Electrochemical cell having semi-solid electrodes and method of manufacturing the same
The use of 3D carbon foam coated with an electrolyte-based slurry and metallic foils in semi-solid electrodes addresses the limitations of conventional electrochemical cells, enhancing energy density and charge-discharge efficiency while reducing costs and environmental impact.
Patent Information
- Application Number
- PCT/IN2024/050311
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-19
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional electrochemical cells face challenges such as high manufacturing costs, limited thickness of electrodes, usage of toxic solvents, and difficulties in attaching metallic tabs to carbon foam due to brittleness, which restricts energy density and efficiency.
The development of semi-solid electrodes using a 3D carbon foam coated with an electrode slurry composed of active materials, conductive additives, and a binder dissolved in an electrolyte, with metallic foils attached to form current collectors, reducing Li-ion diffusion paths and enabling successful attachment of metallic tabs for improved electrical connection.
This approach reduces manufacturing costs, increases energy density, and enhances charge-discharge rates by providing a more efficient 3D conducting network, while eliminating the use of toxic solvents and improving the attachment of metallic tabs, resulting in a cost-effective and environmentally friendly electrochemical cell.
Smart Images

Figure IN2024050311_24102024_PF_FP_ABST
Abstract
Description
ELECTROCHEMICAL CELL HAVING SEMI-SOLID ELECTRODES AND METHOD OF MANUFACTURING THE SAMEFIELD OF INVENTION
[0001] The present invention relates to electrochemical cells, and more particularly, to an electrochemical cell having semi- solid electrodes and a method of manufacturing the same.BACKGROUND OF THE INVENTION
[0002] Batteries are typically constructed of solid electrodes, separators, electrolyte, and ancillary components such as, for example, packaging, thermal management, cell balancing, consolidation of electrical current carriers into terminals, and / or other such components. The electrodes typically include an active material, conductive materials, binders and other additives. Conventional manufacturing processes of electrodes include coating a current collector with a slurry composed of the active material, conductive additives and a binder dissolved or dispersed in a solvent. The solvent is evaporated, and the dry solid matrix is calendared to a desired thickness. Thereafter, the electrodes are cut and packaged with other components. Electrolyte is injected thereto, and the entire electrode package is sealed for forming the electrochemical cell.
[0003] Conventional batteries use two-dimensional (2D) current collectors made of metals such as, aluminium (Al) or copper (Cu), which are expensive metals. Also, fabrication of such batteries requires complicated and expensive manufacturing processes, such as, electrode casting, calendaring, electrode drying, etc. In addition, the manufacturing processes are only suitable for electrodes having a limited thickness. Generally, the thickness of conventional electrodes is limited to 100 pm, since porosity, tortuosity, impedance, and ion diffusion via the thickness of the electrodes worsen significantly with an increase in the thickness of the electrodes. Any increase is the thickness greater than 100 pm results in significant decrease in rate capability thereof.
[0004] Conventional electrochemical cells are generally constructed by coating the active material on both sides of the current collector to increase a ratio of active material to inactive material. A spacer is often placed between the electrodes, i.e., the anode and thecathode, to make a standard electrochemical cell. Several such electrochemical cells are typically stacked on top of each other, usually with a spacer between them, to form a stack of electrochemical cells.
[0005] The conventional techniques for preparation of the electrode slurry involves dispersing the active material into a solvent and then coating the slurry on the 2D current collector. However, such conventional techniques involve usage of toxic solvents. Also, energy density of the electrode slurry is highly limited as a limited amount of surface gets exposed to an electrolyte. In such conventional techniques, a major problem is limited points of contact between the electrode slurry and the current collector, and internal connection within the active material in the electrode slurry.
[0006] For connection of the electrochemical cell to an external circuit, it is required that the electrodes are connected with metallic tabs. Further, attaching metallic tabs to a carbon foam to form semi-solid electrodes can be challenging due to brittleness of the carbon foam, and also due to different properties of the carbon foam and the metallic tabs.
[0007] It is therefore desirable to provide techniques for manufacturing an electrochemical cell capable of addressing the aforesaid shortcomings, in a manner that the cost of the manufacturing process thereof is reduced while bringing greater amount of electrolyte material in contact with the electrodes. It is also desired to make the electrochemical cell more environment friendly by doing away with toxic solvents, while reducing Li-ion diffusion paths in the electrodes. There also exists a need in the art to provide a technique for successfully attaching metallic tabs to the carbon foam irrespective of the brittleness of the carbon foam, and different properties of the metallic tabs and the carbon foam.OBJECTS OF THE INVENTION
[0008] An object of the present invention is to provide an electrochemical cell having semi- solid electrodes fabricated by coating an electrode slurry on a carbon foam, and a method of manufacturing the same.
[0009] Another object of the present invention is to provide an environment friendly electrochemical cell and a manufacturing method thereof.
[0010] Another object of the present invention is to efficiently reduce Li-ion diffusion paths in the electrodes by using a three-dimensional (3D) conductive network in the electrode slurry.
[0011] Another object of the present invention is to provide an electrochemical cell having metallic tabs successfully attached to the carbon foam to provide electrical connection to external circuits, and a manufacturing method thereof.
[0012] Still another object of the present invention is to provide a cost-effective electrochemical cell and a method of manufacturing the same, several such electrochemical cells capable of being stacked together to form a battery.SUMMARY OF THE INVENTION
[0013] The summary is provided to introduce aspects related to electrochemical cells and method of manufacturing of the same. Other aspects and advantages of the invention will become apparent from the following description, taken in conjunction with the accompanying drawings, illustrating by way of example the principles of the invention.
[0014] An aspect of the present invention relates to an electrochemical cell including one or more semi-solid electrodes. Each semi-solid electrode has a three-dimensional (3D) carbon foam coated with an electrode slurry prepared through mixing of an active material, one or more conductive additives and a binder dissolved in an electrolyte. At least one metallic foil is attached to the 3D carbon foam coated with the electrode slurry to form the semi- solid electrode.
[0015] According to an embodiment of the present invention, the at least one metallic foil acts as a current collector of the semi-solid electrode. The metallic foil is made of a conductive material including any of Aluminium (Al) and Copper (Cu).
[0016] According to an embodiment of the present invention, the active material is selected from the group consisting of Lithium Iron Phosphate (LFP) and graphite.
[0017] Another aspect of the present invention pertains to a method of manufacturing the electrochemical cell. The method includes preparing an electrode slurry by mixing an active material, one or more conductive additives and a binder dissolved in an electrolyte,impregnating the 3D carbon foam with the electrode slurry, and attaching the metallic foil with the 3D carbon foam coated with the electrode slurry to form a semi-solid electrode.
[0018] According to an embodiment of the present invention, the preparation of the electrode slurry includes mixing the active material and the conductive additives at room temperature, after the binder is dissolved in the electrolyte for 2-3 hours of mixing.
[0019] According to an embodiment of the present invention, the metallic foil is coated with a binder dissolved in a solvent. The metallic foil coated with the binder is pasted and pressed to the 3D carbon foam impregnated with the electrode slurry, to form the semi-solid electrode.
[0020] According to an embodiment of the present invention, the electrochemical cell includes a separator disposed between adjacent semi-solid electrodes for insulating the adjacent semi-solid electrodes. Several such semi-solid electrodes with the separator arranged therebetween are stacked together to form the electrochemical cell.
[0021] According to an embodiment of the present invention, the electrochemical cell includes a top cap assembly and a bottom cap assembly separated by a sealing gasket. The electrochemical cell including a plurality of semi-solid electrodes with the separator arranged therebetween stacked together are accommodated in the bottom cap assembly with one or more tabs, the metallic foil extending to the top cap assembly for connection of the tabs to external circuits.
[0022] According to an embodiment of the present invention, a plurality of electrochemical cells are stacked together with a spacer therebetween to form a battery.
[0023] Other aspects and advantages of the invention will become apparent from the following description, taken in conjunction with the accompanying drawings, illustrating by way of example the principles of the invention.BRIEF DESCRIPTION OF ACCOMPANYING DRAWINGS
[0024] The accompanying drawings constitute a part of the description and are used to provide further understanding of the present invention. Such accompanying drawings illustrate an embodiment of the present invention which is used to describe the principles of the present invention together with the description. The foregoing aspects and many of theadvantages of this invention will become more readily appreciated as the same becomes better understood by the reference to the following detailed description, when taken in conjunction with the accompanying drawings, wherein:
[0025] Fig. 1 illustrates a perspective front view of an electrochemical cell, in accordance with an embodiment of the present invention;
[0026] Fig. 2A illustrates various representations of a top cap assembly of the electrochemical cell, in accordance with an embodiment of the present invention;
[0027] Fig. 2B illustrates various representations of a bottom cap assembly of the electrochemical cell, in accordance with an embodiment of the present invention;
[0028] Fig. 3 illustrates various representations of two semi-solid electrodes of the electrochemical cell stacked together, in accordance with an embodiment of the present invention;
[0029] Fig. 4 illustrates a flowchart showing various steps involved in a method of manufacturing the electrochemical cell, in accordance with an embodiment of the present invention;
[0030] Fig. 5 illustrates a graphical representation of variation in discharge capacity of a semi- solid electrode of the electrochemical cell with respect to change in capacity rate (C) thereof, in accordance with an embodiment of the present invention;
[0031] Figs. 6A and 6B illustrate graphical representations showing variation in rate capability performance and cyclic stability at the capacity rate of C / 3 of the semi-solid electrode with respect to change in charge-discharge cycle, in accordance with an embodiment of the present invention;
[0032] Fig. 7 illustrates a graphical representation of variation in charge-discharge capacity of the semi-solid electrode at different capacity rates, in accordance with an embodiment of the present invention;
[0033] Figs. 8A and 8B illustrate graphical representations showing variation in rate capability performance of the electrochemical cell at different charge-discharge cycles andthe cyclic stability at a fixed rate of C / 3, in accordance with an embodiment of the present invention;
[0034] Fig. 9 illustrates a graphical representation of Electrochemical Impedance Spectroscopic (EIS) data of the semi-solid electrode with a series resistance of 1.5 Ohm, in accordance with an embodiment of the present invention; and
[0035] Fig. 10 illustrates a graphical representation showing variation in capacity of the semi-solid electrodes at different C rates, in accordance with an embodiment of the present invention.DETAILED DESCRIPTION OF THE INVENTION
[0036] The detailed description set forth below in connection with the appended drawings is intended as a description of various embodiments of the present invention and is not intended to represent the only embodiments in which the present invention may be practiced. Each embodiment described in this disclosure is provided merely as an example or illustration of the present invention, and should not necessarily be construed as preferred or advantageous over other embodiments. The detailed description includes specific details for the purpose of providing a thorough understanding of the present invention. However, it will be apparent to those skilled in the art that the present invention may be practiced without these specific details.
[0037] As used in the description herein and throughout the claims that follow, the meaning of “a,” “an,” and “the” includes plural reference unless the context clearly dictates otherwise. Also, as used in the description herein, the meaning of “in” includes “in” and “on” unless the context clearly dictates otherwise.
[0038] The present invention relates to an electrochemical cell comprising at least two semi-solid electrodes stacked with a separator therebetween to form cathode and anode of the electrochemical cell, and a method for manufacturing the same. The semi-solid electrodes of the electrochemical cell are fabricated by impregnating a carbon foam in an electrode slurry composed of an active material, conductive additives, and a binding agent dissolved or dispersed in an electrolyte. The carbon form is a three-dimensional (3D) carbon foam capable of introducing a 3D conducting network within the electrode slurry so as to efficiently reduce Li-ion diffusion path in the electrode slurry. This improves charging rateof the electrochemical cell. The carbon foam impregnated with the electrolyte based slurry is connected with metallic foils to form current collectors at the anode and the cathode side of the electrochemical cell.
[0039] Fig. 1 illustrates a perspective view of the electrochemical cell 100 which includes a top cap assembly 102 and a bottom cap assembly 104 with a sealing gasket 106 arranged therebetween. The top cap assembly 102 and the bottom cap assembly 104 may include threaded slots. One or more bolts 108, such as M3 bolts, may be used to fasten the top cap assembly 102 and the bottom cap assembly 104 by passing the bolts 108 through the threaded slots. The sealing gasket 106 may be made of an elastomeric material, and may be in the form of a rectangular ring. The sealing gasket 106 is disposed on a groove formed in the bottom cap assembly 104. The sealing gasket 106 may be formed of Ethylene Propylene Diene Monomer (EPDM) or Neoprene, and the like. The top case assembly 102 may contain terminals 110 for connection of a cathode and an anode of the electrochemical cell 100 to external circuits.
[0040] Referring now to Fig. 2A, where various representations of the top cap assembly102 are shown. A body / housing of the top cap assembly 102 may be made of Polytetrafluoroethylene (PTFE), and may include the threaded slots 202 for fastening with the bottom cap assembly 104. The top cap assembly 102 may also include a cathode terminal 204-1 and an anode terminal 204-2, each having a slit 206 for accommodating a tab of a current collector of an electrode of the electrochemical cell 100. Each slit 206 may have a width of approximately 0.5mm. The tabs of the current collectors are tightly held in the slits 206 with the help of terminal bolts 208, such as M2 bolts, passing through threaded holes 210 formed in the cathode terminal 204-1 and the anode terminal 204-2. Copper lugs 212 are coupled with the cathode terminal 204-1 and the anode terminal 204-2 to provide a path for electric current to pass from the cathode terminal 204-1 and the anode terminal 204-2 to the terminals 110 of the electrochemical cell 100. The cathode terminal 204-1 and the anode terminal 204-2 may be made of metals, such as, Al or Cu. The terminal bolts 208 are passed into the threaded holes 210 through the copper lugs 212 and sealing O-rings 214. The sealing O-rings 214 may be made of elastomeric material, such as, Ethylene Propylene Diene Monomer (EPDM), neoprene, and the like.
[0041] Fig. 2B illustrates the bottom cap assembly 104 including a slot 216 for accommodating a separator / filter 218 for insulating electrodes arranged on both sidesthereof. The separator 218 may include a rectangular PTFE frame 220 with a Polythene (PE) micromesh filter 222 attached thereto. The bottom cap assembly 104 may be made of PTFE material.
[0042] Fig. 3 illustrates various representations of semi-solid electrodes 302-1 and 302- 2 stacked together with the separator 218 disposed therebetween to form a stack 300 of cathode and anode of the electrochemical cell 100. The electrodes 302-1 and 302-2 are disposed in corresponding slots provided in the bottom cap assembly 104. Each of the electrodes 302-1 and 302-2 is formed by immersing or coating a 3D carbon foam 304-1 / 304- 2 with an electrode slurry composed of an active electrode material, conductive additives and a binding agent dissolved or dispersed in an electrolyte. The active material of the electrode slurry may be selected as Lithium Ferrophosphate (LFP) or graphite, depending on requirements of the electrode. Mixing of the active material in the electrolyte based slurry increases interaction points for conductive paths of the 3D carbon foam 304-1 / 304-2, thereby improving energy density of the electrochemical cell 100. Further, since the electrode slurry is not dissolved in a toxic solvent, the electrodes formed by deposition of the electrode slurry on the carbon foam 304-1 / 304-2 is free from toxic chemicals.
[0043] The 3D carbon foam 304-1 / 304-2 impregnated with the electrolyte based slurry is attached to a metallic foil 306-1 / 306-2 made of a conducting metal, such as, Aluminium (Al) or Copper (Cu). The metallic foils 306-1 / 306-2 include a tab 308-1, 308-2 for contacting the cathode and anode terminals 204-1, 204-2 of the top cap assembly 102. Attachment of the metallic foils 306-1, 306-2 with the 3D carbon foams 304-1, 304-2 impregnated with the electrolyte based slurry is done by firstly coating the metallic foils 306-1, 306-2 with a binder dissolved in a solvent, and thereafter pasting and pressing the binder coated metallic foils 306-1, 306-2 to the 3D carbon foams 304-1, 304-2, to form the semi-solid electrodes 302-1, 302-2. This integration of the slurry coated carbon foam 304- 1, 304-2 with the Al / Cu foil 306-1, 306-2 enhances conductivity of the electrode 302-1, 302- 2, and reduces the internal resistance of the electrochemical cell 100.
[0044] The slurry coated carbon foam 304-1, 304-2 introduces a 3D conducting framework in slurry dissolved in the electrolyte. The 3D conductive framework increases conducting contact points throughout the active material slurry. This reduces Li-ion diffusion pathways in the slurry. The 3D conducting framework remains in close contact with slurry particles, and hence provides an increased number of contact points for easyelectron transfer. This improves charge-discharge rates and also lowers heat production while reducing internal resistance of the electrochemical cell 100.
[0045] The bottom cap assembly 104 shown in Fig. 2B accommodates a full cell stack 300 with current collectors (foils 306-1, 306-2) with tabs 308-1, 308-2 of both the anode and cathode extending towards the top cap assembly 102. When the stack 300 of the semisolid electrodes 302-1, 302-2 are accommodated in the bottom cap assembly 104, the tabs 308-1, 308-2 of the metallic foils 306-1 / 306-2 pass into the slits 206 of the cathode and anode terminals 204-1, 204-2 of the top cap assembly 102 to pass electric current to the terminals 110 through the copper lugs 212.
[0046] The electrodes 302-1, 302-2, both the anode and the cathode, are in semi-solid form. Particularly, the electrochemical cell 100 includes a semi-solid positive electrode 302- 1 coated on the 3D carbon foam 304-1. The current collector 306-1, such as Al current collector, may be attached on back side of the 3D carbon foam 304-1. In a similar manner, a semi-solid negative electrode 302-2 is coated on another 3D carbon foam 304-2. Another current collector 306-2, such as Cu current collector, may be attached on back side of the 3D carbon foam 304-2. The separator 218 is disposed between the semi-solid positive electrode 302-1 and the semi-solid negative electrode 302-2 to keep the two semi-solid electrodes 302-1, 302-2 apart and prevent electrical short circuits, while also allowing transport of ionic charge carriers that are needed to close the circuit during the passage of current in the electrochemical cell 100.
[0047] Fig. 4 illustrates a flowchart showing various steps involved in a method 400 of manufacturing the electrochemical cell 100. The method 400 includes a step S402 of preparing an electrode slurry by mixing an active material, one or more conductive additives and a binding agent dissolved in an electrolyte. The method 400 includes, at step S404, impregnating the 3D carbon foam with the electrolyte based slurry. Thereafter, at step S406, the 3D carbon foam impregnated with the electrolyte based slurry is pasted on to a metallic foil to form a semi-solid electrode. Two such semi-solid electrodes are stacked together to form a cathode and an anode of the electrochemical cell 100.
[0048] The binder of the electrode slurry is dissolved in the electrolyte, preferably an organic electrolyte. After the binder is dissolved in the electrolyte, preferably after 2-3 hr of mixing, the active material and conductive additives are mixed and dispersed properly bymechanical mixing at room temperature. This provides the anode or cathode slurry depending on the type of active material being used.
[0049] The 3D carbon foam 304-1, 304-2 may include any commercially available carbon foam and may have the following properties:Density: 0.2 - 1.0g / cm3;Porosity: 30 - 80%;Aperture: 0.01 - 6mm;Tensile strength: 2 - 5mpa;Tensile modulus: 300 - 500MPa;Thermal expansion coefficient: 5.0ppm / °C;Thermal conductivity: 25 - 80W / m.k;Resistivity: 1.0 x 10-2 - 10-5 Q M;Maximum operating temperature: 600 °C (in air), 3000 °C (in inert gas).
[0050] The 3D carbon foam 304-1, 304-2 is preferably cut into rectangular shape, and then poured and coated with the electrolyte based slurry. Preferably, the slurry coated carbon foam 304-1, 304-2 is left for settling at room temperature for overnight.
[0051] The slurry coated carbon foams 304-1, 304-2 are attached to metal foils 306-1, 306-2. For attaching the metal foil 306-1, 306-2, a binder is dissolved in the solvent, and the binder dissolved solvent is coated to the metal foils 306-1, 306-2. Thereafter, the slurry coated carbon foam 304-1, 304-2 is attached to the binder coated metal foil 306-1, 306-2.
[0052] Fig. 5 illustrates a graphical representation of variation in discharge capacity of the semi-solid electrodes 302-1 / 302-2 contained of half of the electrochemical cell 100 at various capacity rates (C). At the C rate of C / 20, the discharge capacity reached a value of 168 mAh / g. At C / 10, the discharge capacity reached a value of 167 mAh / g. Further, at the C rates of C / 5 and C / 3, the discharge capacity reached the values of 163 and 157 mAh / g. Fig. 6A illustrates a graphical plot showing variation in specific capacity with discharging and charging efficiency at various C rates of the semi-solid electrode 302-1 / 302-2. The charging-discharging efficiency remains close to 99.7% for the progressive chargedischarge cycles. Fig. 6B shows a graphical plot depicting variation in specific capacity while showing charging-discharging efficiency variation at various cycles at the fixed C rateof C / 3 of the semi-solid electrode 302-1 / 302-2 showing 96.1% of charging / discharge capacity retention after 200 cycles.
[0053] Fig. 7 illustrates a graphical representation showing variation in chargedischarge capacity of the semi-solid electrode 302-1 / 302-2 at different C rates at a mass loading of 12.9 mg / cm2At the C rate of C / 10, the discharge capacity reached approximately 135 mAh / g. Fig. 8A illustrates a graphical representation showing variation in specific capacity along with discharging and charging-discharging efficiency at various C rates of the electrochemical cell 100. Fig. 8B shows a graphical plot depicting variation in specific discharge capacity with charging-discharging efficiency and the cyclic stability at various cycles at the C rate of C / 3 of the electrochemical cell 100 at C / 3 showing 96.6% of discharge capacity retention after 35 cycles.
[0054] Fig. 9 illustrates a graphical representation depicting Electrochemical Impedance Spectroscopic (EIS) data of the semi-solid electrode 302-1 / 302-2 with a series resistance of 1.5 Ohm. Fig. 10 illustrates a graphical representation showing variation in capacity of the semi-solid electrodes 302-1 / 302-2 depicting charge-discharge traces at different capacity rates. The discharge capacity reached a value of approximately 143 mAh / g at the C rate of C / 20.
[0055] The electrochemical cell 100 of the present invention is capable of achieving a reduction in capex and operating cost in the manufacturing method thereof. A cell processing energy as a result of simplified manufacturing method may be reduced, and less number of equipment are utilized for production of the electrochemical cell 100. Water and NMP consumption involved in the electrode manufacturing is reduced, as the electrolyte based slurry is made in the electrolyte directly and not in water and NMP. The electrochemical cell 100 achieves higher energy density as a result of higher mass loading of the electrode active material. The denser semi-solid electrode material results in tailoring of volume, mass and cost contribution of inactive materials, making the electrochemical cell 100 commercially viable. The time involved in fabrication and assembling the electrochemical cell 100 is significantly reduced. The reduction in electrode preparation time also reduces exposure time of the electrode materials to temperature fluctuations or humidity, thus reducing the risk of degradation of the electrode materials, and thereby, the electronic properties of the electrodes.
[0056] In view of the present disclosure which describes the present invention, all changes, modifications and variations within the meaning and range of equivalency are considered within the scope and spirit of the invention. It is to be understood that the aspects and embodiment of the disclosure described above may be used in any combination with each other. Several of the aspects and embodiment may be combined together to form a further embodiment of the disclosure.
Claims
CLAIMS:
1. An electrochemical cell (100) comprising: one or more semi-solid electrodes (302-1, 302-2), each semi-solid electrode comprising a three-dimensional (3D) carbon foam (304-1, 304-2) coated with an electrode slurry prepared through mixing of an active material, one or more conductive additives and a binder dissolved in an electrolyte, wherein at least one metallic foil (306-1, 306-2) is attached to the 3D carbon foam (304-1, 304-2) coated with the electrode slurry.
2. The electrochemical cell (100) as claimed in claim 1, wherein: the at least one metallic foil (306-1, 306-2) acts as a current collector of the semisolid electrode (30-1, 302-2), and the at least one metallic foil (306-1, 306-2) is made of a conductive material including any of Aluminium (Al) and Copper (Cu).
3. The electrochemical cell (100) as claimed in claim 1, wherein the at least one metallic foil (306-1, 306-2) is coated with a binder dissolved in a solvent.
4. The electrochemical cell (100) as claimed in claim 3, wherein the at least one metallic foil (306-1, 306-2) coated with the binder is pasted to the 3D carbon foam (304-1, 304-2).
5. The electrochemical cell (100) as claimed in claim 1, further comprising a separator disposed between adjacent semi-solid electrodes (30-1, 302-2) of the one or more semi-solid electrodes (30-1, 302-2) for insulating the adjacent semi-solid electrodes (30-1, 302-2).
6. The electrochemical cell (100) as claimed in claim 1, wherein the active material is selected from the group consisting of Lithium Iron Phosphate (LFP) and graphite.
7. The electrochemical cell (100) as claimed in claim 1, further comprising a top cap assembly and a bottom cap assembly separated by a sealing gasket, wherein the electrochemical cell (100) is accommodated in the bottom cap assembly with one or more tabs the at least one metallic foil (306-1, 306-2) extending to the top cap assembly.
8. A method of manufacturing an electrochemical cell (100), the method comprising: preparing an electrode slurry by mixing an active material, one or more conductive additives and a binder dissolved in an electrolyte; impregnating a three-dimensional (3D) carbon foam (304-1, 304-2) with the electrode slurry; and attaching at least one metallic foil (306-1, 306-2) with the 3D carbon foam (304-1, 304-2) coated with the electrode slurry to form a semi-solid electrode (30-1, 302-2).
9. The method as claimed in claim 8, wherein the preparation of the electrode slurry comprises mixing the active material and the one or more conductive additives at room temperature, after the binder is dissolved in the electrolyte for 2-3 hours of mixing.
10. The method as claimed in claim 8, wherein: the at least one metallic foil (306-1, 306-2) is coated with a binder dissolved in a solvent, and the at least one metallic foil (306-1, 306-2) coated with the binder is pasted to the 3D carbon foam (304-1, 304-2).
11. The method as claimed in claim 8, wherein the at least one metallic foil (306- 1 , 306- 2) is made of a conductive material including any of Al and Cu.
Citation Information
Patent Citations
Lithium-ion cell utilizing electrodes made from aqueous slurry
IN202241045461A
Porous semi-solid electrode and methods of manufacturing the same
US20150357626A1
Semi-solid electrodes with porous current collectors and methods of manufacture
US20160308218A1