Infrared absorbing composition, film, optical filter, solid-state imaging device, image display device, and infrared sensor

JP7651661B2Active Publication Date: 2025-03-26FUJIFILM CORP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023202375
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-03-01
Filing Date
2023-11-30
Publication Date
2025-03-26
Estimated Expiration
2041-05-10

AI Technical Summary

Benefits of technology

【0009】 本発明によれば、赤外線遮蔽性に優れた膜を形成できる赤外線吸収組成物、膜、光学フィルタ、固体撮像素子、画像表示装置および赤外線センサを提供することができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007651661000042
    Figure 0007651661000042
  • Figure 0007651661000001
    Figure 0007651661000001
  • Figure 0007651661000002
    Figure 0007651661000002
Patent Text Reader

Abstract

To provide an infrared-absorbing composition which can form a film excellent in an infrared shielding property.SOLUTION: An infrared-absorbing composition includes particles of an infrared-absorbing coloring agent and a solvent. The infrared-absorbing coloring agent is at least one kind selected from a pyrrolopyrrole compound having one or more groups expressed by a formula (1) and the groups expressed by a formula (2), and a squarylium compound having one or more groups expressed by the formula (1) and the groups expressed by the formula (2).SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an infrared absorbing composition containing an infrared absorbing dye. The present invention also relates to a film, an optical filter, a solid-state imaging device, an image display device, and an infrared sensor using the composition containing the infrared absorbing dye. [Background technology]

[0002] Video cameras, digital still cameras, and mobile phones with camera functions use solid-state imaging elements for color images, such as CCDs (charge-coupled devices) and CMOS (complementary metal-oxide semiconductors). These solid-state imaging elements use silicon photodiodes that are sensitive to infrared light in the light receiving section. For this reason, infrared cut filters are sometimes used to correct visibility.

[0003] The infrared cut filter is produced using a composition containing an infrared absorbing dye.

[0004] Patent Document 1 describes an invention relating to a resin composition containing an oxocarbon compound and a resin, in which an uncured product of the resin composition has one or more absorption peaks having a maximum absorption in the wavelength range of 600 nm or more and 1100 nm or less, and a cured product of the resin composition has more absorption peaks having a maximum absorption in the wavelength range of 600 nm or more and 1100 nm or less than the uncured product. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2018-041047 A Summary of the Invention [Problem to be solved by the invention]

[0006] In recent years, there has been a demand for further improvement in the spectral characteristics of films obtained using compositions containing infrared absorbing dyes. For example, there is a demand for the ability to block infrared rays over a wide wavelength range. As a result of the inventor's investigation of the composition described in Patent Document 1, it was found that there is still room for further improvement in these characteristics of this composition.

[0007] Therefore, an object of the present invention is to provide an infrared absorbing composition capable of forming a film having excellent infrared shielding properties, and also to provide a film, an optical filter, a solid-state imaging device, an image display device, and an infrared sensor using the infrared absorbing composition. [Means for solving the problem]

[0008] The present invention provides the following: <1> An infrared absorbing composition comprising particles of an infrared absorbing dye and a solvent, the particles in the infrared absorbing composition have two or more maximum absorption wavelengths in a wavelength range of 650 to 1500 nm, and the absorbance at the maximum absorption wavelength located on the shortest wavelength side in the above range is 0.6 to 2.0 when the absorbance at the maximum absorption wavelength located on the second shortest wavelength side is taken as 1. <2> The difference between the maximum absorption wavelength on the shortest wavelength side and the maximum absorption wavelength on the second shortest wavelength side in the above range is 30 to 80 nm. <1> The infrared absorbing composition according to claim 1. <3> The infrared absorbing dye is at least one selected from a pyrrolopyrrole compound, a squarylium compound, a pyrromethene compound, a croconium compound, and a cyanine compound. <1> or <2> The infrared absorbing composition according to claim 1. <4> An infrared absorbing composition comprising particles of an infrared absorbing dye and a solvent, an infrared absorbing composition, wherein the infrared absorbing dye is at least one selected from a pyrrolopyrrole compound having one or more groups represented by formula (1) and one or more groups represented by formula (2), and a squarylium compound having one or more groups represented by formula (1) and one or more groups represented by formula (2); [ka] In formula (1), R 1a represents an alkyl group, a halogen atom, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, or a cyano group; R 1b represents a substituent, and n1 represents an integer of 0 to 4; In formula (2), L 1 is an aliphatic hydrocarbon group, an aromatic hydrocarbon group, a heterocyclic group, -O-, -S-, -NR L1 R represents an n2+1-valent linking group consisting of -, -CO-, -COO-, -OCO-, -SO2- or a combination thereof; L1 represents a hydrogen atom, an alkyl group, or an aryl group; X 1 represents an acid group or a basic group, n2 represents an integer of 1 or more, and when n2 is 1, L 1 may be a single bond. <5> the maximum absorption wavelength on the shortest wavelength side of the particle is on the shorter wavelength side than the wavelength at which a dye solution obtained by dissolving the infrared absorbing dye constituting the particle in a good solvent for the infrared absorbing dye exhibits the largest absorbance; <1> ~ <4> 13. The infrared absorbing composition according to claim 12, <6> The particles have three or more maximum absorption wavelengths in the infrared absorbing composition in the wavelength range of 650 to 1500 nm. <1> ~ <5> 13. The infrared absorbing composition according to claim 12, <7> the number of maximum absorption wavelengths exhibited by the particles in the infrared absorbing composition in a wavelength range of 650 to 1500 nm is greater than the number of maximum absorption wavelengths exhibited by a dye solution in which the infrared absorbing dye constituting the particles is dissolved in a good solvent for the infrared absorbing dye in a wavelength range of 650 to 1500 nm; <1> ~ <6> 13. The infrared absorbing composition according to claim 12, <8> The infrared absorbing dye is a compound represented by formula (PP-1): <1> ~ <7> 1. An infrared absorbing composition according to claim 1 ; [ka] In the formula, R 1arepresents an alkyl group, a halogen atom, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, or a cyano group, R 1b represents a substituent, R 2 represents an alkyl group, an aryl group, or a heteroaryl group; R 3 , R 4 , R 5 and R 6 each independently represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, an arylsulfinyl group, or a heteroaryl group, R 7 and R 8 each independently represents a hydrogen atom, an alkyl group, an aryl group, a heteroaryl group, -BR 9 R 10 or a metal atom, R 9 and R 10 each independently represents a hydrogen atom, a halogen atom, an alkyl group, an alkenyl group, an aryl group, a heteroaryl group, an alkoxy group, an aryloxy group, or a heteroaryloxy group, R 9 and R 10 may be bonded to each other to form a ring, R 7 is R 3 or R 5 may be covalently or coordinately bonded to R 8 is R 2 , R 4 or R 6 may be covalently or coordinately bonded to L 1 is an aliphatic hydrocarbon group, an aromatic hydrocarbon group, a heterocyclic group, -O-, -S-, -NR L1 represents a n2+1-valent linking group consisting of -, -CO-, -COO-, -OCO-, -SO2- or a combination thereof, and when n2 is 1, L 1 may be a single bond, R L1 represents a hydrogen atom, an alkyl group, or an aryl group, X 1 represents an acid group or a basic group, n1 represents an integer from 0 to 4; n2 represents an integer of 1 or more, m represents an integer of 1 or more. <9> Further comprising a curable compound, <1> ~ <8> 13. The infrared absorbing composition according to claim 12, <10> For optical filters or inks, <1> ~ <9> 13. The infrared absorbing composition according to claim 12, <11> <1> ~ <9> A film using the infrared absorbing composition according to any one of claims 1 to 5. <12> <11> An optical filter comprising the film according to claim 1. <13> <11> A solid-state imaging device comprising the film according to claim 1. <14> <11> An image display device comprising the film according to claim 1. <15> <11> An infrared sensor comprising the film according to claim 1. Effect of the Invention

[0009] According to the present invention, it is possible to provide an infrared absorbing composition capable of forming a film having excellent infrared shielding properties, a film, an optical filter, a solid-state imaging device, an image display device, and an infrared sensor. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic diagram illustrating an embodiment of an infrared sensor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The present invention will be described in detail below. In this specification, the symbol "to" is used to mean that the numerical values ​​before and after it are included as the lower limit and upper limit. In the description of groups (atomic groups) in this specification, when there is no indication of substitution or non-substitution, the notation includes both groups (atomic groups) that have no substituents and groups (atomic groups) that have a substituent. For example, an "alkyl group" includes not only an alkyl group that has no substituents (unsubstituted alkyl group) but also an alkyl group that has a substituent (substituted alkyl group). In this specification, unless otherwise specified, "exposure" includes not only exposure using light but also drawing using particle beams such as electron beams and ion beams. Examples of light used for exposure include the bright line spectrum of a mercury lamp, far ultraviolet light represented by an excimer laser, extreme ultraviolet light (EUV light), X-rays, active rays or radiation such as electron beams. In this specification, "(meth)acrylate" refers to both or either of acrylate and methacrylate, "(meth)acryl" refers to both or either of acryl and methacryl, and "(meth)acryloyl" refers to both or either of acryloyl and methacryloyl. In this specification, the weight average molecular weight and the number average molecular weight are defined as values ​​calculated in terms of polystyrene as measured by gel permeation chromatography (GPC). In this specification, Me in the chemical formulae represents a methyl group, Et represents an ethyl group, Bu represents a butyl group, and Ph represents a phenyl group. In this specification, infrared rays refer to light (electromagnetic waves) with a wavelength of 700 to 2500 nm. In this specification, the total solids content refers to the total mass of all components of the composition excluding the solvent. In this specification, a pigment means a coloring material that is difficult to dissolve in a solvent. In this specification, the term "process" refers not only to an independent process, but also to a process that cannot be clearly distinguished from other processes, as long as the intended effect of the process is achieved.

[0012] <Infrared absorbing composition> A first aspect of the infrared absorbing composition of the present invention is An infrared absorbing composition comprising particles of an infrared absorbing dye and a solvent, The particles in the infrared absorbing composition are characterized in that they have two or more maximum absorption wavelengths in the wavelength range of 650 to 1500 nm, and the absorbance at the maximum absorption wavelength on the shortest wave side in the above range is 0.6 to 2.0 when the absorbance at the maximum absorption wavelength on the second shortest wave side is taken as 1.

[0013] The first aspect of the infrared absorbing composition of the present invention contains the above-mentioned particles, and thus can form a film having excellent infrared shielding properties that can shield infrared rays in a wide wavelength range. Furthermore, according to the first aspect of the infrared absorbing composition of the present invention, it is also possible to form a film that can shield infrared rays in a wide wavelength range using only one type of infrared absorbing dye, without using multiple types of infrared absorbing dyes.

[0014] One embodiment of particles that satisfy the above-mentioned spectral characteristics is an infrared absorbing dye particle having one or more groups represented by formula (1) and one or more groups represented by formula (2). Although the detailed reason why the above-mentioned spectral characteristics can be achieved by using infrared absorbing dye particles having such a structure is unclear, it is presumed to be due to the following. When an infrared absorbing dye is used by dissolving it in a solvent, it is able to move freely in the solution, and therefore only an absorption peak derived from a single molecule of the infrared absorbing dye is observed. Since the group represented by formula (2) is a group with a highly hydrophilic structure, it is presumed that during dispersion in the infrared absorbing composition, the side of the infrared absorbing dye having the group represented by formula (2) forms an association so that it faces the solvent side. And since the group represented by formula (1) has a substituent at the ortho position of the benzene ring, it is presumed that when the infrared absorbing dye has the group represented by formula (1), the infrared absorbing dyes are unlikely to overlap in parallel due to steric hindrance, and the transition moment is arranged at an angle, so that the infrared absorbing dyes are associated so as to be obliquely oriented with each other. It is presumed that particles of an infrared absorbing dye having one or more groups represented by formula (1) and one or more groups represented by formula (2) described below form such an association state (hereinafter also referred to as a specific state) in the infrared absorbing composition, whereby the absorption peak of the infrared absorbing dye shifts to the shorter or longer wavelength side, and as a result, an absorption peak derived from the specific state appears in addition to an absorption peak derived from a single molecule of the infrared absorbing dye, thereby achieving the above-mentioned spectroscopic characteristics.

[0015] In addition, a second aspect of the infrared absorbing composition of the present invention is An infrared absorbing composition comprising particles of an infrared absorbing dye and a solvent, The infrared absorbing dye is characterized in that it is at least one selected from a pyrrolopyrrole compound having one or more groups represented by formula (1) and one or more groups represented by formula (2), and a squarylium compound having one or more groups represented by formula (1) and one or more groups represented by formula (2).

[0016] The second aspect of the infrared absorbing composition of the present invention contains the above-mentioned particles, and thus can form a film having excellent infrared shielding properties capable of shielding infrared rays in a wide wavelength range. Also, the second aspect of the infrared absorbing composition of the present invention can form a film capable of shielding infrared rays in a wide wavelength range using only one type of infrared absorbing dye, without using multiple types of infrared absorbing dyes.

[0017] The infrared absorbing composition of the present invention can be used for ink (ink composition). Examples of the ink composition include printing ink and inkjet ink. When the infrared absorbing composition of the present invention is used as an ink composition, a solvent containing water can also be used. That is, the infrared absorbing composition of the present invention can also be used as an aqueous ink composition. When the infrared absorbing composition of the present invention is used as an ink composition, the solid content concentration of the infrared absorbing composition is preferably 0.1 to 50% by mass, more preferably 1 to 30% by mass.

[0018] The infrared absorbing composition of the present invention can also be used as a composition for an optical filter. Types of optical filters include infrared cut filters and infrared transmission filters. When the infrared absorbing composition of the present invention is used as a composition for an optical filter, it is preferable that the infrared absorbing composition of the present invention further contains a resin. When the infrared absorbing composition of the present invention is used as a composition for an optical filter, the solid content concentration of the infrared absorbing composition is preferably 1 to 70 mass%, more preferably 2 to 60 mass%. It is more preferably 5 to 50% by mass.

[0019] Hereinafter, each component used in the infrared absorbing composition of the present invention will be described.

[0020] <<Infrared absorbing pigment particles (specific particles)>> The infrared absorbing composition of the present invention contains particles of an infrared absorbing dye (hereinafter referred to as specific particles) that satisfy the following requirement 1 or 2.

[0021] (Requirement 1) Particles of an infrared absorbing dye, which particles in an infrared absorbing composition have two or more maximum absorption wavelengths in the wavelength range of 650 to 1500 nm, and the absorbance at the shortest maximum absorption wavelength in the above range is 0.6 to 2.0 when the absorbance at the second shortest maximum absorption wavelength is taken as 1. The absorbance at the shortest maximum absorption wavelength in the above range is preferably 0.8 to 1.8, and more preferably 1.0 to 1.6, when the absorbance at the second shortest maximum absorption wavelength is taken as 1.

[0022] (Requirement 2) Particles of an infrared absorbing dye, the infrared absorbing dye being at least one selected from a pyrrolopyrrole compound having one or more groups represented by formula (1) and one or more groups represented by formula (2), and a squarylium compound having one or more groups represented by formula (1) and one or more groups represented by formula (2). The infrared absorbing dye is preferably a pyrrolopyrrole compound having one or more groups represented by formula (1) and one or more groups represented by formula (2).

[0023] [ka] In formula (1), R 1a represents an alkyl group, a halogen atom, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, or a cyano group; R 1b represents a substituent, and n1 represents an integer of 0 to 4; In formula (2), L 1 is an aliphatic hydrocarbon group, an aromatic hydrocarbon group, a heterocyclic group, -O-, -S-, -NR L1 R represents an n2+1-valent linking group consisting of -, -CO-, -COO-, -OCO-, -SO2- or a combination thereof; L1 represents a hydrogen atom, an alkyl group, or an aryl group; X 1 represents an acid group or a basic group, and n2 represents an integer of 1 or more. When n2 is 1, L 1 may be a single bond.

[0024] R 1a The halogen atom represented by the formula (I) includes a fluorine atom, a chlorine atom, a bromine atom and an iodine atom. R 1a The number of carbon atoms in the alkyl group represented by is preferably 1 to 30, more preferably 1 to 20, further preferably 1 to 10, even more preferably 1 to 5, and particularly preferably 1 to 3. The alkyl group may be linear, branched, or cyclic, but is preferably linear or branched, and more preferably linear. R 1a The alkenyl group represented by the formula (I) preferably has 2 to 30 carbon atoms, more preferably 2 to 20 carbon atoms, further preferably 2 to 10 carbon atoms, and even more preferably 2 to 5 carbon atoms. R 1a The alkynyl group represented by the formula (I) preferably has 2 to 30 carbon atoms, more preferably 2 to 20 carbon atoms, further preferably 2 to 10 carbon atoms, and even more preferably 2 to 5 carbon atoms. R 1a The aryl group represented by the formula (I) preferably has 6 to 30 carbon atoms, more preferably has 6 to 20 carbon atoms, and further preferably has 6 to 12 carbon atoms. R 1aThe number of carbon atoms constituting the heteroaryl group represented by is preferably 1 to 30, more preferably 1 to 12. Examples of the types of heteroatoms constituting the heteroaryl group include nitrogen atoms, oxygen atoms, and sulfur atoms. The number of heteroatoms constituting the heteroaryl group is preferably 1 to 3, more preferably 1 to 2. The heteroaryl group is preferably a monocyclic or condensed ring, more preferably a monocyclic or condensed ring having 2 to 8 condensed rings, and even more preferably a monocyclic or condensed ring having 2 to 4 condensed rings. R 1a The alkyl group, alkenyl group, alkynyl group, aryl group and heteroaryl group represented by may further have a substituent. Examples of the substituent include the substituent T described below. The substituent is preferably a group other than the group represented by formula (2).

[0025] R in Equation (1) 1a is preferably an alkyl group, a halogen atom or an aryl group, more preferably an alkyl group or an aryl group, and further preferably an alkyl group.

[0026] R in Equation (1) 1b Examples of the substituent represented by include an alkyl group, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, an alkoxy group, an aryloxy group, a heteroaryloxy group, an acyl group, an alkylcarbonyl group, an arylcarbonyl group, an alkoxycarbonyl group, an aryloxycarbonyl group, an acyloxy group, an acylamino group, an alkoxycarbonylamino group, an aryloxycarbonylamino group, a sulfonylamino group, a sulfamoyl group, a carbamoyl group, an alkylthio group, an arylthio group, a heteroarylthio group, an alkylsulfonyl group, an arylsulfonyl group, a sulfinyl group, a ureido group, a hydroxy group, a mercapto group, a halogen atom, a cyano group, a nitro group, an imino group, and a silyl group, and it is preferable that the substituent is an alkyl group, an alkoxy group, an aryloxy group, or a halogen atom. These groups may further have a substituent. Examples of the substituent include the substituent T described later. It is preferable that the substituent is a group other than the group represented by formula (2).

[0027] In the formula (1), n1 represents an integer of 0 to 4, preferably an integer of 0 to 2, and more preferably 0.

[0028] L in Equation (2) 1 is an aliphatic hydrocarbon group, an aromatic hydrocarbon group, a heterocyclic group, -O-, -S-, -NR L1 R represents an n2+1-valent linking group consisting of -, -CO-, -COO-, -OCO-, -SO2- or a combination thereof; L1 represents a hydrogen atom, an alkyl group, or an aryl group. When n2 is 1, L 1 may be a single bond.

[0029] The number of carbon atoms in the aliphatic hydrocarbon group is preferably 1 to 20, more preferably 2 to 20, still more preferably 2 to 10, and particularly preferably 2 to 5. The aliphatic hydrocarbon group may be linear, branched, or cyclic. Furthermore, the cyclic aliphatic hydrocarbon group may be monocyclic or polycyclic. The number of carbon atoms in the aromatic hydrocarbon group is preferably 6 to 18, more preferably 6 to 14, and still more preferably 6 to 10. The aliphatic hydrocarbon group may have a substituent.

[0030] The number of carbon atoms in the aromatic hydrocarbon group is preferably 6 to 18, more preferably 6 to 14, and even more preferably 6 to 10. The aromatic hydrocarbon group is preferably a monocyclic or condensed ring aromatic hydrocarbon group having 2 to 4 condensed rings, and more preferably a monocyclic aromatic hydrocarbon group. The aromatic hydrocarbon group is preferably a benzene ring group.

[0031] The heterocyclic group is preferably a single ring or a condensed ring having 2 to 4 condensed rings. The number of heteroatoms constituting the ring of the heterocyclic group is preferably 1 to 3. The heteroatoms constituting the ring of the heterocyclic group are preferably a nitrogen atom, an oxygen atom, or a sulfur atom. The number of carbon atoms constituting the ring of the heterocyclic group is preferably 3 to 30, more preferably 3 to 18, and more preferably 3 to 12. Specific examples of the heterocyclic group include a piperazine ring group, a pyrrolidine ring group, a pyrrole ring group, a piperidine ring group, a pyridine ring group, an imidazole ring group, a pyrazole ring group, an oxazole ring group, a thiazole ring group, a pyrazine ring group, a morpholine ring group, a thiazine ring group, an indole ring group, an isoindole ring group, a benzimidazole ring group, a purine ring group, a quinoline ring group, an isoquinoline ring group, a quinoxaline ring group, a cinnoline ring group, a carbazole ring group, and groups represented by the following formulas (L-1) to (L-7). [ka] In the formula, * represents a bond to P, L, or X. R represents a hydrogen atom or a substituent. Examples of the substituent include the substituent T described above in relation to formula (1).

[0032] The aliphatic hydrocarbon group, aromatic hydrocarbon group and heterocyclic group may have a substituent. Examples of the substituent include the groups exemplified as the substituent T described later.

[0033] R L1 The number of carbon atoms in the alkyl group represented by R is preferably 1 to 20, more preferably 1 to 15, and further preferably 1 to 8. The alkyl group may be linear, branched, or cyclic, preferably linear or branched, and more preferably linear. L1 The alkyl group represented by may further have a substituent. Examples of the substituent include the substituent T described below.

[0034] R L1 The number of carbon atoms in the aryl group represented by R is preferably 6 to 30, more preferably 6 to 20, and further preferably 6 to 12. L1 The aryl group represented by may further have a substituent. Examples of the substituent include the substituent T described below.

[0035] X in Equation (2) 1 The acid group represented by the formula (I) includes a sulfo group, a carboxyl group, a phosphoric acid group, a boronic acid group, a sulfonimide group, a sulfonamide group, and salts thereof. The atoms or atomic groups constituting the salt include an alkali metal ion (Li + , Na + , K + etc.), alkaline earth metal ions (Ca 2+ , Mg 2+ etc.), ammonium ion, imidazolium ion, pyridinium ion, phosphonium ion, etc.

[0036] X in Equation (2) 1 Examples of the basic group represented by include an amino group, a pyridinyl group and its salts, an ammonium salt, and a phthalimidomethyl group. Examples of the atoms or atomic groups constituting the salt include a hydroxide ion, a halogen ion, a carboxylate ion, a sulfonate ion, and a phenoxide ion.

[0037] The amino group is -NRx 1 Rx 2 and a cyclic amino group.

[0038] -NRx 1 Rx 2 In the group represented by 1 and Rx 2 are each independently a hydrogen atom, an alkyl group or an aryl group, and are preferably an alkyl group. The number of carbon atoms in the alkyl group is preferably 1 to 10, more preferably 1 to 5, and even more preferably 1 to 3. The alkyl group may be linear, branched, or cyclic, but is preferably linear or branched, and more preferably linear. The alkyl group may have a substituent. An example of the substituent is the substituent T described later. The number of carbon atoms in the aryl group is preferably 6 to 30, more preferably 6 to 20, and even more preferably 6 to 12. The aryl group may have a substituent. An example of the substituent is the substituent T described later. In addition, Rx 1 and Rx 2 may be bonded to form a ring.

[0039] Examples of the cyclic amino group include a pyrrolidine group, a piperidine group, a piperazine group, and a morpholine group. These groups may further have a substituent. Examples of the substituent include the substituent T described below. Specific examples of the substituent include an alkyl group and an aryl group.

[0040] X in Equation (2) 1 is preferably a sulfo group, a phosphate group, a group represented by formula (X-1), a group represented by formula (X-2), a group represented by formula (X-3) or a group represented by formula (X-4), and more preferably a sulfo group, a group represented by formula (X-1) or a group represented by formula (X-3). [ka] In formulas (X-1) to (X-4), R 100 ~R 106 each independently represents a hydrogen atom, an alkyl group, an alkenyl group, or an aryl group; R 100 and R 101 may be linked together to form a ring, and M represents an atom or an atomic group that forms a salt with an anion. M is an alkali metal ion (Li + , Na + , K + etc.), alkaline earth metal ions (Ca 2+ , Mg 2+ etc.), ammonium ion, imidazolium ion, pyridinium ion, phosphonium ion, etc.

[0041] In formula (2), n2 represents an integer of 1 or more, and is preferably an integer of 1 to 3, more preferably 1 or 2, and further preferably 1.

[0042] (substituent T) Examples of the substituent T include the following groups: a halogen atom (for example, a fluorine atom, a chlorine atom, a bromine atom, an iodine atom), an alkyl group (preferably an alkyl group having 1 to 30 carbon atoms), an alkenyl group (preferably an alkenyl group having 2 to 30 carbon atoms), an alkynyl group (preferably an alkynyl group having 2 to 30 carbon atoms), an aryl group (preferably an aryl group having 6 to 30 carbon atoms), a heteroaryl group (preferably a heteroaryl group having 1 to 30 carbon atoms), an amino group (preferably an amino group having 0 to 30 carbon atoms), an alkoxy group (preferably an alkoxy group having 1 to 30 carbon atoms), an aryloxy group (preferably or an aryloxy group having 6 to 30 carbon atoms), a heteroaryloxy group (preferably a heteroaryloxy group having 1 to 30 carbon atoms), an acyl group (preferably an acyl group having 2 to 30 carbon atoms), an alkoxycarbonyl group (preferably an alkoxycarbonyl group having 2 to 30 carbon atoms), an aryloxycarbonyl group (preferably an aryloxycarbonyl group having 7 to 30 carbon atoms), a heteroaryloxycarbonyl group (preferably a heteroaryloxycarbonyl group having 2 to 30 carbon atoms), an acyloxy group (preferably an acyloxy group having 2 to 30 carbon atoms). group), acylamino group (preferably an acylamino group having 2 to 30 carbon atoms), aminocarbonylamino group (preferably an aminocarbonylamino group having 2 to 30 carbon atoms), alkoxycarbonylamino group (preferably an alkoxycarbonylamino group having 2 to 30 carbon atoms), aryloxycarbonylamino group (preferably an aryloxycarbonylamino group having 7 to 30 carbon atoms), sulfamoyl group (preferably a sulfamoyl group having 0 to 30 carbon atoms), sulfamoylamino group (preferably a sulfamoylamino group having 0 to 30 carbon atoms), carbazole group (preferably a carbazole group having 2 to 30 carbon atoms), aryloxycarbonylamino group (preferably a aryloxycarbonylamino group having 7 ... a bamoyl group (preferably a carbamoyl group having 1 to 30 carbon atoms), an alkylthio group (preferably an alkylthio group having 1 to 30 carbon atoms), an arylthio group (preferably an arylthio group having 6 to 30 carbon atoms), a heteroarylthio group (preferably a heteroarylthio group having 1 to 30 carbon atoms), an alkylsulfonyl group (preferably an alkylsulfonyl group having 1 to 30 carbon atoms), an alkylsulfonylamino group (preferably an alkylsulfonylamino group having 1 to 30 carbon atoms), an arylsulfonyl group (preferably an arylsulfonyl group having 6 to 30 carbon atoms),An arylsulfonylamino group (preferably an arylsulfonylamino group having 6 to 30 carbon atoms), a heteroarylsulfonyl group (preferably a heteroarylsulfonyl group having 1 to 30 carbon atoms), a heteroarylsulfonylamino group (preferably a heteroarylsulfonylamino group having 1 to 30 carbon atoms), an alkylsulfinyl group (preferably an alkylsulfinyl group having 1 to 30 carbon atoms), an arylsulfinyl group (preferably an arylsulfinyl group having 6 to 30 carbon atoms), a heteroarylsulfinyl group, Examples of the substituent include an alkyl group (preferably a heteroarylsulfinyl group having 1 to 30 carbon atoms), an ureido group (preferably a ureido group having 1 to 30 carbon atoms), a hydroxyl group, a nitro group, a carboxyl group, a sulfo group, a phosphoric acid group, a carboxylic acid amide group, a sulfonic acid amide group, an imido group, a phosphino group, a mercapto group, a cyano group, an alkylsulfino group, an arylsulfino group, an arylazo group, a heteroarylazo group, a phosphinyl group, a phosphinyloxy group, a phosphinylamino group, a silyl group, a hydrazino group, and an imino group. When these groups are groups that can be further substituted, they may further have a substituent. Examples of the substituent include the groups explained above for the substituent T.

[0043] The particles satisfying the above requirement 1 are preferably particles of an infrared absorbing dye having at least one group represented by the above formula (1) and at least one group represented by the above formula (2). Examples of the infrared absorbing dye constituting the specific particles satisfying the above requirement 1 include pyrrolopyrrole compounds, squarylium compounds, pyrromethene compounds, croconium compounds, and cyanine compounds, preferably pyrrolopyrrole compounds and squarylium compounds, and more preferably pyrrolopyrrole compounds.

[0044] It is preferable that the particles satisfying the above requirement 2 further satisfy the characteristics of the above requirement 1.

[0045] The specific particles exhibit two or more maximum absorption wavelengths in the infrared absorbing composition in the wavelength range of 650 to 1500 nm, and the difference (λ2-λ1) between the maximum absorption wavelength (λ1) on the shortest side and the maximum absorption wavelength (λ2) on the second shortest side in the above range is preferably 20 to 90 nm, more preferably 30 to 80 nm, and even more preferably 35 to 70 nm. When the difference in wavelength is within the above range, a film with excellent infrared shielding properties that can shield infrared rays in a wide wavelength range can be formed.

[0046] The maximum absorption wavelength on the shortest wavelength side of the specific particle is preferably on the short wavelength side of the wavelength at which the dye solution obtained by dissolving the infrared absorbing dye constituting the specific particle in a good solvent for the infrared absorbing dye has the highest absorbance, more preferably on the short wavelength side by 30 nm or more, and even more preferably on the short wavelength side by 50 nm or more. By using particles that satisfy such spectral characteristics, a film with good infrared absorption tail can be formed. In this specification, a good solvent for the infrared absorbing dye means a solvent in which the amount of infrared absorbing dye dissolved in 100 g of the solvent at 25 ° C is 0.1 g or more. The good solvent is preferably a solvent in which the amount of infrared absorbing dye dissolved in 100 g of the solvent at 25 ° C is 0.1 g or more, and more preferably a solvent in which the amount of dissolved is 0.2 g or more. The type of good solvent varies depending on the type of infrared absorbing dye, and examples of the good solvent include dimethyl sulfoxide and chloroform.

[0047] The specific particles preferably have three or more maximum absorption wavelengths in the infrared absorbing composition in the wavelength range of 650 to 1500 nm. The absorbance at the third shortest absorption wavelength is preferably 0.2 to 2, more preferably 0.3 to 1.8, and even more preferably 0.4 to 1.5, when the absorbance at the second shortest absorption wavelength is taken as 1. The difference (λ3-λ2) between the second shortest absorption maximum wavelength (λ2) and the third shortest absorption maximum wavelength (λ3) is preferably 20 to 100 nm, more preferably 30 to 90 nm, and even more preferably 35 to 80 nm. The difference (λ3-λ1) between the shortest absorption maximum wavelength (λ1) and the third shortest absorption maximum wavelength (λ3) is preferably 60 to 200 nm, more preferably 70 to 170 nm, and even more preferably 80 to 150 nm.

[0048] The number of maximum absorption wavelengths exhibited by the specific particles in the infrared absorbing composition in the wavelength range of 650 to 1500 nm is preferably greater than the number of maximum absorption wavelengths exhibited by a dye solution in the wavelength range of 650 to 1500 nm obtained by dissolving the infrared absorbing dye constituting the specific particles in a good solvent for the infrared absorbing dye. By using such specific particles, a film having excellent infrared shielding properties that can shield infrared rays in a wider wavelength range can be formed.

[0049] In this specification, the maximum absorption wavelength and absorbance of the specific particle in the infrared absorbing composition can be determined by measuring the absorbance of the infrared absorbing composition. In addition, when the infrared absorbing composition contains two or more types of specific particles, the absorbance of the composition obtained by removing the specific particles other than the type to be measured from the infrared absorbing composition is measured. For example, in the case of an infrared absorbing composition containing specific particle A, specific particle B, a solvent, and other additives, the maximum absorption wavelength and absorbance of the specific particle A in the infrared absorbing composition are determined by measuring the absorbance of the composition obtained by removing the specific particle B from the infrared absorbing composition. In addition, the maximum absorption wavelength and absorbance of the specific particle B in the infrared absorbing composition are determined by measuring the absorbance of the composition obtained by removing the specific particle A from the infrared absorbing composition. In addition, when the infrared absorbing composition further contains materials such as an infrared absorbing agent, a chromatic colorant, and a black colorant other than the specific particles in addition to the specific particles, the absorbance of the composition obtained by removing these materials from the infrared absorbing composition is measured. For example, in the case of an infrared absorbing composition containing specific particles, an infrared absorbing agent other than the specific particles, a solvent, and other additives, the maximum absorption wavelength and absorbance of the specific particles A in the infrared absorbing composition are determined by measuring the absorbance of a composition obtained by removing the infrared absorbing agents other than the specific particles from the above infrared absorbing composition.

[0050] The amount of the specific particles that dissolves in 100 g of water at 25° C. is preferably 0.075 g or less, more preferably 0.05 g or less, and even more preferably 0.025 g or less.

[0051] The amount of the specific particles dissolved in 100 g of propylene glycol monomethyl ether at 25° C. is preferably 0.075 g or less, more preferably 0.05 g or less, and even more preferably 0.025 g or less.

[0052] The amount of the specific particles that dissolves in 100 g of cyclopentanone at 25° C. is preferably 0.075 g or less, more preferably 0.05 g or less, and even more preferably 0.025 g or less.

[0053] The infrared absorbing dye constituting the specific particles is preferably a compound represented by formula (PP-1). That is, the specific particles are preferably particles of a compound represented by formula (PP-1). [ka] In the formula, R 1a represents an alkyl group, a halogen atom, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, or a cyano group, R 1b represents a substituent, R 2 represents an alkyl group, an aryl group, or a heteroaryl group; R 3 , R 4 , R 5 and R 6 each independently represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, an arylsulfinyl group, or a heteroaryl group, R 7 and R 8 each independently represents a hydrogen atom, an alkyl group, an aryl group, a heteroaryl group, -BR 9 R 10 or a metal atom, R 9 and R 10 each independently represents a hydrogen atom, a halogen atom, an alkyl group, an alkenyl group, an aryl group, a heteroaryl group, an alkoxy group, an aryloxy group, or a heteroaryloxy group, R 9 and R 10 may be bonded to each other to form a ring, R 7 is R 3 or R 5 may be covalently or coordinately bonded to R 8 is R 2 , R 4 or R 6 may be covalently or coordinately bonded to L 1represents an aliphatic hydrocarbon group, an aromatic hydrocarbon group, a nitrogen-containing heterocyclic group, -O-, -S-, -NR L1 represents a n2+1-valent linking group consisting of -, -CO-, -COO-, -OCO-, -SO2- or a combination thereof, and when n2 is 1, L 1 may be a single bond, R L1 represents a hydrogen atom, an alkyl group, or an aryl group, X 1 represents an acid group or a basic group, n1 represents an integer from 0 to 4; n2 represents an integer of 1 or more, m represents an integer of 1 or greater.

[0054] R in formula (PP-1) 1a , R 1b and n1 is R in formula (1). 1a , R 1b and n1, and the preferred ranges are also the same. 1 , X 1 and n2 is L in Eq. (2). 1 , X 1 and n2, and the preferred ranges thereof are also the same.

[0055] R in formula (PP-1) 2 represents an alkyl group, an aryl group or a heteroaryl group, preferably an aryl group or a heteroaryl group, and more preferably an aryl group. R 2 The alkyl group represented by the formula (I) preferably has 1 to 30 carbon atoms, more preferably has 1 to 20 carbon atoms, and further preferably has 1 to 10 carbon atoms. R 2 The aryl group represented by the formula (I) preferably has 6 to 30 carbon atoms, more preferably has 6 to 20 carbon atoms, and further preferably has 6 to 12 carbon atoms. R 2The number of carbon atoms constituting the heteroaryl group represented by is preferably 1 to 30, more preferably 1 to 12. Examples of the types of heteroatoms constituting the heteroaryl group include nitrogen atoms, oxygen atoms, and sulfur atoms. The number of heteroatoms constituting the heteroaryl group is preferably 1 to 3, more preferably 1 to 2. The heteroaryl group is preferably a monocyclic or condensed ring, more preferably a monocyclic or condensed ring having 2 to 8 condensed rings, and even more preferably a monocyclic or condensed ring having 2 to 4 condensed rings. R 2 The alkyl group, aryl group and heteroaryl group represented by may be unsubstituted or may have a substituent. Examples of the substituent include the groups explained above for the substituent T. R 2 In formula (PP-1), "-L 1 -(X 1 ) n2 " is preferably bonded.

[0056] R in formula (PP-1) 3 , R 4 , R 5 and R 6 each independently represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, an arylsulfinyl group, or a heteroaryl group. R 3 and R 5 It is preferable that one of R represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, or an arylsulfinyl group, and the other represents a heteroaryl group; 3 and R 5 It is more preferable that one of these groups represents a cyano group and the other represents a heteroaryl group. R 4 and R 6 It is preferable that one of R represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, or an arylsulfinyl group, and the other represents a heteroaryl group; 4 and R 6 It is more preferable that one of these groups represents a cyano group and the other represents a heteroaryl group.

[0057] R 3 ~R 6 The number of carbon atoms constituting the heteroaryl group represented by is preferably 1 to 30, more preferably 1 to 12. Examples of the type of heteroatom constituting the heteroaryl group include a nitrogen atom, an oxygen atom, and a sulfur atom. The number of heteroatoms constituting the heteroaryl group is preferably 1 to 3, more preferably 1 to 2. The heteroaryl group is preferably a monocyclic or condensed ring, more preferably a monocyclic or condensed ring having 2 to 8 condensed rings, and even more preferably a monocyclic or condensed ring having 2 to 4 condensed rings. The heteroaryl group may be unsubstituted or may have a substituent. Examples of the substituent include the groups explained in the above-mentioned substituent T.

[0058] R in formula (PP-1) 7 and R 8 each independently represents a hydrogen atom, an alkyl group, an aryl group, a heteroaryl group, -BR 9 R 10 or a metal atom, -BR 9 R 10 It is preferable that:

[0059] R 7 and R 8 The alkyl group, aryl group and heteroaryl group represented by R 2 The preferred ranges are the same as those described above. R 7 and R 8 Examples of the metal atom represented by the formula (I) include magnesium, aluminum, calcium, barium, zinc, tin, aluminum, vanadium, iron, cobalt, nickel, copper, palladium, iridium, and platinum, and aluminum, zinc, vanadium, iron, copper, palladium, iridium, and platinum are preferred.

[0060] -BR 9 R 10 R in the group represented by 9 and R 10each independently represents a hydrogen atom, a halogen atom, an alkyl group, an alkenyl group, an aryl group, a heteroaryl group, an alkoxy group, an aryloxy group, or a heteroaryloxy group, preferably a halogen atom, an alkyl group, an aryl group, or a heteroaryl group, more preferably a halogen atom, an alkyl group, or an aryl group, and further preferably an aryl group.

[0061] R 9 and R 10 Examples of the halogen atom represented by the formula (I) include a fluorine atom, a chlorine atom, a bromine atom and an iodine atom, with a fluorine atom being preferred. R 9 and R 10 The number of carbon atoms of the alkyl group and alkoxy group represented by is preferably 1 to 40. The lower limit is, for example, more preferably 3 or more. The upper limit is, for example, more preferably 30 or less, and further preferably 25 or less. The alkyl group and alkoxy group may be linear, branched, or cyclic, but is preferably linear or branched. R 9 and R 10 The number of carbon atoms of the alkenyl group represented by is preferably 2 to 40. The lower limit is, for example, more preferably 3 or more. The upper limit is, for example, more preferably 30 or less, and further preferably 25 or less. R 9 and R 10 The number of carbon atoms of the aryl group and aryloxy group represented by is preferably 6 to 20, more preferably 6 to 12. The aryl group and aryloxy group may have a substituent or may be unsubstituted. Examples of the substituent include an alkyl group, an alkoxy group, and a halogen atom. R 9 and R 10The heteroaryl group and heteroaryloxy group represented by may be monocyclic or polycyclic. The number of heteroatoms constituting the heteroaryl ring of the heteroaryl group and heteroaryloxy group is preferably 1 to 3. The heteroatom constituting the heteroaryl ring is preferably a nitrogen atom, an oxygen atom or a sulfur atom. The number of carbon atoms constituting the heteroaryl ring is preferably 3 to 30, more preferably 3 to 18, further preferably 3 to 12, and particularly preferably 3 to 5. The heteroaryl ring is preferably a 5-membered or 6-membered ring. The heteroaryl group and the heteroaryloxy group may have a substituent or may be unsubstituted. Examples of the substituent include an alkyl group, an alkoxy group, and a halogen atom.

[0062] -BR 9 R 10 R 9 and R 10 may be bonded to each other to form a ring. Examples include the structures shown in (B-1) to (B-4) below. In the following, Rb represents a substituent, 1 ~Rb 4 each independently represents a hydrogen atom or a substituent, b1 to b3 each independently represents an integer of 0 to 4, and * represents the bonding position with formula (PP-1). 1 ~Rb 4 Examples of the substituent represented by include the substituents explained above for the substituent T, and a halogen atom, an alkyl group, or an alkoxy group is preferable. [ka]

[0063] R in formula (PP-1) 7 is R 3 or R 5 may be covalently or coordinately bonded to R 8 is R 2 , R 4 or R 6 may be covalently or coordinately bonded to

[0064] In formula (PP-1), m represents an integer of 1 or more, preferably an integer of 1 to 4, more preferably an integer of 1 to 3, further preferably 1 or 2, and particularly preferably 1.

[0065] The compound represented by formula (PP-1) is preferably a compound represented by formula (PP-2). [ka]

[0066] R in formula (PP-2) 1a , R 1b , R 3 ~R 8 , L 1 , X 1 , n1 and n2 are R in formula (PP-1) 1a , R 1b , R 3 ~R 8 , L 1 , X 1 , n1 and n2 have the same meanings and preferred ranges.

[0067] In formula (PP-2), m1 represents an integer of 1 to 4, preferably an integer of 1 to 3, more preferably 1 or 2, and particularly preferably 1.

[0068] Specific examples of the compound represented by formula (PP-1) include compounds having the structures shown below: In the following structural formula, Me represents a methyl group, Et represents an ethyl group, and Ph represents a phenyl group. [ka] [ka] [ka]

[0069] The content of the specific particles is preferably 1% by mass or more, more preferably 5% by mass or more, more preferably 10% by mass or more, and particularly preferably 15% by mass or more, based on the total solid content of the infrared absorbing composition. The upper limit of the content of the specific particles is preferably 70% by mass or less, more preferably 60% by mass or less, and even more preferably 50% by mass or less. The infrared absorbing composition may contain only one type of specific particles, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0070] <<Solvent>> The infrared absorbing composition of the present invention contains a solvent. Examples of the solvent include water and organic solvents. Examples of the organic solvent include ester-based solvents, ketone-based solvents, alcohol-based solvents, amide-based solvents, ether-based solvents, carbonate-based solvents, and hydrocarbon-based solvents. For details of these, refer to paragraph 0223 of International Publication No. 2015 / 166779, the contents of which are incorporated herein by reference. In addition, ester-based solvents substituted with a cyclic alkyl group and ketone-based solvents substituted with a cyclic alkyl group can also be preferably used. Specific examples of organic solvents include polyethylene glycol monomethyl ether, dichloromethane, methyl 3-ethoxypropionate, ethyl 3-ethoxypropionate, ethyl cellosolve acetate, ethyl lactate, diethylene glycol dimethyl ether, butyl acetate, methyl 3-methoxypropionate, 2-heptanone, cyclohexanone, 2-pentanone, 3-pentanone, 4-heptanone, 2-methylcyclohexanone, 3-methylcyclohexanone, 4-methylcyclohexanone, cycloheptanone, cyclooctanone, cyclohexyl acetate, cyclopentanone, ethyl carbitol acetate, butyl carbitol acetate, propylene glycol monomethyl ether, propylene glycol monomethyl Examples of suitable ether acetates include 3-methoxy-N,N-dimethylpropanamide, 3-butoxy-N,N-dimethylpropanamide, propylene glycol diacetate, 3-methoxybutanol, methyl ethyl ketone, gamma butyrolactone, sulfolane, anisole, 1,4-diacetoxybutane, diethylene glycol monoethyl ether acetate, butane-1,3-diyl diacetate, dipropylene glycol methyl ether acetate, diacetone alcohol (also known as diacetone alcohol and 4-hydroxy-4-methyl-2-pentanone), 2-methoxypropyl acetate, 2-methoxy-1-propanol, isopropyl alcohol, propylene carbonate, and methyl isobutyl ketone.However, it may be better to reduce the amount of aromatic hydrocarbons (benzene, toluene, xylene, ethylbenzene, etc.) used as organic solvents for environmental reasons (for example, it can be reduced to 50 ppm (parts per million) by mass or less, 10 ppm by mass or less, or 1 ppm by mass or less, relative to the total amount of organic solvents).

[0071] The organic solvent may be used alone or in combination of two or more kinds. When two or more kinds of organic solvents are used, In one preferred embodiment of the combined use of two or more organic solvents, a first organic solvent that is an ester-based solvent is combined with a second organic solvent that is different from the first organic solvent and contains at least one organic solvent selected from ester-based solvents, ketone-based solvents, amide-based solvents, ether-based solvents, and carbonate-based solvents. In this case, the boiling point of the second organic solvent is preferably 150 to 250°C. The boiling point of the first organic solvent is preferably 100 to 200°C.

[0072] In the present invention, it is preferable to use an organic solvent with a low metal content, and the metal content of the organic solvent is preferably 10 mass ppb (parts per billion) or less. If necessary, an organic solvent with a mass ppt (parts per trillion) level may be used, and such an organic solvent is provided, for example, by Toyo Gosei Co., Ltd. (The Chemical Daily, November 13, 2015).

[0073] Methods for removing impurities such as metals from organic solvents include, for example, distillation (molecular distillation, thin film distillation, etc.) and filtration using a filter. The filter used for filtration has a filter pore size of preferably 10 μm or less, more preferably 5 μm or less, and even more preferably 3 μm or less. The filter material is preferably polytetrafluoroethylene, polyethylene, or nylon.

[0074] The organic solvent may contain isomers (compounds having the same number of atoms but different structures). In addition, the organic solvent may contain only one type of isomer or multiple types of isomers.

[0075] The organic solvent preferably has a peroxide content of 0.8 mmol / L or less, and more preferably contains substantially no peroxide.

[0076] When the infrared absorbing composition of the present invention is used as an ink composition, it is preferable to use water or a mixed solvent of water and an aqueous organic solvent as the solvent. Examples of the water-soluble organic solvent include polyhydric alcohols such as glycerin, ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, dipropylene glycol, tripropylene glycol, 1,3-butanediol, and 2,3-butanediol; Sugar alcohols; Alkyl alcohols having 1 to 4 carbon atoms, such as ethanol, methanol, butanol, propanol, and isopropanol; Aliphatic diols such as 2-ethyl-2-methyl-1,3-propanediol, 3,3-dimethyl-1,2-butanediol, 2,2-diethyl-1,3-propanediol, 2-ethyl-1,3-hexanediol, and 2,2,4-trimethyl-1,3-pentanediol; Examples of glycol ethers include ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, ethylene glycol monobutyl ether, ethylene glycol monomethyl ether acetate, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, diethylene glycol mono-n-propyl ether, ethylene glycol mono-iso-propyl ether, diethylene glycol mono-iso-propyl ether, ethylene glycol mono-n-butyl ether, ethylene glycol mono-t-butyl ether, diethylene glycol mono-t-butyl ether, triethylene glycol monoethyl ether, 1-methyl-1-methoxybutanol, propylene glycol monomethyl ether, propylene glycol monoethyl ether, propylene glycol mono-t-butyl ether, propylene glycol mono-n-propyl ether, propylene glycol mono-iso-propyl ether, dipropylene glycol, dipropylene glycol monomethyl ether, dipropylene glycol monoethyl ether, dipropylene glycol mono-n-propyl ether, dipropylene glycol mono-iso-propyl ether, and tripropylene glycol monomethyl ether.

[0077] The proportion of water in the mixed solvent is preferably from 30 to 99 mass %, more preferably from 40 to 99 mass %, and further preferably from 50 to 99 mass %.

[0078] The content of the solvent is preferably 10 to 97% by mass relative to the total amount of the infrared absorbing composition. The lower limit is preferably 30% by mass or more, more preferably 40% by mass or more, even more preferably 50% by mass or more, even more preferably 60% by mass or more, and particularly preferably 70% by mass or more. The upper limit is preferably 96% by mass or less, more preferably 95% by mass or less. The infrared absorbing composition may contain only one type of solvent, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0079] <<Other infrared absorbers>> The infrared absorbing composition of the present invention may contain an infrared absorbing agent (another infrared absorbing agent) other than the above-mentioned specific particles. By further containing another infrared absorbing agent, a film capable of blocking infrared rays in a wider wavelength range can be formed. The other infrared absorbing agent may be a dye or a pigment (particle). Examples of the other infrared absorbing agent include pyrrolopyrrole compounds, cyanine compounds, squarylium compounds, phthalocyanine compounds, naphthalocyanine compounds, quaterrylene compounds, merocyanine compounds, croconium compounds, oxonol compounds, iminium compounds, dithiol compounds, triarylmethane compounds, pyrromethene compounds, azomethine compounds, anthraquinone compounds, dibenzofuranone compounds, dithiolene metal complexes, metal oxides, and metal borides. Examples of pyrrolopyrrole compounds include compounds described in paragraphs 0016 to 0058 of JP 2009-263614 A, compounds described in paragraphs 0037 to 0052 of JP 2011-068731 A, and compounds described in paragraphs 0010 to 0033 of WO 2015 / 166873 A. Examples of squarylium compounds include compounds described in paragraphs 0044 to 0049 of JP 2011-208101 A, compounds described in paragraphs 0060 to 0061 of Japanese Patent No. 6065169 A, compounds described in paragraphs 0040 of WO 2016 / 181987 A, compounds described in JP 2015-176046 A, and compounds described in paragraph 0072 of WO 2016 / 190162 A. Compounds described in JP 2016-074649 A, paragraphs 0196 to 0228, compounds described in JP 2017-067963 A, paragraph 0124, compounds described in WO 2017 / 135359, compounds described in JP 2017-114956 A, compounds described in Japanese Patent No. 6197940, compounds described in WO 2016 / 120166, and the like.Examples of the cyanine compound include the compounds described in paragraphs 0044-0045 of JP 2009-108267 A, the compounds described in paragraphs 0026-0030 of JP 2002-194040 A, the compounds described in JP 2015-172004 A, the compounds described in JP 2015-172102 A, the compounds described in JP 2008-088426 A, the compounds described in paragraph 0090 of WO 2016 / 190162 A, the compounds described in JP 2017-031394 A, etc. Examples of the croconium compound include the compounds described in JP 2017-082029 A. Examples of the iminium compound include the compounds described in JP-T-2008-528706, JP-A-2012-012399, JP-A-2007-092060, and WO-2018 / 043564, paragraphs 0048-0063. Examples of the phthalocyanine compound include the compounds described in JP-A-2012-077153, paragraph 0093, oxytitanium phthalocyanine described in JP-A-2006-343631, the compounds described in JP-A-2013-195480, paragraphs 0013-0029, and vanadium phthalocyanine compounds described in Japanese Patent No. 6081771. Examples of the naphthalocyanine compound include the compounds described in JP-A-2012-077153, paragraph 0093. Examples of dithiolene metal complexes include compounds described in Japanese Patent No. 5733804. Examples of metal oxides include indium tin oxide, antimony tin oxide, zinc oxide, Al-doped zinc oxide, fluorine-doped tin dioxide, niobium-doped titanium dioxide, and tungsten oxide. For details of tungsten oxide, refer to paragraph 0080 of JP 2016-006476 A, the contents of which are incorporated herein by reference. Examples of metal borides include lanthanum boride. Examples of commercially available lanthanum boride include LaB6-F (manufactured by Nippon Shinkinzoku Co., Ltd.). In addition, compounds described in International Publication No. 2017 / 119394 can also be used as metal borides. Examples of commercially available indium tin oxide include F-ITO (manufactured by DOWA High-Tech Co., Ltd.).

[0080] Examples of the infrared absorbent include squarylium compounds described in JP 2017-197437 A, squarylium compounds described in JP 2017-025311 A, squarylium compounds described in WO 2016 / 154782 A, squarylium compounds described in Japanese Patent No. 5884953 A, squarylium compounds described in Japanese Patent No. 6036689 A, squarylium compounds described in Japanese Patent No. 5810604 A, squarylium compounds described in Japanese Patent No. 5810604 B, squarylium compounds described in Japanese Patent No. 5810604 C, squarylium compounds described in Japanese Patent No. 5810604 D, squarylium compounds described in Japanese Patent No. 5810604 E, squarylium compounds described in Japanese Patent No. 5810604 H ... the squarylium compounds described in paragraphs 0090 to 0107 of WO 2017 / 213047; the pyrrole ring-containing compounds described in paragraphs 0019 to 0075 of JP 2018-054760 A; the pyrrole ring-containing compounds described in paragraphs 0078 to 0082 of JP 2018-040955 A; Pyrrole ring-containing compounds described in JP-A-2018-041047, squarylium compounds having an aromatic ring at the amide α-position described in paragraphs 0024 to 0086 of JP-A-2018-041047, amide-linked squarylium compounds described in JP-A-2017-179131, compounds having a pyrrole bis-type squarylium skeleton or croconium skeleton described in JP-A-2017-141215, dihydrocarbazole bis-type squarylium compounds described in JP-A-2017-082029, asymmetric compounds described in paragraphs 0027 to 0114 of JP-A-2017-068120, pyrrole ring-containing compounds (carbazole type) described in JP-A-2017-067963, phthalocyanine compounds described in JP-A-6251530, and the like can also be used.

[0081] When the infrared absorbing dye constituting the specific particle is a compound represented by formula (PP-1), the other infrared absorbing agent is preferably a pyrrolopyrrole compound, and more preferably a compound represented by formula (PP-100), because this can provide better dispersibility and improve the storage stability of the composition. [ka] In the formula, R 51a and R 51ceach independently represents an alkyl group, a halogen atom, an alkenyl group, an alkynyl group, an aryl group, a heteroaryl group, or a cyano group, R 51b and R 51d each independently represents a substituent, R 53 , R 54 , R 55 and R 56 each independently represents a cyano group, an acyl group, an alkoxycarbonyl group, an alkylsulfinyl group, an arylsulfinyl group, or a heteroaryl group, R 57 and R 58 each independently represents a hydrogen atom, an alkyl group, an aryl group, a heteroaryl group, -BR 59 R 60 or a metal atom, R 59 and R 60 each independently represents a hydrogen atom, a halogen atom, an alkyl group, an alkenyl group, an aryl group, a heteroaryl group, an alkoxy group, an aryloxy group, or a heteroaryloxy group, R 59 and R 60 may be bonded to each other to form a ring, R 57 is R 53 or R 55 may be covalently or coordinately bonded to R 58 is R 54 or R 56 may be covalently or coordinately bonded to n1 represents an integer from 0 to 4; m1 represents an integer of 0 to 4.

[0082] R in formula (PP-100) 51a and R 51c is R in formula (PP-1). 1a The same definition and preferred range are also the same. 51b and R 51d is R in formula (PP-1). 1bThe same definition and preferred range are also the same. 53 ~R 58 is R in formula (PP-1). 3 ~R 8 The meaning and preferred range of n1 in formula (PP-100) is the same as those in formula (PP-100). n1 in formula (PP-100) represents an integer of 0 to 4, preferably an integer of 0 to 2, and more preferably 0. m1 in formula (PP-100) represents an integer of 0 to 4, preferably an integer of 0 to 2, and more preferably 0.

[0083] Specific examples of other infrared absorbing agents include infrared absorbing dyes B-1 to B-9 described in the examples below.

[0084] The content of the other infrared absorbing agent is preferably 5 to 1000 parts by mass, more preferably 10 to 500, and even more preferably 30 to 300, relative to 100 parts by mass of the specific particles. The total content of the specific particles and the other infrared absorbing agent is preferably 1% by mass or more, more preferably 5% by mass or more, and even more preferably 15% by mass or more, based on the total solid content of the infrared absorbing composition. The upper limit of the total content is preferably 70% by mass or less, more preferably 60% by mass or less, and even more preferably 50% by mass or less.

[0085] Since the infrared absorbing composition of the present invention contains the above-mentioned specific particles, it can form a film that can block infrared rays in a wide wavelength range without using other infrared absorbing agents, so it can be substantially free of other infrared absorbing agents. "Substantially free of other infrared absorbing agents" means that the content of other infrared absorbing agents in the total solid content of the infrared absorbing composition is 0.1 mass% or less, preferably 0.05 mass% or less, and more preferably 0.01 mass% or less.

[0086] <<Dye derivatives>> The infrared absorbing composition of the present invention may further contain a dye derivative in addition to the specific particles described above. Examples of the dye derivative include compounds having a structure in which an acid group or a basic group is bonded to a dye skeleton.

[0087] Examples of the dye skeleton constituting the dye derivative include a squarylium dye skeleton, a pyrrolopyrrole dye skeleton, a diketopyrrolopyrrole dye skeleton, a quinacridone dye skeleton, an anthraquinone dye skeleton, a dianthraquinone dye skeleton, a benzisoindole dye skeleton, a thiazine indigo dye skeleton, an azo dye skeleton, a quinophthalone dye skeleton, a phthalocyanine dye skeleton, a naphthalocyanine dye skeleton, a dioxazine dye skeleton, a perylene dye skeleton, a perinone dye skeleton, a benzimidazolone dye skeleton, a benzothiazole dye skeleton, a benzimidazole dye skeleton, and a benzoxazole dye skeleton. Of these, the squarylium dye skeleton, the pyrrolopyrrole dye skeleton, the diketopyrrolopyrrole dye skeleton, the phthalocyanine dye skeleton, the quinacridone dye skeleton, and the benzimidazolone dye skeleton are preferred, and the squarylium dye skeleton and the pyrrolopyrrole dye skeleton are more preferred.

[0088] Examples of the acid group include a sulfo group, a carboxyl group, a phosphoric acid group, a boronic acid group, a sulfonimide group, a sulfonamide group, and salts thereof. Examples of the atoms or atomic groups constituting the salts include an alkali metal ion (Li + , Na + , K + etc.), alkaline earth metal ions (Ca 2+ , Mg 2+ etc.), ammonium ion, imidazolium ion, pyridinium ion, phosphonium ion, etc.

[0089] Examples of basic groups include amino groups, pyridinyl groups and their salts, ammonium salts, and phthalimidomethyl groups. Examples of atoms or atomic groups that form salts include hydroxide ions, halogen ions, carboxylate ions, sulfonate ions, and phenoxide ions.

[0090] Specific examples of the dye derivatives include those described in JP-A-56-118462, JP-A-63-264674, JP-A-01-217077, JP-A-03-009961, JP-A-03-026767, JP-A-03-153780, JP-A-03-045662, JP-A-04-285669, JP-A-06-145546, Also included are the compounds described in JP-A-06-212088, JP-A-06-240158, JP-A-10-030063, JP-A-10-195326, paragraphs 0086 to 0098 of WO 2011 / 024896, and paragraphs 0063 to 0094 of WO 2012 / 102399, the contents of which are incorporated herein by reference.

[0091] The content of the dye derivative is preferably 1 to 50 parts by mass relative to 100 parts by mass of the above-mentioned specific particles. The lower limit is preferably 3 parts by mass or more, and more preferably 5 parts by mass or more. The upper limit is preferably 40 parts by mass or less, and more preferably 30 parts by mass or less. Only one type of dye derivative may be used, or two or more types may be used. When two or more types are used, it is preferable that the total amount is within the above range.

[0092] <<Resin>> The infrared absorbing composition of the present invention may contain a resin. The resin is blended, for example, for dispersing particles such as pigments in the infrared absorbing composition or for use as a binder. Note that a resin used mainly for dispersing particles such as pigments is also called a dispersant. However, such uses of the resin are merely examples, and the resin may also be used for purposes other than these uses.

[0093] The weight average molecular weight (Mw) of the resin is preferably 2000 to 2000000. The upper limit is preferably 1000000 or less, and more preferably 500000 or less. The lower limit is preferably 3000 or more, and more preferably 5000 or more.

[0094] Examples of the resin include (meth)acrylic resin, epoxy resin, enethiol resin, polycarbonate resin, polyether resin, polyarylate resin, polysulfone resin, polyethersulfone resin, polyphenylene resin, polyarylene ether phosphine oxide resin, polyimide resin, polyamide resin, polyamideimide resin, polyolefin resin, cyclic olefin resin, polyester resin, styrene resin, vinyl acetate resin, polyvinyl alcohol resin, polyvinyl acetal resin, polyurethane resin, and polyurea resin. One of these resins may be used alone, or two or more may be mixed and used. As the cyclic olefin resin, norbornene resin is preferable from the viewpoint of improving heat resistance. Examples of commercially available norbornene resins include the ARTON series (e.g., ARTON F4520) manufactured by JSR Corporation. In addition, the resin described in the examples of International Publication No. 2016 / 088645 can also be used. In addition, when the resin has an ethylenically unsaturated bond-containing group, particularly a (meth)acryloyl group, in a side chain, it is also preferable that the main chain and the ethylenically unsaturated bond-containing group are bonded via a divalent linking group having an alicyclic structure.

[0095] The infrared absorbing composition of the present invention preferably contains a resin having an acid group. The resin having an acid group can be used as an alkali-soluble resin. For the resin having an acid group (alkali-soluble resin), the description in paragraphs 0558 to 0571 of JP 2012-208494 A (corresponding paragraphs 0685 to 0700 of US Patent Application Publication No. 2012 / 0235099) and the description in paragraphs 0076 to 0099 of JP 2012-198408 A can be referred to, and the contents of these can be incorporated herein. In addition, a commercially available product can also be used as the resin having an acid group. In addition, there is no particular limitation on the method of introducing an acid group into the resin, and for example, the method described in Japanese Patent No. 6349629 A can be mentioned. Furthermore, as a method of introducing an acid group into a resin, a method of reacting an acid anhydride with a hydroxyl group generated by a ring-opening reaction of an epoxy group to introduce an acid group can be mentioned.

[0096] The type of acid group contained in the resin having an acid group includes a carboxyl group, a phosphate group, a sulfo group, a phenolic hydroxy group, etc., and the carboxyl group is preferable.

[0097] The acid value of the resin having an acid group is preferably 30 to 500 mgKOH / g. The lower limit is preferably 50 mgKOH / g or more, more preferably 70 mgKOH / g or more. The upper limit is preferably 400 mgKOH / g or less, more preferably 300 mgKOH / g or less, and even more preferably 200 mgKOH / g or less. The weight average molecular weight (Mw) of the resin having an acid group is preferably 5,000 to 100,000. The number average molecular weight (Mn) of the resin having an acid group is preferably 1,000 to 20,000.

[0098] The resin having an acid group preferably contains a repeating unit having an acid group on a side chain, and more preferably contains 5 to 70 mol % of the repeating units having an acid group on a side chain in all repeating units of the resin. The upper limit of the content of the repeating units having an acid group on a side chain is preferably 50 mol % or less, and more preferably 30 mol % or less. The lower limit of the content of the repeating units having an acid group on a side chain is preferably 10 mol % or more, and more preferably 20 mol % or more.

[0099] As the resin, it is also preferable to use a resin containing a repeating unit derived from a compound represented by the following formula (ED1) and / or a compound represented by the following formula (ED2) (hereinafter, these compounds may be referred to as "ether dimers").

[0100] [ka]

[0101] In formula (ED1), R 1 and R 2 each independently represents a hydrogen atom or a hydrocarbon group having 1 to 25 carbon atoms which may have a substituent. [ka] In formula (ED2), R represents a hydrogen atom or an organic group having a carbon number of 1 to 30. Specific examples of formula (ED2) can be found in JP-A-2010-168539.

[0102] For specific examples of ether dimers, reference can be made to paragraph

[0317] of JP2013-029760A, the contents of which are incorporated herein by reference.

[0103] It is also preferable to use a resin containing a repeating unit having a polymerizable group, such as a (meth)allyl group or a (meth)acryloyl group.

[0104] As the resin, it is also preferable to use a resin containing a repeating unit derived from a compound represented by formula (X). [ka] In the formula, R 1 represents a hydrogen atom or a methyl group, and R 21 and R 22 each independently represents an alkylene group, and n represents an integer of 0 to 15. 21 and R 22 The number of carbon atoms in the alkylene group represented by is preferably 1 to 10, more preferably 1 to 5, even more preferably 1 to 3, and particularly preferably 2 or 3. n represents an integer of 0 to 15, preferably an integer of 0 to 5, more preferably an integer of 0 to 4, and even more preferably an integer of 0 to 3.

[0105] Examples of the compound represented by formula (X) include ethylene oxide or propylene oxide modified (meth)acrylate of paracumylphenol, etc. Examples of commercially available products include Aronix M-110 (manufactured by Toagosei Co., Ltd.).

[0106] The infrared absorbing composition of the present invention may also contain a resin as a dispersant. Examples of dispersants include acidic dispersants (acidic resins) and basic dispersants (basic resins). Here, the acidic dispersant (acidic resin) refers to a resin in which the amount of acid groups is greater than the amount of basic groups. The acidic dispersant (acidic resin) is preferably a resin in which the amount of acid groups is 70 mol% or more when the total amount of the acid groups and the basic groups is 100 mol%. The acid group possessed by the acidic dispersant (acidic resin) is preferably a carboxyl group. The acid value of the acidic dispersant (acidic resin) is preferably 10 to 105 mgKOH / g. Moreover, the basic dispersant (basic resin) refers to a resin in which the amount of basic groups is greater than the amount of acid groups. The basic dispersant (basic resin) is preferably a resin in which the amount of basic groups is greater than the amount of acid groups when the total amount of the acid groups and the basic groups is 100 mol%. The basic group possessed by the basic dispersant is preferably an amino group.

[0107] The resin used as the dispersant is preferably a graft resin. For details of the graft resin, refer to paragraphs 0025 to 0094 of JP2012-255128A, the contents of which are incorporated herein by reference.

[0108] The resin used as the dispersant is also preferably a polyimine-based dispersant containing nitrogen atoms in at least one of the main chain and the side chain. The polyimine-based dispersant is preferably a resin having a main chain with a partial structure having a functional group with a pKa of 14 or less, a side chain with an atomic number of 40 to 10,000, and having a basic nitrogen atom in at least one of the main chain and the side chain. There is no particular limitation on the basic nitrogen atom as long as it is a nitrogen atom that exhibits basicity. For the polyimine-based dispersant, the description in paragraphs 0102 to 0166 of JP 2012-255128 A can be referred to, and the contents thereof are incorporated herein.

[0109] The resin used as the dispersant is preferably a resin having a structure in which a plurality of polymer chains are bonded to a core portion. For example, such a resin may be a dendrimer (including a star-shaped polymer). Specific examples of dendrimers include polymer compounds C-1 to C-31 described in paragraphs 0196 to 0209 of JP2013-043962A.

[0110] The resin used as the dispersant is also preferably a resin containing a repeating unit having an ethylenically unsaturated bond-containing group in a side chain. The content of the repeating unit having an ethylenically unsaturated bond-containing group in a side chain is preferably 10 mol% or more, more preferably 10 to 80 mol%, and even more preferably 20 to 70 mol% of all repeating units of the resin. In addition, the resin described in JP 2018-087939 A can also be used as the dispersant.

[0111] Dispersants are also available as commercially available products, and specific examples thereof include the DISPERBYK series manufactured by BYK Japan Co., Ltd., the SOLSPERSE series manufactured by Lubrizol Japan Co., Ltd., the Efka series manufactured by BASF, and the AJISPAR series manufactured by Ajinomoto Fine-Techno Co., Ltd. In addition, the products described in paragraph number 0129 of JP 2012-137564 A and the products described in paragraph number 0235 of JP 2017-194662 A can also be used as dispersants.

[0112] Furthermore, the resin used as the dispersant may be the block copolymers (EB-1) to (EB-9) described in paragraphs 0219 to 0221 of Japanese Patent No. 6432077.

[0113] The content of the resin is preferably 1 to 50% by mass based on the total solid content of the infrared absorbing composition. The lower limit is preferably 5% by mass or more, more preferably 7% by mass or more. The upper limit is preferably 40% by mass or less, more preferably 30% by mass or less.

[0114] In addition, when the infrared absorbing composition of the present invention contains a resin as a dispersant, the content of the resin as a dispersant is preferably 0.1 to 40 mass% of the total solid content of the infrared absorbing composition. The upper limit is preferably 20 mass% or less, more preferably 10 mass% or less. The lower limit is preferably 0.5 mass% or more, more preferably 1 mass% or more. In addition, the content of the resin as a dispersant is preferably 1 to 100 mass parts relative to 100 mass parts of the specific particles described above. The upper limit is preferably 80 mass parts or less, more preferably 60 mass parts or less. The lower limit is preferably 2.5 mass parts or more, more preferably 5 mass parts or more.

[0115] The infrared absorbing composition of the present invention may contain only one type of resin, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0116] <<Curable compound>> The infrared absorbing composition of the present invention may contain a curable compound. As the curable compound, a known compound capable of being crosslinked by radicals, acid or heat can be used. As the curable compound, a compound having an ethylenically unsaturated bond-containing group, a compound having a cyclic ether group, etc. can be mentioned, and a compound having an ethylenically unsaturated bond-containing group is preferable. As the ethylenically unsaturated bond-containing group, a vinyl group, a (meth)allyl group, a (meth)acryloyl group, etc. can be mentioned. As the cyclic ether group, an epoxy group, an oxetanyl group, etc. can be mentioned. The curable compound used in the present invention is preferably a polymerizable compound, more preferably a radically polymerizable compound.

[0117] (polymerizable compound) The polymerizable compound may be in any chemical form such as a monomer, a prepolymer, or an oligomer, but is preferably a monomer. The molecular weight of the polymerizable compound is preferably 100 to 3000. The upper limit is more preferably 2000 or less, and even more preferably 1500 or less. The lower limit is more preferably 150 or more, and even more preferably 250 or more.

[0118] The polymerizable compound is preferably a polyfunctional polymerizable monomer. The polyfunctional polymerizable monomer is preferably a compound containing 3 or more ethylenically unsaturated bond-containing groups, more preferably a compound containing 3 to 15 ethylenically unsaturated bond-containing groups, and even more preferably a compound containing 3 to 6 ethylenically unsaturated bond-containing groups. The polyfunctional polymerizable monomer is preferably a 3-15 functional (meth)acrylate compound, and more preferably a 3-6 functional (meth)acrylate compound. Specific examples of the polymerizable compound include compounds described in paragraphs 0095 to 0108 of JP 2009-288705 A, paragraph 0227 of JP 2013-029760 A, paragraphs 0254 to 0257 of JP 2008-292970 A, paragraphs 0034 to 0038 of JP 2013-253224 A, paragraph 0477 of JP 2012-208494 A, JP 2017-048367 A, Japanese Patent No. 6057891 A, Japanese Patent No. 6031807 A, and JP 2017-194662 A, the contents of which are incorporated herein by reference.

[0119] Preferred polymerizable compounds include dipentaerythritol triacrylate (commercially available product: KAYARAD D-330, manufactured by Nippon Kayaku Co., Ltd.), dipentaerythritol tetraacrylate (commercially available product: KAYARAD D-320, manufactured by Nippon Kayaku Co., Ltd.), dipentaerythritol penta(meth)acrylate (commercially available product: KAYARAD D-310, manufactured by Nippon Kayaku Co., Ltd.), dipentaerythritol hexa(meth)acrylate (commercially available products: KAYARAD DPHA, manufactured by Nippon Kayaku Co., Ltd., and NK Ester A-DPH-12E, manufactured by Shin-Nakamura Chemical Co., Ltd.), and compounds having a structure in which these (meth)acryloyl groups are bonded via ethylene glycol and / or propylene glycol residues (e.g., SR454, SR499, commercially available from Sartomer Co., Ltd.). In addition, examples of the polymerizable compound that can be used include diglycerol EO (ethylene oxide) modified (meth)acrylate (commercially available product is M-460; manufactured by Toagosei Co., Ltd.), pentaerythritol tetraacrylate (manufactured by Shin-Nakamura Chemical Co., Ltd., NK Ester A-TMMT), 1,6-hexanediol diacrylate (manufactured by Nippon Kayaku Co., Ltd., KAYARAD HDDA), RP-1040 (manufactured by Nippon Kayaku Co., Ltd.), Aronix TO-2349 (manufactured by Toagosei Co., Ltd.), NK Oligo UA-7200 (manufactured by Shin-Nakamura Chemical Co., Ltd.), 8UH-1006, 8UH-1012 (manufactured by Taisei Fine Chemical Co., Ltd.), and light acrylate POB-A0 (manufactured by Kyoeisha Chemical Co., Ltd.).

[0120] In addition, it is also preferable to use, as the polymerizable compound, a trifunctional (meth)acrylate compound such as trimethylolpropane tri(meth)acrylate, trimethylolpropane propylene oxide modified tri(meth)acrylate, trimethylolpropane ethylene oxide modified tri(meth)acrylate, isocyanuric acid ethylene oxide modified tri(meth)acrylate, or pentaerythritol tri(meth)acrylate. Commercially available trifunctional (meth)acrylate compounds include ARONIX M-309, M-310, M-321, M-350, M-360, M-313, M-315, M-306, M-305, M-303, M-452, and M-450 (manufactured by Toagosei Co., Ltd.), NK Ester A9300, A-GLY-9E, A-GLY-20E, A-TMM-3, A-TMM-3L, A-TMM-3LM-N, A-TMPT, and TMPT (manufactured by Shin-Nakamura Chemical Co., Ltd.), KAYARAD GPO-303, TMPTA, THE-330, TPA-330, and PET-30 (manufactured by Nippon Kayaku Co., Ltd.).

[0121] The polymerizable compound may also be a compound having an acid group. By using a polymerizable compound having an acid group, the polymerizable compound in the unexposed area is easily removed during development, and the generation of development residues can be suppressed. Examples of the acid group include a carboxyl group, a sulfo group, and a phosphate group, and a carboxyl group is preferred. Examples of commercially available polymerizable compounds having an acid group include ARONIX M-305, M-510, M-520, and ARONIX TO-2349 (manufactured by Toagosei Co., Ltd.). The preferred acid value of the polymerizable compound having an acid group is 0.1 to 40 mgKOH / g, and more preferably 5 to 30 mgKOH / g. If the acid value of the polymerizable compound is 0.1 mgKOH / g or more, the solubility in the developer is good, and if it is 40 mgKOH / g or less, it is advantageous in terms of production and handling.

[0122] In a preferred embodiment, the polymerizable compound is a compound having a caprolactone structure. Polymerizable compounds having a caprolactone structure are commercially available as the KAYARAD DPCA series from Nippon Kayaku Co., Ltd., and examples thereof include DPCA-20, DPCA-30, DPCA-60, and DPCA-120.

[0123] The polymerizable compound may also be a polymerizable compound having an alkyleneoxy group. The polymerizable compound having an alkyleneoxy group is preferably a polymerizable compound having an ethyleneoxy group and / or a propyleneoxy group, more preferably a polymerizable compound having an ethyleneoxy group, and even more preferably a trifunctional to hexafunctional (meth)acrylate compound having 4 to 20 ethyleneoxy groups. Examples of commercially available polymerizable compounds having an alkyleneoxy group include SR-494, a tetrafunctional (meth)acrylate having four ethyleneoxy groups manufactured by Sartomer Co., Ltd., and KAYARAD TPA-330, a trifunctional (meth)acrylate having three isobutyleneoxy groups manufactured by Nippon Kayaku Co., Ltd.

[0124] The polymerizable compound may also be a polymerizable compound having a fluorene skeleton. Commercially available polymerizable compounds having a fluorene skeleton include OGSOL EA-0200 and EA-0300 (manufactured by Osaka Gas Chemicals Co., Ltd., (meth)acrylate monomers having a fluorene skeleton).

[0125] It is also preferable to use a polymerizable compound that does not substantially contain environmentally regulated substances such as toluene. Examples of commercially available products of such compounds include KAYARAD DPHA LT and KAYARAD DPEA-12 LT (manufactured by Nippon Kayaku Co., Ltd.).

[0126] As the polymerizable compound, urethane acrylates as described in JP-B-48-041708, JP-A-51-037193, JP-B-02-032293, and JP-B-02-016765, and urethane compounds having an ethylene oxide skeleton as described in JP-B-58-049860, JP-B-56-017654, JP-B-62-039417, and JP-B-62-039418 are also suitable. In addition, it is also preferable to use polymerizable compounds having an amino structure or a sulfide structure in the molecule as described in JP-A-63-277653, JP-A-63-260909, and JP-A-01-105238. In addition, commercially available products such as UA-7200 (manufactured by Shin-Nakamura Chemical Co., Ltd.), DPHA-40H (manufactured by Nippon Kayaku Co., Ltd.), UA-306H, UA-306T, UA-306I, AH-600, T-600, AI-600, and LINC-202UA (manufactured by Kyoeisha Chemical Co., Ltd.) can also be used as the polymerizable compound.

[0127] (Compounds Having Cyclic Ether Groups) The compound having a cyclic ether group used as the curable compound is preferably a compound having an epoxy group. Examples of the compound having an epoxy group include a compound having one or more epoxy groups in one molecule, and a compound having two or more epoxy groups is preferable. The epoxy group is preferably 1 to 100 in one molecule. The upper limit of the epoxy group can be, for example, 10 or less, or 5 or less. The lower limit of the epoxy group is preferably 2 or more. As the compound having an epoxy group, the compounds described in paragraphs 0034 to 0036 of JP-A-2013-011869, the compounds described in paragraphs 0147 to 0156 of JP-A-2014-043556, the compounds described in paragraphs 0085 to 0092 of JP-A-2014-089408, and the compounds described in JP-A-2017-179172 can also be used.

[0128] The compound having an epoxy group may be a low molecular weight compound (e.g., a molecular weight less than 2000, or even less than 1000) or a high molecular weight compound (macromolecule) (e.g., a molecular weight of 1000 or more, and in the case of a polymer, a weight average molecular weight of 1000 or more). The weight average molecular weight of the compound having an epoxy group is preferably 200 to 100,000, and more preferably 500 to 50,000. The upper limit of the weight average molecular weight is preferably 10,000 or less, more preferably 5,000 or less, and even more preferably 3,000 or less.

[0129] As the compound having an epoxy group, an epoxy resin can be preferably used. Examples of the epoxy resin include an epoxy resin which is a glycidyl ether of a phenolic compound, an epoxy resin which is a glycidyl ether of various novolac resins, an alicyclic epoxy resin, an aliphatic epoxy resin, a heterocyclic epoxy resin, a glycidyl ester epoxy resin, a glycidyl amine epoxy resin, an epoxy resin obtained by glycidylating halogenated phenols, a condensate of a silicon compound having an epoxy group and another silicon compound, a copolymer of a polymerizable unsaturated compound having an epoxy group and another polymerizable unsaturated compound, and the like. The epoxy equivalent of the epoxy resin is preferably 310 to 3300 g / eq, more preferably 310 to 1700 g / eq, and even more preferably 310 to 1000 g / eq. Examples of commercially available compounds having a cyclic ether group include EHPE3150 (manufactured by Daicel Corporation), EPICLON N-695 (manufactured by DIC Corporation), Marproof G-0150M, G-0105SA, G-0130SP, G-0250SP, G-1005S, G-1005SA, G-1010S, G-2050M, G-01100, and G-01758 (all manufactured by NOF Corporation, epoxy group-containing polymers).

[0130] The content of the curable compound in the total solid content of the infrared absorbing composition is preferably 0.1 to 50 mass%. The lower limit is more preferably 0.5 mass% or more, and even more preferably 1 mass% or more. The upper limit is more preferably 45 mass% or less, and even more preferably 40 mass% or less. The curable compound may be used alone or in combination of two or more types. When two or more types are used in combination, the total of them is preferably within the above range.

[0131] When the infrared absorbing composition of the present invention contains a polymerizable compound as a curable compound, the content of the polymerizable compound in the total solid content of the infrared absorbing composition is preferably 0.1 to 50 mass%. The lower limit is more preferably 0.5 mass% or more, and even more preferably 1 mass% or more. The upper limit is more preferably 45 mass% or less, and even more preferably 40 mass% or less. The polymerizable compound may be used alone or in combination of two or more kinds. When two or more kinds are used in combination, the total of them is preferably within the above range.

[0132] When the infrared absorbing composition of the present invention contains a compound having a cyclic ether group as a curable compound, the content of the compound having a cyclic ether group in the total solid content of the infrared absorbing composition is preferably 0.1 to 20 mass%. The lower limit is preferably 0.5 mass% or more, more preferably 1 mass% or more. The upper limit is preferably 15 mass% or less, more preferably 10 mass% or less. The compound having a cyclic ether group may be used alone or in combination of two or more. When two or more types are used in combination, the total of them is preferably within the above range.

[0133] When the infrared absorbing composition of the present invention contains, as the curable compounds, a polymerizable compound and a compound having a cyclic ether group, the content of the compound having a cyclic ether group is preferably 1 to 400 parts by mass, and more preferably 1 to 100 parts by mass, relative to 100 parts by mass of the polymerizable compound.

[0134] <<Photopolymerization initiator>> When the infrared absorbing composition of the present invention contains a polymerizable compound, it is preferable that the infrared absorbing composition of the present invention further contains a photopolymerization initiator.The photopolymerization initiator is not particularly limited and can be appropriately selected from known photopolymerization initiators.For example, a compound having photosensitivity to light rays in the ultraviolet range to the visible range is preferable.The photopolymerization initiator is preferably a photoradical polymerization initiator.

[0135] Examples of the photopolymerization initiator include halogenated hydrocarbon derivatives (e.g., compounds having a triazine skeleton, compounds having an oxadiazole skeleton, etc.), acylphosphine compounds, hexaarylbiimidazole, oxime compounds, organic peroxides, thio compounds, ketone compounds, aromatic onium salts, α-hydroxyketone compounds, α-aminoketone compounds, etc. From the viewpoint of exposure sensitivity, the photopolymerization initiator is preferably a trihalomethyltriazine compound, a benzyldimethylketal compound, an α-hydroxyketone compound, an α-aminoketone compound, an acylphosphine compound, a phosphine oxide compound, a metallocene compound, an oxime compound, a triarylimidazole dimer, an onium compound, a benzothiazole compound, a benzophenone compound, an acetophenone compound, a cyclopentadiene-benzene-iron complex, a halomethyloxadiazole compound, and a 3-aryl-substituted coumarin compound, more preferably a compound selected from an oxime compound, an α-hydroxyketone compound, an α-aminoketone compound, and an acylphosphine compound, and even more preferably an oxime compound. Further, as the photopolymerization initiator, the compounds described in paragraphs 0065 to 0111 of JP 2014-130173 A and JP Patent No. 6301489 A, the peroxide-based photopolymerization initiator described in MATERIAL STAGE 37 to 60p, vol. 19, No. 3, 2019, the photopolymerization initiator described in WO 2018 / 221177 A, the photopolymerization initiator described in WO 2018 / 110179 A, ​​the photopolymerization initiator described in JP 2019-043864 A, the photopolymerization initiator described in JP 2019-044030 A, and the peroxide-based initiator described in JP 2019-167313 A can be mentioned, the contents of which are incorporated herein by reference.

[0136] Commercially available α-hydroxyketone compounds include Omnirad 184, Omnirad 1173, Omnirad 2959, Omnirad 127 (manufactured by IGM Resins BV), Irgacure 184, Irgacure 1173, Irgacure 2959, Irgacure 127 (manufactured by BASF), etc. Commercially available α-aminoketone compounds include Omnirad 907, Omnirad 369, Omnirad 369E, Omnirad 379EG (manufactured by IGM Resins BV), Irgacure 907, Irgacure 369, Irgacure 369E, Irgacure 379EG (manufactured by BASF), etc. Commercially available acylphosphine compounds include Omnirad 819, Omnirad TPO (both manufactured by IGM Resins BV), Irgacure 819, Irgacure TPO (both manufactured by BASF), and the like.

[0137] Examples of the oxime compound include compounds described in JP-A-2001-233842, compounds described in JP-A-2000-080068, compounds described in JP-A-2006-342166, compounds described in J.C.S. Perkin II (1979, pp. 1653-1660), compounds described in J.C.S. Perkin II (1979, pp. 156-162), compounds described in Journal of Photopolymer Science and Technology (1995, pp. 202-232), compounds described in JP 2000-066385 A, compounds described in JP-T-2004-534797 A, compounds described in JP-A-2017-019766 A, compounds described in Japanese Patent No. 6065596 A, compounds described in WO 2015 / 152153 A, compounds described in WO 2017 / 051680 A, compounds described in JP 2017-198865 A, compounds described in paragraphs 0025 to 0038 of WO 2017 / 164127 A, compounds described in WO 2013 / 167515 A, and the like. Specific examples of the oxime compound include 3-benzoyloxyiminobutan-2-one, 3-acetoxyiminobutan-2-one, 3-propionyloxyiminobutan-2-one, 2-acetoxyiminopentan-3-one, 2-acetoxyimino-1-phenylpropan-1-one, 2-benzoyloxyimino-1-phenylpropan-1-one, 3-(4-toluenesulfonyloxy)iminobutan-2-one, and 2-ethoxycarbonyloxyimino-1-phenylpropan-1-one. Examples of commercially available products include Irgacure OXE01, Irgacure OXE02, Irgacure OXE03, and Irgacure OXE04 (all manufactured by BASF), TR-PBG-304 (manufactured by Changzhou Strong Electronic New Materials Co., Ltd.), and Adeka Optomer N-1919 (manufactured by ADEKA Corporation, photopolymerization initiator 2 described in JP 2012-014052 A). In addition, it is also preferable to use a compound that is not colorable or a compound that is highly transparent and does not easily discolor as the oxime compound. Examples of commercially available products include Adeka Arcles NCI-730, NCI-831, and NCI-930 (all manufactured by ADEKA Corporation).

[0138] As the photopolymerization initiator, an oxime compound having a fluorene ring can also be used. Specific examples of the oxime compound having a fluorene ring include the compounds described in JP-A-2014-137466 and the compounds described in JP-A-06636081.

[0139] As the photopolymerization initiator, an oxime compound having a skeleton in which at least one benzene ring of a carbazole ring is replaced with a naphthalene ring can also be used. Specific examples of such oxime compounds include the compounds described in WO 2013 / 083505.

[0140] As the photopolymerization initiator, an oxime compound having a fluorine atom can also be used. Specific examples of the oxime compound having a fluorine atom include the compounds described in JP-A-2010-262028, compounds 24, 36 to 40 described in JP-A-2014-500852, and compound (C-3) described in JP-A-2013-164471.

[0141] As the photopolymerization initiator, an oxime compound having a nitro group can be used. It is also preferable that the oxime compound having a nitro group is a dimer. Specific examples of the oxime compound having a nitro group include the compounds described in paragraphs 0031 to 0047 of JP 2013-114249 A, paragraphs 0008 to 0012, and 0070 to 0079 of JP 2014-137466 A, the compounds described in paragraphs 0007 to 0025 of Japanese Patent No. 4223071 A, and Adeka Arcles NCI-831 (manufactured by ADEKA Corporation).

[0142] As the photopolymerization initiator, an oxime compound having a benzofuran skeleton can also be used. Specific examples include OE-01 to OE-75 described in WO 2015 / 036910.

[0143] As the photopolymerization initiator, an oxime compound in which a substituent having a hydroxyl group is bonded to a carbazole skeleton can also be used. Examples of such photopolymerization initiators include the compounds described in WO 2019 / 088055.

[0144] Specific examples of oxime compounds that can be preferably used in the present invention are shown below, but the present invention is not limited to these.

[0145] [ka] [ka]

[0146] The oxime compound is preferably a compound having a maximum absorption wavelength in the wavelength range of 350 to 500 nm, more preferably a compound having a maximum absorption wavelength in the wavelength range of 360 to 480 nm. In addition, the molar absorption coefficient of the oxime compound at a wavelength of 365 nm or 405 nm is preferably high from the viewpoint of sensitivity, more preferably 1000 to 300000, even more preferably 2000 to 300000, and particularly preferably 5000 to 200000. The molar absorption coefficient of the compound can be measured using a known method. For example, it is preferable to measure using a spectrophotometer (Varian Cary-5 spectrophotometer) using ethyl acetate as a solvent at a concentration of 0.01 g / L.

[0147] As the photopolymerization initiator, a bifunctional or trifunctional or higher functional photoradical polymerization initiator may be used. By using such a photoradical polymerization initiator, two or more radicals are generated from one molecule of the photoradical polymerization initiator, so that good sensitivity can be obtained. In addition, when a compound having an asymmetric structure is used, the crystallinity is reduced and the solubility in a solvent or the like is improved, so that precipitation is less likely to occur over time, and the stability of the composition over time can be improved. Specific examples of bifunctional or trifunctional or higher functional photoradical polymerization initiators include dimers of oxime compounds described in JP-T-2010-527339, JP-T-2011-524436, WO-P-2015 / 004565, WO-P-2016-532675, paragraphs 0407 to 0412, and WO-P-2017 / 033680, paragraphs 0039 to 0055, compounds (E) and (G) described in WO-P-2013-522445, and compounds (C) and (D) described in WO-P-2015-004565, ... Examples of the photoinitiator include Cmpd1 to 7 described in JP 2016 / 034963 A, the oxime ester photoinitiator described in paragraph 0007 of JP 2017-523465 A, the photoinitiator described in paragraphs 0020 to 0033 of JP 2017-167399 A, the photopolymerization initiator (A) described in paragraphs 0017 to 0026 of JP 2017-151342 A, and the oxime ester photoinitiator described in Japanese Patent No. 6,469,669 A.

[0148] The content of the photopolymerization initiator is preferably 0.1 to 40 mass% of the total solid content of the infrared absorbing composition, more preferably 0.5 to 30 mass%, and even more preferably 1 to 20 mass%. The infrared absorbing composition may contain only one type of photopolymerization initiator, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0149] <<Chromatic colorants>> The infrared absorbing composition of the present invention may contain a chromatic colorant. In the present invention, the chromatic colorant means a colorant other than a white colorant and a black colorant. The chromatic colorant is preferably a colorant having absorption in the wavelength range of 400 nm or more and less than 650 nm.

[0150] Examples of chromatic colorants include red colorants, green colorants, blue colorants, yellow colorants, purple colorants, and orange colorants. The chromatic colorants may be pigments or dyes. Pigments and dyes may be used in combination. The pigments may be either inorganic or organic pigments. As the pigments, materials in which inorganic pigments or organic-inorganic pigments are partially substituted with organic chromophores may also be used. Substituting inorganic pigments or organic-inorganic pigments with organic chromophores makes it easier to design the hue.

[0151] The average primary particle diameter of the pigment is preferably 1 to 200 nm. The lower limit is preferably 5 nm or more, more preferably 10 nm or more. The upper limit is preferably 180 nm or less, more preferably 150 nm or less, and even more preferably 100 nm or less. If the average primary particle diameter of the pigment is within the above range, the dispersion stability of the pigment in the infrared absorbing composition is good. In the present invention, the primary particle diameter of the pigment can be obtained by observing the primary particles of the pigment with a transmission electron microscope and obtaining an image photograph. Specifically, the projected area of ​​the primary particles of the pigment is obtained, and the corresponding circle equivalent diameter is calculated as the primary particle diameter of the pigment. In addition, the average primary particle diameter in the present invention is the arithmetic average value of the primary particle diameters of 400 primary particles of the pigment. In addition, the primary particles of the pigment refer to independent particles without aggregation.

[0152] The chromatic colorant preferably contains a pigment. The content of the pigment in the chromatic colorant is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, and particularly preferably 90% by mass or more. Examples of the pigment include the following.

[0153] Color Index (CI) Pigment Yellow 1,2,3,4,5,6,10,11,12,13,14,15,16,17,18,20,24,31,32,34,35,35:1,36,36:1,37,37:1,40,42,43,53,55,60,61,62,63,65,73,74,77,81,83,86,93,94,95,97,98,100,101,104,106,108,109,110,113,114,115,116,117,118,119,120,123,125,126,127,128,129,137,13 8,139,147,148,150,151,152,153,154,155,156,161,162,164,166,167,168,169,170,171,172,173,174,175,176,177,179,180,181,182,185,187,188,193,194,199,213,214,215,228,231,232 (methine type), 233 (quinoline type), 234 (amino ketone type), 235 (amino ketone type), 236 (amino ketone type), etc. (above, yellow pigments), CI Pigment Orange 2, 5, 13, 16, 17:1, 31, 34, 36, 38, 43, 46, 48, 49, 51, 52, 55, 59, 60, 61, 62, 64, 71, 73, etc. (orange pigments) CIPigment Red 1,2,3,4,5,6,7,9,10,14,17,22,23,31,38,41,48:1,48:2,48:3,48:4,49,49:1,49:2,52:1,52:2,5 3:1,57:1,60:1,63:1,66,67,81:1,81:2,81:3,83,88,90,105,112,119,122,123,144,146,149,150, 155,166,168,169,170,171,172,175,176,177,178,179,184,185,187,188,190,200,202,206,207,208,209,210,216,220,224,226,242,246,254,255,264,269,270,272,279,291,294 (xanthene, Organo Ultramarine, Bluish Red), 295 (monoazo), 296 (diazo), 297 (aminoketone), etc. (above, red pigments), CI Pigment Green 7, 10, 36, 37, 58, 59, 62, 63, 64 (phthalocyanine type), 65 (phthalocyanine type), 66 (phthalocyanine type), etc. (above, green pigments), CI Pigment Violet 1, 19, 23, 27, 32, 37, 42, 60 (triarylmethane type), 61 (xanthene type), etc. (purple pigments) CI Pigment Blue 1, 2, 15, 15:1, 15:2, 15:3, 15:4, 15:6, 16, 22, 29, 60, 64, 66, 79, 80, 87 (monoazo type), 88 (methine type), etc. (all blue pigments).

[0154] In addition, as the green pigment, a halogenated zinc phthalocyanine pigment having an average of 10 to 14 halogen atoms, an average of 8 to 12 bromine atoms, and an average of 2 to 5 chlorine atoms in one molecule can also be used. Specific examples include compounds described in International Publication No. 2015 / 118720. In addition, as the green pigment, compounds described in Chinese Patent Application No. 106909027, phthalocyanine compounds having a phosphoric acid ester as a ligand described in International Publication No. 2012 / 102395, phthalocyanine compounds described in JP-A-2019-008014, phthalocyanine compounds described in JP-A-2018-180023, compounds described in JP-A-2019-038958, and the like can also be used.

[0155] In addition, an aluminum phthalocyanine compound having a phosphorus atom can also be used as a blue pigment. Specific examples include the compounds described in paragraphs 0022 to 0030 of JP-A No. 2012-247591 and paragraph 0047 of JP-A No. 2011-157478.

[0156] Further, as yellow pigments, compounds described in JP-A-2017-201003, compounds described in JP-A-2017-197719, compounds described in paragraphs 0011 to 0062 and 0137 to 0276 of JP-A-2017-171912, compounds described in paragraphs 0010 to 0062 and 0138 to 0295 of JP-A-2017-171913, compounds described in paragraphs 0011 to 0062 and 0139 to 0190 of JP-A-2017-171914, compounds described in paragraphs 0010 to 0065 and 0142 to 0222 of JP-A-2017-171915, , quinophthalone compounds described in paragraphs 0011 to 0034 of JP 2013-054339 A, quinophthalone compounds described in paragraphs 0013 to 0058 of JP 2014-026228 A, isoindoline compounds described in JP 2018-062644 A, quinophthalone compounds described in JP 2018-203798 A, quinophthalone compounds described in JP 2018-062578 A, quinophthalone compounds described in Japanese Patent No. 6432076, quinophthalone compounds described in JP 2018-155881 A, JP 2018-1117 57, quinophthalone compounds described in JP 2018-040835 A, quinophthalone compounds described in JP 2017-197640 A, quinophthalone compounds described in JP 2016-145282 A, quinophthalone compounds described in JP 2014-085565 A, quinophthalone compounds described in JP 2014-021139 A, quinophthalone compounds described in JP 2013-209614 A, quinophthalone compounds described in JP 2013-209435 A, quinophthalone compounds described in JP 2013-181015 A Quinophthalone compounds, quinophthalone compounds described in JP 2013-061622 A, quinophthalone compounds described in JP 2013-032486 A, quinophthalone compounds described in JP 2012-226110 A, quinophthalone compounds described in JP 2008-074987 A, quinophthalone compounds described in JP 2008-081565 A, quinophthalone compounds described in JP 2008-074986 A, quinophthalone compounds described in JP 2008-074985 A, quinophthalone compounds described in JP 2008-050420 A,Quinophthalone compounds described in JP 2008-031281 A, JP 48-032765 B, JP 2019-008014 A, JP 6607427 A, compounds described in Korean Patent Publication No. 10-2014-0034963, compounds described in JP 2017-095706 A, compounds described in Taiwan Patent Publication No. 201920495, JP 6607427 A Compounds described in JP-A-2020-033525, compounds described in JP-A-2020-033524, compounds described in JP-A-2020-033523, compounds described in JP-A-2020-033522, compounds described in JP-A-2020-033521, compounds described in WO 2020 / 045200, compounds described in WO 2020 / 045199, and compounds described in WO 2020 / 045197 can also be used. In addition, oligomers of these compounds are also preferably used from the viewpoint of improving color value. ,

[0157] As the red pigment, a diketopyrrolopyrrole compound in which at least one bromine atom is substituted in the structure described in JP 2017-201384 A, a diketopyrrolopyrrole compound described in paragraphs 0016 to 0022 of Japanese Patent No. 6248838 A, a diketopyrrolopyrrole compound described in WO 2012 / 102399 A, a diketopyrrolopyrrole compound described in WO 2012 / 117965 A, a naphthol azo compound described in JP 2012-229344 A, etc. can also be used. In addition, as the red pigment, a compound having a structure in which an aromatic ring group in which a group in which an oxygen atom, a sulfur atom or a nitrogen atom is bonded to an aromatic ring is introduced and bonded to a diketopyrrolopyrrole skeleton can also be used.

[0158] In the present invention, dyes can also be used as the chromatic colorant. There is no particular limitation on the dye, and known dyes can be used. For example, pyrazole azo dyes, anilino azo dyes, triarylmethane dyes, anthraquinone dyes, anthrapyridone dyes, benzylidene dyes, oxonol dyes, pyrazolotriazole azo dyes, pyridone azo dyes, cyanine dyes, phenothiazine dyes, pyrrolopyrazole azomethine dyes, xanthene dyes, phthalocyanine dyes, benzopyran dyes, indigo dyes, pyrromethene dyes, etc. can be mentioned. In addition, thiazole compounds described in JP-A-2012-158649, azo compounds described in JP-A-2011-184493, and azo compounds described in JP-A-2011-145540 can also be preferably used as the dye.

[0159] When the infrared absorbing composition of the present invention contains a chromatic colorant, the content of the chromatic colorant is preferably 1 to 50 mass % of the total solid content of the infrared absorbing composition of the present invention. When the infrared absorbing composition of the present invention contains two or more chromatic colorants, the total amount thereof is preferably within the above range.

[0160] <<Coloring material that transmits infrared rays but blocks visible light>> The infrared absorbing composition of the present invention may also contain a coloring material that transmits infrared rays and blocks visible light (hereinafter, also referred to as a coloring material that blocks visible light). The infrared absorbing composition containing a coloring material that blocks visible light is preferably used as an infrared absorbing composition for forming an infrared transmission filter.

[0161] The coloring material that blocks visible light is preferably a coloring material that absorbs light in the purple to red wavelength region. Also, the coloring material that blocks visible light is preferably a coloring material that blocks light in the wavelength region of 450 to 650 nm. Also, the coloring material that blocks visible light is preferably a coloring material that transmits light in the wavelength region of 900 to 1500 nm. The coloring material that blocks visible light preferably satisfies at least one of the following requirements (A) and (B). (A): Contains two or more types of chromatic colorants, and forms black with a combination of two or more types of chromatic colorants. (B): Contains an organic black colorant.

[0162] Examples of the chromatic colorant include those mentioned above. Examples of the organic black colorant include bisbenzofuranone compounds, azomethine compounds, perylene compounds, and azo compounds, and bisbenzofuranone compounds and perylene compounds are preferred. Examples of the bisbenzofuranone compounds include compounds described in JP-T-2010-534726, JP-T-2012-515233, and JP-T-2012-515234, and are available as "Irgaphor Black" manufactured by BASF. Examples of the perylene compounds include compounds described in paragraphs 0016 to 0020 of JP-A-2017-226821, CI Pigment Black 31, 32, and the like. Examples of the azomethine compound include compounds described in JP-A-01-170601 and JP-A-02-034664, and are available as "Chromofine Black A1103" manufactured by Dainichi Seika Chemicals Co., Ltd.

[0163] When black color is formed by combining two or more chromatic colorants, the combination of chromatic colorants may be, for example, the following embodiments (1) to (8). (1) An embodiment containing a yellow colorant, a blue colorant, a purple colorant, and a red colorant. (2) An embodiment containing a yellow colorant, a blue colorant, and a red colorant. (3) An embodiment containing a yellow colorant, a purple colorant, and a red colorant. (4) An embodiment containing a yellow colorant and a purple colorant. (5) An embodiment containing a green colorant, a blue colorant, a purple colorant, and a red colorant. (6) An embodiment containing a purple colorant and an orange colorant. (7) An embodiment containing a green colorant, a purple colorant, and a red colorant. (8) An embodiment containing a green colorant and a red colorant.

[0164] When the infrared absorbing composition of the present invention contains a coloring material that blocks visible light, the content of the coloring material that blocks visible light is preferably 1 to 50 mass% of the total solid content of the infrared absorbing composition. The lower limit is preferably 5 mass% or more, more preferably 10 mass% or more, even more preferably 20 mass% or more, and particularly preferably 30 mass% or more.

[0165] <<Surfactants>> The infrared absorbing composition of the present invention preferably contains a surfactant. As the surfactant, various surfactants such as fluorine-based surfactants, nonionic surfactants, cationic surfactants, anionic surfactants, and silicone-based surfactants can be used. The surfactant is preferably a fluorine-based surfactant or a silicone-based surfactant. As the surfactant, the surfactants described in paragraphs 0238 to 0245 of WO 2015 / 166779 can be mentioned, the contents of which are incorporated herein. The surfactant can also be used as a dispersant for specific particles.

[0166] Examples of fluorine-based surfactants include those described in JP2014-041318A, paragraphs 0060 to 0064 (corresponding to WO2014 / 017669, paragraphs 0060 to 0064) and those described in JP2011-132503A, paragraphs 0117 to 0132, the contents of which are incorporated herein by reference. Commercially available fluorine-based surfactants include, for example, Megafac F-171, F-172, F-173, F-176, F-177, F-141, F-142, F-143, F-144, F-437, F-475, F-477, F-479, F-482, F-554, F-555-A, F-556, F-557, F-558, F-559, F-560, F-561, F-565, F-563, F-568, F-575, F-780, EXP, MFS-330, and R-41. , R-41-LM, R-01, R-40, R-40-LM, RS-43, TF-1956, RS-90, R-94, RS-72-K, DS-21 (all manufactured by DIC Corporation), Fluorard FC430, FC431, FC171 (all manufactured by Sumitomo 3M Limited), Surflon S-382, SC-101, SC-103, SC-104, SC-105, SC-1068, SC-381, SC-383, S-393, KH-40 (all manufactured by AGC Corporation), PolyFox Examples of such agents include PF636, PF656, PF6320, PF6520, and PF7002 (all manufactured by OMNOVA), and Ftergent 710FM, 610FM, 601AD, 601ADH2, 602A, 215M, and 245F (all manufactured by NEOS Corporation).

[0167] In addition, the fluorosurfactant may be an acrylic compound that has a molecular structure with a functional group containing a fluorine atom, and when heat is applied, the functional group containing the fluorine atom is broken and the fluorine atom volatilizes. Examples of such fluorosurfactants include the Megafac DS series manufactured by DIC Corporation (The Chemical Daily (February 22, 2016), Nikkei Business Daily (February 23, 2016)), such as Megafac DS-21.

[0168] In addition, it is also preferable to use a polymer of a fluorine atom-containing vinyl ether compound having a fluorinated alkyl group or a fluorinated alkylene ether group and a hydrophilic vinyl ether compound as the fluorine-based surfactant. Examples of such a fluorine-based surfactant include the fluorine-based surfactants described in JP 2016-216602 A, the contents of which are incorporated herein by reference.

[0169] The fluorosurfactant may be a block polymer. The fluorosurfactant may be a fluorine-containing polymer compound that contains a repeating unit derived from a (meth)acrylate compound having a fluorine atom and a repeating unit derived from a (meth)acrylate compound having two or more (preferably five or more) alkyleneoxy groups (preferably ethyleneoxy groups, propyleneoxy groups). In addition, the fluorine-containing surfactants described in paragraphs 0016 to 0037 of JP-A-2010-032698 and the following compounds are also exemplified as the fluorosurfactant used in the present invention. [ka] The weight average molecular weight of the above compound is preferably 3,000 to 50,000, for example, 14,000. In the above compound, % indicating the proportion of repeating units is mol %.

[0170] In addition, the fluorine-based surfactant may be a fluorine-containing polymer having an ethylenically unsaturated bond-containing group in a side chain.Specific examples include the compounds described in paragraphs 0050 to 0090 and 0289 to 0295 of JP 2010-164965 A, and Megafac RS-101, RS-102, RS-718K, and RS-72-K manufactured by DIC Corporation.In addition, the fluorine-based surfactant may be the compounds described in paragraphs 0015 to 0158 of JP 2015-117327 A.

[0171] Examples of nonionic surfactants include glycerol, trimethylolpropane, trimethylolethane, and their ethoxylates and propoxylates (e.g., glycerol propoxylate, glycerol ethoxylate, etc.), polyoxyethylene lauryl ether, polyoxyethylene stearyl ether, polyoxyethylene oleyl ether, polyoxyethylene octylphenyl ether, polyoxyethylene nonylphenyl ether, polyethylene glycol dilaurate, polyethylene glycol distearate, and sorbitan fat. Examples of the fatty acid ester include Pluronic L10, L31, L61, L62, 10R5, 17R2, and 25R2 (manufactured by BASF), Tetronic 304, 701, 704, 901, 904, and 150R1 (manufactured by BASF), Solsperse 20000 (manufactured by Lubrizol Japan Co., Ltd.), NCW-101, NCW-1001, and NCW-1002 (manufactured by Wako Pure Chemical Industries, Ltd.), Paionin D-6112, D-6112-W, and D-6315 (manufactured by Takemoto Oil Co., Ltd.), Olfin E1010, and Surfynol 104, 400, and 440 (manufactured by Nissin Chemical Industry Co., Ltd.).

[0172] Examples of cationic surfactants include tetraalkylammonium salts, alkylamine salts, benzalkonium salts, alkylpyridinium salts, imidazolium salts, etc. Specific examples include dihydroxyethylstearylamine, 2-heptadecenyl-hydroxyethylimidazoline, lauryldimethylbenzylammonium chloride, cetylpyridinium chloride, stearamidomethylpyridinium chloride, etc.

[0173] Examples of anionic surfactants include dodecylbenzenesulfonic acid, sodium dodecylbenzenesulfonate, sodium lauryl sulfate, sodium alkyldiphenyletherdisulfonate, sodium alkylnaphthalenesulfonate, sodium dialkylsulfosuccinate, sodium stearate, potassium oleate, sodium dioctyl sulfosuccinate, sodium polyoxyethylene alkyl ether sulfate, sodium polyoxyethylene alkyl ether sulfate, sodium polyoxyethylene alkylphenyl ether sulfate, sodium dialkylsulfosuccinate, sodium stearate, sodium oleate, and sodium t-octylphenoxyethoxypolyethoxyethyl sulfate.

[0174] Examples of silicone surfactants include Toray Silicone DC3PA, Toray Silicone SH7PA, Toray Silicone DC11PA, Toray Silicone SH21PA, Toray Silicone SH28PA, Toray Silicone SH29PA, Toray Silicone SH30PA, and Toray Silicone SH8400 (manufactured by Toray Dow Corning Co., Ltd.), TSF-4440, TSF-4300, TSF-4445, TSF-4460, and TSF-4452 (manufactured by Momentive Performance Materials, Inc.), KP-341, KF-6000, KF-6001, KF-6002, and KF-6003 (manufactured by Shin-Etsu Chemical Co., Ltd.), BYK307, BYK323, and BYK330 (manufactured by BYK-Chemie).

[0175] The content of the surfactant is preferably from 0.001 to 1 mass %, more preferably from 0.001 to 0.5 mass %, and even more preferably from 0.001 to 0.2 mass %, based on the total solid content of the infrared absorbing composition.

[0176] When a surfactant is used as a dispersant for the specific particles, the content of the surfactant is preferably 1 to 200 parts by mass, more preferably 2 to 100 parts by mass, and even more preferably 5 to 50 parts by mass, per 100 parts by mass of the specific particles.

[0177] The infrared absorbing composition may contain only one type of surfactant, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0178] <<Polymerization inhibitor>> The infrared absorbing composition of the present invention may contain a polymerization inhibitor. Examples of the polymerization inhibitor include hydroquinone, p-methoxyphenol, di-tert-butyl-p-cresol, pyrogallol, tert-butylcatechol, benzoquinone, 4,4'-thiobis(3-methyl-6-tert-butylphenol), 2,2'-methylenebis(4-methyl-6-t-butylphenol), and N-nitrosophenylhydroxyamine salts (ammonium salts, cerous salts, etc.), and p-methoxyphenol is preferred. The content of the polymerization inhibitor is preferably 0.0001 to 5 mass% of the total solid content of the infrared absorbing composition. The infrared absorbing composition may contain only one type of polymerization inhibitor, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0179] <<Silane coupling agents>> The infrared absorbing composition of the present invention may contain a silane coupling agent. In this specification, the silane coupling agent means a silane compound having a hydrolyzable group and other functional groups. The hydrolyzable group means a substituent that is directly bonded to a silicon atom and can generate a siloxane bond by at least one of a hydrolysis reaction and a condensation reaction. Examples of the hydrolyzable group include a halogen atom, an alkoxy group, and an acyloxy group, and an alkoxy group is preferred. That is, the silane coupling agent is preferably a compound having an alkoxysilyl group. Examples of functional groups other than the hydrolyzable group include a vinyl group, a styryl group, a (meth)acryloyl group, a mercapto group, an epoxy group, an oxetanyl group, an amino group, a ureido group, a sulfide group, an isocyanate group, and a phenyl group, and a (meth)acryloyl group and an epoxy group are preferred. Examples of the silane coupling agent include compounds described in paragraphs 0018 to 0036 of JP-A-2009-288703 and compounds described in paragraphs 0056 to 0066 of JP-A-2009-242604, the contents of which are incorporated herein by reference. The content of the silane coupling agent is preferably 0.01 to 15.0 mass% of the total solid content of the infrared absorbing composition, more preferably 0.05 to 10.0 mass%. The infrared absorbing composition may contain only one type of silane coupling agent, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0180] <<Ultraviolet absorber>> The infrared absorbing composition may contain an ultraviolet absorbing agent. Examples of ultraviolet absorbing agents include conjugated diene compounds, aminodiene compounds, salicylate compounds, benzophenone compounds, benzotriazole compounds, acrylonitrile compounds, hydroxyphenyltriazine compounds, indole compounds, triazine compounds, and merocyanine dyes. Specific examples of such compounds include those described in paragraphs 0038-0052 of JP 2009-217221 A, paragraphs 0052-0072 of JP 2012-208374 A, paragraphs 0317-0334 of JP 2013-068814 A, and paragraphs 0061-0080 of JP 2016-162946 A, the contents of which are incorporated herein by reference. Commercially available ultraviolet absorbing agents include the Tinuvin series and Uvinul series manufactured by BASF. In addition, examples of the benzotriazole compound include the MYUA series manufactured by Miyoshi Oil & Fat (The Chemical Daily, February 1, 2016). In addition, the ultraviolet absorber may be a compound described in paragraphs 0049-0059 of Japanese Patent No. 6268967 and paragraphs 0059-0076 of International Publication No. 2016 / 181987. The content of the ultraviolet absorber is preferably 0.01-30% by mass, more preferably 0.05-25% by mass, based on the total solid content of the infrared absorbing composition. The infrared absorbing composition may contain only one type of ultraviolet absorber, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0181] <<Antioxidants>> The infrared absorbing composition of the present invention may contain an antioxidant. Examples of the antioxidant include phenolic compounds, phosphite compounds, and thioether compounds. As the phenolic compound, any phenolic compound known as a phenolic antioxidant may be used. Examples of preferred phenolic compounds include hindered phenolic compounds. Compounds having a substituent at the site (ortho position) adjacent to the phenolic hydroxyl group are preferred. As the aforementioned substituent, a substituted or unsubstituted alkyl group having 1 to 22 carbon atoms is preferred. In addition, as the antioxidant, a compound having a phenolic group and a phosphite group in the same molecule is also preferred. As the antioxidant, a phosphorus-based antioxidant may also be suitably used. Examples of phosphorus-based antioxidants include tris[2-[[2,4,8,10-tetrakis(1,1-dimethylethyl)dibenzo[d,f][1,3,2]dioxaphosphepin-6-yl]oxy]ethyl]amine, tris[2-[(4,6,9,11-tetra-tert-butyldibenzo[d,f][1,3,2]dioxaphosphepin-2-yl)oxy]ethyl]amine, and ethyl bis(2,4-di-tert-butyl-6-methylphenyl)phosphite. Examples of commercially available antioxidants include ADK STAB AO-20, ADK STAB AO-30, ADK STAB AO-40, ADK STAB AO-50, ADK STAB AO-50F, ADK STAB AO-60, ADK STAB AO-60G, ADK STAB AO-80, and ADK STAB AO-330 (all manufactured by ADEKA CORPORATION). In addition, the antioxidant may be a compound described in paragraphs 0023 to 0048 of Japanese Patent No. 6268967, a compound described in International Publication No. WO 2017 / 006600, or a compound described in International Publication No. WO 2017 / 164024. The content of the antioxidant is preferably 0.01 to 20% by mass, more preferably 0.3 to 15% by mass, based on the total solid content of the infrared absorbing composition. The infrared absorbing composition may contain only one type of antioxidant, or may contain two or more types. When two or more types are contained, the total amount thereof is preferably within the above range.

[0182] <<Other ingredients>> The infrared absorbing composition of the present invention may contain, as necessary, a sensitizer, a curing accelerator, a filler, a heat curing accelerator, a plasticizer, and other auxiliaries (for example, conductive particles, a filler, an antifoaming agent, a flame retardant, a leveling agent, a peeling accelerator, a fragrance, a surface tension modifier, a chain transfer agent, etc.). By appropriately incorporating these components, it is possible to adjust properties such as film properties. For these components, for example, the description in paragraphs 0183 and after of JP 2012-003225 A (corresponding to paragraph 0237 of the specification of US Patent Application Publication No. 2013 / 0034812), and the description in paragraphs 0101 to 0104, 0107 to 0109, etc. of JP 2008-250074 A can be referred to, and the contents of these are incorporated herein. In addition, the infrared absorbing composition of the present invention may contain, as necessary, a latent antioxidant. Examples of the latent antioxidant include compounds in which the site functioning as an antioxidant is protected by a protecting group, and the protecting group is removed by heating at 100 to 250° C. or at 80 to 200° C. in the presence of an acid / base catalyst, thereby functioning as an antioxidant. Examples of the latent antioxidant include compounds described in International Publication No. 2014 / 021023, International Publication No. 2017 / 030005, and JP-A No. 2017-008219. Examples of commercially available latent antioxidants include ADEKA ARCLES GPA-5001 (manufactured by ADEKA Corporation).

[0183] Furthermore, when the infrared absorbing composition of the present invention is used as various inks such as inkjet inks and printing inks, other additives such as lubricants, fillers, defoamers, gelling agents, thickeners, resistivity adjusters, film-forming agents, anti-fading agents, anti-mold agents, and anti-rust agents can be blended in. Examples of these additives include those described in paragraphs 0163 to 0170 of JP2014-024980A, the contents of which are incorporated herein by reference.

[0184] <Containment Container> The container for storing the infrared absorbing composition of the present invention is not particularly limited, and a known container can be used. In addition, it is also preferable to use a multi-layer bottle whose inner wall is made of six types of six-layer resin or a bottle with a seven-layer structure made of six types of resin as the container, in order to suppress the incorporation of impurities into the raw materials or the infrared absorbing composition. Examples of such containers include the containers described in JP-A-2015-123351. In addition, it is also preferable that the inner wall of the container is made of glass or stainless steel in order to prevent metal elution from the inner wall of the container, increase the storage stability of the infrared absorbing composition, and suppress the deterioration of the components.

[0185] <Method for preparing infrared absorbing composition> The infrared absorbing composition of the present invention can be prepared by mixing the above-mentioned components. When preparing the infrared absorbing composition, all the components may be simultaneously dissolved or dispersed in a solvent to prepare the infrared absorbing composition, or, if necessary, two or more solutions or dispersions in which the components are appropriately mixed may be prepared in advance, and these may be mixed at the time of use (application) to prepare the composition.

[0186] It is preferable that the infrared absorbing composition is prepared by including a process for dispersing particles. In the process for dispersing particles, examples of mechanical forces used for dispersing particles include compression, squeezing, impact, shear, and cavitation. Specific examples of these processes include a bead mill, a sand mill, a roll mill, a ball mill, a paint shaker, a microfluidizer, a high-speed impeller, a sand grinder, a flow jet mixer, high-pressure wet atomization, and ultrasonic dispersion. In addition, in the grinding of particles in a sand mill (bead mill), it is preferable to use beads with a small diameter, increase the filling rate of beads, and perform the treatment under conditions that increase the grinding efficiency. In addition, it is preferable to remove coarse particles by filtration, centrifugation, or the like after the grinding treatment. In addition, the process and dispersing machine for dispersing particles can be suitably used as described in "Dispersion Technology Encyclopedia, published by Information Technology Co., Ltd., July 15, 2005" or "Suspension (solid / liquid dispersion system)-centered dispersion technology and industrial application practice general data collection, published by Management Development Center Publishing Department, October 10, 1978", and JP2015-157893A, paragraph number 0022. In addition, in the process for dispersing particles, a salt milling process may be performed to refine the particles. The materials, equipment, processing conditions, etc. used in the salt milling process can be referred to, for example, JP2015-194521A and JP2012-046629A.

[0187] In preparing the infrared absorbing composition, it is preferable to filter the infrared absorbing composition with a filter for the purpose of removing foreign matter and reducing defects. As the filter, any filter that has been used for filtering purposes can be used without any particular limitation. For example, there are filters using materials such as fluororesins such as polytetrafluoroethylene (PTFE), polyamide resins such as nylon (e.g., nylon-6, nylon-6,6), and polyolefin resins such as polyethylene and polypropylene (PP) (including high-density and ultra-high-molecular-weight polyolefin resins). Among these materials, polypropylene (including high-density polypropylene) and nylon are preferred.

[0188] The pore size of the filter is preferably 0.01 to 7.0 μm, more preferably 0.01 to 3.0 μm, and even more preferably 0.05 to 0.5 μm. If the pore size of the filter is within the above range, fine foreign matter can be removed more reliably. The nominal value of the filter manufacturer can be referred to for the pore size value of the filter. Various filters provided by Nippon Pall Corporation (DFA4201NIEY, DFA4201NAEY, DFA4201J006P, etc.), Advantech Toyo Co., Ltd., Nippon Integris Co., Ltd. (formerly Nippon Microlith Co., Ltd.), Kitz Microfilter Co., Ltd., etc. can be used.

[0189] It is also preferable to use a fibrous filter medium as the filter. Examples of fibrous filter medium include polypropylene fiber, nylon fiber, glass fiber, etc. Commercially available products include SBP type series (SBP008, etc.), TPR type series (TPR002, TPR005, etc.), and SHPX type series (SHPX003, etc.) manufactured by ROKI TECHNO CO., LTD.

[0190] When using a filter, different filters (for example, a first filter and a second filter, etc.) may be combined. In this case, filtration with each filter may be performed only once or two or more times. Filters having different pore sizes within the above-mentioned range may be combined. Filtration with the first filter may be performed only on the dispersion liquid, and filtration with the second filter may be performed after mixing with other components.

[0191] <Membrane> Next, the film of the present invention will be described. The film of the present invention is obtained from the infrared absorbing composition of the present invention described above. The film of the present invention can be preferably used as an optical filter. The use of the optical filter is not particularly limited, but it can be preferably used as a near-infrared cut filter on the light receiving side of a solid-state imaging element (for example, for a near-infrared cut filter for a wafer level lens), a near-infrared cut filter on the back side (opposite the light receiving side) of a solid-state imaging element, a near-infrared cut filter for an environmental light sensor (for example, an illuminance sensor that senses the illuminance and color tone of the environment in which an information terminal device is placed and adjusts the color tone of the display, or a color correction sensor that adjusts the color tone). In particular, it can be preferably used as a near-infrared cut filter on the light receiving side of a solid-state imaging element. It can also be used as a near-infrared cut filter for an infrared sensor that detects an object by detecting light with a wavelength of 700 to 1550 nm. It can also be used to form an infrared transmission filter that can transmit only near-infrared rays of a specific wavelength or more by using an infrared absorbing composition containing a color material that transmits infrared rays and blocks visible light. For example, an infrared transmission filter that blocks wavelengths from 400 to 900 nm and transmits near infrared rays having wavelengths of 900 nm or more can be formed. The film of the present invention may have a pattern or may be a film (flat film) that does not have a pattern. The film of the present invention may be used by being laminated on a support, or may be used by peeling off the film from the support. Examples of the support include a semiconductor substrate such as a silicon substrate, and a transparent substrate.

[0192] A charge-coupled device (CCD), a complementary metal oxide semiconductor (CMOS), a transparent conductive film, etc. may be formed on the semiconductor substrate used as a support. A black matrix for isolating each pixel may also be formed on the semiconductor substrate. If necessary, an undercoat layer may be provided on the semiconductor substrate to improve adhesion with an upper layer, prevent diffusion of substances, or flatten the substrate surface.

[0193] The transparent substrate used as the support is not particularly limited as long as it is made of a material that can transmit at least visible light. For example, the substrate may be made of a material such as glass or resin. Examples of the resin include polyester resins such as polyethylene terephthalate and polybutylene terephthalate, polyolefin resins such as polyethylene, polypropylene, and ethylene-vinyl acetate copolymer, acrylic resins such as norbornene resin, polyacrylate, and polymethyl methacrylate, urethane resin, vinyl chloride resin, fluororesin, polycarbonate resin, polyvinyl butyral resin, and polyvinyl alcohol resin. Examples of the glass include soda-lime glass, borosilicate glass, alkali-free glass, quartz glass, and glass containing copper. Examples of the glass containing copper include phosphate glass containing copper and fluorophosphate glass containing copper. The glass containing copper may be a commercially available product. Examples of the glass containing copper include NF-50 (manufactured by AGC Technoglass Co., Ltd.).

[0194] The thickness of the membrane of the present invention can be appropriately adjusted depending on the purpose. The thickness of the membrane is preferably 20 μm or less, more preferably 10 μm or less, and even more preferably 5 μm or less. The lower limit of the membrane thickness is preferably 0.1 μm or more, and more preferably 0.2 μm or more.

[0195] When the film of the present invention is used as an infrared cut filter, the film of the present invention preferably has a maximum absorption wavelength in the wavelength range of 650 to 1500 nm (preferably 700 to 1300 nm, more preferably 700 to 1000 nm). In addition, the average transmittance of light with a wavelength of 400 to 600 nm is preferably 50% or more, more preferably 70% or more, even more preferably 80% or more, and particularly preferably 85% or more. In addition, the transmittance in the entire wavelength range of 400 to 600 nm is preferably 50% or more, more preferably 70% or more, and even more preferably 80% or more. In addition, the film of the present invention preferably has a transmittance of 15% or less, more preferably 10% or less, and even more preferably 5% or less at at least one point in the wavelength range of 650 to 1500 nm (preferably 700 to 1300 nm, more preferably 700 to 1000 nm). Furthermore, in the film of the present invention, the ratio (A1 / A2) of the maximum absorbance A1 in the wavelength range of 400 to 600 nm to the absorbance A2 at the maximum absorption wavelength on the shortest side in the wavelength range of 650 to 1500 nm is preferably 0.30 or less, more preferably 0.20 or less, even more preferably 0.15 or less, and particularly preferably 0.10 or less.

[0196] When the film of the present invention is used as an infrared transmission filter, it is preferable that the maximum transmittance in the wavelength range of 400 to 830 nm is 20% or less (preferably 15% or less, more preferably 10% or less) and the minimum transmittance in the wavelength range of 1100 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). The film of the present invention used as an infrared transmission filter preferably satisfies any one of the following spectral characteristics (1) to (4). (1): The maximum transmittance in the wavelength range of 400 to 750 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum transmittance in the wavelength range of 900 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (2): The maximum transmittance in the wavelength range of 400 to 830 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum transmittance in the wavelength range of 1000 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (3): The maximum transmittance in the wavelength range of 400 to 950 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum transmittance in the wavelength range of 1100 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more). (4): The maximum transmittance in the wavelength range of 400 to 1050 nm is 20% or less (preferably 15% or less, more preferably 10% or less), and the minimum transmittance in the wavelength range of 1200 to 1500 nm is 70% or more (preferably 75% or more, more preferably 80% or more).

[0197] The film of the present invention can also be used in combination with a color filter containing a chromatic colorant. The color filter can be manufactured using a coloring composition containing a chromatic colorant. When the film of the present invention is used as an infrared cut filter and is used in combination with the film of the present invention and a color filter, it is preferable that a color filter is arranged on the optical path of the film of the present invention. For example, it is preferable to use the film of the present invention and a color filter as a laminate by laminating them. In the laminate, the film of the present invention and the color filter may be adjacent to each other in the thickness direction, or may not be adjacent to each other. When the film of the present invention and the color filter are not adjacent to each other in the thickness direction, the film of the present invention may be formed on a support other than the support on which the color filter is formed, and other members (e.g., microlenses, flattening layers, etc.) constituting a solid-state imaging device may be interposed between the film of the present invention and the color filter.

[0198] The film of the present invention can be used in various devices such as solid-state imaging devices such as CCDs (charge-coupled devices) and CMOSs ​​(complementary metal-oxide semiconductors), infrared sensors, and image display devices.

[0199] <Membrane manufacturing method> The film of the present invention can be produced via a step of applying the infrared absorbing composition of the present invention.

[0200] Examples of the support include those mentioned above. A known method can be used as a coating method for the infrared absorbing composition. Examples include a dropping method (drop casting); a slit coating method; a spray method; a roll coating method; a rotary coating method (spin coating); a casting coating method; a slit and spin method; a pre-wetting method (for example, a method described in JP-A-2009-145395); various printing methods such as inkjet (for example, on-demand method, piezo method, thermal method), ejection printing such as nozzle jet, flexographic printing, screen printing, gravure printing, reverse offset printing, and metal mask printing; a transfer method using a mold, etc.; and a nanoimprint method. The application method for inkjet is not particularly limited, and examples thereof include the method described in “Expanding and Usable Inkjet - Infinite Possibilities Seen in Patents -”, published in February 2005 by Sumibe Techno Research (particularly pages 115 to 133) and the methods described in JP-A Nos. 2003-262716, 2003-185831, 2003-261827, 2012-126830, and 2006-169325.

[0201] The infrared absorbing composition layer formed by applying the infrared absorbing composition may be dried (prebaked). When prebaking is performed, the prebaking temperature is preferably 150° C. or lower, more preferably 120° C. or lower, and even more preferably 110° C. or lower. The lower limit can be, for example, 50° C. or higher, and can also be 80° C. or higher. The prebaking time is preferably 10 seconds to 3000 seconds, more preferably 40 to 2500 seconds, and even more preferably 80 to 220 seconds. Drying can be performed using a hot plate, an oven, or the like.

[0202] The infrared absorbing composition layer after pre-baking may be further baked. By performing the additional bake, it is possible to further reduce the aggregation of infrared absorbing dye particles that occurs during post-baking, and the change in the ratio of the absorbance at the maximum absorption wavelength on the shortest side to the absorbance at the maximum absorption wavelength on the second shortest side in the wavelength range of 650 to 1500 nm. When performing the additional bake, the additional bake temperature is preferably 100 to 180°C, more preferably 120 to 160°C. The additional bake time is preferably 10 to 3000 seconds, more preferably 40 to 2500 seconds, and even more preferably 300 to 1200 seconds. The additional bake can be performed using a hot plate, an oven, or the like.

[0203] The film manufacturing method may further include a step of forming a pattern. The pattern forming method may include a pattern forming method using a photolithography method or a pattern forming method using a dry etching method, and the pattern forming method using a photolithography method is preferable. Note that, when the film of the present invention is used as a flat film, the step of forming a pattern may not be performed. The step of forming a pattern will be described in detail below.

[0204] (When forming patterns using photolithography) The pattern forming method by photolithography preferably includes a step of exposing the infrared absorbing composition layer formed by applying the infrared absorbing composition of the present invention to light in a pattern (exposure step), and a step of developing and removing the infrared absorbing composition layer in the unexposed area to form a pattern (development step). If necessary, a step of baking the developed pattern (post-baking step) may be provided. Each step will be described below.

[0205] <<Exposure process>> In the exposure step, the infrared absorbing composition layer is exposed in a pattern. For example, the infrared absorbing composition layer can be exposed in a pattern by using a stepper exposure machine or a scanner exposure machine through a mask having a predetermined mask pattern. This allows the exposed part to be cured.

[0206] Examples of radiation (light) that can be used for exposure include g-line and i-line. Light with a wavelength of 300 nm or less (preferably light with a wavelength of 180 to 300 nm) can also be used. Examples of light with a wavelength of 300 nm or less include KrF line (wavelength 248 nm) and ArF line (wavelength 193 nm), with KrF line (wavelength 248 nm) being preferred. Long-wave light sources with wavelengths of 300 nm or more can also be used.

[0207] In addition, the exposure may be performed by irradiating the light continuously or by irradiating the light in pulses (pulse exposure). Pulse exposure is an exposure method in which light irradiation and pauses are repeated in a short cycle (for example, on the order of milliseconds or less).

[0208] The irradiation amount (exposure amount) is, for example, 0.03 to 2.5 J / cm 2 is preferable, and 0.05 to 1.0 J / cm 2 is more preferable. The oxygen concentration during exposure can be appropriately selected. In addition to exposure in air, exposure may be performed in a low-oxygen atmosphere with an oxygen concentration of 19 volume% or less (e.g., 15 volume%, 5 volume%, or substantially oxygen-free), or in a high-oxygen atmosphere with an oxygen concentration of more than 21 volume% (e.g., 22 volume%, 30 volume%, or 50 volume%). The exposure illuminance can be appropriately set, and is usually 1000 W / m 2 ~100000W / m 2 (For example, 5000W / m 2 , 15000W / m 2 , or 35000W / m 2 The oxygen concentration and exposure illuminance may be appropriately combined. For example, the oxygen concentration is 10% by volume and the illuminance is 10,000 W / m 2 , oxygen concentration 35% by volume, illuminance 20000W / m 2 etc.

[0209] <<Developing process>> Next, the infrared absorbing composition layer in the unexposed portion of the infrared absorbing composition layer after exposure is developed and removed to form a pattern. The infrared absorbing composition layer in the unexposed portion can be developed and removed using a developer. As a result, the infrared absorbing composition layer in the unexposed portion in the exposure step is dissolved in the developer, and only the photocured portion remains on the support. The temperature of the developer is preferably, for example, 20 to 30°C. The development time is preferably 20 to 180 seconds. In addition, in order to improve the removability of residues, the process of shaking off the developer every 60 seconds and supplying a new developer may be repeated several times.

[0210] Examples of the developer include organic solvents and alkaline developers, and alkaline developers are preferably used. As the alkaline developer, an alkaline aqueous solution (alkaline developer) obtained by diluting an alkaline agent with pure water is preferred. Examples of the alkaline agent include organic alkaline compounds such as ammonia, ethylamine, diethylamine, dimethylethanolamine, diglycolamine, diethanolamine, hydroxylamine, ethylenediamine, tetramethylammonium hydroxide, tetraethylammonium hydroxide, tetrapropylammonium hydroxide, tetrabutylammonium hydroxide, ethyltrimethylammonium hydroxide, benzyltrimethylammonium hydroxide, dimethylbis(2-hydroxyethyl)ammonium hydroxide, choline, pyrrole, piperidine, and 1,8-diazabicyclo[5.4.0]-7-undecene, and inorganic alkaline compounds such as sodium hydroxide, potassium hydroxide, sodium carbonate, sodium hydrogencarbonate, sodium silicate, and sodium metasilicate. As the alkaline agent, compounds with a large molecular weight are preferred in terms of the environment and safety. The concentration of the alkaline agent in the alkaline aqueous solution is preferably 0.001 to 10% by mass, more preferably 0.01 to 1% by mass. The developer may further contain a surfactant. As the surfactant, a nonionic surfactant is preferable. The developer may be produced as a concentrated solution from the viewpoint of convenience of transportation and storage, and then diluted to a necessary concentration when used. The dilution ratio is not particularly limited, but can be set in the range of, for example, 1.5 to 100 times. It is also preferable to wash (rinse) with pure water after development. It is also preferable to perform rinsing by supplying a rinsing liquid to the developed composition layer while rotating the support on which the developed composition layer is formed. It is also preferable to perform rinsing by moving a nozzle that ejects the rinsing liquid from the center of the support to the periphery of the support. In this case, the nozzle may be moved while gradually decreasing the moving speed when moving the nozzle from the center of the support to the periphery. By performing rinsing in this manner, it is possible to suppress in-plane variation in rinsing. The same effect can also be obtained by gradually decreasing the rotation speed of the support while moving the nozzle from the center to the periphery of the support.

[0211] After development and drying, it is preferable to perform additional exposure treatment or heating treatment (post-baking). Additional exposure treatment and post-baking are curing treatments after development to complete curing. The heating temperature in post-baking is, for example, preferably 100 to 240°C, more preferably 200 to 240°C. Post-baking can be performed continuously or batchwise using a heating means such as a hot plate, a convection oven (hot air circulation dryer), or a high-frequency heater to achieve the above conditions for the developed film. When additional exposure treatment is performed, it is preferable that the light used for exposure has a wavelength of 400 nm or less. The additional exposure treatment may be performed by the method described in Korean Patent Publication No. 10-2017-0122130.

[0212] (When forming patterns using dry etching) The pattern formation by the dry etching method can be carried out by applying the infrared absorbing composition on a support to form an infrared absorbing composition layer, curing the layer to form a cured product layer, forming a patterned photoresist layer on the cured product layer, and then dry etching the cured product layer using an etching gas with the patterned photoresist layer as a mask. In forming the photoresist layer, it is preferable to carry out a pre-bake treatment. For the pattern formation by the dry etching method, the description in paragraphs 0010 to 0067 of JP 2013-064993 A can be referred to, and the contents thereof are incorporated herein.

[0213] <Optical filters> The optical filter of the present invention has the above-mentioned film of the present invention. Types of the optical filter include an infrared cut filter and an infrared transmission filter.

[0214] The optical filter of the present invention may further have a copper-containing layer, a dielectric multilayer film, an ultraviolet absorbing layer, etc., in addition to the above-mentioned film of the present invention. Examples of the ultraviolet absorbing layer include the absorbing layer described in paragraphs 0040 to 0070 and 0119 to 0145 of International Publication No. 2015 / 099060. Examples of the dielectric multilayer film include the dielectric multilayer film described in paragraphs 0255 to 0259 of JP-A-2014-041318. Examples of the copper-containing layer include a glass substrate (copper-containing glass substrate) made of glass containing copper, and a layer containing a copper complex (copper complex-containing layer). Examples of the copper-containing glass substrate include copper-containing phosphate glass and copper-containing fluorophosphate glass. Examples of commercially available copper-containing glass include NF-50 (manufactured by AGC Technoglass Co., Ltd.), BG-60, BG-61 (all manufactured by Schott Co., Ltd.), CD5000 (manufactured by HOYA Corporation), etc.

[0215] <Solid-state imaging element> The solid-state imaging device of the present invention includes the above-mentioned film of the present invention. The configuration of the solid-state imaging device is not particularly limited as long as it has the film of the present invention and functions as a solid-state imaging device. For example, the following configurations can be mentioned.

[0216] The solid-state imaging device has a plurality of photodiodes constituting a light receiving area of ​​the solid-state imaging element and a transfer electrode formed of polysilicon or the like on a support, a light shielding film formed of tungsten or the like with only the light receiving portion of the photodiode opened on the photodiode and the transfer electrode, a device protection film formed of silicon nitride or the like formed on the light shielding film so as to cover the entire light shielding film and the light receiving portion of the photodiode, and a film of the present invention on the device protection film. Furthermore, the device protection film may have a light collecting means (e.g., a microlens, etc., the same below) on the device protection film and below the film of the present invention (on the side closer to the support), or a light collecting means on the film of the present invention. The color filter may have a structure in which a film forming each pixel is embedded in a space partitioned, for example, in a lattice shape by partition walls. In this case, it is preferable that the partition walls have a lower refractive index than each pixel. Examples of imaging devices having such a structure include devices described in JP 2012-227478 A and JP 2014-179577 A.

[0217] <Image display device> The image display device of the present invention includes the film of the present invention. Examples of the image display device include a liquid crystal display device and an organic electroluminescence (organic EL) display device. The definition and details of the image display device are described in, for example, "Electronic Display Devices" (written by Akio Sasaki, published by Kogyo Chosakai Co., Ltd. in 1990) and "Display Devices" (written by Junsho Ibuki, published by Sangyo Tosho Co., Ltd. in 1989). The liquid crystal display device is described in, for example, "Next Generation Liquid Crystal Display Technology" (edited by Tatsuo Uchida, published by Kogyo Chosakai Co., Ltd. in 1994). There is no particular limitation on the liquid crystal display device to which the present invention can be applied, and the present invention can be applied to various types of liquid crystal display devices described in the above-mentioned "Next Generation Liquid Crystal Display Technology". The image display device may have a white organic EL element. The white organic EL element is preferably in a tandem structure. The tandem structure of organic EL elements is described in JP 2003-045676 A, and Akiyoshi Mikami (ed.), "The Frontline of Organic EL Technology Development - High Brightness, High Precision, Long Life, Know-How Collection", Technical Information Association, pp. 326-328, 2008. The spectrum of white light emitted by the organic EL element preferably has strong maximum emission peaks in the blue region (430-485 nm), green region (530-580 nm), and yellow region (580-620 nm). More preferably, the spectrum has a maximum emission peak in the red region (650-700 nm) in addition to these emission peaks.

[0218] <Infrared sensor> The infrared sensor of the present invention includes the above-mentioned film of the present invention. The configuration of the infrared sensor is not particularly limited as long as it functions as an infrared sensor. Hereinafter, one embodiment of the infrared sensor of the present invention will be described with reference to the drawings.

[0219] In Fig. 1, reference numeral 110 denotes a solid-state imaging element. An infrared cut filter 111 and an infrared transmission filter 114 are disposed on an imaging region of the solid-state imaging element 110. A color filter 112 is disposed on the infrared cut filter 111. A microlens 115 is disposed on the incident light hv side of the color filter 112 and the infrared transmission filter 114. A planarization layer 116 is formed so as to cover the microlens 115.

[0220] The infrared cut filter 111 can be formed using the infrared absorbing composition of the present invention. The spectral characteristics of the infrared cut filter 111 are selected according to the emission wavelength of the infrared light emitting diode (infrared LED) used. The color filter 112 is a color filter in which pixels that transmit and absorb light of a specific wavelength in the visible region are formed, and is not particularly limited, and a conventionally known color filter for forming pixels can be used. For example, a color filter in which red (R), green (G), and blue (B) pixels are formed can be used. For example, the description in paragraphs 0214 to 0263 of JP 2014-043556 A can be referred to, and the contents thereof are incorporated herein. The characteristics of the infrared transmission filter 114 are selected according to the emission wavelength of the infrared LED used.

[0221] In the infrared sensor shown in FIG. 1, an infrared cut filter (another infrared cut filter) other than the infrared cut filter 111 may be further disposed on the planarization layer 116. Examples of the other infrared cut filter include those having a copper-containing layer and / or a dielectric multilayer film. Details of these filters are as described above. Also, a dual bandpass filter may be used as the other infrared cut filter. EXAMPLES

[0222] The present invention will be described in more detail with reference to the following examples. The materials, amounts used, ratios, processing contents, processing procedures, etc. shown in the following examples can be appropriately changed without departing from the spirit of the present invention.

[0223] <Synthesis example of infrared absorbing dye A-1> Infrared absorbing dye A-1 was synthesized according to the following scheme: In the following structural formula, Me represents a methyl group, and Ph represents a phenyl group. [ka]

[0224] (Synthesis of compound a) Compound a was synthesized using ethyl 2-methylbenzoylacetate (Tokyo Chemical Industry Co., Ltd.) as a raw material according to the method described in Tetrahedron 62 (2006) 6018-6028.

[0225] (Synthesis of compound b) Compound b was synthesized using 4-(1-methylheptoxy)benzonitrile and compound a as raw materials according to the method described in paragraph 0342 of WO 2016 / 194527.

[0226] (Synthesis of compound c) Compound c was synthesized according to the method described in Chemistry-A European Journal, 2009, vol. 15, #19, p. 4857-4864.

[0227] (Synthesis of compound d) Compound d was synthesized according to the method described in paragraph 0072 of Japanese Patent No. 6353060.

[0228] (Synthesis of compound e) Compound e was synthesized according to the method described in paragraph 0072 of Japanese Patent No. 6353060.

[0229] (Synthesis of infrared absorbing dye A-1) 3.0 parts by mass of compound e and 1.75 parts by mass of potassium carbonate were stirred in 36 parts by mass of dimethylacetamide (DMAc), and then 3.0 parts by mass of butane sultone and 4 parts by mass of DMAc were added and stirred at room temperature for 10 minutes. The circumscribing temperature was raised to 95°C and heated for 3 hours. Next, the mixture was allowed to cool to an internal temperature of 30°C, and the precipitated crystals were filtered off. The obtained crystals were added little by little to 30 parts by mass of 4 mol / L hydrochloric acid aqueous solution while maintaining the internal temperature at 30°C or less, and the mixture was stirred at room temperature for 30 minutes, and the precipitated crystals were filtered off. This operation was performed twice: 60 parts by mass of ethyl acetate was added to the obtained crystals, heated to reflux for 30 minutes, allowed to cool to 30°C, and the crystals were filtered off. The obtained crystals were dried at 50°C for 24 hours by blowing air to obtain 2.0 parts by mass of compound A-1.

[0230] <Synthesis Examples of Infrared Absorbing Dyes A-2 to A-7> Infrared absorbing dyes A-2 to A-7 were synthesized in the same manner as in the synthesis of infrared absorbing dye A-1.

[0231] <Evaluation of the amount of dissolved infrared absorbing dye> The infrared absorbing dyes shown in the table below were added to the measurement solvents shown in the table below, which had been adjusted to a temperature of 25°C, under atmospheric pressure. After stirring for 1 hour, the amount of each infrared absorbing dye dissolved in the measurement solvent at 25°C was determined. The amount of infrared absorbing dye dissolved was evaluated according to the following criteria. Case A was determined to be a good solvent, and case B was determined to be a poor solvent. In the poor solvent, the infrared absorbing dye exists as particles. Note that PGMEA in the measurement solvent column in the table below is an abbreviation for propylene glycol monomethyl ether acetate. A: The amount of infrared absorbing dye dissolved in 100 g of measurement solvent at 25°C is 0.1 g or more. B: The amount of infrared absorbing dye dissolved in 100 g of the measurement solvent at 25° C. is less than 0.1 g %.

[0232] [Table 1] [Table 2]

[0233] <Maximum absorption wavelength of infrared absorbing dye in a good solvent> Each infrared absorbing dye was dissolved in the solvent (good solvent) shown in the table below to obtain an infrared absorbing dye concentration of 2.5 x 10 -6 A mol / L dye solution was prepared and the absorption spectrum of the dye solution was measured. The number of maximum absorption wavelengths in the wavelength range of 650 to 1500 nm and the wavelength (λmax) showing the highest absorbance value are shown in the table below. [Table 3]

[0234] The structures of infrared absorbing dyes A-1 to A-7 and comparative dyes 1 to 3 are as follows: In the following structural formulae, Me represents a methyl group, and Ph represents a phenyl group. [ka] [ka] [ka]

[0235] <Preparation of infrared absorbing compositions of Examples 1 to 5 and Comparative Examples 1 and 2> The raw materials described below were mixed and filtered using a nylon filter (manufactured by Nippon Pall Co., Ltd.) with a pore size of 0.45 μm to prepare an infrared absorbing composition. In Examples 1 to 5 and Comparative Examples 1 and 2, the infrared absorbing dye was present in the form of particles in the infrared absorbing composition. The dispersion was prepared as follows. The types of infrared absorbing dyes, surfactants, and solvents described in the Dispersion column of the table below were mixed in the amounts described in the Dispersion column of the table below, and 500 parts by mass of zirconia beads with a diameter of 0.1 mm were added. The mixture was treated in a planetary ball mill at 300 rpm for 5 hours, and the zirconia beads were separated by filtration to prepare a dispersion.

[0236] [Table 4]

[0237] Surfactant 1: Sodium dodecylbenzenesulfonate (Neogen SC, Daiichi Kogyo Seiyaku Co., Ltd.) Surfactant 2: Dodecylbenzenesulfonic acid (Tokyo Chemical Industry Co., Ltd.) Resin 1: 20% by weight aqueous solution of polyvinyl alcohol

[0238] <Preparation of infrared absorbing compositions of Examples 6 to 27> The raw materials shown in the table below were mixed and filtered using a nylon filter (manufactured by Nippon Pall Co., Ltd.) with a pore size of 0.45 μm to prepare infrared absorbing compositions of Examples 6 to 27. In each infrared absorbing composition, the infrared absorbing dye was present in the form of particles. The dispersion liquid was prepared as follows. The infrared absorbing dye, dispersant, and solvent of the types shown in the dispersion liquid column in the table below were mixed in the amounts shown in the table below, and 230 parts by mass of zirconia beads with a diameter of 0.3 mm were added, and a dispersion treatment was performed for 8 hours using a paint shaker, and the beads were separated by filtration to prepare a dispersion liquid.

[0239] <Preparation of infrared absorbing composition of Comparative Example 3> The resin compositions were obtained by adding and dissolving the infrared absorbing dyes shown in the following table to resin solutions prepared by dissolving the resins shown in the following table in the solvents shown in the following table, and removing insoluble matters by filtration. In the composition of Comparative Example 3, Comparative Dye 3 was dissolved in the solvent in the infrared absorbing composition.

[0240] [Table 5] [Table 6]

[0241] (solvent) S-1: Propylene glycol monomethyl ether acetate S-2: Cyclopentanone S-3: Propylene carbonate S-4: Cyclohexyl acetate S-5: Methyl isobutyl ketone

[0242] (Dispersant) C-1: Resin with the following structure. (The numbers attached to the main chain are the molar ratios, and the numbers attached to the side chains are the numbers of repeating units. Weight average molecular weight: 21,000, acid value: 36.0 mg KOH / g, amine value: 47.0 mg KOH / g) [ka] C-2: Resin with the following structure (the number attached to the main chain is the molar ratio, and the number attached to the side chain is the number of repeating units. Weight average molecular weight 38,000, acid value 99.1 mgKOH / g) [ka]

[0243] (resin) P-1: Resin with the following structure (the numbers attached to the main chain are molar ratios. Weight average molecular weight 10,000, acid value = 69.2 mg KOH / g) [ka] P-2: Copolymer of allyl methacrylate (AMA) and methacrylic acid (MAA) (composition ratio (mass ratio): AMA / MAA = 80 / 20, weight average molecular weight 15,000) P-3: Copolymer of α-allyloxymethyl acrylate (AOMA) and N-phenylmaleimide (PME) (composition ratio (mass ratio): AOMA / PME = 66 / 34, weight average molecular weight 31600) P-4: Copolymer of methyl methacrylate (MMA) and glycidyl methacrylate (GMA) (composition ratio (mass ratio): MMA / GMA = 50 / 50, weight average molecular weight 25,000)

[0244] (curable compound) M-1: A mixture of compounds with the following structure (the molar ratio of the compound on the left to the compound on the right is 7:3) [ka] M-2: Compound having the following structure [ka] M-3: EPICLON N-695 (cresol novolac epoxy resin, manufactured by DIC Corporation) M-4: EHPE3150 (1,2-epoxy-4-(2-oxiranyl)cyclohexane adduct of 2,2-bis(hydroxymethyl)-1-butanol, manufactured by Daicel Corporation)

[0245] (Photopolymerization initiator) F-1: Compound having the following structure [ka] F-2: Compound having the following structure [ka]

[0246] (Surfactant) G-1: Compound having the following structure (weight average molecular weight: 14,000, the percentage of repeating units is mol%) [ka] G-2: KF-6001 (silicone surfactant, manufactured by Shin-Etsu Chemical Co., Ltd.) G-3: PolyFox PF6320 (fluorosurfactant, manufactured by OMNOVA) (Polymerization inhibitor) H-1: p-Methoxyphenol

[0247] <Maximum absorption wavelength and absorbance> The absorption spectrum of each infrared absorbing composition was measured, and the number of maximum absorption wavelengths existing in the wavelength range of 650 to 1500 nm, the maximum absorption wavelength (λ1) existing on the shortest side among the maximum absorption wavelengths existing in the wavelength range of 650 to 1500 nm, the maximum absorption wavelength (λ2) existing on the second shortest side among the maximum absorption wavelengths existing in the wavelength range of 650 to 1500 nm, and the absorbance value (Z1) at the maximum absorption wavelength (λ1) when the absorbance at the maximum absorption wavelength (λ2) was set to 1. In the infrared absorbing compositions of Examples 1 to 18 and Comparative Examples 1 to 3, the characteristics of the maximum absorption wavelength and absorbance in the wavelength range of 650 to 1500 nm were derived from the infrared absorbing dyes A-1 to A-7 and comparative dyes 1 to 3 contained in each infrared absorbing composition.

[0248] <Production of cured film> (Production Example 1) Method for producing a cured film using the infrared absorbing composition of Examples 1 to 5 and 18 and Comparative Examples 1 to 3 The infrared absorbing compositions of Examples 1 to 5 and 18 and Comparative Examples 1 to 3 were applied onto a glass substrate (Corning, "1737") using a spin coater, and initially dried by heat treatment (pre-baking) for 120 seconds using a hot plate at 100°C. Thereafter, the atmosphere was replaced with nitrogen at 50°C for 30 minutes using an inert oven, and the temperature was raised to 150°C in about 10 minutes, and the composition was further dried at 150°C for 30 minutes under a nitrogen atmosphere to obtain a cured film.

[0249] (Production Example 2) Method for producing a cured film using the infrared absorbing composition of Examples 6 to 12, 21, 24, and 27 The infrared absorbing compositions of Examples 6 to 12, 21, 24, and 27 were applied onto a glass substrate (Corning, "1737") using a spin coater, and heat-treated (pre-baked) for 120 seconds using a hot plate at 100°C. Next, the layers were exposed to 500 mJ / cm using an i-line stepper exposure system FPA-3000i5+ (Canon). 2The entire surface was exposed to light at 4000 K. Then, paddle development was performed at 23° C. for 60 seconds using a developing machine (CD-2060, manufactured by FUJIFILM Electronic Materials Co., Ltd.), followed by rinsing with pure water and spin drying. Further, a heat treatment (post-baking) was performed for 300 seconds using a hot plate at 200° C. to obtain a cured film.

[0250] (Production Example 3) Method for producing a cured film using the infrared absorbing composition of Examples 13 to 17 The infrared absorbing compositions of Examples 13 to 17 were applied onto a glass substrate (Corning, "1737") using a spin coater, and heat-treated (pre-baked) for 120 seconds using a hot plate at 100°C. Further, heat-treated (post-baked) for 480 seconds using a hot plate at 200°C to obtain a cured film.

[0251] (Production Example 4) Method for producing a cured film using the infrared absorbing composition of Examples 19, 20, 22, 23, 25, and 26 The infrared absorbing compositions of Examples 19, 20, 22, 23, 25, and 26 were applied onto a glass substrate (Corning, "1737") using a spin coater, and heat-treated (pre-baked) for 600 seconds using a hot plate at 120°C. Further, heat-treated (post-baked) for 480 seconds using a hot plate at 200°C to obtain a cured film.

[0252] <Evaluation of Spectral Characteristics> (Slope shape) In each of the above-mentioned methods for producing the cured film, the thickness of the cured film is adjusted so that the transmittance at the shortest maximum absorption wavelength (λ1) among the maximum absorption wavelengths in the wavelength range of 650 to 1500 nm is 10%, and the transmittance at the longest wavelength (λ) showing 60% on the short wavelength side of λ1 is 10%. SH60 ) was measured. SH60 The difference between (λ1-λ SH60 ) was calculated, and the slope shape was evaluated according to the following criteria. The smaller the difference in wavelength, the better the cutoff of infrared absorption, indicating that infrared radiation can be blocked more selectively. -Evaluation criteria- A: (λ1-λ SH60 )≦50nm B: 50nm<(λ1-λ SH60 )≦70nm C: 70nm<(λ1-λ SH60 )

[0253] (Infrared shielding) In each of the above-mentioned methods for producing the cured film, the thickness of the cured film is adjusted so that the transmittance at the wavelength (λmaxA) showing the highest absorbance value in the wavelength range of 650 to 1500 nm is 1%, and the transmittance at the shortest wavelength (λmaxA) showing 20% ​​on the long-wave side of λmax is 20%. LH20 ) and the longest wavelength at which the transmittance is 20% on the short-wave side of λmax (λ SH20 ) was measured. LH20 and λ SH20 The difference (λ LH20 -λ SH20 The infrared shielding property was evaluated according to the following criteria. A larger difference in the wavelengths indicates that a wider range of infrared rays can be shielded. -Evaluation criteria- A:(λ LH20 -λ SH20 )≧110nm B: 85 nm ≦ (λ LH20 -λ SH20 )<110nm C: 60 nm ≦ (λ LH20 -λ SH20 )<85nm D: (λ LH20 -λ SH20 )<60nm

[0254] (Heat resistance) The 1.0 μm thick cured film obtained above was heated at 200° C. for 3 hours using a hot plate. The transmittance of the film before and after heating to light with wavelengths of 400 to 2000 nm was measured using a spectrophotometer U-4100 (Hitachi High-Technologies Corporation). In the wavelength range of 400 to 1500 nm, the change in transmittance at the wavelength where the change in transmittance was the largest before and after heating was calculated from the following formula, and the change in transmittance was evaluated according to the following criteria. It can be said that the smaller the change in transmittance, the more excellent the heat resistance. Change in transmittance = |(transmittance after light irradiation - transmittance before light irradiation)| -Evaluation criteria- A: The change in transmittance is less than 3%. B: The change in transmittance is 3% or more and less than 5%. C: The change in transmittance is 5% or more and less than 10%. D: The change in transmittance is 10% or more.

[0255] (Lightfastness) The 1.0 μm thick cured film obtained above was set in a discoloration tester equipped with a super xenon lamp (200,000 lux) and irradiated with 200,000 lux of light for 55 hours without using an ultraviolet cut filter. Next, the transmission spectrum of the film after light irradiation was measured using a spectrophotometer U-4100 (manufactured by Hitachi High-Technologies Corporation). In the wavelength range of 400 nm to 2,000 nm, the change in transmittance at the wavelength with the largest change before and after light irradiation was calculated from the following formula, and the heat resistance was evaluated according to the following criteria. Change in transmittance = |(transmittance after light irradiation - transmittance before light irradiation)| -Evaluation criteria- A: The change in transmittance is less than 3%. B: The change in transmittance is 3% or more and less than 5%. C: The change in transmittance is 5% or more and less than 10%. D: The change in transmittance is 10% or more.

[0256] [Table 7]

[0257] As shown in the above table, the infrared absorbing compositions of the examples had a good slope shape and excellent infrared shielding properties. In addition, in the infrared absorbing compositions of the examples, the infrared absorbing dyes A-1 to A-7 all existed as particles in the infrared absorbing compositions. In addition, in the infrared absorbing compositions of the examples, these particles had two or more maximum absorption wavelengths in the wavelength range of 650 to 1500 nm. In addition, the absorbance (Z1) at the maximum absorption wavelength (λ1) on the shortest side in the above range was 0.6 to 2.0 when the absorbance at the maximum absorption wavelength (λ2) on the second shortest side was taken as 1. In addition, the difference (λ2-λ1) between the maximum absorption wavelength (λ1) on the shortest side and the maximum absorption wavelength (λ2) on the second shortest side was in the range of 30 to 80 nm. Also, referring to Table 3, the above λ1 values ​​in the infrared absorbing compositions of Examples 1 to 27 were on the shorter wavelength side than the wavelength (λmax) at which the absorbance was highest in the dye solutions prepared by dissolving each of the infrared absorbing dyes A-1 to A-7 in a good solvent (dimethyl sulfoxide). On the other hand, in the cured film state of Comparative Example 3, the film had maximum absorption wavelengths at 749 nm and 920 nm, but the wavelength difference was large at more than 100 nm, and the infrared shielding properties were insufficient. By using a cured film made of the infrared absorbing composition of Example 6 in an infrared sensor, noise can be further reduced.

[0258] (Example 28) An infrared absorbing composition was produced in the same manner as in Example 6, except that 1.7 parts by mass of infrared absorbing dye B-1 and 2.0 parts by mass of ultraviolet absorber UV-1 were further blended when preparing the dispersion in Example 6, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 28 had a slope shape equivalent to that of Example 6. In addition, the infrared shielding property was superior to that of Example 6, and was rated A.

[0259] (Example 29) An infrared absorbing composition was produced in the same manner as in Example 9, except that 1.7 parts by mass of infrared absorbing dye B-2 and 2.0 parts by mass of an ultraviolet absorber (Tinuvin 326, 2-(5-chloro-2-benzotriazolyl)-6-tert-butyl-p-cresol, manufactured by BASF) were further blended when preparing the dispersion liquid in Example 9, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 29 had a slope shape equivalent to that of Example 9. In addition, the infrared shielding property was superior to that of Example 9, and was rated A.

[0260] (Example 30) An infrared absorbing composition was produced in the same manner as in Example 10, except that 1.7 parts by mass of infrared absorbing dye B-3 and 2.0 parts by mass of an ultraviolet absorber (Tinuvin 477, a hydroxyphenyl triazine compound, manufactured by BASF) were further blended when preparing the dispersion in Example 10, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 30 had a slope shape equivalent to that of Example 10. In addition, the infrared shielding property was superior to that of Example 10, and was rated A. (Example 31) An infrared absorbing composition was produced in the same manner as in Example 11, except that 1.7 parts by mass of infrared absorbing dye B-4 and 2.0 parts by mass of an ultraviolet absorber (Tinuvin 460, a hydroxyphenyl triazine compound, manufactured by BASF) were further blended when preparing the dispersion in Example 11, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 31 had a slope shape equivalent to that of Example 11. In addition, the infrared shielding property was superior to that of Example 11, and was rated A. Example 32 An infrared absorbing composition was produced in the same manner as in Example 12, except that 1.7 parts by mass of infrared absorbing dye B-5 and 2.0 parts by mass of an ultraviolet absorber (Tinuvin 405, a hydroxyphenyl triazine compound, manufactured by BASF) were further blended when preparing the dispersion in Example 12, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 32 had a slope shape equivalent to that of Example 12. In addition, the infrared shielding property was superior to that of Example 12, and was rated A. (Example 33) In Example 14, an infrared absorbing composition was produced in the same manner as in Example 14, except that 1.7 parts by mass of infrared absorbing dye B-2, 0.3 parts by mass of infrared absorbing dye B-6, and 9.0 parts by mass of an ultraviolet absorber (Tinuvin 479, a hydroxyphenyl triazine compound, manufactured by BASF) were further blended during preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 33 had a slope shape equivalent to that of Example 14. In addition, the infrared shielding property was superior to that of Example 14, and was rated as A.

[0261] (Example 34) In Example 15, an infrared absorbing composition was produced in the same manner as in Example 15, except that 1.7 parts by mass of infrared absorbing dye B-3, 0.3 parts by mass of infrared absorbing dye B-7, and 9.0 parts by mass of an ultraviolet absorber (Uvinul3050, a dihydroxybenzophenone compound, manufactured by BASF) were further blended during preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 34 had a slope shape equivalent to that of Example 15. In addition, the infrared shielding property was superior to that of Example 15, and was rated as A. Example 35 In Example 16, an infrared absorbing composition was produced in the same manner as in Example 16, except that 1.7 parts by mass of infrared absorbing dye B-4, 0.3 parts by mass of infrared absorbing dye B-8, and 9.0 parts by mass of an ultraviolet absorber (Tinuvin 477, a hydroxyphenyl triazine compound, manufactured by BASF) were further added during the preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 35 had a slope shape equivalent to that of Example 16. In addition, the infrared shielding property was superior to that of Example 16, and was evaluated as A.

[0262] (Example 36) In Example 17, an infrared absorbing composition was produced in the same manner as in Example 17, except that 1.7 parts by mass of infrared absorbing dye B-5, 0.3 parts by mass of infrared absorbing dye B-9, and 9.0 parts by mass of an ultraviolet absorber (Uvinul3049, a dihydroxybenzophenone compound, manufactured by BASF) were further added during the preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 36 had a slope shape equivalent to that of Example 17. In addition, the infrared shielding property was superior to that of Example 17, and was rated as A.

[0263] (Example 37) In Example 14, an infrared absorbing composition was produced in the same manner as in Example 14, except that 1.7 parts by mass of infrared absorbing dye B-10, 0.3 parts by mass of infrared absorbing dye B-6, and 9.0 parts by mass of ultraviolet absorber Uvinul3050 (dihydroxybenzophenone compound, manufactured by BASF) were further blended during preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 37 had a slope shape equivalent to that of Example 14. In addition, the infrared shielding property was superior to that of Example 14, and was rated as A.

[0264] (Example 38) In Example 20, an infrared absorbing composition was produced in the same manner as in Example 20, except that 1.7 parts by mass of infrared absorbing dye B-10, 0.3 parts by mass of infrared absorbing dye B-6, and 9.0 parts by mass of ultraviolet absorber Tinuvin 477 (hydroxyphenyl triazine compound, manufactured by BASF) were further blended during preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 38 had a slope shape equivalent to that of Example 20. In addition, the infrared shielding property was superior to that of Example 20, and was rated as A.

[0265] (Example 39) In Example 21, an infrared absorbing composition was produced in the same manner as in Example 21, except that 1.7 parts by mass of infrared absorbing dye B-10, 0.3 parts by mass of infrared absorbing dye B-6, and 9.0 parts by mass of ultraviolet absorber Tinuvin 479 (hydroxyphenyl triazine compound, manufactured by BASF) were further blended during preparation of the dispersion liquid, and each property was evaluated in the same manner as above. The infrared absorbing composition of Example 39 had a slope shape equivalent to that of Example 21. In addition, the infrared shielding property was superior to that of Example 21, and was rated as A.

[0266] The infrared absorbing dyes B-1 to B-10 are compounds having the structures shown below. [ka] [ka]

[0267] The ultraviolet absorber UV-1 is a compound having the structure shown below. [ka] [Explanation of symbols]

[0268] 110: solid-state imaging element, 111: infrared cut filter, 112: color filter, 114: infrared transmission filter, 115: microlens, 116: flattening layer

Claims

1. An infrared absorbing composition comprising particles of an infrared absorbing dye and a solvent, The infrared absorbing dye is an infrared absorbing composition containing a compound represented by formula (PP-2): 【Chemistry 1】 In formula (PP-2), R 1a represents an alkyl group having 1 to 3 carbon atoms, R 1b represents a substituent, R 3 and R 5 one of the groups represents a cyano group and the other represents a heteroaryl group; R 4 and R 6 one of the groups represents a cyano group and the other represents a heteroaryl group; R 3 ~R 6 the number of carbon atoms constituting the heteroaryl group represented by the formula (I) is 6 to 9, the heteroatom constituting the heteroaryl group is a nitrogen atom, an oxygen atom or a sulfur atom, the number of heteroatoms constituting the heteroaryl group is 1 to 2, the heteroaryl group is a condensed ring, and the number of condensation of the condensed ring is 2, R 7 and R 8 Each independently represents -BR 9 R 10 represents R 9 and R 10 each independently represents an aryl group having 6 to 12 carbon atoms, L 1 represents an (n2+1)-valent linking group consisting of an aliphatic hydrocarbon group, -O-, or a combination thereof, X 1 represents a sulfo group and its salts, or -NRx 1 Rx 2 The atom or atomic group constituting the salt is an ammonium ion, and Rx 1 and Rx 2 each independently represents an alkyl group having 1 to 3 carbon atoms, n1 represents 0, n2 represents 1; m1 represents 1.

2. The infrared absorbing composition of claim 1 further comprising a curable compound.

3. 3. The infrared absorbing composition according to claim 1, which is for use in an optical filter or an ink.

4. A film using the infrared absorbing composition according to any one of claims 1 to 3.

5. An optical filter comprising the film of claim 4.

6. A solid-state imaging device comprising the film according to claim 4 .

7. An image display device comprising the film according to claim 4.

8. An infrared sensor comprising the film of claim 4.

Citation Information

Patent Citations

  • Infrared absorptive compound and fine particles comprising the compound

    JP2009263614A

  • Oxocarbonic compound, resin composition, and light selective transmission filter

    JP2018041047A

  • Composition, film, optical filter, layered product, solid imaging element, image display device, infrared sensor, and compound

    WO2018020861A1

  • Optical filter and device using optical filter

    WO2018043564A1

  • Pigment-dispersed liquid, curable composition, film, near-infrared ray cut-off filter, solid-state image pickup element, image display device, and infrared ray sensor

    WO2018101189A1