Electromagnetic wave reflecting device, electromagnetic wave reflecting fence, and reflective panel

By providing gaps in the adhesive layer of electromagnetic wave reflectors, the reflection efficiency is maintained at 60% or higher, addressing the issue of decreased performance due to dielectric and adhesive layer interactions, and improving durability.

JP7948314B2Active Publication Date: 2026-11-11AGC INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024524246
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-06-01
Filing Date
2023-04-26
Publication Date
2026-11-11
Estimated Expiration
2043-04-26

AI Technical Summary

Technical Problem

The challenge of maintaining high reflection efficiency in electromagnetic wave reflectors with metal patterns bonded via adhesive layers is exacerbated by the dielectric constants of the dielectric substrate and adhesive layer, which can lead to decreased performance.

Method used

Incorporating gaps in the adhesive layer that bonds the conductive pattern to the dielectric layer, ensuring the adhesive layer does not cover the entire surface, thereby suppressing the decrease in reflection efficiency.

Benefits of technology

This configuration maintains reflection efficiency at 60% or higher, preferably 70% or more, by reducing the influence of the adhesive layer on the dielectric layer, while also enhancing durability and weather resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007948314000003
    Figure 0007948314000003
  • Figure 0007948314000004
    Figure 0007948314000004
  • Figure 0007948314000005
    Figure 0007948314000005
Patent Text Reader

Abstract

The present invention suppresses a decrease in the reflection efficiency of an electromagnetic wave reflecting device that has a metal pattern bonded by an adhesive layer. The electromagnetic wave reflecting device comprises a reflective panel that reflects radio waves in a desired band selected from frequency bands of 1 GHz to 170 GHz, and a frame that holds the reflective panel. The reflective panel includes: a dielectric layer; a periodic conductive pattern provided on one surface of the dielectric layer; a ground layer provided on the other surface of the dielectric layer; and an adhesive layer that bonds the conductive pattern to the one surface of the dielectric layer. Gaps are provided in the adhesive layer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] This invention relates to an electromagnetic wave reflecting device, an electromagnetic wave reflecting fence, and a reflecting panel. [Background technology]

[0002] While the fifth-generation (hereinafter referred to as "5G") mobile communication standard is expected to provide high-speed, high-capacity communication, it uses radio waves with strong directivity, which can result in areas where radio waves are difficult to reach. In places with many metal machines, such as factories, or in urban areas with many reflections from walls and street trees, a means of delivering radio waves to the target terminal devices and wireless equipment is necessary. Similar requirements exist in places where base station antennas cannot be seen (NLOS: Non-Line-Of-Sight), such as medical facilities, event venues, and large commercial facilities.

[0003] In recent years, reflective surfaces with artificial surfaces called "metasurfaces" have been developed. Metasurfaces are formed from periodic structures or patterns finer than the wavelength and are designed to reflect radio waves in a desired direction (see, for example, Non-Patent Literature 1). While metasurfaces themselves are realized from periodically repeating fine structures or metallic patterns, in actual manufacturing, the metallic pattern is often provided on one side of a dielectric substrate, and a ground layer is provided on the opposite side. Because metasurfaces can achieve a desired reflection angle while maintaining a planar arrangement, they can function effectively as reflectors even in environments where there is not enough space to install many electromagnetic wave reflecting panels.

[0004] Metal patterns and ground layers are often formed from highly conductive metals such as copper (Cu), nickel (Ni), and silver (Ag). Reflective surfaces, including metasurfaces, function through metal patterns, requiring precise patterning. Ground layers are formed on one surface of the dielectric substrate by processes such as sputtering and vapor deposition. Metal patterns can be formed by etching or electroplating. [Prior art documents] [Non-patent literature]

[0005] [Non-Patent Document 1] Diaz-Rubio et al., Sci. Adv. 2017: 3: e1602714 1 [Overview of the project] [Problems that the invention aims to solve]

[0006] It is not easy to directly form a metal pattern by patterning on the other side of a dielectric substrate that has a metal ground layer formed on it. Therefore, it is conceivable to bond the metal pattern via an adhesive layer. On a reflective surface where the metal pattern is bonded with an adhesive layer, the dielectric constants of the dielectric substrate and the adhesive layer greatly affect the reflection angle and reflection efficiency. To improve the propagation environment, it is preferable that the reflection efficiency be 60% or higher, or 70% or higher.

[0007] The inventors have found that providing gaps in the adhesive film, rather than placing a conductive pattern on the adhesive film that covers the entire surface of the dielectric substrate, suppresses the decrease in reflection efficiency. One objective of the present invention is to suppress the decrease in reflection efficiency in an electromagnetic wave reflecting device having a metal pattern joined by an adhesive layer. [Means for solving the problem]

[0008] In one embodiment, the electromagnetic wave reflector comprises a reflecting panel that reflects radio waves in a desired frequency band selected from a frequency band of 1 GHz or higher and 170 GHz or lower, and a frame that holds the reflecting panel. The reflective panel comprises a dielectric layer, a periodic conductive pattern provided on one surface of the dielectric layer, a ground layer provided on the other surface of the dielectric layer, and an adhesive layer that bonds the conductive pattern to the one surface of the dielectric layer. A gap is provided in the aforementioned adhesive layer. [Effects of the Invention]

[0009] In an electromagnetic wave reflection device having a metal pattern bonded via an adhesive layer, a decrease in reflection efficiency can be suppressed. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] [Figure 1] This is a schematic diagram of an electromagnetic wave reflection fence formed by connecting a plurality of electromagnetic wave reflection devices. [Figure 2] This is a horizontal cross-sectional view of the frame taken along line A-A in Figure 1. [Figure 3] This is a diagram showing a state where a panel is inserted into the frame of Figure 2. [Figure 4A] This is a diagram showing an example of the layer configuration of a reflection panel. [Figure 4B] This is a diagram showing another example of the layer configuration of a reflection panel. [Figure 4C] This is a diagram showing still another example of the layer configuration of a reflection panel. [Figure 5] This is a diagram showing a model of a conductive pattern used for evaluation of reflection characteristics. [Figure 6] This is a schematic diagram showing the configuration of a unit cell of the model in Figure 5. [Figure 7] This is a diagram showing an arrangement example of the conductive pattern on the adhesive layer. [Figure 8] This is a diagram showing an analysis space. [Figure 9A] This is a schematic diagram of the XY plane of the analysis space. [Figure 9B] This is a schematic diagram of the XZ plane of the analysis space. [Figure 9C] This is a schematic diagram of the YZ plane of the analysis space. DETAILED DESCRIPTION OF EMBODIMENTS FOR CARRYING OUT THE INVENTION

[0011] To improve the propagation environment using an electromagnetic wave reflector, it is desirable that the reflectance efficiency of the electromagnetic wave reflector be 60% or higher, preferably 70% or higher. In this embodiment, in order to suppress a decrease in the reflectance efficiency of the electromagnetic wave reflector, a gap is provided in the adhesive layer that bonds the conductive pattern to the dielectric layer. The "gap" refers to a portion where the adhesive layer is partially interrupted, and its form and shape are not limited to grooves, trenches, or openings. In other words, the adhesive layer that bonds the conductive pattern does not cover the entire surface of the dielectric layer, but is interrupted in at least a part of it. By keeping the occupancy rate of the adhesive layer over the dielectric layer within a predetermined range, a decrease in the reflectance efficiency of the electromagnetic wave reflector is suppressed.

[0012] Figure 1 is a schematic diagram of an electromagnetic wave reflective fence 100 formed by connecting electromagnetic wave reflectors 60-1, 60-2, and 60-3. In Figure 1, the electromagnetic wave reflective fence 100 is constructed by connecting three electromagnetic wave reflectors 60-1, 60-2, and 60-3 (hereinafter, they may be collectively referred to as "electromagnetic wave reflectors 60" as appropriate), but there is no particular limit to the number of electromagnetic wave reflectors 60 that are connected.

[0013] Electromagnetic wave reflectors 60-1, 60-2, and 60-3 each have reflective panels 10-1, 10-2, and 10-3, respectively (hereinafter collectively referred to as "reflective panel 10" as appropriate). The width direction of the reflective panel 10 is the X direction, the height direction is the Y direction, and the thickness direction is the Z direction. Each reflective panel 10 reflects electromagnetic waves between 1 GHz and 170 GHz, preferably between 1 GHz and 100 GHz, and more preferably between 1 GHz and 80 GHz. Each reflective panel 10 has a conductive pattern or conductive film as a reflective film, designed according to the desired reflection mode, frequency band, etc. The conductive film may be formed of a periodic pattern, a mesh pattern, a geometric pattern, a transparent film, etc. As described later, by providing a gap in the adhesive layer that joins the conductive pattern on the reflective panel 10-1, a decrease in the reflection efficiency of the electromagnetic wave reflector 60 is suppressed.

[0014] Each of the reflective panels 10-1, 10-2, and 10-3 may have a specular surface where the angle of incidence and the angle of emission of electromagnetic waves are equal, or it may have a non-specular surface where the angle of incidence and the angle of reflection are different. Non-specular surfaces include diffusing and scattering surfaces, as well as metasurfaces, which are artificial reflective surfaces designed to reflect radio waves in a desired direction.

[0015] Reflective panels 10-1, 10-2, and 10-3 are sometimes desirable to be electrically connected to each other from the viewpoint of maintaining the continuity of the reflected potential, but if a metasurface is included, electrical connection between adjacent reflective panels 10 is not necessary. By holding adjacent reflective panels 10 by the frame 50, an electromagnetic wave reflection fence 100 connected in the X direction is obtained.

[0016] The electromagnetic wave reflector 60 may have legs 56 to support the frame 50, in addition to the reflecting panel 10 and the frame 50. As shown in Figure 1, when the electromagnetic wave reflector 60 or electromagnetic wave reflecting fence 100 is to stand on its own on the installation surface, it is desirable to provide legs 56, but the legs 56 are not essential. In addition to the frame 50, a top frame 57 to hold the upper end of the reflecting panel 10 and a bottom frame 58 to hold the lower end may be used. In this case, the frame 50, the top frame 57, and the bottom frame 58 constitute a frame that holds the entire circumference of the reflecting panel 10. The frame 50 may be called a "side frame" due to its positional relationship with the top frame 57 and the bottom frame 58. By providing the top frame 57 and the bottom frame 58, mechanical strength and safety are ensured during the transport and assembly of the reflecting panel 10. Depending on the application, the electromagnetic wave reflector 60 may be installed on a wall or ceiling by holding the reflecting panel 10 with the frame 50, the top frame 57, and the bottom frame 58.

[0017] Figure 2 shows an example of the configuration of the frame 50 along the AA line in Figure 1, in a cross-sectional view parallel to the XZ plane. The frame 50 has a conductive body 500 and slits 51 formed on both sides of the body 500 in the width direction. The slits 51 hold the side edges of the reflective panel 10. The side edges of the reflective panel 10 are the edges along the Y direction in Figure 1.

[0018] The main body 500 has a cavity 52 that communicates with the slit 51, a groove 53 provided in the cavity 52, and a hollow 55 that does not communicate with the cavity 52 and the groove 53, but is not limited to this example. The groove 53 is provided at a position opposite the slit 51 with the cavity 52 in between, and holds the side edge of the reflective panel 10 inserted from the slit 51. By providing the cavity 52 and the hollow 55 in the frame 50, the frame 50 can be made lighter. By providing the groove 53 in the cavity 52, the holding of the reflective panel 10 becomes stronger.

[0019] A non-conductive cover 501 made of resin or the like may be provided on the outer surface of the main body 500, but the cover 501 is not mandatory. If a cover 501 is provided, the cover 501 functions as a protective member that protects the frame 50.

[0020] Figure 3 shows the insertion state of the reflective panels 10 into the frame 50 in a cross-sectional view parallel to the XZ plane. Reflective panels 10-1 and 10-2 are inserted through slits 51 (see Figure 2) on both sides of the main body 500. Reflective panels 10-1 and 10-2 do not necessarily have to be inserted all the way to the back of the groove 53 (see Figure 2) in the cavity 52 and in contact with the bottom surface of the groove 53. By inserting each of the reflective panels 10-1 and 10-2 into the slit 51, adjacent reflective panels 10-1 and 10-2 can be held stably. Part of the main body 500 may be made of a non-conductive material.

[0021] Figures 4A, 4B, and 4C show examples of the layer configuration of the reflective panel 10. These layer configurations are the layer configurations in the thickness (Z) direction of the reflective panel 10. In Figure 4A, the reflective panel 10A has a dielectric layer 14, a conductive pattern 151 provided on one surface of the dielectric layer 14, a ground layer 13 provided on the opposite surface of the dielectric layer 14, and an adhesive layer 152A that bonds the conductive pattern 151 to the dielectric layer 14. A gap 155 is provided in at least a portion of the adhesive layer 152A.

[0022] The dielectric layer 14 is an insulating polymer film such as polycarbonate, cycloolefin polymer (COP), polyethylene terephthalate (PET), or fluororesin, with a thickness of approximately 0.3 mm to 1.0 mm. The dielectric layer 14 can be any material that has a relative permittivity and dielectric loss tangent suitable for achieving the target reflection characteristics in combination with the occupancy rate of the adhesive layer 152A.

[0023] The conductive pattern 151 forms the reflective surface of the reflective panel 10. The reflective surface formed by the conductive pattern 151 may include a metasurface whose reflective properties are artificially controlled. The conductive pattern 151 in this embodiment has a periodic pattern. The conductive pattern 151 is formed of a good conductor such as Cu, Ni, or Ag, and its thickness is 10 μm or more and 50 μm or less.

[0024] The adhesive layer 152A is a material capable of bonding the conductive pattern 151 to the dielectric layer 14, and may be a thermoplastic resin such as vinyl acetate resin, acrylic resin, cellulose resin, or silicone resin. The thickness of the adhesive layer 152A is 2 μm or more and 50 μm or less, and from the viewpoint of ensuring adhesive strength, it is desirable to have a thickness of 10 μm or more and 50 μm or less. In the example in Figure 4A, the adhesive layer 152A has a planar shape that is almost the same as that of the conductive pattern 151, and the occupancy rate of the adhesive layer 152A is almost the same as that of the conductive pattern 151.

[0025] In Figure 4B, the reflective panel 10B includes a dielectric layer 14, a conductive pattern 151 provided on one surface of the dielectric layer 14, a ground layer 13 provided on the opposite surface of the dielectric layer 14, and an adhesive layer 152B that bonds the conductive pattern 151 to the dielectric layer 14. Similar to Figure 4A, a gap 155 is provided in at least a portion of the adhesive layer 152B. In the example in Figure 4B, the planar shape of the adhesive layer 152B is larger than the planar shape of the conductive pattern 151. Multiple conductive patterns 151 may be held by a single adhesive layer 152B. However, the difference in occupancy between the conductive pattern 151 and the adhesive layer 152B is preferably 0.0% to 40.0%, more preferably 0.0% to 35.0%. A 0.0% occupancy difference includes cases where the pattern shapes of the conductive pattern 151 and the adhesive layer 152A match within the allowable tolerance range, as shown in Figure 4A, and cases where, even if the conductive pattern 151 and the adhesive layer 152 are misaligned in some locations, the average in-plane occupancy is approximately the same. If the occupancy difference between the conductive pattern 151 and the adhesive layer 152B exceeds 40.0%, the occupancy of the adhesive layer 152B becomes too large, making it difficult to suppress the decrease in reflective efficiency. Also, the occupancy of the conductive pattern 151 becomes too small, making it difficult to achieve the desired reflective characteristics and reflective efficiency. For these reasons, the conductive pattern 151 and the adhesive layer 152B are bonded to each other within the range of an occupancy difference between 0.0% and 40.0%.

[0026] In Figure 4C, the reflective panel 10C includes a dielectric layer 14, a conductive pattern 151 provided on one surface of the dielectric layer 14, a ground layer 13 provided on the opposite surface of the dielectric layer 14, and an adhesive layer 152 that bonds the conductive pattern 151 to the dielectric layer 14. The adhesive layer 152 may have a shape substantially the same as the conductive pattern 151, as shown by adhesive layer 152A in Figure 4A, or it may have a planar shape larger than the conductive pattern 151, as shown by adhesive layer 152B in Figure 4B. The reflective panel 10C also includes an intermediate layer 16 that covers the conductive pattern 151 and the adhesive layer 152A, a dielectric substrate 17 bonded to the conductive pattern 151 side by the intermediate layer 16, an intermediate layer 12 that covers the ground layer 13, and a dielectric substrate 11 bonded to the ground layer 13 side by the intermediate layer 12.

[0027] At least a portion of the gap 155 is filled by the intermediate layer 16. The intermediate layer 16 protects the surface of the conductive pattern 151 and also adheres to the dielectric substrate 17. The intermediate layer 16 is preferably durable and moisture resistant, and can be made of, for example, ethylene-vinyl acetate (EVA) copolymer or cycloolefin polymer (COP). The thickness of the intermediate layer 16 is 10 μm to 400 μm.

[0028] The dielectric substrate 17, as the outermost layer of the reflective panel 10C, is preferably made of a material with excellent impact resistance, durability, and transparency. Polycarbonate, acrylic resin, PET, etc., can be used as the dielectric substrate 17. The thickness of the dielectric substrate 17 is, for example, 1.0 mm to 10.0 mm.

[0029] The intermediate layer 12 protects the surface of the ground layer 13 and adheres to the dielectric substrate 11. The intermediate layer 12 is preferably durable and moisture-resistant, and can be made of materials such as ethylene-vinyl acetate (EVA) copolymer or cycloolefin polymer (COP). The thickness of the intermediate layer 12 is 10 μm to 400 μm.

[0030] The dielectric substrate 11, as the outermost layer of the reflective panel 10C, is preferably made of a material with excellent impact resistance, durability, and transparency. Polycarbonate, acrylic resin, PET, etc., can be used as the dielectric substrate 11. The thickness of the dielectric substrate 11 is, for example, 1.0 mm to 10.0 mm.

[0031] By covering the conductive pattern 151 with an intermediate layer 16 and joining it to the dielectric substrate 17, the intrusion of moisture and air into the surface of the conductive pattern 151 is suppressed, and the deterioration of the reflective surface is suppressed. By covering the ground layer 13 with an intermediate layer 12 and joining it to the dielectric substrate 11, the intrusion of moisture and air into the surface of the ground layer 13 is suppressed, and the surface deterioration of the ground layer 13 is suppressed. As a result, the capacitance between the ground layer 13 and the conductive pattern 151 is kept constant, and the magnitude of the designed phase delay can be maintained. In other words, the reflection efficiency of radio waves in the designed direction can be maintained.

[0032] As long as the conductive pattern 151 can be stably bonded to the dielectric layer 14, the planar shape of the adhesive layer may be smaller than the planar shape of the conductive pattern 151, the opposite of Figure 4B. Generally, if the adhesive layer is smaller than the conductive pattern 151, the conductive pattern 151 tends to peel off, but by adopting the configuration in Figure 4C, the conductive pattern 151 can be stably held. Even in this case, it is desirable that the difference in occupancy between the conductive pattern 151 and the adhesive layer 152B be 0.0% or more and 40.0% or less, preferably 0.0% or more and 35.0% or less. If the conductive pattern 151 is larger than the adhesive layer 152B, and the difference in occupancy between the conductive pattern 151 and the adhesive layer 152B exceeds 40.0%, the conductive pattern 151 may tilt with respect to the XY plane, which may make it difficult to achieve the designed reflection characteristics.

[0033] From the viewpoint of maintaining the reflectivity of the reflective panel 10 at 60% or higher, more preferably at 70% or higher, and suppressing a decrease in transmittance to visible light, the conductive pattern 151 has an appropriate occupancy rate. Specifically, it is desirable that the occupancy rate of the conductive pattern 151 relative to the dielectric layer 14 be between 10.0% and 45%. If the occupancy rate of the conductive pattern 151 exceeds 45%, the occupancy rate of the adhesive layer 152 will increase, which may make it impossible to maintain good reflectivity. In addition, the transmittance of the reflective panel 10 will decrease. If the occupancy rate of the conductive pattern 151 is less than 10.0%, it becomes difficult to achieve a reflectivity of 60% or higher.

[0034] In this embodiment, an appropriate occupancy ratio of the adhesive layer 152 that can suppress a decrease in reflectivity is investigated. The reflectivity characteristics of the reflective panel 10 having the layer configuration described above are evaluated by changing the occupancy ratio of the adhesive layer. Hereinafter, "occupancy ratio" refers to the area occupancy ratio.

[0035] Figure 5 shows Model 21 of the conductive pattern 151 used to evaluate the reflective panel 10. The evaluation model 21 includes a periodic arrangement of unit cells (also called "supercells") 210. The unit cells 210 are arranged in 6 rows in the X direction and 36 rows in the Y direction, forming a metasurface that reflects electromagnetic waves at an angle different from the angle of incidence.

[0036] Figure 6 is a schematic diagram showing the configuration of the unit cell 210 of Model 21. The unit cell 210 is formed by six metal patches 211, 212, 213, 214, 215, and 216. The width (W) and length (L) of metal patches 211-216 correspond to the width (X) and height (Y) of the reflective panel 10 in Figure 1, respectively. The metal patches 211-216 have equal width W and different lengths L, but their central axes are aligned (the Y coordinate position of the central axis is constant). The pitch in the X direction is constant. The phase of reflection is controlled by the shape and size of the metal patches 211-216, and the superposition of reflected waves forms a reflected beam in the desired direction. In this example, the unit cell 210 is designed so that the peak of the reflected wave of a normally incident (incident angle 0°) electromagnetic wave appears at a direction of 50° from the normal.

[0037] Figure 7 shows an example of the arrangement of conductive patterns 151 on the adhesive layer 152. Multiple conductive patterns 151 of different shapes and sizes constitute the unit cell 210 shown in Figure 6 on the adhesive layer 152. As shown in Figure 7, multiple conductive patterns 151 may be arranged on a single adhesive layer 152 to constitute a single unit cell 210. In this case, gaps 155 are provided between the adhesive layers 152 to separate the unit cells 210. As long as gaps 155 are provided at a predetermined ratio, the conductive patterns 151 may be arranged on a single adhesive layer 152 so as to form two or more unit cells 210 aligned in the Y direction. Alternatively, the conductive patterns 151 may be arranged on a single adhesive layer 152 so as to form two or more unit cells 210 aligned in the X direction.

[0038] In the evaluation, the conductive pattern 151 of Model 21 in Figure 5 is used, and a 28.0 GHz plane wave is incident at an incidence angle of 0° using general-purpose three-dimensional electromagnetic field simulation software, and the scattering cross-section of the reflected wave is analyzed. The scattering cross-section, or radar cross-section (RCS), is used as an indicator of the ability to reflect incident electromagnetic waves.

[0039] In the case of a metasurface that reflects at a different angle of reflection than the angle of incidence, the calculated power reflection efficiency needs to be corrected. An ideal conductive plate exhibits perfect specular reflection, reflecting electromagnetic waves in the same direction for perpendicular incidence, whereas a metasurface reflects electromagnetic waves in a direction different from the angle of incidence. The power reflection efficiency of a metasurface is calculated by dividing the power reflection efficiency obtained from the gain value by the correction value.

[0040] The reflected electric field on the lossless metasurface determined by the model pattern in Figure 5 is E. MR The reflected electric field in an ideal conductive plate is E PEC Therefore, the correction value ε p to |E MR / E PEC | 2 Let's assume that. |E MR / E PEC | is,

[0041]

number

[0042] [Formula] is expressed as. Here, θ is the angle of incidence on the metasurface, and φ is the reflection angle in the case of corresponding specular reflection. When the reflection angle of the metasurface is θ=50°, or θr=50°, the incident angle is θi=0°, and the reflection angle φ of specular reflection is 25°, the correction value ε p is 0.7826.

[0043] Figure 8 shows the analysis space 101 for electromagnetic wave simulation. The thickness direction of the layer structure of the reflection panel 10 is defined as the Z direction, the width direction of the metal patch of the model 21 in Figure 5 is defined as the X direction, and the length direction is defined as the Y direction, and the analysis space is expressed as (size in X direction) × (size in Y direction) × (size in Z direction). The size of the analysis space 101 when the frequency of the incident electromagnetic wave is 28.0 GHz is set to 83.9 mm × 192.6 mm × 3.7 mm. The boundary condition is designed such that an electromagnetic wave absorber 102 is arranged around the analysis space 101.

[0044] Figure 9A is a schematic diagram of the XY plane of the analysis space 101 surrounded by the electromagnetic wave absorber 102, Figure 9B is a schematic diagram of the XZ plane of the analysis space 101, and Figure 9C is a schematic diagram of the YZ plane of the analysis space 101. Within this analysis space 101, the power reflection efficiency is calculated by varying the occupancy rate of the adhesive layer 152 carrying the conductive pattern 151. All conductive patterns 151 used in the simulation are common. The six conductive patterns 151 constituting the unit cell 210 are each in the shape of a rectangle with a uniform width W of 0.4 mm, and their lengths L are 2.9751 mm, 3.0739 mm, 3.7536 mm, 2.0344 mm, 2.7300 mm, and 2.8497 mm, respectively. The center-to-center distance (pitch) in the X direction between the metal patches is uniformly 1.9283 mm.

[0045] <Example 1> A 0.7 mm thick polycarbonate film is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using a 0.36 mm thick Ag-based multilayer film. A 0.05 mm thick conductive pattern 151 is placed on the other side of the polycarbonate film via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 9.2%. An acrylic resin with a relative permittivity of 2.39 and a dielectric loss tangent of 0.05 at a frequency of 28.0 GHz is used as the adhesive layer 152. The conductive pattern 151 is formed from a 0.05 mm thick copper foil and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incident angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 10.2930 dB. This gain value is corrected by ε p The power reflection efficiency after correction with =0.7826 is 73.7%. With the occupancy rate of the adhesive layer 152 in Example 1, a power reflection efficiency of 70% or more can be obtained.

[0046] <Example 2> In Example 2, the layer structure is the same as in Example 1, but the occupancy rate of the adhesive layer 152 is changed. Specifically, a polycarbonate film with a thickness of 0.7 mm is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using an Ag-based multilayer film with a thickness of 0.36 mm. On the other side of the polycarbonate film, a conductive pattern 151 with a thickness of 0.05 mm is placed via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 11.5%. The adhesive layer 152 is an acrylic resin with a relative permittivity of 2.39 and a dielectric loss tangent of 0.05 at a frequency of 28.0 GHz. The conductive pattern 151 is formed from a copper foil with a thickness of 0.05 mm and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incident angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 11.4780 dB. This gain value is corrected by ε p The power reflection efficiency after correction with =0.7826 is 76.9%. With the occupancy rate of the adhesive layer 152 in Example 2, a power reflection efficiency of 75% or more can be obtained.

[0047] <Example 3> In Example 3, the layer structure is the same as in Examples 1 and 2, but the occupancy rate of the adhesive layer 152 is changed. Specifically, a polycarbonate film with a thickness of 0.7 mm is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using an Ag-based multilayer film with a thickness of 0.36 mm. On the other side of the polycarbonate film, a conductive pattern 151 with a thickness of 0.05 mm is placed via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 23.0%. The adhesive layer 152 is an acrylic resin with a relative permittivity of 2.39 and a dielectric loss tangent of 0.05 at a frequency of 28.0 GHz. The conductive pattern 151 is formed from a copper foil with a thickness of 0.05 mm and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incident angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 11.4530 dB. This gain value is corrected by ε p The power reflection efficiency after correction with =0.7826 is 76.4%. With the occupancy rate of the adhesive layer 152 in Example 3, a power reflection efficiency of 76% or more can be obtained.

[0048] <Example 4> In Example 4, the layer structure is the same as in Examples 1-3, but the occupancy rate of the adhesive layer 152 is changed. A polycarbonate film with a thickness of 0.7 mm is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using an Ag-based multilayer film with a thickness of 0.36 mm. On the other side of the polycarbonate film, a conductive pattern 151 with a thickness of 0.05 mm is placed via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 35.5%. The adhesive layer 152 is an acrylic resin with a relative permittivity of 2.39 and a dielectric loss tangent of 0.05 at a frequency of 28.0 GHz. The conductive pattern 151 is formed from a copper foil with a thickness of 0.05 mm and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incident angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 11.5220 dB. This gain value is corrected by ε p The power reflection efficiency after correction with =0.7826 is 77.7%. With the occupancy rate of the adhesive layer 152 in Example 4, a power reflection efficiency of 77% or more can be obtained.

[0049] <Example 5> In Example 4, the layer structure is the same as in Examples 1-4, but the occupancy rate of the adhesive layer 152 is changed. A polycarbonate film with a thickness of 0.7 mm is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using an Ag-based multilayer film with a thickness of 0.36 mm. On the other side of the polycarbonate film, a conductive pattern 151 with a thickness of 0.05 mm is placed via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 46.0%. The adhesive layer 152 is an acrylic resin with a relative permittivity of 2.39 and a dielectric loss tangent of 0.05 at a frequency of 28.0 GHz. The conductive pattern 151 is formed from a copper foil with a thickness of 0.05 mm and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incident angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 11.4940 dB. This gain value is corrected by ε p The power reflection efficiency after correction with =0.7826 is 77.2%. With the occupancy rate of the adhesive layer 152 in Example 5, a power reflection efficiency of 77% or more can be obtained.

[0050] <Comparative Example 1> In Comparative Example 1, the same layer structure and thickness of the adhesive layer 152 and conductive pattern 151 as in Examples 1-5 are used, but the occupancy rate of the adhesive layer 152 is set to 100%. This corresponds to a configuration in which the entire surface of one side of the dielectric layer 14 is covered with the adhesive layer 152. A polycarbonate film with a thickness of 0.7 mm is used as the dielectric layer 14. A ground layer 13 is set on one side of the polycarbonate film using an Ag-based multilayer film with a thickness of 0.36 mm. On the other side of the polycarbonate film, the conductive pattern 151 is placed via an adhesive layer 152 with a thickness of 0.01 mm and an occupancy rate of 100.0%. The adhesive layer 152 is an acrylic resin with a relative permittivity of 3.01 and a dielectric loss tangent of 0.08 at a frequency of 28.0 GHz. The conductive pattern 151 is formed from a copper foil with a thickness of 0.05 mm and has the pattern shape described above. When a 28.0 GHz plane wave incident at an incidence angle of 0° is reflected at a reflection angle of 50°, the gain value (peak value of the reflected waveform) at 50° in the RCS plot is 9.9770 dB. This gain value is corrected by εp The power reflection efficiency after correction with =0.7826 is 54.4%. With the occupancy rate of the adhesive layer 152 in Comparative Example 1, it is not possible to obtain a power reflection efficiency of 60% or more.

[0051] Examples 1 to 5 and Comparative Example 1 show that in order to maintain a power reflection efficiency of 60% or more, more preferably 70% or more, it is preferable that the adhesive layer 152 does not cover the entire surface of the dielectric layer 14. By providing a gap 155 in at least a part of the adhesive layer 152, the decrease in power reflection efficiency can be suppressed. This is thought to be because the influence of the adhesive layer 152 on the dielectric layer 14 can be reduced. When the thickness of the adhesive layer 152 is 0.02 μm or more and 0.05 μm or less, the power reflection efficiency can be maintained at 70% or more by setting the occupancy rate of the adhesive layer 152 to 9.0% or more and 50.0% or less.

[0052] Within the range of the occupancy rate of the adhesive layer 152 described above, the occupancy rate of the conductive pattern 151 relative to the dielectric layer 14 when the thickness of the conductive pattern 151 is 0.01 mm or more and 0.05 mm or less may be 10.0% or more and 45% or less.

[0053] The range of occupancy of the adhesive layer 152 partially provided on the surface of the dielectric layer 14 also applies to the configuration in Figure 4C. That is, the adhesive layer 152 provided with an occupancy of 9.0% to 50% and the conductive pattern 151 on the adhesive layer 152 may be covered with an intermediate layer 16. By covering the conductive pattern 151 and the adhesive layer 152 with an intermediate layer 16, changes in the surface state of the conductive pattern 151 due to the effects of oxygen, moisture, etc. can be suppressed, and weather resistance is improved.

[0054] When the dielectric substrate 17 is bonded to the conductive pattern 151 by the intermediate layer 16, the impact resistance and durability of the reflective panel 10 are improved. In this case, the thickness of the intermediate layer 16 should be such that it is possible to ensure moisture resistance and protection for the conductive pattern 151 and bond the dielectric substrate 17. For example, an adhesive film with a thickness of 10 μm to 400 μm can be used as the intermediate layer 16. The same applies to the intermediate layer 12 provided on the ground layer 13 side.

[0055] The outermost dielectric substrate 17 can be any substrate that is transparent to the operating frequency, highly transparent to visible light, and has excellent durability. On the other hand, to prevent the thickness and weight of the reflective panel 10 from becoming too large, it is desirable that the thickness be 1.0 mm or more and 5.0 mm or less, more preferably 1.0 mm or more and 3.0 mm or less. The dielectric substrate 11 provided on the ground layer 13 side is similar.

[0056] The electromagnetic wave reflecting device of the embodiment is not limited to the configuration examples described above. In Examples 1 to 5, an acrylic resin with specific relative permittivity and dielectric loss tangent is used as the adhesive layer 152 in the calculation, but the occupancy rate of the adhesive layer 152 (9.0% to 50.0%) is also valid when using a general adhesive with a relative permittivity of 2.0 to 4.5 and a dielectric loss tangent of 0.10 or less. Furthermore, the range of the occupancy rate of the adhesive layer 152 is valid over a range from 1 GHz to 28 GHz ± 4 GHz. The reflection angle for perpendicular incidence can be appropriately designed in the range of 35° to less than 90° by designing the size, shape, and pitch of the conductive pattern 151 and the dielectric constant of the dielectric layer 14. The in-plane size of the reflective panel 10 of the electromagnetic wave reflecting device can be appropriately selected in the range of 30 cm × 30 cm to 3 m × 3 m. The entire surface of the reflective panel 10 may be a metasurface, or a part of it may be a metasurface and the rest a specular reflective surface. In that case as well, the entire surface of the reflective surface may be covered with a moisture-resistant and durable adhesive film (intermediate layer) and then bonded to the dielectric substrate. When forming a metasurface provided on part or all of the reflective surface, a gap 155 is provided so that the adhesive layer 152 supporting the conductive pattern 151 is not continuous across the entire surface of the dielectric layer 14. At this time, the occupancy rate of the adhesive layer 152 over the dielectric layer 14 may be set to 9.0% or more and 50.0% or less. The electromagnetic wave reflecting device 60 and electromagnetic wave reflecting fence of this embodiment can be installed both indoors and outdoors.

[0057] This application claims priority based on Japanese Patent Application No. 2022-089849, filed on June 1, 2022, and includes the entire contents of that Japanese Patent Application. [Explanation of Symbols]

[0058] 10, 10-1, 10-2, 10-3 Reflective Panels 11, 17 Dielectric substrate 12, 16 Middle class 13 Ground Layer 14 Dielectric layer 151 Conductive Patterns 152, 152A, 152B adhesive layer 50 Frame (Side Frame) 57 Top Frame 58 Bottom Frame 60, 60-1, 60-2, 60-3 Electromagnetic wave reflector 100 Electromagnetic wave reflective fence 210 unit cells

Claims

1. A reflective panel that reflects radio waves in a desired frequency band selected from the frequency band of 1 GHz or more and 170 GHz or less, A frame that holds the reflective panel, Equipped with, The reflective panel comprises a dielectric layer, a periodic conductive pattern provided on one surface of the dielectric layer, a ground layer provided on the other surface of the dielectric layer, and an adhesive layer that bonds the conductive pattern to the one surface of the dielectric layer. A gap is provided in the aforementioned adhesive layer, An electromagnetic wave reflecting device wherein the thickness of the adhesive layer is 0.002 mm or more and 0.05 mm or less, and the occupancy rate of the adhesive layer over the dielectric layer is 9.0% or more and 50.0% or less.

2. The electromagnetic wave reflecting device according to claim 1, wherein the thickness of the conductive pattern is 0.01 mm or more and 0.05 mm or less, and the occupancy rate of the conductive pattern over the dielectric layer is 10.0% or more and 45.0% or less.

3. The electromagnetic wave reflecting device according to claim 2, wherein the adhesive layer and the conductive pattern are bonded to each other, and the difference in occupancy is 0.0% or more and 40.0% or less.

4. A reflective panel that reflects radio waves in a desired frequency band selected from the frequency band of 1 GHz or more and 170 GHz or less, A frame that holds the reflective panel, Equipped with, The reflective panel comprises a dielectric layer, a periodic conductive pattern provided on one surface of the dielectric layer, a ground layer provided on the other surface of the dielectric layer, and an adhesive layer that bonds the conductive pattern to the one surface of the dielectric layer. A gap is provided in the aforementioned adhesive layer, The adhesive layer and the intermediate layer covering the conductive pattern, An electromagnetic wave reflecting device further comprising the intermediate layer filling at least a portion of the gap in the adhesive layer.

5. The intermediate layer provides a dielectric substrate that is bonded onto the conductive pattern. The electromagnetic wave reflecting device according to claim 4, further comprising:

6. An electromagnetic wave reflecting fence comprising a plurality of electromagnetic wave reflecting devices according to any one of claims 1 to 5, connected by the frame.

7. The electromagnetic wave reflective fence according to claim 6, wherein at least a portion of the reflective panel is a metasurface with different angles of incidence and reflection.

8. Dielectric layer and A periodic conductive pattern is provided on one surface of the dielectric layer, A ground layer provided on the other surface of the dielectric layer, The conductive pattern is bonded to one surface of the dielectric layer, and the adhesive layer is provided for this purpose. A gap is provided in the aforementioned adhesive layer, It reflects radio waves in a desired frequency band selected from the frequency band between 1 GHz and 170 GHz. A reflective panel in which the thickness of the adhesive layer is 0.002 mm or more and 0.05 mm or less, and the occupancy rate of the adhesive layer over the dielectric layer is 9.0% or more and 50.0% or less.

9. Dielectric layer and A periodic conductive pattern is provided on one surface of the dielectric layer, A ground layer provided on the other surface of the dielectric layer, The conductive pattern is bonded to one surface of the dielectric layer, and the adhesive layer is provided for this purpose. A gap is provided in the aforementioned adhesive layer, It reflects radio waves in a desired frequency band selected from the frequency band between 1 GHz and 170 GHz. A reflective panel further comprising the adhesive layer and an intermediate layer covering the conductive pattern, wherein the intermediate layer fills at least a portion of the gaps in the adhesive layer.

Citation Information

Patent Citations

  • Filters created with metamaterials

    JP2014534459A

  • 3-dimensional standing type metamaterial structure and method of fabricating the same

    US20120113502A1

  • Wireless transmission system

    WO2021199504A1