Method for manufacturing heating mattress pad
The manufacturing method for a heating mattress pad using carbon fiber and fluororubber coatings addresses durability and flexibility issues, ensuring stability and safety at high temperatures.
Patent Information
- Application Number
- KR1020250006528
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-01-16
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2045-01-16
AI Technical Summary
Existing heating mattress pads face issues with physical property changes at high temperatures, lack of durability, and flexibility due to carbon fiber limitations, and safety concerns from metal resistors.
A manufacturing method involving carbon fiber weft, microwire warp, fluororubber coating, and surface coating to create a heating mattress pad with enhanced rigidity, durability, and flexibility, using materials like fluororubber, conductive microwires, and specific coatings to address these issues.
The method produces a heating mattress pad that maintains physical properties at high temperatures, offers excellent durability and flexibility, and ensures safety by minimizing harmful magnetic fields.
Smart Images

Figure 112025006025778-PAT00002_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a method for manufacturing a heating mattress pad, and more specifically, to a method for manufacturing a heating mattress pad that is rigid and does not change in physical properties even at high temperatures by coating the heating pad with fluororubber, and has excellent durability and rigidity against repeated vertical pressure or impact, which is a disadvantage of carbon fiber, and good flexibility by strongly bonding and coating the electrode metal wire and carbon fiber yarn. Background Technology
[0003] Generally, a heating element is an object that converts electrical energy into thermal energy and transmits energy by radiating that heat to the outside.
[0004] These heating elements are widely used in various home appliances and general industrial fields, and are classified into metallic resistors, non-metallic resistors, and other resistors depending on the material. Recently, due to a renewed awareness of energy conservation and environmental issues, extensive research on the manufacturing and application of heating elements is being conducted in many countries.
[0005] However, while metal resistors have the advantages of minimal deformation at high temperatures, good processability, and good oxidation resistance, they generate heat at high pressures, meaning the magnetic field generated when current flows can be harmful to the human body. Additionally, since high-voltage AC power is typically used, the high voltage poses a safety risk in itself. In particular, conventional resistors made by adding barium, titanium, and other additives to ceramics—a type of other resistor—have the disadvantages of high power consumption and magnetic fields that are harmful to the human body when current flows.
[0006] Conventionally, to implement planar heating elements, resistors arranged in a meandering pattern were inserted into a fabric and Velcro was attached to the fabric to heat or warm the required areas. However, this method had the problem of the resistors easily breaking due to repeated bending, and powder was also generated as the rubber surrounding the resistors dried out. Furthermore, there were limitations in realizing the desired shape during the sewing process, and production costs were high because the entire process was primarily manual, involving sewing. Prior art literature
[0008] Korean Registered Patent No. 10-2098314 (Registered April 1, 2020) Korean Registered Patent No. 10-2052717 (Registered November 29, 2019) Korean Registered Patent No. 10-1545699 (Registered August 12, 2015) The problem to be solved
[0009] The problem that the present invention aims to solve is to provide a method for manufacturing a heating mattress pad that is rigid and does not change in physical properties even at high temperatures by coating the heating pad with fluororubber, and has excellent durability, robustness, and flexibility against repeated vertical pressure or impact, which are disadvantages of carbon fiber, by strongly bonding and coating the electrode metal wire and carbon fiber yarn.
[0010] The various problems that the present invention aims to solve are not limited to those mentioned above, and other unmentioned problems will be clearly understood by those skilled in the art from the description below. means of solving the problem
[0012] In one embodiment of the technical concept of the present invention, a method for manufacturing a heating mattress pad is disclosed.
[0013] The method for manufacturing the above-described heating mattress pad comprises: a carbon fiber weft manufacturing step (S100) for manufacturing a carbon fiber weft formed including carbon fibers; a microwire warp manufacturing step (S200) for manufacturing a microwire warp formed including microwires; a heating fabric manufacturing step (S300) for manufacturing a heating fabric using the carbon fiber weft and the microwire warp; a fluororubber coating layer forming step (S400) for forming a fluororubber coating layer on the heating fabric; and a surface coating step (S500) for forming a surface coating layer on the heating fabric on which the fluororubber coating layer is formed.
[0014] In the above microwire gradient manufacturing step (S200), the microwire gradient is manufactured by preparing a glass fiber and coating the glass fiber with a conductive material, wherein the conductive material may be a conductive polymer, a carbon nanostructure, a metal oxide, a metal nanowire, a metal nanoparticle, a carbon paste, a metal paste, or a combination thereof.
[0015] In the above fluororubber coating layer formation step (S400), the fluororubber coating layer is formed by applying a fluororubber coating composition to the heating fabric and then drying it, wherein the fluororubber may be selected from the group consisting of a binary copolymer of vinylidene fluoride (VF) and hexafluoropropylene (HFP); a ternary copolymer of vinylidene fluoride (VF), tetrafluoroethylene (TFE), and perfluoromethylvinyl ether (PMVE); a ternary copolymer of vinylidene fluoride (VF), hexafluoropropylene (HFP), and tetrafluoroethylene (TFE); and combinations thereof.
[0016] In the fluororubber coating layer formation step (S400), the fluororubber coating composition comprises fluororubber, a rust inhibitor, a filler, a crosslinking agent, a vulcanizing agent, and a vulcanization accelerator, wherein the fluororubber coating composition may be included in a weight ratio of 80 to 120 parts by weight of fluororubber, 1 to 5 parts by weight of rust inhibitor, 5 to 10 parts by weight of filler, 1 to 3 parts by weight of crosslinking agent, 2 to 4 parts by weight of vulcanizing agent, and 0.5 to 1.5 parts by weight of vulcanization accelerator.
[0017] In the above step of forming a fluororubber coating layer (S400), the filler may include illite powder, volcanic scoria powder, seashell powder, and bamboo charcoal powder, wherein the filler may be included in a weight ratio of 1 to 5 parts by weight of illite powder, 3 to 7 parts by weight of volcanic scoria powder, 2 to 4 parts by weight of seashell powder, and 1 to 3 parts by weight of bamboo charcoal powder.
[0018] In the surface coating step (S500), the surface coating liquid composition is prepared by mixing 10 to 30 parts by weight of an additive with respect to 100 parts by weight of the total content of the thermosetting resin, and by adding 10 to 30 parts by weight of a solvent to the mixture to disperse and mix it, wherein melamine resin is used as the thermosetting resin, and the additive may be included in a weight ratio of 80 to 120 parts by weight of expanded graphite powder, 60 to 80 parts by weight of a flame retardant, 1 to 10 parts by weight of graphene, 1 to 10 parts by weight of nanoceramic particles, and 1 to 10 parts by weight of titanium dioxide nanoparticles.
[0019] Specific details of other embodiments are included in the detailed description. Effects of the invention
[0021] A method for manufacturing a heating mattress pad according to various embodiments of the technical concept of the present invention can manufacture a heating mattress pad that is rigid and does not change in physical properties even at high temperatures by coating the heating pad with fluororubber, and has excellent durability and rigidity against repeated vertical pressure or impact, which is a disadvantage of carbon fiber, and has good flexibility by strongly bonding and coating the electrode metal wire and carbon fiber yarn.
[0022] It will be fully understood that various embodiments of the technical concept of the present invention may provide various effects not specifically mentioned. Brief explanation of the drawing
[0024] FIG. 1 is a flowchart for schematically explaining a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention. FIG. 2 is a plan view showing an example of a heating element manufactured using a heating fabric in a method for manufacturing a heating mattress pad according to an embodiment of the technical concept of the present invention. Specific details for implementing the invention
[0025] The advantages and features of the present invention, and the methods for achieving them, will become clear by referring to the embodiments described in detail below. However, the present invention is not limited to the embodiments described herein and may be embodied in other forms. Rather, the embodiments introduced herein are provided to ensure that the disclosed content is thorough and complete, and to ensure that the spirit of the present invention is sufficiently conveyed to those skilled in the art.
[0026] The terms used in this application are used merely to describe specific embodiments and are not intended to limit the invention. The singular expression includes the plural expression unless the context clearly indicates otherwise.
[0027] Unless otherwise defined, all terms used herein, including technical or scientific terms, have the same meaning as generally understood by those skilled in the art to which the present invention pertains. Terms such as those defined in commonly used dictionaries should be interpreted as having a meaning consistent with their meaning in the context of the relevant technology, and should not be interpreted in an ideal or overly formal sense unless explicitly defined in this application.
[0029] Hereinafter, a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention will be described in detail with reference to the attached drawings.
[0031] FIG. 1 is a flowchart for schematically explaining a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention, and FIG. 2 is a plan view showing an example of a heating element manufactured using a heating fabric in a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention.
[0033] Referring to FIGS. 1 and 2, a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention includes a carbon fiber weft manufacturing step (S100), a fine wire warp manufacturing step (S200), a heating fabric manufacturing step (S300), a fluororubber coating layer forming step (S400), and a surface coating step (S500).
[0035] 1. Carbon fiber weft manufacturing step (S100)
[0036] The above carbon fiber weft manufacturing step (S100) is a step of manufacturing a carbon fiber weft formed including carbon fibers.
[0037] In the above carbon fiber weft manufacturing step (S100), the carbon fiber weft can be woven to intersect at a right angle with the fine wire warp to form a heating fabric, and the carbon fiber weft is manufactured including carbon fibers and can be manufactured by the following method.
[0038] That is, in order to manufacture the above carbon fiber weft, carbon fibers can be prepared first.
[0039] The carbon fiber mentioned above is one-fifth lighter than steel but has a strength that is more than ten times greater. Accordingly, carbon fiber is used as a high-strength structural material in various industrial fields such as aerospace, sports, automobiles, and bridges. As carbon fiber has begun to receive full attention as a next-generation material due to the rapid development and sophistication of the automotive and aerospace industries, demand is increasing, particularly in the automotive industry as it aims for eco-friendly, low-energy consumption future vehicles.
[0040] Generally, carbon fibers are manufactured through an oxidation / stabilization process in which heat is applied in an oxidizing atmosphere to infuse precursor fibers, thereby oxidizing and stabilizing them, and a carbonization process in which the oxidized / stabilized fibers are carbonized at high temperatures. A subsequent graphitization process may also be performed. At this time, precursor fibers for carbon fibers include polyacrylonitrile (PAN), pitch, rayon, lignin, and polyethylene. Among these, polyacrylonitrile (PAN) fibers are the optimal precursor for manufacturing high-performance carbon fibers compared to other precursors because they possess a high carbon yield of over 50% and a high melting point. Accordingly, most current carbon fibers are manufactured from polyacrylonitrile (PAN) fibers.
[0041] The carbon fiber mentioned above can be purchased commercially and used. Since the composition of the carbon fiber is a known technology, a detailed description thereof will be omitted for the sake of convenience of explanation and clarity of the technical concept of the present invention.
[0043] Next, a mixed yarn can be manufactured by mixing acrylic yarn with the carbon fiber.
[0044] For example, the above-mentioned mixed yarn can be manufactured by mixing acrylic yarn in a weight ratio of 5 to 15 parts by weight with respect to 100 parts by weight of the total carbon fiber content, and by mixing acrylic yarn with the carbon fiber, physical properties such as durability and heat resistance can be further improved.
[0045] The above acrylic yarn may be prepared from a copolymer of 85 to 95 wt% acrylonitrile, 6 to 10 wt% vinyl acetate, and 0.1 to 1.0 wt% sodium methacrylate sulfonate. Alternatively, the above acrylic yarn may be prepared from a copolymer comprising acrylonitrile, methyl or ethyl, methacrylic acid, and sulfonic acid, but is not limited thereto and may be prepared by various methods known in the art.
[0046] The above acrylic yarn may have high thermal shrinkage stress; for example, the acrylic yarn may have a thermal shrinkage stress of 0.1 to 0.3 g / d, a shrinkage rate of 20 to 30%, and a high thermal shrinkage rate of 30 to 40%. Additionally, the acrylic yarn has a thermal shrinkage stress of 250 to 350 kg / mm 2 It can have a Young's modulus of 35 to 45 g / d and a strength of 35 to 45 g / d.
[0048] Next, a coated mixed yarn can be manufactured by applying a coating solution composition to the above mixed yarn and then drying it.
[0049] That is, by applying a coating solution composition to the above-mentioned mixture and drying it to form a coating layer, physical properties such as insulation, antibacterial properties, and durability can be enhanced, and the coating solution composition comprises melamine resin, activated carbon, ceramic powder, a curing agent, and a solvent.
[0050] Specifically, the coating liquid composition may be included in a weight ratio of 100 to 200 parts by weight of melamine resin, 5 to 15 parts by weight of activated carbon, 1 to 10 parts by weight of ceramic powder, 40 to 60 parts by weight of curing agent, and 10 to 20 parts by weight of solvent.
[0051] The above melamine resin is a thermosetting resin produced by reacting melamine with formaldehyde, and the melamine resin can serve to strengthen the surface while improving adhesion, durability, strength, etc.
[0052] For example, the above melamine resin can be prepared by mixing a mixed solution in a weight ratio of 30 to 40 parts by weight of melamine, 20 to 40 parts by weight of formaldehyde, 15 to 25 parts by weight of water, 1 to 3 parts by weight of diethylene glycol, and 1 to 2 parts by weight of sodium hydroxide at a temperature of 38 to 42°C, adjusting the pH of the mixed solution to 7.8 to 8.2, polymerizing the mixed solution at a temperature of 93 to 97°C for 1 to 3 hours, cooling the polymerized reaction product to 30 to 35°C and adjusting the pH to 7.2 to 7.7, and then adding 3 to 7 parts by weight of (5-Ethyl-2-methyl-1,3,2-dioxaphosphorinan-5-yl)methyl dimethyl phosphonate P-oxide to 100 parts by weight of the cooled reaction product.
[0053] The above activated carbon is a carbon aggregate with developed micropores, which can change its internal surface area through an activation process, and has excellent properties of absorption and adsorption, such that adsorption with surrounding liquid or gas occurs through internal carbon atomic functional groups.
[0054] The above-mentioned activated carbon can adsorb and remove harmful substances or gases and absorb fine moisture. Additionally, the above-mentioned activated carbon can be used in powder form. This powder form not only enhances the adsorption capacity of the porous activated carbon itself, but also increases adhesion as the particles become denser due to the finer the powder, and can impart antioxidant and hydrophobic functions.
[0055] The above-mentioned activated carbon has a strong power to expel toxins from the body, and therefore exhibits excellent efficacy against various adult diseases, dermatitis, and allergic symptoms caused by the accumulation of toxins in the body; for example, the above-mentioned activated carbon has a hardness of 90 mass fraction% or more, a packing density of 0.47 to 0.55 g / ml, and a specific surface area of 1,050 to 1,150 m² 2 / g, the pore distribution may be used with a pore diameter of 3 Å to 10 Å, an iodine adsorption capacity of 1,000 mg / g or more, a pore volume of 0.5 to 0.6 ml / g, a pH of 10 to 11, a phenol adsorption capacity of 18 to 23 ml / g, and an M·B decolorization capacity of 150 to 200 ml / g.
[0056] The ceramic powder can be used as an inorganic filler, for example, the ceramic powder may be included in a weight ratio of 30 to 70 parts by weight of silicon dioxide (SiO2) and 5 to 15 parts by weight of alumina nanopowder.
[0057] Since the above silicon dioxide is easy to procure and reduces manufacturing costs while having excellent resistance to heat, it is possible to manufacture an economical and flame-retardant heating mattress pad.
[0058] The above alumina (Al2O3) is a white powder with a molecular weight of 101.96, a specific gravity of 3.965, and a melting point of 2072°C, and has a hexagonal crystal structure. Most alumina is manufactured through the Bayer process using bauxite minerals as raw materials, and due to its high heat resistance, chemical resistance, corrosion resistance, and high strength, it is widely used as a wear-resistant material, spark plug, insulator, abrasive refractory, ceramic tile, glass, cutting tool, biomaterial, catalyst carrier, filter, heat exchanger parts, refractory, resin filler, fiber, etc.
[0059] Generally, metals such as aluminum alloys, titanium alloys, and magnesium alloys naturally form a thin oxide film with high corrosion resistance due to their high reactivity with air in the atmosphere. However, since the naturally formed oxide film has limitations in terms of uniformity and corrosion resistance, anodizing surface treatment methods are widely used to artificially form an oxide film with greater uniformity and higher corrosion resistance.
[0060] Anodizing is a compound word of anode and oxidizing. The anodizing process can prevent rusting and improve appearance, wear resistance, heat resistance, and adhesion. The anodizing surface treatment method involves artificially creating an oxide film on the surface of metals such as aluminum alloys, titanium alloys, and magnesium alloys to protect the interior of the metal. Examples include the hydroxyl method and the sulfuric acid method.
[0061] The device used for such anodizing surface treatment immerses the metal to be treated in an electrolyte mainly containing sulfuric acid or sodium hydroxide, and when direct current is passed through the electrolyte as the cathode side and the metal to be treated as the anode side, an oxide film is formed on the surface of the metal to be treated.
[0062] For example, when a metal (part) is placed on the anode and electrolyzed in a diluted acid solution, an oxide film (aluminum oxide; Al2O3) with excellent adhesion to the base metal is formed by the oxygen generated at the anode. This differs from electroplating, where the part is placed on the cathode for plating. The most representative material for this anodizing process is aluminum (Al), but anodizing treatment is also performed on metal materials such as Mg, Zn, Ti, and Ta.
[0063] In the present invention, the alumina nanopowder may be an alumina nanopowder prepared through the following process.
[0064] In order to manufacture the above alumina nanopowder, first, aluminum can be processed to manufacture an aluminum plate.
[0065] That is, aluminum (Al) can be prepared and processed into a predetermined size and shape through mechanical processing to manufacture an aluminum plate. Since the aluminum (Al) naturally has an aluminum oxide layer formed on its surface to protect the inner surface, it has excellent corrosion resistance and excellent ductility, making it easy to form and machine.
[0066] For example, the above aluminum can be prepared and processed in the form of foil or sheet.
[0067] Next, the aluminum plate can be cleaned.
[0068] By washing the aluminum plate, impurities remaining on the aluminum plate can be removed. For example, the aluminum plate can be washed using a mixture of a surfactant and deionized water mixed in a weight ratio of 10:90.
[0069] The above surfactant can improve penetration power against impurities attached to the aluminum plate and improve cleaning efficiency. As the surfactant, one or more selected from the group consisting of glycerol, triethylene glycol, and polyethylene glycol can be used, and preferably, triethylene glycol can be used.
[0070] In addition, the above deionized water is water from which ions have been removed, and it is preferable to use deionized water with a resistivity of 18 MΩ·cm or higher.
[0071] Next, the cleaned aluminum plate can be subjected to an anodizing process to form an alumina (Al2O3) film.
[0072] For example, an alumina (Al2O3) film can be formed on the surface of the aluminum plate by connecting the cleaned aluminum plate to an anode, immersing it in an electrolyte, and then applying an electric field to anodize it. In the anodizing process, oxygen generated at the anode through an electrolysis reaction while the aluminum plate is immersed in an acidic electrolyte reacts with the surface of the aluminum plate to form an alumina oxide film.
[0073] In addition, the electrolyte may consist of 1 to 3 weight% sulfuric acid, 0.1 to 1.5 weight% amino acid, 10 to 20 weight% oxalic acid, 5 to 15 weight% citric acid, and the remainder being deionized water, and the electrolyte may maintain a temperature of 26 to 28°C and perform anodizing for 1 to 5 minutes under conditions of a constant current of 3.3A and a voltage of 14 to 18V.
[0074] Next, the alumina (Al2O3) film can be melted.
[0075] For example, the above melting can produce corundum-type (α-Al2O3) alumina by melting the alumina (Al2O3) film using an arc furnace, but the technical concept of the present invention is not limited to the arc furnace, and any furnace having an appropriate temperature capable of melting the alumina film can be used.
[0076] In addition, during the process of melting the above alumina (Al2O3) film in an arc furnace, oxides, sodium, iron, etc. are removed using an impurity removal agent, thereby producing corundum-type alumina free of impurities (e.g., 99.8% or more).
[0077] Next, the molten alumina (Al2O3) film solution is poured into a mold and cooled to produce an ingot, and the ingot is crushed and classified by size to produce alumina nanopowder.
[0078] For example, the above alumina nanopowder can be manufactured by pouring the molten alumina (Al2O3) coating liquid into a mold and cooling it to produce an ingot, and then finely grinding the ingot using a Raymond Mill and classifying it by size using a blower, etc. Since the composition of the grinding is a known technique, a specific description thereof will be omitted for the convenience of explanation and for the clarity of the technical concept of the present invention.
[0079] The above curing agent can play a role in promoting the curing of the coating liquid composition. For example, the above curing agent may be one or more selected from the group consisting of glycerin, p-toluenesulfonic acid monohydrate (PTSA), morpholine, ammonium chloride, ammonium sulfate, and phthalic anhydride.
[0080] The above solvent may be used to uniformly mix the coating solution composition and control the viscosity. For example, one or more solvents selected from the group consisting of isopropyl alcohol (IPA), ethanol, and methanol may be used.
[0082] Next, the above-mentioned coating mixture yarn can be carbonized to produce a carbon fiber weft yarn.
[0083] The carbon fiber weft yarn can be heated in a carbonization chamber maintained at 1,300 to 1,700°C, and gases such as nitrogen or hydrogen discharged during the carbonization process can be discharged by a vacuum pump. The carbonization can be carried out by winding the coating mixture yarn onto a roller and adjusting the tension of another roller to allow the coating mixture yarn to pass through the carbonization chamber.
[0084] Furthermore, the carbonization described above may be carried out in multiple stages, and a preliminary firing may be performed first based on the softening point of the coated mixed yarn. Since the configuration for manufacturing carbon fiber weft yarn by carbonizing the coated mixed yarn is a known technology, a detailed description thereof will be omitted for the sake of convenience of explanation and clarity of the technical concept of the present invention.
[0086] 2. Microwire gradient manufacturing step (S200)
[0087] The above microwire slope manufacturing step (S200) is a step of manufacturing a microwire slope formed including a microwire.
[0088] In the above microwire warp manufacturing step (S200), the microwire warp can be woven to intersect perpendicularly with the carbon fiber weft to form a heating fabric, and the microwire warp can generate heat by receiving power by including conductive microwires, and can be manufactured by the following method.
[0089] That is, in order to manufacture the above-mentioned microwire gradient, glass fibers can first be prepared.
[0090] The above glass fiber is made by melting and processing glass with silicate as the main component into a fiber shape, and is also called glass fiber or glass wool. The above glass fiber is not only excellent in terms of heat resistance, corrosion resistance, moisture resistance, thermal insulation, and sound absorption, but also has the characteristic that tensile strength and flexibility increase as the diameter of the glass fiber decreases. Therefore, it is widely used in a wide variety of industrial fields, such as raw materials for reinforced plastics, electrical insulation materials, separators for batteries, sound-absorbing (soundproofing) materials, thermal insulation materials, decorative fabrics, and filter materials.
[0092] Next, a microwire gradient can be manufactured by coating the glass fiber with a conductive material.
[0093] The above-mentioned microwire gradient can be manufactured by coating the glass fiber with a conductive material. Since the configuration for coating with the conductive material is a known technique, a detailed description thereof will be omitted for the sake of convenience of explanation and clarity of the technical concept of the present invention.
[0094] In the present invention, the conductive material is not particularly limited as long as it is one that can be generally used in the relevant technical field. For example, the conductive material may be a conductive polymer, a carbon nanostructure, a metal oxide, a metal nanowire, a metal nanoparticle, a carbon paste, a metal paste, or a combination thereof.
[0095] The conductive polymer may be polyethylenedioxythiophene (PEDOT), polystyrene sulfonate (PSS), polyaniline, polypyrrole, or a combination thereof, and the carbon nanostructure may be graphene, carbon nanotubes, carbon nanofibers, fullerene, carbon black, or a combination thereof. The metal oxide may be, for example, indium tin oxide, zinc tin oxide, indium gallium zinc oxide, zinc aluminum oxide, indium zinc oxide, zinc oxide, or a combination thereof, and the metal nanowire or metal nanoparticle may be a nanowire or nanoparticle of a metal selected from silver, gold, platinum, copper, nickel, aluminum, titanium, palladium, cobalt, cadmium, rhodium, or a combination thereof.
[0096] In addition, the carbon paste may be a mixture of graphene, carbon nanotubes, carbon nanofibers, fullerene, carbon black, or a combination thereof, in an organic binder, etc., and the metal paste may be a mixture of a metal including silver, gold, platinum, copper, nickel, aluminum, titanium, palladium, cobalt, cadmium, rhodium, or a combination thereof, in an organic binder, etc.
[0098] 3. Heating fabric manufacturing step (S300)
[0099] The above heating fabric manufacturing step (S300) is a step of manufacturing a heating fabric using the carbon fiber weft and fine wire warp.
[0100] In the above heating fabric manufacturing step (S300), the heating fabric can be manufactured by weaving the carbon fiber weft and fine wire warp in a cross shape in the horizontal and vertical directions. For example, in the above heating fabric manufacturing step (S300), the weaving of the carbon fiber weft and fine wire warp can be performed by arranging the carbon fiber weft and fine wire warp at equal intervals so as to be adjacent to each other, or by twisting and weaving the carbon fiber weft and fine wire warp.
[0101] In the above heating fabric manufacturing step (S300), the heating fabric is woven using carbon fiber weft and fine wire warp. Since this is a known technology in the relevant technical field, a detailed explanation thereof will be omitted for the sake of clarity and convenience.
[0103] 4. Fluororubber coating layer formation step (S400)
[0104] The above fluororubber coating layer formation step (S400) is a step of forming a fluororubber coating layer on the heating fabric.
[0105] In the above fluororubber coating layer formation step (S400), the fluororubber coating layer can be formed by applying a fluororubber coating composition to the heating fabric and then drying it, and the fluororubber (fluoro-elastomer) is a ternary copolymer polymer compound of monomers such as tetrafluoroethylene (TFE), perfluoromethylvinyl-ether (PFMVE), and CSM (Cure Site Monomer), and has the following structure.
[0106]
[0107] In other words, the above-mentioned fluororubber is a hydrocarbon polymer with a high degree of fluoridation. Generally, all polymers with a high degree of fluoridation are very stable and possess excellent resistance to many fluids, such as oxidation resistance, weather resistance, flame retardancy, and chemical resistance.
[0108] This stability is due to the high CF bond strength compared to CH bonds. The monomers that form this rubber are polyvinylidene fluoride (PVF) and hexafluoropropylene (HFP).
[0109] For example, in the fluororubber coating layer formation step (S400), the fluororubber coating composition comprises fluororubber, a rust inhibitor, a filler, a crosslinking agent, a vulcanizing agent, and a vulcanization accelerator.
[0110] Specifically, in the fluororubber coating layer forming step (S400), the fluororubber coating composition may be included in a weight ratio of 80 to 120 parts by weight of fluororubber, 1 to 5 parts by weight of rust inhibitor, 5 to 10 parts by weight of filler, 1 to 3 parts by weight of crosslinking agent, 2 to 4 parts by weight of vulcanizing agent, and 0.5 to 1.5 parts by weight of vulcanizing accelerator.
[0112] The above-mentioned fluororubber is a known material with excellent physical properties such as heat resistance and oil resistance, and is mainly used in automobile, ship, and aircraft engine systems. In the present invention, the above-mentioned fluororubber is not specifically limited, and various known types of fluororubber can be applied.
[0113] For example, one or more selected from the group consisting of vinylidenefluoride (VF), hexafluoropropylene (HFP), tetrafluoroethylene (TFE), and perfluoromethylvinylether (PMVE) may be used as the fluororubber.
[0114] Preferably, the fluororubber may be selected from the group consisting of a binary copolymer of vinylidene fluoride (VF) and hexafluoropropylene (HFP); a ternary copolymer of vinylidene fluoride (VF), tetrafluoroethylene (TFE), and perfluoromethylvinyl ether (PMVE); a ternary copolymer of vinylidene fluoride (VF), hexafluoropropylene (HFP), and tetrafluoroethylene (TFE); and combinations thereof.
[0116] The above-mentioned rust inhibitor can prevent the deterioration of the physical properties of the heat-generating fabric due to moisture and optimize the corrosion prevention effect, and the rust inhibitor includes zinc, aluminum, dicyclohexyl ammonium carbamate, cellulose, trimethoxyvinylsilane, and arabic gum.
[0117] Specifically, the rust inhibitor may be included in a weight ratio of 20 to 30 parts by weight of zinc, 10 to 20 parts by weight of aluminum, 5 to 15 parts by weight of dicyclohexyl ammonium carbamate, 1 to 10 parts by weight of cellulose, 1 to 5 parts by weight of trimethoxyvinylsilane, and 5 to 15 parts by weight of arabic gum.
[0118] The above zinc and aluminum are included in the rust inhibitor and perform a corrosion prevention role, and can exhibit excellent rust prevention performance.
[0119] The above dicyclohexyl ammonium carbamate can be used as a rust-preventing material, sodium carboxymethyl cellulose can be used as the cellulose, and the above trimethoxyvinylsilane can be used as an inorganic binder.
[0121] The above filler may be added to reinforce hardness and mechanical properties, etc. For example, the above filler includes illite powder, volcanic scoria powder, seashell powder and bamboo charcoal powder.
[0122] Specifically, the filler may be included in a weight ratio of 1 to 5 parts by weight of illite powder, 3 to 7 parts by weight of volcanic scoria powder, 2 to 4 parts by weight of seashell powder, and 1 to 3 parts by weight of bamboo charcoal powder.
[0123] The above illite powder can be manufactured by crushing illite into powder. Illite is a representative natural clay mineral defined as a porous mica mineral. It has a thin, sheel-like structure with flexibility and elasticity, possessing superior elasticity and adsorption properties compared to other minerals.
[0124] The main components of the above illite mineral include silicon oxide (SiO2) 57.5%, which removes waste and fruit sebum from pores; aluminum oxide (Al2O3) 23.3%, which promotes blood circulation; iron oxide (Fe2O3) 6.76%, which acts as a collagen binder; calcium oxide (C2O) 0.1%, which acts as a detoxifier and suppresses and relieves stress; sodium oxide (Na2O) 1.21%, which provides osmotic pressure regulation and moisture regulation functions; magnesium oxide (MgO) 0.38%; potassium oxide (K2O) 6.43%; and titanium dioxide (TiO2), MnO, Li, Cr, Zn, Sr, etc. 4.32%.
[0125] In addition, the main functions of the above illite include adsorbing suspended solids in water, and because it carries an anion, it causes aggregation and precipitation through electrical neutralization with positively charged suspended fine particles, thereby providing water purification functions and excellent adsorption / decomposition capabilities for specific radioactive materials, adsorbing, deodorizing, and decomposing various heavy metals and toxic gases in water, soil, and air, activating cells, enhancing immunity, emitting a large amount of dissolved oxygen in water, activating water molecules, generating a large amount of anions from the illite itself, emitting 93% far-infrared rays at 40℃, bacteriostatic action against viruses, bacteria, and fungi, adsorbing and decomposing various heavy metals, organic substances, and toxic substances on the skin, and having excellent adhesion because it has good elasticity and does not clump.
[0127] The above volcanic scoria powder is manufactured by crushing and pulverizing volcanic scoria. Since the volcanic scoria (or Jeju Island scoria, volcanic ash) is a porous material, it not only has excellent efficacy in adsorbing harmful substances in water or the atmosphere, but also performs the function of neutralizing metallic toxic energy and organic toxic energy among the energies radiated from the volcanic scoria.
[0128] Furthermore, the aforementioned volcanic scoria is an eco-friendly raw material that possesses a far-infrared effect, which stimulates molecular motion to activate human cells and promote blood circulation and metabolism, and exhibits excellent blocking effects against heavy metals and electromagnetic waves. Additionally, the volcanic scoria has excellent functions in inhibiting the growth of various molds and the habitation of pathogens and bacteria, thereby possessing antifungal and antibacterial effects, and is highly effective in removing odors such as ammonia, formaldehyde, and organic compounds.
[0130] The above-mentioned shell powder can be manufactured by crushing shells. Generally, a shell is an inorganic secretory material formed by mollusks that surrounds and protects the body. Depending on the type of shellfish, such as abalone, oyster, clam, and scallop shells, when crushed, these shells exhibit a very beautiful and diverse texture and color. Furthermore, due to their biochemically composed porous calcium components, they possess significant thermal insulation performance and the ability to adsorb airborne pollutants through respiration with the surrounding air, making them known as hygienic and eco-friendly materials.
[0131] The above shell powder may be calcined shell fine powder prepared by the following method.
[0132] First, in order to manufacture the above shell powder, shells can be prepared.
[0133] For example, the above shell may be one or more shells selected from the group consisting of abalone shells, oyster shells, conch shells, clam shells, and scallop shells.
[0134] Next, the above shell can be washed.
[0135] The washing of the above shell can be performed by immersing the shell in a washing solution at a temperature of 20 to 30°C for 5 to 15 minutes, wherein the washing solution comprises 1 to 3 weight% of a thiourea compound, 3 to 5 weight% of hydrogen peroxide, 2 to 4 weight% of sodium citrate, 0.1 to 0.3 weight% of a chelating agent, and the remainder being deionized water.
[0136] The above thiourea compound may be included to ensure that the washing solution remains stable when washing shells, and the above thiourea compound may include thiourea (NH2)2CS or a thiourea derivative represented by the general formula (R1R2N)(R3R4N)C=S (where R1, R2, R3, and R4 are each independently selected from a hydrogen atom, an ethyl group, or a methyl group).
[0137] The above hydrogen peroxide is a substance used as an oxidizing agent, and the above hydrogen peroxide can play a role in enabling cleaning to be performed easily.
[0138] The above sodium citrate may be included to enhance the deodorizing effect on shells and increase stability.
[0139] The above chelating agent may be added to prevent a decrease in the cleaning ability of the cleaning solution and to prevent foreign substances or metal ions from being re-adsorbed through chemical bonding. For example, as the above chelating agent, diethylene trinitrilopentaacetic acid (DTPA) and glutamic acid-2-acetic acid may be mixed in a weight ratio of 1:1 and used.
[0140] The above deionized water is water from which ions have been removed, and it is preferable to use deionized water with a resistivity of 18 MΩ·cm or higher.
[0141] Next, the washed shells can be crushed to produce shell aggregate powder.
[0142] The above-mentioned shell granulation powder can be produced by crushing the washed shells using a known granulator, such as a pan granulator, a drum granulator, or a compression pelletizer, but is not necessarily limited to the aforementioned granulators.
[0143] Next, the above shell aggregate powder can be heated in a kiln to produce calcined shell aggregate powder.
[0144] The above-mentioned calcined shell aggregate powder can be manufactured by introducing the above-mentioned shell aggregate powder into a calcination furnace and heating it at a temperature of 1,100 to 1,300°C for 20 to 60 minutes. By heating the above-mentioned shell aggregate powder to produce the calcined shell aggregate powder, contaminants adsorbed in the fine pores of the above-mentioned shell aggregate powder can be removed by thermal oxidation through heating and the shell aggregate powder can be activated.
[0145] As the above-mentioned shell aggregate powder undergoes calcination, the calcium carbonate constituting the above-mentioned shell aggregate powder can be decomposed into calcium oxide and carbon dioxide as follows.
[0146] Calcium carbonate (CaCO3) → Calcium oxide (CaO) + Carbon dioxide (CO2)
[0147] Next, calcined shell fine powder can be produced by grinding the calcined shell aggregate powder.
[0148] The above-mentioned calcined shell fine powder can be produced by grinding the above-mentioned calcined shell granular powder using a ball mill or various known grinders, and the grinding can be performed so that the particle size of the above-mentioned calcined shell fine powder is 1 to 100 μm.
[0149] As the configuration of grinding using a ball mill or the like when manufacturing the above-mentioned calcined shell fine powder is a known technique, a detailed description thereof will be omitted for the convenience of explanation and to clarify the technical concept of the present invention.
[0151] The above bamboo charcoal powder can be manufactured by crushing and pulverizing bamboo charcoal, and the bamboo charcoal has about twice as much inorganic matter content as ordinary charcoal, and in particular, it is used as a deodorizer because it contains a larger amount of silica, which is the main component of silica gel used as an adsorbent, than ordinary charcoal.
[0152] In addition, the above bamboo charcoal softens tap water and is used as a bath additive as it is recognized for its disinfecting effect due to the generation of trace amounts of chloride ions. Furthermore, high-temperature charcoal has a very high far-infrared radiation rate, is recognized for its electromagnetic shielding effect, and has an anion generation effect, so it can be applied to health products.
[0153] Since the above bamboo charcoal is produced by high-temperature treatment of bamboo material at 400°C or higher, it remains sterile for a certain period after production, and contains only a very small amount of inorganic matter, and since about 60% of the inorganic matter consists of alkaline components such as calcium and potassium, strong alkalinity is exhibited.
[0154] In addition, the above bamboo charcoal is a porous body with a large surface area and has a very low organic matter content, so even if microorganisms that cause decay invade the bamboo charcoal, they cannot multiply, and in some cases, the multiplication of microorganisms that prefer acidity is inhibited due to the alkalinity of the bamboo charcoal.
[0156] The above crosslinking agent may have a function that influences crosslinking during the vulcanization of the fluororubber coating composition; for example, trialallyl isocyanurate (Taic) may be used as the crosslinking agent.
[0158] One or more of the above vulcanizing agents selected from the group consisting of cyclohexanone peroxide, t-butylperoxyisopropylcarbonate, t-butylperoxylaurylate, t-butylperoxyacetate, di-t-butyldiperoxyphthalate, t-dibutylperoxymaleic acid, t-butylcumyl peroxide, t-butyl hydroperoxide, dibenzoyl peroxide, and dicumyl peroxide may be used.
[0160] The above vulcanization accelerator can enable rapid vulcanization; for example, BTPPC (Benzyltriphenylphosphonium) can be used as the vulcanization accelerator.
[0162] 5. Surface coating step (S500)
[0163] The above surface coating step (S500) is a step of forming a surface coating layer on the heating fabric on which the fluororubber coating layer is formed.
[0164] In the above surface coating step (S500), a surface coating liquid composition is applied to the surface of the heating fabric on which the fluororubber coating layer is formed, and then dried to form a surface coating layer, thereby strengthening the physical properties of the heating mattress, such as durability and flame retardancy. In the above surface coating step (S500), the surface coating liquid composition can be prepared by mixing and dispersing an additive and a solvent in a thermosetting resin.
[0165] For example, in the surface coating step (S500), the surface coating liquid composition can be prepared by mixing 10 to 30 parts by weight of an additive with respect to 100 parts by weight of the total content of the thermosetting resin to prepare a mixture, and adding 10 to 30 parts by weight of a solvent to the mixture to disperse and mix it.
[0166] The above thermosetting resin can harden upon fire to exhibit excellent non-combustible or flame-retardant performance; for example, melamine resin may be used as the above thermosetting resin.
[0167] The above melamine resin is a thermosetting resin produced by reacting melamine with formaldehyde, and the melamine resin can serve to strengthen the surface while improving adhesion, durability, strength, etc.
[0168] For example, the above melamine resin can be prepared by mixing a mixed solution in a weight ratio of 30 to 40 parts by weight of melamine, 20 to 40 parts by weight of formaldehyde, 15 to 25 parts by weight of water, 1 to 3 parts by weight of diethylene glycol, and 1 to 2 parts by weight of sodium hydroxide at a temperature of 38 to 42°C, adjusting the pH of the mixed solution to 7.8 to 8.2, polymerizing the mixed solution at a temperature of 93 to 97°C for 1 to 3 hours, cooling the polymerized reaction product to 30 to 35°C and adjusting the pH to 7.2 to 7.7, and then adding 3 to 7 parts by weight of (5-Ethyl-2-methyl-1,3,2-dioxaphosphorinan-5-yl)methyl dimethyl phosphonate P-oxide to 100 parts by weight of the cooled reaction product.
[0170] The above additives may be used to enhance physical properties such as durability and flame retardancy. For example, the additives may be used by mixing expanded graphite powder, a flame retardant, graphene, nanoceramic particles, and titanium dioxide nanoparticles.
[0171] Specifically, the additive may be included in a weight ratio of 80 to 120 parts by weight of expanded graphite powder, 60 to 80 parts by weight of flame retardant, 1 to 10 parts by weight of graphene, 1 to 10 parts by weight of nanoceramic particles, and 1 to 10 parts by weight of titanium dioxide nanoparticles.
[0173] The above expanded graphite powder is obtained by pulverizing expanded graphite. Generally, graphite is a mineral in which planar macromolecules, consisting of six-membered rings of carbon atoms connected infinitely in a planar manner, are stacked in layers. Its properties include being a good conductor of electricity, being flexible and smooth due to the layered structure of polycene, and having the characteristics of being easy to cleave but having low reactivity because it is a macromolecule.
[0174] However, since the carbon planes of the polycene structure of graphite are connected only by van der Waals forces, the spacing between carbon atoms is 35.5 nm, which is wider than the 14.2 nm gap between carbon atoms, so it is possible to form interlayer compounds by inserting other atoms into the gaps between the layers. In other words, interlayer compounds are formed by inserting many atoms, molecules, or ions into the gaps between the planes while maintaining the network plane of the graphite crystal.
[0175] That is, when an interlayer compound or residual compound, in which an acid such as sulfuric acid is applied between layers of graphite, is rapidly heated to a temperature close to 1000°C, the acid vaporizes and gas is generated, and the interlayers of graphite expand by tens to hundreds of times due to the expansion pressure of the gas, and this is called expanded graphite.
[0177] The above flame retardant may be used by mixing an organic flame retardant and an inorganic flame retardant in a weight ratio of 1:1, wherein a phosphorus-based flame retardant is used as the organic flame retardant, and the phosphorus-based flame retardant may be one or more selected from the group consisting of red, ammonium phosphate, and ammonium polyphosphate.
[0178] The phosphorus-based flame retardant reacts with a combustible material during the combustion process to form a carbonaceous layer on the surface of the polymer, and this carbonaceous layer blocks the oxygen required for combustion, thereby exhibiting a flame-retardant effect. Specifically, the phosphorus-based flame retardant generates phosphoric acid and polyphosphoric acid through thermal decomposition; the phosphoric acid and polyphosphoric acid generated at this time produce char through esterification and dehydration reactions, and the char exhibits a flame-retardant effect by blocking oxygen and heat. In addition, radicals such as HPO2 and PO are generated by the decomposition of phosphoric acid, which play a role in stabilizing the active radicals OH· and H·.
[0179] The above inorganic flame retardant may be a mixture of aluminum hydroxide and antimony trioxide in a weight ratio of 1:1. The aluminum hydroxide is a filler used to prevent oxidation and corrosion, and when mixed with antimony trioxide, it can be used to increase the oxygen index more significantly than when using the organic flame retardant alone, and to increase heat resistance to enhance the flame retardant effect.
[0181] The aforementioned graphene is the most superior material among existing substances in terms of various characteristics, such as strength, thermal conductivity, electron mobility, deodorizing properties, and antibacterial properties. Accordingly, it is applied in diverse fields including displays, secondary batteries, solar cells, automobiles, and lighting, and is recognized as a strategic core material that drives the growth of related industries; as a result, technologies for the commercialization of graphene are receiving significant attention.
[0182] In other words, graphene consists of carbon atoms sp 2 Graphene is a carbon allotrope with a two-dimensional structure that forms a hexagonal honeycomb lattice structure through hybridization, and the thickness of a single layer of graphene is 0.2 to 0.3 nm, which is the thickness of one carbon atom. Because graphene has high electrical conductivity and a specific surface area, it is used in various fields such as supercapacitors, sensors, batteries, electrodes (electrode active materials) for actuators, touch panels, flexible displays, high-efficiency solar cells, heat dissipation films, coating materials, seawater desalination filters, electrodes for secondary batteries, and ultra-fast chargers.
[0184] The above nanoceramic particles can improve physical properties such as wear resistance and scratch resistance. For example, the nanoceramic particles used have an average particle size of 500 to 1,500 nm, and one or more selected from the group consisting of silicon carbide, alumina, and silica may be used.
[0186] The titanium dioxide nanoparticles mentioned above can be used as a UV blocking material and can have a particle size of 10 to 1000 nm.
[0187] The above titanium dioxide has high UV absorption and good infrared reflection, so it has a blocking effect not only on UV rays but also on infrared rays. It blocks UV rays by scattering them, and it has the advantage of not causing side effects on the skin and not being decomposed by UV rays, and it is widely used as a photocatalyst for decomposing organic matter.
[0189] The above solvent may be included to uniformly mix materials such as expanded graphite powder and flame retardants, for example, one or more selected from the group consisting of methanol, ethanol, and formaldehyde may be used as the solvent.
[0191] In a method for manufacturing a heating mattress pad according to one embodiment of the technical concept of the present invention, a heating element (10) is manufactured using a heating fabric having a surface coating layer formed thereon, and a heating mattress pad can be manufactured using the heating element (10).
[0192] That is, the heating element (10) includes a pair of metal electrodes (20), a carbon fiber weft (30), a fine wire warp (40), and an external power line (50), and the heating element (10) may include other components in addition.
[0193] The above external power line (50) is connected to a pair of metal electrodes (20) to supply power to the heating element (10), and the pair of metal electrodes (20) are extended in the x-axis direction. The pair of metal electrodes (20) may be manufactured from a material such as copper or nickel. The metal electrodes (20) may be manufactured in the form of a thin film or a rod. The pair of metal electrodes (20) are spaced apart from each other and receive power by being connected to an external power source through the external power line (50).
[0194] Additionally, the microwire slope (40) is extended in the y-axis direction, which is a direction that intersects the direction in which the metal electrodes (20) are extended, and the microwire slope (40) can generate heat by connecting the pair of metal electrodes (20) to receive power from the pair of metal electrodes (20).
[0195] In addition, the microwire warp (40) supplied with power from the metal electrodes (20) is connected in direct contact with the carbon fiber weft (30) formed of a conductive material, so that not only the microwire warp (40) but also the carbon fiber weft (30) can generate heat.
[0196] The carbon fiber weft (30) and the fine wire warp (40) can be woven together by crossing each other. Since the carbon fiber weft (30) and the fine wire warp (40) are woven by crossing each other, their strength is high, so they can withstand strong external forces.
[0197] The carbon fiber weft (30) and the fine wire warp (40) can each be manufactured using an Oxford weaving method in which two strands are crossed, or a taffeta weaving method in which a grid pattern is woven. Since the configuration of manufacturing a heating element using a heating fabric with a surface coating layer formed thereon and manufacturing a heating mattress pad using the heating element is a known technology, a detailed description thereof will be omitted for the convenience of explanation and to clarify the technical concept of the present invention.
[0199] Although a preferred embodiment of the present invention has been described above with reference to the attached drawings, those skilled in the art will understand that the present invention may be implemented in other specific forms without altering its technical concept or essential features. Therefore, the embodiment described above should be understood as illustrative in all respects and not restrictive. Explanation of the symbols
[0201] 10; heating element 20; metal electrodes 30; carbon fiber weft 40; Microwire gradient 50; external power cord
Claims
Claim 1 A carbon fiber weft manufacturing step (S100) for manufacturing a carbon fiber weft formed including carbon fibers; a microwire warp manufacturing step (S200) for manufacturing a microwire warp formed including microwires; a heating fabric manufacturing step (S300) for manufacturing a heating fabric using the carbon fiber weft and microwire warp; and a fluororubber coating layer forming step (S400) for forming a fluororubber coating layer on the heating fabric. The method includes a surface coating step (S500) for forming a surface coating layer on a heating fabric having a fluororubber coating layer formed thereon, wherein in the microwire gradient manufacturing step (S200), the microwire gradient is manufactured by preparing glass fibers and coating the glass fibers with a conductive material, wherein the conductive material is a conductive polymer, a carbon nanostructure, a metal oxide, a metal nanowire, a metal nanoparticle, a carbon paste, a metal paste, or a combination thereof, and in the fluororubber coating layer formation step (S400), the fluororubber coating layer is formed by applying a fluororubber coating composition to the heating fabric and then drying it, wherein the fluororubber is a binary copolymer of vinylidene fluoride (VF) and hexafluoropropylene (HFP); or a ternary copolymer of vinylidene fluoride (VF), tetrafluoroethylene (TFE), and perfluoromethylvinyl ether (PMVE). A method for manufacturing a heating mattress pad, wherein the fluororubber coating composition comprises a ternary copolymer of vinylidene fluoride (VF), hexafluoropropylene (HFP), and tetrafluoroethylene (TFE); and a combination thereof, wherein in the fluororubber coating layer forming step (S400), the fluororubber coating composition comprises fluororubber, a rust inhibitor, a filler, a crosslinking agent, a vulcanizing agent, and a vulcanization accelerator, wherein the fluororubber coating composition comprises 80 to 120 parts by weight of fluororubber, 1 to 5 parts by weight of a rust inhibitor, 5 to 10 parts by weight of a filler, 1 to 3 parts by weight of a crosslinking agent, 2 to 4 parts by weight of a vulcanizing agent, and 0.5 to 1.5 parts by weight of a vulcanization accelerator. Claim 2 delete Claim 3 delete Claim 4 delete Claim 5 A method for manufacturing a heating mattress pad according to claim 1, wherein in the fluororubber coating layer forming step (S400), the filler comprises illite powder, volcanic scoria powder, seashell powder, and bamboo charcoal powder, wherein the filler is included in a weight ratio of 1 to 5 parts by weight of illite powder, 3 to 7 parts by weight of volcanic scoria powder, 2 to 4 parts by weight of seashell powder, and 1 to 3 parts by weight of bamboo charcoal powder. Claim 6 A method for manufacturing a heating mattress pad according to claim 5, wherein in the surface coating step (S500), the surface coating layer is formed by applying a surface coating liquid composition to the surface of a heating fabric formed on the fluororubber coating layer and then drying it, and the surface coating liquid composition is prepared by mixing 10 to 30 parts by weight of an additive with respect to 100 parts by weight of a total thermosetting resin to prepare a mixture, and adding 10 to 30 parts by weight of a solvent to the mixture to disperse and mix, wherein melamine resin is used as the thermosetting resin, and the additive is included in a weight ratio of 80 to 120 parts by weight of expanded graphite powder, 60 to 80 parts by weight of a flame retardant, 1 to 10 parts by weight of graphene, 1 to 10 parts by weight of nanoceramic particles, and 1 to 10 parts by weight of titanium dioxide nanoparticles.
Citation Information
Patent Citations
Making method of electric heat seat for mat having aheat and negative electric potential
KR1020030019491A
Geogrid heater
KR1020120038952A
Plate type heater with-excellent flexibilty and durability
KR1020130012992A