Production of rechargeable sodium sulfur (Na-S) batteries containing composite S / Ru / RuxOy / ZrOz@C cathode active material.

A composite cathode material for Na-S batteries, using S/Ru/RuO/ZrO@C, addresses conductivity and stability issues by enhancing electron transfer and adsorbing polysulfides, enabling stable operation at room temperature with high capacitance and long cycle life.

TR202522661A3Pending Publication Date: 2026-10-21INONU UNIVERSITESI REKTORLUGU
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
TR202522661
Authority / Receiving Office
TR · TR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-12-30
Publication Date
2026-10-21

AI Technical Summary

Technical Problem

Current sodium-sulfur (Na-S) batteries face issues with low electrical conductivity, polysulfide shuttle effect, and structural instability, leading to poor electron transfer, ion transport, and rapid capacity drop, which hinder their practical application at room temperature.

Method used

Development of a composite cathode active material comprising S/Ru/RuO/ZrO@C, synthesized through a process involving microfiber cellulose, metal-organic frameworks, and ruthenium doping, which enhances electron conductivity and adsorbs polysulfides, thereby stabilizing the electrode structure.

Benefits of technology

The composite cathode material achieves high electrical conductivity, minimizes the polysulfide shuttle effect, and ensures long cycle life with high specific capacitance and Coulombic efficiency, suitable for commercial use at room temperature.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the synthesis of advanced composite cathode reactives with S / Ru / RuxOy / ZrOz@C (0<x ≥ 3, 0<y ≥ 4, 1 ≥ z ≥ 2) formulations in sodium sulfur (Na-S) batteries, the fabrication of room temperature sodium sulfur batteries using cathode electrodes constructed from these reactives, and the investigation of the electrochemical performance of these batteries. This invention focuses on the production of sodium sulfur batteries containing a sodium anode electrode against a cathode electrode made from S / Ru / RuxOy / ZrOz@C (0<x ≥ 3, 0<y ≥ 4, 1 ≥ z ≥ 2) cathode reactive materials, and a membrane and electrolyte between the two electrodes.
Need to check novelty before this filing date? Find Prior Art

Description

Rechargeable sodium sulfur containing composite S / Ru / RuxOy / ZrOz@C cathode active material. Production of (Na-S) batteries TECHNICAL FIELD The invention features high electrochemical capacitance and approximately 10,000 (ten thousand) charge / discharge cycles. High performance, high stability, and inexpensive operation at room temperature. For the production of sodium sulfur (Na-S) batteries, 80 units of S / Ru / Ru O / ZrO @C (0< x ≤ 3, 0< xyz Composite cathodes of different compositions with the general formulation (y ≤ 4, 1 ≤ z ≤ 2). It deals with the production of electrode reactives and cathode electrodes produced from these reactives. STATE OF THE ART Today, sodium-sulfur (Na-S) batteries operate at room temperature. Elemental sulfur and sulfur-carbon are predominantly used as cathodic reactive agents in these technologies. composites, porous carbon structures, and metal / heteroatom-doped sulfur hosts. These approaches are used because of the high theoretical potential of sulfur. Although it aims to benefit from it, sodium-sulfur batteries that operate at room temperature are impractical. Significant technical limitations exist in these applications. These mentioned... The following technical problems are observed in the applications: - First, sulfur and sodium sulfide derivative intermediates (Na₂Sₓ 4 ≤ x ≤ 8) Low electrical conductivity leads to insufficient electron transfer to the cathode electrode. opening and poor rate of ion transport, especially at high current densities. It demonstrates this performance. Therefore, only carbon is used in such batteries. The use of essentially conductive matrices is often not sufficient. - The second and most critical problem is the soluble sodium formed during discharge-charge. formed by the transition of polysulfide (Na₂Sₓ, 4 ≤ x ≤ 8) species to the electrolyte phase This is the "shuttle or cycling" effect. The shuttle effect leads to active sulfur loss, low sulfur content. Coulombic efficiency, rapid capacity drop, and cathode in long cycles. causing the chemical and physical structure of the electrode to become unstable. This is the case. Carbon-based or currently used as cathode electrode active materials. Host structures with weak polar surfaces support these polysulfide species (Na₂Sₓ, 4 ≤ x ≤ 8). 2 It is not holding on strong enough. This is the "shuttle effect". This is what causes it to emerge. - Thirdly, many metal-organic frameworks or Metal organic framework (MOF) and MOF-derived cathode materials, high Despite having a specific surface area, they have insufficient electrical conductivity. limited catalytic activity and structural integrity after carbonization They exhibit disadvantages such as degradation. Furthermore, MOFs alone... Their use is expensive and they are often mechanically fragile. This negatively affects the long-term cycle stability of the electrodes. - Finally, some studies use cathode-active species with metal or metal oxide dops. The aim was to accelerate the polysulfide conversion kinetics (shuttle effect). (although attempts have been made to minimize its impact) these approaches generally involve metal / metal non-homogeneous distribution of oxide types, agglomeration, active phase problems such as dissolution in the electrolyte or poor contact with the conductive network Therefore, it is unable to sustainably deliver the desired performance. Sodium sulfide batteries, which can operate at room temperature, have a high capacity due to the high sulfur content. Despite its potential, the polysulfide shuttle effect cannot be effectively suppressed, leading to redox reactions. slow conversion kinetics and electrodes over long cycles Limiting disadvantages such as the inability to ensure structural / electrochemical stability. These are the fundamental technical problems that arise in current applications. These problems, room The biggest obstacle to widespread and commercial applications of Na-S batteries operating at high temperatures This constitutes significant obstacles. Document JPH1025531A, encountered under the known state of the art, refers to sodium- Cathode electrode housing (slot) material made of cobalt-based alloy for sulfur batteries. This document is related to high strength Na-S batteries and Na and S. Positive corrosion resistance, made of Co-based alloy. The aim was to provide electrode casing material. To achieve this, Na-S The positive electrode casing material for the battery should be 15-30% Cr and 5-30% Ni by weight. 10-20% W, 0.1-5% Fe, 0.2-2% Mn, 0.01-0.3% C, and the remaining more than 35% Co. containing unavoidable impurities and, if necessary, may also contain 0.01-0.2% La. It has been stated that it consists of a Co-based alloy. 3 Document number US12482814B2 describes electrode materials and their production and... It relates to the methods of use. According to the summary of this document; electrode material, each one of which is approximately 100-400 nm in diameter and consists of a nucleus and an inner core. It consists of numerous nanoparticles forming a shell. The shell contributes to the total mass. according to this, approximately 70-90% carbon and approximately 5-20% nitrogen respectively. It contains approximately 40-97% sulfur by mass. It contains. The nucleus constitutes approximately 50% of the total mass of each nanoparticle. It contains 90% mass. The solutions developed in the documents mentioned above, in the current technology It has not been able to provide solutions to the problems mentioned. As a result, improvements are being made to the electrode structures of Na-S batteries, therefore It will eliminate the disadvantages mentioned above and provide solutions to existing systems. New structures are needed to bring about this. THE PURPOSE OF THE INVENTION The present invention eliminates or overcomes the disadvantages identified for Na-S batteries. The production of cathode electrode reactives by minimizing and offering some additional advantages. the electrochemical performance of Na-S batteries created with these cathode-active species and It is related to examining their determination. Therefore, the aim of the invention is to create a shuttle effect in Na-S batteries that can operate at room temperature. by eliminating or minimizing existing disadvantages, especially At room temperature, with a current density of 5°C A / g (1°C: 1675 mA / g), at least 5000-10000 at the end of the cycle, in the range of 400-800 mAh / g (depending on the composition of the cathode active material) (measured lowest and highest capacitance) capacitance values, high electrical low-cost cathode reactives with conductivity for commercial uses and this The goal is to synthesize Na-S batteries from active ingredients. To this general purpose, the following inventions serve the general purpose of the invention: The objectives / sub-objectives are listed. 4 The aim of the invention is to strongly cathode sodium polysulfides (Na₂S₄, 4 ≤ x ≤ 8). 2 x The goal is to synthesize cathode electrode reactives that can adsorb active substances into the electrode. Another aim / goal of the invention is; accelerated conversion kinetics of cathode electrode. The goal is to synthesize its active ingredients. Another aim / goal of the invention is to produce inexpensive and sustainable microfiber derived from cellulose. three-dimensional, self-supporting carbon network cathode electrode reactives It is to synthesize. Another aim / objective of the invention is to have a high sulfur loading capacity and especially The goal is to synthesize cathode electrode reactives with long-cycle stability. All the disadvantages mentioned above and which will be understood from the detailed explanation below The existing invention to eliminate; S / Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ xyz Synthesis of advanced cathode electrode materials with a formulation of z ≤ 2) and discusses its use as a cathode electrode. The structural and characteristic features and all the advantages of the invention are detailed below. This will be understood more clearly thanks to the explanation. Therefore, the evaluation will also be clearer. This should be done taking this detailed explanation into account. DETAILED EXPLANATION OF THE INVENTION This detailed description outlines the preferred configurations of the cathode reagents that are the subject of this invention. purely for the purpose of better understanding the subject and without any limiting influence. It is explained in a way that will not create a problem. The invention relates to composite cathode electrode actives for Na-S batteries; • Benzene-1,3,5-tricarboxylic acid (BTC) or 4,4′-biphenyldicarboxylic acid Microfiber cellulose (MFC) with a mass 1-5 times that of (BPDC) ligands. dispersion of its structure in a suspension medium, • 1 mmol benzene-1,3,5-tricarboxylic acid (BTC) or 4,4′-biphenyldicarboxylic In MFC surface induction was achieved using 3 mmol of zirconium precursors with BPDC acid. in situ form of Zr cluster unit metal-organic lattice (MOF) structures 6 creation, • 1–10% depending on the total metal content in the MFC and MOF structures in question by adding ruthenium (Ru) in the range (by mass or atomic percentage) Obtaining Ru@MOF@MFC structures, • Ru-added Ru@MOF@MFC structures in an inert atmosphere (N, Ar or Ar / H) 2 2 MFCs are carbonized at temperatures in the range of 600–900 °C. a derived fibrous carbon transport network with varying ratios of Ru / RuO and ZrO xyzz predominantly different microporous carbons containing polar centers based on polar cores has a matrix and Ru / Ru O / ZrO@C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) xyz Formulation of composite cathode active structures, • obtained Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) composite xyz By loading sulfur into their structures S / Ru / Ru O / ZrO @C ((0< x ≤ 3, 0< y ≤ 4, xyz Synthesis of cathode reactive agents (1 ≤ z ≤ 2) It involves applying the steps in the correct order. The invention describes a method in which microfiber cellulose (MFC) is first mixed with an aqueous or alcohol-based solution. It is dispersed in the medium. This process takes 0.5-3 hours at room temperature, 300-1000 It consists of mixing at rpm and ultrasonic dispersion stages for 10-30 minutes. The resulting fibrous structure is the growth of metal-organic lattice (MOF) crystals. It serves as a mechanical support and guiding framework. Then benzene- to 1,3,5-tricarboxylic acid (BTC) or 4,4′-biphenyldicarboxylic acid (BPDC) ligands 4+ individual zirconium (Zr) precursors (ZrCl, ZrOCl .8H O or Zr(IV)-oxocumelets) 4 2 2 By adding them, Zr-containing MOF structures with Zr units are formed on cellulose fibers. 6 This approach allows MOF particles to be transferred to the MFC surface. Thanks to the functional -OH groups, it adheres homogeneously and is MOF Maximum agglomeration of particles is prevented, ensuring a wide network. A certain amount of MOF (host) is created (MOF@MFC). In this process, BTC is primarily used. or the BPDC ligand is dissolved in a separate container. Zr(IV) precursor (ZrCl₄ or ZrOCl₂·8H₂O or Zr(IV)-oxoclumes) will be added to form Zr₆ unit nodes (points) The reaction medium is prepared. These solutions are added separately to the MFC suspension. This allows for the in-situ formation of Zr-MOF on the MFC surface, thus creating MOF@MFC. he structures are obtained. The temperature applied in the process is 120°C, the reaction time is 24 hours, and The mixing speed is 800 rpm. 6 The resulting MOF@MFC composite structures were treated with 1–10% Zr₆ content, depending on the total Zr₆ content. Ruthenium (Ru) is added during this period. Ru is synthesized using a metal salt (RuCl). 3 or incorporated into the system in the form of Ru(acac)); Zr-O node in MOF pores. 3 High dispersion in regions near the points or on the surface of MOF crystals and They are homogeneously distributed. Thus, Na-S works at room temperature. Polysulfides formed during charging / discharging due to the presence of Ru in the cathode active ingredient of batteries Active substances that catalyze the adsorption and redox conversion of (Na₂S₄, 4 ≤ x ≤ 8). 2 x It enables the formation of centers. The process of obtaining Ru@MOF@MFC is 20- he It is carried out at a temperature of 50°C and over a period of 1-12 hours. Ru-doped MOF@MFC structure (Ru@MOF@MFC), inert atmosphere (N or Ar or 2 under Ar / H gas mixture at different temperatures in the range of 600–900 °C 2 (Applicable temperatures of 600 / 700 / 800 / 900 °C) are used for carbonization. Different temperatures. Since the microstructures of the structures obtained by applying this method will be different, different pore structures will be required. Different types of materials are obtained. During this process: - MOF structure, Zr-based metal / metal oxide (ZrO , 1≤ z ≤ 2) nanocenters z carbon matrix containing micro-, micro-meso and / or meso-pores It is transforming. - Cellulose fibers, on the other hand, are highly conductive, fibrous, and contain defects (structural irregularities). It transforms into a carbon network containing. - Ru types, nanoparticle metallic Ru (Ru NP) and / or Ru / Ru O (0< x ≤ 3, 0< xy (y ≤ 4) is fixed to the carbon skeleton in the form of similar catalytic phases. The resulting structures exhibit hierarchical porosity (micro- / meso) and continuous electron flow. It offers transmission pathways. In this process step; temperature 600–900 °C, duration 1-3 hours and The heating rate is 1-10 °C / min. 40%- It is loaded with 70% sulfur. The porous carbon matrix ensures the homogeneous distribution of sulfur. While facilitating its distribution, Zr-based polar centers and Ru catalytic sites, sodium By strongly binding polysulfides, the biggest problem in Na-S batteries is... the shuttle effect which causes instability and low cycle life or service life It minimizes or eliminates it. In this process step; solution diffusion 7 temperature 120-180 °C (above the melting point of sulfur), time 5-12 hours and N₂ or Ar It is a closed environment containing gases (to reduce oxidation). The resulting S / Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) composite structures, xyz Chamber in the form of cathode electrode together with binding and conductive dopants. It is used as a cathode active material in Na-S batteries operating at high temperatures. This composite Cathode electrode actives; high specific capacitance, low polarization, long cycle life. and has high Coulombic Efficiency (CE) performance.

Claims

1. Composite cathode electrode material for room temperature operating Na-S batteries. Its characteristic is; • Benzene-1,3,5-tricarboxylic acid (BTC) or 4,4′-biphenyldicarboxylic acid The structure of microfiber cellulose (MFC) is 1-5 times the mass of (BPDC). dispersion in a suspension medium, • 1 mmol benzene-1,3,5-tricarboxylic acid (BTC) or 4,4′- 3 mmol zirconium precursors with biphenyldicarboxylic acid (BPDC) Zr cluster unit metal- by using in-situ formation on the MFC surface. 6 Formation of organic frame (MOF) structures, • 1–10% of the total metal content in the MFC and MOF structures in question. by adding ruthenium (Ru) in the range (by mass or atomic percentage) Obtaining Ru@MOF@MFC structures, • Ru-added Ru@MOF@MFC structures in an inert atmosphere (N, Ar or 2 Carbonized at temperatures in the range of 600–900 °C under Ar / H ) 2 by being combined with an MFC-derived fibrous carbon delivery network in different ratios Predominantly different microstructures containing Ru / RuO and ZrO-based polar centers. xyz having a porous carbon matrix and Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, xyz Formulation of composite cathode reagents with 1≤ z ≤ 2) • obtained Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) composite xyz by loading sulfur into their structures S / Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ xyz 4, 1≤ z ≤ 2) Formation of cathode reactive agents • S / Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) 80% of cathode actives, xyz prepared with 10% binder polymer and 10% conductive carbon. The cathode electrode is obtained by spreading the mixture onto aluminum foil. Na-S electrolyte with 1 M electrolyte and sodium metal used as the anode electrode creation of batteries, It includes the steps involved in the process.

2. Composite cathode electrode material conforming to Claim 1, with the characteristic of being MOF. Zirconium precursors ZrCl or used in the formation of structures 4 ZrOCl .8H O or Zr(IV)-oxocumelets. 2 2 9 3. Composite cathode electrode material conforming to Claim 1, with the following characteristics: Loaded onto Ru / Ru O / ZrO @C (0< x ≤ 3, 0< y ≤ 4, 1≤ z ≤ 2) composite structures xyz The sulfur content should be in the range of 40–70% of the total cathode mass.