Fabric coloring method and finished fabric product

Through fabric coloring methods, desizing agents, modifiers, etc. are used to treat polyester, linen, lyocell and other combined fabrics under specific conditions, which solves the problem of inconspicuous distressing effect, lack of hand feel and substandard color fastness of finished fabrics. It achieves uniform coloring and improved hand feel, is suitable for dark-colored products, overcomes the problem of high temperature requirements, and improves the coloring effect.

WO2024216481A1PCT designated stage expired Publication Date: 2024-10-24ZHENG XUHUI
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/088823
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing coloring methods for finished fabrics are mainly made of cotton. The distressed effect is not obvious, the hand feel is lacking, the color fastness is not up to standard, it is difficult to dye dark colors, and the semi-finished product is not colored after quilting and sewing. The requirements are high and it is difficult to achieve uniform results.

Method used

Adopt a fabric coloring method, including pre-treatment, modification treatment, dyeing, color fixation, adding softener and dehydration and drying steps, using desizing agent, modifier, color fixing agent and softener at a specific temperature and Processing under pH value conditions is suitable for semi-finished products quilted and sewn from polyester, linen, lyocell and other combination fabrics or uncolored chemical fiber fabrics to achieve uniform coloring and improved hand feel.

Benefits of technology

It achieves uniform coloring of fabrics with multiple components and overcomes the problems of lack of hand feel, substandard color fastness and uneven dyeing of dark colors. The distressed effect is more detailed, the color layering is obvious, and the hand feel becomes softer. It is suitable for dark colors. The product overcomes the problem of high temperature requirements in traditional technology and improves the coloring effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023088823_24102024_PF_FP_ABST
    Figure CN2023088823_24102024_PF_FP_ABST
Patent Text Reader

Abstract

A fabric coloring method and a finished fabric product. The coloring method comprises the following steps: S1, pre-treating a fabric; S2, modifying the fabric obtained in step S1; S3, dyeing the fabric obtained in step S2; S4, subjecting the fabric obtained in step S3 to color fixation; S5, adding a softener to the fabric obtained in step S4; and S6, dehydrating the fabric obtained in step S5, and drying same. The coloring method can not only achieve uniform coloring of fabrics of various components at the same time, but can also achieve overall uniform coloring of uncolored semi-finished fabrics formed by means of directly sewing quilting seams; and a more delicate antique finish effect and a more obvious sense of color depth are obtained while the problems of poor tactile feel, substandard color fastness, non-uniform dark color dyeing, etc., are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Fabric coloring method and fabric finished product Technical Field

[0001] The present invention relates to the field of fabric coloring, in particular to a fabric coloring method and a fabric finished product. Background Art

[0002] At present, the finished products on the market are mainly made of pure cotton. The aging effect produced by using paint dyes is not obvious, and it is basically a solid color effect. The hand feel is lacking, the color fastness does not meet the standard, and it is difficult to dye dark colors, etc. and defects.

[0003] Secondly, the finished products currently on the market are basically all colored by first coloring the fabric and then sewing it into a finished product. This will result in the coloring of the overall finished product lacking characteristics, the appearance being popular, and the feel not being soft.

[0004] In view of the problems existing in the prior art, it is of great significance to provide a fabric coloring method and a fabric finished product.

[0005] Summary of the Invention

[0006] In order to solve the above problems, the present invention provides a fabric coloring method and a fabric finished product.

[0007] To achieve the above-mentioned object, the present invention provides a fabric coloring method, comprising the following steps: S1, pre-treating the fabric; S2, modifying the fabric obtained in step S1; S3, dyeing the fabric obtained in step S2; S4, fixing the color of the fabric obtained in step S3; S5, adding a softener to the fabric obtained in step S4 and washing it with water; S6, dehydrating and drying the fabric obtained in step S5;

[0008] Furthermore, the fabric is specifically a three-component fabric composed of polyester, linen and lyocell, and the method is specifically as follows: S1', placing the fabric in a dye vat, adding a desizing agent, a detergent and hydrogen peroxide to the dye vat, and adjusting the pH value to 8-9, the water-bath ratio to 1:20-1:25, desizing for 20-30 minutes in an environment of 70-90 degrees, and then draining; S2', adding water to the dye vat to a water-bath ratio of 1:20-1:25, and adding a modifier and 3%-7% NaOH to the dye vat, and drying at a water temperature of 50-60 degrees. , turning over for 10-15 minutes in an environment with a pH value of 8.5-9.5 and then draining; S3', dyeing and washing the fabric obtained in step S2'; S4', refilling the dye vat of the fabric obtained in step S3' with water and adding a fixing agent, turning over for 3-10 minutes and then draining; S5', adding a softener to the fabric obtained in step S4' and washing it with water, turning over for 3-10 minutes and then draining; S6', taking the fabric obtained in step S5' out of the dye vat and placing it in a dehydrator to perform a dehydration operation for 10 minutes;

[0009] Furthermore, the step S3', dyeing and washing the fabric obtained in step S2', specifically includes the following sub-steps: S3.1', adding water, paint and 1g / L adhesive to the dye vat, and dyeing the fabric in an environment of 70-90 degrees, and draining after 1-2 hours; S3.2', adding water and 2g / L enzyme to the dye vat, fermenting and washing in an environment of 70-90 degrees for 10-30 minutes, and draining; S3.3', sampling and coloring the fabric obtained in step S3.2', and adding reactive dye according to the dyeing situation, tumbling in 70-90 degree water for 10-30 minutes, and draining;

[0010] Furthermore, the step S3.1′ of coloring the fabric in an environment of 70-90 degrees specifically comprises: coloring the fabric in an environment of 70 degrees and gradually increasing the temperature at a rate of 2°C / min until the temperature reaches 90 degrees;

[0011] Furthermore, in step S1', desizing agent, detergent and hydrogen peroxide are added into the dye vat: 5 g / L of desizing agent, 2 g / L of detergent and 10 g / L of hydrogen peroxide are added into the dye vat;

[0012] Furthermore, in the step S6', after the fabric obtained in the step S5' is taken out of the dye vat and placed in a dehydrator for 10 minutes of dehydration, the following steps are further included: S7', placing the fabric obtained in the step S6' in an oven and drying it at a temperature of 80-90 degrees for 1-2 hours;

[0013] Furthermore, the fabric may be a three-component fabric composed of recycled polyester, linen and lyocell, or a three-component fabric composed of polyester, linen and viscose, or a three-component fabric composed of recycled polyester, linen and viscose.

[0014] Furthermore, the fabric is a semi-finished product, and the semi-finished product is specifically a semi-finished product made of uncolored chemical fiber fabric quilted and sewn, and the method is specifically as follows: S1", putting the semi-finished product into a dyeing vat, degreasing and decontaminating the semi-finished product, turning it over in an environment heated to 50-70 degrees for 10-20 minutes to drain the water, and rinsing the semi-finished product with clean water; S2", adding water to the dyeing vat and adding a modifier to the dyeing vat, turning it over in an environment with a water temperature of 50-70 degrees for 25 minutes, draining the water, and rinsing the semi-finished product with clean water; S3", Add water and slowly add dye, and turn over for 20-30 minutes in an environment with a water temperature of 50-70 degrees; S4" takes out the semi-finished product obtained in step S3", shakes out the water, blows dry, and takes samples for color matching; S5" puts the semi-finished product obtained in step S4" into the dye vat, refills with water and adds a fixing agent, and turns over for 10 minutes; S6" adds a softener to the semi-finished product obtained in step S5", and turns over for 6 minutes; S7" takes out the semi-finished product obtained in step S6" from the dye vat, puts it into a dehydrator for dehydration, and then dry it at a temperature of 60-80 degrees;

[0015] Furthermore, the step S4" takes out the semi-finished product obtained in step S3", spins out the water, blows dry, and takes samples for color matching, which specifically includes the following sub-steps: S4.1" takes out the semi-finished product obtained in step S3", spins out the water, blows dry, and takes samples for color matching; S4.2" adds lotion for washing; S4.3" takes out the semi-finished product obtained in step S4.2", spins out the water, blows dry, and takes samples for color matching, and determines whether the color matches the sample color. If not, re-execute step S4.2"; S4.4" if yes, rinse the semi-finished product obtained in step S4.3" with cold water three times;

[0016] The present invention provides a finished fabric product, which is specifically prepared by the fabric coloring method according to any one of claims 1 to 9.

[0017] The present invention provides a method for coloring fabrics and a finished fabric product. By providing a new dyeing and washing method and process, it is not only possible to achieve uniform coloring of fabrics of multiple components at the same time, but also to achieve uniform coloring of uncolored semi-finished fabrics directly quilted and sewn. While overcoming the problems of poor hand feel, substandard color fastness, and uneven dyeing of dark colors, the faded effect is more detailed and the color layering is more obvious. While achieving a softer hand feel, the color layering is more obvious, and compared with pure cotton finished products, there is a more obvious faded effect. These advantages are particularly prominent on dark-colored products. At the same time, the coloring method provided by the present invention can directly dye and wash uncolored semi-finished products made by quilting and sewing at a relatively low temperature to achieve a faded and aged appearance. This not only overcomes the difficulty of traditional technology in which uncolored semi-finished products after quilting and sewing are difficult to achieve perfectly due to the high temperature requirements, but also makes the effect of the colored finished product better. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] FIG1 is a schematic flow diagram of the method for coloring fabrics according to the present invention;

[0019] FIG2 is a schematic diagram of a process of Embodiment 1 of the present invention;

[0020] FIG3 is a schematic diagram of a flow chart of the second embodiment of the present invention. DETAILED DESCRIPTION

[0021] The technical solution and working principle of the present invention are further described below with reference to the accompanying drawings.

[0022] As shown in FIG1 , FIG1 is a schematic flow chart of the fabric coloring method of the present invention.

[0023] The fabric coloring method of the present invention, in a preferred embodiment of the present invention, the fabric can be specifically polyester, linen, lyocell; recycled polyester, linen, lyocell; polyester, linen, viscose; recycled polyester, linen, viscose and other three-component fabrics; in another preferred embodiment of the present invention, the fabric is a semi-finished fabric quilted by sewing uncolored chemical fiber fabric, and the chemical fiber fabric can be not only a sanded chemical fiber fabric, but also a non-sanded chemical fiber fabric; the method specifically comprises the following steps:

[0024] S1, pre-treating the fabric;

[0025] S2, modifying the fabric obtained in step S1;

[0026] S3, dyeing the fabric obtained in step S2;

[0027] S4, fixing the fabric obtained in step S3;

[0028] S5, adding softener to the fabric obtained in step S4 and washing with water;

[0029] S6, dehydrating and drying the fabric obtained in step S5.

[0030] As shown in FIG2 , FIG2 is a schematic diagram of a process of Embodiment 1 of the present invention; in Embodiment 1 of the present invention, the fabric is specifically a three-component fabric composed of polyester, linen and lyocell, and the method is specifically as follows:

[0031] S1', placing the fabric into a dye vat, adding 5g / L of desizing agent, 2g / L of detergent and 10g / L of hydrogen peroxide into the dye vat, adjusting the pH value to 8-9, and the water-bath ratio to 1:20-1:25, desizing the fabric in an environment of 70-90 degrees for 20-30 minutes and then draining the water;

[0032] S2', adding water to the dye vat to a water-bath ratio of 1:20-1:25, and adding a modifier and 3%-7% NaOH to the dye vat, turning the dye vat for 10-15 minutes in an environment with a water temperature of 50-60 degrees and a pH value of 8.5-9.5, and then draining the water. Furthermore, the amount of the modifier is 4%-10%;

[0033] S3.1', add water, paint, and 1g / L adhesive to the dye vat, dye the fabric in an environment with a starting temperature of 70 degrees Celsius, and gradually increase the temperature at a rate of 2 degrees Celsius / min until the temperature reaches 90 degrees Celsius. Drain the water after 1-2 hours;

[0034] S3.2', add water to the dye vat and add 2g / L enzyme, ferment and wash in an environment of 70-90 degrees for 10-30 minutes and then drain;

[0035] S3.3', sample the fabric obtained in step S3.2' and perform color matching, add reactive dye according to the dyeing conditions, tumble in 70-90 degree water for 10-30 minutes and then drain;

[0036] S4', refilling the dye vat of the fabric obtained in step S3' with water and adding a fixing agent at a fixing agent ratio of 1%, turning the vat over for 3-10 minutes, and then draining the water;

[0037] S5', adding softener to the fabric obtained in step S4' and washing with water, wherein the softener ratio is 1-3%, turning the fabric over for 3-10 minutes and then draining the fabric;

[0038] S6', taking the fabric obtained in step S5' out of the dye vat and placing it in a dehydrator to perform a dehydration operation for 10 minutes;

[0039] S7', putting the fabric obtained in step S6' into an oven and drying it at a temperature of 80-90 degrees for 1-2 hours.

[0040] As shown in FIG3 , FIG3 is a flow chart of the second embodiment of the present invention; in the second embodiment of the present invention, the fabric is a semi-finished product, and the semi-finished product is specifically a semi-finished product made of quilted uncolored chemical fiber fabric, wherein the chemical fiber fabric is specifically a non-sanded chemical fiber fabric, preferably, the chemical fiber fabric can be a chemical fiber fabric such as recycled fiber and synthetic fiber, and the method is specifically as follows:

[0041] S1”, placing the semi-finished product into a dye vat, degreasing and cleaning the semi-finished product, turning it over in an environment heated to 50-70 degrees for 10-20 minutes to drain the water, and rinsing the semi-finished product with clean water 3 times;

[0042] S2”, adding water and modifier into the dye vat, turning it over in a water temperature of 50-70 degrees for 25 minutes, draining the water, and rinsing the semi-finished product with clean water for 3 times;

[0043] S3”, add water to the dye vat, slowly add dye, and turn it over in a water temperature of 50-70 degrees for 20-30 minutes;

[0044] S4.1 "Take out the semi-finished product obtained in step S3", spin off the water, blow dry, and take samples for color comparison;

[0045] S4.2” Add detergent for cleaning; the detergent is specifically adhesive B-3340P, and the specific amount of detergent is 1-4g / L;

[0046] S4.3" takes out the semi-finished product obtained in step S4.2", spins out the water, blows it dry, and takes a sample for color comparison to determine whether the color matches the sample color. If not, repeat step S4.2";

[0047] If yes, rinse the semi-finished product obtained in step S4.3 with cold water three times.

[0048] S5: placing the semi-finished product obtained in step S4 into the dye vat, refilling with water and adding a fixing agent, and turning the dye vat over for 10 minutes;

[0049] S6" adds softener to the semi-finished product obtained in step S5" and turns it over for 6 minutes;

[0050] In step S7, the semi-finished product obtained in step S6 is taken out of the dye vat, placed in a dehydrator for dehydration, and dried at a temperature of 60-80 degrees.

[0051] The above is only an illustrative description of the present invention. Those skilled in the art should know that various improvements can be made to the present invention without departing from the working principle of the present invention, which all fall within the scope of protection of the present invention.

Claims

1. A method for coloring fabrics, characterized in that: The following steps are involved: S1, pre-treat the fabric; S2, modifying the fabric obtained in step S1; S3, dyeing the fabric obtained in step S2; S4, fixing the color of the fabric obtained in step S3; S5, adding softener to the fabric obtained in step S4 and washing it with water; S6, dehydrating and drying the fabric obtained in step S5.

2. The method for coloring fabric according to claim 1, wherein: The fabric is specifically a three-component fabric composed of polyester, linen and lyocell, and the method is specifically as follows: S1', putting the fabric into a dye vat, adding a desizing agent, a detergent and hydrogen peroxide into the dye vat, adjusting the pH value to 8-9, the water-bath ratio to 1:20-1:25, desizing for 20-30 minutes in an environment of 70-90 degrees, and then draining; S2', add water to the dye vat to a water-bath ratio of 1:20-1:25, add a modifier and 3%-7% NaOH to the dye vat, turn it over for 10-15 minutes in an environment with a water temperature of 50-60 degrees and a pH value of 8.5-9.5, and then drain; S3', dyeing the fabric obtained in step S2'; S4', refilling the dye vat of the fabric obtained in step S3' with water and adding a color fixing agent, turning it over for 3-10 minutes and then draining the water; S5', adding softener to the fabric obtained in step S4' and washing with water, turning over for 3-10 minutes and then draining; S6', taking the fabric obtained in step S5' out of the dyeing vat, and placing it in a dehydrator to perform a dehydration operation for 10 minutes.

3. The coloring method of fabric as claimed in claim 2, characterized in that: The step S3', dyeing and washing the fabric obtained in step S2', specifically comprises the following sub-steps: S3.1', add water, paint and 1g / L adhesive into the dyeing vat, and dye the fabric in an environment of 70-90 degrees, and drain after 1-2 hours; S3.2', add water to the dyeing vat and add 2g / L enzyme, and wash in an environment of 70-90 degrees for 10-30 minutes and then drain; S3.3', sampling and color matching of the fabric obtained in step S3.2', and adding reactive dye according to the dyeing conditions, rolling in 70-90 degree water for 10-30 minutes and then draining.

4. The method for coloring a fabric as claimed in claim 3, characterized in that: The step S3.1' of coloring the fabric in an environment of 70-90 degrees specifically includes: coloring the fabric in an environment of 70 degrees, and gradually raising the temperature at a rate of 2°C / min until the temperature reaches 90 degrees.

5. The method for coloring fabric according to claim 2, wherein: In the step S1', desizing agent, detergent and hydrogen peroxide are added into the dye vat. Specifically, 5 g / L of desizing agent, 2 g / L of detergent and 10 g / L of hydrogen peroxide are added into the dye vat.

6. The method for coloring fabric according to claim 2, wherein: In the step S6', the fabric obtained in the step S5' is taken out from the dyeing vat and placed in a dehydrator for 10 minutes of dehydration, and then the following steps are further included: S7', putting the fabric obtained in step S6' into an oven and drying it at a temperature of 80-90 degrees for 1-2 hours.

7. The method for coloring fabrics according to claim 2, wherein: The fabric can specifically be a three-component fabric composed of recycled polyester, linen and lyocell, or a three-component fabric composed of polyester, linen and viscose, or a three-component fabric composed of recycled polyester, linen and viscose.

8. The method for coloring fabrics according to claim 1, wherein: The fabric is a semi-finished product, and the semi-finished product is specifically a semi-finished product made by quilting uncolored chemical fiber fabric. The method is specifically as follows: S1", placing the semi-finished product into a dye vat, degreasing and cleaning the semi-finished product, turning it over for 10-20 minutes in an environment heated to 50-70 degrees to drain the water, and rinsing the semi-finished product with clean water; S2", adding water and a modifier into the dye vat, turning it over in an environment with a water temperature of 50-70 degrees for 25 minutes, draining the water, and rinsing the semi-finished product with clean water; S3”, add water to the dye vat, add dye slowly, and turn it over for 20-30 minutes in a water temperature of 50-70 degrees; S4" taking out the semi-finished product obtained in step S3", drying it, blowing it dry, and taking samples for color matching; S5”: placing the semi-finished product obtained in step S4” into the dye vat, refilling with water and adding a fixing agent, and turning the dye vat over for 10 minutes; S6" adds softener to the semi-finished product obtained in step S5" and turns it over for 6 minutes; S7" takes the semi-finished product obtained in step S6" out of the dyeing vat, puts it into a dehydrator to perform a dehydration operation, and then dries it at a temperature of 60-80 degrees.

9. The method for coloring a fabric as claimed in claim 8, characterized in that: The step S4" is to take out the semi-finished product obtained in step S3", spin off the water, blow dry, and take samples for color matching, which specifically includes the following sub-steps: S4.1" Take out the semi-finished product obtained in step S3", spin off the water, blow dry, and take samples for color matching; S4.2” Add detergent to clean; S4.3" Take out the semi-finished product obtained in step S4.2" and spin off the water, blow dry, and take a sample for color matching to determine whether the color matches the sample color. If not, re-execute step S4.2"; S4.4" If yes, rinse the semi-finished product obtained in step S4.3" with cold water for 3 times.

10. A finished fabric product, characterized in that: The finished fabric product is specifically prepared by the fabric coloring method according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Multicomponent fiber blended fabric and preparation thereof

    CN101275327A

  • Deep color coating dyeing method of all cotton yarn fabric

    CN101457490A

  • Coloring method of chemical fiber product

    CN114075794A

  • Environment-friendly anti-wrinkle moisture-removing polyester-viscose-linen dyed cloth and preparation process thereof

    CN114855386A

  • Method of pretreatment of cellulose containing textiles

    US20170356128A1