Security tag

The security tag with a two-dimensional crystal arrangement in a resin layer addresses the challenge of visible light region counterfeiting by being invisible in visible light and detectable in other regions, providing a robust anti-counterfeiting solution through its unique diffraction pattern.

WO2024219017A1PCT designated stage expired Publication Date: 2024-10-24MURATA MFG CO LTD +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/045925
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2023-12-21
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing security tags lack effective anti-counterfeiting measures, particularly in the visible light region, making them susceptible to forgery and counterfeiting.

Method used

A security tag featuring a resin layer with colloidal particles arranged to form a unique two-dimensional crystal, which is difficult to visually recognize in the visible light region, and detectable through a distinct diffraction pattern in other light regions, ensuring a high anti-counterfeiting effect.

Benefits of technology

The security tag effectively prevents counterfeiting by being invisible in visible light, making it difficult to replicate, and its unique diffraction pattern in other light regions ensures authenticity verification, thereby enhancing the anti-counterfeiting effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023045925_24102024_PF_FP_ABST
    Figure JP2023045925_24102024_PF_FP_ABST
Patent Text Reader

Abstract

A security tag 1 includes a plurality of colloidal particles 10 and a resin layer 20. The plurality of colloidal particles 10 are, when in a state of being embedded in the resin layer 20, arranged so as to be spaced apart from each other in a plane direction perpendicular to the thickness direction, and at least one type of two-dimensional crystal R1 composed of the plurality of colloidal particles 10 is present.
Need to check novelty before this filing date? Find Prior Art

Description

Security Tag

[0001] The present invention relates to security tags.

[0002] Patent Document 1 discloses an anti-counterfeiting structure comprising a particle fixing layer having spherical particles and a particle fixing resin for holding and fixing the spherical particles, the particle fixing resin containing one or more types of resin and arranged so that more than half of the height of the spherical particles is not buried, the spherical particles are arranged in a single plane with an area filling rate of 30% or more over the entire surface or in any shape, and the average particle size is 2.5 μm or less, and 70% or more of the particles are within the range of 0.8 to 1.2 times the average particle size.

[0003] Patent No. 5228666

[0004] The authenticity of the anti-counterfeit structure described in Patent Document 1 is determined by utilizing a color change that is confirmed by moving the position of the light source or observation point.

[0005] However, in the anti-counterfeiting structure described in Patent Document 1, the color change is visible, so it is not possible to make it difficult to see in the visible light range. Therefore, the anti-counterfeiting structure described in Patent Document 1 has room for improvement in terms of increasing the anti-counterfeiting effect.

[0006] The present invention has been made to solve the above problems, and has as its object to provide a security tag that can exhibit a high degree of anti-counterfeiting effect.

[0007] The security tag of the present invention is characterized in that it comprises a plurality of colloidal particles and a resin layer, the plurality of colloidal particles being embedded in the resin layer and arranged at a distance from each other along a plane direction perpendicular to the thickness direction, and at least one type of two-dimensional crystal formed by the plurality of colloidal particles is present.

[0008] According to the present invention, it is possible to provide a security tag that can exhibit a high degree of anti-counterfeiting effect.

[0009] Fig. 1 is a schematic plan view showing an example of a security tag according to a first embodiment of the present invention. Fig. 2 is a schematic cross-sectional view showing an example of a cross-section along the thickness direction of the security tag shown in Fig. 1. Fig. 3 is a schematic cross-sectional view showing another example of a cross-section along the thickness direction of the security tag shown in Fig. 1. Fig. 4 is a schematic diagram showing an example of a diffraction pattern derived from the two-dimensional crystal shown in Fig. 1. Fig. 5 is a schematic plan view showing an example of a security tag according to a second embodiment of the present invention. Fig. 6 is a schematic diagram showing an example of a diffraction pattern derived from the two-dimensional crystal shown in Fig. 5. Fig. 7 is a schematic plan view showing an example of a security tag according to a third embodiment of the present invention.

[0010] The security tag of the present invention is described below. Note that the present invention is not limited to the following configuration and may be modified as appropriate without departing from the spirit of the present invention. In addition, a combination of multiple individual preferred configurations described below also constitutes the present invention.

[0011] The following embodiments are merely examples, and it goes without saying that partial substitution or combination of the configurations shown in different embodiments is possible. From embodiment 2 onwards, descriptions of matters common to embodiment 1 will be omitted, and differences will be mainly described. In particular, similar effects resulting from similar configurations will not be mentioned one after the other for each embodiment.

[0012] In the following description, when no particular distinction is made between the various embodiments, they will simply be referred to as the "security tag of the present invention."

[0013] The drawings shown below are schematic diagrams, and the dimensions, aspect ratio, scale, etc. may differ from those of the actual product.

[0014] In this specification, unless otherwise specified, terms indicating the relationship between elements (e.g., "parallel," "perpendicular," etc.) and terms indicating the shape of elements not only mean the literal strict form, but also mean a range that is substantially equivalent, for example, a range that includes a difference of about a few percent.

[0015] The security tag of the present invention is characterized in that it comprises a plurality of colloidal particles and a resin layer, the plurality of colloidal particles being embedded in the resin layer and arranged at a distance from each other along a plane direction perpendicular to the thickness direction, and at least one type of two-dimensional crystal formed by the plurality of colloidal particles is present.

[0016] The security tag of the present invention is used for security purposes, such as determining the authenticity of an article. For example, if a manufacturer, distributor, or the like attaches the security tag of the present invention to a genuine article in advance, it becomes possible to determine whether the article is genuine or counterfeit by checking whether the security tag of the present invention is attached to the article in question.

[0017] [First Embodiment] In a security tag according to a first embodiment of the present invention, the two-dimensional crystal has six-fold symmetry when viewed in the thickness direction.

[0018] Fig. 1 is a schematic plan view showing an example of a security tag according to embodiment 1 of the present invention, and Fig. 2 is a schematic cross-sectional view showing an example of a cross section along the thickness direction of the security tag shown in Fig. 1.

[0019] The security tag 1 shown in FIGS. 1 and 2 includes a plurality of colloidal particles 10 and a resin layer 20 .

[0020] The plurality of colloid particles 10 are embedded in the resin layer 20. As a result, the plurality of colloid particles 10 are fixed to the resin layer 20.

[0021] In this specification, the colloidal particles being embedded in the resin layer means that 90% or more of the height of the colloidal particles in the thickness direction (the direction perpendicular to the paper surface in FIG. 1, and the vertical direction in FIG. 2) is embedded in the resin layer.

[0022] 2, the colloid particles 10 are completely buried in the resin layer 20. As a result, the colloid particles 10 are protected by the resin layer 20.

[0023] The modes in which the colloid particles 10 are completely embedded in the resin layer 20 include a mode in which the colloid particles 10 are in contact with the surface of the resin layer 20 from the inside, and a mode in which the colloid particles 10 are located inside the surface of the resin layer 20.

[0024] The colloid particles 10 are arranged apart from one another along a plane direction perpendicular to the thickness direction. The colloid particles 10 are not arranged so as to pile up in the thickness direction. In other words, the colloid particles 10 are arranged two-dimensionally, not three-dimensionally.

[0025] In the security tag 1, the colloid particles 10 are arranged two-dimensionally while embedded in the resin layer 20, making the colloid particles 10 less visible in the visible light range than when the colloid particles 10 are arranged three-dimensionally. Furthermore, in the security tag 1, the resin layer 20 is often transparent, making the resin layer 20 less visible in the visible light range. Therefore, the security tag 1 having such a plurality of colloid particles 10 and resin layer 20 is less visible in the visible light range.

[0026] It is assumed that the security tag 1 is attached to, for example, an expensive item, such as a painting or a watch. In this case, it is assumed that the security tag 1 is attached, for example, to the back of the painting or the back of the frame that houses the painting. It is also assumed that the security tag 1 is attached, for example, to the back of the dial of a watch. In either case, a third party attempting to counterfeit these expensive items would need to include the security tag 1 in the counterfeiting. However, because the security tag 1 is difficult to see in the visible light range, it is difficult for a third party attempting to manufacture a counterfeit product to notice the presence of the security tag 1. Therefore, it is unlikely that a third party would consider manufacturing a counterfeit product that includes the security tag 1, and therefore it is difficult to manufacture a complete counterfeit product that includes the security tag 1.

[0027] Therefore, the security tag 1, which is difficult to see in the visible light range, can exhibit a high degree of anti-counterfeiting effect.

[0028] Furthermore, the security tag 1 contains a two-dimensional crystal R1 made up of a plurality of colloidal particles 10.

[0029] When viewed in the thickness direction, the two-dimensional crystal R1 has six-fold symmetry.

[0030] The rotational symmetry of the two-dimensional crystal when viewed in the thickness direction is confirmed by the diffraction pattern described below.

[0031] The effect of the presence of the two-dimensional crystal R1 in the security tag 1 will be described below while showing an example of a method for manufacturing the security tag 1.

[0032] The security tag 1 is manufactured, for example, as follows.

[0033] First, a colloidal dispersion liquid is prepared in which a plurality of colloidal particles 10 are dispersed in a dispersion medium.

[0034] Examples of the dispersion medium include inorganic solvents such as water, and organic solvents such as alcohol.

[0035] Next, the colloidal dispersion is placed on the surface of a substrate such as a glass plate, whereby the colloidal particles 10 are arranged two-dimensionally on the surface of the substrate while being spaced apart from one another by electrostatic repulsion.

[0036] Then, after the dispersion medium in the colloidal dispersion is dried, a resin layer 20 is formed on the surface of the substrate so that the plurality of colloidal particles 10 remaining on the surface of the substrate are buried.

[0037] In this manner, the security tag 1 is manufactured.

[0038] In the security tag 1 manufactured in the above manner, a plurality of colloid particles 10 are arranged two-dimensionally while being spaced apart from one another, thereby forming a two-dimensional crystal R1. In the security tag 1 manufactured in the above manner, the two-dimensional crystal R1 is formed by utilizing the electrostatic repulsion between the plurality of colloid particles 10, and is therefore a unique two-dimensional crystal that cannot be reproduced. Therefore, it is impossible to counterfeit another security tag that contains the exact same two-dimensional crystal as the two-dimensional crystal R1.

[0039] Therefore, the security tag 1 having the two-dimensional crystal R1 can exhibit a high degree of anti-counterfeiting effect.

[0040] From the above, the security tag 1, which is difficult to see in the visible light region and contains the two-dimensional crystals R1, can realize a security tag that can exhibit a high degree of anti-counterfeiting effect.

[0041] When viewed in the thickness direction, the plurality of colloidal particles 10 are preferably provided over the entire security tag 1 .

[0042] When viewed in the thickness direction, the plurality of colloid particles 10 may be provided in only a portion of the security tag 1. In other words, when viewed in the thickness direction, the plurality of colloid particles 10 may not be provided in only a portion of the security tag 1.

[0043] When viewed in the thickness direction, the colloid particles 10 are preferably evenly spaced such that the distance (pitch) between the centers of adjacent colloid particles 10 in the surface direction is constant. In this case, when viewed in the thickness direction, the colloid particles 10 may be evenly spaced over the entire security tag 1 or may be evenly spaced over only a portion of the security tag 1.

[0044] The resin layer 20 has a first surface 20a and a second surface 20b that face each other in the thickness direction. In this case, the plurality of colloid particles 10 may be present on the first surface 20a side of the first surface 20a or the second surface 20b of the resin layer 20. In other words, the distance between the colloid particle 10 and the first surface 20a of the resin layer 20 may be smaller than the distance between the colloid particle 10 and the second surface 20b of the resin layer 20.

[0045] The plurality of colloid particles 10 may be present on the second surface 20b of the first surface 20a or the second surface 20b of the resin layer 20. In other words, the distance between the colloid particle 10 and the first surface 20a of the resin layer 20 may be greater than the distance between the colloid particle 10 and the second surface 20b of the resin layer 20.

[0046] Furthermore, the plurality of colloid particles 10 may be present between the first surface 20a and the second surface 20b of the resin layer 20. In other words, the distance between the colloid particle 10 and the first surface 20a of the resin layer 20 may be the same as the distance between the colloid particle 10 and the second surface 20b of the resin layer 20.

[0047] The colloidal particles 10 preferably have the same average particle size.

[0048] In this specification, the term "the same average particle size" means that the ratio of the average particle sizes is 0.97 or more and 1.03 or less.

[0049] The average particle diameters of the plurality of colloidal particles 10 may be different from one another, or may be partially different from one another.

[0050] In this specification, different average particle sizes means that the ratio of the average particle sizes is smaller than 0.97 or larger than 1.03.

[0051] The average particle size of the colloidal particles 10 is preferably 1 nm or more and 50 μm or less.

[0052] The average particle size of the colloidal particles is measured using a scanning electron microscope (SEM) for 100 to 200 colloidal particles out of all the colloidal particles contained in the security tag.

[0053] The colloid particles 10 may be inorganic particles or organic particles.

[0054] When the colloidal particles 10 are inorganic particles, examples of the constituent materials thereof include silica, titanium oxide, alumina, gold, silver, etc. Among these, silica and titanium oxide are preferred.

[0055] When the colloidal particles 10 are organic particles, examples of the constituent materials thereof include polymers such as polystyrene, polyacrylic acid ester, polymethacrylic acid ester, polyacrylonitrile, etc. Among these, polystyrene is preferred.

[0056] The resin layer 20 is preferably made of an ultraviolet curable resin.

[0057] Examples of materials constituting the resin layer 20 include polymer resins such as acrylic resins, epoxy resins, polyurethane resins, and polystyrene resins, as well as silicone resins and biopolymers. Among these resins, acrylic resins are preferred. Furthermore, among acrylic resins, polydialkylacrylamide is preferred. When the resin layer 20 is made of polydialkylacrylamide, if the colloid particles 10 are made of silica particles, the resin layer 20 is more likely to adsorb to the colloid particles 10, and the colloid particles 10 are more likely to be fixed to the resin layer 20.

[0058] In the visible light region, the refractive index of the colloidal particles 10 may be the same as the refractive index of the resin layer 20. In this case, the security tag 1 becomes completely invisible in the visible light region, thereby further enhancing the anti-counterfeiting effect of the security tag 1.

[0059] If security tag 1 becomes completely invisible in the visible light range, a third party attempting to manufacture a counterfeit product will not be able to detect the presence of security tag 1. Therefore, a third party will not be tempted to manufacture a counterfeit product that includes security tag 1, and therefore a complete counterfeit product that includes security tag 1 will not be manufactured. Furthermore, if security tag 1 becomes completely invisible, it is possible to prevent security tag 1 from adversely affecting the appearance (design) of an article.

[0060] In this specification, the visible light region means a wavelength region of 360 nm or more and 830 nm or less.

[0061] In this specification, the refractive indexes being the same in the visible light region means that the ratio of the refractive indexes in the visible light region is 0.95 or more and 1.05 or less.

[0062] In the visible light region, the refractive index of the colloidal particles 10 may be different from the refractive index of the resin layer 20 .

[0063] In this specification, the refractive indexes being different in the visible light region means that the ratio of the refractive indexes in the visible light region is smaller than 0.95 or larger than 1.05.

[0064] The refractive index of the colloidal particles 10 in the visible light region is preferably 1.3 or more and 2.3 or less.

[0065] The refractive index of the resin layer 20 in the visible light region is preferably 1.3 or more and 2.3 or less.

[0066] The refractive indexes of the colloidal particles and the resin layer in the visible light region are measured by the V-block method.

[0067] In the infrared region, the refractive index of the colloidal particles 10 may be different from the refractive index of the resin layer 20. In this case, the security tag 1 becomes detectable in the infrared region.

[0068] In this specification, the infrared light region means a wavelength region of 830 nm or more and 1 mm or less.

[0069] In this specification, the refractive indexes being different in the infrared region means that the ratio of the refractive indexes in the infrared region is smaller than 0.95 or larger than 1.05.

[0070] In the infrared light region, the refractive index of the colloidal particles 10 may be the same as the refractive index of the resin layer 20 .

[0071] In this specification, the refractive index in the infrared region being the same means that the ratio of the refractive indexes in the infrared region is 0.95 or more and 1.05 or less.

[0072] The refractive index of the colloidal particles 10 in the infrared region is preferably 0.4 or more and 5.7 or less.

[0073] The refractive index of the resin layer 20 in the infrared region is preferably 0.4 or more and 5.7 or less.

[0074] The refractive indexes of the colloidal particles and the resin layer in the infrared region are measured by the V-block method.

[0075] In the security tag 1, the refractive index of the colloid particles 10 is the same as that of the resin layer 20 in the visible light region, and the refractive index of the colloid particles 10 is different from that of the resin layer 20 in the infrared light region, making the security tag 1 invisible (undetectable) in the visible light region but detectable in the infrared light region. In this case, a third party attempting to manufacture a counterfeit product will not only be unable to notice the presence of the security tag 1, but even if they were to notice the presence of the security tag 1, they would be unable to manufacture a counterfeit security tag 1 that contains the unique, irreproducible two-dimensional crystal R1 and in which the refractive index of the colloid particles 10 is different from that of the resin layer 20 in the infrared light region.

[0076] If security tag 1 is detectable in the infrared light region, it can be attached to, for example, the back of a painting or the back of the dial of a watch, so that security tag 1 is not visible from the front of the painting, watch, etc. Even in this case, because infrared light (infrared rays) can pass through glass, plastic, etc., security tag 1 can be detected in the infrared light region.

[0077] In the security tag 1, if the refractive index of the colloid particles 10 is the same as the refractive index of the resin layer 20 in the visible light region, then the refractive index of the colloid particles 10 may be the same as the refractive index of the resin layer 20 in the infrared light region, or may be different from the refractive index of the resin layer 20. For example, in the security tag 1, if the refractive index of the colloid particles 10 is the same as the refractive index of the resin layer 20 in the visible light region and the refractive index of the colloid particles 10 is the same as the refractive index of the resin layer 20 in the infrared light region, then the detectability of the security tag 1 may be reduced, but the visibility of the security tag 1 is ensured.

[0078] In the security tag 1, if the refractive index of the colloid particles 10 is different from the refractive index of the resin layer 20 in the visible light region, that is, if the security tag 1 is detectable in the visible light region, the refractive index of the colloid particles 10 may be the same as or different from the refractive index of the resin layer 20 in the infrared light region. This is because, when the security tag 1 is not to be detected in the infrared light region, the relationship between the refractive indices of the colloid particles 10 and the resin layer 20 in the infrared light region does not affect the detectability of the security tag 1.

[0079] As shown in FIG. 2 , the security tag 1 may further include a substrate 30 in contact with the first surface 20 a of the resin layer 20 .

[0080] Since security tag 1 has substrate 30 , colloidal particles 10 are protected not only by resin layer 20 but also by substrate 30 .

[0081] In the example shown in Fig. 2, the colloid particles 10 are present on the first surface 20a side of the first surface 20a and the second surface 20b of the resin layer 20, and specifically, are in contact with the first surface 20a of the resin layer 20 from the inside. Furthermore, in the example shown in Fig. 2, the substrate 30 is in contact with the first surface 20a of the resin layer 20. Therefore, in the example shown in Fig. 2, the substrate 30 is in contact with the colloid particles 10.

[0082] The configuration in which the substrate 30 is in contact with the colloid particles 10, as shown in FIG. 2, is realized, for example, when the security tag 1 is manufactured by the above-described method, by using the substrate 30 as a substrate on which a colloidal dispersion containing the colloid particles 10 is placed.

[0083] The substrate 30 may be, for example, a transparent plate such as a glass plate or a plastic plate.

[0084] FIG. 3 is a schematic cross-sectional view showing another example of a cross section along the thickness direction of the security tag shown in FIG.

[0085] As shown in FIG. 3, security tag 1 may further include an intermediate layer 40 disposed between colloidal particles 10 and substrate 30 .

[0086] In the example shown in Fig. 3, the colloid particles 10 are present on the first surface 20a side of the first surface 20a and the second surface 20b of the resin layer 20, and specifically, are located more inward than the first surface 20a of the resin layer 20. That is, in the example shown in Fig. 3, the colloid particles 10 are spaced apart from the first surface 20a of the resin layer 20. Furthermore, in the example shown in Fig. 3, the substrate 30 is in contact with the first surface 20a of the resin layer 20. Therefore, in the example shown in Fig. 3, the colloid particles 10 and the substrate 30 are spaced apart from each other. In the above configuration, an intermediate layer 40 is provided between the colloid particles 10 and the first surface 20a of the resin layer 20, i.e., between the colloid particles 10 and the substrate 30.

[0087] By providing the intermediate layer 40 between the colloid particles 10 and the substrate 30, the colloid particles 10 are fixed to the substrate 30 via the intermediate layer 40. When the colloid particles 10 are fixed to the substrate 30, the structure of the two-dimensional crystal R1 made up of the colloid particles 10 is more likely to be maintained even if an external force is applied to the security tag 1, for example.

[0088] 3 , the configuration in which the intermediate layer 40 is provided between the colloid particles 10 and the substrate 30 can be realized, for example, when manufacturing the security tag 1 using the method described above, by using a substrate 30 on which the intermediate layer 40 has been formed in advance as the substrate on which the colloidal dispersion containing the colloid particles 10 is placed. When the colloidal dispersion is placed on the surface of the substrate 30 on which the intermediate layer 40 has been formed in advance, the colloidal particles 10 are adsorbed to the intermediate layer 40 and are aligned two-dimensionally.

[0089] The thickness of the intermediate layer 40 is, for example, 1 nm or more and 100 nm or less. That is, when the colloid particles 10 are separated from the first surface 20 a of the resin layer 20, the distance between the colloid particles 10 and the first surface 20 a of the resin layer 20 is, for example, 1 nm or more and 100 nm or less. When the colloid particles 10 are separated from the substrate 30, the distance between the colloid particles 10 and the substrate 30 is, for example, 1 nm or more and 100 nm or less.

[0090] Examples of materials that can be used to form the intermediate layer 40 include a silane coupling agent.

[0091] The security tag 1 is used to determine the authenticity of an article, for example, in the following manner.

[0092] When light is irradiated onto the security tag 1, a diffraction pattern originating from the two-dimensional crystal R1 appears. In the example shown in Fig. 1, the two-dimensional crystal R1 has six-fold symmetry, and therefore a six-fold symmetric diffraction pattern appears as shown in Fig. 4. Fig. 4 is a schematic diagram showing an example of a diffraction pattern originating from the two-dimensional crystal shown in Fig. 1. By detecting the diffraction pattern in this manner, it is possible to detect the security tag 1, which is difficult to see in the visible light region.

[0093] Furthermore, because the two-dimensional crystal R1 is a unique two-dimensional crystal that cannot be reproduced, the diffraction pattern derived from the two-dimensional crystal R1 is also a unique diffraction pattern that cannot be reproduced. In this way, a unique diffraction pattern determined by the arrangement, particle size, etc. of the colloidal particles 10 that make up the two-dimensional crystal R1 is detected from the security tag 1 containing the two-dimensional crystal R1.

[0094] Therefore, when the security tag 1 is attached to a genuine item, the authenticity of the item can be determined, for example, by the following procedure.

[0095] First, when light is irradiated onto the target item, it is confirmed whether a diffraction pattern derived from two-dimensional crystals is detected, thereby confirming whether a security tag of the same type as security tag 1 is attached to the target item. Then, if it is determined that a security tag is attached to the target item, it is confirmed whether the diffraction pattern detected from the target item is identical to the unique diffraction pattern of security tag 1 attached to the genuine item, thereby confirming whether the security tag attached to the target item is identical to security tag 1 attached to the genuine item.

[0096] When detecting security tag 1, light may be irradiated from a perpendicular direction (incident angle: 90°) to the main surface of security tag 1, or from another direction (incident angle: other than 90°).

[0097] When detecting the security tag 1, a diffraction pattern can be detected by the light reflected from the security tag 1 when the security tag 1 is irradiated with light.

[0098] When detecting the security tag 1, a diffraction pattern can be detected from the light that passes through the security tag 1 when the security tag 1 is irradiated with light.

[0099] When detecting security tag 1, a diffraction pattern can be detected by irradiating security tag 1 with light from a direction perpendicular to its main surface (incident angle: 90°) and detecting the light reflected perpendicularly from security tag 1. Therefore, when detecting security tag 1, the position of the light source that irradiates security tag 1 with light and the position of the detector that detects the light reflected from security tag 1 can be aligned; for example, the light source and detector can be integrated.

[0100] In contrast, the technology described in Patent Document 1 detects an anti-counterfeit structure by checking a color change by moving the positions of the light source or observation point. Therefore, the technology described in Patent Document 1 cannot detect an anti-counterfeit structure without moving the positions of the light source and observation point, for example, by aligning the positions of the light source and observation point.

[0101] As described above, when detecting the security tag 1, conditions such as the positional relationship between the light source and the detector are not limited, unlike when detecting the anti-counterfeit structure described in Patent Document 1.

[0102] Second Embodiment In a security tag according to a second embodiment of the present invention, the two-dimensional crystal has four-fold symmetry when viewed in the thickness direction.

[0103] Except for the above points, the security tag of the second embodiment of the present invention is similar to the security tag of the first embodiment of the present invention.

[0104] FIG. 5 is a schematic plan view showing an example of a security tag according to a second embodiment of the present invention.

[0105] The security tag 2 shown in FIG. 5 includes a two-dimensional crystal R2 formed of a plurality of colloidal particles 10.

[0106] When viewed in the thickness direction, the two-dimensional crystal R2 has four-fold symmetry.

[0107] When light is irradiated onto the security tag 2, a diffraction pattern originating from the two-dimensional crystal R2, in this case a diffraction pattern with four-fold symmetry as shown in Fig. 6, appears. Fig. 6 is a schematic diagram showing an example of a diffraction pattern originating from the two-dimensional crystal shown in Fig. 5.

[0108] The two-dimensional crystal R2 having four-fold symmetry is more difficult to realize than the two-dimensional crystal R1 having six-fold symmetry, and therefore the security tag 2 having the two-dimensional crystal R2 having four-fold symmetry can exhibit a higher anti-counterfeiting effect than the security tag 1 having the two-dimensional crystal R1 having six-fold symmetry.

[0109] Two-dimensional crystal R2 having four-fold symmetry can be realized, for example, by adjusting the thickness of the colloidal dispersion placed on the surface of a substrate when manufacturing security tag 2 using the same method as security tag 1. For example, the thickness of the colloidal dispersion can be changed by placing the colloidal dispersion on the surface of the substrate and then placing another substrate, such as a glass plate, on the surface of the colloidal dispersion. In this case, changing the thickness of the other substrate placed on the surface of the colloidal dispersion can change the weight of this other substrate, thereby adjusting the thickness of the colloidal dispersion. When the thickness of the colloidal dispersion is within a specific range, two-dimensional crystal R2 having four-fold symmetry is realized.

[0110] The above examples show that the two-dimensional crystals present in the security tag of the present invention have six-fold symmetry (Embodiment 1) or four-fold symmetry (Embodiment 2) when viewed in the thickness direction. However, the two-dimensional crystals present in the security tag of the present invention may have symmetry other than six-fold and four-fold symmetry when viewed in the thickness direction.

[0111] [Embodiment 3] In a security tag according to embodiment 3 of the present invention, there are multiple types of two-dimensional crystals.

[0112] In the security tag of the third embodiment of the present invention, the two-dimensional crystals of the plurality of types have symmetry axes along the plane direction that are different from one another.

[0113] Except for the above points, the security tag of the third embodiment of the present invention is similar to the security tags of the first and second embodiments of the present invention.

[0114] FIG. 7 is a schematic plan view showing an example of a security tag according to a third embodiment of the present invention.

[0115] The security tag 3 shown in FIG. 7 includes two-dimensional crystals R3a, R3b, R3c, R3d, and R3e, each of which is made up of a plurality of colloidal particles 10.

[0116] The two-dimensional crystal R3a, the two-dimensional crystal R3b, the two-dimensional crystal R3c, the two-dimensional crystal R3d, and the two-dimensional crystal R3e each have six-fold symmetry when viewed in the thickness direction.

[0117] The two-dimensional crystal R3a, the two-dimensional crystal R3b, the two-dimensional crystal R3c, the two-dimensional crystal R3d, and the two-dimensional crystal R3e may each have a symmetry other than six-fold symmetry, for example, four-fold symmetry, when viewed from the thickness direction.

[0118] The two-dimensional crystal R3a, the two-dimensional crystal R3b, the two-dimensional crystal R3c, the two-dimensional crystal R3d, and the two-dimensional crystal R3e each have a symmetry axis X3a, a symmetry axis X3b, a symmetry axis X3c, a symmetry axis X3d, and a symmetry axis X3e as symmetry axes along the surface direction.

[0119] In this specification, the symmetry axis along the plane direction means the symmetry axis along the plane direction when the two-dimensional crystal is line-symmetric when viewed from the thickness direction.

[0120] The directions of the symmetry axis X3a, the symmetry axis X3b, the symmetry axis X3c, the symmetry axis X3d, and the symmetry axis X3e are different from one another.

[0121] When the types of two-dimensional crystals in the security tag 3 are classified by the direction of the symmetry axis along the surface direction, there are five types of two-dimensional crystals: two-dimensional crystal R3a, two-dimensional crystal R3b, two-dimensional crystal R3c, two-dimensional crystal R3d, and two-dimensional crystal R3e, each of which has a different direction of the symmetry axis along the surface direction.

[0122] The two-dimensional crystals R3a, R3b, R3c, R3d, and R3e are each unique two-dimensional crystals that cannot be reproduced, and the combinations of the directions of the symmetry axes along the plane directions of these crystals are also unique combinations that cannot be reproduced. Therefore, a security tag 3 that includes the two-dimensional crystals R3a, R3b, R3c, R3d, and R3e can exhibit a higher level of anti-counterfeiting effectiveness.

[0123] The number of types of two-dimensional crystals present in the security tag 3 is not limited to five, and may be any number other than five.

[0124] In the security tag of the present invention, in embodiment 3, an example is given in which the types of two-dimensional crystals are classified according to the direction of the symmetry axis along the surface direction, but the types of two-dimensional crystals may also be classified according to their symmetry when viewed from the thickness direction, or according to other characteristics.

[0125] For example, when two-dimensional crystal types are classified by their symmetry when viewed in the thickness direction, the security tag of the present invention may contain multiple types of two-dimensional crystals that have different symmetries when viewed in the thickness direction. In this case, the security tag of the present invention may contain, for example, a mixture of two-dimensional crystals that have six-fold symmetry when viewed in the thickness direction (Embodiment 1) and two-dimensional crystals that have four-fold symmetry when viewed in the thickness direction (Embodiment 2). If the security tag of the present invention contains two-dimensional crystals that have four-fold symmetry when viewed in the thickness direction, the anti-counterfeiting effect is further enhanced.

[0126] By encoding information about the diffraction pattern derived from the two-dimensional crystals present in the security tag of the present invention, such as the shape, size, position, and direction of the symmetry axis along the surface direction, as well as information about what diffraction pattern appears when light is irradiated at what angle of incidence, the security tag can be identified using the encoded information, allowing the authenticity of the item to be determined.

[0127] The form of the security tag of the present invention is not particularly limited, and may be, for example, a film, a card, a sticker, or the like.

[0128] The present specification discloses the following:

[0129] <1> A security tag comprising: a plurality of colloidal particles; and a resin layer, wherein the plurality of colloidal particles are embedded in the resin layer and aligned at a distance from one another along a plane direction perpendicular to a thickness direction, and wherein at least one type of two-dimensional crystal constituted by the plurality of colloidal particles is present.

[0130] <2> The security tag according to <1>, wherein the two-dimensional crystal has six-fold symmetry when viewed from the thickness direction.

[0131] <3> The security tag according to <1>, wherein the two-dimensional crystal has four-fold symmetry when viewed from the thickness direction.

[0132] <4> The security tag according to any one of <1> to <3>, wherein there are multiple types of two-dimensional crystals, and the multiple types of two-dimensional crystals have symmetry axes along the plane direction that are different from one another.

[0133] <5> The security tag according to any one of <1> to <4>, wherein the resin layer has a first surface and a second surface that face each other in the thickness direction, and the colloidal particles are present on the first surface side of the first surface or the second surface of the resin layer.

[0134] <6> The security tag according to <5>, further comprising a substrate in contact with the first surface of the resin layer.

[0135] <7> The security tag according to <6>, wherein the substrate is in contact with the colloid particles.

[0136] <8> The security tag according to <6>, further comprising an intermediate layer provided between the colloidal particles and the substrate.

[0137] 1, 2, 3 Security tag 10 Colloid particle 20 Resin layer 20a First surface of resin layer 20b Second surface of resin layer 30 Substrate 40 Intermediate layer R1, R2, R3a, R3b, R3c, R3d, R3e Two-dimensional crystal X3a, X3b, X3c, X3d, X3e Axes of symmetry

Claims

1. A security tag comprising: a plurality of colloidal particles; and a resin layer, wherein the plurality of colloidal particles are embedded in the resin layer and aligned apart from one another along a plane direction perpendicular to a thickness direction, and wherein at least one type of two-dimensional crystal composed of the plurality of colloidal particles is present.

2. The security tag of claim 1, wherein said two-dimensional crystal has six-fold symmetry when viewed in said thickness direction.

3. The security tag of claim 1, wherein the two-dimensional crystal has four-fold symmetry when viewed in the thickness direction.

4. A security tag as described in any one of claims 1 to 3, wherein there are multiple types of two-dimensional crystals, and the multiple types of two-dimensional crystals have mutually different directions of symmetry axes along the plane direction.

5. A security tag as described in any one of claims 1 to 4, wherein the resin layer has a first surface and a second surface opposing each other in the thickness direction, and the colloidal particles are present on the first surface side of the first surface or the second surface of the resin layer.

6. The security tag of claim 5, further comprising a substrate in contact with said first surface of said resin layer.

7. The security tag of claim 6, wherein said substrate contacts said colloidal particles.

8. The security tag of claim 6, further comprising an intermediate layer disposed between said colloidal particles and said substrate.

Citation Information

Patent Citations

  • Display body and article with display body

    JP2014006272A

  • Plasmon resonance laminate, binder part formation composition, manufacturing method of plasmon resonance laminate and information recording medium

    JP2017217903A

  • Multi-hidden image security device

    JP2018517176A

  • Filler-containing film

    JP2022097477A