Manufacturing method for microporous glass skeleton hydrogen storage material

By manufacturing microporous glass skeleton hydrogen storage materials, we solve the problems of glass waste pollution and bottlenecks in the field of hydrogen energy storage, achieve efficient, safe, and environmentally friendly hydrogen storage and release, and improve the efficiency of hydrogen energy use.

WO2024216877A1PCT designated stage expired Publication Date: 2024-10-24SHANGHAI SUPERHIGH ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/123898
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2023-10-11
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

In the existing technology, the widespread use of glass has led to waste glass and glass products polluting the soil and air. At the same time, there are bottlenecks in the field of hydrogen energy storage. Other hydrogen storage products have not yet been commercialized, and there is a lack of effective glass hydrogen storage materials.

Method used

Using the manufacturing method of microporous glass skeleton hydrogen storage materials, by mixing glass powder with foaming agents, modifying additives and foam stabilizers, sintering, increasing pores, annealing and boiling to form a rich microporous framework structure, combined with the media The solution and hydrogen storage composite material are compounded and blended to form a glass hydrogen storage composite material with efficient hydrogen absorption and release capabilities.

Benefits of technology

It improves the recycling value of glass, enhances the mechanical properties of composite materials, realizes reversible large-scale absorption, storage and release of hydrogen at high temperatures, simplifies installation and disassembly, and has high temperature resistance, impact resistance, high safety, low cost, The characteristics of long life, green environmental protection and high energy saving promote the safe use of hydrogen energy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023123898_24102024_PF_FP_ABST
    Figure CN2023123898_24102024_PF_FP_ABST
Patent Text Reader

Abstract

A manufacturing method for a microporous glass skeleton hydrogen storage material, which method comprises the following steps: S1, crushing glass into a powder state with a particle size of 1 micron; S2, adding a foaming agent, a modified additive and a foam stabilizer, and uniformly mixing same; S3, carrying out sintering, pore increasing, pore stabilizing, annealing, water boiling and drying to prepare a microporous glass skeleton structure rich in microporous framework structures, wherein the water boiling temperature is 100ºC, and the time is 30 hours; S4, formulating a medium solution for later use; and S5, composite blending the microporous glass skeleton structure and the medium solution for later use with a hydrogen storage composite material, and drying the blended product into a hydrogen storage finished product.
Need to check novelty before this filing date? Find Prior Art

Description

Method for manufacturing microporous glass skeleton hydrogen storage material Technical Field

[0001] The invention relates to the technical field of glass powder-based skeleton material manufacturing, in particular to a method for manufacturing a microporous glass skeleton hydrogen storage material. Background Art

[0002] Glass is a material commonly used in modern human life. It can be made into various utensils, containers, flat glass, etc.

[0003] However, the widespread use of glass in existing technologies also brings about a series of other glass-related problems. As time goes by, more and more discarded glass and glass products will appear. These discarded glass and glass products piled on the ground can easily pollute the surrounding soil and air. Hydrogen energy is called the ultimate energy source for mankind in the 21st century. The hydrogen energy industry includes three links: hydrogen production, hydrogen storage, and hydrogen application. Hydrogen production is the foundation of hydrogen storage, and hydrogen storage is the bottleneck currently facing the industry. Currently, there are many hydrogen storage products on the market, generally including methanol hydrogen storage, high-pressure hydrogen storage, liquefied hydrogen storage, solid-state adsorption hydrogen storage, and metal hydride hydrogen storage. Except for high-pressure hydrogen storage, which has been commercialized, other hydrogen storage products are still in the experimental stage. There is a lot of room for development in glass hydrogen storage. Technical issues

[0004] The purpose of the present invention is to provide a method for manufacturing a microporous glass skeleton hydrogen storage material to solve the problem that the large-scale use of glass mentioned in the above background technology will also bring about a series of other glass-related problems. As time goes by, more and more waste glass and glass products will appear. These waste glass and glass products piled on the ground can easily pollute the surrounding soil and air. Hydrogen energy is called the ultimate energy source for mankind in the 21st century. The hydrogen energy industry includes three links: hydrogen production, hydrogen storage and application. Hydrogen production is the basis of hydrogen storage, and hydrogen storage is the bottleneck currently facing the industry. There are many hydrogen storage products on the market, generally including methanol hydrogen storage, high-pressure hydrogen storage, liquefied hydrogen storage, solid-state adsorption hydrogen storage and metal hydride hydrogen storage. Except for high-pressure hydrogen storage, which has been commercialized, other hydrogen storage products are still in the experimental stage, and there is a large room for development in glass hydrogen storage. Technical Solutions

[0005] To achieve the above object, the present invention provides the following technical solution: a method for manufacturing a microporous glass skeleton hydrogen storage material, comprising the following steps:

[0006] S1, crushing the glass into a powder state with a particle size of 1 micron;

[0007] S2. Adding a foaming agent, a modifying additive and a foam stabilizer and mixing them uniformly;

[0008] S3, sintering, increasing pores, stabilizing pores, annealing, boiling in water, and drying to form a glass microporous skeleton structure rich in microporous framework structure, and the boiling temperature is 100° C. and the time is 30 hours;

[0009] S4. Prepare medium solution for later use;

[0010] S5. The reserved glass microporous skeleton structure, medium solution and hydrogen storage composite material are compositely blended and the blended product is dried to become a hydrogen storage finished product.

[0011] Preferably, the foaming agent includes sodium bicarbonate, sodium carbonate, and sodium silicate; the modifying additive includes water, griseofulvin, ritonavir, cholesterol, and modified soybean lecithin; and the foam stabilizer includes P2O5, P2O5, and B2O3, respectively, generated under high temperature conditions by trisodium phosphate, tripotassium phosphate, and boric acid. These products have a tetrahedral structure and are easy to form a continuous network, thereby increasing the viscosity of the melt, thereby stabilizing the bubbles and enhancing the network structure.

[0012] Preferably, when preparing the glass microporous skeleton structure in step S3, 30 parts of nitrite, 10 parts by weight of copper salt, 30 parts by weight of spodumene, 15 parts by weight of lepidolite and 15 parts by weight of nano zinc oxide powder are weighed, proportioned and stirred for 120 minutes at a temperature of 120°C.

[0013] Preferably, during the sintering in step S3, the mold is placed into the furnace along with the roller to be heated. When the furnace temperature rises to 130°C, sodium bicarbonate begins to gradually decompose to form sodium carbonate. A large number of through-pore bubbles are generated through this chemical reaction, and the microporous bubbles release carbon dioxide and water. When the temperature reaches 270°C, the sodium bicarbonate is completely decomposed to form a microporous frame of the preliminary structure. When the furnace temperature continues to rise to 850°C, the heated sodium silicate expands in volume, further enlarging the micropores, stabilizing the structural frame, reacting with the broken glass powder and releasing a large amount of gas, and then solidifying and forming by gradual cooling.

[0014] Preferably, during the annealing and demolding in step S3, the mold is placed into the annealing furnace along with the roller to be heated to 98°C-102°C and kept at a constant temperature for 60-120 minutes. The mold is then removed and cooled to 50°C before being opened to take out the formed filter plate or filter cartridge.

[0015] Preferably, when forming the glass microporous skeleton structure in step S3, spodumene, lepidolite and nano zinc oxide are first mixed evenly, and finally nitrite and copper salt are mixed together, and after being fully mixed, the mixture is taken out of the cylinder for use.

[0016] Preferably, in step S4, the medium solution is prepared by taking 40 parts by weight of white latex, 35 parts by weight of deionized water, 15 parts by weight of methanol and 10 parts by weight of other ingredients, placing them in a container according to the preparation ratio and mixing and stirring.

[0017] Preferably, the mixing and stirring is performed at a stirring speed of 60 rpm and a stirring time of 120 min.

[0018] Preferably, the other ingredients (10 parts by weight) include monoethanolamine (MEA), N-methyldiethanolamine (MDEA), and piperazine (PZ), and the content of monoethanolamine (MEA) is 5 parts by weight, N-methyldiethanolamine (MDEA) is 3 parts by weight, and piperazine (PZ) is 10 parts by weight.

[0019] Preferably, when the hydrogen storage product is produced in step S5, the medium solution is first sprayed on the surface of the glass microporous skeleton structure, and then the hydrogen storage composite material is spread flat on the glass microporous structure to allow the composite material and the solution to become one with the glass microporous skeleton structure. After the surface is dried, the coating is repeated three times and then dried again. The dried product is then baked in a high-temperature furnace at a baking temperature of 250°C, and becomes a hydrogen storage product after cooling out of the furnace. Beneficial effects

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] 1. The present invention improves the value of glass recycling and achieves high-quality recycling of resources. At the same time, it improves the mechanical properties of the composite material, keeps the entire glass microporous skeleton structure covered with the hydrogen storage composite material, allows spodumene and lepidolite to play the role of lithium elements, strengthens the catalytic effect of nitrite and copper salts and the crystal structure strength produced by nano-zinc oxide, and enables the glass microporous structure hydrogen storage composite material to reversibly absorb, store and release large amounts of hydrogen in a high temperature environment (200°C), solving the problem that hydrogen storage products produced by traditional technologies have relatively mediocre effects.

[0022] 2. In the present invention, when used for installation in a tank, the composite material with a microporous glass structure only needs to be cut by a saw according to the shape and size of the tank body to meet the assembly requirements, making installation and disassembly very simple. When used, it has the characteristics of high temperature resistance, impact resistance, easy installation, and high safety. At the same time, it has lower cost, longer life, high efficiency and energy saving, green and environmental protection, and the material has a hydrogen storage capacity of more than 18% by weight. It can reversibly absorb, store and release hydrogen in large quantities under high temperature conditions, promote the safe use of hydrogen in power generation, combustion and transportation, and improve the efficiency of green energy use. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] FIG1 is a structural diagram of a method for manufacturing a microporous glass skeleton hydrogen storage material according to the present invention. Best Mode for Carrying Out the Invention

[0024] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the implementation regulations described are only part of the embodiments of the present invention, not all of the embodiments. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making any creative efforts shall fall within the scope of protection of the present invention.

[0025] Referring to FIG1 , a method for manufacturing a microporous glass skeleton hydrogen storage material includes the following steps:

[0026] Step 1: crush the glass into a powder state with a particle size of 1 micron.

[0027] Step 2: Add a foaming agent, a modifying additive and a foam stabilizer and mix them evenly. The foaming agent includes sodium bicarbonate, sodium carbonate, and sodium silicate. The modifying additive includes water, griseofulvin, ritonavir, cholesterol, and modified soybean lecithin. The foam stabilizer includes trisodium phosphate, tripotassium phosphate, boric acid, etc., which are respectively generated under high temperature conditions. P2O5, P2O5, and B2O3. These products have a tetrahedral structure and are easy to form a continuous network, thereby increasing the viscosity of the melt, thereby stabilizing the bubbles and enhancing the network structure.

[0028] Step 3: sintering, pore increase, pore stabilization, annealing, boiling, and drying to form a glass microporous skeleton structure rich in microporous framework structure, and the boiling temperature is 100°C and the time is 30 hours. When preparing the glass microporous skeleton structure, 30 parts by weight of nitrite, 10 parts by weight of copper salt, 30 parts by weight of spodumene, 15 parts by weight of lithium mica and 15 parts by weight of nano zinc oxide powder are weighed and mixed, and stirred for 120 minutes at a temperature of 120°C.

[0029] The mold is put into the furnace along with the roller to be heated. When the furnace temperature rises to 130℃, sodium bicarbonate begins to gradually decompose to form sodium carbonate. Through this chemical reaction, a large number of penetrating microporous bubbles are generated, and the microporous bubbles release carbon dioxide and water. When the temperature reaches 270℃, the sodium bicarbonate is completely decomposed to form a microporous framework with a preliminary structure. When the furnace temperature continues to rise to 850℃, the heated sodium silicate expands in volume, further enlarging the micropores, stabilizing the structural framework, reacting with the broken glass powder and releasing a large amount of gas. It is then gradually cooled and solidified into a shape.

[0030] The mold is placed in an annealing furnace along a roller conveyor to heat up to between 98°C and 102°C and then maintained at a constant temperature for 60 to 120 minutes. The mold is then removed and cooled to 50°C before being opened to remove the formed filter plate or filter cartridge.

[0031] When making the glass microporous skeleton structure, first mix spodumene, lepidolite and nano zinc oxide, and finally mix nitrite and copper salt together. After fully mixing, take out of the cylinder and set aside.

[0032] Step 4: Prepare a medium solution for use: 40 parts by weight of white latex, 35 parts by weight of deionized water, 15 parts by weight of methanol, and 10 parts by weight of other ingredients are placed in a container according to the preparation ratio and mixed and stirred.

[0033] The stirring speed of the mixing was 60 rpm and the stirring time was 120 min.

[0034] The other ingredients (10 parts by weight) include monoethanolamine (MEA), N-methyldiethanolamine (MDEA), and piperazine (PZ), and the proportions include 5 parts by weight of monoethanolamine (MEA), 3 parts by weight of N-methyldiethanolamine (MDEA), and 10 parts by weight of piperazine (PZ).

[0035] Step 5: The prepared glass microporous skeleton structure, medium solution and hydrogen storage composite material are compositely blended and the blended product is dried to become a hydrogen storage finished product.

[0036] First, the medium solution is sprayed on the surface of the glass microporous skeleton structure, and then the hydrogen storage composite material is spread flat on the glass microporous structure to allow the composite material and the solution to become one with the glass microporous skeleton structure. After the surface is dried, it is repeatedly coated three times and then dried again. The dried product is then baked in a high-temperature furnace at a baking temperature of 250°C. After cooling out of the furnace, it becomes a hydrogen storage product.

[0037] The method of use and working principle of this device are as follows: the glass is crushed into a powder state with a particle size of 1 micron, and after adding a foaming agent, a modifying additive and a foam stabilizer and uniformly mixing, it is then melted at high temperature, foamed, annealed and boiled in water (the boiling temperature is 100°C and the time is 30 hours) to form a hydrogen storage skeleton material rich in microporous framework structure. During the sintering process, the inorganic foaming materials of sodium bicarbonate, sodium carbonate and sodium silicate play the role of increasing pores, stabilizing pores, releasing gas and stabilizing microporous structure under different temperatures to form a hydrogen storage skeleton material with a fully through microporous structure; the ratio of the hydrogen storage composite material is 30 parts by weight of nitrite, 10 parts by weight of copper salt, 30 parts by weight of spodumene, 15 parts by weight of lepidolite and nanosilicon. 15 parts by weight of nano zinc oxide powder are weighed, proportioned, and stirred for 120 minutes at a temperature of 120°C. During stirring, spodumene, lepidolite, and nano zinc oxide are first mixed, and finally nitrite and copper salt are mixed together. After being fully mixed, the mixture is taken out of the cylinder for standby use. Then, a medium solution is prepared by taking 45 parts by weight of white latex, 35 parts by weight of deionized water, 10 parts by weight of methanol, and 10 parts by weight of other ingredients, and placing them in a container according to the preparation ratio for mixing and stirring at a speed of 60 rpm and a stirring time of 120 minutes. A mixed solution (medium solution) is obtained by this process for standby use. Then, the reserved glass microporous skeleton structure, medium solution, and hydrogen storage composite material are compositely blended.

[0038] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for manufacturing a microporous glass skeleton hydrogen storage material, characterized in that: The following steps are involved: S1, crushing the glass into a powder state with a particle size of 1 micron; S2, adding a foaming agent, a modifying additive and a foam stabilizer and mixing them uniformly; S3, sintering, pore increasing, pore stabilization, annealing, boiling, and drying to form a glass microporous skeleton structure rich in microporous framework structure, and the boiling temperature is 100° C. and the time is 30 hours; S4, prepare medium solution for standby use; S5. The reserved glass microporous skeleton structure, medium solution and hydrogen storage composite material are compositely blended and the blended product is dried to become a hydrogen storage finished product.

2. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: The foaming agent includes sodium bicarbonate, sodium carbonate, and sodium silicate; The modified additives include water, griseofulvin, ritonavir, cholesterol, and modified soybean lecithin; The foam stabilizer includes trisodium phosphate, tripotassium phosphate and boric acid.

3. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S3, when preparing the glass microporous skeleton structure, 30 parts by weight of nitrite, 10 parts by weight of copper salt, 30 parts by weight of spodumene, 15 parts by weight of lithium mica and 15 parts by weight of nano zinc oxide powder are weighed, proportioned and stirred for 120 minutes at a temperature of 120°C.

4. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S3, during sintering, the mold is placed into the furnace along with the rollers for heating. When the furnace temperature rises to 130°C, sodium bicarbonate begins to decompose to form sodium carbonate, producing interconnected microporous bubbles, which release carbon dioxide and water. When the temperature reaches 270°C, the sodium bicarbonate is completely decomposed to form a microporous framework of the initial structure. When the furnace temperature continues to rise to 850°C, the heated sodium silicate expands in volume to further increase the micropores, stabilize the structural framework, react with the broken glass powder, and release a large amount of gas, and then solidifies into a shape by gradual cooling.

5. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S3, when annealing and demolding, the mold is placed into the annealing furnace along with the roller to be heated to 98°C-102°C for constant temperature, and the constant temperature time is controlled at 60-120 minutes. The mold is then removed and cooled to 50°C for opening the mold, and the formed filter plate or filter cartridge is taken out.

6. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S3, when making the glass microporous skeleton structure, spodumene, lepidolite and nano zinc oxide are first mixed evenly, and nitrite and copper salt are mixed together, and after being fully mixed, the mixture is taken out of the barrel for use.

7. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S4, a medium solution is prepared by taking 40 parts by weight of white latex, 35 parts by weight of deionized water, 15 parts by weight of methanol and 10 parts by weight of other ingredients, placing them in a container according to the preparation ratio and mixing and stirring them.

8. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 7, characterized in that: The mixing and stirring was performed at a stirring speed of 60 rpm and for a stirring time of 120 min.

9. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 7, characterized in that: The other ingredients (10 parts by weight) include monoethanolamine, N-methyldiethanolamine, and piperazine, and the proportions are 5 parts by weight of monoethanolamine, 3 parts by weight of N-methyldiethanolamine, and 10 parts by weight of piperazine.

10. The method for manufacturing a microporous glass skeleton hydrogen storage material according to claim 1, characterized in that: In step S5, when the hydrogen storage product is manufactured, the medium solution is sprayed on the surface of the glass microporous skeleton structure, and the hydrogen storage composite material is spread on the glass microporous structure to make the composite material and the solution become one with the glass microporous skeleton structure. After the surface is dried, it is repeatedly coated three times and then dried again. The dried product is then baked in a high-temperature furnace at a baking temperature of 250°C. After cooling out of the furnace, it becomes a hydrogen storage product.

Citation Information

Patent Citations

  • Micro-crystallographic foamed glass prepared from tailings of titanium separation and preparation method

    CN105948512A

  • Method for preparing microcrystalline foam glass by utilizing solid waste

    CN108423997A

  • Manufacturing method for sintering nanoparticles into hydrogen storage material

    CN113979406A

  • Manufacturing method of hydrogen storage material with waste glass microporous structure

    CN113998667A

  • Manufacturing method of sheet, block, tubular and special-shaped materials for hydrogen storage

    CN113998988A