Resin composition and molded article
The compatibility of polypropylene and polymethylpentene with long chain branched structures in a specific mass ratio enhances the processability and moldability of resin compositions, resulting in improved resin articles with enhanced properties for diverse applications.
Patent Information
- Application Number
- PCT/JP2024/012178
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-27
- Publication Date
- 2024-10-03
AI Technical Summary
Polyethylene, polypropylene, and polymethylpentene are incompatible, making it difficult to pelletize and mold resin compositions containing these materials, which hinders their processability and moldability.
A resin composition comprising polypropylene and polymethylpentene with long chain branched structures, where the mass ratio can range from 99:1 to 50:50, and the content of long chain branched structures is optimized to improve compatibility and processability, allowing for the formation of pellets and molded articles like fibers and nonwoven fabrics.
The resin composition achieves excellent processability and moldability, enabling the production of pellets and molded articles with improved water repellency, non-adhesiveness, bulkiness, rigidity, and heat resistance, suitable for various applications such as dust collection and insulation.
Smart Images

Figure 000001 
Figure 000002 
Figure 000003
Abstract
Description
Resin composition and molded body
[0001] The present invention relates to a resin composition and a molded article.
[0002] Polyolefin resins, which have properties such as electrical properties, hydrophobicity, and light weight, have been used in various applications. Common polyolefin resins include aliphatic polyolefins such as polyethylene, polypropylene, and polymethylpentene. Among these, polymer blends and polymer alloys are known to exhibit properties that cannot be achieved by each resin alone (see, for example, Patent Document 1).
[0003] Japanese Patent Application Publication No. 07-070384
[0004] However, polyethylene, polypropylene, and polymethylpentene are incompatible with one another, making it extremely difficult to pelletize a resin composition obtained by mixing these materials, or to mold the resin composition.
[0005] In view of the above problems, the present invention aims to improve the processability and moldability of a resin composition containing a polyolefin resin.
[0006] As a result of extensive research, the present inventors have found that an excellent composition and molded article can be obtained by the following configuration [1]. The resin composition and molded article according to the present invention are preferably any of the following [2] to
[13] . [1] A resin composition comprising polypropylene and polymethylpentene, wherein the polypropylene comprises polypropylene having long chain branches, and the polymethylpentene comprises polymethylpentene having long chain branches, the mixture being formed from these. [2] The resin composition according to [1], wherein the polypropylene having long chain branches has a carbon number of 8 or more, and the polymethylpentene having long chain branches has a carbon number of 8 to 18. [3] The resin composition according to [1] or [2], wherein the polypropylene further comprises polypropylene without long chain branches. [4] The resin composition according to any of [1] to [3], wherein the mass ratio of the polypropylene to the polymethylpentene is 99:1 to 50:50. [5] The resin composition according to any one of [1] to [3], wherein the mass ratio of the polypropylene to the polymethylpentene is 99:1 to 80:20. [6] The resin composition according to [1], [2], [4], or [5], wherein the polypropylene comprises the polypropylene having long chain branches. [7] The resin composition according to any one of [1] to [6], wherein the polymethylpentene comprises the polymethylpentene having long chain branches. [8] The resin composition according to any one of [1] to [7], wherein the content of the polypropylene having long chain branches is 1 to 60 mass%, and the content of the polymethylpentene having long chain branches is 5 to 60 mass%. [9] The resin composition according to any one of [1] to [8], wherein the content (mass%) of the polymethylpentene having long chain branches is greater than the content (mass%) of the polypropylene having long chain branches.
[10] The resin composition according to any one of [3] to [5] and [7] to [9], wherein the content (% by mass) of the polypropylene having no long chain branches is greater than the content (% by mass) of the polypropylene having long chain branches.
[11] The resin composition according to any one of [2] to
[10] , wherein the number of carbon atoms in the long-chain branches of the long-chain branched polypropylene is 0.50 times or less, 0.40 times or less, 0.30 times or less, 0.20 times or less, or 0.10 times or less the number of carbon atoms in the main chain.
[12] A molded article containing the resin composition according to any one of [1] to
[11] .
[13] The molded article according to
[12] , which is a fiber or a nonwoven fabric.
[14] The molded article according to
[13] , wherein the nonwoven fabric is a meltblown nonwoven fabric or a spunbonded nonwoven fabric.
[0007] According to the present invention, a resin composition having excellent processability and a molded article using the same can be obtained.
[0008] The resin composition and molded body according to the embodiment of the present invention will be described in detail below, but the present invention is not limited to the following, and the optimum configuration can be selected for each application in accordance with the spirit of the present invention.
[0009] The resin composition according to the embodiment contains polypropylene and polymethylpentene, the polypropylene containing polypropylene having a long-chain branched structure (hereinafter, also referred to as long-chain branched polypropylene), and the polymethylpentene containing polymethylpentene having a long-chain branched structure (hereinafter, also referred to as long-chain branched polymethylpentene), and these are mixed together.
[0010] The resin composition preferably contains polyolefin as a main component, and the proportion of polyolefin in the resin composition is preferably 90% by mass or more, more preferably 95% by mass or more, and even more preferably 97% by mass or more. On the other hand, the proportion of polyolefin in the resin composition is preferably 100% by mass or less, and may be 99% by mass or less.
[0011] In the resin composition, the ratio of polypropylene to polymethylpentene can be used in a preferred range of 99:1 to 1:99 by mass depending on the required properties. More preferably, it is 99:1 to 50:50, even more preferably 99:1 to 70:30, and most preferably 99:1 to 80:20. By using such a range, a preferred composition having the properties of both polypropylene and polymethylpentene can be obtained. It is preferable that the continuous phase side is polypropylene.
[0012] The polypropylene contains long-chain branched polypropylene. The proportion of long-chain branched polypropylene in 100% by mass of polypropylene is preferably 1% by mass or more, more preferably 5% by mass or more, and even more preferably 10% by mass or more. It is also preferable that the entire polypropylene contains long-chain branches.
[0013] The polymethylpentene includes long-chain branched polymethylpentene. The proportion of long-chain branched polymethylpentene in 100% by mass of polymethylpentene is preferably 1% by mass or more, more preferably 5% by mass or more, and even more preferably 10% by mass or more, and it is also preferable that the entire polymethylpentene has long-chain branches. The presence of long-chain branches in each component provides good processability due to the compatibility of the components and entanglement of molecular chains.
[0014] The long-chain branched polyolefin, i.e., the long-chain branched polypropylene and the long-chain branched polymethylpentene, is not particularly limited as long as it can provide desired properties, and can be preferably obtained by a method of irradiating each or a mixture of polypropylene and polymethylpentene with high energy such as electron beams or radiation, a method of copolymerizing an α-olefin having 10 or more carbon atoms, a method of grafting a long-chain peroxide, a method of grafting a peroxide and an α-olefin in combination, or the like.
[0015] Among these, the method of introducing long-chain branches during polymerization is preferred, as this method results in a resin with excellent fluidity and stretchability due to the absence of an irregular crosslinked structure. In this case, the long-chain branched polypropylene preferably contains 80 to 99.9 mass% of structural units derived from propylene, more preferably 90 to 99.5 mass%, and even more preferably 95 to 99.0 mass%. Furthermore, the long-chain branched polymethylpentene preferably contains 80 to 99.9 mass% of structural units derived from 4-methyl-1-pentene, more preferably 90 to 99.5 mass%, and even more preferably 95 to 99.0 mass%.
[0016] Furthermore, the component copolymerized to introduce long chain branches is preferably an α-olefin having 10 or more carbon atoms or an α-olefin having 10 to 20 carbon atoms, such as 1-decene, 1-dodecene, 1-tetradecene, 1-hexadecene, 1-octadecene, 1-eicosene, etc. It is preferable to form long chain branched polypropylene or long chain branched polymethylpentene by using not only one but two or more of these copolymerization components with propylene or methylpentene.
[0017] The carbon number of the long-chain branch of the long-chain branched polypropylene is preferably 8 or more, more preferably 10 or more, and even more preferably 21 or more. The carbon number of the long-chain branch of the long-chain branched polypropylene may be 0.50 or less, 0.40 or less, 0.30 or less, 0.20 or less, or 0.10 or less times the number of carbon atoms in the main chain. Furthermore, the carbon number of the long-chain branch of the long-chain branched polymethylpentene is preferably 8 to 18. This improves pelletizing processability. The carbon number of the long-chain branch is the number of carbon atoms per branch.
[0018] The content of the long-chain branched polypropylene in 100% by mass of the resin composition is preferably 1 to 60% by mass, more preferably 3 to 55% by mass. The content of the long-chain branched polymethylpentene in 100% by mass of the resin composition is preferably 5 to 60% by mass, more preferably 10 to 55% by mass. Since long-chain branched polymethylpentene and long-chain branched polypropylene are easily miscible with each other, the polymethylpentene becomes more miscible with polypropylene when the resin composition contains a certain amount of these.
[0019] The melt flow rate (MFR) of the long-chain branched polymethylpentene is preferably 80 to 200 g / 10 min, more preferably 100 to 180 g / 10 min. The melt flow rate (MFR) of the long-chain branched polypropylene is preferably 1 to 20 g / 10 min, more preferably 5 to 10 g / 10 min. This makes the polymethylpentene and polypropylene more compatible. The MFR can be measured by the method described in JIS K7210.
[0020] The content (mass %) of long-chain branched polymethylpentene is preferably greater than or equal to the content (mass %) of long-chain branched polypropylene, and more preferably greater than the content (mass %) of long-chain branched polypropylene. This makes the polymethylpentene more compatible with polypropylene. The content of long-chain branched polymethylpentene is preferably 1.0 to 10.0 times, more preferably 1.5 to 8.0 times, and even more preferably 2.0 to 5.0 times the content of long-chain branched polypropylene.
[0021] The polypropylene is preferably a long-chain branched polypropylene. That is, the resin composition preferably contains a long-chain branched polypropylene and does not contain a polypropylene that does not have a long-chain branched structure. This improves pelletizing processability and spunbonding processability.
[0022] On the other hand, the polypropylene preferably contains both long-chain branched polypropylene and polypropylene without a long-chain branching structure. This improves melt-blowing processability. In this case, the content of the polypropylene without a long-chain branching structure is preferably 40 to 90% by mass, more preferably 60 to 85% by mass, based on 100% by mass of the resin composition. Furthermore, the content of the long-chain branched polypropylene is preferably 1 to 20% by mass, more preferably 2 to 10% by mass, based on 100% by mass of the resin composition.
[0023] The content (mass%) of polypropylene having no long-chain branching structure is preferably greater than the content (mass%) of long-chain branched polypropylene. This further improves melt-blowing processability. The content of polypropylene having no long-chain branching structure is preferably 2 to 30 times, more preferably 8 to 25 times, and even more preferably 10 to 20 times the content of long-chain branched polypropylene.
[0024] The polymethylpentene is preferably a long-chain branched polymethylpentene. That is, the resin composition preferably contains long-chain branched polymethylpentene and does not contain polymethylpentene that does not have a long-chain branched structure. This makes the polymethylpentene more compatible with polypropylene.
[0025] The resin composition preferably contains various compounding agents as functional materials, and may contain various antioxidants, light resistance agents, charge enhancers, antistatic agents, pigments, antibacterial agents, fillers, lubricants, etc.
[0026] The resin composition can be molded into various shapes as needed and used as a molded body. Examples of molded bodies include, but are not limited to, fibers and nonwoven fabrics. A typical melt spinning method can be used to mold fibers. After spinning the fibers, nonwoven fabrics can be molded into nonwoven fabrics by direct methods such as spunbonding and meltblowing. The resin composition provides good mixing and strand stability during the pelletizing process using a twin-screw extruder, and is less likely to separate the mixed resins during spinning in a single-screw extruder with low shear capacity. Furthermore, improved compatibility allows the individual resins to be supplied as pellets and directly mixed in a single-screw extruder.
[0027] Examples of molded articles using the resin composition include fibers and nonwoven fabrics. Molded articles containing the resin composition are superior in water repellency, non-stickiness, bulkiness, rigidity, and heat resistance to those made of polypropylene alone, and superior in strength and moldability to those made of polymethylpentene alone. Therefore, fibers and nonwoven fabrics obtained from the resin composition can be widely used as functional materials for dust collection, protection, ventilation, stain resistance, waterproofing, insulation, sound absorption, etc. The resin composition may also be molded into objects other than fibers and nonwoven fabrics. The basis weight of the molded article is 10 to 50 g / m 2 is preferred, and 20 to 40 g / m 2 The fiber diameter of the fibers in the molded body is preferably 1 to 100 μm, and more preferably 2 to 40 μm.
[0028] This application claims the benefit of priority based on Japanese Patent Application No. 2023-053418, filed on March 29, 2023. The entire content of the specification of Japanese Patent Application No. 2023-053418, filed on March 29, 2023, is incorporated herein by reference.
[0029] Examples of the present invention will be described below, but the present invention is not limited to the following. In the examples and comparative examples, the following polymethylpentenes and polypropylenes were used. (Polymethylpentene) Long-chain branched polymethylpentene A: 98.5% by mass of methylpentene, 1.5% by mass of decene, MFR 180 Long-chain branched polymethylpentene B: 97.5% by mass of methylpentene, 2.5% by mass of octadecene, MFR 100 (Polypropylene) Polypropylene A ("S119", manufactured by Prime Polymer Co., Ltd.): 100% by mass of propylene, MFR 60 Polypropylene B ("HP461Y", manufactured by Polymiley Co., Ltd.): 100% by mass of propylene, MFR 1300 Long-chain branched polypropylene C ("MFX3", manufactured by Japan Polypropylene Corporation): 100% long-chain branched polypropylene, MFR 8
[0030] Example 1 Long-chain branched polymethylpentene A and long-chain branched polypropylene C were mixed in a mass ratio of 50:50 and melt-mixed at 250°C using a twin-screw extruder. The molten resin composition was then extruded from a nozzle under nitrogen pressure into strands, which were then immersed in cooling water in a water tank and cut at intervals of approximately 5 mm using a strand cutter. As a result, roughly cylindrical pellets with a diameter of approximately 3.5 mm and a length of approximately 5 mm were obtained. Thus, pellets were obtained without any problems in Example 1, and pelletization processability was good.
[0031] Furthermore, the pellets obtained were used to form a nonwoven fabric by a spunbond method using a single-screw extruder, resulting in a basis weight of 30 g / m 2 The appearance of the long-fiber nonwoven fabric was satisfactory, and the spunbonding processability was good.
[0032] Example 2 Long-chain branched polymethylpentene B, polypropylene B, and long-chain branched polypropylene C were mixed in a mass ratio of 15:80:5 and melt-mixed at 250°C using a twin-screw extruder. Subsequently, pelletizing was performed in the same manner as in Example 1, resulting in roughly cylindrical pellets with a diameter of about 3 mm and a length of about 5 mm. Thus, pellets were obtained without any problems in Example 2, and pelletizing processability was good.
[0033] The pellets were then melt-blown using a single-screw extruder to form a nonwoven fabric with a basis weight of 30 g / m. 2 The appearance of the long-fiber nonwoven fabric was satisfactory, and the melt-blowing processability was good.
[0034] Comparative Example 1 Long-chain branched polymethylpentene A and polypropylene A were mixed in a mass ratio of 50:50 and melt-mixed using a twin-screw extruder at 250° C. Pelletization was performed in the same manner as in Example 1, but sagging strands and thread breakage occurred during pelletizing, making processing difficult.
[0035] Comparative Example 2 Long-chain branched polymethylpentene A and polypropylene B were mixed in a mass ratio of 50:50 and melt-mixed using a twin-screw extruder at 250° C. Pelletization was performed in the same manner as in Example 1, but the molten resin sagged significantly, making pelletization impossible.
[0036] Examples 1 and 2 and Comparative Examples 1 and 2 show that the resin composition obtained by mixing polypropylene having a long chain branching structure and polymethylpentene having a long chain branching structure has excellent processability and moldability.
[0037] The present invention can provide a resin composition having excellent processability and a molded article using the same, and therefore can make a great contribution to industry.
Claims
1. A resin composition comprising a mixture of polypropylene and polymethylpentene, wherein the polypropylene comprises a polypropylene having a long chain branching structure, and the polymethylpentene comprises a polymethylpentene having a long chain branching structure.
2. The resin composition according to claim 1, wherein the polypropylene having a structure with long chain branches has 8 or more carbon atoms in its long chain branches, and the polymethylpentene having a structure with long chain branches has 8 to 18 carbon atoms in its long chain branches.
3. The resin composition according to claim 1 or 2, wherein the polypropylene further comprises a polypropylene having no long chain branching structure.
4. A resin composition according to claim 1 or 2, wherein the mass ratio of said polypropylene to said polymethylpentene is 99:1 to 50:
50.
5. A resin composition according to claim 1 or 2, wherein the mass ratio of said polypropylene to said polymethylpentene is 99:1 to 80:
20.
6. The resin composition according to claim 1 or 2, wherein the polypropylene comprises the polypropylene having the long chain branched structure.
7. A resin composition according to claim 1 or 2, wherein the polymethylpentene comprises polymethylpentene having a long chain branched structure.
8. The resin composition according to claim 1 or 2, wherein the content of the polypropylene having a long chain branching structure is 1 to 60 mass %, and the content of the polymethylpentene having a long chain branching structure is 5 to 60 mass %.
9. The resin composition according to claim 8, wherein the content (mass %) of the polymethylpentene having a structure with long chain branches is greater than the content (mass %) of the polypropylene having a structure with long chain branches.
10. The resin composition according to claim 3, wherein the content (mass %) of the polypropylene not having a structure with long chain branches is greater than the content (mass %) of the polypropylene having a structure with long chain branches.
11. A molded article containing the resin composition according to claim 1 or 2.
12. The molded article according to claim 11, which is a fiber or nonwoven fabric.
13. The molded body according to claim 12, wherein the nonwoven fabric is a meltblown nonwoven fabric or a spunbonded nonwoven fabric.
Citation Information
Patent Citations
Polypropylene film for capacitor and capacitor composed the film
JP2006093689A
Thermoplastic elastomer composition and its laminated molding
JP2006274119A
Thermoplastic elastomer composition and method for producing it
JP2009161721A
Olefinic resin composition for foam-molding and foam
JP2011089140A
Packaging wrapping film
JP2017141047A