Protective plate, battery pack, and electric device

By using synergistic inorganic-organic composite layers, metal plates and honeycomb core protective panels in new energy vehicle battery packs, the problem of thick and heavy battery pack protective panels is solved, achieving efficient impact resistance and lightweighting. The design enhances the market competitiveness and safety of the vehicle.

WO2024222776A1PCT designated stage expired Publication Date: 2024-10-31BYD CO LTD

Patent Information

Application Number
PCT/CN2024/089739
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-28
Filing Date
2024-04-25
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing new energy vehicle battery pack protective panels are thick and heavy, which affects the lightweight process and market competitiveness. Common weight reduction methods cannot effectively improve impact resistance and cannot solve the problem of vehicle chassis design height.

Method used

A protective panel composed of a first inorganic-organic composite layer, a metal plate and a honeycomb core layer is used. The parameters of each layer meet specific mathematical relationships and cooperate to achieve high protective performance with a smaller thickness, including the first inorganic-organic composite layer, metal The board and the second inorganic-organic composite layer, the honeycomb core layer, further optimize the mechanical properties and anti-corrosion properties through the adhesive layer and anti-corrosion layer.

Benefits of technology

It achieves excellent protective performance and impact resistance at a smaller thickness, reduces the weight of the protective plate, improves the height and safety of the vehicle chassis, and enhances the anti-collision and anti-corrosion performance of the battery pack.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024089739_31102024_PF_FP_ABST
    Figure CN2024089739_31102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided are a protective plate, a battery pack, and an electric device. All layers of the protective plate cooperate with each other, and specific parameters of the layers meet a certain mathematical relationship, so that the protective plate can achieve good protection performance with a small thickness, and therefore the protective plate has great application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Protective panels, battery packs, and electrical equipment

[0001] This disclosure claims priority to patent application number 202310491525.9 filed with the National Intellectual Property Administration of China on April 28, 2023, and entitled “Protective plate, battery pack, and electrical equipment,” the entire contents of which are incorporated herein by reference. Technical Field

[0002] The present disclosure relates to the field of new energy technology, and in particular to a protective plate, a battery pack, and an electrical device. Background Art

[0003] The battery pack of a new energy electric vehicle is usually installed at the bottom of the vehicle. When the vehicle is driving on uneven or other abnormal roads, the bottom of the battery pack is easily bumped or impacted by hard objects such as stones. Therefore, a certain protective structure (for example, a protective plate) needs to be installed at the bottom of the battery pack to protect the battery pack and thus improve the safety of the vehicle.

[0004] Currently, commonly used fenders are typically composed primarily of steel plates combined with a layer of cushioning material. However, these fenders are thick and heavy, significantly hindering the lightweighting efforts of new energy vehicles and affecting their chassis height, severely limiting their market competitiveness. Literature has reported using resin-reinforced materials to partially replace the steel plates to reduce fender weight. However, to meet protection standards, the industry typically increases the thickness of each layer. This blindly increasing thickness can degrade the fender's impact resistance, not improve it, and has limited weight reduction benefits. Furthermore, these technical solutions still fail to address the limitations on vehicle chassis design height.

[0005] Summary of the Invention

[0006] In view of this, the present disclosure provides a protective plate. The layers of the protective plate cooperate with each other and the specific parameters of the layers satisfy a certain mathematical relationship, so that the protective plate can achieve good protective performance with a small thickness, thus having great application prospects.

[0007] A first aspect of the present disclosure provides a protective plate, comprising a first inorganic-organic composite layer, a metal plate, a honeycomb core layer, and a second inorganic-organic composite layer stacked in sequence;

[0008] The thickness of the first inorganic-organic composite layer is h1 mm, and the tensile strength is σ1 MPa; the thickness of the second inorganic-organic composite layer is h2 mm, and the tensile strength is σ2 MPa; the thickness of the metal plate is h3 mm, and the tensile strength is σ3 MPa; the thickness of the honeycomb core layer is h4 mm, the static compression strength is σ4 MPa, and the effective buffer stroke ratio is ε D; The protective plate satisfies the following formula:

[0009] The above-mentioned protective plate includes a honeycomb core layer that can provide buffering performance and impact resistance, a first and a second inorganic-organic composite layer of a metal plate that can provide greater strength and can provide stress bearing, anti-corrosion protection and weight reduction effects for the protective plate, and the thickness, strength and other parameters of each layer of material satisfy the above-mentioned mathematical relationship, so that the various mechanical properties of the protective plate as a whole can be balanced to achieve a better comprehensive protective effect, and the thickness of the protective plate can be reduced while achieving a better protective effect, so that the protective plate has great application prospects.

[0010] Optionally,

[0011] Optionally, 1.0≤(h1+h2)≤3.0.

[0012] Optionally, h1≥h2, and / or, σ1≥σ2.

[0013] Optionally, σ1=σ2.

[0014] Optionally, 280≤σ1≤380; 280≤σ2≤380.

[0015] Optionally, 0.5≤h3≤1.5; 270≤σ3≤1500.

[0016] Optionally, 5≤h4≤8; 5≤σ4≤30; 65%≤ε D ≤80%.

[0017] Optionally, adhesive layers are provided between the first inorganic-organic composite layer and the metal plate, between the metal plate and the honeycomb core layer, and between the honeycomb core layer and the second inorganic-organic composite layer, and the thickness of each adhesive layer is in the range of 0.1 mm to 0.2 mm.

[0018] Optionally, the components of either the first inorganic-organic composite layer or the second inorganic-organic composite layer include reinforcing fibers and resin, wherein the reinforcing fibers include at least one of carbon fibers, glass fibers, aramid fibers, ceramic fibers, silicon carbide fibers, and basalt fibers.

[0019] Optionally, the honeycomb core layer is smaller than the metal plate in length and / or width. A first anti-corrosion layer is further provided on the surface of the metal plate not covered by the honeycomb core layer.

[0020] Optionally, the material of the first anti-corrosion layer is the same as that of the first inorganic-organic composite layer. Alternatively, the material of the first anti-corrosion layer is the same as that of the second inorganic-organic composite layer.

[0021] Optionally, the metal plate and the side walls of the honeycomb core layer are further wrapped with a second anti-corrosion layer.

[0022] Optionally, the material of the second anti-corrosion layer is the same as that of the first inorganic-organic composite layer. Alternatively, the material of the second anti-corrosion layer is the same as that of the second inorganic-organic composite layer.

[0023] A second aspect of the present disclosure provides a battery pack comprising a tray, a battery cell assembly, and the protective plate provided in the first aspect of the present disclosure, wherein the battery cell assembly and the protective plate are mounted on opposite sides of the tray. Due to the use of the protective plate provided in the present disclosure, the battery pack has both high crash resistance and good corrosion resistance.

[0024] Optionally, the second inorganic-organic composite layer is disposed close to the tray.

[0025] A third aspect of the present disclosure provides an electrical device comprising the battery assembly provided in the second aspect of the present disclosure. Due to the inclusion of the battery pack, the area of ​​the electrical device containing the battery pack has both good anti-collision and good anti-corrosion properties, resulting in better safety. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] FIG1 is a schematic structural diagram of a battery pack provided by one embodiment of the present disclosure;

[0027] FIG2 is a schematic structural diagram of the protective plate in FIG1 in one state;

[0028] FIG3 is a schematic structural diagram of the protective plate in FIG1 in another state;

[0029] FIG4 is an exploded view of the protective plate in FIG3 ;

[0030] FIG5 is a schematic structural diagram of the honeycomb core layer in FIG4 ;

[0031] FIG6 is a schematic diagram showing the distribution of ball hitting points on the protective plate to be tested used in the impact resistance test of the present disclosure.

[0032] Explanation of reference numbers: 1-battery pack; 11-tray; 12-cell assembly; 13-sealing cover; 100-protective plate; 100b-back of protective plate; 100a-front of protective plate; 10-first inorganic-organic composite layer; 20-second inorganic-organic composite layer; 30-metal plate; 40-honeycomb core layer; 50-first anti-corrosion layer; 60-second anti-corrosion layer. DETAILED DESCRIPTION

[0033] The directional terms mentioned in this disclosure, such as "up", "down", "front", "back", "left", "right", "inside", "outside", "front", "back", "bottom", "top", "thickness", "length", "width", etc., are only with reference to the orientations shown in the accompanying drawings. Therefore, the directional terms used are for better and clearer explanation and understanding of this disclosure, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as a limitation of this disclosure. The terms "set", "connect", and "install" in this disclosure should be understood in a broad sense, for example, they can be directly set, connected, or installed, or they can be indirectly set, connected, or installed through an intermediate medium.

[0034] The terms "first", "second", etc. used in this disclosure are used to distinguish different objects rather than to describe a specific order. In the description of this disclosure, unless otherwise specified, the meaning of "plurality" refers to greater than or equal to two. In addition, the numerical range represented by "-" in this specification refers to the range that includes the numerical values ​​recorded before and after "-" as the minimum and maximum values, respectively. In the accompanying drawings, units with similar or identical structures are represented by the same reference numerals.

[0035] The various specific technical features and embodiments described in the detailed description may be combined in any suitable manner, unless there is any contradiction. For example, different specific technical features / examples may be combined to form different embodiments. To avoid unnecessary repetition, this disclosure will not further describe various possible combinations.

[0036] The following describes the protective plate and battery pack provided by the embodiments of the present disclosure. Please refer to Figures 1 to 5 . Figure 1 is a schematic diagram of the structure of a battery pack 1 using the protective plate 100 of the present disclosure. Figures 2 and 3 are schematic diagrams of the structure of the protective plate 100 in Figure 1 in two different states, respectively. Figure 4 is an exploded view of the protective plate 100 in Figure 3. Figure 5 is a schematic diagram of the structure of the honeycomb core layer 40 in Figure 4.

[0037] 1 , the battery pack 1 may include a tray 11, a cell assembly 12 mounted on the tray 11, and a protective plate 100. The cell assembly 12 and the protective plate 100 are respectively mounted on opposite sides of the tray 11. Specifically, the cell assembly 12 and the protective plate 100 may be mounted on opposite sides of the bottom plate of the tray 11. The protective plate 100 is mounted on the side of the tray 11 facing away from the cell assembly 12 (i.e., the bottom of the tray 11). Specifically, a receiving groove may be provided at the bottom of the tray 11, and the protective plate 100 is mounted in the receiving groove.

[0038] The battery pack 1 also includes a sealing cover 13 that covers the tray 11. The sealing cover 13 and the tray 11 enclose a housing space within which the battery cell assembly 12 can be housed, protecting the battery cell assembly 12 from all directions. The battery cell assembly 12 can be one or more single cells or one or more battery modules. In some embodiments, the battery cell assembly 12 includes multiple battery modules to increase the capacity of the battery pack 1.

[0039] The battery pack 1 can be fixed to the underbody of the vehicle in which it is used. When the underbody is impacted or squeezed by hard objects such as stones during driving, the protective plate 100 at the bottom of the battery pack 1 can resist impact deformation, preventing external impact forces from directly acting on the battery cell assembly 12 of the battery pack 1, thereby protecting the battery.

[0040] For ease of understanding, the present disclosure defines the surface of the protective plate 100 facing away from the pallet 11 as the front side 100a of the protective plate 100, which is also the main force-bearing surface of the protective plate 100 and faces the ground on which the vehicle is traveling; and defines the surface of the protective plate 100 facing the pallet 11 as the back side 100b of the protective plate 100.

[0041] At present, the protective plate for battery components is generally composed of a steel plate and a buffer layer. In order to improve the lightweight degree of the protective plate, the industry usually chooses to add a fiber-reinforced resin layer to the protective plate and reduce the thickness of the steel plate to reduce the weight of the protective plate. It is understandable that the increase in the number of layers will make the structure of the protective plate more complicated, and the selection of parameters such as the properties and thickness of each layer of material itself will become more complicated. It is often the case that the thickness of the fiber-reinforced resin layer is blindly increased in order to meet the protection standard. However, the above situation may cause the impact resistance of the protective plate to decrease instead of increase, and the weight reduction effect of the protective plate is limited, which seriously restricts the practical application of the above protective plate. In order to solve the above problems, the embodiment of the present disclosure provides a protective plate 100, including a first inorganic-organic composite layer 10, a metal plate 30, a honeycomb core layer 40 and a second inorganic-organic composite layer 20 stacked in sequence.

[0042] The thickness of the first inorganic-organic composite layer 10 is h1 mm, and the tensile strength of the first inorganic-organic composite layer 10 is σ1 MPa; the thickness of the second inorganic-organic composite layer 20 is h2 mm, and the tensile strength is σ2 MPa; the thickness of the metal plate 30 is h3 mm, and the tensile strength of the metal plate 30 is σ3 MPa; the thickness of the honeycomb core layer 40 is h4 mm, and the static compression strength of the honeycomb core layer 40 is σ4 MPa, and the effective buffer stroke ratio of the honeycomb core layer 40 is ε D ; The protective plate 100 satisfies the following formula:

[0043] The honeycomb core layer 40 has excellent load buffering and energy absorption capabilities, and can evenly and quickly disperse external forces applied to the metal plate 30, significantly improving the ability of the protective plate 100 to resist impact deformation and increasing the utilization rate of the reserved buffer space at the bottom of the battery pack tray. The metal plate 30 can enhance the overall mechanical properties of the protective plate 100, thereby improving the anti-collision capability of the protective plate 100. The first and second inorganic-organic composite layers provide mechanical support and anti-corrosion protection for the metal plate 30 and the honeycomb core layer 40, while also reducing the weight of the protective plate 100. It is understandable that the primary properties of the aforementioned layers differ, and simply changing the thickness or other parameters of a single layer will result in changes in the overall performance of the protective plate. The present disclosure coordinates the mechanical properties and thickness of each layer, fully leveraging the synergistic relationship between the layers. This significantly reduces the thickness of the protective plate 100 while improving its overall protective performance. This can further increase the height of the vehicle chassis from the ground, providing more technical support for further lowering the vehicle chassis. In addition, when the mathematical relationship between the parameters of each layer is controlled to satisfy the above formula, by further regulating the parameters of each layer, the weight of the protective plate 100 can be reduced while reducing the thickness of the protective plate 100.

[0044] In addition, the side surface with the first inorganic-organic composite layer 10 is generally used as the front side 100a of the protective plate, and the metal plate 30 is arranged close to the first inorganic-organic composite layer 10, which can reduce the stress transmitted to the honeycomb core layer 40 and can quickly disperse and transmit the stress to the honeycomb core layer 40, thereby uniformizing the impact force that the honeycomb core layer 40 needs to withstand, reducing the loss of the honeycomb core layer 40 and reducing the risk of irreversible deformation of the honeycomb core layer 40, so that the front side 100a of the protective plate can have better anti-collision performance, thereby improving the impact resistance of the protective plate 100 and extending its service life.

[0045] For the convenience of description, the above Denoted as λ, in some specific embodiments of the present disclosure, 0.680<λ<0.995. The value of λ can be 0.685, 0.690, 0.695, 0.700, 0.705, 0.710, 0.715, 0.720, 0.725, 0.730, 0.735, 0.740, 0.745, 0.750, 0.755, 0.760, 0.765, 0.770, 0.780, 0.790, 0.800, 0.820, 0.850, 0.880, 0.900, 0.920, 0.950, 0.980, 0.990, 0.994, etc. Controlling the value of λ within the above range can ensure that the protective plate 100 has good protective performance and is easy to manufacture.

[0046] In the present disclosure, the thickness of the first inorganic-organic composite layer 10 can be equal to the thickness of the second inorganic-organic composite layer 20 (h1=h2), or the thickness of the first inorganic-organic composite layer 10 can be greater than the thickness of the second inorganic-organic composite layer 20 (h1>h2). In some embodiments of the present disclosure, the tensile strength of the second inorganic-organic composite layer 20 is σ2 MPa, h1≥h2, and / or σ1≥σ2. That is, the inorganic-organic composite layer with a greater thickness and / or a higher tensile strength is identified as the first inorganic-organic composite layer. For example, the strength σ1 of the first inorganic-organic composite layer 10 is the same as the tensile strength σ2 of the second inorganic-organic composite layer 20, σ1=σ2, and h1>h2; or, the strength σ1 of the first inorganic-organic composite layer 10 is different from the tensile strength σ2 of the second inorganic-organic composite layer 20, in which case σ1>σ2 and h1=h2. In some embodiments of the present disclosure, h1≥h2 and σ1≥σ2. At this time, it is more conducive to the protective performance of the protective plate, especially the impact resistance.

[0047] Understandably, the tensile strength of the first and second inorganic-organic composite layers can be adjusted by parameters such as the choice of resin and reinforcing fiber, and the density of the reinforcing fiber placement. When σ1 > σ2, while maintaining good mechanical properties of the protective plate 100, the density of the reinforcing fibers in the second inorganic-organic composite layer 20 can be reduced, or reinforcing fibers or resins with relatively weaker mechanical properties can be selected, thereby further reducing the production cost of the protective plate 100. In some embodiments of the present disclosure, h1 > h2. Thus, when the first inorganic-organic composite layer 10 serves as the front surface 100a of the protective plate, the protective effect is even better.

[0048] In some specific embodiments of the present disclosure, σ1=σ2. In this way, the mechanical properties of the two opposite sides of the protective plate can be better balanced, and the comprehensive protective performance of the protective plate 100 can be further optimized.

[0049] In some embodiments of the present disclosure, 1.0≤(h1+h2)≤3.0. That is, the sum of the thicknesses of the first inorganic organic composite layer 10 and the second inorganic organic composite layer 20 is in the range of 1.0mm-3.0mm. For example, the sum of the thicknesses of the first inorganic organic composite layer 10 and the second inorganic organic composite layer 20 can be 1.0mm, 1.2mm, 1.5mm, 1.8mm, 2.0mm, 2.2mm, 2.5mm, 2.8mm, 3.0mm, etc. In this way, the protective plate 100 can have better corrosion resistance and better impact resistance. In some specific embodiments of the present disclosure, the thickness of the first inorganic organic composite layer 10 is in the range of 0.8mm-2.8mm, and the thickness of the second inorganic organic composite layer 20 is in the range of 0.2mm-0.5mm. For example, the thickness of the first inorganic-organic composite layer 10 may be 0.8 mm, 0.9 mm, 1.0 mm, 1.2 mm, 1.5 mm, 1.8 mm, 2.0 mm, 2.2 mm, 2.5 mm, 26 mm, 2.7 mm, etc. For example, the thickness of the second inorganic-organic composite layer 20 may be 0.2 mm, 0.3 mm, 0.4 mm, 0.5 mm, etc.

[0050] In the present disclosure, the first inorganic-organic composite layer 10 and the second inorganic-organic composite layer 20 are each composed of a resin and reinforcing fibers. The resin can be selected from resin materials well-known to those skilled in the art for composite materials, including but not limited to thermoplastic resins and thermosetting resins. Specifically, the resins of the first and second inorganic-organic composite layers each include but are not limited to at least one of epoxy resin, phenolic resin, polypropylene resin, nylon resin, and the like. The reinforcing fibers include chopped fibers and continuous fibers. In the present disclosure, the reinforcing fibers can be commonly selected from reinforcing fibers for composite materials. Specifically, the reinforcing fibers in the first and second inorganic-organic composite layers each include but are not limited to at least one of carbon fiber, glass fiber, aramid fiber, ceramic fiber, silicon carbide fiber, and basalt fiber. In some specific embodiments, the reinforcing fibers in both the first and second inorganic-organic composite layers are selected from glass fibers. This further balances the mechanical properties and production costs of the protective plate 100. In some embodiments, the reinforcing fibers in the first and second inorganic-organic composite layers 10 and 20 include continuous fibers. In some specific embodiments, the first inorganic-organic composite layer 10 and the second inorganic-organic composite layer 20 each include a plurality of sequentially stacked continuous fiber layers, where any two adjacent continuous fiber layers are defined as a first continuous fiber layer and a second continuous fiber layer, the continuous fibers in the first continuous fiber layer are oriented along a first direction, and the continuous fibers in the second continuous fiber layer are oriented along a second direction, where the first direction and the second direction are different. In some embodiments, the first direction is perpendicular to the second direction.

[0051] In some embodiments of the present disclosure, 280≤σ1≤380. That is, the tensile strength of the first inorganic-organic composite layer 10 is in the range of 280MPa-380MPa. For example, the tensile strength of the first inorganic-organic composite layer 10 can be 280MPa, 290MPa, 300MPa, 310MPa, 320MPa, 330MPa, 340MPa, 350MPa, 360MPa, 370MPa, 380MPa, etc. In this way, the first inorganic-organic composite layer 10 has a certain degree of rigidity and toughness. While better supporting the metal plate 30 and the honeycomb core layer 40, it can also withstand a certain degree of impact to achieve the target protection effect and extend the service life of the protective plate 100. In some embodiments of the present disclosure, 280≤σ2≤380. That is, the tensile strength of the second inorganic-organic composite layer 20 is in the range of 280MPa-380MPa. For example, the tensile strength of the second inorganic-organic composite layer 20 may be 280 MPa, 290 MPa, 300 MPa, 310 MPa, 320 MPa, 330 MPa, 340 MPa, 350 MPa, 360 MPa, 370 MPa, 380 MPa, etc. In this way, the second inorganic-organic composite layer may have both certain rigidity and toughness.

[0052] In this disclosure, the tensile strength of the inorganic-organic composite layer was determined by preparing a 250 mm × 25 mm × 2.5 mm specimen according to ASTM D3039, Standard Test Method for Tensile Properties of Polymer-Based Composite Materials. The specimen dimensions were verified using a vernier caliper. The center of the specimen was polished, and surface damage was minimized. The specimen surface was cleaned, and the specimen was carefully aligned during installation. After installation, the specimen was debugged, the equipment acquisition frequency was set to 2 Hz, the equipment control system was reset, and the specimen was stretched at a speed of 2 mm / min until failure. The test data was recorded. At least five valid specimens were used.

[0053] In some embodiments of the present disclosure, 0.5 ≤ h3 ≤ 1.5. That is, the thickness of the metal plate 30 is within the range of 0.5 mm to 1.5 mm. A metal plate 30 of appropriate thickness can ensure that it can provide good support and can bear part of the impact / extrusion force caused by foreign objects such as stones. For example, the thickness of the metal plate 30 can be 0.5 mm, 0.6 mm, 0.7 mm, 0.8 mm, 0.9 mm, 1.0 mm, 1.1 mm, 1.2 mm, 1.3 mm, 1.4 mm, 1.5 mm, etc.

[0054] In some embodiments of the present disclosure, 270 ≤ σ3 ≤ 1180. That is, the tensile strength of the metal plate 30 is within the range of 270 MPa-1180 MPa. In the present disclosure, the tensile strength of the metal plate 30 can be adjusted by changing the material of the metal plate 30. The material of the metal plate 30 includes, but is not limited to, at least one of aluminum, an aluminum alloy, magnesium, a magnesium alloy, and steel. In the present disclosure, the tensile strength of the metal plate 30 is measured in accordance with GB / T228-2002, "Method for Tensile Test of Metallic Materials at Room Temperature."

[0055] In some embodiments of the present disclosure, 5 ≤ h4 ≤ 8. That is, the thickness of the honeycomb core layer 40 is within the range of 5 mm to 8 mm. For example, the thickness of the honeycomb core layer 40 may be 5.0 mm, 5.5 mm, 6.0 mm, 6.5 mm, 7.0 mm, 7.5 mm, etc. A honeycomb core layer 40 of appropriate thickness ensures that it can fully buffer and disperse external forces, while effectively reducing the thickness and weight of the overall protective plate 100.

[0056] In some embodiments of the present disclosure, 5≤σ4≤30. That is, the static compressive strength of the honeycomb core layer 40 is within the range of 5MPa-30MPa. Exemplarily, the static compressive strength of the honeycomb core layer 40 may be 5MPa, 8MPa, 10MPa, 12MPa, 15MPa, 20MPa, 22MPa, 25MPa, 28MPa, and the like. In this way, it is beneficial to ensure that the honeycomb core layer has a strong ability to resist impact deformation, so as to stably disperse and absorb the impact force applied to the front of the protective plate 100. In the present disclosure, the static compressive strength is measured by placing the honeycomb core layer on a quasi-static testing machine for an axial compression test; specifically, refer to GBT1453-2005 "Test method for flat compression performance of sandwich structures or cores".

[0057] In the present disclosure, the honeycomb core layer 40 includes, but is not limited to, an aluminum honeycomb core layer. The honeycomb core layer 40 includes a plurality of through-holes, which may form a honeycomb structure. The cross-section of each through-hole may be a polygon such as a hexagon, a triangle, or a circle.

[0058] In some embodiments of the present disclosure, 65%≤ε D≤85%. That is, the effective buffer stroke ratio of the honeycomb core layer 40 is in the range of 65%-85%. Exemplarily, the effective buffer stroke ratio of the honeycomb core layer 40 can be 65%, 67.5%, 70%, 72.5%, 75%, 77.5%, 80%, 82.5%, 85%, etc. In this way, it is beneficial to improve the impact resistance of the protective plate 100. Among them, the effective buffer stroke ratio can be understood as: the material splines of the honeycomb core layer are subjected to a compression test on an electronic universal testing machine with model LD26.305, and the stress value corresponding to the platform of the measured stress-strain curve is the effective compression strength, and the maximum compression stroke within the effective compression strength is the effective compression stroke. The ratio of the effective compression stroke to the original length of the material spline of the honeycomb core layer is the above-mentioned effective buffer stroke ratio.

[0059] In some embodiments of the present disclosure, a glue layer is provided between the first inorganic-organic composite layer 10 and the metal plate 30, between the metal plate 30 and the honeycomb core layer 40, and between the honeycomb core layer 40 and the second inorganic-organic composite layer 20, and the thickness of a single glue layer is in the range of 0.1 mm to 0.2 mm. In this way, the interfacial bonding force between the layers can be improved, which is conducive to ensuring that the mechanical properties of the protective plate 100 are good. In some embodiments, during the preparation of the protective plate 100, a glue layer is provided on both sides of the metal plate, and a glue layer is provided on the side of the honeycomb core layer close to the second inorganic-organic composite layer, and then the above-mentioned first inorganic-organic composite layer, the metal plate with glue layers on both sides, the honeycomb core layer with glue layers on one side, and the second inorganic-organic composite layer are stacked in sequence, and hot pressed to obtain the protective plate 100.

[0060] In the present disclosure, the edges of the first inorganic-organic composite layer 10, the metal plate 30, the honeycomb core layer 40, and the second inorganic-organic composite layer 20 may be flush. Alternatively, the orthographic projections of the metal plate 30, the honeycomb core layer 40, and the second inorganic-organic composite layer 20 along the thickness direction of the protective plate 100 all fall within the first inorganic-organic composite layer 10. Alternatively, the orthographic projections of the honeycomb core layer 40 and the second inorganic-organic composite layer 20 along the thickness direction of the protective plate 100 all fall within the orthographic projections of the metal plate 30 and the first inorganic-organic composite layer 10. In this case, the edge of the metal plate 30 may be flush with the edge of the first inorganic-organic composite layer 10, or there may be a certain distance between the edge of the metal plate 30 and the edge of the first inorganic-organic composite layer 10.

[0061] In some embodiments of the present disclosure, at least the honeycomb core layer 40 and the second inorganic-organic composite layer 20 each have their orthographic projections along the thickness direction of the protective plate 100 falling within the first inorganic-organic composite layer 10. In this case, the protective plate 100 has a stepped surface, which further facilitates assembly of the protective plate 100. For example, when the protective plate 100 is loaded onto the battery pack 1 (including the protective plate 100, battery tray, and sealing cover), the protective plate 100 can align with the grooves reserved in the tray, further reducing the overall thickness of the battery pack 1.

[0062] In some embodiments of the present disclosure, the exposed surfaces of the metal plate 30 and the honeycomb core layer 40 have an anti-corrosion layer. The exposed surface of the metal plate 30 includes but is not limited to the side walls of the metal plate 30, and any surface of the metal plate 30 that is not covered by the honeycomb core layer 40; the exposed surface of the honeycomb core layer 40 specifically includes but is not limited to the side walls of the honeycomb core layer 40. In this way, the anti-corrosion performance of the protective plate 100 can be further improved. The anti-corrosion layer can be a traditional anti-corrosion coating (without reinforcing fibers), for example, a polyvinyl chloride (PVC) coating. In some embodiments, the anti-corrosion layer can also be an inorganic-organic composite layer made of the same material as the first inorganic-organic composite layer or the second inorganic-organic composite layer.

[0063] In some embodiments of the present disclosure, the honeycomb core layer 40 is smaller than the metal plate 30 in length and / or width. A first anti-corrosion layer 50 is also provided on the surface of the metal plate 30 that is not covered by the honeycomb core layer 40. The material of the first anti-corrosion layer 50 is the same as the material of the first inorganic-organic composite layer 10, or the material of the first anti-corrosion layer 50 is the same as the material of the second inorganic-organic composite layer 20. At this time, there may or may not be an interface between the first anti-corrosion layer 50 and the first inorganic-organic composite layer 10 and / or the second inorganic-organic composite layer 20. It can be understood that when there is no interface, the first anti-corrosion layer 50 and the first inorganic-organic composite layer 10 and / or the second inorganic-organic composite layer 20 are integrally formed. In this way, it can be ensured that the protective plate 100 is easy to install while having good mechanical properties. In some specific embodiments, the metal plate and the side walls of the honeycomb core layer are further wrapped with a second anti-corrosion layer 60. The material of the second anti-corrosion layer 60 is the same as that of the first inorganic-organic composite layer, or the material of the second anti-corrosion layer 60 is the same as that of the second inorganic-organic composite layer 20. In this way, the anti-corrosion performance of the protective plate 100 can be improved, and it is also beneficial to improve the interfacial bonding force between the first inorganic-organic composite layer 10 and / or the second inorganic-organic composite layer 20 and the metal plate, so that the protective plate 100 can have better protective performance. It is understandable that there may or may not be an interface between the second anti-corrosion layer 60 and the first inorganic-organic composite layer 10 and / or the second inorganic-organic composite layer 20. It is understandable that when there is no interface, the second anti-corrosion layer 60 and the first inorganic-organic composite layer 10 and / or the second inorganic-organic composite layer 20 are integrally formed.

[0064] The present disclosure also provides a battery pack with the above-mentioned protective structure of the embodiment of the present disclosure. The battery pack includes a tray, a battery cell assembly, and a protective plate provided by the embodiment of the present disclosure, wherein the battery cell assembly and the protective plate are respectively installed on opposite sides of the tray.

[0065] For details, please refer to Figure 1 and the above description of the battery pack. In addition to the tray 11, battery cell assembly 12, sealing cover 13, and protective plate 100 mentioned above, the battery pack 1 may also include a battery management system, which is used to monitor the charging and discharging status information of each single battery in the battery cell assembly 12, such as voltage, current, internal resistance, temperature, etc.

[0066] In some embodiments of the present disclosure, the second inorganic-organic composite layer is disposed close to the tray.

[0067] The protective plate implemented in the present disclosure combines the advantages of light weight, thin thickness, and excellent impact resistance. When the battery pack is equipped with this protective plate, if the underside of the vehicle is impacted or squeezed by foreign objects such as stones during driving, the protective plate located at the bottom of the battery pack 1 can effectively resist the external impact force caused by the foreign objects, preventing the external impact force from directly acting on the tray 11 and battery cell assembly 12 of the battery pack 1, thereby damaging the battery pack 1 and even causing fire or explosion, thereby ensuring that the battery pack is well protected.

[0068] The present disclosure also provides an electrical device comprising the aforementioned battery pack. In some embodiments, the electrical device is a vehicle, wherein the battery pack 1 can be secured to the underbody of the vehicle, with the protective plate 100 positioned thereunder. The inclusion of the protective plate ensures the safety of the battery pack 1, thereby enhancing the safe operation of the vehicle using the battery pack.

[0069] The battery pack 1 is used to provide electric energy for a vehicle. The vehicle using the battery pack to provide electric energy can be one or more of a pure electric vehicle, a hybrid electric vehicle, an electric motorcycle, an electric bicycle, etc., with pure electric vehicles or hybrid electric vehicles being more common.

[0070] The technical solution of the present disclosure is further explained below with multiple technical solutions.

[0071] Example 1

[0072] A protective plate includes a first inorganic-organic composite layer, a metal plate (specifically a steel plate), an aluminum honeycomb core layer, and a second inorganic-organic composite layer stacked in sequence. The first inorganic-organic composite layer has a thickness of 0.8 mm and a tensile strength of 380 MPa. The second inorganic-organic composite layer has a thickness of 0.2 mm and a tensile strength of 280 MPa. The metal plate has a thickness of 0.5 mm and a tensile strength of 270 MPa. The honeycomb core layer has a thickness of 5 mm and a static compressive strength of 5 MPa. The effective buffer stroke ratio ε is ε. D is 65%.

[0073] The metal plate and the side walls of the honeycomb core layer are coated with a polyvinyl chloride (PVC) anti-corrosion layer. The first inorganic-organic composite layer and the second inorganic-organic composite layer are each independently a glass fiber composite material.

[0074] Example 2

[0075] The difference from Example 1 is that the metal plate and the side wall of the aluminum honeycomb core layer are wrapped with a first anti-corrosion layer, the material of which is the same as that of the first inorganic-organic composite layer, and there is no interface between the two.

[0076] Example 3-Example 10

[0077] The difference between Examples 3-10 and Example 1 is that the parameter settings of the protective plate are different. The parameters of each example are summarized in Table 1. Please refer to Table 1.

[0078] Example 11

[0079] The difference between Example 11 and Example 1 is that adhesive layers are provided between the first inorganic-organic composite layer and the metal plate, between the metal plate and the honeycomb core layer, and between the honeycomb core layer and the second inorganic-organic composite layer, and the thickness of each adhesive layer is 0.1 mm.

[0080] In order to highlight the beneficial effects of the embodiments of the present disclosure, the following comparative examples are provided.

[0081] Comparative Example 1

[0082] The difference from Example 1 is that the parameter settings of the protective plate are different. For the parameters of each layer in the protective plate of Comparative Example 1, please refer to Table 1.

[0083] Comparative Example 2

[0084] A protective plate includes stacked metal plates (specifically DP270 steel plates with a thickness of 1.5 mm, with a 1 mm thick PVC layer coated on both opposite sides and the side walls) and a microporous expanded polypropylene (MPP) buffer layer, wherein the MPP buffer layer is close to the bottom of the battery pack tray and has a thickness of 7 mm.

[0085] Table 1

[0086] The performance tests were performed on the protective plates of the above embodiments and comparative examples:

[0087] (1) Impact resistance test: Arrange the light source, camera, and sensor to the computer to complete the debugging preparation; Calibrate the ball hitting point: According to the test requirements, calibrate the position of the ball hitting point on each protective plate; Calibrate the ball hitting energy: Use infrared clamps to clamp the load weight, and after the ball hitting point is found, the crane rises to the height corresponding to the energy (accurately calibrated with an infrared rangefinder); Release the clamps: After the position calibration and energy calibration, and after the data monitoring is normal, the remote control infrared sensing clamps are released, allowing the weight to complete the impact on the calibration point; Among them, the ball hitting point is within the ball hitting area, and the distance between two adjacent ball hitting points is more than 150mm. For the specific ball hitting point distribution, please refer to Figure 6; the weight of the weight is 26.2Kg, and the diameter of the impact ball head of the weight is 25mm.

[0088] Results Collection: A digital camera was used to capture images of the ball after impact. A computer was used to organize the video footage and sensor data, and to calculate the impact test results of the protective plate. The results are summarized in Table 2.

[0089] (2) Anticorrosion Test: Tested according to the test method of Q / BYDQ-A1901.402.2-2017: 0.5 mol / L sulfuric acid was dripped onto the surface of the tested protective plate specimens. After 24 hours at room temperature, the changes in the material were observed. The protective plate specimens were square specimens with a length and width of 50 mm and a thickness equal to the actual thickness of the protective plate. A minimum of five specimens were tested. The results are summarized in Table 2.

[0090] Table 2

[0091] Combining the parameters in Table 1 and the data in Table 2, it can be found that the protective plate provided by the embodiment of the present disclosure has a good protective effect. When the thickness of the protective plate provided by the embodiment of the present disclosure is equivalent to or smaller than the thickness of the ordinary protective plate (Comparative Example 2), the impact resistance of the embodiment protective plate is even better than that of Comparative Example 2. Furthermore, the metal plate in Example 6 has the same tensile strength and thickness as the steel plate in Comparative Example 2, and the total thickness of the protective plate is also the same, but the impact resistance of Example 6 is much better than that of Comparative Example 2. Even if the structure is the same, but the mathematical relationship between the parameters of each layer does not meet the requirements of the present disclosure (Comparative Example 1), the impact resistance of the protective plate is poor. Furthermore, when the thickness and tensile strength of the first composite layer and the second composite layer are further improved, it is more conducive to improving the impact resistance of the protective plate. Please refer to the protective plates of Examples 1 to 4 and Examples 7 to 11. The thickness of the metal substrate is only 0.5 mm, which can reduce the weight of the protective plate and contribute to the lightweighting of the vehicle.

[0092] The above is an exemplary embodiment of the present disclosure. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made thereto without departing from the principles of the present disclosure. These improvements and modifications are also considered to be within the scope of protection of the present disclosure.

Claims

1. A protective plate (100), It is characterized in that The protective plate (100) comprises a first inorganic-organic composite layer (10), a metal plate (30), a honeycomb core layer (40), and a second inorganic-organic composite layer (20) which are stacked in sequence; The thickness of the first inorganic-organic composite layer (10) is h 1 mm, tensile strength is σ 1 MPa; the thickness of the second inorganic-organic composite layer (20) is h 2 mm, tensile strength is σ 2 MPa; the thickness of the metal plate (30) is h 3 mm, tensile strength is σ 3 MPa; the thickness of the honeycomb core layer (40) is h 4 mm, static compressive strength is σ 4 MPa, effective buffer stroke ratio is ε D ; The protective plate (100) satisfies the following formula:

2. The protective plate (100) according to claim 1, It is characterized in that 3. The protective plate (100) according to claim 1 or 2, It is characterized in that 1.0≤(h 1 +h 2 )≤3.0。 4. The protective plate (100) according to claim 1 or 2, It is characterized in that h 1 ≥h 2 , and / or, σ 1 ≥σ 2 .

5. The protection plate (100) according to claim 3, It is characterized in that σ1=σ2。 6. The protective plate (100) according to claim 1 or 2, It is characterized in that 280≤σ 1 ≤380;280≤σ 2 ≤380。 7. The protection plate (100) according to claim 1 or 2, It is characterized in that 0.5≤h 3 ≤1.5;270≤σ 3 ≤1500。 8. The protective plate (100) according to claim 1 or 2, It is characterized in that 5≤h 4 ≤8;5≤σ 4 ≤30;65%≤ε D ≤80%。 9. The protective plate (100) according to any one of claims 1 to 8, It is characterized in that An adhesive layer is provided between the first inorganic-organic composite layer (10) and the metal plate (30), between the metal plate (30) and the honeycomb core layer (40), and between the honeycomb core layer (40) and the second inorganic-organic composite layer (20), and the thickness of each adhesive layer is in the range of 0.1 mm to 0.2 mm.

10. The protection plate (100) according to any one of claims 1 to 8, It is characterized in that The components of any one of the first inorganic-organic composite layer (10) and the second inorganic-organic composite layer (20) include reinforcing fibers and resin; wherein the reinforcing fibers include at least one of carbon fibers, glass fibers, aramid fibers, ceramic fibers, silicon carbide fibers and basalt fibers.

11. The protection plate (100) according to any one of claims 1 to 10, It is characterized in that The honeycomb core layer (40) is smaller than the metal plate (30) in length and / or width direction; and a first anti-corrosion layer (50) is also provided on the surface of the metal plate (30) not covered by the honeycomb core layer (40).

12. The protection plate (100) according to claim 11, It is characterized in that The material of the first anti-corrosion layer (50) is the same as that of the first inorganic-organic composite layer (10), or the material of the first anti-corrosion layer (50) is the same as that of the second inorganic-organic composite layer (20).

13. The protection plate (100) according to claim 11 or 12, It is characterized in that The first anti-corrosion layer (50) and the first inorganic-organic composite layer (10) and / or the second inorganic-organic composite layer (20) are integrally formed.

14. The protection plate (100) according to any one of claims 1 to 10, It is characterized in that The metal plate (30) and the side wall of the honeycomb core layer (40) are also wrapped with a second anti-corrosion layer (60).

15. The protection plate (100) according to claim 14, It is characterized in that The material of the second anti-corrosion layer is the same as that of the first inorganic-organic composite layer (10), or the material of the second anti-corrosion layer (60) is the same as that of the second inorganic-organic composite layer (20).

16. The protection plate (100) according to any one of claims 1 to 15, It is characterized in that The thickness of the first inorganic-organic composite layer (10) is in the range of 0.8 mm to 2.8 mm, and the thickness of the second inorganic-organic composite layer (20) is in the range of 0.2 mm to 0.5 mm.

17. A battery pack (1), It is characterized in that The battery pack (1) comprises a tray (11), a battery cell assembly (12) and a protective plate (100) according to any one of claims 1 to 14, wherein the battery cell assembly (12) and the protective plate (100) are respectively installed on opposite sides of the tray (11).

18. The battery pack (1) according to claim 17, It is characterized in that The second inorganic-organic composite layer (20) is arranged close to the tray (11).

19. The battery pack (1) according to claim 17 or 18, It is characterized in that It also includes a sealing cover (13) arranged on the tray (11), wherein the sealing cover (13) and the tray (11) enclose a containing space.

20. An electrical device, It is characterized in that Comprising the battery pack (1) as claimed in claim 17.

Citation Information

Patent Citations

  • Preparation method of PP honeycomb composite reinforced steel protection plate

    CN115923308A

  • Battery pack protection plate, battery pack module and vehicle

    CN211907530U

  • Battery pack and vehicle

    CN213483866U

  • Protective plate for battery pack, battery pack and vehicle

    CN216980743U

  • Protective plate for battery pack

    CN217319639U

Cited By

  • Battery for electric or hybrid vehicles comprising a first plate and a second plate

    FR3173723A1

  • BATTERY FOR ELECTRIC OR HYBRID VEHICLES INCLUDING A JUNCTION PLATE

    FR3174259A1