Polymer stirring device and recycling system

The polymer stirring device with an adhesion position detection unit addresses the variability in PET quality by evaluating and adjusting the polymer's viscosity and degree of polymerization, enhancing the recycling system's efficiency and output quality.

WO2024202715A1PCT designated stage expired Publication Date: 2024-10-03SUMITOMO HEAVY IND LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/006078
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-02-20
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The quality of PET flakes and pellets varies when PET bottles of different qualities undergo the same recycling process, making it challenging to consistently evaluate and improve the quality of recycled polymers.

Method used

A polymer stirring device with a rotating body and an adhesion position detection unit is used to evaluate the quality of polymers by detecting the position of polymer adhesion, which indirectly indicates viscosity and degree of polymerization, and a recycling system that includes a polymer supply device and a polymer stirring device to enhance the recycling process.

Benefits of technology

Effectively evaluates the quality of polymers like PET, ensuring consistent high-quality output by adjusting the stirring mode to achieve desired viscosity and degree of polymerization, thereby improving the recycling efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024006078_03102024_PF_FP_ABST
    Figure JP2024006078_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A polymer stirring device 700 is provided with: a container 710 to which a polymer PM is supplied; a first rotating body 720 and a second rotating body 730 which rotate in the container 710 to stir the polymer PM; and an adhered position detection unit 760 which detects the position of polymer PM adhered to the first rotating body 720 and / or the second rotating body 730. The adhered position detection unit 760 detects a highest arrival position H, in the vertical direction, of polymer PM adhered to the first rotating body 720 and / or the second rotating body 730. The first rotating body 720 and the second rotating body 730 are provided with a first rotating plate 721 and a second rotating plate 731 which rotate around a first rotational axis 722 and a second rotational axis 732 both extending in a direction that intersects the vertical direction, and the adhered position detection unit 760 detects a highest arrival position H, in the vertical direction, of polymer PM adhered to the first rotating plate 721 and / or the second rotating plate 731.
Need to check novelty before this filing date? Find Prior Art

Description

Polymer mixing equipment, recycling system

[0001] The present disclosure relates to polymer agitation devices and the like.

[0002] Patent Document 1 discloses a method for recycling PET (polyethylene terephthalate) bottles by crushing the PET bottles to produce PET flakes, which serve as the raw material for new PET bottles. Specifically, known methods include mechanical recycling, in which crushed PET bottles are heated and melted, and then PET flakes are obtained by solid-state polymerization, and chemical recycling, in which crushed PET bottles are decomposed into intermediates such as bis(2-hydroxyethyl) terephthalate (BHET) or depolymerized polymers by a depolymerization reaction, and then PET flakes are obtained by a repolymerization reaction.

[0003] JP 2016-153176 A JP 2022-27158 A

[0004] The quality of the above-mentioned PET flakes and PET pellets (hereinafter simply referred to as flakes or pellets, and this also refers to flakes and pellets that are not made from PET) depends on the quality of their raw materials, PET bottles, etc. Therefore, if PET bottles of different qualities are subjected to the same recycling process, the quality of the flakes and pellets may vary.

[0005] The present disclosure has been made in view of these circumstances, and aims to provide a polymer agitation device and the like that can effectively evaluate the quality of polymers such as PET.

[0006] In order to solve the above problems, a polymer stirring device according to one embodiment of the present disclosure comprises a container into which a polymer is supplied, a rotor that rotates within the container to stir the polymer, and an adhesion position detection unit that detects the position of the polymer adhered to the rotor.

[0007] In this embodiment, the position of the polymer adhering to the rotor that stirs the polymer is detected, and based on this position, the viscosity and degree of polymerization of the polymer can be indirectly recognized, thereby enabling effective evaluation of the quality of the polymer.

[0008] Another aspect of the present disclosure is a recycling system. The recycling system includes a polymer supply device that supplies a polymer derived from a first molded article, and a polymer agitation device that agitates the polymer and supplies it to a molding machine that molds a second molded article. The polymer agitation device includes a container to which the polymer is supplied, a rotor that rotates within the container to agitate the polymer, and an adhesion position detection unit that detects the position of the polymer adhered to the rotor.

[0009] Any combination of the above components, or any conversion of these expressions into methods, devices, systems, recording media, computer programs, etc., are also encompassed within the present disclosure.

[0010] According to the present disclosure, the quality of polymers such as PET can be effectively evaluated.

[0011] Schematic showing the configuration of a chemical recycling molding system. Schematic showing the polymerization reaction and depolymerization reaction of PET. Schematic showing the configuration of a polymer agitator. Schematic showing the configuration of a polymer agitator. Illustrated is a first modified example of a chemical recycling molding system. Illustrated is a second modified example of a chemical recycling molding system.

[0012] Hereinafter, with reference to the drawings, a detailed description will be given of a mode for carrying out the present disclosure (hereinafter also referred to as an embodiment). In the description and / or drawings, identical or equivalent components, members, processes, etc. are designated by the same reference numerals, and redundant description will be omitted. The scale and shape of each part shown in the drawings are set for convenience to simplify the description and should not be interpreted as limiting unless otherwise specified. The embodiment is an example and does not limit the scope of the present disclosure in any way. Not all features and their combinations presented in the embodiment are necessarily essential to the present disclosure. For convenience, the embodiment is presented broken down into components for each function and / or functional group that realizes the embodiment. However, one component in the embodiment may actually be realized by a combination of multiple separate components, or multiple components in the embodiment may actually be realized by a single integrated component.

[0013] 1 is a schematic diagram illustrating the configuration of a chemical recycling molding system as one embodiment of a recycling system according to the present disclosure. The chemical recycling molding system includes a chemical recycling device 100 and an injection molding machine 1. The chemical recycling device 100 performs a chemical recycling process, described in detail below, on a first molded product such as a PET bottle. Note that the recycling system according to the present disclosure is not limited to chemical recycling, and may also perform mechanical recycling.

[0014] The chemical recycling apparatus 100 includes a polymer preparation apparatus 200, a depolymerization reaction tank 300, a polymerization reaction tank 400, a by-product removal apparatus 500, and a polymer supply unit 600. The number of each of the injection molding machines 1 (two of which are shown schematically in FIG. 1 ), polymer preparation apparatus 200, depolymerization reaction tank 300, polymerization reaction tank 400, by-product removal apparatus 500, and polymer supply unit 600 may be installed as desired. In particular, by increasing the number of injection molding machines 1 and polymerization reaction tanks 400, which typically have slower processing speeds or reaction rates than other processing units, compared to the other processing units, the processing performance can be improved so that these processing units do not become serious bottlenecks.

[0015] The polymer preparation apparatus 200 prepares a polymer such as PET constituting a first molded article such as a PET bottle for the subsequent depolymerization reaction tank 300. Specifically, the polymer preparation apparatus 200 subjects the first molded article such as a PET bottle to treatments such as pulverization, heat melting, and mixing to prepare the polymer such as PET in a state (phase, shape, size, etc.) suitable for the depolymerization reaction in the depolymerization reaction tank 300. The first molded article may be any molded article other than a bottle, such as a sheet, film, or fiber. The polymer constituting the first molded article may be any polymer other than PET, such as polyester (including PET), polyamide, or polyurethane.

[0016] The depolymerization reaction tank 300 decomposes the polymer, such as PET, prepared by the polymer preparation apparatus 200 into depolymers through a depolymerization reaction. When the polymer supplied from the polymer preparation apparatus 200 is PET, the intermediate BHET is obtained as the depolymer through the depolymerization reaction in the depolymerization reaction tank 300. The depolymer obtained in the depolymerization reaction tank 300 may contain a monomer or monomers of the polymer. When the polymer is PET, examples of the monomer include ethylene glycol, terephthalic acid, dimethyl terephthalate, and ethylene terephthalate.

[0017] As shown schematically in FIG. 2 , in the depolymerization reaction (300) of PET as a polymer, PET is decomposed by ethylene glycol (EG) as a depolymerization agent supplied from a depolymerization agent supply unit 310 ( FIG. 1 ) to the depolymerization reaction vessel 300, to obtain BHET as a depolymerized product. Instead of or in addition to the depolymerization agent supply unit 310, EG may be supplied from the polymer preparation apparatus 200. To promote this depolymerization reaction, the inside of the depolymerization reaction vessel 300 is maintained at a temperature suitable for the depolymerization reaction by a heater 320 ( FIG. 1 ) or a warmer provided next to the depolymerization reaction vessel 300. The temperature suitable for the depolymerization reaction of PET to BHET in FIG. 2 is between 220°C and 250°C, preferably between 230°C and 245°C, and more preferably between 235°C and 240°C. 2, the pressure suitable for the depolymerization reaction of PET to BHET is between 0.3 MPa and 0.8 MPa, preferably between 0.4 MPa and 0.6 MPa, and more preferably between 0.45 MPa and 0.55 MPa. The pressure in depolymerization reaction tank 300 is adjusted by a pump (not shown) or the like provided in addition to depolymerization reaction tank 300.

[0018] The viscosity of the fluid in the depolymerization reaction tank 300, where BHET, which has a smaller molecular weight than PET, is produced, is lower than the viscosity of the fluid in the polymerization reaction tank 400, which will be described later, where PET, which has a larger molecular weight, is produced. Therefore, a low-viscosity agitator blade 330 is used to agitate the fluid in the depolymerization reaction tank 300 and promote the depolymerization reaction. Examples of the low-viscosity agitator blade 330 include a propeller blade, a disk turbine blade, and a paddle blade.

[0019] Installed downstream of the depolymerization reaction tank 300 are foreign matter removal devices 340, 350, and 360 that remove foreign matter from the fluid primarily composed of depolymerized BHET. The foreign resin removal device 340 removes resins other than the target resin, such as PET, and / or depolymerized resins thereof using the principles of flotation separation and sedimentation removal. The colored matter removal device 350 removes colored matter using activated carbon or the like. The metal ion removal device 360 ​​removes metal ions using the principles of ion exchange or the like. Installed downstream of the foreign matter removal devices 340, 350, and 360 is a buffer tank 370 that temporarily stores the fluid primarily composed of BHET and the like after the foreign matter has been removed before supplying it to the polymerization reaction tank 400.

[0020] The buffer tank 370 may be provided with a first preheater 371 that heats or keeps warm the depolymerized polymer (a fluid mainly composed of BHET, etc.) before it is supplied to the downstream polymerization reaction tank 400. The first preheater 371 may maintain the depolymerized polymer at a temperature (between 220°C and 250°C) similar to that of the heater 320 provided in the depolymerization reaction tank 300, or may maintain the depolymerized polymer at a temperature (between 250°C and 300°C) suitable for the polymerization reaction similar to that of the heater 410 provided in the polymerization reaction tank 400, which will be described later. In this way, by providing the buffer tank 370 equipped with a preheating mechanism (first preheater 371) as needed upstream of the polymerization reaction tank 400, the depolymerized polymer can be stored at an appropriate temperature while being fed into the polymerization reaction tank 400, which typically has a slower processing speed or reaction rate than other processing units, such as the depolymerization reaction tank 300 and the by-product removal device 500, which will be described later. As a result, the overall capacity of the chemical recycling apparatus 100 can be increased, and the chemical recycling apparatus 100 can be operated stably and continuously (without running out of resin) while supplying appropriate amounts of reactants in a timely manner to each processing section, such as the depolymerization reaction tank 300, the polymerization reaction tank 400, the by-product removal apparatus 500, and the polymer supply section 600. Note that the preheating mechanism such as the first preheater 371 is not limited to being provided in the buffer tank 370, but may be provided in any desired location between the depolymerization reaction tank 300 and the polymerization reaction tank 400 (for example, in the foreign matter removal apparatuses 340, 350, 360) in any desired manner.

[0021] The polymerization reactor 400 polymerizes depolymerized materials such as BHET produced in the depolymerization reactor 300 and from which foreign matter has been removed by the foreign matter removal devices 340, 350, and 360 through a polymerization reaction. When the depolymerized material produced in the depolymerization reactor 300 is BHET, the polymer PET is re-obtained through a polymerization reaction in the polymerization reactor 400.

[0022] As shown schematically in FIG. 2 , the polymerization reaction (400) of BHET as a depolymerization product produces PET as a main polymer product, as well as EG as a by-product. This EG may be recycled to the depolymerization agent supply unit 310 and used in the depolymerization reaction of PET in the depolymerization reaction tank 300. Because the EG produced in the polymerization reaction tank 400 can be reused on-site (in the depolymerization reaction tank 300) without being wasted, the operating efficiency of the chemical recycling apparatus 100 can be improved. In particular, the amount of EG purchased for the depolymerization reaction of PET in the depolymerization reaction tank 300 can be significantly reduced, leading to a reduction in the operating costs of the chemical recycling apparatus 100.

[0023] To promote the above-described polymerization reaction, the interior of the polymerization reactor 400 is maintained at a temperature suitable for the polymerization reaction by a heater 410 ( FIG. 1 ) or a warmer attached to the polymerization reactor 400 as a second heater. The temperature suitable for the polymerization reaction of BHET to PET in FIG. 2 is between 250°C and 300°C, preferably between 260°C and 290°C, and more preferably between 270°C and 280°C. The polymerization heating temperature by the heater 410 attached to the polymerization reactor 400 is higher than the depolymerization heating temperature by the heater 320 attached to the depolymerization reactor 300. The polymerization reactor 400 produces PET with a high molecular weight and a high melting point. By maintaining the temperature higher than that of the depolymerization reactor 300, which produces BHET with a low molecular weight and a low melting point, the PET, the main product of the polymerization reactor 400, remains molten. The polymerization reaction of BHET to PET in FIG. 2 is preferably carried out under vacuum. For this purpose, the polymerization reaction vessel 400 is provided with a vacuum pump or the like (not shown).

[0024] The viscosity of the fluid in the polymerization reaction tank 400, where PET with a high molecular weight is produced, is higher than the viscosity of the fluid in the depolymerization reaction tank 300, where BHET with a lower molecular weight than PET, a polymer, is produced. Therefore, a stirring blade 420 for high viscosity is used to stir the fluid in the polymerization reaction tank 400 and promote the polymerization reaction. Examples of the stirring blade 420 for high viscosity include an anchor blade and a helical ribbon blade.

[0025] The IV (intrinsic viscosity) value, or inherent viscosity, is known as a value correlated with the degree of polymerization of polymers such as PET. The IV value (dL / g) is also used as an indicator of polymer applications. For PET, an IV value of approximately 0.72 or higher is suitable for bottles, an IV value of approximately 0.65 or higher is suitable for sheets and films, and an IV value of approximately 0.58 or higher is suitable for fibers. The objective of this embodiment is to ultimately obtain PET with an IV value suitable for bottles and sheets. As described below, the IV value can be increased in the by-product removal device 500 and / or the polymer supply unit 600 (the polymer agitation device according to the present disclosure) downstream of the polymerization reactor 400, so the IV value of the PET synthesized in the polymerization reactor 400 may be relatively low. Specifically, the IV value of the PET synthesized in the polymerization reactor 400 is between 0.2 and 0.7, preferably between 0.3 and 0.7, and more preferably between 0.3 and 0.55.

[0026] A buffer tank 430 may be provided downstream of the polymerization reaction tank 400 to temporarily store the polymer synthesized in the polymerization reaction tank 400 before supplying it to the downstream by-product removal device 500 and / or polymer supply unit 600. The buffer tank 430 may be provided with a second preheater 431 to heat or keep the polymer warm before supplying it to the downstream by-product removal device 500 and / or polymer supply unit 600. The second preheater 431 may maintain the polymer at a temperature (between 250°C and 300°C) similar to that of the heater 410 provided adjacent to the polymerization reaction tank 400, or may maintain the polymer at a temperature (between 250°C and 290°C) suitable for polymerization reaction similar to that of the heater 520 provided adjacent to the by-product removal device 500 described below, or may maintain the polymer at a temperature (between 250°C and 290°C) similar to that of the heater 620 provided adjacent to the polymer supply unit 600 described below.

[0027] In this way, by providing a buffer tank 430 equipped with a preheating mechanism (second preheater 431) as needed upstream of the by-product removal apparatus 500 and / or the polymer supply section 600, polymers waiting to be introduced into the by-product removal apparatus 500 and / or the polymer supply section 600 can be stored while being maintained at an appropriate temperature. As a result, the overall capacity of the chemical recycling apparatus 100 can be increased, and the chemical recycling apparatus 100 can be operated stably and continuously while supplying appropriate amounts of reactants to each processing section, such as the depolymerization reaction tank 300, the polymerization reaction tank 400, the by-product removal apparatus 500, and the polymer supply section 600, in a timely manner (without running out of resin). Note that a preheating mechanism such as the second preheater 431 is not limited to the buffer tank 430, but can be provided in any manner at any location between the polymerization reaction tank 400 and the by-product removal apparatus 500 and / or at any location between the by-product removal apparatus 500 and the polymer supply section 600.

[0028] A by-product removal device 500 may be provided downstream of the polymerization reaction tank 400 (and upstream of the polymer supply section 600, described below), through which PET (main product) and EG (by-product) produced by the polymerization reaction in the polymerization reaction tank 400 are passed, and which removes the EG as a by-product. The by-product removal device 500 in the illustrated example includes a number of linear members 510 extending from above to below. The increased surface area provided by the number of linear members 510 promotes the volatilization of EG adhering to the surface of each linear member 510, thereby effectively separating and removing the EG from the highly viscous PET.

[0029] This EG may be recycled to the depolymerization agent supply unit 310 and used in the depolymerization reaction of PET in the depolymerization reaction tank 300. The EG separated and removed in the byproduct removal device 500 can be reused on site (in the depolymerization reaction tank 300) without being wasted, thereby improving the operating efficiency of the chemical recycling apparatus 100. In particular, the amount of EG purchased for the PET depolymerization reaction in the depolymerization reaction tank 300 can be significantly reduced, leading to a reduction in the operating costs of the chemical recycling apparatus 100.

[0030] Furthermore, PET with a relatively low degree of polymerization (i.e., IV value) and BHET that did not react in the polymerization reactor 400 also adhere to the surface of each linear member 510, allowing the large surface area to effectively promote a polymerization reaction similar to that in the polymerization reactor 400. Therefore, by passing through the by-product removal device 500, the IV value of the PET as the main product is increased. Specifically, the IV value of the PET after passing through the by-product removal device 500 is 0.7 or higher, preferably 0.8 or higher, and more preferably 0.85 or higher.

[0031] To promote this polymerization reaction, the inside of the by-product removal apparatus 500 is maintained at a temperature suitable for the polymerization reaction by a heater 520 ( FIG. 1 ) or a warmer attached to the by-product removal apparatus 500 as a second heater. Specifically, the heating temperature by the heater 520 is between 250°C and 290°C, preferably between 260°C and 280°C. The heating temperature by the heater 520 attached to the by-product removal apparatus 500 is preferably higher than the polymerization heating temperature by the heater 410 attached to the polymerization reaction tank 400. Since the polymerization reaction proceeds more rapidly in the by-product removal apparatus 500 than in the polymerization reaction tank 400, the molecular weight of the PET polymer increases and the melting point increases. Therefore, by maintaining the inside of the by-product removal apparatus 500 at a higher temperature than in the polymerization reaction tank 400, the PET product of the by-product removal apparatus 500 can be maintained in a molten state. A heater or a warmer may be provided as a second heater around the piping between the polymerization reaction tank 400 and the by-product removal apparatus 500, which heats or keeps the temperature at least to the polymerization heating temperature of the heater 410 provided next to the polymerization reaction tank 400. The polymerization reaction in the by-product removal apparatus 500 is preferably carried out in a vacuum state, similar to the polymerization reaction in the polymerization reaction tank 400. For this reason, a vacuum pump (not shown) or the like is provided next to the by-product removal apparatus 500. By creating a vacuum state (reduced pressure state) inside the by-product removal apparatus 500, the by-product EG can be efficiently removed.

[0032] The configuration of the by-product removal apparatus 500 is not limited to the "vertical" type shown in Fig. 1 . For example, a "horizontal" stirring apparatus such as that shown in Fig. 3 (described later) may be used as the by-product removal apparatus 500. Furthermore, as will be described later, the configuration or function of the "horizontal" stirring apparatus such as that shown in Fig. 3 (or the like) may be realized as part of the polymer supply section 600 (the polymer stirring apparatus according to the present disclosure). In this case, it is not necessary to provide the by-product removal apparatus 500 separately from the polymer supply section 600.

[0033] The polymer supply unit 600 supplies a polymer such as PET synthesized in the polymerization reaction tank 400 (or the polymerization reaction tank 400 and the by-product removal device 500) to the injection molding machine 1 that molds a second molded product such as a PET bottle. The polymer supply unit 600 is equipped with a transfer pump 610 such as a gear pump or a screw pump that is suitable for supplying the PET in a molten state, from which the by-product EG has been removed in the by-product removal device 500, to the injection molding machine 1.

[0034] The polymer supply section 600 is provided with a heater 620 or a warmer as a first heater that heats or keeps warm the polymer such as PET transferred to the injection molding machine 1 by the transfer pump 610, thereby maintaining the polymer in a molten state. Specifically, the heating temperature by the heater 620 is between 250°C and 290°C, preferably between 260°C and 280°C. Here, the heating temperature (first heating temperature) by the heater 620 (first heater) provided in the polymer supply section 600 is preferably higher than the second heating temperature by a second heater such as the heater 410 provided adjacent to the polymerization reaction tank 400, the heater 520 provided adjacent to the by-product removal device 500, or a heater (not shown) provided between the polymerization reaction tank 400 and the by-product removal device 500. The polymerization reaction initiated in the polymerization reaction tank 400 gradually progresses and is completed in the by-product removal device 500. As a result, the molecular weight of the polymer, such as PET, becomes larger and the melting point becomes higher in the polymer supply section 600 than in the polymerization reaction tank 400 and the by-product removal device 500. Therefore, by setting the first heating temperature in the polymer supply section 600 higher than the previous second heating temperature, the polymer, such as PET, which has a high viscosity (i.e., a high degree of polymerization or a high IV value) and a high melting point, can be maintained in a molten state.

[0035] A temperature gradient may be provided so that the heating temperature increases stepwise from the polymerization reaction tank 400 to the polymer supply unit 600. For example, the heating temperature by a heater (not shown) provided between the polymerization reaction tank 400 and the by-product removal device 500 may be made higher than the heating temperature by the heater 410 provided adjacent to the polymerization reaction tank 400, the heating temperature by the heater 520 provided adjacent to the by-product removal device 500 may be made higher than the heating temperature by the heater (not shown), and the heating temperature by the heater 620 provided in the polymer supply unit 600 may be made higher than the heating temperature by the heater 520. This ensures that a polymer such as PET, whose melting point increases from the polymerization reaction tank 400 to the polymer supply unit 600, can be maintained in a molten state. Note that a heater may be provided between the polymer supply unit 600 and the injection molding machine 1 to heat or keep the polymer such as PET warm and maintain it in a molten state.

[0036] The injection molding machine 1 molds a molten polymer, such as PET, produced in the chemical recycling apparatus 100 into a second molded product. The second molded product may be the same or different from the first molded product, which is subjected to processing such as pulverization in the polymer preparation apparatus 200. For example, both the first and second molded products may be PET bottles. Alternatively, one of the first and second molded products may be a PET bottle, and the other may be a molded product other than a bottle, such as a sheet, film, or fiber. Generally, in mechanical recycling, the IV value of the second molded product after recycling is lower than that of the first molded product before recycling. However, the chemical recycling apparatus 100 according to this embodiment, which is equipped with IV value-increasing mechanisms such as the foreign matter removal devices 340, 350, and 360 and the by-product removal device 500, can increase the IV value of the second molded product after recycling compared to that of the first molded product before recycling. For example, according to this embodiment, PET fiber, which serves as the first molded product with a low IV value, can be recycled into a PET bottle, which serves as the second molded product with a high IV value.

[0037] The injection molding machine 1 molds a molten resin such as PET into a second molded product. An injection molding machine using molten resin as a raw material is disclosed, for example, in Patent Document 2. This application incorporates by reference the entire contents of that document (Japanese Patent Application No. 2020-130985), filed on July 31, 2020. As shown schematically in FIG. 1 , multiple injection molding machines 1 may be arranged in parallel. Note that the molding machine to which the molten resin or the like is supplied from the chemical recycling device 100 is not limited to an injection molding machine, and may be any molding machine (e.g., a compression molding machine).

[0038] In the present embodiment described above, the polymer resynthesized in the polymerization reaction tank 400 is not made into flakes or pellets, but is supplied as is by the polymer supply unit 600 to the injection molding machine 1. Since the conventional cooling and heating processes for flakes and pellets are no longer necessary, molded products such as PET bottles can be recycled with less energy.

[0039] In the chemical recycling apparatus 100 according to this embodiment, the polymer resynthesized in the polymerization reaction tank 400 is directly supplied to the injection molding machine 1, so it is necessary to quickly achieve the IV value of the polymer required for the molded product (second molded product). In this embodiment, a by-product removal device 500 and / or a polymer supply unit 600, which have the function of accelerating the polymerization reaction and increasing the IV value of the polymer, are provided in addition to the polymerization reaction tank 400, so this requirement can be fully met.

[0040] Next, the polymer agitation device according to the present disclosure will be described. In the example of FIG. 1 , the polymer agitation device is constituted by a by-product removal device 500 and / or a polymer supply unit 600 that agitates a polymer such as PET before supplying it to an injection molding machine 1 that molds a second molded product. Furthermore, the polymer adjustment device 200, depolymerization reactor 300, polymerization reactor 400, etc. that supply a polymer such as PET derived from the first molded product to the polymer agitation device constitute a polymer agitation device according to the present disclosure. Note that, although the polymer agitation device in the example of FIG. 1 is a chemical recycling device that supplies a polymer such as PET obtained by a chemical recycling process, the polymer agitation device according to the present disclosure may also be a mechanical recycling device that supplies a polymer such as PET obtained by a mechanical recycling process.

[0041] 3 and 4 are schematic diagrams showing the configuration of a polymer agitation apparatus 700 according to this embodiment. This polymer agitation apparatus 700 is a "horizontal" agitation apparatus that performs the same function as the "vertical" by-product removal apparatus 500 in FIG. 1 , and is configured integrally with the polymer supply section 600. Therefore, when the polymer agitation apparatus 700 shown in FIGS. 3 and 4 is used, it is not necessary to provide the "vertical" by-product removal apparatus 500 shown in FIG. 1 separately from the polymer agitation apparatus 700. For convenience, a three-dimensional coordinate system is set in FIGS. 3 and 4 using X, Y, and Z axes. For example, the X and Y axes are horizontal, and the Z axis is vertical. Here, the "vertical" type (the by-product removal apparatus 500 in FIG. 1 ) refers to a device that is elongated in the Z direction, and the "horizontal" type (the polymer agitation apparatus 700 in FIG. 3 ) refers to a device that is elongated in the X direction.

[0042] The polymer stirring device 700 includes a container 710, a first rotating body 720, a second rotating body 730, a first rotation drive unit 740, a second rotation drive unit 750, an adhesion position detection unit 760, an stirring mode adjustment unit 770, and a polymerization degree estimation unit 780.

[0043] Container 710 is supplied with polymer PM such as PET derived from a first molded product resynthesized in polymerization reactor 400 in a polymer supply device serving as the chemical recycling apparatus in FIG. 1 . Container 710 includes a supply port 711 connected to polymerization reactor 400 to supply polymer PM into container 710, and a discharge port 712 through which polymer PM agitated by a first rotor 720 and a second rotor 730 (described later) is discharged from container 710 and supplied to injection molding machine 1. A transfer pump 610 such as a gear pump or a screw pump capable of adjusting the amount and speed of polymer PM supplied into container 710 may be connected to supply port 711, and a transfer pump 610 such as a gear pump or a screw pump capable of adjusting the amount and speed of polymer PM discharged out of container 710 may be connected to discharge port 712.

[0044] The container 710 is elongated in the X direction as illustrated in FIG. 3 and has a substantially rectangular YZ cross section as illustrated in FIG. 4 . To accommodate the first rotor 720 and the second rotor 730, which are offset in the Y direction as described below, the YZ cross section ( FIG. 4 ) of the container 710 is elongated in the Y direction (i.e., rectangular). In FIG. 4 , the shape of the bottom of the container 710 conforms to the circular first rotor 720 and the circular second rotor 730. In this manner, the space or gap between the bottom of the container 710 and the first rotor 720 and the second rotor 730 is reduced, so that the polymer PM in the container 710 is effectively stirred by the first rotor 720 and / or the second rotor 730 without excessively accumulating at the bottom. As a result, the IV value, viscosity, degree of polymerization, etc. of the polymer PM are uniformed within the container 710.

[0045] 3 , supply port 711 is provided at one end in the X direction of container 710 (the left end in FIG. 3 ), and discharge port 712 is provided at the other end in the X direction of container 710 (the right end in FIG. 3 ). A first rotating body 720 and a second rotating body 730 are provided in the X direction region between supply port 711 and discharge port 712 to agitate the polymer PM in container 710.

[0046] The first rotating body 720 rotates within the container 710 to agitate the polymer PM. The first rotating body 720 includes one or more first rotating plates 721 that rotate around a first rotation axis 722 in a direction (X direction perpendicular to the Z direction in the example of FIG. 3 ) that intersects the vertical direction (Z direction in the example of FIG. 3 ). As shown in FIG. 4 , the first rotating plate 721 is, for example, a disk having a circular YZ cross section. However, the shape of the YZ cross section of the first rotating plate 721 is arbitrary, and may be, for example, an ellipse or a polygon such as a triangle or a rectangle. As shown in FIG. 4 , the center or center of gravity of the first rotating plate 721 in the YZ plane preferably coincides with the center of the first rotation axis 722. In this case, the one or more first rotating plates 721 and the first rotation axis 722 are arranged coaxially.

[0047] In the example of FIG. 3 , the first rotor 720 includes a plurality of first rotor plates 721 spaced apart in the axial direction (X direction) of the first rotor shaft 722. The axial distance between two adjacent first rotor plates 721 may be constant or may vary as illustrated. As will be described later, the closer to the outlet side of the container 710 (i.e., the discharge port 712 side), the higher the viscosity or degree of polymerization of the polymer PM, making it more likely for the polymer PM to adhere to the first rotor plates 721. If the spacing between the first rotor plates 721 on the outlet side of the container 710 is too small, the polymer PM adhering to each first rotor plate 721 may interfere with each other, potentially hindering the agitation of the polymer PM or the rotation of the first rotor 720. Therefore, as illustrated, it is preferable to increase the spacing between the first rotor plates 721 from the supply port 711 toward the discharge port 712 of the container 710. For example, in the illustrated example, the distance d between the two first rotating plates 721 closest to the supply port 711 is smaller than the distance D between the two first rotating plates 721 closest to the discharge port 712 .

[0048] The first rotating body 720 is rotationally driven by a first rotation drive unit 740 configured by a motor or the like. Specifically, the first rotation drive unit 740 is coupled to a first rotation shaft 722 of the first rotating body 720 and drives it to rotate. As schematically shown in FIG. 4 , the first rotation drive direction of the first rotating body 720 by the first rotation drive unit 740 is, for example, a clockwise direction in the YZ plane. In this manner, when the first rotation shaft 722 is rotationally driven by the first rotation drive unit 740, the multiple first rotating plates 721 fixed thereto rotate integrally in the first rotation drive direction. The polymer PM supplied from the supply port 711 into the container 710 and directed toward the discharge port 712 is effectively agitated by the rotating multiple first rotating plates 721.

[0049] Like the first rotating body 720, the second rotating body 730 also rotates within the container 710 to agitate the polymer PM. The second rotating body 730 includes one or more second rotating plates 731 that rotate around a second rotation axis 732 in a direction (X direction perpendicular to the Z direction in the example of FIG. 3 ) that intersects the vertical direction (Z direction in the example of FIG. 3 ). As shown in FIG. 4 , the second rotating plate 731 is, for example, a disk having a circular YZ cross section. However, the shape of the YZ cross section of the second rotating plate 731 is arbitrary, and may be, for example, an ellipse or a polygon such as a triangle or a rectangle. The shape and / or size of the YZ cross section of the second rotating plate 731 may be the same as or different from the shape and / or size of the YZ cross section of the first rotating plate 721. As shown in FIG. 4 , the center or center of gravity of the second rotating plate 731 in the YZ plane preferably coincides with the center of the second rotation axis 732. In this case, one or more second rotary plates 731 and the second rotary shaft 732 are arranged coaxially.

[0050] 4 , the second rotation shaft 732 of the second rotating body 730 is disposed offset at least in the Y direction from the first rotation shaft 722 of the first rotating body 720 (it may be disposed offset in the Z direction). As a result, the first rotating plate 721 rotating around the first rotation shaft 722 does not interfere with or come into contact with the second rotation shaft 732, and the second rotating plate 731 rotating around the second rotation shaft 732 does not interfere with or come into contact with the first rotation shaft 722.

[0051] In the example of FIG. 3 , the second rotor 730 includes a plurality of second rotor plates 731 spaced apart in the axial direction (X direction) of the second rotor shaft 732. The axial distance between two adjacent second rotor plates 731 may be constant or may vary as illustrated. As will be described later, the closer to the outlet side of the container 710 (i.e., the discharge port 712 side), the higher the viscosity or degree of polymerization of the polymer PM, making it more likely for the polymer PM to adhere to the second rotor plates 731. If the spacing between the second rotor plates 731 on the outlet side of the container 710 is too small, the polymer PM adhering to each second rotor plate 731 may interfere with each other, hindering the agitation of the polymer PM and the rotation of the second rotor 730. Therefore, as illustrated, it is preferable to increase the spacing between the second rotor plates 731 from the supply port 711 toward the discharge port 712 of the container 710.

[0052] Furthermore, it is preferable that each second rotating plate 731 is provided between each first rotating plate 721, preferably at the center in the X direction of each first rotating plate 721. Similarly, it is preferable that each first rotating plate 721 (except for those at both ends in the X direction) is provided between each second rotating plate 731, preferably at the center in the X direction of each second rotating plate 731. In this case, the distance between the first rotating plate 721 and the second rotating plate 731 closest to the supply port 711 is d / 2, and the distance between the first rotating plate 721 and the second rotating plate 731 closest to the discharge port 712 is D / 2.

[0053] The second rotating body 730 is rotationally driven by a second rotation drive unit 750 configured by a motor or the like. Specifically, the second rotation drive unit 750 is coupled to a second rotation shaft 732 of the second rotating body 730 and drives it to rotate. As schematically shown in FIG. 4 , the second rotation drive direction of the second rotating body 730 by the second rotation drive unit 750 is, for example, a counterclockwise direction in the YZ plane. That is, the second rotation drive direction of the second rotating body 730 by the second rotation drive unit 750 (counterclockwise direction in FIG. 4 ) is opposite to the first rotation drive direction of the first rotating body 720 by the first rotation drive unit 740 (clockwise direction in FIG. 4 ). In this way, when the second rotation shaft 732 is rotationally driven by the second rotation drive unit 750, the multiple second rotating plates 731 fixed thereto rotate integrally in the second rotation drive direction. The polymer PM supplied from the supply port 711 into the container 710 and directed toward the discharge port 712 is effectively agitated by the rotating second rotary plates 731 .

[0054] As described above, the polymer PM supplied from the supply port 711 into the container 710 and directed toward the discharge port 712 is effectively stirred by the first rotating body 720 and the second rotating body 730, which are arranged offset at least in the Y direction as shown in FIG. 4, and by the plurality of first rotating plates 721 and the plurality of second rotating plates 731, which are arranged alternately in the X direction as shown in FIG. 3.

[0055] The gas phase above the liquid level LL of the liquid (molten) polymer PM in the container 710 is maintained in a vacuum or reduced pressure state by a vacuum device (not shown) connected to one or more exhaust ports 713 provided above the container 710. Therefore, by-products such as EG and various impurities contained in the polymer PM (e.g., PET) stirred by the first rotor 720 and the second rotor 730 are efficiently released into the gas phase in the container 710 and exhausted through the exhaust port 713. Furthermore, stirring by the first rotor 720 and the second rotor 730 also promotes the polymerization reaction of the remaining BHET into PET. As a result, the IV value, viscosity, and degree of polymerization of the polymer PM (e.g., PET) in the container 710 gradually increase from the supply port 711 toward the discharge port 712.

[0056] The height (i.e., Z-direction position) of the liquid level LL in the container 710 is arbitrary, but in order to achieve a good balance between the agitation of the polymer PM by the first rotating body 720 and the second rotating body 730, the exhaust through the gas phase and the exhaust port 713, and the detection of the adhesion position of the polymer PM on the first rotating plate 721 and / or the second rotating plate 731 by the adhesion position detection unit 760 (described later), it is preferable to set the liquid level LL at a height similar to that of the first rotating shaft 722 and / or the second rotating shaft 732 (for example, about half the height of the container 710 itself). In particular, in order to improve the efficiency and accuracy of the detection of the adhesion position by the adhesion position detection unit 760, it is preferable to set the liquid level LL lower than the first rotating shaft 722 and the second rotating shaft 732. In this case, since the first rotating shaft 722 and the second rotating shaft 732 are not immersed in the liquid polymer PM, fluctuations in the liquid level LL caused by the rotation of the first rotating shaft 722 and the second rotating shaft 732 themselves can be minimized, and excessive adhesion of the polymer PM to the first rotating plate 721 and the second rotating plate 731 can be prevented.

[0057] The adhesion position detection unit 760 shown in FIG. 4 detects the position of the polymer PM adhered to the first rotating body 720 and / or the second rotating body 730. As shown in FIG. 3, the adhesion position detection unit 760 may detect the highest position in the vertical direction (Z direction) of the polymer PM adhered to the first rotating plate 721 and / or the second rotating plate 731 above the liquid level LL (the position of height H based on the first rotating shaft 722 and / or the second rotating shaft 732). As shown in FIG. 4, the adhesion position detection unit 760 may detect the highest position in the vertical direction (Z direction) of the polymer PM adhered to the first rotating plate 721 and / or the second rotating plate 731 above the liquid level LL using light L traveling in a direction (Y direction) intersecting the vertical direction (Z direction) and the first rotating shaft 722 and / or the second rotating shaft 732 (X direction).

[0058] The adhesion position detection unit 760 in the example of FIG. 4 includes a light emitter 761 that emits light L to a Z-direction region above the liquid level LL and the first rotating shaft 722 and / or the second rotating shaft 732 and below the top of the first rotating plate 721 and / or the second rotating plate 731, and a light receiver 762 that receives the light from the light emitter 761. The light emitter 761 is provided at one end in the Y direction above the container 710 (the right end in FIG. 4 ) and emits light L, such as laser light, in the Y direction. A portion of this light L is blocked by the first rotating shaft 722 and polymer PM (see FIG. 3 ) that has adhered to the surface of the first rotating plate 721. The light receiver 762 is provided opposite the light emitter 761 at the other end in the Y direction above the container 710 (the left end in FIG. 4 ). The light receiver 762 receives the remaining light L that has not been blocked by the polymer PM, etc., that has adhered to the surface of the first rotating plate 721.

[0059] As a result, the light receiving unit 762 can detect the shape of the polymer PM adhering to the surface of the first rotating plate 721, as schematically shown in FIG. 3 . In particular, the light receiving unit 762 can detect the height H of the adhesion shape as the highest position in the vertical direction (Z direction) of the polymer PM adhering to the first rotating plate 721. Furthermore, the light receiving unit 762 may detect the thickness in the horizontal direction (X direction) of the polymer PM adhering to the surface of the first rotating plate 721 from the adhesion shape. The thickness of the polymer PM adhering to the surface of the first rotating plate 721 increases at lower positions and decreases at higher positions (the position where the thickness becomes zero is the highest position H). The light receiving unit 762 and / or an information processing unit such as a computer (not shown) at a downstream stage may record the thickness of the polymer PM at substantially all heights, may record the thickness of the polymer PM at representative heights, or may record a representative thickness value obtained by performing appropriate statistical processing on the thickness of the polymer PM at each height.

[0060] The adhesion position detection unit 760 is not limited to an optical measuring device such as a laser measuring device having a pair of a light emitting unit 761 and a light receiving unit 762, but may be configured by a camera or the like that directly photographs the polymer PM adhered to the first rotating plate 721 and / or the second rotating plate 731. The adhesion position detection unit 760 may also directly or indirectly detect the polymer PM adhered to the first rotating plate 721 and / or the second rotating plate 731 through any physical means not limited to light.

[0061] Furthermore, the adhesion shape, highest reach position H, thickness, etc. of the polymer PM detected by the light receiving unit 762 not only fluctuate over time, but may also take temporary abnormal values ​​or outliers. Therefore, it is preferable that the light receiving unit 762 and / or an information processing unit such as a computer (not shown) in a subsequent stage perform appropriate statistical processing such as moving average processing on a series of data detected over a predetermined period of time.

[0062] The adhesion shape, highest reach position H, thickness, etc. of the polymer PM on the surface of the first rotating plate 721 detected by the adhesion position detection unit 760 as described above correlate with the IV value, viscosity, and degree of polymerization of the polymer PM. For example, the higher the viscosity and degree of polymerization, the easier it is for the polymer PM to adhere to the surface of the first rotating plate 721, so the highest reach position H detectable by the adhesion position detection unit 760 becomes higher and the thickness increases. Conversely, the lower the viscosity and degree of polymerization, the harder it is for the polymer PM to adhere to the surface of the first rotating plate 721, so the highest reach position H detectable by the adhesion position detection unit 760 becomes lower and the thickness decreases. In this way, the adhesion position detection unit 760 can indirectly detect the viscosity and degree of polymerization of the polymer PM in the container 710 from the adhesion position or adhesion shape of the polymer PM on the surface of the first rotating plate 721.

[0063] The stirring mode adjustment unit 770 adjusts the stirring mode of the polymer PM in the container 710 so as to reduce the deviation of the adhesion position (e.g., highest reached position H) of the polymer PM detected by the adhesion position detection unit 760 from the desired position. The desired position here corresponds to the desired viscosity and degree of polymerization of the polymer PM in the container 710. In other words, the stirring mode adjustment unit 770 adjusts the stirring mode of the polymer PM in the container 710 so that the polymer PM in the container 710 has the desired viscosity and degree of polymerization.

[0064] Specifically, the stirring mode adjustment unit 770 adjusts the stirring mode of the polymer PM in the container 710 by adjusting at least one of the amount of polymer PM supplied into the container 710, the supply rate of polymer PM into the container 710, the amount of polymer PM discharged out of the container 710, the discharge rate of polymer PM out of the container 710, the rotation speed of the first rotating body 720 and / or the second rotating body 730, the pressure inside the container 710, and the temperature inside the container 710.

[0065] The agitation mode of the polymer PM in the container 710, such as the amount of polymer PM supplied into the container 710 and the supply rate of the polymer PM into the container 710, can be adjusted, for example, through a transfer pump 610 such as a gear pump or a screw pump connected to the supply port 711.

[0066] For example, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is higher than the desired position (or the adhesion thickness of the polymer PM is greater than the desired thickness), the polymer PM has a higher viscosity or degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 increases the amount of polymer PM supplied into the container 710 or the supply speed of the polymer PM into the container 710 through the transfer pump 610 on the supply port 711 side. As a result, the substantial residence time of the polymer PM in the container 710 is shortened, and an increase in the viscosity or degree of polymerization of the polymer PM due to excessive stirring by the first rotor 720 and / or the second rotor 730 in the container 710 is suppressed.

[0067] Conversely, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is lower than the desired position (or the adhesion thickness of the polymer PM is smaller than the desired thickness), the polymer PM has a lower viscosity and a lower degree of polymerization than the desired one. Therefore, the stirring mode adjustment unit 770 reduces the amount of polymer PM supplied into the container 710 and the supply speed of the polymer PM into the container 710 through the transfer pump 610 on the supply port 711 side. As a result, the substantial residence time of the polymer PM in the container 710 becomes longer, and the viscosity and degree of polymerization of the polymer PM are increased through sufficient stirring by the first rotor 720 and / or the second rotor 730 in the container 710.

[0068] The stirring mode of the polymer PM in the container 710, the amount of polymer PM discharged outside the container 710, and the discharge rate of the polymer PM outside the container 710 can be adjusted, for example, through a transfer pump 610 such as a gear pump or a screw pump connected to the discharge port 712.

[0069] For example, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is higher than the desired position (or the adhesion thickness of the polymer PM is greater than the desired thickness), the polymer PM has a higher viscosity or degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 increases the amount of polymer PM discharged out of the container 710 and the discharge rate of the polymer PM out of the container 710 through the transfer pump 610 on the discharge port 712 side. As a result, the substantial residence time of the polymer PM in the container 710 is shortened, and an increase in the viscosity and degree of polymerization of the polymer PM due to excessive stirring by the first rotor 720 and / or the second rotor 730 in the container 710 is suppressed.

[0070] Conversely, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is lower than the desired position (or the adhesion thickness of the polymer PM is smaller than the desired thickness), the polymer PM has a lower viscosity and a lower degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 reduces the amount of polymer PM discharged out of the container 710 and the discharge rate of the polymer PM out of the container 710 through the transfer pump 610 on the discharge port 712 side. As a result, the substantial residence time of the polymer PM in the container 710 is lengthened, and the viscosity and degree of polymerization of the polymer PM are increased through sufficient stirring by the first rotor 720 and / or the second rotor 730 in the container 710.

[0071] Note that changing only one of the supply amount / supply rate of polymer PM into container 710 and the discharge amount / discharge rate of polymer PM out of container 710 changes the total amount of polymer PM in container 710. Therefore, in order to suppress changes in the total amount of polymer PM in container 710, it is preferable that the transfer pump 610 connected to the supply port 711 and the transfer pump 610 connected to the discharge port 712 adjust the supply amount / supply rate and the discharge amount / discharge rate in synchronization with each other. For example, when the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is higher (or lower) than the desired position, the agitation mode adjustment unit 770 simultaneously increases (or simultaneously decreases) the supply amount / supply rate and the discharge amount / discharge rate.

[0072] The rotation speed of the first rotor 720 and / or the second rotor 730, which is the agitation mode of the polymer PM in the container 710, can be adjusted, for example, via the first rotation drive unit 740 and / or the second rotation drive unit 750. The relationship between the rotation speed of the first rotor 720 and / or the second rotor 730 and the viscosity or degree of polymerization of the polymer PM indirectly detected by the deposition position detection unit 760 may not be a simple positive or negative correlation, and therefore it is preferable to grasp this relationship in advance through tests using the actual polymer agitation device 700, for example.

[0073] In addition, if the relationship between the rotation speed of the first rotating body 720 and / or the second rotating body 730 and the viscosity and degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 is a simple positive correlation, when the viscosity and degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 are higher than the desired value, the stirring mode adjustment unit 770 reduces the rotation speed of the first rotating body 720 and / or the second rotating body 730, and when the viscosity and degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 are lower than the desired value, the stirring mode adjustment unit 770 increases the rotation speed of the first rotating body 720 and / or the second rotating body 730.

[0074] Furthermore, if the relationship between the rotation speed of the first rotating body 720 and / or the second rotating body 730 and the viscosity or degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 is a simple negative correlation, when the viscosity or degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 is higher than the desired value, the stirring mode adjustment unit 770 increases the rotation speed of the first rotating body 720 and / or the second rotating body 730, and when the viscosity or degree of polymerization of the polymer PM indirectly detected by the adhesion position detection unit 760 is lower than the desired value, the stirring mode adjustment unit 770 decreases the rotation speed of the first rotating body 720 and / or the second rotating body 730.

[0075] The pressure inside the container 710 as a stirring state of the polymer PM inside the container 710 can be adjusted, for example, through a vacuum device connected to the exhaust port 713 .

[0076] For example, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is higher than the desired position (or the adhesion thickness of the polymer PM is greater than the desired thickness), the polymer PM has a higher viscosity or degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 increases the pressure inside the container 710 (decreases the degree of vacuum) through the vacuum device connected to the exhaust port 713. As a result, the gas phase inside the container 710 and the exhaust through the exhaust port 713 are weakened, and an excessive increase in the purity of the polymer PM (i.e., IV value, viscosity, degree of polymerization, etc.) is avoided.

[0077] Conversely, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is lower than the desired position (or the adhesion thickness of the polymer PM is smaller than the desired thickness), the polymer PM has a lower viscosity or degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 lowers the pressure inside the container 710 (increases the degree of vacuum) through a vacuum device connected to the exhaust port 713. As a result, the gas phase inside the container 710 and the exhaust through the exhaust port 713 are strengthened, and the purity of the polymer PM (i.e., IV value, viscosity, degree of polymerization, etc.) is increased.

[0078] The temperature inside the container 710 as a stirring state of the polymer PM inside the container 710 can be adjusted, for example, by a temperature adjusting device (not shown) built into the container 710 .

[0079] For example, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is higher than the desired position (or if the adhesion thickness of the polymer PM is greater than the desired thickness), the polymer PM has a higher viscosity or degree of polymerization than desired. Therefore, the stirring mode adjustment unit 770 lowers the temperature inside the container 710 via the temperature control device. As a result, the release of impurities from the polymer PM into the gas phase of the container 710 and the polymerization reaction of BHET remaining in the polymer PM with PET are suppressed, thereby preventing an excessive increase in the purity of the polymer PM (i.e., IV value, viscosity, degree of polymerization, etc.).

[0080] Conversely, if the highest reach position H of the polymer PM detected by the adhesion position detection unit 760 is lower than the desired position (or the adhesion thickness of the polymer PM is smaller than the desired thickness), the polymer PM has a lower viscosity and degree of polymerization than the desired one. Therefore, the stirring mode adjustment unit 770 raises the temperature inside the container 710 through the temperature control device. As a result, the release of impurities from the polymer PM into the gas phase of the container 710 and the polymerization reaction of BHET and other components remaining in the polymer PM into PET and other components are promoted, thereby increasing the purity of the polymer PM (i.e., the IV value, viscosity, degree of polymerization, etc.).

[0081] In order to effectively adjust the agitation mode of the polymer PM by the agitation mode adjustment unit 770 as described above, it is preferable that the adhesion position detection unit 760 detects the highest vertical position H of the polymer PM adhered to the rotating plate (the first rotating plate 721, the last one in the example of FIG. 3 ) closest to the discharge outlet 712 of the container 710 among the multiple rotating plates 721, 731. This adhesion position detection unit 760 can indirectly detect the viscosity and degree of polymerization of the polymer PM immediately before it is supplied to the injection molding machine 1 from the discharge outlet 712, and the desired viscosity and degree of polymerization can be achieved through adjustment of the agitation mode by the agitation mode adjustment unit 770. The positions and number of the rotating plates 721, 731 at which the adhesion position detection unit 760 detects adhesion of the polymer PM are arbitrary. For example, the adhesion position detection unit 760 may detect the second rotating plate 731 closest to the discharge outlet 712 of the container 710, or may detect one or more rotating plates 721, 731 at any position.

[0082] In addition, instead of automatically adjusting the stirring mode of the polymer PM by the stirring mode adjustment unit 770 as described above, a manager (person) who is presented with the adhesion position of the polymer PM detected by the adhesion position detection unit 760 may manually adjust the stirring mode of the polymer PM.

[0083] In addition to the adhesion position detection unit 760 that indirectly detects the degree of polymerization of the polymer PM, a polymerization degree estimation unit 780 may be provided that estimates the degree of polymerization of the polymer PM based on the adhesion position of the polymer PM detected by the adhesion position detection unit 760. In this case, the stirring mode adjustment unit 770 adjusts the stirring mode of the polymer PM in the container 710 so that the deviation of the degree of polymerization of the polymer PM estimated by the polymerization degree estimation unit 780 from the desired value becomes small.

[0084] The present disclosure has been described above based on the embodiments. Various modifications are possible to the combinations of the components and processes in the exemplary embodiments, and it will be obvious to those skilled in the art that such modifications are included within the scope of the present disclosure.

[0085] In the example of Fig. 1, only one of each of the polymer adjustment apparatus 200, depolymerization reaction tank 300, polymerization reaction tank 400, by-product removal apparatus 500, polymer supply unit 600, etc. is provided, but a plurality of each may be provided. Such a plurality of treatment units can perform equivalent treatments in parallel, thereby improving the treatment performance of the treatment unit group. Furthermore, the difference in treatment speed or reaction rate between treatment units can be reduced by increasing the number of slower treatment units.

[0086] Furthermore, one or more processing units may accept external materials procured from a location or facility different from the chemical recycle molding system shown in FIG. 1 , instead of or in addition to materials from the preceding processing unit. For example, when multiple polymerization reaction tanks 400 are provided, some of them may be supplied with depolymerized polymer from the depolymerization reaction tank 300, and the remaining units may be supplied with externally procured depolymerized polymer (synonymous with depolymerized polymer supplied from the depolymerization reaction tank 300A, described below). Similarly, when multiple by-product removal devices 500 and / or polymer supply units 600 are provided, some of them may be supplied with polymer from the polymerization reaction tank 400, and the remaining units may be supplied with externally procured polymer (synonymous with polymer supplied from the polymer supply unit 400A, described below). In this way, by allowing the acceptance of external materials at each stage of processing in the chemical recycle molding system, the chemical recycle molding system can be operated flexibly and efficiently.

[0087] Figure 5 shows a first modified example of the chemical recycle molding system. Components similar to those in Figure 1 are designated by the same reference numerals, and redundant explanations will be omitted. In this modified example, a depolymerization supply unit 300A is provided instead of the depolymerization reaction tank 300 and the like in Figure 1. The depolymerization supply unit 300A supplies depolymerized materials such as BHET derived from a first molded product decomposed in a depolymerization reaction tank 300 (not shown) installed in a location or facility different from the chemical recycle molding system shown in the figure to a polymerization reaction tank 400.

[0088] A first preheater 371 for heating or preheating the depolymerized polymer, such as BHET, supplied from the depolymerized polymer supply unit 300A to a molten state may be provided downstream of the depolymerization supply unit 300A and upstream of the polymerization reaction tank 400. The first preheater 371 may maintain the depolymerized polymer at a temperature (between 220°C and 250°C) similar to that of the heater 320 provided in the depolymerization reaction tank 300 shown in FIG. 1 , or may maintain the depolymerized polymer at a temperature suitable for the polymerization reaction (between 250°C and 300°C) similar to that of the heater 410 provided in the polymerization reaction tank 400.

[0089] EG, a by-product obtained together with PET as the main product in the polymerization reaction tank 400 and / or the by-product removal device 500, may be stored in the EG storage unit 530. The EG stored in the EG storage unit 530 may be used for other purposes in other locations or facilities, or may be sold to consumers.

[0090] In the first modified example described above, the polymer resynthesized in the polymerization reaction tank 400 is not made into flakes or pellets, but is supplied as is by the polymer supply unit 600 to the injection molding machine 1. Since the cooling and heating processes for flakes and pellets that are conventionally required are no longer necessary, molded products such as PET bottles can be recycled with less energy than conventional methods.

[0091] In the chemical recycling apparatus 100 according to the first modification, the polymer resynthesized in the polymerization reaction tank 400 is directly supplied to the injection molding machine 1, so it is necessary to quickly achieve the IV value of the polymer required for the molded product (second molded product). In this modification, a by-product removal device 500 and / or a polymer supply section 600, which have the function of accelerating the polymerization reaction and increasing the IV value of the polymer, are provided in addition to the polymerization reaction tank 400, so this requirement can be fully met.

[0092] Figure 6 shows a second modified example of the chemical recycle molding system. Components similar to those in Figures 1 and / or 5 are designated by the same reference numerals, and redundant explanations will be omitted. In this modified example, a polymer supply unit 400A is provided in place of the depolymerization reaction tank 300 and the polymerization reaction tank 400 shown in Figure 1. The polymer supply unit 400A supplies a polymer, such as PET, derived from a first molded product synthesized in a polymerization reaction tank 400 (not shown), which is installed in a location or facility different from the illustrated chemical recycle molding system, to a by-product removal device 500 and / or a polymer supply unit 600.

[0093] A second preheater 431 for heating or preheating the polymer such as PET supplied from the polymer supply section 400A to a molten state may be provided downstream of the polymer supply section 400A and upstream of the by-product removal apparatus 500 and / or the polymer supply section 600. The second preheater 431 may maintain the polymer at a temperature (between 250°C and 300°C) similar to that of the heater 410 provided in the polymerization reaction tank 400 shown in FIG. 1 or 5 , or may maintain the polymer at a temperature suitable for polymerization (between 250°C and 290°C) similar to that of the heater 520 provided in the by-product removal apparatus 500, or may maintain the polymer at a temperature (between 250°C and 290°C) similar to that of the heater 620 provided in the polymer supply section 600.

[0094] The EG obtained together with the PET in the by-product removal device 500 may be stored in the EG storage unit 530. The EG stored in the EG storage unit 530 may be used for other purposes in other locations or facilities, or may be sold to consumers.

[0095] In the chemical recycling apparatus 100 according to the second modification, the polymer supplied from the polymer supply section 400A is directly supplied to the injection molding machine 1, so it is necessary to quickly achieve the IV value of the polymer required for the molded product (second molded product). This modification satisfies such a requirement by providing the by-product removal device 500 and / or the polymer supply section 600, which have the function of promoting the polymerization reaction and increasing the IV value of the polymer.

[0096] The configuration, operation, and function of each device and method described in the embodiments can be realized by hardware resources, software resources, or a combination of hardware and software resources. Examples of hardware resources include processors, ROM, RAM, and various integrated circuits. Examples of software resources include operating systems, applications, and other programs.

[0097] The present disclosure relates to polymer agitation devices and the like.

[0098] DESCRIPTION OF SYMBOLS 1 Injection molding machine, 100 Chemical recycling device, 200 Polymer adjustment device, 300 Depolymerization reaction tank, 400 Polymerization reaction tank, 500 By-product removal device, 600 Polymer supply unit, 700 Polymer stirring device, 710 Container, 711 Supply port, 712 Discharge port, 720 First rotating body, 721 First rotating plate, 722 First rotating shaft, 730 Second rotating body, 731 Second rotating plate, 732 Second rotating shaft, 760 Adhesion position detection unit, 761 Light-emitting unit, 762 Light-receiving unit, 770 Stirring mode adjustment unit.

Claims

1. A polymer stirring device comprising: a container to which a polymer is supplied; a rotor that rotates within the container to stir the polymer; and an adhesion position detection unit that detects the position of the polymer adhered to the rotor.

2. The polymer mixing device according to claim 1, wherein the adhesion position detection unit detects the highest vertical position reached by the polymer adhered to the rotating body.

3. The polymer mixing device described in claim 2, wherein the rotating body comprises a rotating plate that rotates around a rotation axis that is in a direction intersecting the vertical direction, and the adhesion position detection unit detects the highest position in the vertical direction reached by the polymer adhered to the rotating plate.

4. A polymer mixing device as described in claim 3, wherein the adhesion position detection unit detects the highest vertical position reached by the polymer adhered to the rotating plate through light traveling vertically and in a direction intersecting the rotation axis.

5. The polymer mixing device described in claim 3, wherein the container has an outlet through which the polymer is discharged, the rotating body has a plurality of rotating plates which rotate around the rotation axis, and the adhesion position detection unit detects the highest vertical position reached by the polymer adhered to the rotating plate among the plurality of rotating plates which is closest to the discharge outlet.

6. The polymer stirring device described in claim 3, wherein the rotating shaft comprises a first rotating shaft and a second rotating shaft, the rotating plate comprises a first rotating plate that rotates around the first rotating shaft and a second rotating plate that rotates around the second rotating shaft, and the adhesion position detection unit detects the highest vertical position reached by the polymer adhered to at least one of the first rotating plate and the second rotating plate.

7. A polymer mixing device as described in any one of claims 1 to 6, wherein the adhesion position detection unit detects the position of the polymer adhered to the rotating body above the liquid surface of the polymer in the container.

8. A polymer stirring device as described in any one of claims 1 to 6, comprising an agitation mode adjustment unit that adjusts the agitation mode of the polymer in the container so as to reduce the deviation of the adhesion position of the polymer detected by the adhesion position detection unit from a desired position.

9. The polymer stirring device described in claim 8, wherein the stirring mode adjustment unit adjusts at least one of the following as the stirring mode of the polymer in the container: the amount of the polymer supplied into the container, the rate at which the polymer is supplied into the container, the amount of the polymer discharged outside the container, the rate at which the polymer is discharged outside the container, the rotation speed of the rotor, the pressure inside the container, and the temperature inside the container.

10. A polymer stirring device as described in any one of claims 1 to 6, comprising a polymerization degree estimation unit that estimates the polymerization degree of the polymer based on the adhesion position of the polymer detected by the adhesion position detection unit.

11. A polymer mixing device as described in any one of claims 1 to 6, wherein the adhesion position detection unit detects the horizontal thickness of the polymer adhered to the rotating body.

12. A polymer mixing device according to any one of claims 1 to 6, wherein the polymer is polyethylene terephthalate.

13. A recycling system comprising: a polymer supplying device for supplying a polymer derived from a first molded product; and a polymer stirring device for stirring the polymer and supplying it to a molding machine that molds a second molded product, wherein the polymer stirring device comprises: a container to which the polymer is supplied; a rotating body that rotates within the container to stir the polymer; and an adhesion position detection unit that detects the position of the polymer adhered to the rotating body.

Citation Information

Patent Citations

  • Polymerization apparatus

    JP1985035001A

  • Reactor for producing polymeric substance

    JP1996259700A

  • Method for producing side-chain crystalline polyolefin powder

    JP2011157468A

  • Process for the regeneration of polyester by reactor addition.

    JP2022528286A

  • Fine powder of mixed plastics and process for producing the same

    WO2007026918A1