Semiconductor module and manufacturing method thereof
Patent Information
- Application Number
- JP2021205933
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-12-20
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2041-12-20
AI Technical Summary
【0007】 本開示では、積層基板は、プリプレグ材の一部が貫通孔に突出した突出部を有する。ダイボンド樹脂の外周部はプリプレグ材の突出部の上面に接着されている。ダイボンド樹脂とプリプレグ材との接着力は強いため、ダイボンド樹脂の剥離を抑制することができる。
Smart Images

Figure 0007589673000001 
Figure 0007589673000002 
Figure 0007589673000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a semiconductor module and a manufacturing method thereof. [Background technology]
[0002] A semiconductor module has been disclosed in which a semiconductor chip is bonded onto a conductive plate in a through hole of a laminated substrate (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 11-040688 Summary of the Invention [Problem to be solved by the invention]
[0004] In the assembly of a semiconductor module, the semiconductor chip is fixed with die-bond resin and further sealed with mold resin. However, the adhesive strength between the die-bond resin and the Au plating on the top surface of the conductor plate is weak. For this reason, when thermal stress is applied to the laminated substrate during a reliability test or the like, the outer periphery of the die-bond resin starts to peel off from the conductor plate. In addition, peeling of the mold resin occurs at the corner where the side wall of the through hole intersects with the conductor plate. And because the mold resin and the semiconductor chip are bonded together, peeling occurs at the interface between the conductor plate and the semiconductor chip, where the adhesive strength is weak. When the semiconductor chip floats off the conductor plate, the thermal conductivity deteriorates, and there is a problem that the product quality is not met.
[0005] The present disclosure has been made to solve the above-mentioned problems, and has an object to provide a semiconductor module capable of suppressing peeling, and a manufacturing method thereof. [Means for solving the problem]
[0006] The semiconductor module according to the present disclosure comprises a laminated substrate having a through hole, a conductive plate provided on the underside of the laminated substrate, a semiconductor chip bonded to the conductive plate in the through hole by a die bond resin, and a molded resin that seals the semiconductor chip, wherein the laminated substrate has a protruding portion in which a portion of a prepreg material protrudes into the through hole, and the outer periphery of the die bond resin is adhered to the upper surface of the protruding portion of the prepreg material. Effect of the Invention
[0007] In the present disclosure, the laminated substrate has a protruding portion in which a part of the prepreg material protrudes into the through hole. The outer periphery of the die bond resin is bonded to the upper surface of the protruding portion of the prepreg material. Since the adhesive strength between the die bond resin and the prepreg material is strong, peeling of the die bond resin can be suppressed. [Brief description of the drawings]
[0008] [Figure 1] 1 is a cross-sectional view showing a semiconductor module according to a first embodiment. [Diagram 2] FIG. 11 is a cross-sectional view showing a semiconductor module according to a second embodiment. [Diagram 3] 11A to 11C are cross-sectional views showing a method for manufacturing a semiconductor module according to a third embodiment. [Figure 4] 11A to 11C are cross-sectional views showing a method for manufacturing a semiconductor module according to a third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] A semiconductor module and a manufacturing method thereof according to an embodiment will be described with reference to the drawings. The same or corresponding components are designated by the same reference numerals, and repeated description may be omitted.
[0010] Embodiment 1 FIG 1 is a cross-sectional view showing a semiconductor module according to a first embodiment. The laminated substrate 1 is a glass epoxy substrate in which prepreg materials 2 and base materials 3 are alternately laminated. The prepreg material 2 is a material in which layers of carbon fiber or glass fiber are impregnated with a resin such as epoxy resin. The base material 3 is, for example, a glass cloth. Wiring 4 is provided on the inner layer and top surface of the laminated substrate 1. A solder resist 5 is provided on the top surface of the laminated substrate 1.
[0011] A through hole 6 penetrates the laminated substrate 1 from the top surface to the bottom surface. A conductive plate 7 is provided on the bottom surface of the laminated substrate 1 and covers the lower part of the through hole 6. The conductive plate 7 has a layered structure of Ni / Pd / Au. The space surrounded by the side wall of the through hole 6 and the conductive plate 7 forms a cavity.
[0012] The semiconductor chip 8 is bonded to the conductive plate 7 in the through hole 6 by a die bond resin 9. The die bond resin 9 is, for example, a sintered Ag paste or an Ag paste. The upper electrodes of the semiconductor chip 8 and the wiring 4 of the laminated substrate 1 are connected by wires 10 such as gold wires. The through hole 6 is filled with a molding resin 11, which seals the semiconductor chip 8 and the wires 10. The molding resin 11 is, for example, an epoxy resin.
[0013] In this embodiment, the laminated substrate 1 has a protruding portion 12 in which a part of the prepreg material 2 protrudes into the through hole 6. The outer periphery of the die bond resin 9 is bonded to the upper surface of the protruding portion 12 of the prepreg material 2. Since the adhesive force between the die bond resin 9 and the prepreg material 2 is strong, peeling of the die bond resin 9 can be suppressed. In addition, since the entire back surface of the semiconductor chip 8 is bonded to the conductive plate 7, good thermal conductivity can be ensured. In addition, since the range of resin selection is widened, it is also effective in reducing resin costs and shortening product launch times.
[0014] In addition, the protruding portion 12 of the prepreg material 2 is processed with a router so that it becomes thinner toward the center of the through hole 6, and the upper surface is tapered. This makes it easier for the die bond resin 9 to wet and spread over the upper surface of the protruding portion 12 of the prepreg material 2. The protruding portion 12 of the prepreg material 2 may be rectangular.
[0015] Embodiment 2 2 is a cross-sectional view showing a semiconductor module according to embodiment 2. Through hole 6 has a shape with no corners from the side surface of through hole 6 to the upper surface of protrusion 12. For example, after the lamination press process of laminated substrate 1, a drill cutter with a round tip is used to form bowl-shaped through hole 6.
[0016] Conventionally, when thermal stress is applied to the laminated substrate 1, the molded resin 11 begins to peel off from the corner where the through hole 6 intersects with the conductive plate 7. In contrast, in the present embodiment, there is no corner within the through hole 6 where thermal stress concentrates. This increases the bonding area between the prepreg material 2 and base material 3 of the laminated substrate 1 and the molded resin 11. This makes it difficult for the molded resin 11 to peel off. The other configurations and effects are the same as those of the first embodiment.
[0017] Embodiment 3 3 and 4 are cross-sectional views showing a method for manufacturing a semiconductor module according to a third embodiment. First, as shown in FIG. 3, a through hole 6 is formed in a laminated substrate 1. A tape material 13 is attached to the lower surface of the laminated substrate 1 to cover the lower portion of the through hole 6. The adhesive force of the tape material 13 is utilized to attach a lower electrode 14 of a semiconductor chip 8 to the tape material 13 in the through hole 6. The upper electrode of the semiconductor chip 8 and the wiring 4 of the laminated substrate 1 are connected by a wire 10. The semiconductor chip 8 and the wire 10 are sealed with a molded resin 11. The prepreg material 2 exposed in the through hole 6 of the laminated substrate 1 becomes an adhesive surface for the molded resin 11. After sealing with the molded resin 11, the tape material 13 is peeled off from the laminated substrate 1 and the semiconductor chip 8 to expose the lower electrode 14 as shown in FIG. 4.
[0018] Since no die bond resin with poor adhesion to Au plating is used, the problem of the die bond resin peeling off does not occur. Furthermore, since there is no conductive plate 7, the mold resin 11 does not peel off from the conductive plate 7. Furthermore, since the lower electrodes 14 of the semiconductor chip 8 are exposed, solder can be applied directly to the lower electrodes 14 when mounting the module. Therefore, good thermal conductivity can be ensured. The other configurations and effects are the same as those of the first or second embodiment.
[0019] The semiconductor chip 8 is not limited to being made of silicon, and may be made of a wide band gap semiconductor having a larger band gap than silicon. The wide band gap semiconductor is, for example, silicon carbide, gallium nitride-based material, or diamond. A semiconductor chip made of such a wide band gap semiconductor has high voltage resistance and allowable current density, and can be miniaturized. By using this miniaturized semiconductor chip, a semiconductor device incorporating this semiconductor chip can also be miniaturized and highly integrated. In addition, since the semiconductor chip has high heat resistance, the heat dissipation fins of the heat sink can be miniaturized, and the water-cooled part can be air-cooled, so the semiconductor device can be further miniaturized. In addition, since the power loss of the semiconductor chip is low and highly efficient, the efficiency of the semiconductor device can be increased. [Explanation of symbols]
[0020] REFERENCE SIGNS LIST 1 laminated substrate, 2 prepreg material, 3 base material, 6 through hole, 7 conductive plate, 8 semiconductor chip, 9 die bond resin, 11 molding resin, 12 protrusion, 13 tape material, 14 bottom electrode
Claims
1. A laminated substrate having a through hole; a conductor plate provided on a lower surface of the laminated substrate; a semiconductor chip bonded to the conductive plate in the through hole by a die bond resin; a molding resin that encapsulates the semiconductor chip; The laminated substrate has prepreg materials and base materials alternately laminated together, and a protruding portion in which a part of the prepreg material protrudes into the through hole, A semiconductor module, characterized in that an outer periphery of the die bond resin is adhered to an upper surface of the protruding portion of the prepreg material.
2. The prepreg material is a material in which a layer of carbon fiber or glass fiber is impregnated with a resin, 2. The semiconductor module according to claim 1, wherein the die bond resin is, for example, a sintered Ag paste or an Ag paste.
3. 3. The semiconductor module according to claim 1, wherein an upper surface of the protruding portion of the prepreg material is tapered.
4. 4. The semiconductor module according to claim 3, wherein the through hole has a shape with no corners extending from a side surface of the through hole to an upper surface of the protruding portion.
5. 5. The semiconductor module according to claim 1, wherein the semiconductor chip is made of a wide band gap semiconductor.
6. forming a through hole in the laminated substrate; a step of attaching a tape material to a lower surface of the laminated substrate to cover a lower portion of the through hole; attaching a bottom electrode of a semiconductor chip to the tape material in the through hole; encapsulating the semiconductor chip with a molding resin; and peeling off the tape material after sealing with the molding resin to expose the lower electrodes.
Citation Information
Patent Citations
Semiconductor package
JP1999040688A
Cavity-down type BGA package
JP2001144203A
Semiconductor device and method for manufacturing the same
JP2001267478A
Multilayer printed wiring board and manufacturing method thereof
JP2008034589A
Resin multilayer substrate manufacturing method
JP2014225504A