Method for manufacturing power storage device
The method of alternating pressing pressures for different active material layers in the manufacturing of power storage devices addresses the issue of current collector foil strain, improving structural integrity and energy density by minimizing pinhole formation.
Patent Information
- Application Number
- PCT/JP2024/006288
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-18
- Filing Date
- 2024-02-21
- Publication Date
- 2024-10-24
AI Technical Summary
Conventional methods for manufacturing power storage devices often result in strain and damage to current collector foils due to the application of hard-to-crush active materials, leading to pinholes and other structural issues.
A manufacturing method involving a first pressing step with a more easily crushed active material layer at higher pressure and a second pressing step with a harder-to-crush layer at lower pressure to minimize strain on the current collector foil.
This approach effectively suppresses damage to the current collector foil, reducing the likelihood of pinholes and enhancing the structural integrity and energy density of the power storage device.
Smart Images

Figure JP2024006288_24102024_PF_FP_ABST
Abstract
Description
Method for manufacturing an electricity storage device
[0001] The present invention relates to a method for manufacturing an electricity storage device.
[0002] Conventionally, there have been known methods for manufacturing an electricity storage device including an electrode unit in which active material layers (positive electrode active material layer and negative electrode active material layer) are formed on both sides of a current collector foil. Patent Document 1 discloses a method for manufacturing a bipolar battery electrode using a double-sided coated electrode for a bipolar battery, in which a crush-resistant active material is first applied to one side of the current collector and pressed, and then a crush-resistant active material is applied to the remaining side and pressed.
[0003] Japanese Patent Application Laid-Open No. 2006-128039
[0004] In the conventional method for manufacturing an electricity storage device, when a crush-resistant active material is first applied to one side of a current collector foil and then pressed, as disclosed in Patent Document 1, distortion is likely to occur in the current collector foil, and pinholes are likely to occur in the current collector foil. In particular, in Patent Document 1, a larger pressing pressure is applied to the side where the active material is less likely to be crushed (see paragraph
[0021] of the specification, etc.), and therefore distortion is likely to occur in the current collector foil due to the large pressing pressure when pressing the crush-resistant active material, and there is a risk of damage to the current collector foil, such as the generation of pinholes in the current collector foil.
[0005] An object of the present invention is to provide a method for manufacturing an electricity storage device that can suppress damage to current collector foils.
[0006] A method for manufacturing an electricity storage device according to one aspect of the present invention is a method for manufacturing an electricity storage device including a plurality of electrode units stacked in a stacking direction, each of the plurality of electrode units having at least a current collector foil, a positive electrode active material layer formed on one surface of the current collector foil, and a negative electrode active material layer formed on the other surface of the current collector foil, and the method for manufacturing the electricity storage device includes a first press step in which one of the positive electrode active material layer and the negative electrode active material layer is placed on the current collector foil and pressed, and a second press step after the first press step in which the other of the positive electrode active material layer and the negative electrode active material layer is placed on the current collector foil and pressed together with the one active material layer, and in the first press step, the one active material layer, which is more easily crushed than the other active material layer, is placed on the current collector foil and pressed with a pressure that is the same as or higher than a pressure used to press the other active material layer in the second press step.
[0007] According to the method for manufacturing an electricity storage device of the present invention, damage to the current collecting foil can be suppressed.
[0008] FIG. 1 is a perspective view showing the appearance of an electricity storage device according to an embodiment. FIG. 2 is a cross-sectional view showing the internal configuration of the electricity storage device according to an embodiment. FIG. 3 is a perspective view and a cross-sectional view showing the configuration of an electrode unit included in the electricity storage device according to an embodiment. FIG. 4 is a flowchart showing manufacturing steps in a manufacturing method for an electricity storage device according to an embodiment. FIG. 5 is a cross-sectional view showing manufacturing steps in a manufacturing method for an electricity storage device according to an embodiment. FIG. 6 is a cross-sectional view showing the configuration of an electricity storage pack. FIG. 7 is a cross-sectional view showing another configuration of an electricity storage pack.
[0009] (1) A method for manufacturing an electricity storage device according to one aspect of the present invention is a method for manufacturing an electricity storage device including a plurality of electrode units stacked in a stacking direction, each of the plurality of electrode units having at least a current collector foil, a positive electrode active material layer formed on one surface of the current collector foil, and a negative electrode active material layer formed on the other surface of the current collector foil. The method for manufacturing the electricity storage device includes: a first press step in which one of the positive electrode active material layer and the negative electrode active material layer is disposed on the current collector foil and pressed; and a second press step after the first press step in which the other of the positive electrode active material layer and the negative electrode active material layer is disposed on the current collector foil and pressed together with the one active material layer. In the first press step, the one active material layer, which is more easily crushed than the other active material layer, is disposed on the current collector foil and pressed with a pressure that is the same as or higher than a pressure used to press the other active material layer in the second press step.
[0010] According to this, in the method for manufacturing an electricity storage device, in the first press step, one active material layer that is more easily crushed than the other active material layer is placed on the current collector foil, and in the second press step, the current collector foil is pressed with a pressure that is the same as or higher than the pressure used to press the other active material layer. In this way, by making the active material layer that is more easily crushed the first press step is pressed with a relatively high pressure, distortion is less likely to occur in the current collector foil, and pinholes are less likely to occur in the current collector foil. In the second press step, the less crushable active material layer is pressed with a relatively low pressure, which prevents distortion in the current collector foil and therefore prevents pinholes from occurring in the current collector foil. This reduces damage to the current collector foil.
[0011] (2) In the method for manufacturing an electricity storage device described in (1) above, in the first pressing step, one of the active material layers having a higher porosity than the other active material layer may be placed on the current collector foil and pressed.
[0012] According to this, in the first pressing step, by disposing an active material layer that is highly porous before pressing on the current collector foil, it is possible to dispose an active material layer that is easily crushed on the current collector foil.
[0013] (3) In the method for manufacturing an energy storage device described in (1) or (2) above, in the first pressing step, one of the active material layers may be pressed, the one of the active material layers being larger in size than the other active material layer when viewed from the stacking direction.
[0014] If a smaller active material layer is placed on a current collector foil and pressed, and then a larger active material layer is placed on the current collector foil, the portion of one active material layer that protrudes beyond the other active material layer will not be supported by the other active material layer. In this case, when placing one active material layer on the current collector foil, the pressure applied to the portion where the other active material layer is placed may cause the current collector foil to be pushed in at the portion where the other active material layer is placed, resulting in an excessive amount of one active material layer being placed in that area. As a result, the amount of the protruding portion of the one active material layer may be unstable. When pressing one active material layer, the protruding portion is not faced by the other active material layer, so the protruding portion cannot be pressed sufficiently, and the protruding portion may become thick. As a result, the thickness of the protruding portion of one active material layer increases, and when stacking the electrode units, the thickened portion of one active material layer may apply a large amount of pressure to press down on the current collector foil, or wrinkles may form in the current collector foil, making stacking difficult. The protruding portion that cannot be pressed sufficiently may not sufficiently increase the bonding strength with the current collector foil, making the active material more likely to fall off. For this reason, in the first pressing step, the larger active material layer is pressed before the smaller active material layer. This prevents the above-mentioned problems from occurring.
[0015] (4) In the method for manufacturing an energy storage device described in any one of (1) to (3) above, in the first pressing step, a negative electrode active material layer may be pressed as the one active material layer, and in the second pressing step, a positive electrode active material layer may be pressed as the other active material layer.
[0016] According to this, since the negative electrode active material layer is generally larger in size than the positive electrode active material layer, the negative electrode active material layer is pressed before the positive electrode active material layer in the first pressing step, which prevents the thickness of the portion of the negative electrode active material layer that protrudes from the positive electrode active material layer from increasing, thereby preventing problems caused by the thickness of the protruding portion.
[0017] Hereinafter, with reference to the drawings, a description will be given of an energy storage device and a manufacturing method thereof according to an embodiment of the present invention (including its modified examples). The embodiments described below all show comprehensive or specific examples. The numerical values, shapes, materials, components, component arrangement and connection forms, manufacturing processes, and the order of manufacturing processes shown in the following embodiments are examples and are not intended to limit the present invention. In each drawing, dimensions and the like are not strictly illustrated. In each drawing, the same or similar components are designated by the same reference numerals.
[0018] In the following description and drawings, the longitudinal direction of the energy storage device, or the direction in which a pair of short side surfaces of the energy storage device face each other, is defined as the X-axis direction. The direction in which a pair of long side surfaces of the energy storage device face each other is defined as the Y-axis direction. The thickness direction of the energy storage device, the stacking direction of multiple electrode units, the stacking direction of current collecting foils and active material layers, the arrangement direction of a pair of end members, or the up-down direction is defined as the Z-axis direction. These X-axis, Y-axis, and Z-axis directions intersect each other (orthogonal in this embodiment). Depending on the usage mode, the Z-axis may not be the up-down direction, but for convenience of explanation, the following description will be made assuming that the Z-axis direction is the up-down direction.
[0019] In the following description, the positive X-axis direction refers to the direction of the X-axis arrow, and the negative X-axis direction refers to the direction opposite to the positive X-axis direction. When simply referring to the X-axis direction, it refers to both or either of the positive X-axis direction and the negative X-axis direction. The same applies to the Y-axis direction and the Z-axis direction. Expressions indicating relative directions or attitudes, such as parallel and orthogonal, also include cases where the directions or attitudes are not strictly those. Two directions being parallel does not only mean that the two directions are completely parallel, but also means that the directions are substantially parallel, that is, there is a difference of about a few percent. In the following description, when the term "insulation" is used, it means "electrical insulation."
[0020] (Embodiment) [1. General Description of Energy Storage Device 10] First, a general description of the energy storage device 10 according to the present embodiment will be provided. FIG. 1 is a perspective view showing the exterior of the energy storage device 10 according to the present embodiment. FIG. 2 is a cross-sectional view showing the internal configuration of the energy storage device 10 according to the present embodiment. Specifically, FIG. 2 is a cross-sectional view of the energy storage device 10 of FIG. 1 cut along the YZ plane passing through line II-II. FIG. 2 shows each component included in the energy storage device 10. FIG. 3 is a perspective view and a cross-sectional view showing the configuration of an electrode unit 100 included in the energy storage device 10 according to the present embodiment. Specifically, FIG. 3A is a perspective view showing the exterior of the electrode unit 100. FIG. 3B is a cross-sectional view showing the configuration of the electrode unit 100 of FIG. 3A cut along the YZ plane passing through line IIIb-IIIb. For ease of explanation, FIG. 3 omits the illustration of a seal portion 210 included in the electrode unit 100.
[0021] The power storage device 10 is a device that can charge with electricity from an external source and discharge electricity to an external source. In this embodiment, the power storage device 10 has a substantially rectangular parallelepiped shape. Specifically, the power storage device 10 is a bipolar battery. The power storage device 10 is used as a battery for driving or starting the engine of a mobile object such as an automobile, a motorcycle, a personal watercraft, a boat, a snowmobile, an agricultural machine, a construction machine, an automatic guided vehicle (AGV), or a railway vehicle for an electric railway. Examples of the automobile include an electric vehicle (EV), a hybrid electric vehicle (HEV), a plug-in hybrid electric vehicle (PHEV), and a fossil fuel (gasoline, diesel, liquefied natural gas, etc.) vehicle. Examples of the railway vehicle for an electric railway include a train, a monorail, a linear motor car, and a hybrid train equipped with both a diesel engine and an electric motor. The power storage device 10 can also be used as a stationary battery for home or business use.
[0022] As shown in FIGS. 1 and 2 , the energy storage device 10 includes a plurality of electrode units 100, end units 101 and 102, a plurality of separators 140, and a pair of end members 300. Each of the electrode units 100, end units 101, and end units 102 is a rectangular plate-like portion in a plan view, and is stacked in the Z-axis direction. In this embodiment, a plan view refers to a view from the stacking direction (Z-axis direction). The direction in which the electrode units 100, end units 101, and end units 102 are stacked (Z-axis direction) is also referred to as the stacking direction. The separators 140 are disposed between the electrode units 100 and the end units 101 and 102. The pair of end members 300 are disposed on both sides of the electrode units 100 and the end units 101 and 102 in the stacking direction (Z-axis direction). In this embodiment, two electrode units 100 are stacked in the stacking direction between the end unit 101 and the end unit 102, but the number of stacked electrode units 100 is not particularly limited. The shapes of the electrode units 100, end units 101, end units 102, etc. in plan view are also not particularly limited.
[0023] [1.1 Description of Electrode Unit 100] The configuration of the electrode unit 100 will be described in detail below, also with reference to Figure 3. The electrode unit 100 is a single unit in which active material layers are formed on both sides of a single current collector foil. Each of the multiple electrode units 100 has at least a current collector foil 110, a positive electrode active material layer 120 formed on one side of the current collector foil 110, a negative electrode active material layer 130 formed on the other side of the current collector foil 110, and a seal portion 210. In this embodiment, the thickness of the electrode unit 100 (thickness in the stacking direction) is approximately 135 µm to 190 µm.
[0024] The current collector foil 110 is a plate-like member that is rectangular in plan view. The current collector foil 110 is a metal foil. As shown in FIG. 3 , the current collector foil 110 has two metal layers 111 and 112 that are aligned in the stacking direction (Z-axis direction). The metal layers 111 and 112 are plate-like portions that have the same size and shape in plan view. Hereinafter, of the metal layers 111 and 112, the metal layer 111 on which the positive electrode active material layer 120 is formed will also be referred to as the positive electrode metal layer 111, and the metal layer 112 on which the negative electrode active material layer 130 is formed will also be referred to as the negative electrode metal layer 112. The positive electrode metal layer 111 is a metal layer that is located in the positive direction of the current collector foil 110 on the Z-axis, and the negative electrode metal layer 112 is a metal layer that is located in the negative direction of the current collector foil 110 on the Z-axis. In other words, the current collector foil 110 is formed by stacking the positive electrode metal layer 111 and the negative electrode metal layer 112 in a stacking direction, with the positive electrode metal layer 111 and the negative electrode metal layer 112 connected (contacting or bonded) to each other. One of the positive electrode metal layer 111 and the negative electrode metal layer 112 may be a metal foil, and the other may be a plated layer formed by plating the metal foil. Alternatively, both the positive electrode metal layer 111 and the negative electrode metal layer 112 may be metal foil. When both the positive electrode metal layer 111 and the negative electrode metal layer 112 are metal foils, the current collector foil 110 may be a clad material formed by bonding two metal foils together, or may have two metal foils that are connected (contacting) without being bonded to each other.
[0025] The material for the positive electrode metal layer 111 may be a metal such as aluminum, titanium, tantalum, or stainless steel, or an alloy thereof. Among these, aluminum or an aluminum alloy is preferred as the material for the positive electrode metal layer 111 from the perspective of balancing potential resistance, high conductivity, and cost. The positive electrode metal layer 111 may be in the form of a plated layer, but foil is preferred from the perspectives of processability and cost. In other words, aluminum foil is preferred as the positive electrode metal layer 111. The material for the negative electrode metal layer 112 may be a metal such as copper, nickel, stainless steel, or nickel-plated steel, or an alloy thereof, and among these, copper or a copper alloy is preferred. The negative electrode metal layer 112 may be in the form of a plated layer or foil (copper foil), and examples of copper foil include rolled copper foil and electrolytic copper foil. The thickness (thickness in the stacking direction) of the current collector foil 110 is approximately 20 μm to 30 μm. The thickness of the positive electrode metal layer 111 (thickness in the stacking direction) is about 5 μm to 20 μm, and the thickness of the negative electrode metal layer 112 (thickness in the stacking direction) is about 5 μm to 15 μm.
[0026] The positive electrode active material layer 120 is a positive electrode active material layer formed on one surface (the surface in the positive Z-axis direction) of the current collector foil 110. Specifically, the positive electrode active material layer 120 is formed on the positive electrode metal layer 111 (the outer surface (the surface in the positive Z-axis direction) of the positive electrode metal layer 111). The positive electrode active material layer 120 is formed in a rectangular shape that is smaller in size than the positive electrode metal layer 111 in a planar view, in accordance with the shape of the positive electrode metal layer 111. Smaller in size in a planar view means that the area in the XY plane is small. The same applies below. The thickness of the positive electrode active material layer 120 (thickness in the stacking direction) is approximately 70 μm to 100 μm.
[0027] The positive electrode active material layer 120 contains a positive electrode active material, and optionally contains a conductive agent, a binder, a thickener, a filler, and other optional components as needed. 2 (M1 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.), layered lithium transition metal oxides such as LiM2 2 O 4(M2 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.), spinel-type lithium transition metal oxides such as LiM3PO 4 , LiMSiO 4 , LiM3BO 3 Examples of suitable conductive materials include polyanion compounds such as Cr, Fe, Ni, Mn, Co, and the like (M3 is one or more metal elements selected from Li, Fe, Ni, Mn, Co, etc.). As the positive electrode active material, one of these compounds may be used alone, or two or more may be mixed together. The conductive agent contained in the positive electrode active material layer 120 is not particularly limited as long as it is conductive. Examples of conductive agents include carbon black such as furnace black, acetylene black, and ketjen black, and natural or artificial graphite. Examples of binders include fluororesins (polytetrafluoroethylene (PTFE), polyvinylidene fluoride (PVDF), etc.), sulfonated EPDM, and styrene butadiene rubber (SBR). Examples of thickeners include polysaccharide polymers such as carboxymethyl cellulose (CMC) and methyl cellulose.
[0028] The negative electrode active material layer 130 is a negative electrode active material layer formed on the other surface (the surface in the negative Z-axis direction) of the current collector foil 110. Specifically, the negative electrode active material layer 130 is formed on the negative electrode metal layer 112 (on the outer surface (the surface in the negative Z-axis direction) of the negative electrode metal layer 112). The negative electrode active material layer 130 is formed in a rectangular shape that is smaller in size than the negative electrode metal layer 112 in a planar view, in accordance with the shape of the negative electrode metal layer 112. The negative electrode active material layer 130 is formed in a larger size than the positive electrode active material layer 120 in a planar view. A larger size in a planar view refers to a larger area in the XY plane. The same applies below. In other words, the area in the XY plane of the negative electrode active material layer 130 is larger than that of the positive electrode active material layer 120. The thickness (thickness in the stacking direction) of the negative electrode active material layer 130 is approximately 45 μm to 60 μm.
[0029] The negative electrode active material layer 130 contains a negative electrode active material and, if necessary, contains optional components such as a conductive agent, a binder, a thickener, and a filler. The optional components such as the conductive agent, binder, thickener, and filler can be the same as those used in the positive electrode active material layer 120. The negative electrode active material is typically a material that can absorb and release lithium ions. Examples of negative electrode active materials include metals or semimetals such as Si and Sn; metal oxides or semimetal oxides such as Si oxide and Sn oxide; and carbon materials such as graphite and non-graphitic carbon (easily graphitizable carbon or non-graphitizable carbon).
[0030] The sealing portion 210 is a portion that is arranged around the positive electrode active material layer 120 or the negative electrode active material layer 130. In the present embodiment, the sealing portion 210 is an annular portion that is arranged around the positive electrode active material layer 120 and the negative electrode active material layer 130 over the entire periphery of the positive electrode active material layer 120 and the negative electrode active material layer 130. Specifically, the sealing portion 210 is formed in a rectangular annular shape along the outer periphery of the current collector foil 110 so as to cover the outer periphery of the current collector foil 110. The sealing portion 210 is formed from an insulating material such as polycarbonate (PC), polypropylene (PP), polyethylene (PE), polystyrene (PS), polyphenylene sulfide resin (PPS), polyphenylene ether (PPE (including modified PPE)), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polyether ether ketone (PEEK), tetrafluoroethylene perfluoroalkyl vinyl ether (PFA), polytetrafluoroethylene (PTFE), polyethersulfone (PES), polyamide (PA), ABS resin, or a composite material thereof.
[0031] The seal portions 210 of two adjacent electrode units 100 are connected to each other. The seal portions 210 may be connected to each other by being formed as a continuous, integral unit, or may be connected to each other by being joined by heat sealing (thermal welding), ultrasonic welding, laser welding, an adhesive, or the like. As a result, the seal portion 210 is disposed around the positive electrode active material layer 120 of one of the two electrode units 100 and the negative electrode active material layer 130 of the other of the two electrode units 100, and the seal portion 210 is provided between the current collecting foils 110 of the two electrode units 100. In other words, the seal portion 210 is provided continuously between the current collecting foils 110 of the two electrode units 100, sealing the space between the current collecting foils 110.
[0032] An electrolyte layer (not shown) is formed inside the seal portion 210 of each of the multiple electrode units 100. In this embodiment, the electrolyte layer is a non-aqueous liquid electrolyte (electrolytic solution), but it may also be a solid electrolyte (solid electrolyte) or a gel electrolyte. Any known electrolyte can be used as appropriate. The electrolyte solution (nonaqueous electrolyte) can be one in which an electrolyte salt is dissolved in a nonaqueous solvent. Examples of nonaqueous solvents include cyclic carbonates such as ethylene carbonate (EC) and propylene carbonate (PC), and chain carbonates such as diethyl carbonate (DEC), dimethyl carbonate (DMC), and ethyl methyl carbonate (EMC). A lithium salt is preferred as the electrolyte salt. Examples of the lithium salt include LiPF 6 , LiPO 2 F 2 , LiBF 4 , LiClO 4 , LiN(SO 2 F) 2 , LiN(SO 2 CF 3 ) 2 Examples of inorganic lithium salts include:
[0033] [1.2 Description of End Units 101 and 102] Next, the configuration of the end units 101 and 102 will be described in detail. The end unit 101 is disposed at the end of the multiple electrode units 100 in the negative Z-axis direction. The end unit 102 is disposed at the end of the multiple electrode units 100 in the positive Z-axis direction. The end units 101 and 102 are parts that sandwich the multiple electrode units 100 in the Z-axis direction.
[0034] The end unit 101 has at least a positive electrode metal layer 111, a positive electrode active material layer 120 formed on the surface of the positive electrode metal layer 111 in the Z-axis positive direction, and a sealing portion 220. The positive electrode metal layer 111 and the positive electrode active material layer 120 of the end unit 101 have the same configuration as the positive electrode metal layer 111 and the positive electrode active material layer 120 of the current collector foil 110 of the electrode unit 100 described above.
[0035] The sealing portion 220 is a portion arranged around the positive electrode active material layer 120. In the present embodiment, the sealing portion 220 is an annular portion arranged around the positive electrode active material layer 120 over the entire periphery of the positive electrode active material layer 120. Specifically, the sealing portion 220 is formed in a quadrangular annular shape along the outer periphery of the positive electrode metal layer 111 and the end member 300 so as to cover the outer periphery of the positive electrode metal layer 111 and the end member 300. The sealing portion 220 is formed of the same material as the sealing portion 210 of the electrode unit 100.
[0036] The seal portion 220 is connected to the seal portion 210 of the electrode unit 100 adjacent to the end unit 101. The connection between the seal portion 220 and the seal portion 210 is similar to the connection between the seal portions 210 described above, and therefore a detailed description thereof will be omitted. This provides a seal between the positive electrode metal layer 111 of the end unit 101 and the current collecting foil 110 of the electrode unit 100. The above-mentioned electrolyte layer (not shown) is formed inside the seal portion 220.
[0037] The end unit 102 has at least a current collector foil 110, a negative electrode active material layer 130 arranged on the surface of the current collector foil 110 in the negative Z-axis direction, and a seal portion 230. The current collector foil 110 and negative electrode active material layer 130 of the end unit 102 have the same configuration as the current collector foil 110 and negative electrode active material layer 130 of the electrode unit 100 described above.
[0038] The sealing portion 230 is a portion that is arranged around the negative electrode active material layer 130. In the present embodiment, the sealing portion 230 is an annular portion that is arranged around the negative electrode active material layer 130 over the entire periphery of the negative electrode active material layer 130. Specifically, the sealing portion 230 is formed in a quadrangular annular shape along the outer peripheries of the current collector foil 110 and the end member 300 so as to cover the outer peripheries of the current collector foil 110 and the end member 300. The sealing portion 230 is made of the same material as the sealing portion 210 of the electrode unit 100.
[0039] The seal portion 230 is connected to the seal portion 210 of the electrode unit 100 adjacent to the end unit 102. The connection between the seal portion 230 and the seal portion 210 is similar to the connection between the seal portions 210 described above, and therefore a detailed description will be omitted. This provides a seal between the current collector foil 110 of the end unit 102 and the current collector foil 110 of the electrode unit 100. The above-mentioned electrolyte layer (not shown) is formed inside the seal portion 230.
[0040] In this manner, the seal portions 210, 220, and 230 are connected to one another to form the seal member 200. The seal member 200 is a cylindrical (square cylindrical) member that is arranged so as to surround the entire periphery of the positive electrode metal layer 111, the negative electrode metal layer 112, the positive electrode active material layer 120, the negative electrode active material layer 130, the separator 140, and the end member 300, and seals these elements from the outside.
[0041] [1.3 Description of Separator 140 and End Member 300] The separator 140 is a microporous sheet made of resin. The separator 140 is disposed between the electrode units 100, between the end unit 101 and the electrode unit 100, and between the end unit 102 and the electrode unit 100. Specifically, the separator 140 is disposed between the positive electrode active material layer 120 and the negative electrode active material layer 130. Examples of materials used for the separator 140 include woven fabric, nonwoven fabric, and porous resin film. Among these, porous resin film is preferred. From the viewpoint of strength, a polyolefin such as polyethylene or polypropylene is preferred as the main component of the porous resin film. The separator 140 may be a multilayer film in which a layer containing a filler is formed on the surface of such a porous resin film. The separator 140 is formed in a rectangular shape that is larger than the negative electrode active material layer 130 in a plan view. In this embodiment, the size of separator 140 is smaller than that of current collector foil 110 in plan view, but may be larger than current collector foil 110 in plan view. The thickness of separator 140 (thickness in the stacking direction) is approximately 15 μm to 20 μm.
[0042] The end members 300 are members disposed closer to the ends of the energy storage device 10 in the stacking direction (Z-axis direction) than the plurality of electrode units 100. In the present embodiment, a pair of end members 300 are disposed at the ends of the energy storage device 10 closest to the negative Z-axis direction and the positive Z-axis direction. The pair of end members 300 are connected to the end units 101 and 102 (the positive electrode metal layers 111 of the end units 101 and 102). As a result, the pair of end members 300 sandwich the plurality of electrode units 100 and the end units 101 and 102 located therebetween from both sides in the stacking direction (Z-axis direction). The end members 300 are flat plate-shaped members (end plates). The end members 300 are electrically connected to other end members 300 of other energy storage devices 10 via other conductive members (bus bars, cooling plates, etc., not shown). The end members 300 are formed of a conductive member made of a metal such as aluminum, an aluminum alloy, copper, a copper alloy, or nickel, or a combination thereof, or a conductive member other than a metal. Because the end member 300 is connected to the positive electrode metal layer 111, it is preferably formed of the same material as the positive electrode metal layer 111, such as aluminum. The thickness of the end member 300 (thickness in the stacking direction) is approximately 0.5 mm to 3 mm. The energy storage device 10 may have another conductive member on the outside of the end member 300 (outside in the Z-axis direction).
[0043] In the above configuration, the separator 140, the positive electrode active material layer 120 and the negative electrode active material layer 130 sandwiching the separator 140 in the Z-axis direction, and the positive electrode metal layer 111 and the negative electrode metal layer 112 sandwiching these in the Z-axis direction may be referred to as a single energy storage element. In this case, the energy storage device 10 can also be said to be a group of energy storage elements having a configuration in which a plurality of energy storage elements stacked in the Z-axis direction are sandwiched between a pair of end members 300 in the Z-axis direction and are surrounded by a sealing member 200.
[0044] [2 Description of Manufacturing Method of Energy Storage Device 10] Next, a manufacturing method of the energy storage device 10 will be described. FIG. 4 is a flowchart showing manufacturing steps in the manufacturing method of the energy storage device 10 according to the present embodiment. Specifically, FIG. 4 is a flowchart showing manufacturing steps in the manufacturing method of the electrode unit 100, which is part of the manufacturing method of the energy storage device 10. FIG. 5 is a cross-sectional view showing manufacturing steps in the manufacturing method of the energy storage device 10 according to the present embodiment. Specifically, FIG. 5(a) shows a first press step in the manufacturing method of the energy storage device 10 (the manufacturing method of the electrode unit 100), and FIG. 5(b) shows a second press step in the manufacturing method of the energy storage device 10 (the manufacturing method of the electrode unit 100). FIG. 5 is a view corresponding to FIG. 3(b), and the seal portion 210 of the electrode unit 100 is not shown. In the first press step and the second press step, the seal portion 210 may or may not be formed in the electrode unit 100. In this embodiment, after the second pressing step, the seal portion 210 is disposed around the positive electrode active material layer 120 and the negative electrode active material layer 130 .
[0045] As shown in FIG. 4 , first, a current collector foil 110 is prepared, and a first pressing step is performed in which an active material layer is placed on one surface of the current collector foil 110 and pressed (S102). In the first pressing step, one of the positive electrode active material layer 120 and the negative electrode active material layer 130 is placed on the current collector foil 110 and pressed. In the present embodiment, the one active material layer is the negative electrode active material layer 130. That is, in the first pressing step, the negative electrode active material layer 130 is pressed as one active material layer. Specifically, as shown in FIG. 5 , in the first pressing step, the negative electrode active material layer 130 is placed on the surface of the current collector foil 110 facing in the negative Z-axis direction, and the negative electrode active material layer 130 is pressed with a pressure P1. The pressure P1 and a pressure P2, which will be described later, refer to pressures in the press line pressure. In (a) of Figure 5, instead of pressing the negative electrode active material layer 130 in a state where it is placed on the surface of the current collector foil 110 in the negative direction of the Z axis, the current collector foil 110 may be placed upside down, the negative electrode active material layer 130 may be placed on the surface of the current collector foil 110 in the positive direction of the Z axis, and pressed, and then the current collector foil 110 may be turned upside down to return to the position of (a) of Figure 5.
[0046] Next, after the first pressing step, a second pressing step is performed in which an active material layer is also placed on the other surface of the current collector foil 110 and pressed (S104). In the second pressing step, after the first pressing step, the other active material layer of the positive electrode active material layer 120 and the negative electrode active material layer 130 is placed on the current collector foil 110 and pressed together with one of the active material layers. In this embodiment, the other active material layer is the positive electrode active material layer 120. That is, in the second pressing step, the positive electrode active material layer 120 is pressed as the other active material layer. Specifically, as shown in FIG. 5 , in the second pressing step, the positive electrode active material layer 120 is placed on the surface of the current collector foil 110 in the positive direction of the Z axis, and the positive electrode active material layer 120 is pressed together with the negative electrode active material layer 130 with a pressure P2.
[0047] As described above, one active material layer is the negative electrode active material layer 130, and the other active material layer is the positive electrode active material layer 120. Therefore, one active material layer (negative electrode active material layer 130) is larger in size than the other active material layer (positive electrode active material layer 120) when viewed from the stacking direction (Z-axis direction). For this reason, in the first pressing step, one active material layer that is larger in size than the other active material layer when viewed from the stacking direction is pressed.
[0048] In this embodiment, one active material layer (negative electrode active material layer 130) is more easily crushed than the other active material layer (positive electrode active material layer 120). The pressure P1 in the first press step is the same as or higher than the pressure P2 in the second press step. Therefore, in the first press step, one active material layer that is more easily crushed than the other active material layer is placed on the current collector foil 110, and pressed at a pressure that is the same as or higher than the pressure used to press the other active material layer in the second press step. Specifically, in the first press step, the negative electrode active material layer 130 that is more easily crushed than the positive electrode active material layer 120 is placed on the current collector foil 110, and pressed at a pressure P1 that is the same as or higher than the pressure P2 used to press the positive electrode active material layer 120 in the second press step.
[0049] The definition of "easily crushed" is as follows. Ease of crushing can be determined by the press linear pressure applied to form active material layers with the same porosity. The press linear pressure refers to the value obtained by dividing the weight applied by the press by the width of the active material layer in contact with the press roll. A large press linear pressure applied to form active material layers with the same porosity means that the active material layer is less likely to be crushed, while a small press linear pressure means that the active material layer is more likely to be crushed. In designing the energy storage device 10, the porosity of each active material layer is optimized, so it is not necessarily the same and may even be different. In other words, arranging a negative electrode active material layer 130 that is easily crushed (arranging a positive electrode active material layer 120 that is not easily crushed) means arranging an active material layer that meets the following two conditions. The first condition is that an active material layer is disposed such that the linear pressure required for pressing the negative electrode active material layer 130 to form it with the porosity of the negative electrode active material layer 130 is smaller than the linear pressure required for pressing the positive electrode active material layer 120 to form it with the porosity of the negative electrode active material layer 130. The second condition is that an active material layer is disposed such that the linear pressure required for pressing the positive electrode active material layer 120 to form it with the porosity of the positive electrode active material layer 120 is larger than the linear pressure required for pressing the negative electrode active material layer 130 to form it with the porosity of the positive electrode active material layer 120.
[0050] The relatively crushable negative electrode active material layer 130 preferably contains a negative electrode active material containing more small particle diameter carbon material than large particle diameter carbon material. The relatively crushable positive electrode active material layer 120 preferably contains a positive electrode active material such as large particle diameter aggregated particles. The pressure P1 in the first pressing step is preferably 350 kg / cm or more and 600 kg / cm or less, and more preferably 400 kg / cm or more and 500 kg / cm or less. The pressure P2 in the second pressing step is preferably 300 kg / cm or more and 500 kg / cm or less, and more preferably 300 kg / cm or more and 400 kg / cm or less. The difference between the pressure P1 in the first pressing step and the pressure P2 in the second pressing step is preferably 50 kg / cm or more and 100 kg / cm or less. The active material layers (positive electrode active material layer 120, negative electrode active material layer 130) are pressed between an upper press roll and a lower press roll whose rotation axes are aligned. The upper press roll and the lower press roll are circular when viewed from the direction of the rotation axis, and linear (one-dimensional) pressure is applied to the active material layer. The upper roll and the lower roll may apply a load to the active material layer using a hydraulic cylinder. The load (kg) applied to the active material layer by pressing is the total load (kg) of the load (kg) applied by the upper roll to the active material layer with the lower roll fixed and the load (kg) of the upper roll itself, minus the load (kg) lifting the upper roll. The linear press pressure (pressure, kg / m) applied to the active material layer can be calculated by dividing the load (kg) applied to the active material layer by the length (m) of the active material layer in the direction in which the rolls extend (the axial direction of the rolls).
[0051] In this embodiment, one active material layer (negative electrode active material layer 130) has a higher porosity than the other active material layer (positive electrode active material layer 120), and is therefore more easily crushed than the other active material layer (positive electrode active material layer 120). That is, in the first pressing step, one active material layer having a higher porosity than the other active material layer is placed on the current collector foil 110 and pressed. The porosity of one active material layer (negative electrode active material layer 130) before pressing (before the first pressing step) is preferably 50% or more and 70% or less, and more preferably 55% or more and 65% or less. The porosity of the other active material layer (positive electrode active material layer 120) before pressing (before the second pressing step) is preferably 45% or more and 65% or less, and more preferably 50% or more and 60% or less. The difference in porosity between the active material layer pressed in the first pressing step and the active material layer pressed in the second pressing step is preferably 5% or more and 10% or less.
[0052] The "porosity" of the positive electrode active material layer 120 and the negative electrode active material layer 130 is calculated by the formula (1-V2 / V1) x 100, where V1 is the apparent volume (volume including voids) of the positive electrode active material layer 120 (negative electrode active material layer 130) and V2 is the sum of the actual volumes of the materials that make up the positive electrode active material layer 120 (negative electrode active material layer 130). The sum V2 of the actual volumes of the materials that make up the positive electrode active material layer 120 (negative electrode active material layer 130) is calculated from the content of each material in the positive electrode active material layer 120 (negative electrode active material layer 130) and the true density of each material.
[0053] As described above, the manufacturing method of the energy storage device 10 (the manufacturing method of the electrode unit 100) includes a first press step and a second press step. After the second press step (after the electrode unit 100 is manufactured), the plurality of electrode units 100 and the end units 101 and 102 are stacked in the stacking direction with the separator 140 sandwiched between them, and then sandwiched between a pair of end members 300, thereby manufacturing the energy storage device 10.
[0054] [3 Description of Effects] As described above, according to the manufacturing method for the energy storage device 10 according to the embodiment of the present invention, in the first press step, one active material layer (negative electrode active material layer 130) that is more easily crushed than the other active material layer (positive electrode active material layer 120) is placed on the current collector foil 110. In the first press step, pressing is performed with a pressure that is the same as or higher than the pressure used to press the other active material layer (positive electrode active material layer 120) in the second press step. In this way, by pressing the active material layer that is more easily crushed with a relatively high pressure in the first press step, distortion is less likely to occur in the current collector foil 110, and pinholes are less likely to occur in the current collector foil 110. In the second press step, pressing the less crushable active material layer with a relatively low pressure can suppress distortion in the current collector foil 110, thereby suppressing pinholes from occurring in the current collector foil 110. This suppresses damage to the current collector foil 110.
[0055] If a pinhole occurs in the positive electrode metal layer 111 or the negative electrode metal layer 112 of the current collector foil 110, the electrolyte may penetrate through the pinhole, potentially causing a short circuit (a short circuit between the metal layer and the active material of the opposite electrode). A pinhole in the positive electrode metal layer 111 shorts the positive electrode active material layer 120 and the negative electrode metal layer 112 (e.g., Cu plating) via the electrolyte, and furthermore, pinholes are formed in the Cu due to elution of Cu, ultimately causing a short circuit between the positive electrode active material layer 120 and the negative electrode active material layer 130. A pinhole in the negative electrode metal layer 112 shorts the negative electrode active material layer 130 and the positive electrode metal layer 111 (e.g., Al foil) via the electrolyte, and furthermore, Li from the negative electrode penetrates into the Al, forming a Li / Al alloy. The alloy expands and cracks form, ultimately causing a short circuit between the positive electrode active material layer 120 and the negative electrode active material layer 130. Therefore, by preventing pinholes from occurring in the current collector foil 110 (positive electrode metal layer 111 or negative electrode metal layer 112), it is possible to prevent short circuits (liquid junctions) from occurring inside the electricity storage device 10.
[0056] Furthermore, by pressing one active material layer (negative electrode active material layer 130) and then pressing the other active material layer (positive electrode active material layer 120), each active material layer can be pressed with a more appropriate pressure, resulting in a more appropriate density. By pressing one active material layer (negative electrode active material layer 130), which is easily crushed, with a relatively large pressure, the thickness of one active material layer (negative electrode active material layer 130) can be compressed relatively greatly, thereby reducing the thickness of the energy storage device 10 and achieving an energy storage device 10 with a high energy density. By pressing the active material layers (positive electrode active material layer 120 and negative electrode active material layer 130) with a relatively small pressure in the second pressing step, excessive compression of the active material layer (negative electrode active material layer 130) arranged in the first pressing step can be prevented.
[0057] The crush-resistant active material layer may undergo a change in thickness due to being left after pressing (springback phenomenon). If the crush-resistant active material layer (negative electrode active material layer 130) is pressed with a pressure greater than that in the second pressing step, the thickness after the first pressing step is less likely to change, and it is easy to press the other active material layer (positive electrode active material layer 120) with high precision in the second pressing step. Even if a crush-resistant active material layer is used in the second pressing step, springback is less likely to occur because an active material layer with a lower pressing pressure is selected and pressed.
[0058] In the first pressing step, by disposing an active material layer (negative electrode active material layer 130) that has high porosity before pressing on the current collector foil 110, it is possible to dispose an active material layer (negative electrode active material layer 130) that is easily crushed on the current collector foil 110. One active material layer that has high porosity is easily deformed by pressing, but by pressing before disposing (applying (coating)) the other active material layer on the current collector foil 110, deformation in thickness is suppressed, and the other active material layer can be precisely disposed (applied (coated)) on the current collector foil 110.
[0059] If the other active material layer, which is smaller in size, is placed on the current collector foil 110 and pressed, and then the other active material layer, which is larger in size, is placed on the current collector foil 110, the portion of one active material layer that protrudes from the other active material layer will not have a support for the other active material layer. In this case, when one active material layer is placed (applied (coated)) on the current collector foil 110, the portion where the other active material layer is not supported may be pushed into by the pressure applied to the portion where the other active material layer is placed (the coated portion) during the placement (application (coating)) of the other active material layer, and an excessive amount of one active material layer may be placed (applied (coated)) in that portion. As such, there is a risk that the amount of the protruding portion of the one active material layer (the applied amount (coated amount)) will be unstable (the lack of a support will result in a large gap and a large applied amount (coated amount)). When pressing one active material layer in the second pressing step, the protruding portion is not opposed to the other active material layer, so the protruding portion cannot be pressed sufficiently, which may result in the protruding portion becoming thicker. As a result, the protruding portion of one active material layer becomes thicker, which may cause problems such as the thickened portion of one active material layer applying a large pressure to the current collector foil 110 when stacking the electrode units 100, or wrinkles forming in the current collector foil 110, making stacking difficult. The protruding portion that cannot be pressed sufficiently may not sufficiently increase the bonding strength with the current collector foil 110, making the active material more likely to fall off. For this reason, in the first pressing step, the larger active material layer is pressed before the smaller active material layer. This prevents the above problems from occurring.
[0060] Since the negative electrode active material layer 130 is generally larger in size than the positive electrode active material layer 120, in the first pressing step, the negative electrode active material layer 130 is pressed before the positive electrode active material layer 120. This makes it possible to prevent the thickness of the portion of the negative electrode active material layer 130 that protrudes from the positive electrode active material layer 120 from increasing, thereby preventing problems caused by the thickness of the protruding portion increasing.
[0061] [4 Description of Modifications] While the manufacturing method of the energy storage device 10 according to the present embodiment has been described above, the present invention is not limited to the above-described embodiment. The disclosed embodiment is illustrative in all respects and is not restrictive, and the scope of the present invention includes all modifications within the meaning and scope of the claims.
[0062] In the above embodiment, the current collector foil 110 is formed of multiple layers (two layers) of the positive electrode metal layer 111 and the negative electrode metal layer 112, but the current collector foil 110 may be formed of a single layer (one metal foil). In other words, the current collector foil 110 may be formed of a single sheet of stainless steel foil or the like, and the single sheet of stainless steel foil or the like may have the functions of both the positive electrode metal layer and the negative electrode metal layer.
[0063] In the above embodiment, the negative electrode active material layer 130 is placed on the surface of the current collector foil 110 facing in the negative Z-axis direction and pressed in the first press step, and the positive electrode active material layer 120 is placed on the surface of the current collector foil 110 facing in the positive Z-axis direction and pressed in the second press step, but this is not limiting. The negative electrode active material layer 130 may be placed on the surface of the current collector foil 110 facing in the positive Z-axis direction and pressed in the first press step, and the positive electrode active material layer 120 may be placed on the surface of the current collector foil 110 facing in the negative Z-axis direction and pressed in the second press step.
[0064] In the above embodiment, the negative electrode active material layer 130 is pressed first in the first pressing step, but the positive electrode active material layer 120 may also be pressed first in the first pressing step. That is, one active material layer may be the positive electrode active material layer 120, and the other active material layer may be the negative electrode active material layer 130. That is, one active material layer that is more easily crushed than the other active material layer may be the positive electrode active material layer 120. One active material layer that is more porous than the other active material layer may be the positive electrode active material layer 120. In the first pressing step, one active material layer that is smaller in size than the other active material layer when viewed in the stacking direction may be pressed.
[0065] In the above embodiment, all of the electrode units 100 are manufactured by the above method, but it is not necessary to manufacture any of the electrode units 100 by the above method. It is sufficient that one or more of the electrode units 100 included in the energy storage device 10 are manufactured by the above method.
[0066] In the above embodiment, the active material layer placed on the current collector foil 110 during the first press step was referred to as one active material layer, and the active material layer placed on the current collector foil 110 during the second press step was referred to as the other active material layer. The active material layer placed on the current collector foil 110 during the first press step may be referred to as the first active material layer, and the active material layer placed on the current collector foil 110 during the second press step may be referred to as the second active material layer. The first active material layer is more easily crushed than the second active material layer.
[0067] In the above embodiment, the surface of the current collector foil 110 on which one active material layer is disposed during the first press process is referred to as the first surface, and the surface of the current collector foil 110 on which the other active material layer is disposed during the second press process is referred to as the other surface. The surface of the current collector foil 110 on which one active material layer is disposed during the first press process may be referred to as the first surface, and the surface of the current collector foil 110 on which the other active material layer is disposed during the second press process may be referred to as the second surface. The first and second surfaces are surfaces of the current collector foil 110 that are perpendicular to the direction in which the electrode units 100 are stacked (the Z-axis direction) and that face each other. In FIG. 5( b ), the surface of the current collector foil 110 facing in the negative Z-axis direction is the first surface, and the surface facing in the positive Z-axis direction is the second surface.
[0068] In the above embodiment, the negative electrode active material layer 130, which is one of the active material layers, is pressed with a pressure P1 during the first pressing step, and the positive electrode active material layer 120, which is the other active material layer, is pressed with a pressure P2 during the second pressing step. The pressure P1 may be referred to as the first pressure P1, and the pressure P2 may be referred to as the second pressure P2.
[0069] The energy storage device 10 may be used in an energy storage pack 1 as shown in FIG. 6 . FIG. 6 is a cross-sectional view showing the configuration of the energy storage pack 1. The internal configuration of the energy storage device 10 is omitted from FIG. 6 . As shown in FIG. 6 , the energy storage pack 1 includes an energy storage device stack 2 in which a plurality of energy storage devices 10 are stacked, and a conductive member 3. In this case, the technology of the present invention may be applied to at least one of the energy storage devices 10 included in the energy storage pack 1. Two adjacent energy storage devices 10 in the energy storage device stack 2 are electrically connected by contact or bonding (welding, etc.). The conductive member 3 is made of a metal such as stainless steel, and the energy storage device 10 located at the end in the stacking direction (Z-axis direction) and the conductive member 3 are electrically connected by contact or bonding (welding, etc.). An adhesive may be used for bonding. The plurality of energy storage devices 10 in the energy storage device stack 2 are connected in series, and charging and discharging are performed via the conductive member 3. The electricity storage pack 1 may be restrained in the stacking direction (Z-axis direction) by using a restraining member such as a screw, a resin band, or a metal band. The electricity storage device stack 2 and the conductive member 3 may be housed in a metal case or a resin case.
[0070] As another example of the electricity storage pack 1, a configuration in which individual electricity storage devices 10 are housed in an exterior body 4 is shown in FIG. 7. FIG. 7 is a cross-sectional view showing the configuration of an electricity storage pack 1a. As shown in FIG. 7, the electricity storage device 10 of this configuration has a connection portion 5 exposed from the exterior body 4. A laminate film or the like can be used as the exterior body 4. The connection portions 5 of adjacent electricity storage devices 10 are electrically connected to each other by contact or bonding (welding, etc.). The connection portions 5 of the electricity storage devices 10 located at the ends in the stacking direction (Z-axis direction) and the conductive member 3 are electrically connected to each other by contact or bonding (welding, etc.). The other configuration is the same as that of the above-described electricity storage pack 1, so description thereof will be omitted.
[0071] Any combination of the components included in the above-described embodiments and their modifications is also included within the scope of the present invention.
[0072] The present invention can be applied to a method for manufacturing an electricity storage device such as a bipolar battery.
[0073] REFERENCE SIGNS LIST 1, 1a Electricity storage pack 2 Electricity storage device laminate 3 Conductive member 4 Exterior body 5 Connection portion 10 Electricity storage device 100 Electrode unit 101, 102 End unit 110 Current collector foil 111 Positive electrode metal layer (metal layer) 112 Negative electrode metal layer (metal layer) 120 Positive electrode active material layer 130 Negative electrode active material layer 140 Separator 200 Sealing member 210, 220, 230 Sealing portion 300 End member
Claims
1. A method for manufacturing an electricity storage device including a plurality of electrode units stacked in a stacking direction, each of the plurality of electrode units having at least a current collecting foil, a positive electrode active material layer formed on one surface of the current collecting foil, and a negative electrode active material layer formed on the other surface of the current collecting foil, the method including: a first press step of arranging one of the positive electrode active material layer and the negative electrode active material layer on the current collecting foil and pressing it; and a second press step after the first press step of arranging the other of the positive electrode active material layer and the negative electrode active material layer on the current collecting foil and pressing it together with the one of the active material layers, wherein in the first press step, the one of the active material layers, which is more easily crushed than the other active material layer, is arranged on the current collecting foil and pressed with a pressure equal to or higher than a pressure used to press the other active material layer in the second press step.
2. The method for producing an electricity storage device according to claim 1, wherein in the first pressing step, the one active material layer having a higher porosity than the other active material layer is placed on the current collector foil and pressed.
3. The method for producing an electricity storage device according to claim 1 or 2, wherein in the first pressing step, one of the active material layers having a size larger than that of the other active material layer as viewed in the stacking direction is pressed.
4. The method for producing an energy storage device according to claim 1 or 2, wherein in the first press step, a negative electrode active material layer is pressed as the one active material layer, and in the second press step, a positive electrode active material layer is pressed as the other active material layer.
Citation Information
Patent Citations
Manufacturing method of battery electrode
JP2006128039A
Battery electrode manufacturing method and manufacturing apparatus
JP2010251018A
Bipolar electrode and manufacturing method of the bipolar electrode
JP2012129070A
Bipolar electrode, method for manufacturing the same, and power storage divice
JP2018088379A
Electrode manufacturing method
JP2021082504A
Cited By
Negative plate, battery and negative plate manufacturing method
CN119812520A