Manufacturing method of badminton racket grip

TWI945526BActive Publication Date: 2026-11-11张益煌
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
TW113116679
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-05-06
Publication Date
2026-11-11
Estimated Expiration
2044-05-05

AI Technical Summary

Technical Problem

Existing badminton racket grips made from single materials suffer from discomfort due to lack of shock absorption, poor durability, and limited hitting performance, and traditional injection molding processes are constrained by holding pressure time, center misalignment, and poor yield.

Method used

A manufacturing method using a micro-foaming injection molding process (MuCell) to create a badminton racket grip with an inner core and outer shell made of different materials, such as carbon fiber and nano-nylon 6 or its composite, through a micro-foaming two-color injection molding machine, eliminating the need for holding pressure and reducing cooling time.

Benefits of technology

The method produces a lightweight, durable racket grip with improved structural strength and shock absorption, enhancing comfort and hitting performance while significantly reducing production time and material waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure TWG2TB001920271_001
    Figure TWG2TB001920271_001
  • Figure TWG2TB001920271_002
    Figure TWG2TB001920271_002
  • Figure TWG2TB001920271_003
    Figure TWG2TB001920271_003
Patent Text Reader

Abstract

This invention proposes a method for manufacturing a badminton racket grip, which involves preparing a main body, a front sleeve, and a rear end cap, and assembling the main body, front sleeve, and rear end cap into a badminton racket grip. The main body is manufactured using a micro-foaming injection molding process (MuCell). The main body includes an inner core formed using a first material via the MuCell process, and an outer shell formed using a second material via the MuCell process on the outside of the inner core, thus forming an integrated structure with the inner core. This method eliminates the need for holding pressure time in traditional plastic injection molding processes, thereby shortening cooling time and molding cycle, and reducing problems such as center misalignment and poor yield. It allows for the injection molding of two different materials using the same micro-foaming dual-color injection molding machine. The dissimilar material components provide excellent structural strength, offering sufficient rigid support during swings, and providing shock absorption and lightweight properties.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] This invention relates to a method for manufacturing a badminton racket, and more particularly to a method for manufacturing a badminton racket grip. [Previous Technology]

[0002] The structure of a badminton racket consists of three main parts: the head frame, the shaft, and the grip. The head frame is strung to form the hitting surface, and the head frame is connected to the grip through the shaft.

[0003] A badminton racket is disclosed in the approved Republic of China Invention Patent Certificate No. I772198, which includes a frame, a handle, a front sleeve, and a shaft. The handle includes a grip portion, a sleeve portion, a fixing member, a plurality of support members, and an adjustment ring. The grip portion has a front end. The sleeve portion is connected to the front end of the grip portion. The front sleeve is sleeved on the sleeve portion of the handle. One end of the shaft is connected to the frame, and the other end passes through a first opening to be inserted into the fixing member; wherein the grip portion is made of plastic material by injection molding.

[0004] However, in the aforementioned invention patent, the central tube is inserted into the sleeve portion; a plurality of support members are disposed in the grip portion, and the front edge of the support members is connected to the inner sidewall of one of the sleeve portions. When hitting the ball, although the plurality of support members can disperse the impact force, they cannot achieve the effect of shock absorption or shock reduction, which will cause discomfort to the palm and arm. Furthermore, the sleeve portion, the plurality of support members, and the grip portion are made of the same material. If the material is relatively hard, such as carbon fiber, the whole structure is too hard and lacks elasticity. In addition to being uncomfortable, the racket is also prone to breakage and has poor durability. If the material is relatively soft, such as nylon plastic, the grip portion lacks rigidity, and the hitting force cannot be effectively released, thus affecting the hitting performance.

[0005] One of the conventional manufacturing methods for badminton racket grips is to use a one-time injection molding process. The molded badminton racket grips are prone to center offset and poor yield. On the other hand, since the traditional plastic injection molding process is used, a certain amount of holding pressure and cooling time is required, which limits the production capacity. The one-time injection molding process can only use a single material to make badminton racket grips, and cannot use two or more different materials.

[0006] Another known method for manufacturing badminton racket grips involves using two separate plastic injection molding machines. The first machine first injects and molds a semi-finished product, which is then transferred to the second machine for secondary encapsulation molding. Although different materials can be used to make badminton racket grips through encapsulation molding technology, the traditional plastic injection molding process still requires a certain amount of holding pressure and cooling time, which limits production capacity. [Summary of the Invention]

[0007] The technical problem to be solved by the present invention is to provide a method for manufacturing a badminton racket grip that can use two different materials, and can eliminate the problems of holding pressure time, center offset and poor yield that are common in traditional plastic injection molding processes.

[0008] To solve the above-mentioned technical problems, the present invention proposes a method for manufacturing a badminton racket grip, comprising: preparing a main body, preparing a front sleeve for assembly at the front end of the main body, preparing a rear end cap for assembly at the rear end of the main body, and assembling the main body, the front sleeve, and the rear end cap into a badminton racket grip, wherein the front sleeve is hollow inside and has a through hole for a middle tube of the badminton racket to pass through; characterized in that the main body is manufactured by the following steps, including:

[0008] An inner core is formed using a micro-foaming injection molding process (MuCell) with a first material. The inner core comprises a straight tube and several ribs protruding outwards along a radial direction from the outer surface of the straight tube. The straight tube is an axially continuous tubular member into which the shaft of a badminton racket can be inserted; and

[0008] Using a second material, a shell is formed on the outside of the inner core using a micro-foaming injection process. The shell is a hollow tubular body, and the ends of the ribs extending in the direction of extension are connected to the inner wall of the shell.

[0009] In a preferred embodiment of the method for manufacturing the badminton racket grip of the present invention, the second material comprises either nano-nylon 6 (PA6) or a composite material consisting of nano-nylon 6 (PA6) with 10% glass fiber (GF); the first material is carbon fiber.

[0010] A preferred embodiment of the method for manufacturing the badminton racket grip of the present invention includes:

[0010] A first mold, a second mold, and a slider are provided. The first mold includes a first cavity and a second cavity. The second mold includes the same first cavity and second cavity. The slider can enter and exit the first cavity and the second cavity. The first cavity can cooperate with the slider to form the inner core. The inner core and the slider can enter and exit the second cavity together. The second cavity can cooperate with the slider to form the outer shell on the outside of the inner core.

[0010] A micro-foaming two-color injection molding machine is provided, the micro-foaming two-color injection molding machine having a first injection tube and a second injection tube, the first injection tube being used to inject the first material into a first cavity at a first injection position, and the second injection tube being used to inject the second material into a second cavity at a second injection position; and

[0010] A rotating shaft is provided, which can drive the first mold, the second mold and the slider to rotate 180 degrees back and forth, so as to alternately move the first mold and the second mold to the first injection position and the second injection position.

[0011] The advantages and effects of the badminton racket grip manufacturing method of the present invention are as follows: The badminton racket grip manufactured by the present invention using micro-foaming injection molding process (MuCell) not only has the advantage of being lightweight, but also eliminates the pressure holding time. In addition, due to the reduction of plastic content, the processing heat is greatly reduced, thereby shortening the cooling time and molding cycle. Two different materials can be injection molded in the same micro-foaming dual-color injection molding machine. The components of different materials can provide excellent structural strength, and can provide sufficient rigid support and comfortable shock absorption of the grip when swinging.

[0012] The specific embodiments, technical features and effects of the present invention will be described below in conjunction with the drawings. [Simplified Explanation of the Diagram]

[0013] Figure 1 is a structural diagram of an embodiment of the badminton racket grip of the present invention.

[0013] Figure 2 is an exploded view of the structure of the embodiment of Figure 1.

[0013] Figure 3 is a cross-sectional view of Figure 1 at position AA.

[0013] Figure 4 shows a schematic diagram of the structure of a micro-foaming two-color injection molding machine.

[0013] Figure 5 is a schematic diagram illustrating the structure of an embodiment of a micro-foaming two-color injection molding machine and its mold for implementing the method of the present invention.

[0013] Figure 6 is a schematic diagram of the structure of a mold for implementing the method of the present invention.

[0013] Figures 7A-7D illustrate the continuous operation of the micro-foaming two-color injection molding machine and its mold for implementing the method of the present invention.

Implementation Method

[0014] In the embodiments disclosed in the specification and drawings of this invention, the directions mentioned (e.g., up, down, left, right, front, and back) are based on the content shown in the drawings and are used to illustrate the relative relationships (e.g., positional relationships, connection relationships, and operational relationships) between various elements or structures in the embodiments. In principle, the stated direction is appropriate when the position of the element or structure mentioned in the specification matches the position shown in the drawings. If the position of the element or structure mentioned in the specification changes, the stated direction should also be changed accordingly.

[0015] Please first refer to Figures 1 and 2, which are structural diagrams and exploded views of an embodiment of the badminton racket grip of the present invention. A preferred embodiment of the badminton racket grip proposed by the present invention includes: a main body 10, a front sleeve 20, and a rear end cap 30.

[0016] The front sleeve 20 is assembled at the front end of the main body 10, and the rear cover 30 is assembled at the rear end of the main body 10. The badminton racket grip can be completed by assembling the main body 10, the front sleeve 20 and the rear cover 30. The front sleeve 20 is hollow inside and has a through hole for the middle tube 40 of the badminton racket to pass through.

[0017] The manufacturing method of the badminton racket grip of the present invention mainly involves fabricating the main body 10 through a micro-foaming injection molding process (MuCell). As a preferred embodiment of the manufacturing method of the badminton racket grip of the present invention, the main body 10 is fabricated through the following steps, which include:

[0017] An inner core 11 is formed using a micro-foaming injection molding process with the first material. The inner core 11 includes a straight tube 111 and several ribs 112 protruding outward from the outer surface of the straight tube 111 along a radial direction (see Figure 3). The straight tube 111 is an axially continuous tubular member into which the middle tube 40 of a badminton racket can be inserted; and

[0017] Using a second material, a shell 12 is formed on the outside of the inner core 11 by a micro-foaming injection process. The shell 12 is a hollow tubular body. The ends of the ribs 112 extending in the direction of extension are connected to the inner wall of the shell 12, thereby forming an integrated structure.

[0018] In a preferred embodiment of the method for manufacturing the badminton racket grip of the present invention, the second material, namely the material used to make the outer shell 12, includes either nano nylon 6 (PA6) or a composite material made of nano nylon 6 (PA6) with 10% glass fiber (GF); preferably, the first material, namely the material used to make the inner core 11, is carbon fiber.

[0019] In a preferred embodiment of the method of the present invention, the main body 10 is manufactured using a micro-foaming two-color injection molding machine; please refer to Figure 4, which illustrates an exemplary structural schematic diagram of the micro-foaming two-color injection molding machine. The micro-foaming injection molding process of plastic involves injecting a precisely metered supercritical fluid into the injection tube 50 of the injection molding machine through a syringe 51. The supercritical fluid is generally nitrogen (N2) or carbon dioxide (CO2). Through a specially designed screw 52, ​​the supercritical fluid and plastic are uniformly mixed and diffused to form a single-phase solution 53 of supercritical fluid-molten polymer. Then, the single-phase solution 53 is injected into the cavity of the mold for low-pressure filling. Due to the instantaneous pressure drop causing thermodynamic imbalance, the supercritical fluid after entering the cavity can diffuse from the molten plastic to nucleate and grow into uniform microbubbles. When the cavity is filled, the bubble growth stops, and the bubble growth generates uniform holding pressure within the cavity.

[0020] Plastic containing microbubbles is cooled and solidified to obtain a micro-foamed finished product. This process eliminates the pressure holding stage of traditional plastic injection molding, thus saving process cycle time. It also solves problems such as uneven shrinkage and warping deformation in traditional injection molded products, resulting in a significant improvement in product dimensional accuracy. Furthermore, the microfoaming process has a shorter production cycle than general injection molding. Because it uses gas as the foaming medium, its products also offer advantages such as environmentally friendly processing, lightweight design, and recyclable plastic.

[0021] Please refer to Figures 5 and 6, which illustrate a structural schematic diagram of an embodiment of a micro-foaming two-color injection molding machine and its mold for implementing the method of the present invention. According to a preferred embodiment of the aforementioned method of the present invention, the main body 10 is fabricated through a micro-foaming injection molding process (MuCell), including the following steps:

[0021] A first mold M1, a second mold M2, and a slider 60 are provided. The first mold M1 includes a first cavity C1 and a second cavity C2. The second mold M2 includes the same first cavity C1 and second cavity C2. The slider 60 can enter and exit the first cavity C1 and the second cavity C2. The first cavity C1 can work with the slider 60 to form the inner core 11. The inner core 11 and the slider 60 can enter and exit the second cavity C2 together. The second cavity C2 can work with the slider 60 to form the outer shell 12 on the outside of the inner core 11.

[0021] A micro-foaming two-color injection molding machine is provided, the micro-foaming two-color injection molding machine having a first injection tube 50A and a second injection tube 50B, the first injection tube 50A being used to inject the first material into a first cavity C1 at a first injection position P1, and the second injection tube 50B being used to inject the second material into a second cavity C2 at a second injection position P2; and

[0021] A rotating shaft 70 is provided, which can drive the first mold M1, the second mold M2 and the slider 60 to rotate 180 degrees back and forth, so as to alternately move the first mold M1 and the second mold M2 to the first injection position P1 and the second injection position P2.

[0022] In a preferred embodiment, the first mold M1 and the second mold M2 have the same structure, that is, both the first mold M1 and the second mold M2 have a first cavity C1 for molding the inner core 11 and a second cavity C2 for molding the outer shell 12. The first injection tube 50A and the second injection tube 50B are respectively disposed on both sides of the axis of the rotating shaft 70. The first injection tube 50A is used to inject the first material into the first mold M1 or the second mold M2 rotated to the first injection position P1; the second injection tube 50B is used to inject the second material into the first mold M1 or the second mold M2 rotated to the second injection position P2.

[0023] Please refer to Figures 7A to 7D, which illustrate an exemplary continuous operation diagram of a micro-foaming two-color injection molding machine and its mold for implementing the method of the present invention.

[0024] First, as shown in Figure 7A, the first mold M1 rotates to the first injection position P1, and the second mold M2 rotates to the second injection position P2. Slider 60 is placed in the first cavity C1 and the second cavity C2 of the first mold M1, and slider 60 is also placed in the first cavity C1 and the second cavity C2 of the second mold M2. Then, the first injection tube 50A injects the first material into the first cavity C1 of the first mold M1, and the inner core 11 (including the forming of straight tube 111 and several ribs 112) is formed by the synergistic action of the first cavity C1 and slider 60.

[0025] As shown in Figure 7B, after the inner core 11 is formed, the mold is opened once to complete the micro-foaming injection molding of the inner core 11. Then, the rotating shaft 70 drives the first mold M1, the second mold M2 and the slider 60 to rotate 180 degrees, and rotates the first mold M1 together with the formed inner core 11 to the second injection position P2, and simultaneously rotates the second mold M2 to the first injection position P1.

[0026] As shown in Figure 7C, the first injection tube 50A injects the first material into the first cavity C1 of the second mold M2. The inner core 11 is formed in the second mold M2 by the synergistic action of the first cavity C1 and the slider 60. At the same time, the second injection tube 50B injects the second material into the second cavity C2 of the first mold M1. The outer shell 12 is formed on the outside of the inner core 11 by the synergistic action of the second cavity C2 and the slider 60. The ends of the extension directions of the several ribs 112 of the inner core 11 will be connected to the inner wall of the outer shell 12, thereby forming an integrated structure.

[0027] As shown in Figure 7D, after the main body 10 (including the inner core 11 and the outer shell 12) is molded by micro-foaming injection process, a mold opening is performed. A core puller 80 is used to pull the slider 60 and the molded main body 10 out of the first mold M1. After the main body 10 is removed, the free slider 60 is put back into the first cavity C1 and the second cavity C2 of the first mold M1, returning to the state shown in Figure 7A. Then, the operations of Figures 7A to 7D are repeated. With the cooperation of automated control and mechanical operation, a continuous and automated badminton racket grip manufacturing process can be realized.

[0028] The present invention uses a micro-foaming injection molding process to form the main body 10 of a badminton racket grip. Preferably, the gas content is 5% to 10% of the total content, which has little impact on the structural strength of the finished product. In addition to the advantages of lightweight, it can also eliminate the pressure holding time. Furthermore, due to the reduction in plastic content, the processing heat is greatly reduced, thereby shortening the cooling time and molding cycle. Two different materials can be injection molded in the same micro-foaming dual-color injection molding machine. Components of different materials can provide excellent structural strength and can provide sufficient rigid support and comfortable shock absorption of the grip when swinging.

[0029] Although the present invention has been disclosed above through the above embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications and refinements without departing from the spirit and scope of the present invention. Therefore, the scope of patent protection of the present invention shall be determined by the claims attached to this specification.

Claims

1. A method for manufacturing a badminton racket grip, comprising: The invention comprises: fabricating a main body; fabricating a front sleeve for mounting at the front end of the main body; fabricating a rear end cap for mounting at the rear end of the main body; and assembling the main body, the front sleeve, and the rear end cap into a badminton racket grip. The front sleeve is hollow inside and has a through hole for a middle tube of the badminton racket to pass through. The main body is characterized by being manufactured through the following steps: forming an inner core using a micro-foaming injection molding process with a first material, the first material being carbon fiber. The inner core includes a straight tube and an outer portion extending from the outside of the straight tube. The inner core has several ribs protruding outward along the radial direction on its side surface. The straight tube is an axially penetrating tubular member into which the middle tube of a badminton racket can be inserted. A shell is formed on the outside of the inner core using a second material and a micro-foaming injection molding process. The second material includes either nano-nylon 6 (PA6) or a composite material of nano-nylon 6 (PA6) with 10% glass fiber (GF). The shell is a hollow tubular body, and the ends of the ribs extending in the radial direction are connected to the inner wall of the shell.

2. A method for manufacturing a badminton racket grip as described in claim 1, comprising: The system provides a first mold, a second mold, and a slider. The first mold includes a first cavity and a second cavity, and the second mold includes the same first cavity and second cavity. The slider can enter and exit the first cavity and the second cavity. The first cavity can cooperate with the slider to form an inner core. The inner core and the slider can enter and exit the second cavity together. The second cavity can cooperate with the slider to form a shell on the outside of the inner core. The system also provides a micro-foaming two-color injection molding machine with a first injection tube and a second injection tube. The first injection tube is used to inject a first material into the first cavity at a first injection position, and the second injection tube is used to inject a second material into the second cavity at a second injection position. Finally, the system provides a rotating shaft that can drive the first mold, the second mold, and the slider to rotate 180 degrees reciprocally, thereby alternately moving the first mold and the second mold to the first injection position and the second injection position.

Citation Information

Patent Citations

  • Integrally-formed badminton racket and manufacturing method thereof

    CN115487473A

  • Badminton racket handle and badminton racket

    CN115518355A

  • Metal thermoplastic sandwich overmold

    US20230373140A1

  • Badminton racket handle structure

    US5425534A