5.86 mm, calculated by (6.56 mm + 5.16 mm) ÷ 2.

[0030] FIG. 6 shows the results of an analysis of the relationship between the operating conditions (torque ratio) and the average magnetic flux density of the teeth when motor 400 rotates at 3,000 rpm and the width of the teeth is constant all around stator core 421. FIG. 6 shows the torque ratio [%], which is the operating condition of the motor 400, and the average magnetic flux density B [T peak]. Here, the torque ratio indicates the torque ratio under each operating condition, with the maximum torque being 100%. For example, a torque ratio of 20% means operation at a torque value [Nm] of maximum torque [Nm] x 0.2. The average magnetic flux density of the teeth is the average of the maximum magnetic flux density values ​​at each location on the 48 teeth. In other words, [T peak The peak in [ indicates the peak magnetic flux density when the magnetic flux density changes over time. In Fig. 6, the average magnetic flux density of the teeth increases as the torque ratio increases. The relationship between the torque ratio and the average magnetic flux density of the teeth shown in Fig. 6 can be derived by performing electromagnetic field analysis (numerical analysis) based on Maxwell's equations, or by measuring the induced voltage using a search coil in the core of the manufactured motor and integrating the induced voltage. When calculating from electromagnetic field analysis (numerical analysis), the average magnetic flux density is calculated by calculating the maximum magnetic flux density for each element (all meshes) included in the teeth part (all 48 teeth in this example) using the finite element method, and averaging them taking into account the area of ​​each element. When measuring using a search coil, the average magnetic flux density is calculated by integrating the induced voltage measured for each search coil to obtain the time waveform of the magnetic flux density, and then calculating the maximum magnetic flux density, and averaging them taking into account the cross-sectional area of ​​the core surrounded by each search coil.

[0031] The average magnetic field strength H [A / m] of the teeth is calculated from the average magnetic flux density of the teeth shown in Figure 6. The average magnetic field strength of the teeth can be calculated based on the relative permeability of material A. Here, the average magnetic field strength of the teeth is calculated for each torque ratio (i.e., for each average magnetic flux density of the teeth shown in Figure 6). Next, the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth is calculated based on the material properties of material A. Therefore, the magnetic flux density of the teeth for each angle from the rolling direction is calculated for each torque ratio (i.e., for each average magnetic flux density of the teeth shown in Figure 6).

[0032] 7 is a table showing the relationship between the torque ratio [%] and the magnetic flux density B [T] of the teeth for each angle from the rolling direction. Here, angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction are set as representative values, and the three teeth centered on the representative angle have the same magnetic flux density. The teeth at an angle of 0° from the rolling direction are teeth 501a and 501b included in the 0° range (A1) shown in Fig. 5. The teeth at an angle of 22.5° from the rolling direction are teeth 501c-501e included in the 22.5° range shown in Fig. 5. The teeth at an angle of 45° from the rolling direction are teeth 501f-501h included in the 45° range (A3) shown in Fig. 5. The teeth at an angle of 67.5° from the rolling direction are teeth 501i-501k included in the 67.5° range (A4) shown in Fig. 5. The teeth at an angle of 90° from the rolling direction are teeth 501l and 501m included in the 90° range (A5) shown in Fig. 5.

[0033] As shown in FIG. 7, when the torque ratio is 20[%], 40[%], 60[%], and 80[%], the magnetic flux density of the teeth varies depending on the angle from the rolling direction. Also, when the torque ratio is 40[%], 60[%], and 80[%], the magnetic flux density of the teeth at angles of 0° and 90° from the rolling direction is large, and the magnetic flux density of the teeth at an angle of 45° from the rolling direction is small. This tendency is consistent with the tendency shown in graph 201 of material A in FIG. 2, where the B50 ratio is large at angles of 0° and 90° from the rolling direction, and the B50 ratio is small at an angle of 45° from the rolling direction. On the other hand, as shown in FIG. 7, when the torque ratio is 100[%], the magnetic flux density of the teeth is constant regardless of the angle from the rolling direction due to magnetic saturation. The relationship between the torque ratio shown in FIG. 7 and the magnetic flux density of the teeth for each angle from the rolling direction can be derived from the BH characteristics of material A at each angle from the rolling direction.

[0034] Next, to reduce the variation in magnetic flux density of the teeth, the optimum teeth width is determined for each angle from the rolling direction. Specifically, based on the magnetic flux density of the teeth for each angle from the rolling direction shown in Fig. 7, the teeth width is determined so that "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth. Here, the teeth width is determined for each torque ratio. For example, in the case of a torque ratio of 60% in FIG. 7, the magnetic flux density of the teeth is 1.65[T] at an angle of 0° from the rolling direction, 1.61[T] at an angle of 22.5°, 1.55[T] at an angle of 45°, 1.56[T] at an angle of 67.5°, and 1.59[T] at an angle of 90°. Therefore, the width of the teeth is determined so that "teeth width" x "teeth magnetic flux density" is approximately constant regardless of the angle of 0°, 22.5°, 45°, 67.5°, or 90°. The width of the teeth determined in this way is called the optimal width.

[0035] FIG. 8 is a table showing the relationship between the torque ratio [%] and the optimum width [mm] of the teeth determined for each angle from the rolling direction. For example, in the case of a torque ratio of 60% in Fig. 8, the optimum width of the teeth is 5.64mm at an angle of 0° from the rolling direction, 5.76mm at an angle of 22.5°, 5.99mm at an angle of 45°, 5.96mm at an angle of 67.5°, and 5.85mm at an angle of 90°. Here, the product of the "magnetic flux density of the teeth" at a torque ratio of 60% in Fig. 7 multiplied by the "optimum width of the teeth" at a torque ratio of 60% in Fig. 8 for each angle from the rolling direction is always 9.3, which is approximately constant.

[0036] The optimum width of the teeth thus determined is applied to the width of the teeth according to the angle from the rolling direction to design the stator core. For example, in FIG. 8, in the case of a torque ratio of 60%, the width of teeth 501a, 501b included in the 0° range (A1) shown in FIG. 5 is designed to be 5.64 [mm], the width of teeth 501c-501e included in the 22.5° range (A2) is designed to be 5.76 [mm], the width of teeth 501f-501h included in the 45° range (A3) is designed to be 5.99 [mm], the width of teeth 501i-501k included in the 67.5° range (A4) is designed to be 5.96 [mm], and the width of teeth 501l, 501m included in the 90° range (A5) is designed to be 5.85 [mm].

[0037] As explained in the graph 201 showing the relationship between the angle from the rolling direction and the magnetic properties of material A in Fig. 2, the magnetic flux density of material A in the angle range of 0° to 90° and the magnetic flux density in the angle range of 90° to 180° are substantially symmetrical with respect to the angle of 90°. Furthermore, the magnetic flux density of material A in the angle range of 0° to 180° and the magnetic flux density in the angle range of 180° to 360° are substantially symmetrical with respect to the angle of 180°. Therefore, since the magnetic flux density B [T] of the teeth for each angle from the rolling direction shown in Figure 7 is approximately the same not only in the range of 0° angle from the rolling direction (angles 348.75° to 11.25°: A1) but also in the range of 168.75° to 191.25° shown in Figure 4, the teeth within the angle range of 168.75° to 191.25° are designed to have approximately the same width as the teeth within the 0° range (A1). Similarly, the teeth within the angles 146.25° to 168.75°, 191.25° to 213.75°, and 326.25° to 348.75° shown in FIG. 4 are designed to have approximately the same width as the teeth within the 22.5° range (11.25° to 33.75°: A2). Similarly, the teeth within the angles of 123.75° to 146.25°, 213.75° to 236.25°, and 303.75° to 326.25° shown in FIG. 4 are designed to have approximately the same width as the teeth within the 45° range (angles 33.75° to 56.25°: A3). Similarly, the teeth within the angles of 101.25° to 123.75°, 236.25° to 258.75°, and 281.25° to 303.75° shown in FIG. 4 are designed to have approximately the same width as the teeth within the 67.5° range (angles 56.25° to 78.75°: A4). Similarly, the teeth within the angle range of 258.75° to 281.25° shown in FIG. 4 are designed to have approximately the same width as the teeth within the angle range of 90° (78.75° to 101.25°: A5).

[0038] In this way, in the designed stator core, the width of the teeth along the direction with superior magnetic properties is narrower than the width of the teeth along the direction with inferior magnetic properties. In the material A, the teeth along the direction with superior magnetic properties are not limited to the teeth along the 0° angle from the rolling direction and the teeth along the 90° angle from the rolling direction, but also include teeth located in the vicinity of these teeth. Specifically, in the material A, the teeth along the direction with superior magnetic properties are the teeth within the angle range of 348.75° to 11.25°, the teeth within the angle range of 168.75° to 191.25°, the teeth within the angle range of 78.75° to 101.25°, and the teeth within the angle range of 258.75° to 281.25°. In addition, in the material A, the teeth along the direction with inferior magnetic properties are not limited to the teeth along the angle of 45° from the rolling direction and the teeth along the angles of 135°, 225°, and 315° from the rolling direction, but also include teeth located in the vicinity of these teeth. Specifically, in the material A, the teeth along the direction with inferior magnetic properties are the teeth within the angle range of 33.75° to 56.25°, the teeth within the angle range of 123.75° to 146.25°, the teeth within the angle range of 213.75° to 236.25°, and the teeth within the angle range of 303.75° to 326.25°.

[0039] FIG. 9 is a table showing the relationship between the iron loss ratio [-] for each torque ratio [%] between a stator core with the teeth width designed to be the optimum width and a stator core with the teeth width constant over the entire circumference. The iron loss ratio is a value obtained by dividing the iron loss of the motor of the invention example by the iron loss of the motor of the comparative example, where a motor with a stator core with the teeth width designed to be the optimum width is taken as the invention example and a motor with a stator core with the teeth width constant over the entire circumference is taken as the comparative example. Here, the iron loss ratio is calculated for each torque ratio. The iron loss can be derived by performing an electromagnetic field analysis (numerical analysis) under the condition that the motor of the invention example and the motor of the comparative example are operated at a rotation speed of 3,000 [rpm] so as to achieve each of the torque ratios "%" described above. It can also be derived by measuring the manufactured motor.

[0040] From the iron loss ratio results shown in Figure 9, it was confirmed that iron loss could be suppressed by 0.1% to 1.3% at torque ratios of 20%, 40%, 60%, and 80%. On the other hand, at a torque ratio of 100%, as mentioned above, magnetic saturation occurred and the magnetic flux density of the teeth was constant regardless of the angle from the rolling direction, so the effect of suppressing iron loss could not be confirmed. In this way, by determining the width of the teeth so that the "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth depending on operating conditions such as the torque ratio, it was confirmed that the variation in magnetic flux density can be reduced and iron loss can be suppressed in the non-magnetic saturation region.

[0041] In addition, once the width of the teeth is determined, it is impossible to change the width of the teeth of a stator core that is actually manufactured every time the operating conditions such as the torque ratio change. Therefore, to design a stator core, for example, a stator core design device selects one of a plurality of operating conditions (a plurality of torque ratios). Under the selected operating condition, the width of the teeth is determined so that the product of "tooth width" and "magnetic flux density of teeth" is constant for each tooth, and the stator core is designed. This makes it possible to reduce the variation in the magnetic flux density of the stator core under the selected operating condition. On the other hand, when a motor equipped with the designed stator core is operated, if there is little or no time for operation under the selected operating conditions, it is not possible to actually reduce the variation in magnetic flux density and suppress iron loss. Therefore, when designing a stator core, it is necessary to determine the width of the teeth in advance so as to suppress iron loss as much as possible, taking into account the operation of the rotating electric machine. Two design methods for the stator core will be described below. The two design methods may be performed by a stator core design device (to be described later) or by the stator core designer.

[0042] [First design method for stator core] The first design method is a method in which, assuming that a rotating electric machine equipped with the stator core to be designed will be operated, the operating condition that has the highest ratio of operating time to the total operating time among multiple operating conditions is identified, and the optimal width of the teeth is determined under the identified operating condition. Fig. 10 shows an example of operating data when it is assumed that a rotating electric machine equipped with the stator core to be designed is operated. Specifically, Fig. 10 shows an example of the ratio of operating time according to the torque ratio in a motor 600 equipped with the stator core to be designed. Here, the operating time refers to the time during which the motor 600 rotates. The operating data shown in Fig. 10 is acquired in advance before the stator core is designed.

[0043] In Fig. 10, the torque ratio of 30% to 50% among the multiple operating conditions corresponds to 45% of the operating time, which is the operating condition with the highest operating time ratio. Therefore, in this case, the average magnetic flux density of the teeth corresponding to the torque ratio of 40% among the torque ratios shown in Fig. 6 is 1.44 [T peak], the average magnetic field strength H [A / m] of the teeth is calculated. In the explanation of <Example of tooth width determination (teeth with slots parallel to the radial direction (material A))> above, the magnetic flux density B [T] of the teeth for each angle from the rolling direction as shown in FIG. 7 was calculated for each torque ratio, and the optimal width of the teeth for each angle from the rolling direction as shown in FIG. 8 was determined. On the other hand, here, the magnetic flux density B [T] of the teeth for each angle from the rolling direction as shown in FIG. 7 is calculated only for the torque ratio 40 [%] with the highest operating time ratio. The optimal width of the teeth for each angle from the rolling direction as shown in FIG. 8 is determined only for the torque ratio 40 [%] with the highest operating time ratio. Therefore, the optimum width of each tooth is determined to be one each. By applying the optimum width thus determined to the width of the teeth to design the stator core, it is possible to reduce the variation in magnetic flux density and suppress iron loss under the operating conditions with the highest ratio of operating time.

[0044] [Second design method of stator core] The second design method involves identifying the ratio of operating time for each of a number of operating conditions when assuming that a rotating electric machine equipped with the stator core being designed will be in operation, and weighting the width of the teeth based on the ratio of operating time for each of the identified number of operating conditions. The second design method will also be described with reference to an example of the operating data shown in Fig. 10. Also, in the second design method, the operating data shown in Fig. 10 is obtained in advance before designing the stator core.

[0045] In the second design method, similarly to the above-mentioned <Example of tooth width determination (teeth with slots parallel to the radial direction (material A))>, the relationship between the torque ratio and the average magnetic flux density of the teeth shown in Fig. 6 is derived, and the relationship between the torque ratio and the magnetic flux density of the teeth for each angle from the rolling direction shown in Fig. 7 is derived. From this, the optimum width of the teeth for each angle from the rolling direction shown in Fig. 8 is calculated for each torque ratio. Next, the optimum width of the teeth for each angle from the rolling direction is weighted based on the ratio of the operation time corresponding to the torque ratio shown in FIG. 10. Specifically, for each angle from the rolling direction shown in FIG. 8, the optimum width of the teeth for each torque ratio is multiplied by the ratio of the operation time corresponding to the torque ratio shown in FIG. 10. Here, since there are five types of torque ratios, five values ​​are calculated by multiplying the optimum width of the teeth for each torque ratio by the ratio of the operation time corresponding to the torque ratio. Next, the five calculated values ​​are added and divided by 100 to calculate the width of the teeth weighted based on the ratio of the operation time at a given angle from the rolling direction. Similarly, the width of the teeth weighted based on the ratio of the operation time is calculated for the other angles from the rolling direction. For example, in the case of an angle of 0° from the rolling direction, the optimum teeth widths are 5.40mm, 5.57mm, 5.64mm, 5.79mm, and 5.86mm for torque ratios of 20%, 40%, 60%, 80%, and 100% in Fig. 8. By multiplying the optimum teeth widths by the operating time ratios of 20%, 45%, 20%, 10%, and 5% according to the torque ratios shown in Fig. 10, five values ​​are calculated: 108mm·%, 250.65mm·%, 112.8mm·%, 57.9mm·%, and 29.3mm·%. Adding these five values ​​together and dividing by 100% gives a teeth width of 5.58 mm weighted based on the operating time ratio at an angle of 0° from the rolling direction. Similarly, teeth widths weighted based on the operating time ratio are calculated for angles of 22.5°, 45°, 67.5°, and 90° from the rolling direction.

[0046] Fig. 11 is a table showing the teeth widths weighted based on the operating time ratio shown in Fig. 10 for each angle from the rolling direction. In Fig. 10, the operating time ratio for torque ratios of 30% to 50% is 45%, which is the highest operating time ratio. Therefore, the weighted teeth widths shown in Fig. 11 are calculated to be close to the optimal teeth width for a torque ratio of 40% shown in Fig. 8. In this way, by designing the stator core by applying teeth widths weighted based on the ratio of operating time, it is possible to reduce variations in magnetic flux density throughout the entire operating time.

[0047] Here, a motor equipped with a stator core designed with a weighted teeth width as shown in Fig. 11 is taken as an example of the invention, and a motor equipped with a stator core with a constant teeth width all around is taken as a comparative example. When each was operated at a rotation speed of 3,000 [rpm] with the operating time ratio shown in Fig. 10, the iron loss ratio was 0.993, and it was confirmed that the iron loss could be suppressed by 0.7 [%]. In this way, iron loss can be suppressed by designing a stator core by applying a teeth width weighted based on the operating time ratio and configuring a rotating electric machine.

[0048] [How to obtain driving data] In the above-mentioned [first design method of a stator core], it is necessary to specify the operating condition with the highest ratio of operating time among multiple operating conditions in a rotating electric machine including the stator core to be designed before designing the stator core. Also, in the above-mentioned [second design method of a stator core], it is necessary to specify the ratio of operating time according to the operating condition in a rotating electric machine including the stator core to be designed before designing the stator core. That is, in order to design a stator core in either the first design method or the second design method, it is necessary to obtain in advance operating data for the assumed operation of a rotating electric machine equipped with the stator core to be designed.

[0049] Here, the operational data is broadly divided into two types: planned data and actual data. The planned data is data in which the operation of a rotating electric machine is determined in advance and the operation time according to the operating conditions is planned. For example, a rotating electric machine used in a specific production facility often continues a certain operation or repeats a certain operation. For such a rotating electric machine, the planned data can be acquired in advance. By acquiring the planned data, it is possible to identify information on the operating conditions with the highest ratio of operation time and to identify the ratio of operation time according to the operating conditions.

[0050] On the other hand, the actual data is data in which the same type of rotating electric machine is already in operation and the operating time corresponding to the operating conditions is accumulated as an actual result. For example, the rotating electric machine used in an HEV (Hybrid Electric Vehicle) or an EV (Electric Vehicle) cannot acquire planned data because the operating time corresponding to the operating conditions varies depending on the user (driver). In such a case, the actual data can be acquired in advance by collecting a huge amount of data on the actual operation of the vehicle and analyzing the collected big data. For example, the data may be acquired by analyzing the operating time corresponding to the operating conditions of the rotating electric machine when the vehicle is driven in the JC08 mode, which is a fuel consumption measurement standard in Japan. By acquiring the actual data, it is possible to identify information on the operating conditions with the highest ratio of operating time, or to identify the ratio of operating time corresponding to the operating conditions.

[0051] In this way, by obtaining operating data through planned data or actual data, it is possible to identify the operating condition with the highest operating time ratio among multiple operating conditions, or to identify the operating time ratio according to the operating condition, before designing the stator core.

[0052] <Example of tooth width determination (slots parallel to the radial direction (material B))> Next, an example of determining the width of the teeth so that the above-mentioned "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth when designing a stator core of an embedded permanent magnet synchronous motor using electromagnetic steel sheet as material B will be described. Note that the same content as in the above-mentioned <Example of determining the width of the teeth (teeth with slots parallel along the radial direction (material A))> will be omitted as appropriate. Here, the results of an analysis of the relationship between the operating conditions (torque ratio) and the average magnetic flux density of the teeth when the rotation speed of motor 400 shown in Figure 4 is 3,000 rpm and the width of the teeth is constant around the entire circumference of stator core 421 are the same as those shown in Figure 6. The average magnetic field strength H [A / m] of the teeth is calculated from the average magnetic flux density of the teeth shown in Figure 6. Next, the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth is calculated based on the material properties of material B.

[0053] FIG. 12 is a table showing the relationship between the torque ratio [%] and the magnetic flux density B [T] of the teeth for each angle from the rolling direction. As shown in FIG. 12, when the torque ratio is 20[%], 40[%], 60[%], and 80[%], the magnetic flux density of the teeth varies depending on the angle from the rolling direction. Also, when the torque ratio is 20[%], 40[%], 60[%], and 80[%], the magnetic flux density of the teeth at an angle of 45° from the rolling direction is large, and the magnetic flux density of the teeth at angles of 0° and 90° from the rolling direction is small. This tendency is consistent with the tendency shown in graph 202 of material B in FIG. 2, where the B50 ratio is large at an angle of 45° from the rolling direction, and the B50 ratio is small at angles of 0° and 90° from the rolling direction. On the other hand, as shown in FIG. 12, when the torque ratio is 100[%], the magnetic flux density of the teeth is constant regardless of the angle from the rolling direction due to magnetic saturation. Next, based on the magnetic flux density of the teeth for each angle from the rolling direction shown in FIG. 12, the width of the teeth is determined so that "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth.

[0054] 13 is a table showing the relationship between the torque ratio [%] and the optimum teeth width [mm] determined for each angle from the rolling direction. The determined optimum teeth width is applied to the teeth width according to the angle from the rolling direction to design the stator core. In this way, in the designed stator core, the width of the teeth along the direction with superior magnetic properties is narrower than the width of the teeth along the direction with inferior magnetic properties. In the material B, the teeth along the direction with superior magnetic properties are not limited to the teeth along the 45° angle from the rolling direction and the teeth along the 135°, 225°, and 315° angle from the rolling direction, but also include teeth located near these teeth. Specifically, in the material B, the teeth along the direction with inferior magnetic properties are the teeth within the angle range of 33.75° to 56.25°, the teeth within the angle range of 123.75° to 146.25°, the teeth within the angle range of 213.75° to 236.25°, and the teeth within the angle range of 303.75° to 326.25°. In addition, in material B, the teeth along the direction with poor magnetic properties are not limited to the teeth along the angles of 0° and 90° from the rolling direction, but also include teeth located in the vicinity of these teeth. Specifically, in material B, the teeth along the direction with excellent magnetic properties are the teeth within the angle range of 348.75° to 11.25°, the teeth within the angle range of 168.75° to 191.25°, the teeth within the angle range of 78.75° to 101.25°, and the teeth within the angle range of 258.75° to 281.25°.

[0055] FIG. 14 is a table showing the relationship between the iron loss ratio [-] for each torque ratio [%] between a stator core designed with the teeth width at an optimum width and a stator core with the teeth width constant all around. From the results of the iron loss ratio shown in Figure 14, it was confirmed that iron loss could be suppressed by 0.6% to 6.4% at torque ratios of 20%, 40%, 60%, and 80%. On the other hand, at a torque ratio of 100%, magnetic saturation occurred and the magnetic flux density of the teeth was constant regardless of the angle from the rolling direction, so the effect of suppressing iron loss could not be confirmed. In this way, by determining the width of the teeth so that the "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth depending on operating conditions such as the torque ratio, it was confirmed that the variation in magnetic flux density can be reduced and iron loss can be suppressed in the non-magnetic saturation region.

[0056] Next, similarly to the above-mentioned [Second stator core design method], the optimum width of the teeth for each angle from the rolling direction is weighted based on the ratio of the operation time according to the torque ratio shown in FIG. FIG. 15 is a table showing the width of teeth weighted based on the ratio of the operation times shown in FIG. 10 for each angle from the rolling direction. Here, a motor equipped with a stator core designed with weighted teeth width as shown in Fig. 15 was taken as an example of the invention, and a motor equipped with a stator core with teeth width that is constant all around was taken as a comparative example. When both were operated at a rotation speed of 3,000 [rpm] with the operating time ratio shown in Fig. 10, the iron loss ratio was 0.958, and it was confirmed that iron loss could be suppressed by 4.2 [%].

[0057] <Example of tooth width determination (parallel teeth along the radial direction (material A))> Next, when designing a stator core for an induction motor using electromagnetic steel sheet as material A, an example of determining the width of the teeth so that the above-mentioned "tooth width" x "magnetic flux density of teeth" is approximately constant for each tooth will be described. Note that the same content as the above-mentioned <Example of determining the width of teeth (teeth with slots parallel along the radial direction (material A))> will be omitted as appropriate. In the induction motor, the teeth of the stator core are parallel along the radial direction as shown in FIG. 3(a). Fig. 16 is a diagram showing an example of the configuration of a motor 1600 before the width of the teeth is determined, i.e., in which the width of each tooth is constant over the entire circumference. Fig. 16 shows a cross section of the motor 1600 taken perpendicular to its axis O. In FIG. 16, a motor 1600 is an induction motor, and has a rotor 1610 and a stator 1620. The rotor 1610 is attached to the rotating shaft 1630 (axis O) so as to be coaxial with the rotating shaft 1630. The rotor 1610 has a plurality of coils. As shown in Fig. 16, the number of poles of the motor 1600 is four. The outer diameter of the rotor 1610 is 134 mm. Stator 1620 has stator core 1621 and coil 1622. Stator 1620 has an outer diameter of 220 mm, and an inner diameter of 136 mm. Stator core 1621 has 60 slots. Coil 1622 has a distributed winding.

[0058] Fig. 17 is an enlarged view of the stator core 1621 in Fig. 16, which is at an angle of 0° to 90° from the rolling direction. Here, among the teeth 1701a to 1701p of the stator core 1621, the tooth 1701a is positioned at an angle of 0° from the rolling direction, and half of the tooth width is omitted. Among the teeth 1701a to 1701p, the tooth 1701p is positioned at an angle of 90° from the rolling direction, and half of the tooth width is omitted. Also, each tooth is parallel to the radial direction as shown in Fig. 3(a). The width of each tooth is 4 mm.

[0059] FIG. 18 shows the results of an analysis of the relationship between the operating conditions (torque ratio) and the average magnetic flux density of the teeth when the rotation speed of motor 1600 is 3,000 rpm and the width of the teeth is constant all around stator core 1621. FIG. 18 shows the torque ratio [%], which is the operating condition of the motor 1600, and the average magnetic flux density B [T peak ] is a diagram showing the relationship between The average magnetic field strength H [A / m] of the teeth is calculated from the average magnetic flux density of the teeth shown in Figure 18. Next, the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth is calculated based on the material properties of material A.

[0060] FIG. 19 is a table showing the relationship between the torque ratio [%] and the magnetic flux density B [T] of the teeth for each angle from the rolling direction. As shown in FIG. 19, when the torque ratio is 20[%], 40[%], 60[%], and 80[%], the magnetic flux density of the teeth varies for each angle from the rolling direction. Also, when the torque ratio is 40[%], 60[%], and 80[%], the magnetic flux density of the teeth at angles of 0° and 90° from the rolling direction is large, and the magnetic flux density of the teeth at an angle of 45° from the rolling direction is small. This tendency is consistent with the tendency shown in the graph 201 of the material A in FIG. 2 that the B50 ratio is large at angles of 0° and 90° from the rolling direction, and the B50 ratio is small at an angle of 45° from the rolling direction. On the other hand, as shown in FIG. 19, when the torque ratio is 100[%], the magnetic flux density of the teeth is approximately constant regardless of the angle from the rolling direction due to magnetic saturation. Next, based on the magnetic flux density of the teeth for each angle from the rolling direction shown in FIG. 19, the width of the teeth is determined so that "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth.

[0061] FIG. 20 is a table showing the relationship between the torque ratio [%] and the optimum width [mm] of the teeth determined for each angle from the rolling direction. For example, in the case of a torque ratio of 60% in Fig. 20, the optimum width of the teeth is 3.85mm at an angle of 0° from the rolling direction, 3.96mm at an angle of 22.5°, 4.08mm at an angle of 45°, 4.06mm at an angle of 67.5°, and 3.96mm at an angle of 90°. Here, the product of the "magnetic flux density of the teeth" for a torque ratio of 60% in Fig. 19 multiplied by the "optimum width of the teeth" for a torque ratio of 60% in Fig. 20 for each angle from the rolling direction is always 6.7, which is approximately constant.

[0062] The optimum width of the teeth thus determined is applied to the width of the teeth according to the angle from the rolling direction to design the stator core. For example, in FIG. 20, in the case of a torque ratio of 60%, the width of teeth 1701a to 1701b included in the 0° range (A1) shown in FIG. 17 is designed to be 3.85 mm, the width of teeth 1701c to 1701f included in the 22.5° range (A2) is designed to be 3.96 mm, the width of teeth 1701g to 1701j included in the 45° range (A3) is designed to be 4.08 mm, the width of teeth 1701k to 1701n included in the 67.5° range (A4) is designed to be 4.06 mm, and the width of teeth 1701o to 1701p included in the 90° range (A5) is designed to be 3.96 mm.

[0063] In addition, the magnetic flux density B [T] of the teeth for each angle from the rolling direction shown in Figure 19 is approximately the same not only in the range of 0° angle from the rolling direction (angles 11.25° to 33.75°: A1) but also in the range of 168.75° to 191.25° shown in Figure 16, so the teeth included in the angle range of 168.75° to 191.25° are designed to have approximately the same width as the teeth included in the 0° range (A1). Similarly, the teeth within the angles 146.25° to 168.75°, 191.25° to 213.75°, and 326.25° to 348.75° shown in FIG. 16 are designed to have approximately the same width as the teeth within the 22.5° range (A2). Similarly, the teeth within the angles of 123.75° to 146.25°, 213.75° to 236.25°, and 303.75° to 326.25° shown in FIG. 16 are designed to have approximately the same width as the teeth within the 45° range (angles 33.75° to 56.25°: A3). Similarly, the teeth within the angles of 101.25° to 123.75°, 236.25° to 258.75°, and 281.25° to 303.75° shown in FIG. 16 are designed to have approximately the same width as the teeth within the 67.5° range (angles 56.25° to 78.75°: A4). Similarly, the teeth within the angle range of 258.75° to 281.25° shown in FIG. 16 are designed to have approximately the same width as the teeth within the angle range of 90° (78.75° to 101.25°: A5). Although the tooth 1701c located between the 0° range (A1) and the 22.5° range (A2) is set to the 22.5° range, it may be set to the 0° range. Furthermore, the tooth 1701n located on the boundary between the 67.5° range (A4) and the 90° range (A5) is set to the 67.5° range, but it may be set to the 90° range.

[0064] FIG. 21 is a table showing the relationship, for each torque ratio [%], of the iron loss ratio [-] between a stator core designed with the teeth width at an optimum width and a stator core with the teeth width kept constant all around. From the results of the iron loss ratio shown in Fig. 21, it was confirmed that the iron loss could be suppressed by 0.1% to 1.4% at torque ratios of 20[%], 40[%], 60[%], and 80[%]. On the other hand, at a torque ratio of 100[%], magnetic saturation occurred and the magnetic flux density of the teeth was approximately constant regardless of the angle from the rolling direction, so the effect of suppressing iron loss could not be confirmed.

[0065] Next, similarly to the above-mentioned [Second stator core design method], the optimum width of the teeth for each angle from the rolling direction is weighted based on the ratio of the operation time according to the torque ratio shown in FIG. FIG. 22 is a table showing the width of teeth weighted based on the ratio of the operation times shown in FIG. 10 for each angle from the rolling direction. Here, a motor equipped with a stator core designed with weighted teeth width as shown in Fig. 22 was taken as an example of the invention, and a motor equipped with a stator core with teeth width that is constant all around was taken as a comparative example. When both were operated at a rotation speed of 3,000 [rpm] with the operating time ratio shown in Fig. 10, the iron loss ratio was 0.995, and it was confirmed that iron loss could be suppressed by 0.5 [%].

[0066] <Example of tooth width determination (parallel teeth along the radial direction (material B))> Next, an example of determining the width of the teeth so that the above-mentioned "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth when designing a stator core of an induction motor using electromagnetic steel sheet as material B will be described. Note that the same content as in the above-mentioned <Example of determining the width of the teeth (radial parallel teeth (material A))> will be omitted as appropriate. Here, when the rotation speed of motor 1600 shown in FIG. 16 is 3,000 rpm and the width of the teeth is constant around the entire circumference of stator core 1621, the results of an analysis of the relationship between the operating conditions (torque ratio) and the average magnetic flux density of the teeth are the same as those shown in FIG. 18. The average magnetic field strength H [A / m] of the teeth is calculated from the average magnetic flux density of the teeth shown in Figure 18. Next, the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth is calculated based on the material properties of material B.

[0067] FIG. 23 is a table showing the relationship between the torque ratio [%] and the magnetic flux density B [T] of the teeth for each angle from the rolling direction. As shown in Fig. 23, regardless of the torque ratio, there is variation in the magnetic flux density of the teeth for each angle from the rolling direction. Moreover, regardless of the torque ratio, the magnetic flux density of the teeth at an angle of 45° from the rolling direction is large, and the magnetic flux density of the teeth at angles of 0° and 90° from the rolling direction is small. This tendency matches the tendency shown in graph 202 of material B in Fig. 2, where the B50 ratio is large at an angle of 45° from the rolling direction, and the B50 ratio is small at angles of 0° and 90° from the rolling direction. Next, based on the magnetic flux density of the teeth for each angle from the rolling direction shown in FIG. 23, the width of the teeth is determined so that "tooth width" x "magnetic flux density of the teeth" is approximately constant for each tooth.

[0068] FIG. 24 is a table showing the relationship between the torque ratio [%] and the optimum width [mm] of the teeth determined for each angle from the rolling direction. FIG. 25 is a table showing the relationship, for each torque ratio [%], of the iron loss ratio [-] between a stator core designed with the teeth width at an optimum width and a stator core with the teeth width kept constant all around. From the results of the iron loss ratio shown in Fig. 25, it was confirmed that the iron loss could be suppressed by 1.1% to 5.6% at torque ratios of 20[%], 40[%], 60[%], and 80[%]. On the other hand, at a torque ratio of 100[%], magnetic saturation occurred and the magnetic flux density of the teeth was approximately constant regardless of the angle from the rolling direction, so the effect of suppressing iron loss could not be confirmed. In this way, by determining the width of each tooth so that the "tooth width" x "magnetic flux density of the tooth" is approximately constant for each tooth depending on operating conditions such as the torque ratio, it was confirmed that the variation in magnetic flux density can be reduced and iron loss can be suppressed in the non-magnetic saturation region.

[0069] Next, similarly to the above-mentioned [Second stator core design method], the optimum width of the teeth for each angle from the rolling direction is weighted based on the ratio of the operation time according to the torque ratio shown in FIG. FIG. 26 is a table showing the width of teeth weighted based on the ratio of the operation times shown in FIG. 10 for each angle from the rolling direction. Here, a motor equipped with a stator core designed with weighted teeth width as shown in Fig. 26 was taken as an example of the invention, and a motor equipped with a stator core with teeth width that is constant all around was taken as a comparative example. When both were operated at a rotation speed of 3,000 [rpm] with the operating time ratio shown in Fig. 10, the iron loss ratio was 0.972, and it was confirmed that iron loss could be suppressed by 2.8 [%].

[0070] <Stator core design device> Next, a description will be given of a case where the above-mentioned [First stator core design method] and [Second stator core design method] are implemented using a stator core design device 2700. The hardware of the stator core design device 2700 is realized by using, for example, an information processing device having a CPU, a ROM, a RAM, an HDD, and various hardware, or dedicated hardware.

[0071] FIG. 27 is a diagram showing an example of a mechanical configuration of a stator core design device 2700. The stator core design device 2700 has an operating data acquisition unit 2701, an operating condition / operating ratio identification unit 2702, an average magnetic flux density acquisition unit 2703, an evaluated magnetic flux density calculation unit 2704, an average magnetic field strength calculation unit 2705, a teeth magnetic flux density acquisition unit 2706, a teeth width determination unit 2707, and a stator core design unit 2708.

[0072] Fig. 28 is a flowchart showing an example of processing of a stator core design device 2700. The flowchart in Fig. 28 shows an example of implementing the above-mentioned "first stator core design method" by the stator core design device 2700. Note that descriptions similar to those described above will be omitted as appropriate. In S101, the operation data acquisition unit 2701 acquires operation data of a rotating electric machine when the rotating electric machine including the stator core to be designed is operated. That is, the operation data acquisition unit 2701 acquires operation data when it is assumed that the rotating electric machine including the stator core to be designed is operated. As described above, the operation data includes plan data and actual data. The operation data acquisition unit 2701 acquires plan data in the case of a rotating electric machine whose operation is predetermined, and acquires actual data in the case of a rotating electric machine of the same type that has already been operated and accumulated as actual data. Note that the operation data acquisition unit 2710 is not limited to acquiring either the plan data or the actual data, and may acquire at least either the plan data or the actual data. By the process of S101, for example, the operation data shown in FIG. 10 is acquired.

[0073] In S102, the operating condition / operating ratio identifying unit 2702 identifies an operating condition with the highest operating time ratio among the multiple operating conditions based on the operating data acquired in S101. Through the process of S102, for example, a torque ratio of 30[%] to 50[%], that is, a torque ratio of 40[%], is identified as the operating condition with the highest operating time ratio based on the operating data shown in Fig. 10.

[0074] In S103, the average magnetic flux density acquiring unit 2703 acquires information on the average magnetic flux density of the teeth corresponding to the operating conditions specified in S102. Specifically, when the operating conditions specified in S102 are those in which the width of the teeth is constant over the entire circumference of the stator core, the average magnetic flux density acquiring unit 2703 acquires the average magnetic flux density of the teeth by performing an electromagnetic field analysis (numerical analysis) based on Maxwell's equations or by measuring an induced voltage using a search coil and integrating the induced voltage. By the process of S103, for example, as shown in the relationship between the torque ratio and the average magnetic flux density of the teeth in FIG. 6, the average magnetic flux density of the teeth corresponding to a torque ratio of 40% which is the operating condition with the highest ratio of operating time is 1.44 [T peak ] is obtained.

[0075] In S104, the average magnetic field strength calculation unit 2705 calculates the average magnetic field strength of the teeth from the information on the average magnetic flux density of the teeth acquired in S103. The average magnetic field strength of the teeth can be calculated based on the relative magnetic permeability of the electromagnetic steel sheet.

[0076] In S105, the teeth magnetic flux density acquisition unit 2706 acquires information on the magnetic flux density of the teeth when excited with the average magnetic field strength of the teeth calculated in S 104. Specifically, the teeth magnetic flux density acquisition unit 2706 acquires the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth based on the material properties, more specifically, the BH properties for each angle from the rolling direction of the electromagnetic steel sheet. By processing S105, for example, at a torque ratio of 40%, which is the operating condition with the highest operating time ratio shown in Figure 7, magnetic flux densities of the teeth are obtained as 1.51 [T], 1.47 [T], 1.42 [T], 1.42 [T], and 1.44 [T] at angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction, respectively.

[0077] In S106, the teeth width determination unit 2707 determines the teeth width so that the product of the "teeth width" and the "magnetic flux density of the teeth" obtained in S105 is approximately constant for each tooth. The teeth width determined in this way is the optimal teeth width. By processing S106, for example, as shown in FIG. 8, when the torque ratio is 40%, which is the operating condition with the highest operating time ratio, the optimal teeth widths are determined to be 5.57 mm, 5.72 mm, 5.95 mm, 5.93 mm, and 5.85 mm at angles from the rolling direction of 0°, 22.5°, 45°, 67.5°, and 90°, respectively.

[0078] In S107, the stator core design unit 2708 applies the determined optimum width of the teeth to the width of the teeth according to the angle from the rolling direction, thereby designing the stator core. By the process of S107, for example, the starter core is designed by applying the optimal widths of the teeth at angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction to the widths of the teeth included in the 0° range (two A1), 22.5° range (four A2), 45° range (four A3), 67.5° range (four A4), and 90° range (two A5) shown in Figure 4.

[0079] In this way, by designing a stator core using stator core design device 2700, it is possible to reduce variations in magnetic flux density and suppress iron loss under operating conditions with the highest ratio of operating time. In the above description, the operating condition with the highest ratio of operating time among the multiple operating conditions is specified in S102, information on the average magnetic flux density of the teeth corresponding to the specified operating condition is obtained in S103, and the average magnetic field strength of the teeth is calculated from the information on the average magnetic flux density of the teeth in S104. However, this is not limited to the above. For example, the processes from S101 to S104 may be omitted, and the operator of the stator core design device 2700 may input a predetermined magnetic field strength, so that the teeth magnetic flux density acquisition unit 2706 of the stator core design device 2700 may acquire information on the average magnetic field strength of the teeth. In this case, in S105, the teeth magnetic flux density acquisition unit 2706 may acquire information on the average magnetic field strength of the teeth that has been input, and acquire the magnetic flux density of the teeth from the acquired information on the average magnetic field strength of the teeth.

[0080] Fig. 29 is a flowchart showing an example of processing of a stator core design device 2700. The flowchart in Fig. 29 shows an example of implementing the above-mentioned "second stator core design method" by the stator core design device 2700. Note that explanations of processing similar to that in the flowchart in Fig. 28 will be omitted as appropriate.

[0081] In S201, the operation data acquisition unit 2701 acquires operation data of a rotating electric machine when the rotating electric machine including the stator core to be designed is operated. This process is similar to the process of S101. By the process of S201, for example, the operation data shown in FIG. 10 is acquired. In S202, the operating condition / operating ratio identifying unit 2702 identifies the ratio of the operating time for each of the multiple operating conditions based on the operating data acquired in S101. Through the process of S202, for example, the ratio of the operating time according to the torque ratio is identified based on the operating data shown in FIG.

[0082] In S203, the average magnetic flux density acquiring unit 2703 acquires information on the average magnetic flux density of the teeth corresponding to each of a plurality of operating conditions. Specifically, when the width of the teeth is constant around the entire circumference of the stator core for each of a plurality of operating conditions, the average magnetic flux density acquiring unit 2703 acquires the average magnetic flux density of the teeth for each of a plurality of operating conditions by performing an electromagnetic field analysis (numerical analysis) based on Maxwell's equations, or by measuring the induced voltage using a search coil and integrating the induced voltage. By the process of S203, the average magnetic flux density of the teeth is acquired for each torque ratio, for example, like the relationship between the torque ratio and the average magnetic flux density of the teeth shown in FIG.

[0083] In S204, the average magnetic field strength calculation unit 2705 calculates the average magnetic field strength of the teeth for each of the multiple operating conditions from the information on the average magnetic flux density of the teeth corresponding to each of the multiple operating conditions acquired in S203. The average magnetic field strength of the teeth can be calculated based on the relative permeability of the electromagnetic steel sheet.

[0084] In S205, the teeth magnetic flux density acquisition unit 2706 acquires information on the magnetic flux density of the teeth for each of the multiple operating conditions when excited with the average magnetic field strength of the teeth for each of the multiple operating conditions calculated in S204. Specifically, the teeth magnetic flux density acquisition unit 2706 acquires the magnetic flux density B [T] of the teeth for each angle from the rolling direction when excited with the average magnetic field strength of the teeth for each of the multiple operating conditions based on the material properties, more specifically, the BH properties for each angle from the rolling direction of the electromagnetic steel sheet. By the process of S205, for example, as shown in FIG. 7, the magnetic flux density of the teeth is acquired at angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction for each torque ratio.

[0085] In S206, the teeth width determination unit 2707 calculates the teeth width for each of a plurality of operating conditions so that the product of the "teeth width" and the "magnetic flux density of the teeth" obtained in S205 is approximately constant for each tooth. The teeth width calculated in this manner is the optimal teeth width. By the process of S206, for example, as shown in FIG. 8, the optimum width of the teeth is calculated for each torque ratio at angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction.

[0086] In S207, the teeth width determination unit 2707 weights the optimal teeth width for each of the multiple operating conditions calculated in S206 based on the ratio of the operating time for each of the multiple operating conditions identified in S202, and determines the weighted teeth width. By the process of S207, for example, as shown in FIG. 11, the width of the teeth weighted based on the ratio of the operation time is determined.

[0087] In S208, the stator core design unit 2708 applies the weighted teeth width to the teeth width according to the angle from the rolling direction to design the stator core. By processing S208, for example, the starter core is designed by applying the weighted tooth widths at angles of 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction to the tooth widths included in the 0° range (two A1), 22.5° range (four A2), 45° range (four A3), 67.5° range (four A4), and 90° range (two A5) shown in Figure 4. In this way, by designing a stator core using stator core design device 2700, it is possible to reduce variations in magnetic flux density throughout the entire operating time, and to suppress iron loss.

[0088] In the flowchart of FIG. 29, in S207, the optimum width of the teeth for each of the plurality of operating conditions is weighted based on the ratio of the operating time for each of the plurality of operating conditions. However, the present invention is not limited to this case. Fig. 30 is a flowchart showing an example of processing of a stator core design device 2700. The flowchart in Fig. 30 shows an example of a method different from the above-mentioned [second stator core design method] realized by the stator core design device 2700. Note that the same processing as in the flowcharts in Fig. 28 and Fig. 29 will not be described as appropriate.

[0089] In S301, the operation data acquisition unit 2701 acquires operation data of a rotating electric machine when the rotating electric machine including the stator core to be designed is operated. This process is similar to the processes of S101 and S201. By the process of S301, for example, the operation data shown in FIG. 10 is acquired. In S302, the operating condition / operating ratio identifying unit 2702 identifies the ratio of the operating time for each of the multiple operating conditions based on the operating data acquired in S301. This process is similar to the process of S202.

[0090] In S303, the average magnetic flux density acquisition unit 2703 acquires information on the average magnetic flux density of the teeth corresponding to each of a plurality of operating conditions. This process is the same as S203. By the process of S303, the average magnetic flux density of the teeth is acquired for each torque ratio, for example, like the relationship between the torque ratio and the average magnetic flux density of the teeth shown in FIG.

[0091] In S304, the evaluated magnetic flux density calculation unit 2704 calculates an evaluated magnetic flux density of the teeth weighted based on the ratio of the operation time specified in S302 from the information on the average magnetic flux density of the teeth corresponding to each of the multiple operation conditions acquired in S303. The evaluated magnetic flux density is the magnetic flux density of the teeth weighted based on the ratio of the operation time. Specifically, the evaluated magnetic flux density calculation unit 2704 multiplies the average magnetic flux density of the teeth by the ratio of the operation time for each torque ratio, adds up the multiplied values, and divides by 100 to calculate the evaluated magnetic flux density. For example, in the case where the relationship between the torque ratio and the average magnetic flux density of the teeth is as shown in FIG. 6 and the operating data is as shown in FIG. 10, the process of S304 calculates the evaluated magnetic flux density Bv[T peak ] is (1.22[T peak ]×20[%]+1.44[T peak ]×45[%]+1.59[T peak ]×20[%]+1.82[T peak ]×10[%]+2.04[T peak It is calculated by dividing ([%] × 5[%]) by 100.

[0092] In S305, the average magnetic field strength calculation unit 2705 calculates the average magnetic field strength of the teeth from the evaluated magnetic flux density of the teeth calculated in S304. The average magnetic field strength of the teeth can be calculated based on the relative permeability of the electromagnetic steel sheet. In S306, the teeth magnetic flux density acquisition unit 2706 acquires information on the magnetic flux density of the teeth when the teeth are excited with the average magnetic field strength calculated in S305. This process is the same as that in S105.

[0093] In S307, the teeth width determination unit 2707 determines the teeth width so that the product of the "teeth width" and the "magnetic flux density of the teeth" obtained in S306 is approximately constant for each tooth. This process is the same as that in S106. By the process of S307, for example, as shown in FIG. 11, the width of the teeth is determined weighted based on the ratio of the operation time.

[0094] In S308, the stator core design unit 2708 applies the determined width of the teeth to the width of the teeth according to the angle from the rolling direction to design the stator core. This process is the same as that in S107. In this way, by designing a stator core using stator core design device 2700, it is possible to reduce the variation in magnetic flux density throughout the entire operation time, thereby suppressing iron loss. Also, by calculating the evaluated magnetic flux density of the teeth by weighting the average magnetic flux density of the teeth based on the ratio of the operation time, and performing subsequent processing based on the calculated evaluated magnetic flux density of the teeth, it is possible to reduce the amount of processing.

[0095] As described above, according to this embodiment, by determining the width of the teeth so that the "tooth width" x "magnetic flux density of the tooth" is approximately constant for each tooth, it is possible to reduce variation in magnetic flux density and suppress iron loss. As described above, each tooth may be teeth at a predetermined interval, such as 0°, 22.5°, 45°, 67.5°, and 90° from the rolling direction, or all teeth. In addition, "substantially constant" does not necessarily mean a completely constant state, but includes a range in which iron loss can be suppressed more than in the comparative example. Specifically, "substantially constant" means that the difference between the maximum and minimum values ​​of "teeth width" x "teeth magnetic flux density" is within ±1%, preferably within ±0.5%. As described above, the products of the "teeth magnetic flux density" for the torque ratio of 60[%] in FIG. 7 and the "optimum teeth width" for the torque ratio of 60[%] in FIG. 8 multiplied by each angle from the rolling direction are all 9.3, which is approximately constant. Specifically, at an angle of 0° from the rolling direction, the magnetic flux density of the teeth is 1.65 [T] × optimal width of the teeth 5.64 [mm] = 9.306 ≒ 9.3, at an angle of 22.5° from the rolling direction, the magnetic flux density of the teeth is 1.61 [T] × optimal width of the teeth 5.76 [mm] = 9.2736 ≒ 9.3, at an angle of 45° from the rolling direction, the magnetic flux density of the teeth is 1.55 [T] × optimal width of the teeth 5.99 [mm] = 9.2845 ≒ 9.3, at an angle of 67.5° from the rolling direction, the magnetic flux density of the teeth is 1.56 [T] × optimal width of the teeth 5.96 [mm] = 9.2976 ≒ 9.3, and at an angle of 90° from the rolling direction, the magnetic flux density of the teeth is 1.59 [T] × optimal width of the teeth 5.85 [mm] = 9.3015 ≒ 9.3. In this case, the difference between the maximum and minimum values ​​is 9.306÷9.2736≒1.0035, so the approximate constant is within 0.5%. If 9.25 to 9.34 is allowed as the range for rounding 9.3, then 9.34÷9.25≒1.0097, so the approximate constant is within 1%.

[0096] Next, among the above-mentioned electrical steel sheets, Material B can suppress iron loss more than Material A. Here, the electromagnetic steel sheet according to Material B will be described. In the following description, the direction at an angle of 45° from the rolling direction is referred to as the direction inclined 45° from the rolling direction, and the direction at an angle of 135° from the rolling direction is referred to as the direction inclined 135° from the rolling direction. In addition, the direction at an angle of θ° from the rolling direction is referred to as the direction inclined θ° from the rolling direction. Thus, the direction at an angle of θ° from the rolling direction and the direction inclined θ° from the rolling direction have the same meaning.

[0097] First, the chemical composition of the steel material used in an example of the non-oriented electromagnetic steel sheet related to the material B (hereinafter referred to as the non-oriented electromagnetic steel sheet of the present embodiment) and its manufacturing method will be described. In the following description, “%”, which is the unit of the content of each element contained in the non-oriented electromagnetic steel sheet or steel material of the present embodiment, means “mass %” unless otherwise specified. Also, the numerical limit range described with “~” includes the lower limit value and the upper limit value within that range. The numerical value indicated by “less than” or “exceeding” is not included in the numerical range. The non-oriented electromagnetic steel sheet and the steel material have a chemical composition in which ferrite-austenite transformation (hereinafter referred to as α-γ transformation) can occur, and contain C: 0.0100% or less, Si: 1.50% to 4.00%, sol.Al: 0.0001% to 1.0%, S: 0.0100% or less, N: 0.0100% or less, one or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, Au: a total of 2.50% to 5.00%, Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%, and one or more selected from the group consisting of Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd: a total of 0.0000% to 0.0100%, and the balance consists of Fe and impurities. Further, the contents of Mn, Ni, Co, Pt, Pb, Cu, Au, Si, and sol.Al satisfy the predetermined conditions described later. Examples of the impurities include those contained in raw materials such as ore and scrap, and those contained in the manufacturing process.

[0098] <<C: 0.0100% or less>> C increases iron loss and causes magnetic aging. Therefore, the lower the C content, the better. Such a phenomenon is significant when the C content exceeds 0.0100%. For this reason, the C content should be 0.0100% or less. The reduction of the C content also contributes to the uniform improvement of magnetic properties in all directions within the plate surface. Although the lower limit of the C content is not particularly limited, considering the cost of decarburization treatment during refining, it is preferably 0.0005% or more.

[0099] <<Si: 1.50% - 4.00%>> Si increases electrical resistance, reduces eddy current loss, reduces iron loss, increases the yield ratio, and improves the punchability of the iron core. When the Si content is less than 1.50%, these effects cannot be fully obtained. Therefore, the Si content should be 1.50% or more. On the other hand, when the Si content exceeds 4.00%, the magnetic flux density decreases, the punchability decreases due to an excessive increase in hardness, and cold rolling becomes difficult. Therefore, the Si content should be 4.00% or less.

[0100] <<sol.Al: 0.0001% - 1.0%>> sol.Al increases electrical resistance, reduces eddy current loss, and reduces iron loss. sol.Al also contributes to the improvement of the relative magnitude of the magnetic flux density B50 with respect to the saturation magnetic flux density. Here, the magnetic flux density B50 is the magnetic flux density when excited by a magnetic field strength of 5000 A / m. When the sol.Al content is less than 0.0001%, these effects cannot be fully obtained. In addition, Al also has an effect of promoting desulfurization in steelmaking. Therefore, the sol.Al content should be 0.0001% or more. On the other hand, when the sol.Al content exceeds 1.0%, the magnetic flux density decreases, the yield ratio decreases, and the punchability decreases. Therefore, the sol.Al content should be 1.0% or less.

[0101] <<S: 0.0100% or less>> S is not an essential element and is contained as an impurity in steel, for example. S inhibits recrystallization and grain growth during annealing by the precipitation of fine MnS. Therefore, the lower the S content, the better. The increase in iron loss and the decrease in magnetic flux density due to such inhibition of recrystallization and grain growth are significant when the S content exceeds 0.0100%. For this reason, the S content should be 0.0100% or less. Although the lower limit of the S content is not particularly limited, it is preferably 0.0003% or more in view of the cost of desulfurization treatment during refining.

[0102] <<N: 0.0100% or less>> Similar to C, N deteriorates magnetic properties, so the lower the N content, the better. Therefore, the N content should be 0.0100% or less. Although the lower limit of the N content is not particularly limited, it is preferably 0.0010% or more in view of the cost of denitrification treatment during refining.

[0103] <<One or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, Au: 2.50% - 5.00% in total>> Since these elements are necessary for causing α-γ transformation, it is necessary to contain these elements in a total amount of 2.50% or more. On the other hand, if the total exceeds 5.00%, the cost increases and the magnetic flux density may decrease. Therefore, the total amount of these elements should be 5.00% or less.

[0104] Also, as conditions under which α-γ transformation can occur, it is further assumed that the following conditions are satisfied. That is, when the Mn content (mass%) is [Mn], the Ni content (mass%) is [Ni], the Co content (mass%) is [Co], the Pt content (mass%) is [Pt], the Pb content (mass%) is [Pb], the Cu content (mass%) is [Cu], the Au content (mass%) is [Au], the Si content (mass%) is [Si], and the sol.Al content (mass%) is [sol.Al], it is preferably satisfied in mass% by the following formula (1). ([Mn] + [Ni] + [Co] + [Pt] + [Pb] + [Cu] + [Au]) - ([Si] + [sol.Al]) > 0% ···(1)

[0105] When the above-mentioned formula (1) is not satisfied, α-γ transformation does not occur, so the magnetic flux density decreases.

[0106] <<Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%>> Sn and Sb improve the grain structure after cold rolling and recrystallization, and improve their magnetic flux density. Therefore, these elements may be contained as necessary, but if contained in excess, the steel will be embrittled. Therefore, the Sn content and the Sb content are both set to 0.400% or less. Further, P may be contained to ensure the hardness of the steel sheet after recrystallization, but if contained in excess, it will cause embrittlement of the steel. Therefore, the P content is set to 0.400% or less. When further effects such as magnetic properties are imparted as described above, it is preferable to contain one or more selected from the group consisting of 0.020% to 0.400% of Sn, 0.020% to 0.400% of Sb, and 0.020% to 0.400% of P.

[0107] <<One or more selected from the group consisting of Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd: Total 0.0000% to 0.0100%>> Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn and Cd react with S in the molten steel during casting to form precipitates of sulfides or oxysulfides, or both. Hereinafter, Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn and Cd may be collectively referred to as "coarse precipitate forming elements". The particle size of the precipitates of the coarse precipitate forming elements is about 1 μm to 2 μm, which is much larger than the particle size (about 100 nm) of fine precipitates such as MnS, TiN and AlN. Therefore, these fine precipitates adhere to the precipitates of the coarse precipitate forming elements, and are less likely to inhibit recrystallization and grain growth during intermediate annealing. In order to fully obtain these effects, it is preferable that the total content of these elements is 0.0005% or more. However, if the total content of these elements exceeds 0.0100%, the total amount of sulfides or oxysulfides or both will be excessive, which will inhibit recrystallization and grain growth during intermediate annealing. Therefore, the total content of the elements that form coarse precipitates should be 0.0100% or less.

[0108] <<Collective organization>> Next, the texture of the non-oriented electrical steel sheet of this embodiment will be described. The details of the manufacturing method will be described later, but the non-oriented electrical steel sheet of this embodiment has a chemical composition in which α-γ transformation can occur, and the structure is refined by rapid cooling immediately after the end of finish rolling in hot rolling, resulting in a structure in which {100} crystal grains have grown. As a result, the non-oriented electrical steel sheet of this embodiment has a {100} <011> The orientation concentration strength is 5 to 30, and the magnetic flux density B50 in the 45° direction to the rolling direction is particularly high. Thus, the magnetic flux density is high in a specific direction, but overall, a high magnetic flux density is obtained on average in all directions. <011> When the orientation concentration is less than 5, the magnetic flux density is reduced. <112> The intensity of the magnetic flux increases, and the magnetic flux density decreases overall. <011> Manufacturing methods that achieve an orientation integration strength of over 30 require thick hot-rolled sheets, which poses the problem of being difficult to manufacture.

[0109] {100} <011> The orientation integration strength can be measured by X-ray diffraction or electron backscatter diffraction (EBSD). Since the reflection angle of X-rays and electron beams from a sample differs for each crystal orientation, the crystal orientation strength can be determined from the reflection intensity of a randomly oriented sample. <011> The orientation accumulation strength is an X-ray random intensity ratio of 5 to 30. In this case, the crystal orientation may be measured by EBSD and a value converted into an X-ray random intensity ratio may be used.

[0110] <<Thickness>> Next, the thickness of the non-oriented electrical steel sheet of this embodiment will be described. The thickness of the non-oriented electrical steel sheet of this embodiment is 0.50 mm or less. If the thickness exceeds 0.50 mm, excellent high-frequency iron loss cannot be obtained. Therefore, the thickness is set to 0.50 mm or less.

[0111] <<Magnetic properties>> Next, the magnetic properties of the non-oriented electrical steel sheet of this embodiment will be described. When examining the magnetic properties, the value of B50, which is the magnetic flux density of the non-oriented electrical steel sheet of this embodiment, is measured. In the manufactured non-oriented electrical steel sheet, one side of the rolling direction cannot be distinguished from the other side. Therefore, in this embodiment, the rolling direction refers to both sides. If the value of B50 in the rolling direction is B50L, the value of B50 in a direction tilted 45° from the rolling direction is B50D1, the value of B50 in a direction tilted 90° from the rolling direction is B50C, and the value of B50 in a direction tilted 135° from the rolling direction is B50D2, then anisotropy of the magnetic flux density is observed, with B50D1 and B50D2 being the highest and B50L and B50C being the lowest.

[0112] Here, for example, when considering the distribution of magnetic flux density in all directions (0° to 360°) with the clockwise direction (or counterclockwise direction) as the positive direction, and the rolling direction is 0° (one direction) and 180° (the other direction), B50D1 has B50 values ​​at 45° and 225°, and B50D2 has B50 values ​​at 135° and 315°. Similarly, B50L has B50 values ​​at 0° and 180°, and B50C has B50 values ​​at 90° and 270°. The B50 value at 45° and the B50 value at 225° strictly match, and the B50 value at 135° and the B50 value at 315° strictly match. However, B50D1 and B50D2 may not strictly match because it may not be easy to make the magnetic properties the same during actual manufacturing. Similarly, the B50 value at 0° strictly matches the B50 value at 180°, and the B50 value at 90° strictly matches the B50 value at 270°, while B50L and B50C may not strictly match. In the non-oriented electrical steel sheet of this embodiment, the average values ​​of B50D1 and B50D2 and the average values ​​of B50L and B50C are used to satisfy the following formulas (2) and (3). (B50D1+B50D2) / 2>1.7T ···(2) (B50D1+B50D2) / 2>(B50L+B50C) / 2...(3)

[0113] In this way, when the magnetic flux density is measured, the average value of B50D1 and B50D2 is 1.7 T or more as shown in formula (2), and high anisotropy of the magnetic flux density is confirmed as shown in formula (3).

[0114] Furthermore, in addition to satisfying formula (1), it is preferable that the anisotropy of the magnetic flux density is higher than that of formula (3), as shown in the following formula (4). (B50D1+B50D2) / 2>1.1×(B50L+B50C) / 2...(4) Furthermore, it is preferable that the anisotropy of the magnetic flux density is higher, as shown in the following formula (5). (B50D1+B50D2) / 2>1.2×(B50L+B50C) / 2...(5) Furthermore, as shown in the following formula (6), it is preferable that the average value of B50D1 and B50D2 is 1.8T or more. (B50D1+B50D2) / 2>1.8T ···(6)

[0115] The above 45° is a theoretical value, and since it may not be easy to match it to 45° in actual manufacturing, it also includes angles that do not strictly match 45°. This also applies to the 0°, 90°, 135°, 180°, 225°, 270°, and 315°.

[0116] The magnetic flux density can be measured by cutting a 55 mm square sample from a direction at 45°, 0°, etc. with respect to the rolling direction and using a single sheet magnetic measurement device.

[0117] <<Manufacturing method>> Next, an example of a method for manufacturing the non-oriented electrical steel sheet of this embodiment will be described. When manufacturing the non-oriented electrical steel sheet of this embodiment, for example, hot rolling, cold rolling (first cold rolling), intermediate annealing (first annealing), skin pass rolling (second cold rolling), finish annealing (third annealing), stress relief annealing (second annealing), etc. are performed.

[0118] First, the above-mentioned steel material is heated and hot-rolled. The steel material is, for example, a slab produced by normal continuous casting. The rough rolling and finish rolling of the hot rolling are performed at a temperature in the γ region (Ar1 temperature or higher). In other words, the hot rolling is performed so that the finishing temperature of the finish rolling is Ar1 temperature or higher and the coiling temperature is more than 250°C and less than 600°C. As a result, the structure is refined by the transformation from austenite to ferrite by subsequent cooling. If cold rolling is then performed in the refined state, bulging recrystallization (hereinafter, bulging) is likely to occur, and it is possible to facilitate the growth of {100} crystal grains, which are usually difficult to grow.

[0119] Furthermore, when manufacturing the non-oriented electrical steel sheet of this embodiment, the temperature (finishing temperature) during the final pass of finish rolling is set to be equal to or higher than the Ar1 temperature, and the coiling temperature is set to be greater than 250°C and equal to or lower than 600°C. The crystal structure is refined by transforming from austenite to ferrite. By refining the crystal structure in this way, it is possible to make bulging more likely to occur through the subsequent cold rolling and intermediate annealing.

[0120] Thereafter, the hot-rolled steel sheet is coiled without annealing, pickled, and then cold-rolled. The reduction ratio in cold rolling is preferably 80% to 95%. If the reduction ratio is less than 85%, bulging is less likely to occur. If the reduction ratio exceeds 95%, {100} crystal grains tend to grow due to subsequent bulging, but the hot-rolled steel sheet must be thickened, which makes coiling of the hot roll difficult and operation difficult. The reduction ratio in cold rolling is more preferably 86% or more. If the reduction ratio in cold rolling is 86% or more, bulging is more likely to occur.

[0121] After the cold rolling is completed, intermediate annealing is performed. When manufacturing the non-oriented electrical steel sheet of this embodiment, intermediate annealing is performed at a temperature at which transformation to austenite does not occur. In other words, it is preferable that the intermediate annealing temperature is lower than the Ac1 temperature. By performing intermediate annealing in this manner, bulging occurs, and {100} crystal grains tend to grow. In addition, the time for intermediate annealing is preferably 5 seconds to 60 seconds.

[0122] After intermediate annealing, skin pass rolling is performed. As mentioned above, if skin pass rolling and annealing are performed in a state where bulging has occurred, the {100} grains will grow further from the part where bulging has occurred. This is because the {100} grains are further grown by skin pass rolling. <011> The crystal grains are less susceptible to distortion, and the {111} <112> The crystal grains have a tendency to accumulate distortion, and the {100} <011> The crystal grains are driven by the difference in strain {111} <112> This is to corrode the crystal grains. This corrode phenomenon, which occurs with the strain difference as the driving force, is called strain-induced grain boundary migration (hereinafter, SIBM). The reduction ratio of the skin pass rolling is preferably 5% to 25%. If the reduction ratio is less than 5%, the amount of strain is too small, so SIBM does not occur in the subsequent annealing, and the {100} <011> On the other hand, if the rolling reduction rate exceeds 25%, the amount of distortion becomes too large, and the {111} <112> Recrystallization nucleation (hereafter referred to as nucleation) occurs, in which new crystal grains are born from within the crystal grains. In this nucleation, most of the new grains have {111} <112> The magnetic properties are poor due to the crystal grains.

[0123] After the skin pass rolling, the steel is subjected to a final annealing in order to release the distortion and improve the workability. The final annealing is also performed at a temperature that does not cause the steel to transform into austenite, and the final annealing temperature is set to be lower than the Ac1 temperature. By performing the final annealing in this manner, the {100} <011> The grains are {111} <112> This erodes the crystal grains and improves the magnetic properties. In addition, the time required for the final annealing to reach a temperature of 600°C to Ac1 is set to within 1200 seconds. If the annealing time is too short, most of the distortion introduced by the skin pass remains, and warping occurs when punching complex shapes. On the other hand, if the annealing time is too long, the crystal grains become too coarse, causing large sagging during punching and resulting in poor punching precision.

[0124] After the finish annealing is completed, the non-oriented electrical steel sheet is subjected to forming processing, etc., to obtain a desired steel member. Then, in order to remove distortion, etc., caused by forming processing, etc. (e.g., punching) of the steel member made of the non-oriented electrical steel sheet, the steel member is subjected to stress relief annealing. In this embodiment, in order to generate SIBM below the Ac1 temperature and to make the crystal grain size coarse, the stress relief annealing temperature is set to, for example, about 800°C, and the stress relief annealing time is set to about 2 hours. The magnetic properties can be improved by stress relief annealing.

[0125] In the non-oriented electrical steel sheet (steel member) of this embodiment, the high B50 and excellent anisotropy of the formula (1) are obtained by performing finish rolling at an Ar1 temperature or higher mainly in the hot rolling process among the above-mentioned manufacturing methods. Furthermore, by setting the reduction rate in the skin pass rolling process to about 10%, even more excellent anisotropy of the formula (4) is obtained. In this embodiment, the Ar1 temperature is determined from the thermal expansion change of the steel material (steel plate) during cooling at an average cooling rate of 1°C / s. Also, in this embodiment, the Ac1 temperature is determined from the thermal expansion change of the steel material (steel plate) during heating at an average heating rate of 1°C / s.

[0126] As described above, a steel member made of the non-oriented electrical steel sheet of this embodiment can be manufactured.

[0127] Next, the non-oriented electrical steel sheet of this embodiment will be specifically described with reference to examples. The examples shown below are merely examples of the non-oriented electrical steel sheet, and the non-oriented electrical steel sheet is not limited to the examples below.

[0128] <<First Example>> Molten steel was cast to produce ingots with the compositions shown in Tables 1 and 2 below. Here, the left side of the formula represents the value of the left side of the formula (1) above. The produced ingots were then heated to 1150°C and hot-rolled to a plate thickness of 2.5 mm. After the finish rolling, the ingots were water-cooled and the hot-rolled steel plates were coiled. The temperature at the final pass of the finish rolling (finishing temperature) was 830°C, all of which were higher than the Ar1 temperature. For No. 108, which does not undergo γ-α transformation, the finishing temperature was 850°C. The coiling temperature was also set under the conditions shown in Table 1.

[0129] Next, the hot-rolled steel sheet was subjected to pickling to remove scale, and then rolled at the reduction ratio after cold rolling shown in Table 1. Then, intermediate annealing was performed at 700°C for 30 seconds in a non-oxidizing atmosphere. Next, the second cold rolling (skin pass rolling) was performed at the reduction ratio shown in Table 1.

[0130] Next, to examine the magnetic properties, a second cold rolling (skin pass rolling) was performed followed by a finish annealing at 800°C for 30 seconds, and a 55mm square sample was prepared by shearing, after which a stress relief annealing was performed at 800°C for 2 hours, and the magnetic flux density B50 was measured. The measurement samples were 55mm square samples taken in two different directions, 0° and 45° to the rolling direction. These two types of samples were then measured, and the magnetic flux densities B50 at 0°, 45°, 90°, and 135° to the rolling direction were designated B50L, B50D1, B50C, and B50D2, respectively.

[0131] [Table 1]

[0132] [Table 2]

[0133] The underlines in Tables 1 and 2 indicate conditions outside the scope of the present invention. Inventive examples No. 101 to No. 107, No. 109 to No. 111, and No. 114 to No. 130, all of which had good magnetic flux density B50 in both the 45° direction and the average magnetic flux density B50 for the entire circumference. However, No. 116 and No. 127 were slightly lower in magnetic flux density B50 because the coiling temperature was not appropriate. No. 129 and No. 130 had a low cold rolling reduction ratio, so their magnetic flux density B50 was slightly lower than that of No. 118, which had the same composition and coiling temperature. On the other hand, comparative example No. 108 had a high Si concentration, the value of the left side of the formula was 0 or less, and the composition did not undergo α-γ transformation, so all of the magnetic flux densities B50 were low. Comparative example No. 112 had a low skin pass rolling ratio, so the {100} <011> The strength was less than 5, and the magnetic flux density B50 was low in all cases. <011> The strength was over 30, which is outside the scope of the present invention. No. 113 had a drawback in that the thickness of the hot-rolled plate was as much as 7 mm, making it difficult to operate.

[0134] <<Second embodiment>> The molten steel was cast to produce an ingot with the composition shown in Table 3 below. The produced ingot was then heated to 1150°C and hot-rolled to a plate thickness of 2.5 mm. After finish rolling, the ingot was water-cooled and the hot-rolled steel plate was coiled. The finish temperature at the final pass of the finish rolling was 830°C, and all temperatures were higher than the Ar1 temperature.

[0135] Next, the hot-rolled steel sheet was pickled to remove scale, and cold-rolled to a thickness of 0.385 mm. Then, intermediate annealing was performed in a non-oxidizing atmosphere, and the intermediate annealing temperature was controlled so that the recrystallization rate was 85%. Next, a second cold rolling (skin pass rolling) was performed to a thickness of 0.35 mm.

[0136] Next, to examine the magnetic properties, a second cold rolling (skin pass rolling) was followed by a finish annealing at 800°C for 30 seconds, and a 55 mm square sample was prepared by shearing, after which a stress relief annealing was performed at 800°C for 2 hours, and the magnetic flux density B50 and iron loss W10 / 400 were measured. The magnetic flux density B50 was measured using the same procedure as in the first embodiment. On the other hand, the iron loss W10 / 400 was measured as the energy loss (W / kg) that occurred in the sample when a 400 Hz AC magnetic field was applied so that the maximum magnetic flux density was 1.0 T. The iron loss was the average value of the results measured at 0°, 45°, 90°, and 135° with respect to the rolling direction.

[0137] [Table 3]

[0138] [Table 4]

[0139] Nos. 201 to 214 are all examples of the invention, and all had good magnetic properties. In particular, Nos. 202 to 204 had higher magnetic flux density B50 than Nos. 201 and 205 to 214, and Nos. 205 to 214 had lower iron loss W10 / 400 than Nos. 201 to 204.

[0140] Although the present invention has been described above in conjunction with various embodiments, the present invention is not limited to these embodiments, and modifications and the like are possible within the scope of the present invention. In the above description, the operating condition is the torque ratio, but this is not limiting, and the operating condition may be the rotation speed ratio or the torque ratio for each rotation speed ratio. [Industrial Applicability]

[0141] According to the present invention, it is possible to reduce the variation in magnetic flux density and suppress iron loss, and thus the present invention has high industrial applicability. [Explanation of symbols]

[0142] 100: Rotating motor 110:Rotor 120:Stator 121a~121p: Teeth 122: York 130: Rotation axis 400:Motor 410:Rotor 411: Permanent magnet 421: Stator core 422: Coil 501a~501m: Stator 1600:Motor 1610:Rotor 1621: Stator core 1622: Coil 1701a~1701p: Stator 2700: Stator core design device 2701: Operation data acquisition unit 2702: Operation condition / operation ratio specification part 2703: Average magnetic flux density acquisition unit 2704: Evaluation magnetic flux density calculation section 2705: Average magnetic field strength calculation unit 2706: Teeth magnetic flux density acquisition unit 2707: Teeth width determination part 2708: Stator Core Design Department

Claims

1. A stator core having a plurality of laminated electromagnetic steel sheets, Among the plurality of teeth of the stator core, a width of the teeth along a direction having superior magnetic properties is narrower than a width of the teeth along a direction having inferior magnetic properties, The stator core is formed by laminating rolled electromagnetic steel sheets, The electromagnetic steel sheet is In mass percent, C: 0.0100% or less, Si: 1.50% to 4.00%, sol. Al: 0.0001% to 1.0%, S: 0.0100% or less, N: 0.0100% or less, One or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, and Au: 2.50% to 5.00% in total, Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%, and One or more selected from the group consisting of Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd: 0.0000% to 0.0100% in total; When the Mn content (mass%) is [Mn], the Ni content (mass%) is [Ni], the Co content (mass%) is [Co], the Pt content (mass%) is [Pt], the Pb content (mass%) is [Pb], the Cu content (mass%) is [Cu], the Au content (mass%) is [Au], the Si content (mass%) is [Si], and the sol. Al content (mass%) is [sol. Al], the following formula (1) is satisfied, The balance has a chemical composition consisting of Fe and impurities, When the value of B50 in the rolling direction is B50L, the value of B50 in a direction tilted at 45° from the rolling direction is B50D1, the value of B50 in a direction tilted at 90° from the rolling direction is B50C, and the value of B50 in a direction tilted at 135° from the rolling direction is B50D2, the following formulas (2) and (3) are satisfied, The X-ray random intensity ratio of {100}<011> is 5 or more and less than 30; The plate thickness is 0.50 mm or less, The direction in which the magnetic properties are excellent is a direction at an angle of 45° from the rolling direction, and the direction in which the magnetic properties are inferior is a direction at an angle of 0° and 90° from the rolling direction, A stator core characterized in that the width of the teeth along a direction at an angle of 45° from the rolling direction is narrower than both the width of the teeth along a direction at an angle of 0° from the rolling direction and the width of the teeth along a direction at an angle of 90° from the rolling direction. ([Mn] + [Ni] + [Co] + [Pt] + [Pb] + [Cu] + [Au]) - ([Si] + [sol.Al]) > 0% ... (1) (B50D1+B50D2) / 2>1.7T...(2) (B50D1+B50D2) / 2>1.1×(B50L+B50C) / 2...(3)

2. A stator core having a plurality of laminated electromagnetic steel sheets, Among the plurality of teeth of the stator core, a width of the teeth along a direction having superior magnetic properties is narrower than a width of the teeth along a direction having inferior magnetic properties, The stator core is formed by laminating rolled electromagnetic steel sheets, The electromagnetic steel sheet is In mass percent, C: 0.0100% or less, Si: 1.50% to 4.00%, sol. Al: 0.0001% to 1.0%, S: 0.0100% or less, N: 0.0100% or less, One or more selected from the group consisting of Mn, Ni, Co, Pt, Pb, Cu, and Au: 2.50% to 5.00% in total, Sn: 0.000% to 0.400%, Sb: 0.000% to 0.400%, P: 0.000% to 0.400%, and One or more selected from the group consisting of Mg, Ca, Sr, Ba, Ce, La, Nd, Pr, Zn, and Cd: 0.0000% to 0.0100% in total; When the Mn content (mass%) is [Mn], the Ni content (mass%) is [Ni], the Co content (mass%) is [Co], the Pt content (mass%) is [Pt], the Pb content (mass%) is [Pb], the Cu content (mass%) is [Cu], the Au content (mass%) is [Au], the Si content (mass%) is [Si], and the sol. Al content (mass%) is [sol. Al], the following formula (1) is satisfied, The balance has a chemical composition consisting of Fe and impurities, When the value of B50 in the rolling direction is B50L, the value of B50 in a direction tilted at 45° from the rolling direction is B50D1, the value of B50 in a direction tilted at 90° from the rolling direction is B50C, and the value of B50 in a direction tilted at 135° from the rolling direction is B50D2, the following formulas (4) and (5) are satisfied, The X-ray random intensity ratio of {100}<011> is 5 or more and less than 30; The plate thickness is 0.50 mm or less, The direction in which the magnetic properties are excellent is a direction at an angle of 45° from the rolling direction, and the direction in which the magnetic properties are inferior is a direction at an angle of 0° and 90° from the rolling direction, A stator core characterized in that the width of the teeth along a direction at an angle of 45° from the rolling direction is narrower than both the width of the teeth along a direction at an angle of 0° from the rolling direction and the width of the teeth along a direction at an angle of 90° from the rolling direction. ([Mn] + [Ni] + [Co] + [Pt] + [Pb] + [Cu] + [Au]) - ([Si] + [sol.Al]) > 0% ... (1) (B50D1+B50D2) / 2>1.8T...(4) (B50D1+B50D2) / 2>(B50L+B50C) / 2...(5)

3. In the teeth of the stator core, 3. A stator core according to claim 1, wherein the product of the width of the teeth of the stator core and the magnetic flux density of the teeth when excited with a predetermined magnetic field strength is approximately constant for each tooth.

4. 3. The stator core according to claim 1, wherein the following formula (6) is satisfied: (B50D1+B50D2) / 2>1.2×(B50L+B50C) / 2...(6)

5. The electromagnetic steel sheet comprises, in mass%, 5. The rotor core according to claim 1, further comprising: 0.020% to 0.400% of the Sn or 0.020% to 0.400% of the Sb.

6. A rotating electric machine comprising the stator core according to any one of claims 1 to 5.

7. A method for designing a stator core having laminated electromagnetic steel sheets, comprising the steps of: a teeth magnetic flux density acquiring step of acquiring information on the magnetic flux density of the teeth when excited with a predetermined magnetic field strength; a determining step of determining a width of the teeth of the stator core such that a product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquiring step is substantially constant for each tooth; an operation data acquisition step of acquiring operation data of a rotating electric machine including the stator core when the rotating electric machine is operated; A specification step of specifying a ratio of an operation time for each of a plurality of operation conditions based on the operation data acquired by the operation data acquisition step; an average magnetic flux density acquiring step of acquiring information on an average magnetic flux density of the teeth corresponding to each of the plurality of operating conditions; an average magnetic field strength calculation step of calculating an average magnetic field strength of the teeth for each of the plurality of operating conditions from information on the average magnetic flux density of the teeth corresponding to each of the plurality of operating conditions acquired in the average magnetic flux density acquisition step, In the teeth magnetic flux density obtaining step, acquiring information on magnetic flux density of the teeth for each of the plurality of operating conditions when the teeth are excited with the average magnetic field strength of the teeth for each of the plurality of operating conditions calculated in the average magnetic field strength calculation step; In the determining step, A method for designing a stator core, comprising the steps of: calculating a width of the teeth for each of the plurality of operating conditions so that the product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquisition process is approximately constant for each tooth; weighting the calculated width of the teeth for each of the plurality of operating conditions based on the ratio of the operating time identified in the identification process; and determining the weighted width of the teeth.

8. A method for designing a stator core having laminated electromagnetic steel sheets, comprising: a teeth magnetic flux density acquiring step of acquiring information on the magnetic flux density of the teeth when excited with a predetermined magnetic field strength; a determining step of determining a width of the teeth of the stator core such that a product of the width of the teeth of the stator core and the magnetic flux density of the teeth acquired in the teeth magnetic flux density acquiring step is substantially constant for each tooth; an operation data acquisition step of acquiring operation data of a rotating electric machine including the stator core when the rotating electric machine is operated; A specification step of specifying a ratio of an operation time for each of a plurality of operation conditions based on the operation data acquired by the operation data acquisition step; an average magnetic flux density acquiring step of acquiring information on an average magnetic flux density of the teeth corresponding to each of the plurality of operating conditions; an evaluated magnetic flux density calculation step of calculating an evaluated magnetic flux density of the teeth weighted based on the ratio of the operation time specified in the specification step from information on the average magnetic flux density of the teeth corresponding to each of the plurality of operating conditions acquired in the average magnetic flux density acquisition step; an average magnetic field strength calculation step of calculating an average magnetic field strength of the teeth from the evaluated magnetic flux density of the teeth calculated in the evaluated magnetic flux density calculation step, In the teeth magnetic flux density obtaining step, A method for designing a stator core, comprising the steps of: obtaining information on the magnetic flux density of the teeth when excited with the average magnetic field strength of the teeth calculated in the average magnetic field strength calculation process;

9. In the operation data acquisition step, 9. The method for designing a stator core according to claim 7, further comprising acquiring at least one of plan data and performance data of an electric rotating machine including the stator core.

Citation Information

Patent Citations

  • Stator core for rotary electric machine

    JP1984010142A

  • Core for small-sized motor

    JP1996214476A

  • Electric motor

    JP2002320350A

  • Specifying method of core material characteristic, its apparatus, rotary machine designed by the specifying method and its designing method

    JP2005269746A

  • Electromagnetic steel sheet, and manufacturing method of electromagnetic steel sheet

    JP2019178380A