Anode-free solid-state battery adaptable to volume expansion
A porous lithium ion buffer layer in anode-free solid state batteries addresses the expansion issue by storing lithium ions, thereby reducing degradation and maintaining battery performance.
Patent Information
- Application Number
- JP2021567917
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-05-16
- Filing Date
- 2020-05-14
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-05-14
AI Technical Summary
Anode-free solid state batteries experience significant expansion during charging due to lithium ion deposition on the anode current collector, leading to potential degradation and cracking of components.
Incorporation of a porous lithium ion buffer layer between the anode current collector and the solid electrolyte layer to store lithium ions during charging, reducing expansion by accommodating ions within its porous structure.
Significantly reduces battery expansion and degradation by allowing lithium ions to be stored in the buffer layer, maintaining structural integrity and enhancing battery performance.
Smart Images

Figure 0007595357000001 
Figure 0007595357000002 
Figure 0007595357000003
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims the benefit of priority to U.S. patent application Ser. No. 16 / 414,748, filed May 16, 2019, the entire contents of which are incorporated by reference into this application for all purposes. [Background technology]
[0002]
[0002] Anode-free solid-state battery cells with high energy density and / or high power density tend to expand when charged. During charging, ions, such as lithium ions, migrate from the battery's cathode to the battery's anode through the battery's electrolyte. In the case of an anode-free solid-state battery, the anode current collector effectively serves the functions of both the anode and the current collector. When the battery cell is charged, ions can accumulate on the battery's anode current collector and occupy a substantial amount of volume. These ions can accumulate on the anode current collector, causing the battery cell to expand. This expansion can cause major problems. For example, the expansion can create pressure within the battery cell, possibly degrading components within the battery cell. This expansion can degrade the anode current collector over time, causing it to split, crack, or break apart, which can reduce the performance of the battery cell. Summary of the Invention [Means for solving the problem]
[0003]
[0003] Various configurations of anode-free solid-state battery cells are presented herein. The battery cell may include a cathode current collector layer. The battery cell may include a cathode, which is laminated with the cathode current collector layer. The battery cell may include a solid electrolyte layer. The battery cell may include a lithium-ion buffer layer. The solid electrolyte layer may be located between the cathode and the lithium-ion buffer layer. The lithium-ion buffer layer may be porous. The lithium-ion buffer layer may be in direct contact with the solid electrolyte layer. Lithium ions may be stored in the lithium-ion buffer layer during charging of the anode-free solid-state battery cell. The anode current collector may be in direct contact with the lithium-ion buffer layer.
[0004]
[0004] Such an embodiment of the anode-free solid-state battery cell may include one or more of the following features: The lithium-ion buffer layer may be conductive and flexible such that the anode-free solid-state battery cell can be rolled into a jelly-roll type battery cell. The anode current collector may be a copper foil layer. There may be a cylindrical battery cell housing. The cathode current collector layer, the cathode, the solid electrolyte layer, the lithium-ion buffer layer, and the anode current collector may be rolled together to form a jelly-roll type anode-free solid-state battery cell and inserted into the cylindrical battery cell housing. The lithium-ion buffer layer may be less than 20 μm thick. The lithium-ion buffer layer may be graphite. The power density of the anode-free solid-state battery cell may be at least 1000 watt-hours per liter. The energy density of the anode-free solid-state battery cell may be at least 400 watt-hours per kilogram. When the anode-free solid-state battery cell is fully charged, at least 80% of the lithium ions transferred through the solid electrolyte layer to the anode current collector may be stored in the lithium-ion buffer layer. The porosity of the lithium ion buffer layer may be greater than 70%. [Brief description of the drawings]
[0005] [Figure 1]
[0005] Certain embodiments of a battery cell are disclosed that include a buffer layer that provides structural storage for lithium ions. [Diagram 2]
[0006] 1 illustrates certain embodiments of charge-discharge cycles showing lithium deposition as the buffer layer builds up the lithium deposit. [Diagram 3]
[0007] 1 illustrates one embodiment of a charge-discharge cycle for a cross-section of a solid-state battery having a buffer layer that stores lithium ions. [Figure 4]
[0008] 1 illustrates an embodiment of a method for fabricating a battery cell that exhibits reduced amounts of expansion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0006]
[0009] To extend the life of an anode-free solid-state battery cell, the amount of expansion that occurs during a charging cycle may be reduced. Reducing the amount of expansion may slow the rate at which components within the battery cell degrade through charge-discharge cycles. For example, if copper foil is used for both the anode and anode current collector of an anode-free solid-state battery (SSB), the copper foil may be prone to cracking due to the expansion of the battery cell during one or more cycles. Furthermore, in a jelly-roll battery, the amount of expansion may be even greater because the layers of the battery cells may be rolled together and the battery cell layers may be repeated many times within the jelly-roll.
[0007]
[0010] To reduce the amount of expansion, a porous buffer layer may be formed between the anode current collector and the solid electrolyte. The buffer layer may need to meet several requirements, such as being conductive, flexible, thin, and porous enough to accommodate lithium ions. The buffer layer may act as a scaffold to provide a "storage" for the lithium ions during charging of the battery cell. Instead of the majority of the lithium ions depositing directly on the anode current collector, causing expansion between the anode current collector and the solid electrolyte, the lithium ions may deposit or otherwise be stored in the porous structure of the buffer layer. The buffer layer may be porous enough that there are voids to accommodate the lithium ions that migrate toward the anode current collector during charging. The ions fill these existing voids, thereby largely avoiding expansion. During discharge, as the lithium ions migrate through the solid electrolyte to the cathode, the voids in the buffer material are emptied again. Thus, the volume of the buffer material and the entire battery cell may exhibit less expansion with charge-discharge cycles when the buffer layer is present.
[0008]
[0011] Further details of such embodiments are provided with reference to the drawings. FIG. 1 shows an embodiment of a battery cell 100, which includes a buffer layer for structurally storing lithium ions. The battery cell 100 may be a solid-state battery cell. Furthermore, the battery cell 100 may be an anode-free battery cell, meaning that the anode current collector serves the functions of both the current collector and the anode. The battery cell 100 may include a cathode current collector 101, a cathode layer 102, a solid electrolyte layer 103, a buffer layer 104, and an anode current collector 105. Such a battery cell may be designed to have a power density of at least 1000 watt-hours per liter and / or an energy density of at least 400 watt-hours per kilogram.
[0009]
[0012] The battery cell 100 may be made by stacking the layers 101-105 together and rolling them into a "jelly roll" type battery cell. Once rolled, a cylindrical housing may be used to store the rolled layers of the battery cell 100. Because the battery cell 100 may be rolled, the layers 101-105 may need to be flexible so that the layers are not damaged by being rolled. Additionally, reducing expansion in a jelly roll type battery cell may be particularly advantageous since the layers of the battery cells are rolled together, i.e., any expansion that does occur may be compounded as the layers of the battery cells are repeated multiple times within the jelly roll.
[0010]
[0013] The cathode current collector 101 and the anode current collector 105 may be materials that are electrically conductive and electrochemically stable. The cathode current collector 101 may be a metal layer that is electrically conductive, does not react with the cathode layer 102, and is stable at the operating potential of the cathode layer 102. For example, the cathode current collector 101 may be made of aluminum. Typically, a thin aluminum foil may be used. Similarly, the anode current collector 105 may be a metal layer that is electrically conductive, does not react with the buffer layer 104, and is stable at the operating potential at which the anode current collector 105 functions (as the anode of the battery cell). For example, the anode current collector 105 may be made of copper. Typically, a thin copper foil may be used.
[0011]
[0014] The cathode layer 102 can be in direct contact with the cathode current collector 101. The cathode layer 102 can be various types of cathode materials. For example, the cathode layer 102 can be lithium nickel cobalt aluminum oxide ("NCA", LiNiCoAlO2). Other nickel-based cathodes are also possible, such as NCM622, NCM811, and OLO.
[0012]
[0015] The solid electrolyte layer 103 may be in direct contact with the cathode layer 102. The solid electrolyte layer 103 may be an organic or inorganic solid electrolyte in various forms. Possible electrolytes that may be used include LPS, LSPSC, LGPS, LBSO, LATSPO, LISICON, LICGC, LAGP, LLZO, LZO, LAGTP, LiBETI, LiBOB, LiTf, LiTF, LLTO, LLZP, LTASP, LTZP.
[0013]
[0016] A lithium-ion buffer layer 104 may be present between the solid electrolyte layer 103 and the anode current collector 105. The buffer layer 104 may be conductive, flexible, and highly porosity. The thickness of the buffer layer 104 may be between 100 nm and 30 μm. In some embodiments, the preferred thickness of the buffer layer 104 may be 5 μm. In particular, the thickness of the buffer layer 104 may be selected so as not to significantly increase the volume or weight of the battery cell 100. In particular, the thicker the buffer layer 104, the lower the energy and power density of the battery cell 100 may be. Thus, the thickness of the buffer layer 104 may be selected to balance the energy / power density with the ability to avoid expansion.
[0014]
[0017] The buffer layer 104 may have a high porosity, for example, 5% to 90%. In some embodiments, the porosity may be greater than 70%. The voids in the buffer layer 104 may help accommodate the lithium ions that migrate to the anode current collector 105 during charging. That is, the lithium ions fill the voids in the buffer layer 104 during and upon charging of the battery cell 100. Preferably, 50% to 95% of the lithium ions that migrate to the anode current collector 105 during charging remain in the buffer layer 104. The remaining 5% to 50% or less than 5% to 50% are deposited between the buffer layer 104 and the anode current collector 105, or are present or deposited between the solid electrolyte layer 103 and the buffer layer 104.
[0015]
[0018] The buffer layer 104 may be sufficiently flexible so that when the battery cell 100 is wound into a jelly roll, there is no or limited damage to the buffer layer 104. In particular, a strong electrical and physical interface between the material of the anode current collector 105 (e.g., copper) and the buffer layer 104 must remain.
[0016]
[0019] Materials with sufficient porosity, electrical conductivity, flexibility, and ability to interface with copper can include graphene, carbon black, acetylene black (AB), and Ketjen black (KB). These materials can be bound by one of the following binders: SBR-CMC, LiPAA, PvDF. The carbon can be in the form of fibers (i.e., carbon fiber) or in flake form. Other forms of carbon or other materials can also be used as the buffer layer 104. In manufacturing the battery cell 100, the buffer layer 104 can be deposited on the anode current collector 105.
[0017]
[0020] 2 illustrates an embodiment 200 of a charge / discharge cycle showing lithium ion storage when a buffer layer is present against the anode current collector. In embodiment 200, only a portion of the battery cell 100 is shown. In embodiment 200, a highly magnified representation of the anode current collector 105 and buffer layer 104 is shown.
[0018]
[0021] In the uncharged state 210, the buffer layer 104 has few, if any, lithium ions present in the voids formed by the particles of the buffer layer 104. In the illustrated embodiment, the thickness of the buffer layer 104 is about 200 nm, as shown by thickness 211. Upon charging, lithium ions 201 fill the voids formed by the particles of the buffer layer 104, as shown by charged state 220. Thus, although the lithium ions are still deposited directly only on the anode current collector 105, the volume of the lithium ions is mostly present in the voids formed by the particles of the buffer layer 104. In the illustrated embodiment, a slight expansion occurs due to the deposition of lithium ions. Thickness 221 is about 3% to 10% greater than thickness 211 because the amount of lithium ions exceeds the amount of space in the voids of the buffer layer 104. In other embodiments, the buffer layer 104 may be made thicker to fully or nearly fully accommodate the lithium ions when the battery cell is fully charged.
[0019]
[0022] After discharge, lithium ions migrate from the anode current collector 105 to the cathode. The expansion due to lithium ion deposition subsides and the thickness of the buffer layer 104 returns to approximately thickness 211. The amount of expansion when the buffer layer 104 is present may be much less than when the buffer layer 104 is not present and lithium ions can deposit on the anode current collector 105 due to the absence of a porous buffer.
[0020]
[0023] FIG. 3 illustrates one embodiment 300 of a charge-discharge cycle for a cross-section of a solid-state battery having a buffer layer for storing lithium ions.
[0021]
[0024] In the discharged state 310, the buffer layer 104 has few, if any, lithium ions present in the voids formed by the particles of the buffer layer 104. Thickness 302 represents the base thickness without any expansion due to lithium ion deposition. Similarly, thickness 301 represents the base thickness of the battery cell when no expansion is present. Upon charging, as shown in the charged state 320, the lithium ions fill the voids formed by the particles of the buffer layer, thus creating the buffer layer 104 and layer 330 including the lithium deposit. Thickness 303 may be slightly larger than thickness 302 because the deposition of lithium causes some amount of expansion. Thickness 303 may be about 3% to 10% larger than thickness 302 because the amount of lithium ions exceeds the amount of space in the voids of the buffer layer 104. Similarly, thickness 302 may be slightly larger than thickness 301 because the amount of lithium ions exceeds the amount of space in the voids of the buffer layer 104. In other embodiments, the buffer layer 104 may be made thicker so that it fully or nearly fully accommodates lithium ions when the battery cell is fully charged.
[0022]
[0025] During discharge, lithium ions migrate from the anode current collector 105, through the solid electrolyte layer 103, and into the cathode layer 102. Once all or most of the lithium ions have migrated, the discharged state 310 may re-exist. The expansion due to lithium ion deposition subsides, and the thickness of the buffer layer 104 returns to approximately thickness 302. Similarly, the thickness of the battery cell may return to thickness 301. The amount of expansion when the buffer layer 104 is present may be much less than when the buffer layer 104 is not present, and lithium ions may deposit on the anode current collector 105 due to the absence of a porous buffer.
[0023]
[0026] Various methods may be implemented to fabricate a battery cell having an ionic (e.g., lithium ion) buffer layer abutting an anode current collector of an SSB. FIG. 4 illustrates one embodiment of a method 400 for reducing battery cell expansion during charging. At block 405, an anode current collector layer may be fabricated. This anode current collector layer may be copper foil or any other form of conductive flexible layer, such as Ni, Fe, Ni+Fe, carbon fiber sheet, etc. The SSB may be an "anode-free" SSB, such that the anode current collector may function as both the anode and the anode current collector. At block 405, a buffer layer may be fabricated on the anode current collector. For example, carbon particles may be deposited on the anode current collector foil. The carbon layer may be 100 nm to 30 μm thick.
[0024]
[0027] At block 410, a solid electrolyte layer may be placed or deposited on the buffer layer. At block 415, a cathode and a cathode current collector may be placed or deposited on the solid electrolyte layer. In some embodiments, a first group of layers may be fabricated, including an anode current collector and a buffer layer. A second group of layers may be fabricated, including a cathode current collector, a cathode, and a solid electrolyte layer. The two groups of layers may then be laminated together. In other embodiments, the solid electrolyte layer may be included in the first group of layers rather than the second group of layers, or may instead be laminated between the two groups when the battery cell is assembled.
[0025]
[0028] At block 420, a cylindrical jelly roll solid-state battery may be fabricated by rolling the layers together. The resulting cylindrical jelly roll may be inserted into a cylindrical housing, such as a cylindrical canister, for storage. Electrical leads to the current collectors may be connected to the terminals of the battery cells.
[0026]
[0029] At block 425, the battery cell may be charged. Charging results in lithium ions migrating from the cathode to the anode current collector. At block 430, the ions are stored within the voids of the buffer layer directly adjacent to the anode current collector. Because the voids of the already-existing layers are filled with ions, the battery may expand much less than if the buffer layer were not present.
[0027]
[0030] At block 435, the battery may be discharged. Upon discharging, ions may migrate through the solid electrolyte to the cathode. Thus, the voids in the buffer layer may become empty again. Blocks 425-435 may be repeated multiple times. For example, such a battery cell may be incorporated as part of a battery module in an electric vehicle.
[0028]
[0031] For example, a battery cell fabricated by blocks 405-420 may be charged to 7559 Ah. The battery cell may be discharged to 6229 Ah with an initial coulombic efficiency of 82.4%. The battery may experience a radial volume expansion of approximately 86%.
[0029]
[0032] The methods, systems, and devices described above are examples. In various configurations, various procedures or components may be omitted, substituted, or added, as appropriate. For example, in alternative configurations, the methods may be performed in an order different from that described, and / or various stages may be added, omitted, and / or combined. Also, features described with respect to particular configurations may be combined in various other configurations. Different aspects and elements of the configurations may be combined in a similar manner. Also, technology evolves, and thus, many of the elements are examples and do not limit the scope of the disclosure or the claims.
[0030]
[0033] Specific details are provided in the description to provide a thorough understanding of the example configurations (including implementations). However, the configurations may be practiced without these specific details. For example, well-known circuits, processes, algorithms, structures, and techniques have been shown without unnecessary detail so as not to obscure the configurations. This description provides only example configurations and does not limit the scope, applicability, or configuration of the claims. Rather, the above description of the configurations provides one of ordinary skill in the art with an enabling description for implementing the described technology. Various changes may be made in the function and arrangement of elements without departing from the spirit or scope of the present disclosure.
[0031]
[0034] Also, the configurations may be described as processes that are depicted as flow diagrams or block diagrams. Although each may describe operations as a sequential process, many of the operations may occur in parallel or simultaneously. Additionally, the order of operations may be rearranged. A process may have additional steps not included in the figures.
[0032]
[0035] While several exemplary configurations have been described, various modifications, alternative configurations, and equivalents may be used without departing from the spirit of the disclosure. For example, the elements described above may be components of a larger system, and other rules may take precedence or otherwise vary in application of the invention. Also, numerous steps may be taken before, during, or after considering the elements described above.
Claims
1. 1. An anode-free solid-state battery cell, comprising: A cathode current collector layer; a cathode laminated with the cathode current collector layer; A solid electrolyte layer; A lithium ion buffer layer, the solid electrolyte layer is positioned between the cathode and the lithium ion buffer layer; The lithium ion buffer layer is porous and contains at least one of graphene, carbon black, acetylene black (AB), and Ketjen black (KB), and at least one binder of SBR-CMC, LiPAA, and PvDF, and has a porosity of more than 70% based on the porous material; the lithium ion buffer layer is in direct contact with the solid electrolyte layer; Lithium ions are stored in the lithium ion buffer layer when the anode-free solid-state battery cell is charged. A lithium ion buffer layer; an anode current collector in direct contact with the lithium-ion buffer layer; 1. An anode-free solid-state battery cell comprising:
2. 10. The anode-free solid-state battery cell of claim 1, wherein the lithium-ion buffer layer is electrically conductive and flexible such that the anode-free solid-state battery cell can be rolled into a jelly-roll type battery cell.
3. 3. The anode-free solid-state battery cell of claim 2, wherein the anode current collector is a copper foil layer.
4. 4. The anode-free solid-state battery cell of claim 3, wherein the anode-free solid-state battery cell further comprises a cylindrical battery cell housing, and the cathode current collector layer, the cathode, the solid electrolyte layer, the lithium-ion buffer layer, and the anode current collector are rolled together to form a jelly-roll type anode-free solid-state battery cell and inserted into the cylindrical battery cell housing. cell.
5. 5. The anode-free solid-state battery cell of claim 4, wherein the lithium-ion buffer layer has a thickness of less than 20 μm.
6. 6. The anode-free solid-state battery cell of claim 5, wherein the lithium-ion buffer layer is graphite.
7. 5. The anode-free solid-state battery cell of claim 4, having a power density of at least 1000 watt-hours per liter.
8. 5. The anode-free solid-state battery cell of claim 4, having an energy density of at least 400 watt-hours per kilogram.
9. 5. The anode-free solid-state battery cell of claim 4, wherein at least 80% of the lithium ions that migrate through the solid electrolyte layer to the anode current collector are stored in the lithium ion buffer layer when the anode-free solid-state battery cell is fully charged.
10. A method for manufacturing a battery cell, comprising: depositing a lithium ion buffer layer directly on the anode current collector; The lithium ion buffer layer is porous and contains at least one of graphene, carbon black, acetylene black (AB), and Ketjen black (KB), and at least one binder of SBR-CMC, LiPAA, and PvDF, and has a porosity of more than 70% based on the porous material; When the anode-free solid-state battery cell is charged, lithium ions are stored in the lithium ion buffer layer; and placing a solid electrolyte layer in direct contact with the lithium ion buffer layer; placing a cathode in contact with the solid electrolyte layer; placing a cathode current collector in contact with the cathode; A method for manufacturing a battery cell, comprising:
11. The method of claim 10 , wherein the lithium-ion buffer layer is conductive and flexible such that the anode-free solid-state battery cell can be rolled into a jelly-roll type battery cell.
12. fabricating a cylindrical jelly-roll type solid-state battery by winding together the anode current collector, the lithium ion buffer layer, the solid electrolyte layer, the cathode, and the cathode current collector. The method of claim 11 further comprising:
13. charging the battery cell; storing lithium ions migrating to the anode current collector using the buffer layer; and The method of claim 12 further comprising:
14. The method for manufacturing a battery cell according to claim 13, wherein the lithium ion buffer layer has a thickness of less than 20 μm.
15. The method of claim 14 , wherein the lithium ion buffer layer is graphite.
16. 16. The method of claim 15, wherein the anode-free solid-state battery cell has a power density of at least 1000 watt-hours per liter.
17. 17. The method of claim 16, wherein the anode-free solid-state battery cell has an energy density of at least 400 watt-hours per kilogram.
18. 20. The method of claim 17, wherein at least 80% of the lithium ions that migrate through the solid electrolyte layer to the anode current collector are stored in the lithium ion buffer layer when the anode-free solid-state battery cell is fully charged.
19. The method of claim 18 , wherein the anode current collector is a copper foil layer.
Citation Information
Patent Citations
Lithium ion battery before pre-doping and manufacturing method of lithium ion battery
JP2008192540A
Negative electrode for lithium battery, and lithium secondary battery using this
JP2011216193A
Lithium ion secondary battery
JP2013073846A
Negative electrode layer for lithium battery, lithium battery
JP2016115681A