Control device, method for manufacturing three-dimensional object, and control program
A three-dimensional structure with controlled dense and porous regions formed from ceramic and chelating agent reaction addresses the challenge of achieving both high strength and bone integration, ensuring effective bone fusion and reinforcement.
Patent Information
- Application Number
- JP2020169561
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-07
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-10-07
AI Technical Summary
Existing three-dimensional structures made from ceramic materials face challenges in achieving both high density for strength and low density for facilitating new bone growth, with high density hindering fusion with living bone and low density providing insufficient reinforcement.
A three-dimensional structure is formed with dense and porous portions created from a reaction product of a ceramic material and a chelating agent, where the dense portion has a higher application of a curing liquid than the porous portion, allowing for controlled density variation.
The structure achieves high strength in both dense and porous areas, enabling effective fusion and reinforcement with living bone while allowing new bone growth.
Smart Images

Figure 0007595337000001 
Figure 0007595337000002 
Figure 0007595337000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a control device that controls the three-dimensional printing device based on shape data representing a three-dimensional shape of a three-dimensional object; 3D modeling using ceramic materials of It relates to a manufacturing method and a control program. [Background technology]
[0002] Artificial bones are three-dimensional objects formed using ceramic materials. Artificial bones are filled into bone defects caused by fractures and the like. Unlike artificial bones made from metal materials, artificial bones made from bioceramic materials can be replaced by living bones. That is, after filling a bone defect in a living body, artificial bones made from bioceramic materials can be fused to and replaced by the original bone through new bone growth.
[0003] In Patent Document 1, an artificial bone is formed by a powder layering method using powder aggregate of a ceramic material such as calcium phosphate, and then the artificial bone is immersed in an aqueous solution and subjected to a decompression treatment to replace the gas inside the artificial bone with the aqueous solution. The artificial bone is then left to stand to cause a hydration reaction, thereby improving the strength of the artificial bone. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 4575295 Summary of the Invention [Problem to be solved by the invention]
[0005] Conventionally, three-dimensional objects formed using ceramic materials need to have a high internal density in order to ensure strength, but in some cases a low density is preferable. When the three-dimensional object is an artificial bone, the internal density needs to be high in order to ensure the strength of the artificial bone, but if the density is too high, new bone growth is hindered, and it takes time to fuse with or replace living bone. On the other hand, if the density of the artificial bone is low, the strength required to reinforce living bone is insufficient.
[0006] Therefore, a main object of the present invention is to provide a three-dimensional object that can have both the characteristics of a high density and the characteristics of a low density, and also can have high strength.
[0007] A secondary object of the present invention is to provide an artificial bone which has both high strength and at least one of fusion with and replacement by natural bone. [Means for solving the problem]
[0008] In order to achieve the above object, a three-dimensional object according to the present invention has a dense portion formed to be dense on one side and a porous portion formed to be porous on the other side, the dense portion and the porous portion being formed from a reaction product of a ceramic material and a chelating agent. This three-dimensional object may be an artificial bone.
[0009] Further, a method for producing a three-dimensional object according to the present invention includes a layer forming step of forming a ceramic layer by using a powdered ceramic material, and a hardening liquid applying step of applying a hardening liquid containing a chelating agent to a target area of the layer, The layer forming step and the curing liquid applying step are repeated to form a three-dimensional object by a reaction product between the ceramic material and the chelating agent in the target area of the stacked layers; In the target range, the areas that will become one side and the other side of the three-dimensional object are defined as one side region and the other side region, respectively, and in the hardenable liquid application step, the amount of the hardenable liquid applied per unit area to the one side region is made greater than the amount of the hardenable liquid applied per unit area to the other side region.
[0010] A control program according to the present invention is a program for controlling a three-dimensional modeling apparatus, A layer forming process in which a ceramic layer is formed in a three-dimensional modeling device using a powdered ceramic material; a hardening liquid applying process for applying a hardening liquid including a chelating agent to a target area of the layer by the three-dimensional modeling apparatus; causing the computer to repeatedly execute the layer forming process and the curing liquid applying process, and causing the three-dimensional modeling device to form a three-dimensional model using a reaction product between the ceramic material and the chelating agent in the target range of the stacked layers; In the target range, the areas that will become one side and the other side of the three-dimensional object are defined as one side area and the other side area, respectively, and the computer is caused to execute the hardenable liquid application process so that the amount of the hardenable liquid applied per unit area to the one side area is greater than the amount of the hardenable liquid applied per unit area to the other side area. Effect of the Invention
[0011] The three-dimensional structure according to the present invention has a dense portion with a high density and a porous portion with a low density, so that it has both the characteristics of a high density portion and a low density portion. In addition, since the porous portion is formed by a reaction product of a ceramic material and a chelating agent, even the porous portion has high strength. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a schematic diagram illustrating an example of a three-dimensional object according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view taken along line II-II of FIG. [Diagram 3] 4 is a flowchart showing a method for manufacturing a three-dimensional object according to the present embodiment. [Figure 4A] 1A to 1C are explanatory diagrams of a method for producing a three-dimensional object. [Figure 4B] FIG. 11 is another explanatory diagram of the method for producing a three-dimensional object. [Diagram 5] FIG. 11 is a schematic diagram showing another example of a three-dimensional object according to the present embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described with reference to the drawings. In the drawings, the same reference numerals are used to designate the same parts, and duplicated explanations will be omitted.
[0014] (Structure of three-dimensional objects) Fig. 1 is a diagram showing an example of a three-dimensional object 10 in this embodiment. Fig. 1 shows a case where the three-dimensional object 10 is an artificial bone, but the three-dimensional object 10 is not limited to an artificial bone and may be used as a filter, a catalyst carrier, or the like, as described below. In the following, descriptions of the three-dimensional object 10 that are not specific to the artificial bone 10 apply to both the case where the three-dimensional object 10 is an artificial bone and the case where it is not.
[0015] The artificial bone 10 is filled into a defect portion 20a of a natural bone 20 in a living body (human or animal). FIG. 1 shows a state in which the artificial bone 10 is filled into a defect portion 20a of a natural bone 20 inside a human skin 2. The defect portion 20a may be, for example, a portion caused by an injury (e.g., a fracture) or a portion formed by osteotomy in orthopedic surgery. The natural bone 20 illustrated in FIG. 1 is a human femur, but the defect portion that can be filled with the artificial bone 10 according to this embodiment may be a defect portion of a human tibia, humerus, sternum, skull, or other bone, or may be a defect portion of a natural bone of an animal other than a human.
[0016] Fig. 2 is a cross-sectional view taken along line II-II of the artificial bone 10 in Fig. 1. Each cross-section of the artificial bone 10 in Fig. 1 parallel to the cross-section in Fig. 2 may be the same cross-section as Fig. 2.
[0017] The three-dimensional object 10 has a dense portion 3 formed as a dense material on one side (the right side in FIG. 2 ) and a porous portion 5 formed as a porous material on the other side (the left side in FIG. 2 ). In the three-dimensional object 10, the one side that becomes the dense portion 3 and the other side that becomes the porous portion 5 may be one end side and the other end side of the three-dimensional object 10 (the right side and the left side in FIG. 2 ), respectively, but are not limited to this, and may be, for example, the outer periphery side and the internal center side (or the internal center side and the outer periphery side) of the three-dimensional object 10.
[0018] The dense portion 3 and the porous portion 5 are formed by a reaction product between a ceramic material and a chelating agent. That is, the ceramic material hardens into the above-mentioned reaction product as a result of a chelating reaction with the chelating agent. More specifically, the chelating agent dissolves the ceramic material, and the chelating agent traps the calcium ions generated there, thereby obtaining the above-mentioned hardened reaction product. That is, in addition to the chelate reaction, the ceramic material is fixed after melting, thereby obtaining the above-mentioned reaction product. The chelate reaction means a chemical reaction in which a bidentate or more polydentate ligand forms a ring and bonds with a central metal. The chelating agent means a compound having a ligand (polydentate ligand) that forms the above-mentioned reaction product.
[0019] The dense portion 3 is a region whose density is equal to or higher than a first threshold value. The porous portion 5 is a region whose density is lower than a second threshold value. The density indicates the ratio (occupancy) of the space occupied by the constituent material (the reactant) in the three-dimensional object 10. Therefore, the density is 100% in a region in which the constituent material is completely packed so that no voids are generated. The first threshold value may be a value in the range of 70% or more and 90% or less (e.g., 80%), and the second threshold value may be a value in the range of 30% or more and 65% or less (e.g., 60%). The upper limit of the density of the dense portion 3 may be 100%. The lower limit of the density of the porous portion 5 may be a value in the range of 10% or more and 20% or less (e.g., 20%).
[0020] The three-dimensional model 10 may have an intermediate portion 7 between the dense portion 3 and the porous portion 5, which is formed by a reaction product of a ceramic material and a chelating agent. The density of the intermediate portion 7 is higher than that of the porous portion 5 and lower than that of the dense portion 3. The intermediate portion 7 is directly bonded to both the dense portion 3 and the porous portion 5. In one example, the density of the intermediate portion 7 gradually decreases as it moves from the dense portion 3 side to the porous portion 5 side (for example, from the boundary with the dense portion 3 to the boundary with the porous portion 5). In another example, the density may be uniform throughout the entire intermediate portion 7. When the intermediate portion 7 is not provided, the dense portion 3 and the porous portion 5 are directly bonded to each other.
[0021] The entire three-dimensional structure 10 may be formed mainly from the reactants. For example, the weight ratio of the reactants constituting the three-dimensional structure 10 to the total weight of the three-dimensional structure 10 may be 80% or more (or 90% or more) or 100% or less. When the three-dimensional structure 10 is an artificial bone, the artificial bone 10 may contain one or both of cells and growth factors described below as components other than the reactants.
[0022] The ceramic material may be a calcium phosphate, which may be, for example, α-tricalcium phosphate (α-TCP), β-tricalcium phosphate (β-TCP), octacalcium phosphate (OCP), or carbonate apatite, but is not limited to a particular calcium phosphate.
[0023] The chelating agent may be an organic compound having three or more phosphate or carboxyl groups per molecule, such as, but not limited to, etidronic acid, phytic acid, or citric acid.
[0024] The artificial bone 10 is filled into a defect portion 20a of a natural bone 20 to form a bone body 30 together with the natural bone 20. Fig. 1 shows an example of a state in which a bone body 30 is formed by a natural bone 20 and the artificial bone 10 filled into the defect portion 20a of the natural bone 20. The state in which the artificial bone 10 is filled into the defect portion 20a of the natural bone 20 will be simply referred to as a filled state below.
[0025] The artificial bone 10 has an outer surface 10a which becomes the outer surface of the bone body 30 in the filled state, and an inner surface 10b which is located inside the bone body 30 in the filled state. The outer surface of the bone body 30 is the surface facing the outside of the living body (the side of the skin 2). The outer surface 10a (e.g., the entire outer surface 10a) is formed by the dense portion 3, and the porous portion 5 forms the inner surface 10b (the portion of the inner surface 10b that does not belong to the dense portion 3). In the filled state, the inner surface 10b formed by the porous portion 5 is adjacent to (e.g., in contact with) the inner surface of the missing portion 20a, and the inner surface is formed by the living bone 20.
[0026] The dense portion 3 may have a plurality of inner surfaces 10b facing in different directions. In the example of Figs. 1 and 2, first to fifth inner surfaces 10b1 to 10b5 are formed as the inner surfaces 10b. The first inner surface 10b1 faces the opposite side to the outer surface 10a (left side in Fig. 2) and is adjacent to (in contact with) the bottom surface of the missing portion 20a among the inner surfaces that define the missing portion 20a. The second and third inner surfaces 10b2 and 10b3 are located between the first inner surface 10b1 and the outer surface 10a and face opposite sides to each other (upper and lower sides in Fig. 2). The fourth and fifth inner surfaces 10b4, 10b5 are located between the first inner surface 10b1 and the outer surface 10a, and between the second inner surface 10b2 and the third inner surface 10b3, and face opposite each other (upper and lower sides in Figure 1).
[0027] The number of the inner surfaces 10b is not limited to this example, and varies depending on the shape of the defect portion 20a to be filled with the artificial bone 10. The three-dimensional shaped object (artificial bone) 10 may have a rectangular parallelepiped, prism, cylinder, pyramid, cone, truncated cylinder, truncated pyramid, or flake shape. In the case of the artificial bone 10 having a prism or cylinder shape, one end face of the cylinder shape may be the outer surface 10a. In the case of the artificial bone 10 having a pyramid, cone, truncated cylinder, or truncated pyramid shape, the bottom face of the shape may be the outer surface 10a. In the case of the flake-shaped artificial bone 10, the artificial bone 10 may be filled in the defect portion 20a penetrating the skull (e.g., the calvarium) in the thickness direction, and in this case, one side surface facing the thickness direction of the artificial bone 10 is the above-mentioned outer surface 10a.
[0028] The artificial bone 10 may also contain cells and / or growth factors. The cells and growth factors are intended to promote the replacement of the artificial bone 10 with natural bone tissue, as will be described in more detail below.
[0029] (Method of manufacturing three-dimensional objects) FIG. 3 is a flowchart showing a method for producing a three-dimensional object (artificial bone) 10 according to an embodiment of the present invention.
[0030] In step S1, data on the three-dimensional shape of the three-dimensional object 10 to be produced (hereinafter, simply referred to as shape data) is created. When the three-dimensional object 10 is an artificial bone, in step S1, shape data representing the three-dimensional shape of the artificial bone 10 to be filled in the missing portion 20a of the living bone 20 is created based on the three-dimensional shape data of the missing portion 20a. The shape data may include data representing the three-dimensional ranges occupied by the dense portion 3, which is one side of the three-dimensional object 10, and the porous portion 5, which is the other side of the three-dimensional object 10. Furthermore, the shape data may include data representing the three-dimensional range occupied by the intermediate portion 7, which is the portion between the dense portion 3 and the porous portion 5 in the three-dimensional object 10.
[0031] The shape data may be created by a person operating an input device (such as a keyboard or a mouse) of a computer. When the three-dimensional object 10 is an artificial bone 10, for example, data of the three-dimensional shape of the missing portion 20a may be displayed on a computer display, and a person may create the shape data by operating an input device while viewing this data. The three-dimensional shape data of the missing portion 20a is three-dimensional shape data of a region including the missing portion 20a in the biological bone 20, and may be obtained by, for example, a CT scan. The three-dimensional shape data and shape data of the missing portion 20a may be, for example, CAD data.
[0032] In step S2, a modeling process is performed to produce a three-dimensional model 10 by powder layer deposition based on the shape data created in step S1. That is, in step S2, a three-dimensional modeling device 100 (3D printer) described later forms and hardens a layer of powdered ceramic material based on the shape data, performs the same process on the top surface of the hardened layer, and repeats the same process on the top surface of a newly hardened layer to form a three-dimensional artificial bone 10 made of multiple layers that are hardened and integrated. The above-mentioned shape data is composed of multiple slice data corresponding to these multiple layers, respectively.
[0033] FIG. 4A is an explanatory diagram of the modeling process, and shows a configuration example of a three-dimensional modeling apparatus 100 used in step S2. The three-dimensional modeling apparatus 100 in FIG. 4A manufactures a three-dimensional model 10 by a powder layer stacking method. The three-dimensional modeling apparatus 100 includes a modeling container 111 having a lifting bottom surface portion 111a at its bottom that moves up and down and into which a powdered ceramic material 2 (hereinafter also simply referred to as powder 102) is introduced, a powder introducing device 112 that introduces the powder 102 into the modeling container 111, and a hardening device 113 that partially hardens the powder 102 introduced into the modeling container 111. In addition, a storage device 114 that stores the shape data created in the above-mentioned step S1, and a control device 115 that controls the operation of the three-dimensional modeling apparatus 100 are provided.
[0034] Step S2 includes step S21, which is a layer forming step, and step S22, which is a curing liquid applying step. In step S2, the three-dimensional modeling apparatus 100 produces the three-dimensional model 101 by repeating steps S21 and S22 in this order.
[0035] In step S21, a ceramic layer is formed using the powder 102. For example, as shown in Fig. 4A, the control device 115 controls the powder introducing device 112 to introduce one layer of the powder 102 into the modeling container 111. At this time, the powder introducing device 112 introduces the powder 102 into the modeling container 111 so that the upper surface of the powder 102 introduced into the modeling container 111 is horizontal.
[0036] In the example of FIG. 4A, the powder introduction device 112 has a powder container 112a having a liftable bottom surface portion 112a1 in which the powder 102 is stored, and a roller 112b. The top surface of the powder container 112a is open. The control device 115 lifts the liftable bottom surface portion 112a1 by a distance corresponding to one layer. Next, as shown in FIG. 4A, the control device 115 moves the roller 112b horizontally from the opposite side of the opening of the powder container 112a to the modeling container 111 so as to cross this opening and the opening of the modeling container 111. As a result, one layer of the powder 102 that has risen from the opening of the powder container 112a is introduced into the modeling container 111. In this manner, one layer of the powder 102 is introduced into the modeling container 111, and the top surface of the introduced powder 102 is made horizontal.
[0037] In step S22, a hardening liquid containing a chelating agent (hereinafter also simply referred to as hardening liquid) is applied to a target area on the upper surface of the layer formed in step S21. For example, the control device 115 controls the hardening device 113 based on the above-mentioned slice data for one layer, so that the hardening device 113 applies the hardening liquid to the target area of the layer, as shown in Fig. 4B. As a result, the powdered ceramic material 102 in the target area becomes a hardened reactant as a result of a chelating reaction with the chelating agent contained in the hardening liquid.
[0038] In step S22, the amount of hardening liquid applied is controlled. That is, in the above-mentioned target range of the layer formed in step S21, the regions that will become one side portion and the other side portion of the three-dimensional object 10 are defined as one side region and other side region, respectively, and the amount of hardening liquid applied by the hardening device 113 per unit area to the one side region is made larger than the amount of hardening liquid applied by the hardening device 113 per unit area to the other side region based on the shape data. As a result, the one side region is hardened to form the dense layer portion 3, and the other side portion is hardened to form the porous portion 5.
[0039] In such a control of the amount of curing liquid applied, further, in the target range of the layer formed in step S21, a region between one side region and the other side region may be defined as an intermediate region, and the amount of curing liquid applied by the curing device 113 per unit area to the intermediate region may be set to be less than the amount of curing liquid applied by the curing device 113 per unit area to the one side region and more than the amount of curing liquid applied by the curing device 113 per unit area to the other side region. As a result, the intermediate region is cured to form an intermediate portion 7.
[0040] In controlling the amount of hardening liquid applied, the amount of hardening liquid applied by the hardening device 113 per unit area to a position may be changed depending on the position in the intermediate region. For example, the amount of hardening liquid applied by the hardening device 113 per unit area to a position may be gradually decreased as the position moves from one side region side to the other side region side in the intermediate region. This forms an intermediate region 7 whose density gradually decreases as it moves from the dense portion 3 side to the porous portion 5 side.
[0041] The above-mentioned control of the amount of curing liquid applied may be performed by the control device 115 based on the position ranges of the one side region, the other side region, and the middle region indicated by the shape data (slice data).
[0042] After step S22 is completed, the control device 115 lowers the lift-up bottom surface portion 111a by the thickness of one layer. Then, steps S21 and S22 are performed again. In this manner, steps S21 and S22 are repeated to form a three-dimensional object (artificial bone) 10 made of a reaction product between the ceramic material and the chelating agent. That is, the three-dimensional object 10 is formed by forming and hardening all layers corresponding to all slice data of the shape data. After all layers have been formed and hardened in this manner, the process proceeds to step S3.
[0043] In step S3, the three-dimensional object 10 formed in step S2 is removed from the modeling container 111, and the entire three-dimensional object 10 is washed with a liquid (e.g., water). For example, water is poured onto the three-dimensional object 10 to remove the residual chelating agent that did not contribute to the chelate reaction and other components contained in the hardening liquid (e.g., a surfactant, which will be described later) from the three-dimensional object 10.
[0044] The modeling process in step S2 described above will be described in more detail below.
[0045] <Ceramic material and hardening liquid> The powdered ceramic material 102 used in the above-mentioned step S21 may be calcium phosphate, which may be any of α-tricalcium phosphate (α-TCP), β-tricalcium phosphate (β-TCP), octacalcium phosphate (OCP), and carbonate apatite.
[0046] The hardening liquid used in step S22 is a liquid containing at least a chelating agent. This hardening liquid may be a chelating agent dissolved in water. The chelating agent is an organic compound having three or more phosphate groups or carboxyl groups per molecule. This organic compound may be any one of etidronic acid, phytic acid, and citric acid.
[0047] The hardenable liquid may contain other substances in addition to the chelating agent. For example, the hardenable liquid may further contain a surfactant.
[0048] <Examples of 3D modeling equipment> The three-dimensional modeling apparatus 100 may be an inkjet printer. That is, the above-mentioned curing device 113 of the three-dimensional modeling apparatus 100 may be a component of the inkjet printer. In this case, the above-mentioned curing liquid is used as the ink of the inkjet printer or instead of the ink. In this case, the curing device 113 is a movable carriage provided with a plurality of heads 113a that drip or spray the curing liquid.
[0049] In the above-mentioned step S22, the target range of the layer is controlled by the control device 115. of The carriage 113 is moved above along the target area, and the head 113a drops or sprays the hardening liquid onto each position in the target area, thereby applying the hardening liquid to the entire target area of the layer.
[0050] In this case, in controlling the amount of curable liquid applied in step S22, the control device 115 may control the amount of curable liquid applied as described above by making the number of heads 113a used to apply the curable liquid per unit area to the above-mentioned one-side region greater than the number of heads 113a used to apply the curable liquid per unit area to the above-mentioned other-side region.
[0051] Similarly, for the intermediate region, the control device 115 may control the amount of hardening liquid applied by making the number of heads 113a used to apply the hardening liquid per unit area to the intermediate region smaller than the number of heads 113a used to apply the hardening liquid per unit area to the one-side region and larger than the number of heads 113a used to apply the hardening liquid per unit area to the other-side region. In this case, the control device 115 may gradually reduce the number of heads 113a used to apply the hardening liquid per unit area to the intermediate region as the position moves from the one-side region side to the other-side region side in the intermediate region. This may form an intermediate region 7 whose density gradually decreases as it moves from the dense portion 3 side to the porous portion 5 side.
[0052] <Cells and growth factors> When the three-dimensional structure 10 is an artificial bone, in order to promote the replacement of the artificial bone 10 with the original bone tissue of the living bone 20 after filling the living bone 20 with the artificial bone 10, one or both of cells and growth factors may be added to the entire target area of the layer or a predetermined portion in step S22. The cells may be cells present in bone tissue (e.g., osteoblasts or osteoclasts), pre-differentiated stem cells, or one or both of these. The growth factors may be bone morphogenetic proteins (BMPs) that have a strong ability to induce bone regeneration, or may be basic fibroblast growth factor (b-FGF), transforming growth factor (TGFβ), insulin-like growth factor (IGF-1), or the like, which serve as cytokines that promote bone cell growth and matrix growth.
[0053] When cells are to be applied to the artificial bone 10, a cell-containing liquid containing cells is prepared. For example, the cell-containing liquid may be one in which cells are dispersed in liquid. In the above-mentioned step S22, the cell-containing liquid is dripped or sprayed onto the entire target area or a predetermined area of the layer from another head 113b provided on the above-mentioned carriage 113. This predetermined area may be, for example, the other side area that will become the porous portion 5.
[0054] When growth factors are to be applied to the artificial bone 10 in addition to the cells, the above-mentioned cell-containing liquid may contain the growth factors, or a growth factor-containing liquid containing the growth factors may be prepared separately from the above-mentioned cell-containing liquid. In the latter case, in the above-mentioned step S22, the growth factor-containing liquid is dripped or sprayed onto the entire target range or a predetermined region (for example, the above-mentioned other side region) of the layer from another head (not shown) provided on the above-mentioned carriage 113. Note that, when only growth factors out of the cells and growth factors are to be applied to the artificial bone 10, in the above-mentioned step S22, the above-mentioned growth factor-containing liquid is dripped or sprayed onto the entire target range or a predetermined region (for example, the above-mentioned other side region) of the layer from the head 113b provided on the above-mentioned carriage 113.
[0055] (Effects of the embodiment) The above-described three-dimensional structure 10 has the dense portion 3 with high density and the porous portion 5 with low density, and therefore has both the characteristics of a high density portion and the characteristics of a low density portion.
[0056] Since the porous portion 5 is formed from a reaction product between the ceramic material and the chelating agent, high strength can be obtained even in the porous portion 5. For example, when the three-dimensional structure 10 is an artificial bone, the porous portion 5 can obtain a strength of 25 to 30 MPa even if the density is 60%.
[0057] Furthermore, when the three-dimensional object 10 is an artificial bone, in a state where the artificial bone 10 is filled into the defect portion 20a of the natural bone 20 so that the artificial bone 10 and the natural bone 20 form a bone body 30, the dense portion 3, which has a strength higher than that of the porous portion 5, forms the outer surface of the bone body 30. Therefore, the dense portion 3 can reliably protect the defect portion 20a (i.e., the artificial bone 10 filled into the defect portion 20a) against external impacts.
[0058] In addition, in the above-mentioned filled state, the inner surface 10b formed by the porous portion 5 is adjacent to (e.g., in contact with) the inner surface of the defect portion 20a of the living bone 20. Therefore, new bone tissue (bone substance) from the living bone 20 can easily enter the artificial bone 10 from the inner surface of the defect portion 20a. Therefore, the artificial bone 10 having high fusion property and substitution property with the living bone 20 is realized.
[0059] Furthermore, in step S22 of the above-mentioned modeling process, the dense portion 3 and the porous portion 5 can be easily formed simply by changing the amount of hardening liquid applied to the layer of powder 102. Furthermore, the three-dimensional model 10 is formed from a reaction product between a ceramic material and a chelating agent, and the reaction product itself has high strength, making it possible to eliminate the need for a firing process or the like to increase strength.
[0060] An intermediate portion 7 may be provided between the dense portion 3 and the porous portion 5. In this case, the density of the intermediate portion 7 gradually decreases from the dense portion 3 side to the porous portion 5 side, thereby increasing the strength of the three-dimensional object 10.
[0061] (Control Program) A control program for performing the above-mentioned modeling process in step S2 may be stored in the storage device 114, or may be stored in another storage device that is readable by the computer serving as the control device 115.
[0062] The control program causes the computer 115 to execute a layer formation process for causing the 3D modeling apparatus 100 to form a ceramic layer using the powdered ceramic material 102. This layer formation process is a process for causing the 3D modeling apparatus 100 to perform the above-mentioned step S21.
[0063] The control program also causes the computer 115 to execute a hardenable liquid applying process that causes the three-dimensional modeling apparatus 100 to apply a hardenable liquid containing a chelating agent to the target range of the layer. This hardenable liquid applying process is a process that causes the three-dimensional modeling apparatus 100 to perform the above-mentioned step S22.
[0064] The control program causes the computer 115 to repeatedly execute the layer forming process and the curing liquid applying process. In this way, the computer 115 causes the three-dimensional modeling apparatus 100 to execute steps S21 and S22. of Have them do this repeatedly.
[0065] (Other examples of 3D objects) The above-mentioned three-dimensional model 10 may be something other than an artificial bone. For example, the three-dimensional model 10 may be a filter that collects particles in a passing fluid.
[0066] The filter 10 may be, for example, an exhaust gas purification filter, an air purification filter, or a liquid filter. The exhaust gas purification filter is provided in an exhaust flow path of a heat engine such as an internal combustion engine or a boiler, and captures particles contained in the exhaust gas from the heat engine. The air purification filter is provided in a flow path that circulates air inside a building, automobile, etc., and captures particles in the circulating air. The liquid filter captures particles (foreign matter) in liquids such as fuel and hydraulic oil.
[0067] Fig. 5 is a schematic diagram of a filter as a three-dimensional object 10. In filter 10, dense portion 3 and porous portion 5 are capable of passing a fluid. Porous portion 5 constitutes a filter portion on the upstream side of the passing fluid, and dense portion 3 constitutes a filter portion on the downstream side of the passing fluid. Furthermore, when filter 10 is provided with intermediate portion 7 as shown in Fig. 5, intermediate portion 7 also allows fluid to pass through.
[0068] In this configuration, the fluid flows into the filter 10 from the porous portion 5, passes through the porous portion 5, then passes through the intermediate portion 7, and then passes through the dense portion 3 before flowing out of the filter 10. During this process, particles in the fluid are collected by the filter 10. Among the particles in the fluid, larger particles are collected by the porous portion 5, medium-sized particles are collected by the intermediate portion 7, and small particles are collected by the dense portion 3.
[0069] After filter 10 has been used for a predetermined period of time, the particles accumulated in filter 10 may be removed, for example, by flowing pressurized water through filter 10 from the dense portion 3 side toward the porous portion 5 side, and filter 10 may be used again.
[0070] The three-dimensional object 10 may also be a catalyst carrier. In this case, the catalyst carrier 10 may have the same configuration as the above-mentioned filter (the configuration of FIG. 5). The catalyst carrier 10 supports a catalyst in its interior (for example, the porous portion 5, the intermediate portion 7, and the dense portion 3 in FIG. 5). The catalyst carrier 10 promotes a predetermined chemical reaction of a fluid (liquid or gas) passing through its interior. In the example of FIG. 5, the fluid flows from the porous portion 5 into the catalyst carrier 10, passes through the porous portion 5, then passes through the intermediate portion 7, and then passes through the dense portion 3, and flows out of the catalyst carrier 10. Alternatively, the fluid may pass through the catalyst carrier 10 in the reverse order.
[0071] In the example of FIG. 5, the porous portion 5, the dense portion 3, and the intermediate portion 7 are each cylindrical, but may be other shapes. In the example of FIG. 5, the overall shape of the filter 10 or the catalyst carrier 10 is cylindrical, but may be other shapes such as a prismatic shape. In the filter 10 or the catalyst carrier 10, the porous portion 5 may be cylindrical, the intermediate portion 7 may be cylindrical and provided so as to surround the outer circumferential surface of the porous portion 5, and the dense portion 3 may be cylindrical and provided so as to surround the outer circumferential surface of the intermediate portion 7. In this case, the fluid may flow into the porous portion 5 in its axial direction and then pass through the intermediate portion 7 and the dense portion 3 in that order in its radial direction.
[0072] In the case of the catalyst carrier 10, the dense portion 3 may be cylindrical, the intermediate portion 7 may be cylindrical and provided so as to surround the outer circumferential surface of the dense portion 3, and the porous portion 5 may be cylindrical and provided so as to surround the outer circumferential surface of the intermediate portion 7. In this case, the fluid may flow into the dense portion 3 in the axial direction, and then pass through the intermediate portion 7 and the porous portion 5 in that order in the radial direction.
[0073] The present invention is not limited to the above-described embodiment, and various modifications may be made within the scope of the technical concept of the present invention. For example, the three-dimensional structure 10 according to the embodiment of the present invention may not have all of the above-described features, or may have only some of the above-described features. [Explanation of symbols]
[0074] 2 skin, 3 dense part, 5 porous part, 7 middle part, 10 three-dimensional model (artificial bone), 10a outer surface, 10b inner surface, 20 living bone, 20a missing part, 30 bone body, 100 three-dimensional modeling device, 102 powdered ceramic material (powder), 111 modeling container, 111a lifting bottom part, 112 powder introduction device, 112a powder container, 112a1 lifting bottom part, 112b roller, 113 hardening device (carriage), 113a head, 113b head, 114 storage device, 115 control device (computer)
Claims
1. A control device that controls a three-dimensional printing device based on shape data representing a three-dimensional shape of a three-dimensional object, comprising: a layer forming step of forming a ceramic layer using a powdered ceramic material; a curing liquid applying step of applying a curing liquid including a chelating agent to a target area of the layer based on the shape data; by repeatedly executing the steps of the steps 1 to 4 in the three-dimensional printing apparatus, thereby forming the three-dimensional object by the reaction product of the ceramic material and the chelating agent in the target area of the stacked layers in the three-dimensional printing apparatus; and executing the hardenable liquid applying step in the three-dimensional modeling device, in which, in the target range of each layer, regions that will become one side portion and the other side portion of the three-dimensional model are defined as one side portion and the other side portion, respectively, and, based on the position ranges of each of the one side portion and the other side portion indicated by the shape data, the amount of the hardenable liquid applied per unit area to the one side portion is made larger than the amount of the hardenable liquid applied per unit area to the other side portion, thereby forming the one side portion into a dense dense portion and the other side portion into a porous porous portion; the ceramic material is calcium phosphate, the chelating agent is an organic compound having three or more phosphate groups or carboxyl groups per molecule, a control device for the three-dimensional object, the proportion of space occupied by the constituent material of the three-dimensional object being the density, the dense portion being a region where the density is equal to or greater than a first threshold value, and the porous portion being a region where the density is less than a second threshold value, the first threshold value being a value within the range of 70% or more and 90% or less, and the second threshold value being a value within the range of 30% or more and 65% or less.
2. A control device as described in claim 1, which causes the three-dimensional printing device to execute the hardening liquid application step of forming the intermediate portion into a portion having a density higher than that of the porous portion and lower than that of the dense portion by defining, in the target range of each layer, a region that is intermediate between the one side portion and the other side portion of the three-dimensional object as an intermediate portion, and setting, based on the respective positional ranges of the one side portion, the other side portion, and the intermediate portion indicated by the shape data, the amount of the hardening liquid applied per unit area to the intermediate portion less than the amount of the hardening liquid applied per unit area to the one side portion and more than the amount of the hardening liquid applied per unit area to the other side portion.
3. 3. The control device according to claim 1, wherein the density of the dense portion is 80% or more, and the density of the porous portion is less than 60%.
4. The control device according to any one of claims 1 to 3, wherein the calcium phosphate is any one of α-tricalcium phosphate (α-TCP), β-tricalcium phosphate (β-TCP), octacalcium phosphate (OCP), and carbonate apatite.
5. The control device according to any one of claims 1 to 4, wherein the organic compound is any one of etidronic acid, phytic acid, and citric acid.
6. The three-dimensional object is an artificial bone, The artificial bone is filled into a defect portion of a living bone to form a bone body together with the living bone, The artificial bone has an outer surface which is an outer surface of the bone body and an inner surface which is to be located inside the bone body, The control device according to any one of claims 1 to 5, wherein the outer surface is formed by the dense portion, and the porous portion forms the inner surface.
7. The control device according to claim 6 , wherein the inner surface formed by the porous portion is a surface adjacent to an inner surface of the defect portion formed by the living bone.
8. A control device as described in claim 6 or 7, which controls the three-dimensional printing device so that, in the hardening liquid application process, a cell-containing liquid containing cells, a cell-containing liquid containing both cells and growth factors, or a growth factor-containing liquid containing growth factors is dripped or sprayed onto the entire target range or a specified area of each layer.
9. A method for manufacturing a three-dimensional object based on shape data representing a three-dimensional shape of the three-dimensional object, comprising: a layer forming step of forming a ceramic layer using a powdered ceramic material; a curing liquid applying step of applying a curing liquid containing a chelating agent to a target area of the layer based on the shape data, The layer forming step and the hardening liquid applying step are repeated to form the three-dimensional object formed of a reaction product between the ceramic material and the chelating agent in the target area of the stacked layers; in the target range of each layer, regions that become one side portion and the other side portion of the three-dimensional model are defined as one side region and the other side region, respectively, and in the hardening liquid applying step, based on the position ranges of each of the one side region and the other side region indicated by the shape data, an amount of the hardening liquid applied per unit area to the one side region is made larger than an amount of the hardening liquid applied per unit area to the other side region, thereby forming the one side portion into a dense dense portion and the other side portion into a porous porous portion; the ceramic material is calcium phosphate, the chelating agent is an organic compound having three or more phosphate groups or carboxyl groups per molecule, a porous portion being a region where the density is less than a second threshold value, the dense portion being a region where the density is less than a second threshold value, the first threshold value being a value within the range of 70% or more and 90% or less, and the second threshold value being a value within the range of 30% or more and 65% or less.
10. A method for manufacturing a three-dimensional object as described in claim 9, wherein, in the target range of each layer, a region that is intermediate between the one side portion and the other side portion of the three-dimensional object is defined as an intermediate region, and in the hardening liquid applying step, based on the positional ranges of the one side portion, the other side portion, and the intermediate region indicated by the shape data, the amount of the hardening liquid applied per unit area to the intermediate region is less than the amount of the hardening liquid applied per unit area to the one side portion and more than the amount of the hardening liquid applied per unit area to the other side portion, thereby forming the intermediate portion into a portion having a density higher than that of the porous portion and lower than that of the dense portion.
11. The method for producing a three-dimensional object according to claim 9 or 10, further comprising a cleaning step of cleaning the three-dimensional object after forming the three-dimensional object.
12. A control program for controlling a three-dimensional printing device based on shape data representing a three-dimensional shape of a three-dimensional object, comprising: a layer forming process for forming a ceramic layer on the three-dimensional modeling apparatus using a powdered ceramic material; a hardening liquid applying process for applying a hardening liquid including a chelating agent to a target area of the layer based on the shape data by the three-dimensional modeling apparatus; causing the computer to repeatedly execute the layer formation process and the curing liquid application process, and causing the three-dimensional modeling device to form the three-dimensional model using a reaction product between the ceramic material and the chelating agent in the target range of the stacked layers; and causing the computer to execute the hardening liquid application process in which, in the target range of each layer, regions that will become one side portion and the other side portion of the three-dimensional model are defined as one side portion and the other side portion, respectively, and, based on the position ranges of each of the one side portion and the other side portion indicated by the shape data, the amount of the hardening liquid applied per unit area to the one side portion is made larger than the amount of the hardening liquid applied per unit area to the other side portion, thereby forming the one side portion into a dense dense portion and the other side portion into a porous porous portion; the ceramic material is calcium phosphate, the chelating agent is an organic compound having three or more phosphate groups or carboxyl groups per molecule, a control program for determining density of the three-dimensional object as the proportion of space occupied by a constituent material of the three-dimensional object, the dense portion being a region where the density is equal to or greater than a first threshold value, and the porous portion being a region where the density is less than a second threshold value, the first threshold value being a value in the range of 70% or more and 90% or less, and the second threshold value being a value in the range of 30% or more and 65% or less.
Citation Information
Patent Citations
Directional multi-stage-hole filter and preparation method thereof
CN104529505A
Sintered apatite compact having cellular surface and production thereof
JP1991261688A
Production of ceramic article of multilayer structure having dense layer and porous layer
JP1992305075A
Method of joining member for living body
JP2004224658A
Manufacturing method for medical implants made of calcium phosphate cement and medical implants
JP2007501054A