Ai-vision based method for automatically welding large steel mesh

Through the collaborative work of AI vision technology and industrial computers, the problem of automatic welding difficulties caused by irregular large-scale steel mesh and uneven gaps has been solved, and efficient and stable welding effects have been achieved, which is suitable for welding under extreme conditions.

WO2024213186A1PCT designated stage expired Publication Date: 2024-10-17CHINA CONSTR FIFTH ENG DIV CORP LTD

Patent Information

Application Number
PCT/CN2024/099140
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-11-27
Filing Date
2024-06-14
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

Due to the irregularity and uneven gaps of large steel mesh, automatic welding is difficult. Existing mechanical automatic welding technology is difficult to effectively weld under extreme conditions such as high temperature and high pressure.

Method used

An automatic welding method for large steel mesh based on AI vision is adopted. Through the work platform and industrial computer, the first vision device is used to continuously take pictures to generate a physical 3D model. The starting point position of the weld is adjusted based on the preset gap value to ensure that the welding gun is always perpendicular to the plane of the steel bar. , achieve precise welding.

Benefits of technology

It improves the quality and efficiency of steel mesh welding, ensures the stability and continuity of the welding process, and is suitable for welding under extreme conditions such as high temperature and high pressure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024099140_17102024_PF_FP_ABST
    Figure CN2024099140_17102024_PF_FP_ABST
Patent Text Reader

Abstract

An AI-vision based method for automatically welding a large steel mesh. A working platform and an industrial personal computer are involved. The working platform comprises a guide rail and a carriage moving along the guide rail, wherein a support arm is rotatably arranged on the carriage, a robot is slidably arranged on the support arm, the robot is provided with a welding gun and a second vision device, and the support arm is provided with a first vision device. The working platform further comprises an operation station arranged below the robot. The method further comprises the following steps: establishing a three-dimensional template, laying a steel mesh, performing first preliminary positioning, performing fine positioning, turning over the steel mesh, performing second preliminary positioning, and then performing fine positioning. Compared with the prior art, the present invention completes preliminary positioning of a steel mesh by means of the first vision device, and then improves the positioning accuracy of the steel mesh by means of the second vision device, thereby satisfying the requirements of robotic welding, such that the welding speed and efficiency of the steel mesh are high. Especially for the welding of a large steel mesh, the welding speed of the present invention is far higher than the welding speed of a robot which requires manual teaching.
Need to check novelty before this filing date? Find Prior Art

Description

An automatic welding method for large steel mesh based on AI vision Technical Field

[0001] The present invention relates to the technical field of steel mesh welding, and in particular to an automatic welding method for large steel meshes based on AI vision. Background Art

[0002] In the construction industry, a large number of prefabricated steel mesh structures are widely used. Current prefabricated steel mesh structures are generally manually tied or welded at the intersections of the steel mesh. However, manual welding has limitations, such as unstable welding quality, low construction efficiency, high welding costs, and an inability to operate under extreme conditions such as high temperature and high pressure. Currently, mechanical automatic welding technology is widely used in various fields, including automotive, aerospace, and industrial manufacturing, but it usually requires high-precision workpiece positioning and multiple robot arm welding gun path teaching to meet welding process requirements. However, the steel bars themselves are prone to bending, and the bent steel bars will also have errors due to the characteristics of the elastic modulus. The spliced ​​steel mesh is inevitably irregular, and the gaps between the steel bars are uneven, and there will also be height differences between the steel bars. These factors may lead to arc failure, arc breakage, collisions, and ultimately failure of automatic mechanical welding.

[0003] Summary of the Invention

[0004] The present invention provides an automatic welding method for large steel meshes based on AI vision, which is used to solve the problem that large steel meshes are irregular and have large gaps, making them difficult to weld automatically.

[0005] The present invention provides an automatic welding method for large steel mesh based on AI vision, comprising a work platform and an industrial computer, wherein the work platform comprises a guide rail and a machine base that moves along the guide rail, an arm is rotatably provided on the machine base, a robot is slidably provided on the arm, the robot is provided with a welding gun and a second vision device, the arm is provided with a first vision device, the work platform further comprises an operating table provided below the robot, and the following steps are further included:

[0006] Establishing a three-dimensional template: establishing a 3D model template of the work platform, the 3D model template including: the coordinate position of the robot, the coordinate position of the operating table, the coordinate position of the guide rail, the coordinate position of the machine base, the coordinate position of the support arm, and the coordinate position of the first visual device, the 3D model template including a first steel mesh model and a second steel mesh model pre-established on the operating table, the second steel mesh model being the first steel mesh model flipped 180 degrees, the first steel mesh model and the second steel mesh model each including the coordinate positions of a plurality of connecting segments, the industrial computer respectively sorting the connecting segments of the first steel mesh model and the second steel mesh model, the connecting segments including welds, the length of the welds being less than the length of the connecting segments, and the connecting segments and the welds corresponding one to one;

[0007] Laying steel mesh: Lay multiple steel bars on the operating table to form a steel mesh, and fix adjacent steel bars with clamps on the operating table;

[0008] First initial positioning: The machine base moves along the guide rail, driving the support arm from one end of the steel mesh to the other. During the movement of the support arm, the first vision device continuously photographs the steel mesh and generates a first physical 3D model. The connecting segment of the first steel mesh model is compared with the connecting segment of the first physical 3D model to obtain the offset of the connecting segment of the first physical 3D model with respect to the first steel mesh model.

[0009] Precision positioning: Based on the offset and 3D model template, the robot moves to the first connection segment. The second vision device captures images of the first connection segment to obtain a 3D model of the first connection segment. Using this 3D model, the industrial computer obtains the position coordinates of weld A within the first connection segment and then adjusts the starting point of weld A using a preset gap value. The welding gun strikes an arc on a rebar at the starting point of weld A, then moves in an oscillating motion to position D, midway between the two rebars. Starting from position D, the gun then moves in an oscillating motion along the extension direction of the rebar to complete the welding of the first connection segment.

[0010] Repeat the precise positioning steps and the robot completes the welding of the remaining connection segments;

[0011] Turn over: Loosen the clamp and turn the steel mesh 180 degrees so that the reverse side of the steel mesh faces upwards;

[0012] Second initial positioning: The machine base moves along the guide rail, driving the support arm from one end of the steel mesh to the other. During the movement of the support arm, the first vision device continuously photographs the steel mesh and generates a second physical 3D model. The connecting segment of the second steel mesh model is compared with the connecting segment of the second physical 3D model to obtain the offset of the connecting segment of the second physical 3D model with respect to the second steel mesh model.

[0013] The welding of the reverse side of the steel mesh is completed through a precise positioning step.

[0014] Preferably, the specific steps for adjusting the starting position of weld A by a preset gap value are: if the gap at the starting point of weld A is less than the preset value, the starting point of weld A is the current position; if the gap at the starting point of weld A is greater than the preset value, weld A is moved Lmm from the starting position to a narrower direction, and if the gap at the starting point of weld A after movement is less than the preset value, the starting point of weld A is the current position, otherwise the above process is repeated until the gap at the starting point of weld A is less than the preset value.

[0015] Preferably, in the step of striking an arc on a steel bar at the starting point of the weld A, the gap Wmm at the starting point of the weld A is obtained through the 3D model of the first connection segment, and the welding gun located at the middle position of the starting point of the weld A is offset by half of Wmm and then offset by Hmm, and the welding wire on the welding gun contacts a steel bar, wherein H is the thread depth of the steel bar thread.

[0016] Preferably, during the precise positioning process, the welding gun adjusts its posture according to the coordinate positions of the two steel bars in the 3D model of the first connecting section so that the welding gun is always perpendicular to the plane where the two steel bars are located.

[0017] Preferably, during the precise positioning process, if the weld gap is small, the welding gun travels at a fast speed and the wire feeds at a slow speed; if the weld gap is large, the welding gun travels at a slow speed and the wire feeds at a fast speed.

[0018] Preferably, in the precise positioning step: the industrial computer calculates the spatial position information of the connection segment of the first steel mesh model based on the offset and the 3D model template, and then the robot moves to the first connection segment according to the spatial position information of the connection segment of the first steel mesh model; or the industrial computer calculates the spatial position information of the connection segment of the second steel mesh model based on the offset and the 3D model template, and then the robot moves to the first connection segment according to the spatial position information of the connection segment of the second steel mesh model.

[0019] Preferably, there are two operating platforms, which are respectively located on both sides of the guide rail. When the robot is welding the steel mesh on one operating platform, the other operating platform is laying or flipping the steel mesh.

[0020] Preferably, in the first initial positioning step: while the arm is moving, the first visual device captures images of the steel mesh and also captures images of the operating table, and the first visual device processes the captured images to obtain a first physical 3D model on the operating table model.

[0021] Preferably, the steel mesh includes a plurality of second steel bars and a plurality of straight first steel bars, and one end or both ends of the second steel bars are curved.

[0022] Preferably, in the turning over step: the support arm is rotated so that the support arm does not stay above the operating table, and the steel mesh is turned 180 degrees by the sling.

[0023] Compared with the prior art, in the present invention, the first visual device continuously takes photos along the steel mesh from beginning to end to obtain the coordinate position of the steel mesh. Although the accuracy of the steel mesh is low, the speed of obtaining the steel mesh position is fast and efficient. Then, using the obtained coordinate position of the steel mesh, it moves to the vicinity of each connection segment and takes photos through the second visual device to obtain the 3D model of each connection segment. Then, using the 3D model of the connection segment, the starting position of the weld is adjusted, and the welding gun is offset so that the welding wire of the welding gun contacts the steel bar. The welding of the connection segment is completed by setting two ups and downs. During the welding process, the posture of the welding gun is adjusted so that the welding gun is always perpendicular to the plane where the two steel bars are located. This ensures that the arc can be started smoothly, the arc is continuous during the welding process, the stability of the dry extension length parameter of the welding is guaranteed, the effect of the welding molten pool is guaranteed, and the welding process is ensured to be carried out smoothly. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0025] FIG1 is a top view of the present invention;

[0026] FIG2 is a front view of the present invention;

[0027] FIG3 is a left side view of the present invention;

[0028] FIG4 is a schematic diagram of the structure of adjusting the welding gun posture according to the present invention;

[0029] FIG5 is a schematic diagram of the structure of adjusting the starting point of the weld according to the present invention;

[0030] FIG6 is a schematic diagram of the travel path of the welding gun of the present invention.

[0031] Reference numerals: 100. Working platform, 1. Guide rail, 2. Machine base, 3. Support arm, 4. Robot, 5. Operating table, 6. Clamp, 7. Steel mesh. DETAILED DESCRIPTION

[0032] To make the objectives, technical solutions, and advantages of the present invention more clear, the technical solutions of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts shall fall within the scope of protection of the present invention.

[0033] 1-3 , this embodiment provides a method for welding a cap beam reinforcement mesh, including a work platform 100 and an industrial computer. The work platform 100 includes a guide rail 1 and a machine base 2 that moves along the guide rail 1 . A support arm 3 is rotatably provided on the machine base 2 , a robot 4 is slidably provided on the support arm 3 , the robot 4 is provided with a welding gun 8 and a second vision device, and the support arm 3 is provided with a first vision device. The work platform 100 also includes an operating table 5 provided below the robot 4 , and a plurality of clamps 6 are provided on the operating table 5 . The method further includes the following steps:

[0034] Establish a three-dimensional template: establish a 3D model template of the work platform 100, the 3D model template includes: the coordinate position of the robot 4, the coordinate position of the operating table 5, the coordinate position of the guide rail 1, the coordinate position of the machine base 2, the coordinate position of the support arm 3 and the coordinate position of the first visual device, the 3D model template includes a first steel mesh model and a second steel mesh model pre-established on the operating table 5, the second steel mesh model is the first steel mesh model flipped 180 degrees, the first steel mesh model and the second steel mesh model both include the coordinate positions of multiple connecting segments 200, the industrial computer sorts the connecting segments 200 of the first steel mesh model and the connecting segments 200 of the second steel mesh model respectively; the connecting segment 200 includes a weld 300, the length of the weld 300 is less than the length of the connecting segment 200, the connecting segment 200 and the weld 300 correspond one to one, each connecting segment 200 includes a weld 300, and locating the position of the connecting segment 200 is equivalent to locating the position of the weld 300. After welding the first side (front) of the steel mesh 7, it needs to be flipped over to weld the other side (back), so two steel mesh 7 models need to be built on the operating table 5. The connecting section 200 is the part where the two steel bars 71 in the steel mesh 7 are joined. In the connecting section 200, the two steel bars 71 are in contact at some places and not at others, but the gap is relatively small. (This is marked in the figure)

[0035] Laying the steel mesh 7: Lay multiple steel bars 71 on the operating table 5 to form the steel mesh 7, and fix adjacent steel bars 71 by the clamps 6 on the operating table 5; the steel mesh 7 is formed by splicing with the steel bars 71, and many errors will occur in the splicing process, such as the non-straightness of the steel bars 71 themselves and the elastic properties of the steel bars 71. These will cause differences between the spliced ​​steel mesh 7 and the steel mesh 7 in the 3D model template. These differences may cause unsuccessful arc starting, arc breaking during welding, changes in dry extension length, etc., thereby affecting the automatic welding of the steel mesh 7.

[0036] First initial positioning: the machine base 2 moves along the starting point of the guide rail 1 to the end point of the guide rail 1, thereby driving the support arm 3 to move from one end of the steel mesh 7 to the other end. During the movement of the support arm 3, the first visual device continuously takes pictures of the steel mesh 7 and generates a first physical 3D model; in this process, the height position of the support arm 3 is determined, that is, the height position of the first visual device is determined. The first visual device collects images of the steel mesh 7 and also collects images of the operating table 5. The first visual device processes the collected images to obtain the first physical 3D model on the operating table 5 model. A physical 3D model includes a model of the steel mesh 7 and a model of the workbench 5. The workbench 5 remains unchanged throughout, and its coordinate position is fixed. When comparing the connecting segment 200 of the first steel mesh model with the connecting segment 200 of the first physical 3D model, the workbench 5 can be used as their common reference point. After the workbench 5 of the 3D model template and the workbench 5 of the first physical 3D model are aligned, the offset of the connecting segment 200 of the first physical 3D model with respect to the first steel mesh model is obtained; then, using this offset, the coordinate position of the connecting segment 200 of the steel mesh 7 can be obtained. In this step, the coordinate position of the connecting segment 200 of the steel mesh 7 (physical) is obtained by moving the first visual device to perform image acquisition and processing, which is fast and efficient. However, in order to capture the entire width of the steel mesh 7, the first visual device is positioned relatively high, resulting in insufficient imaging accuracy. As a result, the obtained coordinate position of the connecting segment 200 of the steel mesh has a certain error, which is difficult to meet the welding requirements of the robot 4.

[0037] Precise positioning: Based on the offset and the 3D model template, the robot 4 moves to the first connecting segment 200; the second visual device captures an image of the first connecting segment 200 to obtain a 3D model of the first connecting segment 200. Through the 3D model of the first connecting segment 200, the industrial computer obtains the position coordinates of the weld 300A in the first connecting segment 200, and then adjusts the starting position of the weld 300A according to the preset gap value; referring to Figure 6, the welding gun 8 strikes an arc at point C on a steel bar 71 at the starting point of the weld 300A, and then moves to the middle position D between the two steel bars 71 while swinging, and then moves from point D as the starting point along the extension direction of the steel bar 71 while swinging to point E to complete the welding of the first connecting segment 200. In this step, the industrial computer obtains the position coordinates of the weld 300A in the first connecting section 200. Obtaining the position coordinates of the weld 300A solves the difference between the actual steel mesh 7 and the steel mesh 7 in the 3D model template. However, if the gap at the starting point of the weld 300A is too large, it may cause the arc to fail and welding to fail. Therefore, it is necessary to adjust the starting position of the weld 300A by a preset gap value to ensure that the gap at the starting point of the weld 300A meets the arc starting requirements of the welding gun 8, avoid the situation where the arc cannot be started and welding cannot occur, and ensure that the welding process can be carried out smoothly. Second, the welding gun 8 strikes an arc on a rebar 71 at the starting point of the weld 300A. This is the first arc starting point. During the first arc starting point, the welding wire 9 of the welding gun 8 contacts the rebar 71 (ensuring smooth arc starting). The welding gun 8 then moves in an oscillating motion to a point D between the two rebars 71. This point is the second arc starting point. The welding gun 8 then swings in an oscillating motion along the extension direction of the rebar 71, completing the welding of the first connecting section 200. The welded metal strip from the first arc starting point to point D ensures that the welding wire 9 of the welding gun 8 contacts the metal strip during the second arc starting point (ensuring smooth arc starting). Setting two arc starting points ensures that the electric welding arc can be 100% struck, ensuring that the welding process can be carried out smoothly.

[0038] Repeat the precise positioning steps, and the robot 4 completes welding of the remaining connection segments 200; for example, according to the offset and the 3D model template, the robot 4 moves to the second connection segment 200; the second visual device performs image acquisition on the second connection segment 200 to obtain a 3D model of the second connection segment 200, and the industrial computer obtains the position coordinates of the weld 300B in the second connection segment 200 through the 3D model of the second connection segment 200, and then adjusts the starting position of the weld 300B by a preset gap value to obtain the position of the weld 300; the welding gun 8 strikes an arc on a steel bar 71 at the starting point of the weld 300B, and then moves to the middle position D between the two steel bars 71 while swinging, and then moves along the extension direction of the steel bar 71 while swinging with D as the starting point to complete the welding of the second connection segment 200.

[0039] Turn over: Loosen the clamp 6 and turn the steel mesh 7 180 degrees so that the reverse side of the steel mesh 7 faces upwards;

[0040] Second initial positioning: The base 2 moves along the guide rail 1, driving the support arm 3 from one end of the steel mesh 7 to the other. During the movement of the support arm 3, the first vision device continuously photographs the steel mesh 7 and generates a second physical 3D model. The connecting segment 200 of the second steel mesh model is compared with the connecting segment 200 of the second physical 3D model to obtain the offset of the connecting segment 200 of the second physical 3D model with respect to the second steel mesh model.

[0041] The welding of the reverse side of the reinforcement mesh 7 is completed through the fine positioning step.

[0042] Among them, the specific steps of adjusting the starting position of the weld 300A by the preset gap value are: if the gap at the starting point of the weld 300A is smaller than the preset value, for example, the gap at the starting point of the weld 300A is smaller than 10 mm, then the weld 300A does not need to be offset; referring to FIG5, if the gap at the starting point O of the weld 300A is greater than 10 mm, then the weld 300A is moved 2 mm from the starting point O to the narrower direction to reach P (the weld 300A extends to both ends at point O, so one end must be narrow and the other end must be wide. Otherwise, the steel mesh 7 needs to be re-fixed), and it is determined whether the gap at the starting point P of the moved weld 300A is greater than 10 mm. If it is less than 10 mm, the starting point of the weld 300A is P, otherwise the above process is repeated until the gap at the starting point of the weld 300A is less than 10 mm.

[0043] In the step of striking the arc with the welding gun 8 on a rebar 71 at the starting point of the weld 300A, the gap W mm at the starting point of the weld 300A is obtained using the 3D model of the first connecting segment 200. For example, the gap at the starting point of the weld 300A is 10 mm. The welding gun 8, located at the middle of the starting point of the weld 300A, is offset by 5 mm and then offset by H mm, so that the welding wire 9 on the welding gun 8 contacts the rebar 71. There are two rebars 71 within a connecting segment 200, and the welding wire 9 on the welding gun 8 generally contacts the rebar 71 on the inner side of the steel mesh 7. The lowest point determined by the second visual device after scanning is the middle of the starting point of the weld 300A. However, errors exist during the splicing process of the steel mesh 7, and arc striking from the middle of the starting point of the weld 300A is prone to failure. To ensure successful arc striking, an offset is required from the traditional middle position to ensure that the welding wire 9 contacts the rebar 71, thereby achieving a stable arc starting point. The gap value between the steel bars 71 is dynamic, so the gap error between the steel bars 71 is eliminated by first offsetting by 5 mm. However, the steel bars 71 have threads, and the thread depth H is generally set to 5 mm. Therefore, another offset of 5 mm is required to make the welding wire 9 contact the steel bars 71 inside the steel mesh 7.

[0044] Among them, in the precise positioning step: the industrial computer calculates the spatial position information of the connecting segment 200 of the first steel mesh model based on the offset and the 3D model template, and then the robot 4 moves to the first connecting segment 200 according to the spatial position information of the connecting segment 200 of the first steel mesh model; or the industrial computer calculates the spatial position information of the connecting segment 200 of the second steel mesh model based on the offset and the 3D model template, and then the robot 4 moves to the first connecting segment 200 according to the spatial position information of the connecting segment 200 of the second steel mesh model.

[0045] Among them, in the process of precise positioning, referring to FIG4 , the welding gun 8 adjusts the posture of the welding gun 8 according to the coordinate positions of the two steel bars 71 in the 3D model of the first connecting section 200, so that the welding gun 8 is always perpendicular to the plane where the two steel bars 71 are located. After the steel mesh 7 is spliced, there are ups and downs between the steel bars 71. If the height difference between the two exceeds a certain range, the welding gun 8 will hit the higher steel bar 71, causing welding interruption. The second visual device obtains a 3D model of each connecting section 200 through stereo modeling. The 3D model will not only give an accurate weld 300 trajectory but also the coordinate position of the steel bar 71. At this time, the algorithm can be used to guide the welding gun 8 to make an angular offset in the z direction, so that the welding gun 8 is always perpendicular to the plane where the two steel bars 71 are located, so as not to hit the gun, and ensure that the distance between the end of the welding gun 8 and the two steel bars 71 is consistent, ensuring the stability of the dry extension length parameters of the welding and ensuring the effect of the welding pool.

[0046] During the precise positioning process, the welding gun 8's travel speed and wire feed speed are adjusted based on the size of the weld seam 300 gap. If the weld seam 300 gap is small, the welding gun 8's travel speed is fast and the wire feed speed is slow. If the weld seam 300 gap is large, the welding gun 8's travel speed is slow and the wire feed speed is fast. This step ensures a continuous arc and consistent fill volume. The wire feed speed can be adjusted by the current: a higher current results in faster wire feed speed, while a lower current results in slower wire feed speed.

[0047] The swing amplitude of welding gun 8 is fixed, rather than automatically adjusted based on the width of weld seam 300. This setting helps maintain the stability of the welding stickout parameter and the effectiveness of the weld pool. The arc continuity and fill volume are controlled by the travel speed of welding gun 8 and the wire feed speed.

[0048] In another embodiment of the present invention, two operating platforms 5 are provided, one on each side of the guide rail 1. While the robot 4 is welding the steel mesh 7 on one operating platform 5, the arm 3 rotates above the operating platform 5, while the other operating platform 5 lays or flips the steel mesh 7. This eliminates interference between the arm 3 and the robot 4, facilitating these processes. The provision of the rotating arm 3 improves the welding efficiency of the robot 4 and also facilitates the laying and flipping of the steel mesh 7.

[0049] The steel mesh 7 includes a plurality of straight first steel bars 71 and a plurality of second steel bars 71. One end or both ends of the second steel bars 71 are curved. Due to the elastic properties of the steel bars 71, there will always be errors after the second steel bars 71 are produced, which causes the laid steel mesh 7 to be inconsistent with the first steel mesh model.

[0050] In the turning over step: rotate the arm 3 so that the arm 3 does not stay above the operating table 5, and use the sling to turn the steel mesh 7 180 degrees so that the back of the steel mesh 7 faces upward. Of course, the steel bars 71 can also be lifted onto the operating table 5 by the sling.

[0051] In the turning over step: one side of the carrier is overlapped above the operating table 5, and then the steel mesh 7 is turned over to the carrier by the sling, and then the carrier is moved above the operating table 5. Specifically, a plurality of positioning square tubes are fixed on the operating table 5, and the carrier includes a plurality of crossbeams (the crossbeams are also square tubes), one end of the crossbeam is inserted into the positioning square tube, and the sling turns the steel mesh 7 onto the carrier, and the crossbeam moves forward along the positioning square steel until it spans the operating table 5. At this time, the steel mesh 7 is placed on the operating table 5 through the crossbeam. The positioning square tube is provided with a chamfer to facilitate the steel mesh 7 to pass over the positioning square steel. The height of the crossbeam is greater than the height of the clamp 6 to prevent the clamp 6 from affecting the steel mesh 7.

[0052] In the present invention, a first vision device continuously photographs along the entire length of the steel mesh 7 to obtain the coordinate position of the steel mesh 7. Although the accuracy of the steel mesh 7 is low, the speed and efficiency of obtaining the position of the steel mesh 7 are high. Then, using the obtained coordinate position of the steel mesh 7, the device moves to the vicinity of each connecting segment 200 and photographs the 3D model of each connecting segment 200 through a second vision device. Using the 3D model of the connecting segment 200, the starting position of the weld 300 is adjusted, the welding gun 8 is offset so that the welding wire 9 of the welding gun 8 contacts the steel bars 71, and the posture of the welding gun 8 is adjusted so that the welding gun 8 is always perpendicular to the plane of the two steel bars 71. This ensures smooth arc initiation, continuous arcing during welding, the stability of the dry extension length parameter of the weld, the effect of the weld pool, and the smooth execution of the welding process.

[0053] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the present invention.

Claims

1. An automatic welding method for large steel mesh based on AI vision, characterized in that: The method comprises a working platform and an industrial computer, wherein the working platform comprises a guide rail and a machine base moving along the guide rail, wherein a support arm is rotatably arranged on the machine base, a robot is slidably arranged on the support arm, a welding gun and a second visual device are arranged on the robot, and a first visual device is arranged on the support arm. The working platform also comprises an operating table arranged below the robot, and further comprises the following steps: Establishing a three-dimensional template: establishing a 3D model template of the working platform, the 3D model template including: the coordinate position of the robot, the coordinate position of the operating table, the coordinate position of the guide rail, the coordinate position of the base, the coordinate position of the arm and the coordinate position of the first visual device, the 3D model template including a first steel mesh model and a second steel mesh model pre-established on the operating table, the second steel mesh model is the first steel mesh model flipped 180 degrees, the first steel mesh model and the second steel mesh model both include the coordinate positions of a plurality of connecting segments, the industrial computer respectively sorts the connecting segments of the first steel mesh model and the second steel mesh model, the connecting segments include welds, the length of the welds is less than the length of the connecting segments, and the connecting segments and the welds correspond one to one; Laying steel mesh: Lay multiple steel bars on the operating table to form a steel mesh, and fix adjacent steel bars with clamps on the operating table; First initial positioning: the machine base moves along the guide rail to drive the support arm to move from one end of the steel mesh to the other end. During the movement of the support arm, the first visual device continuously takes pictures of the steel mesh and generates a first physical 3D model; the connection segment of the first steel mesh model is compared with the connection segment of the first physical 3D model to obtain the offset of the connection segment of the first physical 3D model on the first steel mesh model; Precise positioning: According to the offset and the 3D model template, the robot moves to the first connection segment; the second visual device collects images of the first connection segment to obtain the 3D model of the first connection segment. Through the 3D model of the first connection segment, the industrial computer obtains the position coordinates of the weld A in the first connection segment, and then adjusts the starting point of the weld A according to the preset gap value. Point position; the welding gun starts an arc on a steel bar at the starting point of the weld A, then moves to the middle position D between the two steel bars in the swing, and then moves along the extension direction of the steel bar in the swing with D as the starting point to complete the welding of the first connection section; Repeat the precise positioning steps, and the robot completes the welding of the remaining connection segments; Turn over: Loosen the clamp and turn the steel mesh 180 degrees so that the reverse side of the steel mesh faces upwards; Second initial positioning: the machine base moves along the guide rail to drive the support arm to move from one end of the steel mesh to the other end. During the movement of the support arm, the first visual device continuously takes pictures of the steel mesh and generates a second physical 3D model; the connecting segment of the second steel mesh model is compared with the connecting segment of the second physical 3D model to obtain the offset of the connecting segment of the second physical 3D model on the second steel mesh model; The welding of the reverse side of the steel mesh is completed through a precise positioning step.

2. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: The specific steps for adjusting the starting position of weld A by a preset gap value are as follows: if the gap at the starting point of weld A is less than the preset value, the starting point of weld A is the current position; if the gap at the starting point of weld A is greater than the preset value, weld A is moved Lmm from the starting position to a narrower direction, and if the gap at the starting point of weld A after the movement is less than the preset value, the starting point of weld A is the current position, otherwise the above process is repeated until the gap at the starting point of weld A is less than the preset value.

3. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: In the step of the welding gun striking an arc on a steel bar at the starting point of the weld A: the gap Wmm at the starting point of the weld A is obtained through the 3D model of the first connection section, and the welding gun located at the middle position of the starting point of the weld A is offset by half of Wmm and then offset by Hmm, and the welding wire on the welding gun contacts a steel bar, wherein H is the thread depth of the steel bar thread.

4. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: During the precise positioning process, the welding gun adjusts its posture according to the coordinate positions of the two steel bars in the 3D model of the first connection segment so that the welding gun is always perpendicular to the plane where the two steel bars are located.

5. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: During the precise positioning process, if the gap of the weld is small, the welding gun moves fast and the wire feeding speed is slow. If the gap of the weld is large, the welding gun moves slow and the wire feeding speed is fast.

6. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: In the precise positioning step: the industrial computer calculates the spatial position information of the connection segment of the first steel mesh model according to the offset and the 3D model template, and then the robot moves to the first connection segment according to the spatial position information of the connection segment of the first steel mesh model; or the industrial computer calculates the spatial position information of the connection segment of the second steel mesh model according to the offset and the 3D model template, and then the robot moves to the first connection segment according to the spatial position information of the connection segment of the second steel mesh model.

7. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: There are two operating tables, which are respectively located on both sides of the guide rail. When the robot is welding the steel mesh on one operating table, the other operating table is laying or flipping the steel mesh.

8. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: In the first initial positioning step: when the arm is moving, the first visual device captures images of the steel mesh and the operating table at the same time, and the first visual device processes the captured images to obtain a first physical 3D model on the operating table model.

9. The automatic welding method of large steel mesh based on AI vision according to claim 1 is characterized in that: The steel mesh includes a plurality of second steel bars and a plurality of straight first steel bars, and one or both ends of the second steel bars are bent.

10. The automatic welding method of large steel mesh based on AI vision according to claim 7 is characterized in that: In the turning over step: rotate the arm so that it does not stay above the operating table, and use the sling to turn the steel mesh 180 degrees.

Citation Information

Patent Citations

  • Robot automatic welding device for space arc path submerged-arc welding

    CN110605463A

  • Visual location welding system and method based on robot welding

    CN112122840A

  • Large square grid component robot welding equipment based on machine vision and welding seam positioning method

    CN113385869A

  • Steel bar welding automation system based on 3D visual guidance

    CN114749848A

  • Robot welding system and method for reinforcing mesh

    CN115026470A

Cited By

  • Full-automatic welding production line for base plates

    CN119304331A

  • Tailor welding device for nuclear fusion large coil AP assembly

    CN120269247A