Forming apparatus and method for forging molten material by vertical multi pressure type
The vertical multi-stage pressure forging apparatus and method improve forging quality and efficiency by using a multi-stage pressurization process with controlled ejection and atmosphere maintenance, addressing challenges in large and complex products.
Patent Information
- Application Number
- KR1020230128851
- Authority / Receiving Office
- KR · KR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-09-26
- Publication Date
- 2026-11-06
- Estimated Expiration
- 2043-09-26
AI Technical Summary
Existing molten metal pressure forging methods face challenges in achieving satisfactory forging formability and quality, especially for large and complex-shaped products, due to issues like oxide incorporation and difficulty in maintaining a closed atmosphere during the forging process.
A vertical multi-stage pressure forging apparatus and method utilizing a workbench, lower and upper molds, temperature control, and an ejection unit, along with a multi-stage pressurization process to improve forging quality and efficiency, including heating, lubrication, and controlled ejection of molten metal.
Enhances precision and quality of forging, particularly for large and complex products, by maintaining a closed atmosphere and reducing oxide incorporation through multi-stage pressurization and controlled ejection, ensuring operational stability and durability.
Smart Images

Figure 112023106670908-PAT00001_ABST
Abstract
Description
Technology Field
[0001] The present invention relates to a vertical multi-stage pressure molten metal forging molding apparatus and a vertical multi-stage pressure molten metal forging molding method. Background Technology
[0002] Generally, various metal products or parts can be manufactured using a molten metal pressure forging method, in addition to the machining (cutting) process, in which molten metal is injected and filled into the mold and then formed by pressure forging.
[0003] In particular, the molten metal pressure forging method is known to be suitable for manufacturing aluminum-based metal products or parts (e.g., AL1000, AL2000, AL3000).
[0004] However, due to the nature of the molten metal pressure forging process, which involves pressurizing the molten metal using pressure, it is difficult to expect satisfactory forging formability when manufacturing products that are large and require complex shapes or precision on the upper and lower surfaces, unlike small products.
[0005] Furthermore, due to the nature of the operation, oxide incorporation caused by contact with air can frequently occur while the molten metal is injected and filled into the mold, and this becomes a major factor that significantly degrades the quality of pressure forging.
[0006] Therefore, in order to ensure forming quality and operational reliability by the molten metal pressure forging method, a work method or device structure capable of improving the aforementioned problems is required. Prior art literature
[0007] (Patent Document 0001) Registered Patent Publication No. 10-1169360. The problem to be solved
[0008] The present invention has been devised to solve the aforementioned problems, and
[0009] The objective of the present invention is to provide a vertical multi-stage pressure molten metal forging apparatus and a vertical multi-stage pressure molten metal forging method that can further improve the pressure forging quality and work efficiency of not only small products but especially large products. means of solving the problem
[0010] In order to achieve the above-mentioned purpose,
[0011] A workbench equipped with a driving source for applying pressure for multi-stage pressure forging;
[0012] A lower mold for forging placed on the above workbench;
[0013] An upper mold for forging formed to enable joining and pressure forging operations in a vertical direction toward the lower mold for forging side;
[0014] A temperature control unit for heating and cooling the lower mold for forging and the upper mold for forging; and
[0015] An ejection part formed on the side of the upper mold for forging or the lower mold for forging, and equipped with an ejection pinhole and an ejection pin for inducing the ejection of a forged product by pressing contact;
[0016] A vertical multi-stage pressurized molten metal forging molding device including
[0017] And, in order to achieve other objectives of the present invention,
[0018] Heating process for forging molds;
[0019] Lubrication process for forging molds;
[0020] Molding molten metal injection process;
[0021] Multistage pressure forging process;
[0022] Cooling process for forging molds;
[0023] Mold release process for forging; and
[0024] Forging process for ejection of molded parts;
[0025] A vertical multi-stage pressurized molten metal forging method including Effects of the invention
[0026] The present invention, by injecting and filling molten metal for molding into the forging mold and performing forging using a pressure forging method, and by carrying out the forging operation using a multi-stage pressure method between the upper and lower forging molds, can be expected to have the effect of further improving the precision and quality of the forging. Brief explanation of the drawing
[0027] FIG. 1 is a schematic diagram showing the overall structure of a vertical multi-stage pressurized molten metal forging molding apparatus according to one embodiment of the present invention. FIG. 2 is a schematic process diagram showing the overall work process of a vertical multi-stage pressurized molten metal forging molding method according to one embodiment of the present invention. FIGS. 3 to 8 are drawings for explaining in detail each of the work processes of FIG. 2. Specific details for implementing the invention
[0028] Hereinafter, preferred embodiments of the present invention will be described with reference to the attached drawings.
[0029] Embodiments of the present invention are described within the scope in which those with average knowledge in the art can practice the present invention. Accordingly, since embodiments of the present invention can be modified in various different forms, the scope of the claims of the present invention is not limited to the embodiments described below.
[0030] FIG. 1 is a schematic diagram showing the overall structure of a vertical multi-stage pressurized molten metal forging molding apparatus according to one embodiment of the present invention, FIG. 2 is a schematic diagram showing the overall work process of a vertical multi-stage pressurized molten metal forging molding method according to one embodiment of the present invention, and FIG. 3 to 8 are drawings for explaining each work process of FIG. 2 in detail.
[0031] First, a preferred structure of a vertical multi-stage pressurized molten metal forging molding apparatus according to one embodiment of the present invention will be described with reference to FIG. 1.
[0032] A vertical multi-stage pressurized molten metal forging molding device includes a workbench (10), a lower mold for forging (20), an upper mold for forging (30), a temperature control unit (40), and an extraction unit (50).
[0033] The workbench (10) is provided with a work surface (12) on its upper side, and the work surface (12) is formed to provide a flat work area suitable for pressure forging and forming processes.
[0034] It is preferable that the workbench (10) be made of a structure and material that has resistance to loads, pressures, shocks, and vibrations that occur during pressure forging operations.
[0035] A pressurizing drive source (14) that generates power for multi-stage pressurizing forging is positioned on the side of the work table (10), and among devices that generate power in a straight forward and backward direction, for example, a hydraulic press can be used as the pressurizing drive source (14).
[0036] The lower mold (20) and the upper mold (30) for forging are provided with cavities (22, 32) for forming a cavity through a joining operation, and are installed on a workbench (10) in a state compatible with vertical forging molding.
[0037] That is, the lower mold (20) for forging is positioned on the work surface (12) of the work table (10) as in FIG. 1 with the cavity (22) side facing upward, and the upper mold (30) for forging can be set up on the upper part of the lower mold (20) for forging with the cavity (32) side facing downward.
[0038] The lower mold (20) and the upper mold (30) for forging can be installed on the workbench (10) side while fixed by their respective clamp devices (A, B).
[0039] For example, the lower mold (20) for forging is installed as a fixed mold type on the working surface (12) side of the work table (10), and the upper mold (30) for forging is fixed by a clamp device (B) but can be installed as an movable mold type that moves up and down toward the lower mold (20) side to enable joining and pressure forging operations.
[0040] The upper mold (30) for forging can be set to perform upper and lower forging operations by driving a driving source (14) for pressure.
[0041] Although the pressurizing drive source (14) is not shown in the drawing, it can be set to control the multi-stage pressurizing operation of the upper mold (30) for forging, for example, by operating a separate controller.
[0042] Additionally, the lower mold (20) and the upper mold (30) for forging may be formed to have a blocking part (C1, C2) to secure a contact gap blocking force (closing force) between the molds during the joining and pressing operations.
[0043] As shown in FIG. 1, the blocking portions (C1, C2) are formed to have a structure that allows for securing a blocking area through contact by being inserted separably into male and female shapes on the perimeter side of the lower mold (20) and the upper mold (30) for forging.
[0044] The blocking portions (C1, C2) can be formed in a stepped shape that can be separated from each other, for example, in a male and female form.
[0045] These blocking parts (C1, C2) can increase the blocking force on the contact gap side between the molds during a pressure forging operation between the lower mold (20) and the upper mold (30), thereby inducing the formation of a closed atmosphere inside the mold in a state consistent with ensuring the stability of the pressure forging operation. In particular, as shown in FIGS. 5 and 6, the blocking parts (C1, C2) are formed integrally on the periphery side of the lower mold (20) and the upper mold (30) for forging, and are formed to have an integrated multi-stage blocking structure that secures an expanded blocking area by being inserted separably into each other in the form of two or more male and female steps. Compared to a blocking structure based on simple contact, the formation of a closed atmosphere is made easier due to the expanded blocking area in the form of steps, and a blocking structure consistent with the improvement of forging quality by multi-stage pressure can be realized by suppressing the outflow of the molten metal (M) for molding.
[0046] And, molten metal (M) for molding is injected and filled into the lower mold (20) side for forging, and the injection of molten metal (M) for molding can be carried out in various ways that correspond to the working conditions or environment.
[0047] For example, the molten metal (M) for molding can be injected using a separate injector (D) of the distributor type while the lower mold (20) and the upper mold (30) for forging are separated from each other, as shown in FIG. 1.
[0048] The injector (D) can be formed to receive and inject molten metal (M) for molding from a separate molten metal supply unit (T) in a conventional manner, and at this time, it is preferable that the molten metal (M) for molding be set to be supplied in a degassed state.
[0049] The injector (D), although not shown in the drawing, can be formed to be operable and operable so as to be positioned at an injection or waiting point while being moved, for example, by a robot arm or rail device.
[0050] In addition to the distributor type described above, the injector (D) may also use various types of tools or devices for injecting molten metal.
[0051] The temperature control unit (40) is formed to have a structure capable of heating and cooling the lower mold (20) and the upper mold (30) for forging.
[0052] The temperature control unit (40) is provided with control channels (42a, 42b) formed on the side of the lower mold (20) and the upper mold (30) for forging as shown in FIG. 1, and the control channels (42a, 42b) are each formed on the mold side in a state that forms a channel section corresponding to the heating or cooling treatment of the lower mold (20) and the upper mold (30) for forging.
[0053] The control channels (42a, 42b) are formed in a channel section on the inner side of the lower mold (20) and the upper mold (30) for forging, and are formed to form a section capable of inducing heat conduction for uniform heating or cooling treatment of the entire surface of the cavity (22, 32) of each mold (20, 30).
[0054] The control channels (42a, 42b) are not shown in the drawing, but can be formed to form zigzag-shaped channel sections extending to correspond to the entire area of the cavity (22, 32) inside each mold (20, 30), for example.
[0055] And, the control pipes (42a, 42b) are formed so as to induce heating or cooling treatment of the mold through heat exchange action by a heating fluid (W1) or a cooling fluid (W2), and these fluids (W1, W2) can be set to be circulated and supplied along the pipe sections by, for example, pumping by a pump (not shown).
[0056] This temperature control unit (40) can induce heat conduction by circulating and supplying a control fluid along the pipe sections of the control pipes (42a, 42b), thereby allowing each mold (20, 30) to be heated or cooled. In particular, as shown in FIG. 3, the control pipes (42a, 42b) are formed to form embedded pipe sections corresponding to the entire surface of the cavities (22, 32) of each mold (20, 30) inside the lower mold (20) and the upper mold (30) for forging, thereby enabling a temperature control structure that can more uniformly and easily induce heating or cooling on the side of the cavities (22, 32) of each mold (20, 30) according to the temperature control conditions required during the forging process.
[0057] The extraction unit (50) is formed to have a structure that allows the product to be ejected from the mold after pressure forging treatment.
[0058] The extraction part (50) may be selectively formed on the lower mold (20) or the upper mold (30) side depending on the pressure forging conditions, and in this embodiment, it is described as being formed on the upper mold (30) side as an example.
[0059] That is, the extraction unit (50) may be formed by having an extraction pin hole (52) formed inside the upper mold (30) for forging as in FIG. 1, and an extraction pin (54) arranged to enable a pressing action for extraction on the side of the pin hole (52).
[0060] The extraction pinhole (52) is formed in the shape of a hole that penetrates vertically from the upper surface side of the upper mold (30) for forging toward the cavity (32) side, and a plurality of them may be formed at spaced intervals on the inner side of the perimeter of the cavity (32).
[0061] A plurality of extraction pins (54) can be set up such that one end is inserted into the extraction pin hole (52) and can be pressed along the hole toward the cavity (32) of the upper mold (30) for forging.
[0062] The extraction pin (54) can be set so that a pressing action for inducing extraction is performed, in which it moves in the upward and downward directions through the extraction pin hole (52) in conjunction with the upward and downward driving of the push plate (56) and protrudes toward the cavity (32) of the upper mold (30) for forging.
[0063] The extraction pin hole (52) is formed to allow for the upward and downward movement of the extraction pin (52), and in particular, it can be formed to have a hole shape that allows for smooth exhaust (air, gas) treatment within the cavity (22, 32) during pressure forging.
[0064] That is, the extraction pinhole (52) is formed to penetrate the cavity (32) side from the upper surface side of the upper mold (30) for forging as in FIG. 1, and can be formed to have a guide groove (52a) at the lower end of the hole portion.
[0065] The guide groove (52a) can be formed to have a groove shape (e.g., an inverted pyramid) that extends from top to bottom and gradually increases in the size of the groove's circumference. Therefore, the guide groove (52a) can guide residual air (gas) in the cavity (22, 32) to be more smoothly exhausted to the outside through the extraction pinholes (52) during the pressure forging operation between the lower mold (20) and the upper mold (30) for forging. In particular, the guide groove (52a) is formed at the lower end of the pinhole in the form of an inverted triangular pyramid groove that is in communication with the side of the extraction pinhole (52) as shown in FIGS. 1 and 7, so that when multi-stage pressurization is performed, the exhaust direction of the remaining air (gas) in the cavity (22, 32) is guided toward the pinhole side toward the inner inclined surface of the guide groove (52a), thereby allowing the exhaust process to be carried out more smoothly through the extraction pinhole (52).
[0066] This extraction unit (50) can facilitate the separation and extraction of a molded product from the cavity (32) side of the upper mold (30) for forging by pressing the extraction pin (54) after the pressure forging process.
[0067] A vertical multi-stage pressurized molten metal forging device according to one embodiment of the present invention can provide a device structure that corresponds to each of the work processes of a vertical multi-stage pressurized molten metal forging method according to one embodiment of the present invention described below.
[0068] Next, a preferred working process of a vertical multi-stage pressurized molten metal forging method according to an embodiment of the present invention will be described with reference to FIGS. 2 to 8.
[0069] Referring to FIG. 2, a vertical multi-stage pressure molten metal forging method according to one embodiment of the present invention comprises a forging mold heating process (S1), a forging mold lubrication process (S2), a molding molten metal injection process (S3), a multi-stage pressure forging process (S4), a forging mold cooling process (S5), a forging mold release process (S6), and a forging molded product removal process (S7).
[0070] The heating process (S1) for the forging mold involves heating the lower mold (20) and the upper mold (30) for the forging, which are arranged facing each other in a vertical direction on the workbench (10) as shown in FIG. 3, to a state suitable for pressure forging operations.
[0071] That is, the heating process is carried out by supplying and circulating a heating fluid (W1) to the control channel (42) of the temperature control unit (40) formed inside the lower mold (20) and the upper mold (30) for forging.
[0072] Then, the lower mold (20) and the upper mold (30) for forging can each be heated by inducing heating through heat exchange action by the circulation of the heating fluid (W1), and the heating temperature can be set within the range of approximately 370 to 420 degrees Celsius.
[0073] Next, the forging mold lubrication process (S2) is performed.
[0074] The forging mold lubrication process (S2) is to lubricate the cavity (22, 32) side of the mold (20, 30) to increase the precision of forging and to facilitate the removal of the product after forging.
[0075] That is, the lubrication process can be carried out by spraying a lubricant (W3) onto the inner surface of the cavities (22, 32) of the lower mold (20) and the upper mold (30) for forging using a sprayer (E) as shown in FIG. 3.
[0076] The lubricant (W3) can be selected from among metal lubricants, and for example, if the molten metal (M) for molding described later is aluminum, it can be selected from among aluminum lubricants that are compatible with it.
[0077] The lubricant (W3) can be sprayed in a manner that adjusts the spray amount and spray angle, etc., to match the gradient and shape of the forged product and the temperature of the mold.
[0078] In addition, after spraying the lubricant (W3), it is desirable to perform post-treatment so that the lubricated surface is uniformly distributed, for example, by an air blow method. Then, the quality of pressure forging and ease of ejection can be further improved through uniform lubrication treatment.
[0079] In addition to the spraying method using a sprayer (E) as described above, the lubrication process may also be carried out by, for example, applying a lubricant (W3).
[0080] Next, the molten metal injection process for molding (S3) is carried out.
[0081] The molding molten metal injection process (S3) involves injecting and filling the molding molten metal (M) into the mold side in a state consistent with the pressure forging process.
[0082] In particular, the molten metal injection process (S3) for molding is carried out by injecting and supplying the molten metal (M) for molding in a manner that does not cause interference with the mold side.
[0083] The injection process can be carried out by injecting the molten metal (M) for molding into the cavity (22) of the lower mold (20) through the space between the lower mold (20) and the upper mold (30) for molding, as shown in FIG. 4, using an injector (D).
[0084] At this time, the molten metal (M) for molding is supplied to the injection device (D) in a degassed state using a conventional method.
[0085] Then, the degassed molten metal (M) for molding can be injected and filled into the cavity (22) side of the lower mold (20) for forging in a state consistent with the pressure forging process through an injection operation using an injector (D).
[0086] Next, a multi-stage pressure forging process (S4) is performed.
[0087] The multi-stage pressure forging process (S4) pressure-forges the molten metal (M) injected and filled into the lower mold (20) for forging, and specifically proceeds by pressurizing the forging process using a multi-stage pressure operation.
[0088] Referring to FIG. 2, the multi-stage pressure forging process (S4) includes a mold joining step (S4-1), a first pressure step (S4-2), and a second pressure step (S4-3), and each of these work steps proceeds by moving the upper mold (30) side for forging in a vertical direction by driving a pressure driving source (14).
[0089] That is, the joining step (S4-1) is to join the lower mold (20) for forging and the upper mold (30) for forging together so that the molten metal (M) filled in the lower mold (20) for forging can be closed.
[0090] As shown in FIG. 5, the molding process proceeds by lowering the upper mold (30) for forging toward the lower mold (20) for forging into which the molten metal (M) for forging is injected and filled, so that the cavities (22, 32) of the two molds (20, 30) form a single molding space (cavity).
[0091] Then, the inner cavity (22, 32) is closed off from the outside by the joining of the two molds (20, 30), and as a result, the air contact of the molten metal (M) filled inside can be blocked.
[0092] The first pressurization step (S4-2) is performed by pressurizing the cavity (22, 32) closed by the joining of the lower mold (20) and the upper mold (30) for forging so that exhaust (air, gas) can be processed.
[0093] That is, the first pressurization operation is performed by a fine downward movement of the upper mold (30) for forging so that the upper surface of the molten metal (M) on the side of the lower mold (20) for forging can be finely pressed when the two molds (20, 30) are joined together as shown in FIG. 6.
[0094] Then, by the fine pressure operation of the upper mold (30) for forging, the molten metal (M) for molding and the remaining air (gas) in the cavity (22, 32) can be exhausted to the outside through the gap of the extraction pinhole (52) of the extraction part (50).
[0095] The upper mold (30) for forging can be set to perform a fine pressure operation for approximately 3 to 6 seconds, and in particular, during the fine pressure operation, the molten metal (M) for molding inside the cavity (22, 32) is not leaked out through the gap between the molds (20, 30) and the operation is carried out.
[0096] The second pressurization step (S4-3) is performed by secondarily pressurizing the molten metal (M) for molding into the upper mold (30) in the first pressurization state.
[0097] In particular, the second pressurization step (S4-3) is to pressurize the molten metal (M) for molding in conjunction with the first pressurization operation so that it is forged into a final near-net shape corresponding to the cavity (22, 32) side of the lower mold (20) and the upper mold (30) for forging.
[0098] That is, the second pressurization process is carried out by first pressurizing the molten metal (M) for molding by two molds (20, 30) and then secondarily pressurizing it by the final pressurization action by lowering the upper mold (30) for forging as shown in FIG. 7.
[0099] The upper mold (30) for forging can be set to perform a secondary pressurization operation for approximately 2 to 5 minutes, and the secondary pressurization operation enables the forging of the molten metal (M) for molding into a final near net shape, and also enables additional exhaust treatment of residual air (gas).
[0100] In this way, if the lower mold (20) and the upper mold (30) for forging are joined together to form a closed atmosphere, and the pressure forging operation is carried out in two stages, the pressure forging can be performed in a state that more smoothly induces the exhaust of residual air (gas) in the cavity (22, 32).
[0101] Therefore, the problem of reduced forging quality caused by residual air (gas) in the cavity (22, 32) during pressure forging treatment of the molten metal (M) for molding can be improved.
[0102] In particular, if the forging process is carried out in a state where the exhaust of residual air (gas) is smoothly induced by a multi-stage pressurization method, satisfactory forming quality can be secured not only for small products but also for large products where forming precision is required on opposing surfaces.
[0103] Furthermore, compared to a method of pressure forging forming with, for example, a single pressure operation, the multi-stage pressure forging method described above can reduce physical stress (pressure, load, shock, and vibration) transmitted to the device, thereby enabling the realization of a working environment that is compatible with ensuring the operational stability and durability of the device.
[0104] Next, the forging mold cooling process (S5) is carried out.
[0105] The forging mold cooling process (S5) is to cool the lower mold (20) and the upper mold (30) to a state consistent with the molten metal forging molding process after multi-stage pressure forging treatment.
[0106] The forging mold cooling process (S5) is carried out by cooling the mold side by the temperature control unit (40) while the lower mold (20) and the upper mold (30) for forging are joined and multi-stage pressed together as shown in FIG. 7.
[0107] That is, the cooling process is carried out by supplying and circulating a cooling fluid (W2) to the control channel (42) of the temperature control unit (40) formed inside the two molds (20, 30).
[0108] Then, the lower mold (20) and the upper mold (30) for forging can each be cooled by inducing cooling through heat exchange action by the circulation of the cooling fluid (W2), and the cooling temperature can be set within the range of approximately 270 to 300 degrees Celsius.
[0109] As described above, by proceeding with the cooling process after multi-stage pressurization, the cooling of the hot water (M) for molding is performed in a state consistent with the improvement of molding precision (quality) by multi-stage pressurized forging treatment, and as a result, the molding of the forged product (F) can be performed in a state having a final shape.
[0110] Next, the mold release process (S6) for forging is performed.
[0111] The mold separation process (S6) for forging separates the lower mold (20) and the upper mold (30) for forging from each other so that the forged product (F) can be ejected after cooling treatment.
[0112] That is, the molding process is carried out by lifting the upper mold (30) side for forging upward with a pressurizing drive source (14) as shown in FIG. 8 so that the two molds (20, 30) are separated from each other.
[0113] Then, the two cavity sides (22, 32) are opened by the separation of the lower mold (20) and the upper mold (30) for forging, and as a result, the forged product (F) can be ejected.
[0114] At this time, the forged product (F) is maintained in a state where it adheres to the cavity (32) side of the upper mold (30) for forging as shown in FIG. 8, and in this state, it can be ejected to the outside of the mold (30) through an ejection operation.
[0115] Next, the forging process (S7) is performed.
[0116] The process of removing the molded product for forging (S7) is carried out by using the removal unit (50) to separate and remove the molded product (F) from the mold (30) in a molded state.
[0117] That is, the extraction operation is carried out in a manner such that, after the release operation of the upper mold (30) for forging as shown in FIG. 8, the forging product (F) attached to the cavity (32) side of the mold (30) is pushed by the pressing operation of the extraction pin (54) of the extraction unit (50) by advancing to induce separation from the cavity (32).
[0118] At this time, a collection platform (F) is positioned between the lower mold (20) for forging and the upper mold (30) for forging, so that the forged product (F) separated and extracted from the upper mold (30) for forging can be collected and processed while placed on the collection platform (G).
[0119] And, although not shown in the drawing, the collected forged product (F) is subjected to a normal deburring operation, for example, to remove residues from the outer surface, thereby completing the manufacture of the forged product (F) by multi-stage pressure forging.
[0120] Accordingly, the present invention provides a device and method that can further improve the quality of forging of products, including small products, as well as large products that require high forming precision on opposing surfaces, by pressurizing and forging a molten metal (M) using a lower mold (20) and an upper mold (30) for forging while going through the above-mentioned work processes, and by performing the forging process in a vertical multi-stage pressurizing method consisting of a joining mold, first pressurization, and second pressurization. Explanation of the symbols
[0121] 10: Workbench 20: Lower formwork for forging 30: Upper mold for forging 40: Temperature control unit 50: Ejection section M: Molten metal for molding F: Forged product
Claims
Claim 1 A workbench having a driving source for pressurizing for multi-stage pressurizing forging; a lower forging mold disposed on the workbench and having a cavity for forging; an upper forging mold disposed vertically toward the lower forging mold side to enable joining and pressurizing forging operations and having a cavity for forging; and a temperature control unit for heating and cooling the lower forging mold and the upper forging mold. and an ejection unit formed on the side of the upper mold for forging or the lower mold for forging, and equipped with an ejection pinhole and an ejection pin for inducing the ejection of a forged product by pressing contact; wherein the temperature control unit is provided with a control channel formed by being embedded in the inner side of the lower mold for forging and the upper mold for forging, in a state that forms a channel section corresponding to the cavity side, respectively, and is formed to induce heating or cooling of the cavity side by a heating fluid or a cooling fluid circulating along the control channel; wherein the lower mold for forging and the upper mold for forging are provided with a blocking unit for forming a closed atmosphere within the mold, and the blocking unit is formed integrally on the periphery side of the mold, and is formed to have an integrated multi-stage blocking structure that secures an expanded blocking area in a state where it is separably fitted into each other in the form of two or more male and female steps; and the ejection unit is in conjunction with a multi-stage pressurization operation between the lower mold for forging and the upper mold for forging A vertical multi-stage pressurized molten metal forging device characterized by being formed so that residual air in the cavity is exhausted through the extraction pinhole, wherein an inverted triangular pyramidal guide groove is formed on the lower end of the hole portion of the extraction pinhole in communication with the pinhole, and the exhaust is formed so that the exhaust direction is guided toward the pinhole by the inner inclined surface of the guide groove. Claim 2 A vertical multi-stage pressure molten metal forging molding apparatus according to claim 1, wherein the upper mold for forging is positioned above the lower mold for forging on the workbench and is set to enable joining and pressing operations in a vertical direction toward the lower mold for forging by the pressurizing driving source. Claim 3 delete Claim 4 delete Claim 5 A vertical multi-stage pressure molten metal forging method using a vertical multi-stage pressure molten metal forging device of claim 1, comprising: a forging mold heating process; a forging mold lubrication process; a molding molten metal injection process; a multi-stage pressure forging process; a forging mold cooling process; a forging mold removal process; and a forging product removal process. Claim 6 A vertical multi-stage pressurized molten metal forging method according to claim 5, wherein the forging mold lubrication process is characterized by lubricating the cavity sides of the lower forging mold and the upper forging mold with a lubricant while they are separated from each other. Claim 7 In claim 5, the molten metal injection process for forming is a vertical multi-stage pressurized molten metal forging method in which molten metal for forming is injected and filled into the lower mold side through the space between the lower mold and the upper mold for forging while the lower mold and the upper mold for forging are separated from each other. Claim 8 In claim 5, the multi-stage pressure forging process comprises a mold joining step, a first pressure step, and a second pressure step, wherein the mold joining step involves lowering the upper mold for forging toward the side of the lower mold for forging into which the molding molten metal is injected and filled to perform a joining process so that the cavities of the two molds are closed, the first pressure step involves applying pressure by finely pressing the upper surface of the molding molten metal on the side of the lower mold for forging with a fine downward movement of the upper mold for forging while the lower mold for forging and the upper mold for forging are joined together, and the second pressure step involves applying pressure by lowering the upper mold for forging so that the molding molten metal in the first-stage pressured state forms a final semi-shaped form, thereby forming a vertical multi-stage pressure molten metal forging method. Claim 9 A vertical multi-stage pressurized molten metal forging method according to claim 8, wherein the first pressurizing step is characterized by pressurizing in a state that induces exhaust within the cavity by a fine pressurizing operation.
Citation Information
Patent Citations
Molten metal forging apparatus and molten metal forging method
JP2005305466A
Mold apparatus to form metal in high vacuum environment
KR101483717B1
Rheo-forming method
KR1020080004295A
Multistage press type casting and forging mold unit using press apparatus and method of the same