Methods for characterizing soil materials and for managing compaction

The compaction test device measures soil rigidity and performs multiple energy tests to correlate stiffness, water content, and dry density, addressing the limitations of conventional tests by enhancing soil compaction management.

JP7590934B2Active Publication Date: 2024-11-27独立行政法人水资源机构 +2

Patent Information

Application Number
JP2021107967
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-06-29
Publication Date
2024-11-27
Estimated Expiration
2041-06-29

AI Technical Summary

Technical Problem

Conventional indoor compaction tests only determine the relationship between dry density and water content in soil compaction, failing to account for soil stiffness, which is crucial for effective construction management.

Method used

A compaction test device with a container, weight, and acceleration sensor measures soil rigidity by analyzing the output from the sensor to derive deformation coefficients, and performs multiple tamping tests with varying energies to establish relationships between stiffness, water content, and dry density.

Benefits of technology

Enables precise measurement of soil stiffness during compaction, allowing for better understanding and management of soil compaction processes by correlating deformation coefficients with water content and dry density.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007590934000002
    Figure 0007590934000002
  • Figure 0007590934000003
    Figure 0007590934000003
  • Figure 0007590934000004
    Figure 0007590934000004
Patent Text Reader

Abstract

To measure stiffness of soil material during a tamping test of the soil material.SOLUTION: A test device 10 is used for a tamping test of soil material (sample 11). The test device 10 comprises a container 12 capable of containing the soil material (sample 11) and having an open upper surface 12a, a weight 13 dropped onto the soil material (sample 11) housed in the container 12, an acceleration sensor 16 attached to the weight 13, and a stiffness measuring unit 20 that measures the stiffness (e.g., coefficient of deformation E) of the soil material (sample 11) in the container 12 based on the output from the acceleration sensor 16.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a test device for use in compaction testing of soil materials, a method for characterizing soil materials, and a method for controlling compaction of a compaction work area. [Background technology]

[0002] When constructing embankments, etc., the soil is compacted by applying static pressure, impact force, vibration, etc., which narrows the spaces between the soil particles, improves the interlocking between the particles, and stabilizes the soil. The effectiveness of soil compaction is judged, for example, by the degree to which the soil density (dry density) increases.

[0003] In density management during soil compaction, for example, the degree of compaction (Dc value) is used as an index, which is expressed as the ratio of the dry density of the soil after compaction to the maximum dry density obtained in an indoor compaction test. One example of this compaction test is JIS A 1210 (Soil compaction test by tamping) (see paragraphs 0002 and 0003 of Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-324429 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, in general, when compacting soil, the stiffness (e.g., deformation coefficient) does not necessarily increase simply as the density (dry density) increases (see, for example, JP 2019-2184 A). Therefore, when performing construction management in soil compaction with a focus on the stiffness of the soil, it is preferable to carry out the construction after understanding in advance the relationship between the dry density, moisture content, and stiffness when the soil is compacted. In this regard, in conventional indoor compaction tests, it was only possible to know the relationship between the dry density and moisture content when the soil was compacted.

[0006] In view of the above circumstances, an object of the present invention is to measure the rigidity during a compaction test. [Means for solving the problem]

[0007] Books Related to the invention The method for characterizing soil materials is a method for characterizing soil materials by performing a compaction test using a testing device. The above Test Equipment 、 soil a container capable of containing a plastic material and having an open top; 、 The above A weight is dropped onto the soil material contained in the container; 、 The above An acceleration sensor attached to a weight 、 The above Based on the output from the acceleration sensor, The above a stiffness measuring unit for measuring the stiffness of the soil material in the container; 、 of Prepare.

[0008] The method for characterizing soil materials according to the present invention is 、 performing a first compaction test at a first compaction energy, in which the soil material in the container is compacted by the weight repeatedly; Obtaining a first compaction curve indicating a relationship between a moisture content and a dry density of the soil material in the first compaction test; Measuring the stiffness of the soil material for each cycle in the first compaction test by the stiffness measuring unit; performing a second compaction test on the soil material at a second compaction energy different from the first compaction energy; Obtaining a second compaction curve showing a relationship between the moisture content and the dry density of the soil material in the second compaction test; Estimating a compaction curve for each cycle in the first compaction test based on the first compaction curve and the second compaction curve; Based on the relationship between the stiffness and the water content of the soil material for each cycle obtained in the first compaction test and the estimated compaction curve for each cycle in the first compaction test, Obtaining the relationship between the stiffness, moisture content and dry density of soil materials and, of include.

[0009] The compaction management method according to the present invention is a method for managing the compaction of a compaction work area. 。 Books The compaction management method according to the invention is 、 The above A moisture content measurement process for measuring the moisture content of the compaction area; 、 The above A stiffness measurement process to measure the stiffness of the compaction area; 、 before The soil material characterization method described above was used to obtain The above The relationship between the stiffness of soil materials, their moisture content and dry density, The above The moisture content of the compaction area measured in the moisture content measurement process; The above Based on the stiffness of the compaction construction area measured in the stiffness measurement process, The above A dry density determination process for determining the dry density of the compaction area; 、 of include.

[0010] Here, the "rigidity" in the present invention is an index that indicates the degree of deformation against an external force. The "rigidity" in the present invention includes, for example, the deformation coefficient. Here, the "deformation coefficient" is a quantity defined for materials that deform greatly against stress, such as soil (see, for example, "Methods and Explanations of Soil Testing," Soil Engineering Society (issued March 31, 1990)). Usually, the quantity calculated from the stress and strain amount at 1 / 3 of the maximum stress in the stress-strain curve of a material is called the elastic coefficient, but for materials that deform greatly, such as soil, the deformation coefficient calculated from the stress and strain amount at 1 / 2 of the maximum stress in the same stress-strain curve is considered to be good for evaluating the characteristics (see paragraph 0008 of Japanese Patent No. 3372012). Effect of the Invention

[0011] According to the present invention, the stiffness measurement unit of the testing device used in the compaction test of soil material measures the stiffness of the soil material in the container based on the output from the acceleration sensor attached to the weight. Therefore, the stiffness can be measured during the compaction test. [Brief description of the drawings]

[0012] [Figure 1]FIG. 1 is a diagram showing a schematic configuration of a test device according to an embodiment of the present invention. [Diagram 2] FIG. 1 shows a schematic configuration of a stiffness measurement unit constituting a testing device. [Diagram 3] Flowchart showing the method for measuring the deformation modulus of soil material [Figure 4] Figure showing the impact acceleration waveform during compaction [Diagram 5] A diagram showing the relationship between the deformation modulus of soil materials and the apparent deformation modulus. [Figure 6] A flow chart illustrating an example of a method for characterizing geological materials. [Figure 7] A diagram showing the compaction position (weight drop position) in the first compaction test [Figure 8] A graph showing the relationship between the number of cycles, water content, and deformation modulus obtained in the first compaction test. [Figure 9] FIG. 1 is a diagram showing a first compaction curve obtained in a first compaction test and a second compaction curve obtained in a second compaction test. [Figure 10] Normalized compaction curve [Figure 11] Graph showing compaction curves for each cycle in the first compaction test [Figure 12] A diagram showing the relationship between the deformation modulus, moisture content, and dry density of soil materials [Figure 13] A diagram showing an example of how to use the diagram shown in FIG. 12. [Figure 14] A flowchart showing an example of a method for managing compaction of a compaction work area. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In addition, the same reference numerals are used to denote the same or corresponding parts throughout the drawings.

[0014] 1 and 2 show a schematic configuration of a test apparatus 10 according to an embodiment of the present invention. The test device 10 is used for a compaction test of soil material. Here, the compaction test of soil material is a test in which soil material is compacted with a predetermined compaction energy CEL, and a compaction curve (water content w and dry density ρ d This refers to a test that obtains a curve showing the relationship between the temperature and the resistance of the material, for example, performed indoors.

[0015] The test device 10 has a similar configuration to that of a test device used in, for example, JIS A 1210 (soil compaction test by tamping). That is, the test device 10 includes a container (mold) 12 capable of containing a sample 11 made of a soil material, and a weight (rammer) 13 to be dropped onto the sample 11 contained in the container 12. In a compaction test of soil material, the weight 13 is repeatedly dropped freely from a specified height onto the sample 11 contained in the container 12 to perform compaction. The sample 11 used in this compaction test may be, for example, one sampled in a compaction work area described below.

[0016] In this embodiment, an example of the soil material is a soil having a gravel content of about 52% (mass), a sand content of about 22% (mass), and a fine grain content of about 26% (mass), and a soil particle density of about 2.8 g / cm 3 However, the composition of the soil material is not limited to this.

[0017] The container 12 has a cylindrical shape extending in the vertical direction. The container 12 has an open upper surface 12a and an opening on a lower surface 12b which is closed by a bottom plate .

[0018] The weight 13 is made of metal and has a cylindrical shape extending in the vertical direction. The actual bottom surface 13a of the weight 13 is a flat surface. The lower end of a handle 15 extending in the vertical direction is attached to the upper end of the weight 13.

[0019] In this embodiment, an acceleration sensor (accelerometer) 16 is attached to weight 13, and weight 13 and acceleration sensor 16 behave as one unit. Acceleration sensor 16 is connected to stiffness measurement unit 20 via cable 17 attached to handle 15. Output from acceleration sensor 16 (e.g., an electrical signal corresponding to the measured acceleration) is sent to stiffness measurement unit 20 via cable 17. Note that, although the communication method between acceleration sensor 16 and stiffness measurement unit 20 is a wired method using cable 17 in this embodiment, it is not limited to the wired method and may be a wireless method.

[0020] The stiffness measuring section 20 constitutes the test device 10. In this embodiment, the deformation modulus E is given as an example of stiffness measured by the stiffness measuring section 20 and will be described below.

[0021] The stiffness measuring unit 20 has a first determining unit 20a and a second determining unit 20b. The first determining unit 20a has a function of determining the apparent deformation coefficient Er based on the output from the acceleration sensor 16. The second determining unit 20b has a function of determining the deformation coefficient E of the sample 11 (deformation coefficient E of the soil material) based on the apparent deformation coefficient Er. That is, the stiffness measuring unit 20 is configured to be able to measure the deformation coefficient E of the sample 11 (deformation coefficient E of the soil material) based on the output from the acceleration sensor 16. This measurement result can be stored in the memory unit 21 in association with, for example, the number of compactions (the number of times the weight 13 falls, the number of counts by the counting device). Note that the various data stored in the memory unit 21 may be displayed on a display unit (not shown), which is, for example, a display, or may be printed on a medium such as paper by a printing device (not shown) such as a printer.

[0022] FIG. 3 is a flowchart showing a method for measuring the deformation modulus E that can be implemented by the stiffness measuring section 20.

[0023] In the method of measuring the deformation coefficient E, first, in step S1, the first determination unit 20a determines the apparent deformation coefficient Er. Here, the method of determining the apparent deformation coefficient Er will be described with reference to FIG. 4 in addition to FIG. 1 to FIG. 3.

[0024] Fig. 4 is a diagram showing an impact acceleration waveform during compaction. By allowing weight 13 to freely fall from a specified height onto sample 11 contained in container 12, the acceleration sensor 16 acquires, for example, the impact acceleration waveform shown in Fig. 4. In this waveform, time T shown in Fig. 4 is the contact time of weight 13 with sample 11 (the impact wavelength when weight 13 lands). The apparent deformation coefficient Er can be calculated based on the following formula (1) based on Hertz's spherical contact theory, assuming that the bottom surface of weight 13 is a spherical surface (virtual spherical surface) 13b.

[0025]

number

[0026] Here, in formula (1), T: contact time of the weight 13 with the sample 11 (soil material) (shock wavelength when the weight 13 lands) α: constant (≒ 4.53) ν1: Poisson's ratio of weight 13 E1: Elastic coefficient of weight 13 ν2: Poisson's ratio of sample 11 (soil material) Er: Apparent deformation modulus of sample 11 (soil sample) M: Mass of weight 13 R: Radius of curvature of spherical surface 13b V0: Landing speed of weight 13 (=(2gh) 1 / 2 ,g:Gravity acceleration, h : Drop height) The radius of curvature R of the spherical surface 13b is equal to the radius of the actual bottom surface 13a which is a circular flat surface.

[0027] In formula (1), for the Poisson's ratio v2 of the sample 11 (soil material), a standard value according to the soil is used, so that if the contact time T can be obtained in formula (1), the apparent deformation coefficient Er of the sample 11 (soil material) can be obtained. In this manner, in step S1, the first specifying unit 20a specifies the deformation coefficient (i.e., the apparent deformation coefficient Er) of the sample 11 (soil sample) when it is assumed that the bottom surface of the weight 13 is a spherical surface 13b.

[0028] Next, in step S2, the second determination unit 20b determines the true deformation coefficient E based on the apparent deformation coefficient Er. In this embodiment, the true deformation coefficient E may correspond to the deformation coefficient E of the sample 11 (deformation coefficient E of the soil material) estimated using the weight 13 whose bottom surface 13a is a flat surface. To determine the deformation coefficient E, for example, a diagram showing the relationship between the deformation coefficient E and the apparent deformation coefficient Er shown in FIG. 5 may be used. FIG. 5 may be obtained, for example, by a prior experiment.

[0029] That is, in the stiffness measuring unit 20, the deformation coefficient (apparent deformation coefficient Er) when it is assumed that the bottom surface of the weight 13 is spherical 13b is determined by substituting the contact time T obtained from the impact acceleration waveform during compaction shown in Fig. 4 into the formula (1), and the deformation coefficient E estimated using the weight 13 whose bottom surface 13a is flat is determined by correcting this using Fig. 5. In this manner, the deformation coefficient E can be measured by the stiffness measuring unit 20.

[0030] FIG. 6 is a flow chart illustrating an example of a method for characterizing soil materials.

[0031] First, in step S11, a first compaction test including measurement of the deformation coefficient E is performed using the test device 10. In the first compaction test, the Ec method of JIS A 1210 (compaction energy CEL ≒ 2500 kJ / m 3; commonly known as 4.5Ec), a sample 11 is placed in a container 12 with an inner diameter of 15 cm in three layers, and each layer is compacted 92 times with a weight 13. Figure 7 shows the compaction positions, and for example, a commercially available automatic compaction device is used to move the compaction positions in the order of "1" to "7" shown in Figure 7 (this is repeated for 13 cycles for each layer, ending at position "1"), and the deformation coefficient E is measured each time at position "7".

[0032] Fig. 8 is a diagram showing the relationship between the number of cycles N, the moisture content w, and the deformation modulus E obtained in the first compaction test. In order to obtain the relationship diagram in Fig. 8, the moisture content w of sample 11 was adjusted to six types shown in Fig. 8 in the above-mentioned step S11. The number of cycles N shown in Fig. 8 is for any one of the above-mentioned three layers, for example the top layer (third layer).

[0033] Next, in step S12, a second compaction test is carried out. In the second compaction test, the same sample as in the first compaction test (not necessarily the same as long as the soil quality is the same) is subjected to the Bc method of JIS A 1210 (compaction energy CEL ≒ 550 kJ / m 3 ; commonly known as 1Ec), a normal compaction test is performed. That is, in step S12, a second compaction test is performed with a compaction energy CEL different from that of the first compaction test. Note that step S12 may be performed prior to step S11, or may be performed in parallel with step S11. Note that in this embodiment, since the actual bottom surface 13a of the weight 13 is a flat surface, the sample in the container 12 can be uniformly compacted.

[0034] 9 is a diagram showing a first compaction curve L1 obtained in the first compaction test in step S11 and a second compaction curve L2 obtained in the second compaction test in step S12. Here, the first compaction curve L1 is a curve showing the relationship between the moisture content w and the dry density ρ d The second compaction curve L2 is a curve showing the relationship between the moisture content w and the dry density ρ obtained in the second compaction test. dFig. 9 shows the relationship between the compaction energy CEL, the water content w, and the dry density ρ d In addition, FIG. 9 shows a curve indicating saturation Sr=100% and a curve indicating the optimum saturation (Sr). opt A curve showing the relationship is shown.

[0035] Next, in step S13, compaction curves F1 to F13 (see FIG. 11 described later) for each cycle in the first compaction test (for example, in the uppermost layer) are estimated. Here, the compaction curves F1 to F13 are compaction curves in the middle of the first compaction test, that is, the moisture content w and the dry density ρ d This is a curve showing the relationship between

[0036] The method of estimating the compaction curves F1 to F13 will be described below. This estimation method includes the items disclosed in Reference 1 below. Reference 1: Tatsuoka Fumio (2019): The significance of saturation and energy management in embankment compaction management, 54th Geotechnical Engineering Research Conference, 0352, pp.703-704.

[0037] First, the maximum dry density ρ of the first compaction curve L1 shown in Figure 9 dmax and the maximum dry density ρ of the second compaction curve L2 dmax Based on the ratio of the compaction energy CEL of the first compaction test to the compaction energy CEL of the second compaction test, the coefficient C of the following formula (2) (see Reference 1) is calculated. In this example, C=0.093.

[0038] ρ dmax4.5 / ρ dmax1 =1+C log 10 (CEL 4.5 / CEL1) …(2)

[0039] The subscripts "1" and "4.5" in formula (2) mean 1Ec and 4.5Ec, respectively. dmax4.5 / ρ dmax1 " is the maximum dry density ρ of the first compaction curve L1 dmaxand the maximum dry density ρ of the second compaction curve L2 dmax This is the ratio of CEL 4.5 / CEL1" is the ratio of the compaction energy CEL of the first compaction test to the compaction energy CEL of the second compaction test.

[0040] Next, using this calculated coefficient C, the compaction energy CEL at the Nth compaction cycle is calculated from equation (2). N Maximum dry density ρ dmax_N Here, the compaction energy CEL N is assumed to be proportional to the cumulative number of compactions up to the N-1 cycle, 7(N-1), plus 4 (the median number of compactions at the Nth cycle).

[0041] Next, for the first compaction curve L1 and the second compaction curve L2 shown in FIG. 9, the dry density ρ d The maximum dry density of each dmax The water content w on the horizontal axis is calculated as Sr-(Sr) using the following formula (3) based on the definition of the degree of saturation Sr. opt The normalized compaction curve Ls (see Reference 1) shown in Figure 10 is obtained by converting the

[0042] Sr = w / (ρ w / ρ d -ρ w / ρ s ) …(3)

[0043] Here, ρ w is the density of water, ρ s is the soil particle density. Optimum degree of saturation (Sr) opt is the peak of the compaction curve L1, L2 (maximum dry density ρ dmax ) corresponds to the degree of saturation Sr at the optimum saturation (Sr) for the same material. opt is assumed to be constant regardless of the compaction energy CEL (see Reference 1), and in this example, the average value of 1Ec and 4.5Ec (89.4%) is used.

[0044] Next, in the normalized compaction curve Ls shown in Figure 10, the vertical axis value ρ d / ρdmax (true compaction degree), and add this value to the maximum dry density ρ dmax_N Multiply by ρ to get the dry density d Calculate the optimum saturation (Sr) for each horizontal axis value. opt The degree of saturation Sr is calculated by adding the above and converting it to the water content w using formula (3), and the compaction curves F1 to F13 (see Figure 11) for each cycle (N = 1 to 13) are estimated. Figure 11 shows the estimated compaction curves F1 to F13 for each cycle (N = 1 to 13).

[0045] After estimating the compaction curves F1 to F13 for each cycle, in step S14, the deformation coefficient E, the moisture content w, and the dry density ρ d In this example, the intersections of the compaction curves F1 to F13 for each cycle (N = 1 to 13) shown in Figure 11 with the contour lines of the six types of moisture content w shown in Figure 8 (solid arrows in Figure 11) are calculated based on the moisture content w and dry density ρ d By considering it as such, the deformation modulus E, moisture content w and dry density ρ d Get the relationship with.

[0046] The deformation modulus E, moisture content w, and dry density ρ obtained in step S14 d An example of the relationship between the deformation modulus E, water content w, and dry density ρ of a soil material is shown in Figure 12. d FIG. 12 is a graph showing the relationship between the dry density ρ d The contours (isopleths) of the deformation coefficient E and the contours of the degree of saturation Sr are plotted on a plane with the horizontal axis representing the water content w. In Fig. 12, each value of the deformation coefficient E is indicated in italics.

[0047] An example of a method for plotting the contour of the deformation coefficient E shown in Fig. 12 will be described below. This example includes the disclosure of Reference 2 below. Reference 2: Tatsuoka, F.; Fujishiro, K.; Kawabe, S.; Kikuchi, Y.; Tateyama, K.; Nemoto, T. (2013): Series on Geotechnical Engineering and Technical Notes, Part 3: Compaction of Embankments (3), Foundation Works, September 2013, pp.103-106.

[0048] According to Reference 2, the deformation coefficient E is a function of the degree of saturation Sr, f(Sr), and the dry density ρ d Function f(ρ d ) can be expressed as the product of

[0049] E = f(Sr) f(ρ d ) …(4)

[0050] Here, the function f(Sr) has the same dimension as the deformation coefficient E, and the function f(ρ d ) is dimensionless. Also, the function f(ρ d ) and the function f(Sr) can be expressed by the following equations (5) and (6).

[0051] f(ρ d )=(ρ d / ρ w -a) b …(5) f(Sr)=t+(st)[1+exp{(u-Sr) / v}] …(6)

[0052] Here, a, b, s, t, u, and v are constants, and equation (6) is a Boltzmann function with a lower limit s and an upper limit t. The deformation coefficient E, moisture content w, and dry density ρ d The deformation coefficient E can be expressed as a formula by selecting the constants a, b, s, t, u, and v that are optimal for the group of data that constitutes the relationship between E and E. Using this formula, the contour of the deformation coefficient E shown in Figure 12 can be plotted.

[0053] Next, an example of how to utilize FIG. 12 will be described with reference to FIG. The deformation coefficient E, moisture content w, and dry density ρ shown in Fig. 12 dIn order to know the deformation coefficient E during on-site compaction using the relationship, it is necessary to clarify the relationship between the number of compaction times Nf and the compaction energy (synonymous with the compaction energy mentioned above) CEL. The method for this is to first carry out a compaction test at at least one type of moisture content w, and then calculate the dry density ρ at each number of compaction times Nf (for example, Nf = 2, 4, 6...) as shown diagrammatically by black triangles (▲) in Figure 13. d is calculated. In FIG. 13, points P2, P4, and P6 correspond to the number of compactions Nf=2, 4, and 6, respectively. Then, an in-situ compaction curve for each number of compactions Nf can be drawn based on the normalized compaction curve Ls so as to pass through these points. In FIG. 13, curves Q2, Q4, and Q6 are in-situ compaction curves corresponding to the number of compactions Nf=2, 4, and 6, respectively. This makes it possible to determine the relationship between the number of compactions Nf and the deformation coefficient E at an arbitrary moisture content w, and the relationship between the number of compactions Nf and the dry density ρ d and the maximum dry density ρ at each number of compaction times Nf. dmax_Nf and optimal water content w opt_Nf It is also possible to estimate the following:

[0054] FIG. 14 is a flow chart illustrating an example of a method for managing the compaction of a compaction work area made of soil material as described above.

[0055] First, in step S21, the water content w of the compaction area is measured (water content measuring step).

[0056] Next, in step S22, the deformation coefficient E of the compaction area is measured (stiffness measurement process). For example, a ground stiffness measuring device disclosed in JP 2015-151826 A or a compaction machine equipped with a stiffness measuring unit disclosed in JP 2019-2184 A may be used to measure the deformation coefficient E. Note that step S22 may be performed prior to step S21, or may be performed in parallel with step S21.

[0057] Next, in step S23, for example, the deformation coefficient E, the moisture content w, and the dry density ρ dBased on the relationship between the water content w and the deformation coefficient E measured in steps S21 and S22, the dry density ρ of the compaction area is calculated. d (dry density determination process).

[0058] In this way, by measuring the moisture content w and deformation modulus E of the compaction area, the dry density ρ d This makes it possible to grasp the degree of compaction, and ultimately makes it easy to carry out construction management using the degree of compaction (Dc value) as an indicator.

[0059] According to this embodiment, a test device 10 used in a compaction test of soil material includes a container 12 capable of containing a soil material (sample 11) and having an open top, a weight 13 to be dropped onto the soil material (sample 11) contained in the container 12, an acceleration sensor 16 attached to the weight 13, and a stiffness measuring unit 20 that measures the stiffness (e.g., deformation modulus E) of the soil material (sample 11) in the container 12 based on an output from the acceleration sensor 16. Therefore, the stiffness (e.g., deformation modulus E) can also be measured during the compaction test.

[0060] According to this embodiment, the bottom surface (actual bottom surface 13a) of the weight 13 is flat. The stiffness measuring unit 20 has a first determining unit 20a that determines the stiffness (e.g., apparent deformation coefficient Er) of the soil material (sample 11) in the container 12 when the bottom surface of the weight 13 is assumed to be a spherical surface 13b based on the output from the acceleration sensor 16, and a second determining unit 20b that determines the stiffness (e.g., deformation coefficient E) of the soil material (sample 11) in the container 12 when the bottom surface of the weight 13 is flat (when the actual bottom surface 13a) based on the stiffness (e.g., apparent deformation coefficient Er) of the soil material (sample 11) determined by the first determining unit 20a. Therefore, for example, a weight (rammer) used in JIS A 1210 can be used as it is for stiffness measurement.

[0061] According to this embodiment, the soil material characteristics The grasping method is to perform at least a first compaction test using the test device 10 to obtain the stiffness (e.g., deformation modulus E), the water content w, and the dry density ρ of the soil material. dThis includes acquiring the relationships between the items and the objects. Therefore, these relationships can be easily understood.

[0062] According to the present embodiment, the method for characterizing a soil material includes: determining the rigidity (e.g., deformation modulus E), the moisture content w, and the dry density ρ d In order to obtain the relationship between the above, multiple tamping tests (first tamping test and second tamping test) with different tamping energies CEL are performed. Therefore, the relationship between the above can be accurately understood.

[0063] According to this embodiment, the method for characterizing soil material includes estimating compaction curves F1-F13 (e.g., compaction curves F1-F13 for each cycle constituting the compaction test) during the compaction test based on the results (e.g., first compaction test and second compaction test) of multiple compaction tests with different compaction energies CEL (see FIG. 11). The number of estimated compaction curves is preferably determined according to the measurement frequency of the stiffness (e.g., deformation modulus E) measured by the test device 10.

[0064] According to the present embodiment, the method for characterizing the soil material includes determining the rigidity (e.g., deformation modulus E), the water content w, and the dry density ρ d This includes creating a diagram (see Figure 12) showing the relationship between the number of compaction times Nf and the deformation coefficient E at an arbitrary moisture content w, and the number of compaction times Nf and the dry density ρ d and the maximum dry density ρ at each number of compaction times Nf. dmax_Nf and optimal water content w opt_Nf It is also possible to estimate the above (see Figure 13).

[0065] According to the present embodiment, the method for managing compaction of the compaction area includes a moisture content measurement step (step S21) for measuring the moisture content w of the compaction area, a stiffness measurement step (step S22) for measuring the stiffness (e.g., the deformation modulus E) of the compaction area, and a dry density ρ of the compaction area. dThe dry density determination step (step S23) determines the stiffness (e.g., deformation modulus E), the moisture content w, and the dry density ρ d Based on the relationship between the water content and the stiffness (e.g., the deformation coefficient E) measured in the stiffness measurement step (step S22), the dry density ρ of the compaction area is calculated. d Therefore, by measuring the moisture content w and deformation modulus E of the compaction area, the dry density ρ d It is possible to grasp the following.

[0066] In this embodiment, the deformation coefficient E has been described as an example of "rigidity" in the present invention, but it is not limited to the deformation coefficient E and may be, for example, a spring constant or a reaction coefficient (see paragraph 0007 of Japanese Patent No. 3908031).

[0067] In the second compaction test in this embodiment, the above-mentioned test device 10 may be used, or a conventional test device used in JIS A 1210 may be used as is. That is, any test device may be used for the second compaction test as long as it is performed at a compaction energy CEL different from that of the first compaction test.

[0068] In this embodiment, the first compaction test involving measurement of stiffness and the second compaction test not involving measurement of stiffness are each performed once, but at least one of the first compaction test and the second compaction test may be performed multiple times. In addition, the first compaction test and the second compaction test may be performed three or more times in total, so that three or more compaction tests with different compaction energies CEL are performed.

[0069] In the first compaction test of this embodiment, when the above-mentioned automatic compaction test machine is used, since the test machine is equipped with a counting device (counter) that counts the number of drops, this may be linked to a data recording device so that acceleration measurement (acquisition of impact acceleration waveform) is performed only when data recording is required. This makes it possible to efficiently and reliably acquire data at the required timing. Of course, it goes without saying that data may be acquired at every timing when the weight falls.

[0070] It goes without saying that the illustrated embodiments are merely illustrative of the present invention, and that the present invention encompasses various modifications and variations that may be made by those skilled in the art within the scope of the claims, in addition to those directly shown in the described embodiments. The claims as originally filed were as follows: [Claim 1] A test device used for compaction testing of soil materials, comprising: A container capable of containing soil material and having an open top; A weight that is dropped onto the soil material contained in the container; An acceleration sensor attached to the weight; a stiffness measuring unit for measuring stiffness of the soil material in the container based on an output from the acceleration sensor; A test apparatus comprising: [Claim 2] The bottom surface of the weight is a flat surface, The stiffness measurement unit includes: A first determination unit that determines the rigidity of the soil material in the container based on an output from the acceleration sensor when the bottom surface of the weight is assumed to be spherical; A second identification unit that identifies the rigidity of the soil material in the container when the bottom surface of the weight is flat based on the rigidity of the soil material identified by the first identification unit; 2. The test device of claim 1, comprising: [Claim 3] A method for characterizing soil material, comprising: performing the compaction test using the testing apparatus according to claim 1 or 2 to obtain a relationship between the stiffness, water content, and dry density of the soil material. [Claim 4] The method for characterizing soil material according to claim 3, wherein the compaction test is carried out a plurality of times with different compaction energies to obtain the relationship. [Claim 5] 5. The method for characterizing soil material according to claim 4, further comprising estimating a compaction curve during the compaction test based on results of a plurality of compaction tests performed with different compaction energies. [Claim 6] 6. The method for characterizing soil materials according to claim 3, further comprising creating a diagram showing the relationship. [Claim 7] A method for managing compaction of a compaction work area, comprising: A moisture content measuring step of measuring the moisture content of the compaction construction area; A stiffness measuring step of measuring the stiffness of the compaction construction area; A dry density determination step of determining the dry density of the compaction area based on the relationship obtained by the characteristic determination method according to any one of claims 3 to 6, the moisture content measured in the moisture content measurement step, and the stiffness measured in the stiffness measurement step; (c) a method for controlling compaction; [Explanation of symbols]

[0071] 10...Test apparatus, 11...Sample (soil material), 12...Container (mold), 12a...Upper surface, 12b...Lower surface, 13...Sinker (rammer), 13a...Bottom surface, 13b...Spherical surface, 14...Bottom plate, 15...Handle, 16...Acceleration sensor (accelerometer), 17...Cable, 20...Stiffness measurement unit, 20a...First determination unit...20b...Second determination unit, 21...Memory unit, F1 to F13...Compaction curve, L1...First compaction curve, L2...Second compaction curve, Ls...Normalized compaction curve, P2, P4, P6...Point, Q2, Q4, Q6...Curve, R...Radius of curvature

Claims

1. A method for determining the characteristics of a soil material by performing a compaction test on the soil material using a test device, comprising: The test device comprises: A container capable of containing soil material and having an open top; A weight that is dropped onto the soil material contained in the container; An acceleration sensor attached to the weight; a stiffness measuring unit for measuring stiffness of the soil material in the container based on an output from the acceleration sensor; Equipped with The method comprises: performing a first compaction test at a first compaction energy, in which the soil material in the container is compacted by the weight repeatedly; obtaining a first compaction curve indicating a relationship between a moisture content and a dry density of the soil material in the first compaction test; measuring the stiffness of the soil material for each cycle in the first compaction test by the stiffness measuring unit; performing a second compaction test on the soil material at a second compaction energy different from the first compaction energy; Obtaining a second compaction curve showing a relationship between the moisture content and the dry density of the soil material in the second compaction test; Estimating a compaction curve for each cycle in the first compaction test based on the first compaction curve and the second compaction curve; obtaining a relationship between the stiffness, the moisture content, and the dry density of the soil material based on the relationship between the stiffness and the moisture content of the soil material for each cycle obtained in the first compaction test and the estimated compaction curve for each cycle in the first compaction test; A method for characterizing geological materials, comprising:

2. 2. The method of claim 1, further comprising producing a plot of the relationship between stiffness, moisture content and dry density of the soil material.

3. A method for characterizing soil materials as described in claim 2, wherein the diagram is a plane whose vertical axis represents the dry density of the soil material and whose horizontal axis represents the moisture content of the soil material, and on which is plotted isolines of the stiffness of the soil material and isolines of the degree of saturation of the soil material.

4. The bottom surface of the weight is a flat surface, The stiffness measurement unit includes: A first determination unit that determines the rigidity of the soil material in the container based on an output from the acceleration sensor when the bottom surface of the weight is assumed to be spherical; A second identification unit that identifies the rigidity of the soil material in the container when the bottom surface of the sinker is flat based on the rigidity of the soil material identified by the first identification unit; The method for characterizing soil material according to any one of claims 1 to 3, comprising:

5. A method for managing compaction of a compaction work area, comprising: A moisture content measuring step of measuring the moisture content of the compaction construction area; A stiffness measuring step of measuring the stiffness of the compaction construction area; A dry density determination process for determining the dry density of the compaction area based on the relationship between the stiffness, moisture content, and dry density of the soil material obtained by the soil material characteristic determination method according to any one of claims 1 to 4, the moisture content measured in the moisture content measurement process, and the stiffness measured in the stiffness measurement process; A method for controlling compaction, including:

Citation Information

Patent Citations

  • Simplified compaction testing machine and compaction testing method by tamping using the same

    JP2001324429A

  • Technique for measuring deformation characteristic of ground material based on contact time

    JP2002030643A

  • Compaction control method for developed ground

    JP2004150147A

  • Strength property measuring method, strength property measuring device, and program

    JP2009228352A

  • Cushioning material for underground pipe, and backfill method for the underground pipe using the same

    JP2016079710A

Cited By

  • Compaction management method and method for determining ground characteristics

    JP2026176043A