Temperature control mold, resin container manufacturing device and manufacturing method

The temperature adjustment mold with an eccentric tube structure addresses the challenge of selective preform temperature control, enabling precise cooling for forming uneven structures and uniform wall thickness in resin containers.

JP7595196B2Active Publication Date: 2024-12-05NISSEI ASB MASCH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023578514
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-02-01
Filing Date
2023-01-26
Publication Date
2024-12-05
Estimated Expiration
2043-01-26

AI Technical Summary

Technical Problem

Existing hot parison blow molding technologies struggle to selectively adjust the temperature of specific portions of a preform in the circumferential direction during the temperature adjustment process, making it difficult to form uneven structures like Braille or control wall thickness deviations in resin containers.

Method used

A temperature adjustment mold with an air introduction part and a cavity type that uses an inner and outer tube structure with eccentric positioning to control the opening width of air supply ports, allowing for selective temperature adjustment of preform portions through compressed air cooling.

Benefits of technology

Enables precise temperature control of specific preform areas, facilitating the formation of uneven structures and uniform wall thickness in resin containers by adjusting the flow rate of compressed air for targeted cooling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595196000001
    Figure 0007595196000001
  • Figure 0007595196000002
    Figure 0007595196000002
  • Figure 0007595196000003
    Figure 0007595196000003
Patent Text Reader

Abstract

This temperature regulating mold comprises: an air introduction unit that is inserted into a preform and introduces compressed air into the interior of the preform to cool the preform; and a cavity mold that accommodates the preform on the inside thereof, and contacts and undergoes heat exchange with the outer peripheral surface of the preform into which compressed air has been introduced. The air introduction unit has: an inner tube that evacuates the compressed air from the preform; an outer tube that is positioned at the outer periphery of the inner tube and, together with the inner tube, defines an air supply port that supplies the compressed air into the preform; and a positioning part that is formed at the outer periphery of the inner tube, and displaces the axial center of the inner tube with respect to the axial center of the outer tube so that the opening width of the air supply port changes along the circumferential direction thereof.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a temperature adjusting mold, and an apparatus and method for manufacturing a resin container. [Background technology]

[0002] A hot parison type blow molding machine has been known as one of the conventional manufacturing devices for resin containers. The hot parison type blow molding machine is configured to blow mold a resin container by utilizing the heat retained during injection molding of a preform, and is advantageous in that it can manufacture a variety of resin containers with excellent aesthetic appearance compared to the cold parison type.

[0003] In order to shorten the molding cycle of the hot parison type, for example, it has been proposed to shorten the injection molding time of the preform, which is the rate-limiting step (for example, the cooling time of the preform in the injection mold that takes place after the injection time (resin filling)), and to perform additional cooling of the hot preform in a temperature adjustment process after injection molding. Also, as a method for additional cooling of the preform, a method is known in which the outer peripheral surface of the preform is brought into contact with a cooling mold in the temperature adjustment process to exchange heat, and compressed air is blown into the preform to cool it (see Patent Documents 1 to 3). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 6505344 [Patent Document 2] International Publication No. 2020 / 158918 [Patent Document 3] Patent No. 2509042 Summary of the Invention [Problem to be solved by the invention]

[0005] For example, when forming a concave-convex structure such as Braille at a specific portion of the circumferential direction of the outer surface of the body of a container, it is preferable to adjust the specific portion so that it is difficult to stretch in the early stages of blow molding and stretch the specific portion in the later stages of blow molding. For example, it is preferable that the specific portion of the circumferential direction of the preform, which corresponds to the concave-convex structure of the container, is adjusted to a state where it is thicker than other portions and has sufficient heat retention for shaping when it is blown and contacts the blow mold. In order to achieve the above-mentioned stretching, it is necessary to selectively lower the temperature or heat retention of the specific portion of the preform in the temperature adjustment process (i.e., to lower the temperature or heat retention of the specific portion relatively to other portions). Also, when correcting unevenness in the circumferential thickness of the container body, it is desirable to adjust the temperature of a specific portion in the circumferential direction of the preform in the temperature adjustment step.

[0006] However, with this type of additional cooling of the preform, it is difficult to selectively adjust the temperature of a specific portion in the circumferential direction of the preform.

[0007] Therefore, the present invention has been made in consideration of such problems, and aims to provide a temperature adjustment mold that can adjust the temperature of specific parts in the circumferential direction of the preform when air cooling is performed in the temperature adjustment process. [Means for solving the problem]

[0008] One aspect of the present invention is a temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom. The temperature control mold includes an air introduction section that is inserted into the preform and introduces compressed air into the interior of the preform to cool the preform, and a cavity mold that houses the preform inside and exchanges heat by contacting the outer peripheral surface of the preform into which the compressed air has been introduced. The air introduction section includes an inner tube that exhausts the compressed air from the preform, an outer tube that is disposed on the outer periphery of the inner tube and forms an air inlet port between the inner tube and the outer tube for supplying compressed air to the preform, and a positioning section that is formed on the outer periphery of the inner tube and shifts the axis of the inner tube from the axis of the outer tube to change the opening width of the air inlet port in the circumferential direction. Effect of the Invention

[0009] According to one aspect of the present invention, it is possible to provide a temperature adjustment mold capable of adjusting the temperature of a specific portion in the circumferential direction of a preform when air-cooling is performed in a temperature adjustment step. [Brief description of the drawings]

[0010] [Figure 1] 1 is a diagram showing a schematic configuration of a blow molding device according to an embodiment of the present invention; [Diagram 2] FIG. 4 is a vertical cross-sectional view showing a configuration example of a temperature adjustment unit. [Diagram 3] FIG. 3 is a vertical sectional view showing a state in which the inner tube is modified from that shown in FIG. 2. [Figure 4] 2, and FIG. 3(b) is a cross-sectional view taken along line BB in FIG. [Diagram 5] FIG. 5 is a diagram showing a modified example of the inner tube in FIG. [Figure 6] 1 is a flow chart showing steps of a blow molding method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, in the drawings, the same elements are given the same reference numerals. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown only for illustrative purposes, and do not represent the actual shapes, dimensions, etc.

[0012] (Explanation of blow molding equipment) 1 is a diagram showing a schematic configuration of a blow molding apparatus 20 according to the present embodiment. The blow molding apparatus 20 according to the present embodiment is an apparatus of the hot parison type (also called one-stage type) that blow molds a container by utilizing the heat (internal heat, heat amount) retained during injection molding without cooling the preform to room temperature.

[0013] The blow molding apparatus 20 includes an injection molding section 21, a temperature adjustment section 22, a blow molding section 23, a removal section 24, and a conveying mechanism 26. The injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 are disposed at positions rotated a predetermined angle (e.g., 90 degrees) around the conveying mechanism 26.

[0014] The transport mechanism 26 includes a transfer plate 28 (not shown in FIG. 1) that moves so as to rotate around an axis perpendicular to the plane of the drawing in FIG. 1. On the transfer plate 28, one or more neck molds 27 (or neck mold fixing plates holding one or more neck molds, both not shown in FIG. 1) that hold the preform 10 or the neck portion 11 of the container are arranged at predetermined angles (for example, for each molding section). The transport mechanism 26 moves the transfer plate 28 by 90 degrees at a time, thereby transporting the preform 10 (or the container) with the neck portion 11 held by the neck mold 27, in this order, to the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24. The transport mechanism 26 further includes a mold opening mechanism for the neck mold 27, and the like.

[0015] (Injection molding section 21) The injection molding section 21 includes an injection cavity mold and an injection core mold, not shown, and manufactures the preform 10 shown in Fig. 2 and Fig. 3, which will be described later. An injection device 25 that supplies a resin material, which is a raw material of the preform 10, is connected to the injection molding section 21.

[0016] In the injection molding section 21, the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26 are closed to form a mold space having a preform shape. Then, a resin material is poured from an injection device 25 into the mold space having the preform shape, whereby the preform 10 is manufactured in the injection molding section 21.

[0017] Here, the overall shape of the preform 10 is a cylindrical shape with one end open and the other end closed at its bottom. As shown in Fig. 2 and Fig. 3 described later, the preform 10 has a neck portion 11 with an opening formed at one end, a body portion 12 connected to the neck portion 11 and formed into a cylindrical shape, and a bottom portion 13 connected to the body portion 12 and closing the other end.

[0018] The material of the container and the preform 10 is a thermoplastic synthetic resin, and can be appropriately selected according to the application of the container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan (registered trademark): a copolyester manufactured by Eastman Chemical Co.), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPSU (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), and PLA (polylactic acid). PET is preferable as the material of the preform 10 and the container in the present application.

[0019] Incidentally, even when the injection molding section 21 is opened, the neck mold 27 of the transport mechanism 26 is not opened, but continues to hold and transport the preforms 10. The number of preforms 10 simultaneously molded in the injection molding section 21 (i.e., the number of containers that can be simultaneously molded by the blow molding device 20) can be set appropriately.

[0020] (Temperature adjustment section 22) The temperature adjustment section 22 performs temperature equalization and temperature deviation removal for the preform 10 manufactured in the injection molding section 21, and adjusts the temperature of the preform 10 to a temperature suitable for blow molding (for example, about 90°C to 105°C) and a temperature distribution suitable for the container shape to be molded. The temperature adjustment section 22 also functions to cool the preform 10 in a high-temperature state after injection molding. When the preform 10 is made of PET, the outer surface temperature of the body 12 of the preform 10 reaches 120°C to 160°C during high-temperature demolding in the injection molding section 21 or when the preform is carried into the temperature adjustment section 22, and the inner part of the body 12 becomes even hotter than the outer surface. If PET in this temperature range is slowly cooled, crystallization (whitening) occurs, so it is necessary to rapidly cool the preform 10 in the temperature adjustment section 22 to suppress whitening.

[0021] 2 and 3 are vertical cross-sectional views showing a configuration example of the temperature adjustment unit 22. The temperature adjustment unit 22 shown in Fig. 2 has a cavity mold (temperature adjustment pot) 31 capable of accommodating the preform 10, and an air introduction member (also referred to as an air introduction / exhaust member) 32, as an example of a temperature adjustment mold.

[0022] The cavity mold 31 is a mold having a temperature-controlled space capable of accommodating the body 12 of the preform 10 produced in the injection molding section 21. The cavity mold 31 accommodates the body 12 and bottom 13 of the preform 10 in the temperature-controlled space. The bottom surface of the neck mold 27 that holds the neck 11 of the preform 10 is in contact with the upper surface of the cavity mold 31. The temperature-controlled space may be the same as or different from the external shape of the body 12 of the preform 10. An example of a case in which the temperature-controlled space of the cavity mold 31 and the external shape of the body 12 are different is when the size of the temperature-controlled space is larger than the size of the body 12 of the preform 10.

[0023] A flow path (not shown) through which a temperature control medium (coolant) flows is formed inside the cavity mold 31. Therefore, the temperature of the cavity mold 31 is maintained at a predetermined temperature by the temperature control medium. The temperature of the temperature control medium of the cavity mold 31 is not particularly limited, but can be appropriately selected within the range of, for example, 5°C to 90°C, preferably 30°C to 80°C.

[0024] The air introduction member 32 is a member that introduces and exhausts compressed air into the preform 10, and has a triple-tube structure in which an outer tube 42 and an inner tube 43 are concentrically inserted inside a cylindrical fitting core 41.

[0025] The fitting core 41 is a metal mold inserted into the neck mold 27. When inserted into the neck mold 27, the fitting core 41 comes into close contact with the inner circumference or upper end surface of the neck portion 11 of the preform 10, and keeps the preform 10 and the air introducing member 32 airtight. A circular opening (hollow space) into which an outer tube 42 can be inserted is formed along the axial direction inside the fitting core 41. The inner diameter of the opening of the fitting core 41 is larger than the outer diameter of the outer tube 42.

[0026] The outer tube 42 is a tube that is inserted and held in the opening of the fitting core 41, and forms a flow path for compressed air between the fitting core 41 and the outer tube 42. When the air introducing member 32 is inserted into the preform 10, the tip of the outer tube 42 is positioned below the neck portion 11 and toward the upper side of the body portion 12. In this embodiment, the flow path between the fitting core 41 and the outer tube 42 is used to exhaust the compressed air.

[0027] The inner pipe 43 is a pipe inserted inside the outer pipe 42 so as to be replaceable or so that the gap between the inner pipe 43 and the outer pipe 42 can be adjusted, and the outer diameter of the inner pipe 43 is smaller than the inner diameter of the outer pipe 42. The inner pipe 43 forms a flow path for compressed air between the outer pipe 42 and the inner pipe 43, and inside the inner pipe 43. In this embodiment, the flow path between the outer pipe 42 and the inner pipe 43 is used for supplying compressed air, and the flow path inside the inner pipe 43 is used for exhausting the compressed air.

[0028] The inner tube 43 has a small-diameter tip portion 43b that is inserted into the preform 10, and a base portion 43c that is connected to the base end side of the tip portion 43b and has a larger diameter than the tip portion 43b.

[0029] Further, a plurality of spacers 44 are provided on the outer periphery of the base 43c of the inner pipe 43, protruding in the radial direction and contacting the inner periphery of the outer pipe 42. As shown in Figs. 4(a) and (b), the spacers (position adjustment parts, protrusions) 44 are arranged, for example, three at intervals of 120 degrees in the circumferential direction, and each of them partially contacts the inner periphery of the outer pipe 42. As a result, the spacers 44 position the tip end 43b of the inner pipe 43 connected to the base 43c and hold it inside the outer pipe 42 without blocking the space (flow path of compressed air) between the base 43c of the inner pipe 43 and the outer pipe 42. The spacers 44 are an example of a positioning part.

[0030] In the temperature adjustment section 22, during cooling blowing, compressed air is introduced into the preform 10 through the opening 42a of the outer tube 42. The compressed air introduced into the preform 10 is then exhausted from the opening 41a of the fitting core 41 and the opening 43a at the tip 43b of the inner tube 43. The opening 42a of the outer tube 42 is an example of an air inlet. As a result, within the preform 10, a flow of compressed air is generated from the opening 42a of the outer tube 42 toward the neck 11, and a flow of compressed air is generated from the opening 42a of the outer tube 42 toward the bottom 13, and these compressed air flows cool the preform 10 from the inside.

[0031] In this embodiment, the amount of eccentricity of the tip 43b of the inner tube 43 with respect to the outer tube 42 can be adjusted. Specifically, the inner tube 43 is provided with a plurality of spacers 44 with different radial protrusion amounts. Then, by changing the spacer that contacts the outer tube 42, the tip 43b of the inner tube 43, which is inserted and disposed within the outer tube 42, is moved in the radial direction to adjust the amount of eccentricity. After adjusting the amount of eccentricity, the inner tube 43 and the outer tube 42 are connected to each other by fixing parts (not shown) provided above each tube so as not to be misaligned.

[0032] In addition, when adjusting the amount of eccentricity of the tip portion 43b of the inner tube 43 relative to the outer tube 42, multiple inner tubes 43 with different radial protrusion amounts of the spacer 44 may be prepared, and the amount of eccentricity of the tip portion 43b of the inner tube 43 relative to the outer tube 42 may be adjusted by replacing the inner tube 43 to be inserted into the outer tube 42 (see Figure 5).

[0033] 2 and 3 show examples in which different inner tubes 43 and 43' are inserted into the outer tube 42. Also, Fig. 4(a) is a cross-sectional view taken along line AA in Fig. 2, and Fig. 4(b) is a cross-sectional view taken along line BB in Fig. 3.

[0034] As shown in Fig. 4(a), the inner pipe 43 in Fig. 2 is configured so that the radial protrusion amount of the spacer 44 is uniform. Therefore, the tip end 43b of the inner pipe 43 is arranged concentrically so that the axis O2 coincides with the axis O1 of the outer pipe 42. In this case, as shown in Fig. 2, the tip end 43b of the inner pipe 43 is located in the center with respect to the outer pipe 42, and the radial distances between the tip ends 43b of the outer pipe 42 and the inner pipe 43 are approximately the same in the circumferential direction. In other words, the compressed air at the opening 42a of the outer pipe 42 flows evenly in the circumferential direction.

[0035] On the other hand, the inner pipe 43' in FIG. 3 is one embodiment of the inner pipe 43, and as shown in FIG. 4(b), the radial protrusion amount of the spacer 44' is non-uniform, and the protrusion amount of the spacer 44' on the right side in the figure is relatively smaller than the others. Here, the inner pipe 43' is rotated or moved horizontally relative to the outer pipe 42, so that the spacer 44' with a smaller protrusion amount is abutted against the inner circumferential surface of the outer pipe 42 and is arranged biased toward the right side in the figure. Then, as the inner pipe 43' moves in the radial direction, a deviation D occurs between the axis O2 of the inner pipe 43' and the axis O1 of the outer pipe 42. In this case, as shown in FIG. 3, the tip portion 43b' of the inner pipe 43' is located toward the right side in FIG. 3 with respect to the outer pipe 42, and the radial distance between the tip portion 43b' of the inner pipe 43' and the outer pipe 42 is maximum on the left side of FIG. 3 (opposite side of the deviation D) and decreases toward the right side of FIG. 3 (the side of the deviation D). That is, at the opening 42a of the outer pipe 42, the compressed air flows more toward the left side in FIG. 3, so that the flow of compressed air at the opening 42a of the outer pipe 42 is biased in the circumferential direction.

[0036] By forming the above-mentioned offset D, a portion where the flow rate of compressed air is increased by enlarging the gap between the tip portion 43b' of the inner tube 43' and the outer tube 44 can be locally formed. By circumferentially aligning the portion of the opening 42a with a specific portion of the body portion 12 of the preform 10 where the temperature or heat capacity is to be reduced, it becomes possible to realize appropriate temperature control, which was previously difficult. When three spacers 44' are provided in the inner tube 43', the length of at least one spacer 44' may be shorter in the radial direction than the other two, and the remaining two spacers 44' may be longer in the radial direction than the short spacer. In this case, the radial lengths of the two spacers 44' may be the same.

[0037] The spacers 44' may be configured so that all of them have different radial protrusions. For example, the spacer 44' having the largest radial protrusion may be brought into contact with the inner peripheral surface of the outer tube 42 to make the axis O2 of the tip end 43b' of the inner tube 43' and the axis O1 of the outer tube 42 concentric, or the smaller spacers 44' having different radial protrusions may be brought into contact with the inner peripheral surface of the outer tube 42 to adjust the misalignment D between the axis O2 of the tip end 43b' of the inner tube 43' and the axis O1 of the outer tube 42. The radial protrusions of the spacers 44' may be non-uniform, so that the entire spacer 44' is in contact with the inner peripheral surface of the outer tube 42. As a result, even if an inner tube 43' having a different radial protrusion amount of the spacer 44' is inserted (replaced) into the outer tube 42, it will be positioned biased toward the right in the figure with respect to the outer tube 42, and a deviation D will occur between the axis O2 of the inner tube 43' and the axis O1 of the outer tube 42. As a result, the flow rate of compressed air from the opening 42a where the deviation D is formed can be adjusted, making it possible to adjust the cooling strength of the preform 10 and increasing versatility.

[0038] FIG. 5 shows a configuration example in which the amount of eccentricity is adjusted by replacing the inner tube 43' as a modified example of the inner tube 43' shown in FIG. 5. In the inner tube 43' shown in FIG. 5, among the three spacers 44', the spacer 44' on the right side in the figure has a relatively small protruding amount, the remaining spacers 44' are equal in length, and all the spacers 44' abut the inner circumferential surface of the outer tube 42. In the configuration of FIG. 5, a deviation D occurs between the axis O2 of the inner tube 43' and the axis O1 of the outer tube 42, as in FIG. 4(b). In the configuration of FIG. 5, the magnitude of the deviation D is adjusted by replacing the spacer 44' with another inner tube 43' having a different protruding amount.

[0039] In the case of the configuration in Fig. 5, all of the spacers 44' abut against the outer tube 42, and the inner tube 43' is stably supported in an eccentric state by these spacers 44', improving the positioning accuracy of the inner tube 43'. In addition, with the configuration in Fig. 5, it is easy to adjust the portion where misalignment D occurs (i.e., the portion where a wide gap occurs between the outer tube 42 and the inner tube 43') in the circumferential direction by rotating the inner tube 43' relative to the outer tube 42, as shown by the double arrow in the figure.

[0040] (Blow molding section 23) Returning to FIG. 1, the blow molding section 23 performs stretch blow molding on the preform 10 whose temperature has been adjusted in the temperature adjustment section 22, to manufacture a container. The blow molding section 23 includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the container, a bottom mold, a stretch rod, and an air introduction member for supplying blow air (blow core mold, neither of which are shown). The blow molding section 23 blow molds the preform 10 while stretching it. This allows the preform 10 to be shaped into the shape of the blow cavity mold to manufacture a container.

[0041] (Removal part 24) The removal section 24 is configured to release the neck of the container manufactured in the blow molding section 23 from the neck mold 27 and remove the container to the outside of the blow molding apparatus 20.

[0042] (Explanation of the blow molding method) Next, a blow molding method using the blow molding apparatus of this embodiment will be described. Fig. 6 is a flow chart showing the steps of the blow molding method. In this embodiment, a mold adjustment step (S100) is performed before each step (S101 to S104) of the blow molding method, which will be described later, is performed.

[0043] (Step S100: Mold adjustment process) The mold adjustment step is a step of adjusting the amount of eccentricity of the inner tube 43 relative to the outer tube 42 of the temperature adjustment unit 22 in accordance with the shape of the container to be formed, etc. As an example, the following operations are performed in the mold adjustment step.

[0044] First, test molding is performed using the blow molding device 20 to obtain information on the container shape before adjustment. For example, during test molding, the temperature adjustment unit 22 aligns the axis O1 of the outer tube 42 with the axis O2 of the inner tube 43 as shown in FIG. 2. The blow molding device 20 is operated in the above state to obtain information on the temperature distribution of the preform 10 or the wall thickness distribution of the container before adjustment. Alternatively, if the container has an uneven structure such as Braille at a specific circumferential position, shape information on the uneven structure (information on the quality of formability) may be obtained.

[0045] If the result of the above test operation indicates that adjustment is required to the temperature distribution of the preform 10 or the thickness distribution of the container, the inner tube 43 of the temperature adjustment section 22 is moved relative to the outer tube 42, or the inner tube 43 is replaced, thereby adjusting the eccentricity of the inner tube 43 relative to the outer tube 42. Specifically, the inner tube is moved so that the spacer 44 with an appropriate protruding amount abuts against the inner peripheral surface of the outer tube 42, or the spacer 44 is replaced with an inner tube having a different shape. This causes the axis O2 of the tip end 43b of the inner tube 43 to be eccentric with respect to the axis O1 of the outer tube 42, thereby changing the opening amount of the opening 42 of the outer tube 42 in the circumferential direction.

[0046] Here, in order to suppress bias in the circumferential temperature distribution of the preform 10, the mold is adjusted so that a specific part of the preform 10 having a high temperature faces a part where the opening amount of the outer tube 42 is increased. In addition, for example, in order to form an uneven structure such as Braille on a container, the mold is adjusted so that a specific part of the preform 10 corresponding to the position where the uneven structure is formed faces a part where the opening amount of the outer tube 42 is increased.

[0047] In addition, when adjusting the mold to suppress bias in the thickness distribution based on the thickness distribution of the container, the thinner parts of the container can be regarded as higher temperature parts of the preform 10, and the thicker parts of the container can be regarded as lower temperature parts of the preform 10, and adjustments can be made in the same manner as described above. When the above-mentioned mold adjustment process is completed, each step of the blow molding method described below is carried out.

[0048] (Step S101: Injection molding process) First, in the injection molding section 21, resin is injected from the injection device 25 into a preform-shaped mold space formed by the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26, thereby producing the preform 10. Then, after the injection (filling and pressure holding) of the resin material is completed, or after a minimum cooling time has elapsed after the completion of the injection, the injection mold of the injection molding portion 21 is opened.

[0049] From the viewpoint of manufacturing a container in a high-speed molding cycle, it is preferable to open the mold in step S101 after the injection of the resin material (filling and pressure holding) is completed without providing a cooling time for the preform 10 in the injection mold.

[0050] On the other hand, when the preform 10 is cooled to a minimum extent in the injection mold, the time to cool the resin material after the injection of the resin material is completed in the injection molding section 21 (cooling time) is preferably 1 / 2 or less of the time to inject the resin material (injection time). The cooling time can be made shorter than the time to inject the resin material depending on the weight of the resin material. For example, the cooling time is more preferably 2 / 5 or less of the injection time of the resin material, even more preferably 1 / 4 or less, and particularly preferably 1 / 5 or less.

[0051] In this embodiment, there is no cooling time for the preform 10 in the injection mold (or the cooling time is very short), so compared to the case where the preform is sufficiently cooled in the injection mold, the skin layer (surface layer in a solidified state) of the preform is formed thin and the core layer (internal layer in a softened or molten state) is formed thick. In other words, in this embodiment, the thermal gradient between the skin layer and the core layer is large, and a preform 10 with high retained heat at high temperatures is molded.

[0052] When the injection mold is opened in step S101, the preform 10 is released from the injection cavity mold and the injection core mold at a high temperature that allows the outer shape to be maintained. After that, the transfer plate 28 of the transfer mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 in the high temperature state held by the neck mold 27 is transferred to the temperature adjustment unit 22.

[0053] (Step S102: Temperature adjustment process) Next, in the temperature adjustment section 22, cooling and temperature adjustment are performed to bring the temperature of the preform 10 close to a temperature suitable for the final blow (blow temperature). In the temperature adjustment section 22, the temperature of the preform 10 is lowered to the blow temperature, and thereafter, the temperature of the preform 10 is maintained at the blow temperature until blow molding is performed. By rapidly cooling the high-temperature preform in the temperature adjustment section 22, whitening (clouding) due to spherulite generation crystallization that may occur when the preform is slowly cooled is suppressed.

[0054] In the temperature adjustment section 22, first, the preform 10 is accommodated in the cavity mold 31. Next, the air introduction member 32 is inserted into the neck portion 11 of the preform 10 accommodated in the cavity mold 31. At this time, the neck portion of the preform 10 and the fitting core 41 are in close contact with each other, maintaining an airtight state between them.

[0055] Thereafter, a cooling blow is performed on the preform 10. In the cooling blow of this embodiment, compressed air is introduced into the preform 10 through an opening 42a at the tip of the outer tube 42. The compressed air introduced into the preform 10 is then exhausted from an opening 41a of the fitting core 41 and an opening 43a at the tip of the inner tube 43, respectively.

[0056] As a result, within the preform 10, a flow of compressed air is generated from the opening 42a of the outer tube 42 toward the neck 11, and a flow of compressed air is generated from the opening 42a of the outer tube 42 toward the bottom 13, and these compressed air flows cool the preform 10 from the inside.

[0057] In this embodiment, in the above-mentioned mold adjustment step (S101), the portion where the opening amount of the outer tube 42 is increased faces a specific portion in the circumferential direction of the preform 10. Therefore, a large amount of compressed air flows from the opening 42a of the outer tube 42 near the specific portion of the preform 10, and the specific portion is cooled more strongly than other portions in the circumferential direction.

[0058] Furthermore, the preform 10 in the temperature adjustment section 22 continues to be in contact with the cavity mold 31, which is maintained at a predetermined temperature by compressed air pressure from the inside, and heat exchange (i.e., cooling and temperature adjustment of the preform 10) also occurs between the preform 10 and the cavity mold 31. This adjusts the temperature of the preform 10 from the outside so that it does not fall below a temperature suitable for blow molding, and also reduces temperature deviations that occur during injection molding. Note that the shape of the preform 10 during the temperature adjustment process is maintained by the cavity mold 31 and does not change significantly.

[0059] After the temperature adjustment step, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate by a predetermined angle, and the preform 10 after temperature adjustment held by the neck mold 27 is conveyed to the blow molding section 23 .

[0060] (Step S103: Blow molding process) Next, in the blow molding section 23, the container is blow molded. First, the blow cavity mold is closed to accommodate the preform 10 in the mold space, and an air introduction member (blow core) for supplying blow air is lowered to bring the air introduction member into contact with the neck of the preform 10. Then, a stretching rod (vertical axis stretching member) is lowered to hold the bottom of the preform 10 from the inside, and while performing vertical axis stretching as necessary, blow air is supplied from the air introduction member to horizontally stretch the preform 10. As a result, the preform 10 is shaped by expanding so as to fit closely into the mold space of the blow cavity mold, and is blow molded into a container. Note that the bottom mold waits at a lower position where it does not come into contact with the bottom of the preform 10 before the blow cavity mold is closed, and quickly rises to the molding position before or after the mold is closed.

[0061] (Step S104: container removal process) When the blow molding is completed, the blow cavity mold and the bottom mold are opened, so that the container can be removed from the blow molding section 23. Next, the transfer plate 28 of the conveying mechanism 26 moves so as to rotate a predetermined angle, and the container is conveyed to the removal section 24. In the removal section 24, the neck of the container is released from the neck mold 27, and the container is removed to the outside of the blow molding apparatus 20.

[0062] This completes the series of steps in the blow molding method. Thereafter, the transfer plate 28 of the conveying mechanism 26 is moved so as to rotate by a predetermined angle, and the above steps S101 to S104 are repeated. When the blow molding apparatus 20 is in operation, four sets of containers are produced in parallel, with a time difference between each step.

[0063] Due to the structure of the blow molding apparatus 20, the time during which the transfer plate is stopped is the same in the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24. Similarly, the transport time of the transfer plate 28 between each section is also the same.

[0064] The effects of this embodiment will be described below. In the temperature adjustment section 22 of this embodiment, a high-temperature preform 10 that does not have time to cool in an injection mold (or has a very short cooling time) is placed in a cavity mold 31, and the preform 10 is cooled and its temperature adjusted by a cooling blow in which compressed air is blown into the preform 10 using an air introduction member 32. The air introduction member 32 has an inner tube 43 that exhausts compressed air from the preform 10, an outer tube 42 that is disposed on the outer periphery of the inner tube 43 and forms an opening 42a between the inner tube 43 and the outer tube 42 that supplies compressed air to the preform 10, and a spacer 44 that is formed on the outer periphery of the inner tube 43 and shifts the axis O2 of the inner tube 43 relative to the axis O1 of the outer tube 42 to change the opening width of the opening 42a in the circumferential direction. The circumferential change in the opening width of the opening 42a causes a difference in the flow rate of compressed air in the circumferential direction of the preform 10, making it possible to adjust the temperature by strongly cooling a specific portion of the preform 10 in the circumferential direction.

[0065] The present invention is not limited to the above-described embodiment, and various improvements and design changes may be made without departing from the spirit of the present invention.

[0066] In the above embodiment, an example was described in which the air introduction member 32 has a triple-tube structure consisting of the fitting core 41, the outer tube 42, and the inner tube 43, but the air introduction member 32 may be configured as a double-tube structure consisting of the outer tube 42 and the inner tube 43, with the outer tube 42 also functioning as the fitting core. In this case, compressed air is introduced from the neck side of the preform and exhausted from the inner tube on the bottom side of the preform.

[0067] In the above embodiment, a configuration example in which three spacers 44 are provided in the circumferential direction of the inner tube 43 has been described, but the shape, arrangement, and the like of the spacers 44 are not limited to the above. For example, the number of spacers 44 may be two or four or more, and an arc-shaped spacer 44 extending in the circumferential direction or a spacer 44 formed in a spiral shape on the inner tube 43 may be used. The spacers 44 may also be arranged staggered in the axial direction of the inner tube 43.

[0068] In addition, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0069] 10...preform, 20...blow molding device, 21...injection molding section, 22...temperature adjustment section, 23...blow molding section, 31...cavity mold, 32...air introduction member, 41...fitting core, 42...outer tube, 42a...opening, 43, 43'...inner tube, 44, 44'...spacer

Claims

1. A temperature control mold for controlling the temperature of an injection-molded resin preform having a bottom, an air introduction section that is inserted into the preform and introduces compressed air into the preform to cool the preform; a cavity mold that accommodates the preform inside and exchanges heat by contacting an outer peripheral surface of the preform into which the compressed air is introduced; The air introduction section is an inner tube for exhausting the compressed air from the preform; an outer tube disposed on an outer periphery of the inner tube and defining an air supply port between the outer tube and the inner tube for supplying the compressed air to the preform; a positioning portion formed on the outer periphery of the inner pipe, the positioning portion shifting an axis of the inner pipe relative to an axis of the outer pipe to change an opening width of the air inlet in a circumferential direction. Mold for temperature adjustment.

2. the inner tube has a plurality of positioning portions that come into contact with the outer tube at different eccentricities, The opening width of the air inlet is adjusted by changing the positioning portion of the inner pipe that contacts the outer pipe. The temperature regulating mold according to claim 1 .

3. the inner tube is replaceable with respect to the outer tube; The opening width of the air inlet is adjusted by replacing the inner pipe with one having a different positioning portion. The temperature regulating mold according to claim 1 .

4. an injection molding unit that injection molds a resin preform; A temperature adjustment section having the temperature adjustment mold according to claim 2 or 3 and adjusting the temperature of the preform manufactured in the injection molding section; a blow molding section for blow molding the temperature-controlled preform to manufacture a resin container. Plastic container manufacturing equipment.

5. A method for producing a resin container using the production apparatus according to claim 4, a die adjustment process for adjusting an opening width and a circumferential position of the air supply port in the temperature adjustment die; After the mold adjustment process, an injection molding step of injection molding the preform; a temperature adjustment step of adjusting the temperature of the preform manufactured in the injection molding step; a blow molding step of producing a resin container by blow molding the temperature-controlled preform; A method for manufacturing a resin container comprising the steps of:

Citation Information

Patent Citations

  • Process and device for producing plastic containers with preforms being cleaned

    DE102015111001A1

  • Preform temperature controller

    JP2509042B2

  • Resin container manufacturing method, mold unit, and molding machine

    JP6505344B1

  • Method for producing resin vessel made of resin, mould unit and moulding apparatus

    WO2019078358A1

  • Blow molding device, blow molding method, and mold unit

    WO2020138292A1