Method for producing fluoroolefin
Patent Information
- Application Number
- JP2024515152
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-10-03
- Filing Date
- 2023-10-02
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2043-10-02
AI Technical Summary
Existing methods for producing fluoroolefins face low reaction conversion rates, high by-product formation, complex reaction processes leading to waste liquid generation, and difficulty in separating impurities with similar physical properties.
A dehydrofluorination reaction using activated carbon containing a metal salt catalyst is performed in a gas phase at controlled temperatures to enhance conversion rates and selectivity, minimizing by-products and waste liquid production.
The method achieves high conversion rates and selectivity for fluoroolefins with reduced by-products and eliminates waste liquid generation, while suppressing the formation of difficult-to-separate impurities.
Abstract
Description
[Technical field]
[0001] The present invention relates to a process for producing fluoroolefins. [Background technology]
[0002] Hydrofluoroolefins (HFOs) are known as desirable alternatives to HCFCs due to their low ODP (Ozone Depletion Potential) and GWP (Global Warming Potential) values. HFOs are known compounds useful as refrigerants, heat transfer fluids, fire extinguishing agents, propellants, foaming agents, blowing agents, gas derivatives, polymerization media or monomers.
[0003] Patent Document 1 describes a method for producing pentafluoropropene by contacting hexafluoropropane with a catalyst containing magnesium, zinc, aluminum, or the like, optionally in the presence of an inert gas, at a temperature of about 200° C. to 500° C. Patent Document 2 describes a method for producing 1,1,1,3,3,3-pentafluoropropene, characterized in that 1,1,1,3,3,3-hexafluoropropane in a gaseous state is contacted with activated carbon to remove hydrofluorination. Patent Document 3 describes a compound represented by formula (a): C3F x Cl y H 8-x-y (b) reacting, in the liquid phase, the halogenated propane with an aqueous base to produce a halogenated propane having the formula: C3F z-1 H 7-z(wherein z is x-1), (c) removing at least a portion of the halogenated propene from the reactor as a vapor stream, and (a), (b) and (c) are carried out at least partially simultaneously. Patent Document 4 describes that 1,1,3,3,3-pentafluoropropene (CF3CH=CF2, HFC-1225zc) can be produced by pyrolysis of 1,1,1,3,3,3-hexafluoropropane (CF3CH2CF3, HFC-236fa) in an empty tubular reactor whose inner surface comprises a material made of material resistant to hydrogen fluoride in the absence of a dehydrofluorination catalyst at a temperature of about 700°C to about 1000°C and at a total pressure of about atmospheric pressure. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Special Publication No. 2001-509803 [Patent Document 2] Japanese Patent Application Publication No. 9-67281 [Patent Document 3] U.S. Patent Publication No. 2011 / 0269999 [Patent Document 4] Special Publication No. 2008-518938 Summary of the Invention [Problem to be solved by the invention]
[0005] However, in Patent Document 1 and Patent Document 2, there is a problem that the reaction conversion rate is low in the method using a catalyst containing magnesium, zinc, aluminum, etc. or coconut shell activated carbon. In addition, in Patent Document 3, there is a problem that the reaction method becomes complicated in the reaction using an aqueous base, such as continuously introducing an aqueous base and a phase transfer catalyst, and returning unreacted raw materials to the reactor under reflux conditions, and a large amount of waste liquid is generated under large-scale production conditions. In addition, in Patent Document 4, there is a problem that the pyrolysis reaction under high temperature conditions synthesizes multiple types of impurities with similar physical properties that are difficult to separate by distillation purification at a high production rate.
[0006] Therefore, an object of the present invention is to provide a method for producing a fluoroolefin which has a high reaction conversion rate and a high selectivity for the target product, which allows the target product to be obtained in a high yield, which has a low ratio of by-products, and which does not produce waste liquid, thereby solving the problems of the conventional techniques. [Means for solving the problem]
[0007] The present invention provides the following: [1] A method for producing a fluoroolefin, comprising subjecting a fluorinated alkane to a dehydrofluorination reaction in the presence of activated carbon containing a metal salt. [2] The fluoroolefin is represented by the following general formula (1): CxHyFz (1) (In the formula, x=3~5, y≧1, z≧1, y+z≦2x) The method according to [1], represented as [3] The fluorinated alkane is represented by the following general formula (2): CxHmFn (2) (In the formula, x=3~5, m≧2, n≧2, m+n=2x+2) The method according to [2], represented as [4] The method according to any one of [1] to [3], wherein the dehydrofluorination reaction is carried out in a gas phase. [5] The method according to [4], wherein the dehydrofluorination reaction is carried out at a temperature of 250 to 650°C. [6] The method according to any one of [1] to [3], wherein the metal of the metal salt is an alkali metal and / or an alkaline earth metal. Effect of the Invention
[0008] According to the present invention, a method for producing fluoroolefins that solves the problems of the prior art is provided, which has a high reaction conversion rate and a high selectivity for the target product, produces the target product in a high yield, has a low ratio of by-products, and does not produce waste liquid. According to the present invention, by using activated carbon containing a metal salt catalyst, a high conversion rate can be achieved even when the reaction temperature is lowered. As a result of lowering the reaction temperature, the production of impurities that have similar physical properties and are difficult to separate in distillation purification is suppressed. A high conversion rate was achieved even at a temperature of about 500°C inside the reactor. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic diagram of an example of an apparatus for carrying out the dehydrofluorination reaction of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] [Feedstock and products] The feedstock of the present invention is a fluorinated alkane composed of fluorine atoms, hydrogen atoms and carbon atoms. In the present invention, since a fluoroolefin is produced by a dehydrofluorination reaction, it is necessary for the fluorinated alkane to have at least one hydrogen atom. The product fluoroolefin is preferably represented by the following general formula (1): CxHyFz (1) (In the formula, x=3 to 5, y≧1, z≧1, and y+z≦2x.) In this case, the fluorinated alkane that is the feed material is preferably represented by the following general formula (2): CxHmFn (2) (In the formula, x=3 to 5, m≧2, n≧2, and m+n=2x+2.) It is expressed as:
[0011] Examples of the fluorinated alkane raw material include 1,1,1,3,3,3-hexafluoropropane (HFC-236fa), 1,1,2,3,3,3-hexafluoropropane (HFC-236ea), 1,1,1,2,4,4,4-heptafluorobutane, 1,1,1,2,3,3,3-heptafluoro-2-methylbutane, 1,1,1,3,3,3-heptafluoro-2-(monofluoromethyl)butane, 1,1,1,2,5,5,5-heptafluoropentane, 1,1,1,3,5,5,5-heptafluoropentane, and 1,1,1,4,4,4-hexafluorobutane. These can be used alone or in a mixture of two or more kinds.
[0012] Examples of product fluoroolefins include 1,1,3,3,3-pentafluoropropene (HFO-1225zc), (E)-1,2,3,3,3-pentafluoropropene ((E)-HFO-1225ye), (Z)-1,2,3,3,3-pentafluoropropene ((Z)-HFO-1225ye), 1,1,1,4,4,4-hexafluorobut-2-ene, 3,3,3-trifluoro-2-trifluoromethylprop-1-ene, 1,1,1,5,5,5-hexafluoropent-2-ene, 1,1,4,4,4-pentafluorobut-1-ene, and the like.
[0013] [Reaction catalyst] In the present invention, activated carbon containing a metal salt is used as a reaction catalyst. Examples of the metal salt include halides (particularly chlorides, fluorides, bromides, iodides, etc.) of alkali metals and alkaline earth metals, hydroxides, carbonates, hydrogen carbonates, nitrates, sulfites, sulfates, acetates, etc. More specific examples of metal salts include alkali metal salts such as lithium chloride, sodium chloride, potassium chloride, lithium fluoride, sodium fluoride, potassium fluoride, lithium hydroxide, sodium hydroxide, potassium hydroxide, lithium carbonate, sodium carbonate, potassium carbonate, lithium hydrogen carbonate, sodium hydrogen carbonate, potassium hydrogen carbonate, lithium sulfate, sodium sulfate, potassium sulfate, lithium acetate, sodium acetate, and potassium acetate; alkaline earth metal salts such as barium chloride, magnesium chloride, calcium chloride, barium fluoride, magnesium fluoride, calcium fluoride, barium hydroxide, magnesium hydroxide, calcium hydroxide, barium carbonate, magnesium carbonate, calcium carbonate, barium hydrogen carbonate, barium hydrogen carbonate, calcium hydrogen carbonate, barium sulfate, magnesium sulfate, calcium sulfate, barium acetate, magnesium acetate, and calcium acetate; and the like. These can be used alone or in a mixture of two or more.
[0014] The present invention is characterized by using activated carbon containing the above-mentioned metal salt. Examples of activated carbon catalysts include coconut shell carbon for gas purification, catalysts, and catalyst carriers (Takeda Pharmaceutical's Granular Shirasagi GX, SX, CX, and XRC, Toyo Calgon's PCB, and Taihei Chemical Industry's Yashikoru, Kuraray Coal GG, and GC), which can be used alone or in combination of two or more. The amount of metal salt supported in the activated carbon is preferably 0.01 to 10% by weight, more preferably 0.1 to 5% by weight, and even more preferably 0.5 to 1.5% by weight, based on the total weight of the supported catalyst. Activated carbon that has not been subjected to an acid washing treatment or the like contains naturally occurring metal salts. In this case, the amount of metal salt supported (i.e., the content) is determined, for example, by SEM-EDX. The amount supported by SEM-EDX is determined by measuring several points on the surface of a sample using SEM-EDX and averaging the measured values. Preferred properties of activated carbon include pH and acetone adsorption capacity, with the pH being preferably in the range of 8 to 12, more preferably 9 to 11, and the acetone adsorption capacity being preferably 29% by weight or more, more preferably 35% by weight or more. The shape of the activated carbon is not particularly limited, and any shape such as granular, powdered, pelleted, spherical, cylindrical, honeycomb, sheet, or fibrous may be used. The type of activated carbon is not particularly limited, and any shape such as steam charcoal, crushed charcoal, or granulated charcoal derived from coconut shell charcoal, coal, or wood charcoal may be used. Coconut shell charcoal is the most preferred activated carbon.
[0015] [Reaction conditions] The reaction temperature is preferably 250° C. to 650° C., more preferably 400° C. to 625° C., even more preferably 500° C. to 600° C., and particularly preferably 500° C. to 550° C. The contact time between the reaction substrate and the catalyst (activated carbon carrying a metal salt) is preferably 0.1 to 300 seconds, more preferably 5 to 120 seconds, and even more preferably 10 to 60 seconds.
[0016] [Carrier gas] In carrying out the present invention, a carrier gas is used for diluting the raw material gas, drying the reactor, etc. In particular, the raw materials, reaction products, and other substances can be moved through the reactor while adjusting the concentration by flowing the carrier gas. A gas that does not react with these substances is selected as the carrier gas. Examples of the carrier gas include nitrogen and rare gases (helium, neon, argon, etc.). When a carrier gas is used, the carrier gas is usually mixed at a ratio of 0 to 99%, more preferably 0 to 75%, and most preferably 0 to 50% with respect to the total flow rate of the raw materials, reaction products, and other substances.
[0017] [Reaction Apparatus] Examples of materials for the reaction apparatus include corrosion-resistant metals such as stainless steel, Inconel, Monel, Hastelloy, nickel, etc. Among these, nickel is preferred from the viewpoint of corrosion resistance.
[0018] An example of an apparatus for carrying out the dehydrofluorination reaction of the present invention is a cylindrical tube equipped with a heater for adjusting the reaction temperature, filled with catalysts of various shapes, and configured to allow the raw material gas to flow from one end of the tube to the other. When the cylindrical tube loaded with the catalyst is extended vertically, the raw material gas is preferably flowed uniformly from top to bottom little by little, since the raw material gas can be flowed little by little by utilizing gravity. When the cylindrical tube is extended vertically and the raw material gas is flowed from bottom to top, it is preferable in terms of reaction efficiency to place a pellet-like catalyst with a large particle size at the bottom of the cylindrical tube and a powder-like catalyst with a small particle size at the top of the cylindrical tube.
[0019] In Fig. 1, which illustrates an outline of a specific example of an apparatus for carrying out a dehydrofluorination reaction of the present invention, the apparatus comprises a raw material storage tank 1 for storing a raw material (reaction substrate), a cylinder (nitrogen cylinder 2 in Fig. 1) for supplying a carrier gas (e.g., nitrogen gas) to an evaporator 4, a cylindrical catalyst tower 3 installed vertically and connected to the raw material storage tank by piping, an evaporator 4 installed just before the catalyst tower, and a collection tank 5 located downstream of the catalyst tower. If the raw material is a liquid at room temperature, it is injected as is into the evaporator 4, which has been heated to a temperature equal to or higher than its boiling point, by a syringe pump (not shown), and is vaporized in the evaporator 4. The raw material gas is mixed with a carrier gas (nitrogen gas) in the evaporator 4, and this mixed gas comes into contact with a catalyst while moving from the top to the bottom of the catalyst tower, promoting the dehydrofluorination reaction. The reaction gas that has passed through the bottom of the catalyst tower passes through a collection tank filled with water, during which the reaction products, unreacted raw materials, and hydrogen fluoride are collected in the collection tank, and only the carrier gas is discharged outside the reactor. EXAMPLES
[0020] [Catalyst preparation] The catalyst used in the examples was granular Shirasagi C2X (grade name: C2x4 / 6-2), a coconut shell-based activated carbon supplied by Osaka Gas Chemicals Co., Ltd., which was immersed in an aqueous solution containing the metal salts listed in Table 1. The amount of catalyst supported was determined by confirming the concentration distribution of elements on the surface of the measurement object using SEM-EDX. The amount of support was determined by measuring three points on the sample surface and averaging the measured values.
[0021] [Examples 1 to 13] Activated carbon containing the metal salts shown in Table 1 was packed into a cylindrical nickel reactor (size: diameter 2 inches, length 1000 mm) and dried by heating. The raw material 1,1,1,3,3,3-hexafluoropropane (HFC-236fa) was then passed from the top to the bottom of the cylindrical reactor without using a carrier gas, and reacted at the temperature, linear velocity, and residence time shown in Table 1. In the downstream of the reactor, the crude product gas was obtained through a water trap to remove the generated HF, a molecular sieve (MS-3A) packed tower for the purpose of dehydrating the crude product gas, and a filter for removing particles. The composition of the crude product gas was confirmed by GC analysis. The results are shown in Table 1.
[0022] [Comparative Examples 1 to 3] The reaction was carried out in the same manner as in Example 1, except that activated carbon not supporting a metal salt was used as a catalyst, or that no catalyst was used. The results are shown in Table 1.
[0023] [Table 1]
[0024] In Table 1, the impurity generation ratio is the GC area ratio (corresponding to the molar ratio) of each impurity when the GC area of the entire crude product injected into a gas chromatograph (GC) is taken as 100%. The conversion rate (%) is 100%-[(after reaction: moles of HFC-236fa in the crude gas) / (before reaction: moles of HFC-236fa introduced)]×100%. The selectivity (%) is [(after reaction: moles of HFO-1225zc in the crude gas / moles of converted HFC-236fa)]×100%. The impurities are indicated as follows: 1225yeZ: Z isomer of CF3-CF=CHF 1225yeE: E isomer of CF3-CF=CHF 1234zeE: E isomer of CF3-CH=CHF
[0025] From Table 1, when dehydrofluorination reaction of 1,1,1,3,3,3-hexafluoropropane (HFC-236fa) was carried out at a temperature of 500 to 550 ° C. in the presence of metal salt-supported activated carbon containing 0.5 to 5 wt % of alkali metal hydroxide, alkali metal hydrogen carbonate, alkali metal carbonate, alkali metal acetate, and alkaline earth metal chloride, the product: 1,1,3,3,3-pentafluoropropene (HFO-1225zc) was obtained with a conversion rate of more than 60% and a selectivity rate of more than 80% when an alkali metal salt was used (Examples 1 to 9), and with a conversion rate of more than 56% and a selectivity rate of more than 86% when an alkaline earth metal salt was used (Examples 10 to 13). From the viewpoint of obtaining high-purity HFO-1225zc free of impurities, a post-purification yield of 60% or more was achieved in Examples 1 to 9, and a post-purification yield of 50% or more was achieved in Examples 10 to 13. When an alkaline earth metal salt was used as the metal salt, the conversion rate was lower than when an alkali metal salt was used, but the selectivity was comparable to when an alkali metal salt was used. On the other hand, in Comparative Example 1, in which activated carbon not supporting a metal salt was used as a catalyst, and Comparative Example 2, in which no catalyst was used, the conversion rates were 38.5% and 37.2%, respectively. In addition, when no catalyst was used but the reaction temperature was as high as 775°C, a conversion rate of 73% was obtained, but impurities (1225yeZ, 1225yeE, 1234zeE) that are difficult to separate from the product HFO-1225zc were each generated at 0.1% or more. Production conditions under which these impurities are generated at a concentration of 0.1% or more cannot be adopted because the impurities cannot be removed by distillation purification.
Claims
1. A method for producing a fluoroolefin, comprising the steps of: subjecting a fluorinated alkane to a dehydrofluorination reaction in the presence of activated carbon containing a metal salt.
2. The fluoroolefin is represented by the following general formula (1): CxHyFz (1) (In the formula, x=3-5, y≧1, z≧1, y+z≦2x) The method of claim 1 , wherein
3. The fluorinated alkane is represented by the following general formula (2): CxHmFn (2) (In the formula, x=3 to 5, m≧2, n≧2, m+n=2x+2) The method according to claim 2 , wherein
4. The method of claim 3, wherein the fluoroolefin is 1,1,3,3,3-pentafluoropropene (HFO-1225zc) and the fluorinated alkane is 1,1,1,3,3,3-hexafluoropropane (HFC-236fa).
5. The process according to any one of claims 1 to 4, wherein the dehydrofluorination reaction is carried out in a gas phase.
6. The process of claim 5, wherein the dehydrofluorination reaction is carried out at a temperature of from 250 to 650° C.
7. The process of claim 6, wherein the dehydrofluorination reaction is carried out at a temperature of from 400 to 625°C.
8. The process according to claim 7, wherein the dehydrofluorination reaction is carried out at a temperature of from 500 to 550°C.
9. The method according to any one of claims 1 to 4, wherein the metal of the metal salt is an alkali metal and / or an alkaline earth metal.
10. 10. The method of claim 9, wherein the metal salt content of the activated carbon is 0.5 to 5% by weight.
11. 5. The method of claim 4, wherein the metal of the metal salt is an alkali metal.
12. The method of claim 11, wherein the metal salt content of the activated carbon is 0.5 to 5% by weight.
13. 13. The method of claim 12, wherein the dehydrofluorination reaction is carried out in the gas phase.
14. The process according to claim 13, wherein the dehydrofluorination reaction is carried out at a temperature of from 500 to 550° C.