Process for producing bases for petrochemistry, comprising ebullated-bed hydrocracking, fixed-bed hydrocracking, catalytic reforming and steam cracking
The process of distillation and subsequent hydroconversion and cracking stages efficiently converts crude oil into petrochemical bases, addressing inefficiencies in olefin and aromatic production by maximizing yield and flexibility in response to market demands.
Patent Information
- Application Number
- PCT/EP2024/061122
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-24
- Filing Date
- 2024-04-23
- Publication Date
- 2024-10-31
AI Technical Summary
Current processes for producing olefins and aromatics from crude oil face inefficiencies, particularly in treating heavy hydrocarbon fractions, leading to reduced yields and increased operability issues in steam cracking, and lack flexibility to adapt to market demands for either olefins or aromatics.
A process involving atmospheric and vacuum distillation followed by bubbling bed hydroconversion, fixed bed hydrocracking, steam cracking, and catalytic reforming, allowing for the conversion of almost all crude oil into petrochemical bases with adjustable parameters to maximize either olefin or aromatic production based on market demand.
Achieves a yield of over 75% petrochemical bases, enhances operability by treating all heavy hydrocarbon fractions efficiently, and allows for flexible production to meet market demands by optimizing the use of all distillation and conversion stages.
Smart Images

Figure EP2024061122_31102024_PF_FP_ABST
Abstract
Description
[0001] PROCESS FOR PRODUCING BASES FOR PETROCHEMICAL INDUSTRY COMPRISING BOILING BED HYDROCRACKING, FIXED UT HYDROCRACKING, CATALYTIC REFORMING AND STEAM CRACKING
[0002] TECHNICAL FIELD
[0003] The present invention relates to a process for producing olefins and aromatics for the petrochemical industry from a crude oil feedstock.
[0004] PRIOR TECHNIQUE
[0005] Improvements in engine power and the gradual electrification of some vehicles have led to a shift in demand for petroleum products, with a tendency to reduce growth in fuel demand. Conversely, growth in demand for petrochemical bases, particularly olefins, is more sustained. Ethylene and propylene, for example, are highly sought-after olefins, as they are essential intermediates for many petrochemical products such as polyethylene and polypropylene. There is therefore an interest in remodeling refining sites to produce at least some petrochemical bases, or in designing new integrated refining-petrochemical schemes, or in designing sites where most or all of the crude is converted into petrochemical bases.
[0006] The main process for the high-yield conversion of hydrocarbon fractions into olefins is steam cracking. The production of the desired olefins is accompanied by co-products, including aromatic compounds and pyrolysis oil, which require purification steps. In addition, the selectivity to the desired olefins is highly dependent on the quality of the feedstocks introduced into the steam cracking step. There is therefore an interest in identifying new processes for the production of olefins from heavy hydrocarbon fractions in a more efficient, cost-effective manner, and independent of the heavy hydrocarbon fraction being processed, including poor-quality feedstocks for steam cracking.
[0007] Furthermore, the main process for producing aromatic compounds is catalytic reforming, which is generally associated with complex separation and transformation steps in a section called the "aromatic complex". This aromatic complex produces commercial grade aromatic molecules (generally among benzene, toluene, ortho and para xylene), as well as a certain number of by-products, including raffinate which can be advantageously used as feedstock for steam cracking. Conversely, steam cracking produces a cut rich in aromatics which can be usefully valorized in the aromatic complex. It is therefore interesting to exploit the synergy of steam cracking with the aromatic complex to improve the economic profitability of a petrochemical complex.
[0008] In heavy hydrocarbon fraction treatment processes, residue hydroconversion removes some of the feedstock contaminants, including metals, sulfur, and asphaltenes. Deasphalting operations are also known. Deasphalting separates an asphaltene-rich asphalt fraction, known as "pitch," from a deasphalted oil fraction, known as DAO, with a significantly reduced asphaltene content, thus facilitating its recovery by catalytic cracking or hydrocracking.
[0009] Conversion products, and more specifically heavy cuts from conversion processes such as deasphalted oils and vacuum distillates, are difficult to process directly in a steam cracking and catalytic reforming stage. The presence of high levels of naphthenic compounds, heavy aromatics, and polyaromatics leads to a sharp drop in the yield of olefins of interest, an increase in the yield of pyrolysis oil, and increased coking of the steam cracking furnace tubes, which impairs operability. It is therefore necessary to improve the operability of the steam cracking stage in order to produce olefins with good yields.
[0010] Document US2019203130 discloses a process for converting a feedstock with a high sulfur content in an ebullated bed to obtain a cracked "fuel oil" effluent, this effluent is then separated into a light fraction and a heavy fraction, the light fraction is then hydrocracked to obtain a light naphtha cut, which can be sent to steam cracking to produce olefins, as well as a heavy naphtha cut which can be sent to a catalytic reforming stage for the production of aromatics.
[0011] Document US2021079305 discloses a method for treating a crude oil feedstock comprising an atmospheric distillation step to obtain at least one diesel cut and an atmospheric residue, a vacuum distillation step of the atmospheric residue to obtain at least one vacuum diesel cut, the diesel and vacuum diesel cuts are treated separately in hydrotreatment units to produce naphtha cuts which are then sent to different zones of a steam cracker. This document does not disclose an ebullated bed hydroconversion step of the vacuum residue or a catalytic reforming step for the production of aromatics.
[0012] The present invention aims to distinguish itself from the processes for producing petrochemical bases of the prior art by providing a process allowing almost total conversion of a crude oil feedstock into petrochemical bases including a step of deep conversion of the vacuum residue using ebullated bed hydroconversion, as well as in one embodiment of the steps of separate hydrocracking of distillate-type cuts according to their origin for the production of light and / or heavy naphtha intended for steam cracking and catalytic reforming steps to respectively produce olefins and aromatics.
[0013] SUMMARY OF THE INVENTION
[0014] The process according to the invention relates to a process for producing olefins and aromatics from a crude oil feedstock comprising the following steps: a) a step of atmospheric distillation of the crude oil feedstock and obtaining at least one naphtha cut, one diesel cut and one atmospheric residue cut; b) a step of vacuum distillation of the atmospheric residue cut obtained in step a) and obtaining at least one vacuum diesel cut and one vacuum residue cut; c) a step of ebullated bed hydroconversion of at least the vacuum residue cut obtained in step b), carried out in the presence of hydrogen and at least one hydroconversion catalyst, at a temperature of between 300 and 550°C, preferably between 400 and 460°C, under a total pressure of between 2 and 38 MPa, preferably between 10 and 25 MPa, at an hourly space velocity of between 0.05 and 10 h' 1 , preferably 0.1 and 0.2 h' 1and at a hydrogen partial pressure of between 5 and 30 MPa, preferably between 10 and 20 MPa, and obtaining at least one second naphtha cut, a second diesel cut and / or vacuum gas oil; d) a fixed-bed hydrocracking step of at least one diesel cut and / or vacuum gas oil chosen from the cuts obtained in steps a), b) and c) alone or as a mixture, carried out in the presence of hydrogen and at least one hydrocracking catalyst, at a temperature of between 250 and 480°C, preferably between 300 and 420°C under a pressure of between 2 and 25 MPa, at an hourly space velocity of between 0.3 and 6 h' 1 , preferably between 1 and 3 hours 1and at a hydrogen / hydrocarbon volume ratio of between 100 and 2000 L / L, and obtaining at least one light naphtha and / or heavy naphtha cut; e) a step of steam cracking at least one naphtha and / or light naphtha and / or heavy naphtha cut chosen from the cuts obtained in steps a), c) and d) alone or as a mixture, and obtaining at least one olefinic cut; f) a step of catalytic reforming of at least the heavy naphtha cut obtained in step d) and obtaining at least one reformate cut; g) a step of transformation and / or separation of the aromatics from at least the reformate cut obtained in step f) of catalytic reforming and obtaining at least one aromatic cut.
[0015] The method according to the present invention has the following advantages:
[0016] - the conversion into petrochemical bases (olefins and aromatics) of almost all of the crude oil, with a yield greater than 75% by weight, preferably 80% by weight of petrochemical bases relative to the weight of the crude oil feedstock.
[0017] - process flexibility allowing the treatment of all heavy hydrocarbon fractions regardless of their origin.
[0018] - The flexibility to direct production towards more olefins or, on the contrary, more aromatic compounds depending on market demand, by adjusting the operating parameters of the process.
[0019] - The conversion into cuts that can feed the steam cracking and / or catalytic reforming stages of almost all the effluents obtainable by the distillation, hydroconversion, hydrocracking units, as well as the recycling of almost all the unwanted cuts obtained in the steam cracking and / or catalytic reforming stages to the hydroconversion and / or hydrocracking units, thus making it possible to obtain an overall process optimized for the production of petrochemical bases with a high yield from crude oil.
[0020] LIST OF FIGURES
[0021] Figure 1
[0022] Process for producing olefins and aromatics according to a first embodiment of the invention.
[0023] Figure 2
[0024] Process for the production of olefins and aromatics according to a second embodiment of the invention further comprising two hydrocracking sections, a deasphalting step and a hydrotreatment step. Figure 3
[0025] A process for producing olefins and aromatics according to a third embodiment of the invention further comprising two hydrocracking sections, a deasphalting step, a hydrotreatment step and a gas distillation step.
[0026] Figure 4
[0027] Process for producing olefins and aromatics according to a fourth embodiment of the invention further comprising a step of isomerization of isobutane.
[0028] Figure 5
[0029] Process for producing olefins and aromatics according to a fifth embodiment of the invention further comprising two hydrocracking sections, a diesel cut and an unconverted oil cut being obtained at the end of the fixed bed hydrocracking step.
[0030] Figure 6
[0031] Process for the production of olefins and aromatics according to a sixth embodiment of the invention comprising sending the hydrotreated heavy naphtha cut to the steam cracking stage.
[0032] DETAILED DESCRIPTION OF THE INVENTION
[0033] According to the present invention, the expression "between ... and ..." and "between .... and ..." are equivalent and mean that the limit values of the interval are included in the range of values described. If this is not the case and the limit values are not included in the range described, such precision will be provided by the present invention.
[0034] For the purposes of the present invention, the different parameter ranges for a given step such as pressure ranges and temperature ranges may be used alone or in combination. For example, for the purposes of the present invention, a preferred pressure value range may be combined with a more preferred temperature value range.
[0035] In the following, particular embodiments of the invention may be described. They may be implemented separately or combined with each other, without limitation of combinations when this is technically feasible. The term “gas cut” means: a cut essentially comprising light gases or C1 to C4 alkanes, i.e. methane, ethane, propane, iso-butane and normal-butane.
[0036] LPG cut means: a cut comprising mainly light gases or C3 and C4 alkanes, i.e. propane, iso-butane and normal-butane.
[0037] Butane cut means: a cut comprising essentially isobutane (Ci-butane) and normal butane (n-butane).
[0038] Propane cut means: a cut comprising essentially propane.
[0039] The term C5+ cut is understood to mean: a cut resulting from the isomerization of butanes containing hydrocarbons with 5 carbon atoms or more.
[0040] Naphtha cut means: a cut comprising essentially hydrocarbon compounds boiling in a range between 28 and 175°C.
[0041] Light naphtha cut means: a cut comprising essentially hydrocarbon compounds boiling in a range between 28 and 101°C.
[0042] Heavy naphtha cut means: a cut comprising essentially hydrocarbon compounds boiling in a range between 65 and 175°C.
[0043] The cut-off point between light and heavy naphtha can vary between 65 and 101°C.
[0044] The higher the cut point between light and heavy naphtha, and in the range between 65°C and 101°C, the more the process maximizes olefin yields. In comparison, the lower the cut point between light and heavy naphtha, and in the range between 65°C and 101°C, the more the process maximizes aromatic yields.
[0045] Diesel cut means: a cut comprising essentially hydrocarbon compounds boiling in a range between 175 and 370°C.
[0046] Vacuum diesel cut means: a cut comprising essentially hydrocarbon compounds boiling in a range between 370 and 540°C.
[0047] Unconverted oil cut means: a cut comprising essentially hydrocarbon compounds boiling above a temperature of 370°C and produced by the distillation of the effluent from a fixed-bed vacuum diesel hydrocracker.
[0048] The term hydroconversion residue cut means: a cut essentially comprising hydrocarbon compounds boiling above a temperature of between 500 and 570°C, preferably above 540°C, and produced by the distillation of the effluent from a bubbling bed hydrocracker.
[0049] Atmospheric residue cut means: a cut comprising essentially hydrocarbon compounds boiling above 370°C.
[0050] Vacuum residue cut means: a cut essentially comprising hydrocarbon compounds boiling above a temperature of between 500 and 570°C, preferably above 540°C, and produced during vacuum distillation, preferably during vacuum distillation of an atmospheric residue cut.
[0051] The term “comprising essentially” means: of which the main constituent(s) by mass is / are, in particular comprising at least 70% by weight, preferably at least 80% by weight, preferentially at least 90% by weight of said constituent(s).
[0052] Purge cut means: a cut from diesel and / or vacuum gas oil hydrocracking processes comprising mainly hydrocarbon compounds boiling above 175°C.
[0053] Olefinic cut means: a cut resulting from steam cracking comprising more than 99% by weight, preferably more than 99.5% of alkenes, preferably with 2 to 4 carbon atoms.
[0054] Reformate cut means: a cut from the catalytic reformer comprising more than 75% by weight of aromatic hydrocarbon compounds.
[0055] Aromatic cut means: a cut comprising more than 99% by weight, preferably more than 99.5% of aromatic hydrocarbon compounds.
[0056] A raffinate cut is understood to mean: a cut from the aromatic complex comprising essentially non-aromatic hydrocarbon compounds having 5 to 8 carbon atoms.
[0057] Light pyrolysis gasoline cut means: the fraction of the steam cracking effluent containing hydrocarbons with 6 to 8 carbon atoms.
[0058] Heavy pyrolysis gasoline cut means: the fraction of the steam cracking effluent containing hydrocarbons with 9 to 10 carbon atoms.
[0059] Pyrolysis oil cut means: the fraction of the steam cracking effluent whose distillation temperature is above that defined for heavy pyrolysis gasoline. Heavy aromatic cut means: a cut from the aromatic complex comprising mainly C9-C10 aromatic compounds.
[0060] Asphalt fraction means: the product of the deasphalter which contains the majority of the asphaltenes contained in the charge of this unit.
[0061] Charge
[0062] The process according to the invention is a process for producing olefins and aromatics from a crude oil feedstock.
[0063] Crude oil feedstock means any type of oil from any geological source in unrefined form.
[0064] The crude oil feedstock can be advantageously chosen from Arabian Heavy, Arabian Medium, Arabian Light, Arabian Extra Light, other Gulf crudes, Brent, North Sea crude, North and West African crude, Indonesian crude, Chinese crude, or a mixture of them.
[0065] Advantageously, the feedstock is a crude whose vacuum residue obtained after atmospheric distillation and vacuum distillation can be converted in an ebullated bed hydroconversion unit. This advantageously corresponds to a crude having the following characteristics:
[0066] Density at 15°C less than 1.1
[0067] Sulphur content less than 7% by weight
[0068] Metal content (Nickel + Vanadium) less than 1000 ppm
[0069] Asphaltene content (nC7 insoluble) less than 15% by weight
[0070] Step a) atmospheric distillation
[0071] The process according to the invention comprises a step a) of atmospheric distillation of the crude oil feedstock and obtaining at least one naphtha cut, one diesel cut and one atmospheric residue cut.
[0072] In one embodiment, in step a) of atmospheric distillation of the crude oil feedstock, a gas cut is also obtained.
[0073] Atmospheric distillation of the crude oil feedstock separates the various components based on their evaporation temperature. The crude oil is desalted, then preheated and injected into a distillation tower and heated to approximately 400°C. The fractions containing the lightest hydrocarbons are recovered in gaseous form at the top of the column, such as the gas and naphtha fractions. The fractions with an intermediate boiling range, such as the diesel fraction, are withdrawn laterally in the middle section of the tower. The higher boiling fractions, such as the atmospheric residue fraction, remain in the lower part of the tower and are sent to a vacuum distillation tower for further fractionation.
[0074] Step b) vacuum distillation
[0075] The process according to the invention comprises a step b) of vacuum distillation of the atmospheric residue cut obtained in step a) and obtaining at least one vacuum diesel cut and one vacuum residue cut.
[0076] Heavy products extracted at the bottom of the atmospheric distillation column, such as the atmospheric residue cut, can no longer be separated by increasing the distillation temperature. Indeed, above 400°C, thermal cracking phenomena occur that can change the chemical nature of the products. To isolate these products, they are distilled at temperatures similar to those of atmospheric distillation, but under reduced pressure. The installations performing this operation are vacuum distillation columns. The vacuum diesel cut is recovered at the top of the column, and the vacuum residue cut is extracted at the bottom of the column and sent to the ebullated bed hydroconversion unit.
[0077] Step c) of hydroconversion in ebullated bed
[0078] The process according to the invention comprises a step c) of ebullated bed hydroconversion of at least the vacuum residue cut obtained in step b), carried out in the presence of hydrogen and at least one hydroconversion catalyst, at a temperature of between 300 and 550°C, preferably between 400 and 460°C, under a total pressure of between 2 and 38 MPa, preferably between 10 and 25 MPa, at an hourly space velocity of between 0.05 and 10 h' 1 , preferably 0.1 and 0.2 h' 1 and at a hydrogen partial pressure of between 5 and 30 MPa, preferably between 10 and 20 MPa, and obtaining at least one naphtha cut, one diesel cut and / or vacuum gas oil.
[0079] The pressure values given in this description are in absolute pressure.
[0080] Residue hydroconversion is a process aimed at converting heavy feedstocks by exposing them to severe temperature conditions in the presence of high-pressure hydrogen, in the presence of a solid catalyst containing metals such as Nickel or Molybdenum for example which are deposited on a support phase, often composed essentially of weakly acidic alumina and with porosity studied to allow the circulation of the reactants. Ebullated bed hydroconversion is a particular hydroconversion technology also called three-phase and well described in the literature.
[0081] Advantageously, the at least one hydroconversion catalyst may contain one or more elements from groups IVB to 11 B of the periodic table of elements, which may or may not be deposited on a support. It is advantageous to use a catalyst comprising a support, preferably amorphous, such as silica, alumina, silica-alumina, titanium dioxide or combinations of these structures, and very preferably alumina.
[0082] In this description, the groups of chemical elements are given according to the CAS classification (CRC Handbook of Chemistry and Physics, publisher CRC press, editor-in-chief DR Lide, 81st edition, 2000-2001). For example, group VIIIB according to the CAS classification corresponds to the metals of columns 8, 9 and 10 according to the new IUPAC classification.
[0083] The catalyst may contain at least one non-noble group VIIIB metal selected from nickel and cobalt, and preferably nickel, said group VIIIB element preferably being used in association with at least one group VIB metal selected from molybdenum and tungsten, and preferably the group VIB metal is molybdenum.
[0084] Advantageously, the hydroconversion catalyst used in the hydroconversion step comprises an alumina support and at least one group VIIIB metal selected from nickel and cobalt, preferably nickel, and at least one group VIB metal selected from molybdenum and tungsten, preferably molybdenum. Preferably, the hydroconversion catalyst comprises nickel as a group VIIIB element and molybdenum as a group VIB element.
[0085] The content of non-noble group VIIIB metal, in particular nickel, is advantageously between 0.5% and 10% expressed by weight of metal oxide (in particular NiO), and preferably between 1% and 6% by weight, and the content of group VI B metal, in particular molybdenum, is advantageously between 1% and 30% expressed by weight of metal oxide (in particular molybdenum trioxide MoO3), and preferably between 4% and 20% by weight. The metal contents are expressed as a percentage by weight of metal oxide relative to the weight of the catalyst.
[0086] This catalyst is advantageously used in the form of extrudates or beads. The extrudates have, for example, a diameter of between 0.5 and 4.0 mm and a length of between 1 and 5 mm. These catalysts are well known to those skilled in the art. In a particular embodiment of the invention, the hydroconversion step c) is carried out in a hybrid bed, simultaneously comprising at least one catalyst which is maintained in the reactor and at least one entrained catalyst which enters the reactor with the feedstock and which is entrained outside the reactor with the effluents. In this case, a type of entrained catalyst, also called "slurry" according to English terminology, is therefore used in addition to the hydroconversion catalyst which is maintained in the reactor in an ebullated bed. The entrained catalyst has, as a difference, a particle size and density adapted to its entrainment.Entrainment of the dispersed catalyst means its circulation in the three-phase reactor(s) by the liquid flows, said catalyst circulating with the feed in said three-phase reactor(s), and being withdrawn from said three-phase reactor(s) with the liquid effluent produced. These catalysts are well known to those skilled in the art.
[0087] The entrained catalyst may advantageously be obtained by injecting at least one active phase precursor directly into the hydroconversion reactor(s) and / or into the feedstock prior to introducing said feedstock into the hydroconversion step(s). The addition of precursor may be introduced continuously or discontinuously (depending on the operation, the type of feedstock being treated, the desired product specifications and the operability). According to one or more embodiments, the entrained catalyst precursor(s) is (are) pre-mixed with a hydrocarbon oil composed, for example, of hydrocarbons of which at least 50% by weight relative to the total weight of the hydrocarbon oil has a boiling point of between 180°C and 540°C, to form a dilute precursor pre-mix.According to one or more embodiments, the precursor or the diluted precursor premix is dispersed in the heavy hydrocarbon feedstock, for example by dynamic mixing (for example using a rotor, an agitator, etc.), by static mixing (for example using an injector, by force-feeding, via a static mixer, etc.), or only added to the feedstock to obtain a mixture. Any mixing and stirring techniques known to those skilled in the art can be used to disperse the precursor or the diluted precursor mixture in the feedstock of one or more hydroconversion stages.
[0088] Said active phase precursor(s) of the unsupported catalyst may be in liquid form such as for example precursors of metals soluble in organic media, such as molybdenum octoates and / or molybdenum naphthenates, or water-soluble compounds, such as phosphomolybdic acids and / or ammonium heptamolybdates. Said entrained catalyst may be formed and activated ex situ, outside the reactor under conditions suitable for activation, and then be injected with the feedstock. Said entrained catalyst may also be formed and activated in situ under the reaction conditions of one of the hydroconversion steps.
[0089] According to one embodiment, said entrained catalyst may be supported. In this case, the supported catalyst may advantageously be obtained:
[0090] - by grinding the supported hydroconversion catalyst, fresh or spent, or by grinding a mixture of fresh and spent catalysts, or
[0091] - by impregnation of at least one active phase precursor on a support having a particle size suitable for its entrainment and preferably a size between 0.001 and 100 μm. The active phase may be that described above as well as the support. Their description is not repeated here.
[0092] The embodiment in which hydroconversion step c) is carried out in a hybrid bed advantageously makes it possible to increase the hydroconversion yield.
[0093] Examples of ebullated bed hydroconversion reactors are Axens' H-OIL® or Lummus' LC FINING®.
[0094] In one embodiment, the ebullated bed hydroconversion step c) is carried out in a section comprising one or more ebullated bed hydroconversion reactors operating in series or in parallel.
[0095] In one embodiment, in step c) of ebullated bed hydroconversion, the vacuum residue cut obtained in step b) is converted together with all or part of the pyrolysis oil cut obtained in step e) of steam cracking. This embodiment advantageously makes it possible to increase the overall yield of the process in petrochemical products of interest.
[0096] In one embodiment, in step c) of ebullated bed hydroconversion, a hydroconversion residue cut is also obtained. This cut is advantageously sent to an optional deasphalting step in order to recover a deasphalted oil cut comprising valuable compounds that can undergo a catalytic hydrocracking step to obtain naphtha-type cuts that can feed the steam cracking and / or catalytic reforming step and thus increase the overall yield of the process in petrochemical bases. In one embodiment, in step c) of ebullated bed hydroconversion, a gas cut is also obtained.
[0097] Stage d) fixed bed hydrocracking
[0098] The process according to the invention comprises a fixed-bed hydrocracking step of at least one diesel and / or vacuum gas oil cut chosen from the cuts obtained in steps a), b) and c) alone or as a mixture, carried out in the presence of hydrogen and at least one hydrocracking catalyst, at a temperature of between 250 and 480°C, preferably between 300 and 420°C under a pressure of between 2 and 25 MPa, at an hourly space velocity of between 0.3 and 6 h' 1 , preferably between 1 and 3 hours 1 and at a hydrogen / hydrocarbon volume ratio of between 100 and 2000 L / L, and obtaining at least one light naphtha and / or heavy naphtha cut.
[0099] According to the invention, fixed bed hydrocracking step d) is carried out in the presence of at least one first hydrocracking catalyst, i.e. it is also possible to use sequences of 2 or more hydrocracking catalysts.
[0100] Preferably, the at least one hydrocracking catalyst is chosen from conventional hydrocracking catalysts known to those skilled in the art.
[0101] Advantageously, the at least one hydrocracking catalyst is of the bifunctional type combining an acid function with a hydrogenating function. The acid function is provided by supports with large surfaces (generally 150 to 1200 m2.g-1) having a surface acidity, such as halogenated aluminas (chlorinated or fluorinated in particular), combinations of boron and aluminum oxides, amorphous silica-aluminas and / or zeolites. The hydrogenating function is provided either by one or more metals from group VI 11 B of the periodic table of elements, or by a combination of at least one metal from group VIB of the periodic table and at least one metal from group VI II B.
[0102] Preferably, the at least one hydrocracking catalyst comprises a hydrogenating function composed of at least one metal from group VIB and at least one metal from group VIIIB of the periodic table, taken alone or as a mixture, said catalyst being a sulfide phase catalyst.
[0103] The metal(s) from group VIB are advantageously chosen from chromium, molybdenum and tungsten, alone or as a mixture and preferably chosen from molybdenum and tungsten. Preferably, the content of metal from group VIB in the hydrocracking catalyst(s) is advantageously between 5 and 35% by weight and preferably between 10 and 30% by weight, very preferably between 15 and 22% by weight, the percentages being expressed as percentage by weight of oxides.
[0104] The metal(s) of group VI HB are advantageously chosen from iron, cobalt, nickel, ruthenium, rhodium, palladium and platinum, and preferably from cobalt or nickel. Preferably, the content of metal of group VIIIB in the hydrocracking catalyst(s) is advantageously between 0.5 and 15.0% by weight and preferably between 2.0 and 10.0% by weight, very preferably between 2.5 and 6.0% by weight, the percentages being expressed as percentage by weight of oxides.
[0105] The at least one hydrocracking catalyst may also optionally comprise at least one promoter element deposited on the catalyst selected from the group consisting of phosphorus, boron and silicon, optionally at least one element from group VI IA (chlorine, fluorine preferred), optionally at least one element from group VI IB (manganese preferred), and optionally at least one element from group VB (niobium preferred).
[0106] Preferably, the at least one hydrocracking catalyst comprises an acid function chosen from alumina, silica alumina and zeolites, preferably chosen from Y zeolites and preferably chosen from silica alumina and zeolites.
[0107] In one embodiment, fixed bed hydrocracking step d) further comprises fixed bed hydrocracking of the deasphalted oil cut obtained in optional deasphalting step h).
[0108] In one embodiment, fixed bed hydrocracking step d) further comprises fixed bed hydrocracking of the heavy pyrolysis gasoline cut obtained in steam cracking step e).
[0109] In one embodiment, in hydrocracking step d), the diesel and vacuum gas oil cuts are hydrocracked jointly or separately in the same hydrocracking section, or separately in separate hydrocracking sections.
[0110] In one embodiment, in hydrocracking step d), the diesel, vacuum diesel, deasphalted oil and heavy pyrolysis gasoline cuts are hydrocracked jointly or separately in the same hydrocracking section, or separately in separate hydrocracking sections.
[0111] Advantageously, in hydrocracking step d), the diesel cuts are cracked in a first hydrocracking section, and the vacuum diesel cuts are cracked in a second hydrocracking section. Advantageously, in hydrocracking step d), the diesel cuts are cracked in a first hydrocracking section, and the vacuum diesel, deasphalted oil and heavy pyrolysis gasoline cuts are cracked in a second hydrocracking section.
[0112] This configuration makes it possible to optimize the operating conditions applied to each of the charges, and consequently, to maximize the yield of recoverable products from the complex, and / or to minimize the catalytic cost of the whole.
[0113] Advantageously, a hydrocracking section consists of a hydrotreatment reactor followed by two hydrocracking reactors.
[0114] In a very particular embodiment, said second hydrocracking section consists of a hydrotreatment reactor followed by a single hydrocracking reactor. This embodiment allows a significant reduction in the investment required for the process.
[0115] In this very particular embodiment, the fixed-bed hydrocracking step of at least one diesel cut in said first hydrocracking section leads to the production of at least one light naphtha cut and / or one heavy naphtha cut; the fixed-bed hydrocracking step of at least one vacuum gas oil cut in said second hydrocracking section leads to the production of at least one light naphtha cut and / or one heavy naphtha cut, one diesel cut and one unconverted oil cut.
[0116] In one embodiment, in step d) of fixed bed hydrocracking, at least one gas cut is further obtained.
[0117] In one embodiment, in step d) of fixed bed hydrocracking, at least one purge cut is further obtained.
[0118] In the process according to the present invention, all the cuts having heavy compounds (all the cuts with a distillation temperature above 175°C, with the exception of the asphalt cut produced by the deasphalter) from the different stages of the process are sent to the hydrocracking stage or stages in order to crack said heavy compounds and maximize the production of light and / or heavy naphtha to feed the steam cracking and catalytic reforming stages and thus increase the yield of bases for petrochemicals.
[0119] Step e) of steam cracking
[0120] The process according to the invention comprises a step e) of steam cracking at least one naphtha and / or light naphtha and / or heavy naphtha cut chosen from the cuts obtained in steps a), c) and d) alone or as a mixture, and obtaining at least one olefinic cut. In the very particular embodiment in which the second hydrocracking section comprises a hydrotreatment reactor and a single hydrocracking reactor, and in which a diesel cut and / or an unconverted oil cut is optionally obtained at the end of step d), the process comprises the steam cracking in step e), of said diesel cut and / or of said unconverted oil cut, obtained at the end of step d).
[0121] Furthermore, in this embodiment, the process comprises steam cracking in step e), the light naphtha cuts originating respectively from the first and second hydrocracking sections.
[0122] When the optional hydrotreatment step i) is carried out, the process comprises steam cracking in step e) of the hydrotreated light naphtha cut and / or a hydrotreated heavy naphtha cut.
[0123] When the optional isobutane isomerization step k) is implemented, the process comprises steam cracking in step e) of the n-butane and C5+ cuts.
[0124] The steam cracking step e) advantageously consists of the non-catalytic decomposition under the combined effect of high temperature and low pressure in the presence of water vapor, of saturated hydrocarbons, in order to produce aliphatic or aromatic unsaturated hydrocarbon fractions. Said fractions are then used for the synthesis of a large number of products, for example polyethylene or polypropylene. In the case of the process according to the invention, the steam cracking step e) makes it possible to produce mainly aliphatic unsaturated hydrocarbons.
[0125] The operating conditions are adjusted according to the nature of the load and the yields targeted for each of the main products.
[0126] Advantageously, the residence time in the steam cracking furnace is limited in order to limit the formation of heavy products. In addition, an effluent quench is implemented in order to freeze the composition of the effluent at the exit of the furnace.
[0127] Advantageously, the temperature at which the steam cracking furnaces are operated depends on the nature of the charge.
[0128] Advantageously, the steam cracking stage is implemented in a plant that consists of a number of furnaces, quenching boilers and a fractionation train. The hydrocarbon feedstock enters the hot section of the unit through the convection zone A of the furnace where it is preheated, then it is mixed with the water vapor also preheated in this same zone; the hydrocarbons and the water then pass through the actual radiation zone of the furnace where the rapid rise in temperature and the pyrolysis reactions take place. At the outlet of the furnace, the effluents are, in order to avoid any subsequent reaction, frozen in their kinetic possibilities of evolution by a sudden quench generally carried out in two stages: an initial indirect quench with water, followed by a direct quench using the heavy residue by-product of pyrolysis.The effluents are then transferred to a primary fractionation tower which separates at the bottom a heavy cut called "pyrolysis oil" and, by withdrawals, a part of the "pyrolysis gasoline" cut and water, while the light pyrolysis products exit at the top in gaseous form. After compression, washing with soda (intended to eliminate H2S and acid gases) and drying, these light effluents then enter the cold section of the unit which can be designed in various ways, but which ensures separation into various cuts of interest.
[0129] Advantageously, when the feed is a light naphtha and / or heavy naphtha cut, the residence time is between 0.1 and 0.4 seconds, the temperature at the tube outlet is between 700 and 900°C, preferably between 780 and 880°C, and the steam / feed ratio is between 0.2 and 1 kg / kg.
[0130] In the very particular embodiment in which a diesel cut and / or an unconverted oil cut is optionally obtained at the end of step d), advantageously, the residence time is between 0.1 and 0.6 seconds, the temperature at the tube outlet is between 700 and 900°C, preferably between 780 and 880°C, and the steam / charge ratio is between 0.5 and 1.5 kg / kg.
[0131] In one embodiment, steam cracking step e) further comprises steam cracking of at least one gas cut chosen from the cuts obtained in steps a), c), d) and f) alone or as a mixture.
[0132] When the optional hydrotreatment step i) is implemented, the gas cut can also be chosen in step i).
[0133] In one embodiment, steam cracking step e) further comprises steam cracking of the LPG fraction obtained in step g).
[0134] When the optional gas distillation step j) is implemented, the LPG cut can also be chosen in step j).
[0135] Advantageously, when the feedstock is an LPG cut, the residence time is between 0.1 and 0.4 seconds, the temperature at the tube outlet is between 700 and 1000°C, preferably between 800 and 900°C, and the steam / feed ratio is between 0.2 and 0.8 kg / kg. In one embodiment, steam cracking step e) further comprises steam cracking of the ethane cut obtained in step g).
[0136] Advantageously, when the feed is an ethane cut, the residence time is between 0.15 and 0.6 seconds, the temperature at the tube outlet is between 700 and 1000°C, preferably between 800 and 900°C, and the steam / feed ratio is between 0.1 and 0.6 kg / kg.
[0137] In one embodiment, steam cracking step e) further comprises steam cracking of the raffinate cut obtained in step g).
[0138] In one embodiment, the different cuts are steam cracked simultaneously or preferably separately. When they are cracked separately, they are cracked under different operating conditions depending on the nature of the cut to be steam cracked.
[0139] In one embodiment, in step e) of steam cracking, a pyrolysis oil cut is also obtained.
[0140] In one embodiment, in step e) of steam cracking, a light and / or heavy pyrolysis gasoline cut is also obtained.
[0141] In one embodiment, in step e) of steam cracking, a cut comprising H2, H2S, CO and CH4 is further obtained.
[0142] In one embodiment, in step e) of steam cracking, a butanes cut is also obtained.
[0143] In one embodiment, in step e) of steam cracking, the at least one olefinic fraction is ethylene.
[0144] In one embodiment, in steam cracking step e), the at least one olefinic fraction is propylene.
[0145] In one embodiment, in steam cracking step e), the at least one olefinic fraction is butadiene.
[0146] In one embodiment, in steam cracking step e), the at least one olefinic fraction is butene- 1
[0147] In one embodiment, in steam cracking step e), the at least one olefinic cut is butene- 2 In one embodiment, in steam cracking step e), the at least one olefinic cut is isobutene
[0148] Step f) of catalytic reforming
[0149] The process according to the invention comprises a step f) of catalytic reforming of at least the heavy naphtha cut obtained in step d) and obtaining at least one reformate cut.
[0150] The objective of catalytic reforming is to transform the naphthenic constituents and part of the paraffinic constituents (with a low octane number) into aromatic constituents with a high octane number. The catalytic reforming unit consists mainly of a series of at least three reactors containing at least one reforming catalyst and a separator to separate the different products at the reactor outlet. The catalyst used may be sensitive to the presence of sulfur and nitrogen products, which is why the inlet feed is advantageously free of sulfur, nitrogen and their derivatives.
[0151] The reaction advantageously takes place under pressures between 0.1 and 25 MPa and at high temperatures between 480 and 570°C. It is an endothermic reaction. The hydrocarbons of the heavy naphtha fraction (particularly paraffins and naphthenes) are transformed during this process into aromatic hydrocarbons and branched paraffins. Catalytic reforming produces a reformate fraction which significantly improves the octane number of petroleum fractions, and also produces hydrogen.
[0152] Advantageously, the hydrogen / hydrocarbon molar ratio (H2 / HC) is between 0.8 and 8 mole / mole.
[0153] Advantageously, the mass flow rate of the heavy naphtha cut to be treated per unit mass of catalyst and per hour is between 0.1 and 10 h' 1 , preferably between 0.5 and 6 h' 1 .
[0154] Advantageously, the reforming catalyst comprises an active phase comprising at least one metal chosen from nickel, ruthenium, rhodium, palladium, iridium or platinum, and at least one promoter chosen from rhenium, tin, germanium, cobalt, nickel, iridium, rhodium or ruthenium. Preferably, the reforming catalyst comprises an active phase comprising platinum and tin. The amount of metal is between 0.02 and 2% by weight, preferably between 0.05 and 1.5% by weight, even more preferably between 0.1 and 0.8% by weight relative to the total weight of the catalyst. Preferably, the reforming catalyst comprises a support chosen from alumina, silica-alumina or silica. Preferably, the support is based on alumina. In one embodiment, in step f) of catalytic reforming, at least one gas cut is further obtained.
[0155] In one embodiment, in step f) of catalytic reforming, at least one hydrogen cut is further obtained.
[0156] Step g) of transformation and / or separation of aromatics
[0157] The process according to the invention comprises a step g) of transformation and / or separation of the aromatics from at least the reformate cut obtained in step f) of catalytic reforming and obtaining at least one aromatic cut.
[0158] The objective of this step is twofold:
[0159] Convert aromatic C9s and possibly aromatic C10s into benzene, toluene, ortho xylene and para xylene,
[0160] - Adjust the proportions of these different molecules by adjusting the number and position of the methyl substituents on the aromatic rings.
[0161] The processes advantageously used to carry out this step are described below. The judicious choice of catalysts and operating conditions advantageously makes it possible to minimize yield losses:
[0162] Less than 5% loss of methyl groups
[0163] Less than 5% loss of aromatic cycles
[0164] Preferably, this step takes place within an aromatic complex which advantageously constitutes a set of steps of separation, purification and conversion of aromatic molecules present in the reformate.
[0165] The objective of an aromatic complex is to produce with very high purity (compatible with polymerization) benzene, para-xylene, and sometimes toluene and ortho-xylene, as well as heavy aromatics, from aromatic-rich fractions such as reformate or pyrolysis gasoline. Advantageously, in a first step, olefins and non-aromatics are removed in units such as earth treatment, hydrogenation units, extractive distillations or liquid / liquid extraction units. Advantageously, in a second step, a separation train, composed of different distillation columns, produces benzene, toluene, an aromatics cut containing 8 carbon atoms (or A8 cut), and one or more cuts containing aromatics with more than 9 carbon atoms.Advantageously, the A8 cut enters the “xylene loop”, in which paraxylene is separated from the other xylene isomers either in a liquid / liquid extraction unit based on simulated moving bed (SMB) technology, or in a crystallization unit. The other constituents of the A8 cut (ortho and meta xylene, ethyl benzene) are advantageously isomerized or converted by means of a liquid-phase or gas-phase isomerization unit, and return to the separation train. All or part of the toluene is advantageously converted in transalkylation, disproportionation, or methyl-alkylation units to produce more C8 aromatics and benzene. Aromatics containing 9 or 10 carbon atoms can advantageously be sent to a transalkylation unit to produce more 8-carbon aromatics.As for the heavier aromatics (11 carbon atoms and more), they are considered by-products, and advantageously exported as gasoline base.
[0166] In one embodiment, step g) of transformation and / or separation of the aromatics further comprises a transformation and / or separation of the aromatics from the light pyrolysis gasoline cut obtained in step e) of steam cracking, preferably jointly with the reformate cut.
[0167] In one embodiment, in step g) of transformation and / or separation of the aromatics, an LPG cut is also obtained.
[0168] In one embodiment, in step g) of transformation and / or separation of the aromatics, an ethane cut is also obtained.
[0169] In one embodiment, in step g) of transformation and / or separation of the aromatics, a raffinate cut is also obtained.
[0170] In one embodiment, in step g) of transformation and / or separation of the aromatics, a heavy aromatic cut is also obtained.
[0171] In one embodiment, in step g) of transformation and / or separation of the aromatics, the at least one aromatic fraction is benzene.
[0172] In one embodiment, in step g) of transformation and / or separation of the aromatics, the at least one aromatic fraction is paraxylene.
[0173] It is also possible to produce other aromatic fractions such as toluene or orthoxylene.
[0174] Optional steps Step h) deasphalting
[0175] In one embodiment, the process according to the invention further comprises a step h) of deasphalting the hydroconversion residue cut obtained in step c) in the presence of at least one solvent, and obtaining at least one deasphalted oil cut.
[0176] Advantageously, deasphalting is a liquid-liquid extraction generally carried out at an average temperature between 45 and 280°C with at least one hydrocarbon solvent.
[0177] Advantageously, the hydrocarbon solvents used for deasphalting are low-boiling solvents, preferably paraffinic solvents, preferably having from 3 to 7 carbon atoms, and preferably heavier than propane. Preferred solvents include propane, butane, isobutane, pentane, isopentane, neopentane, hexane, isohexanes, C6 hydrocarbons, heptane, C7 hydrocarbons, more or less apolar light gasolines, as well as mixtures obtained from the aforementioned solvents. Preferably, the solvent is butane, pentane or hexane, as well as mixtures thereof. The following table gives an example, for some solvents, of the ranges of typical operating conditions for deasphalting as a function of the solvent:
[0178] Table 1
[0179] In one embodiment, in step h) of deasphalting, an asphalt cut is further obtained.
[0180] Stage i) of hydrotreatment
[0181] In one embodiment, the process according to the invention further comprises a step i) of hydrotreatment of the naphtha cut obtained in step a) and / or in step c), and obtaining at least one hydrotreated naphtha cut.
[0182] In a preferred embodiment, step i) of hydrotreatment of the naphtha cut obtained in step a) and / or in step c) is followed by a step of separation and obtaining at least one hydrotreated light naphtha cut and / or hydrotreated heavy naphtha cut. When this hydrotreatment step i) is carried out, then in step e): the at least one naphtha cut is the hydrotreated naphtha cut obtained in step i), the at least one light naphtha cut can also be chosen in step i), the at least one heavy naphtha cut can also be chosen in step i).
[0183] When this hydrotreatment step i) is implemented, then in step f): the heavy naphtha cut can also be chosen in step i).
[0184] When the process includes steam cracking in step e) of the hydrotreated heavy naphtha cut, the process is geared towards the production of olefins.
[0185] The optional hydrotreatment step is preferably carried out in one or more units comprising one or more reactors comprising at least one hydrotreatment catalyst in the presence of dihydrogen, and advantageously allows the elimination of sulfur (hydrodesulfurization), and / or the elimination of nitrogen (hydrodenitrogenation or hydrodenitration) which are poisons for the catalysts used in the downstream units such as the catalytic reforming unit for example,
[0186] The operating conditions used in step i) of the process according to the invention advantageously make it possible to carry out hydrotreatment of the feedstock so as to achieve an organic nitrogen content in the effluent of less than 1 ppm by weight.
[0187] The operating conditions used in step i) of the process according to the invention advantageously make it possible to carry out hydrotreatment of the feedstock so as to achieve a sulfur content in the effluent of less than 1 ppm by weight.
[0188] The hydrotreatment step i) is carried out in the presence of at least one hydrotreatment catalyst, i.e. it is possible to use sequences of 2 or more hydrotreatment catalysts. The hydrotreatment catalyst is advantageously chosen from conventional hydrotreatment catalysts known to those skilled in the art.
[0189] Preferably, the at least one catalyst comprises a hydrogenating function composed of at least one metal from group VI B and at least one metal from group VIII B of the periodic table, taken alone or as a mixture, said catalyst being a catalyst having a sulfide phase as active phase.
[0190] The metal(s) of group VI B are advantageously chosen from chromium, molybdenum and tungsten, alone or as a mixture and preferably chosen from molybdenum and tungsten. Preferably, the content of metal of group VI B in the hydrotreatment catalyst(s) is advantageously between 5 and 40% by weight and preferably between 7 and 30% by weight, very preferably between 10 and 28% by weight, the percentages being expressed as percentage by weight of oxides.
[0191] The group VIII metal(s) are advantageously chosen from iron, cobalt, nickel, ruthenium, rhodium, palladium and platinum, and preferably from cobalt or nickel. Preferably, the group VIII metal content in the hydrotreatment catalyst(s) is advantageously between 0.5 and 15% by weight and preferably between 1.5 and 10% by weight, the percentages being expressed as percentage by weight of oxides.
[0192] The hydrotreatment catalyst(s) may also advantageously comprise at least one promoter element deposited on said catalyst selected from the group formed by phosphorus, boron and silicon, optionally at least one element from group VI IA (chlorine and fluorine preferred), optionally at least one element from group VI IB (manganese preferred), and optionally at least one element from group VB (niobium preferred). The concentration of said promoter is advantageously less than 20% by weight, and preferably less than 10% by weight.
[0193] Advantageously, the catalyst may further contain one or more adjuvant additives leading to better dispersion and promotion of the active phase of the catalyst, so as to improve its activity. Said additives are typically one or more organic compounds containing oxygen and / or one or more organic compounds containing nitrogen and / or one or more organic compounds containing sulfur. Preferably, the catalyst according to the invention may further comprise one or more organic compounds containing oxygen and / or one or more organic compounds containing nitrogen. Preferably, the organic compound contains at least 2 carbon atoms and at least one oxygen and / or nitrogen atom, without containing other heteroatoms. A catalyst containing an adjuvant additive is typically prepared by a process of impregnating a support with metal salts, in ranges such as those described for the catalyst without adjuvant additive.The introduction of the organic compound advantageously comprises several modes of implementation which are distinguished in particular by the time of the introduction of the organic compound in relation to the introduction of the metals. It can be carried out either at the same time as the impregnation of the metals (co-impregnation), or after the impregnation of the metals (post-impregnation), or finally before the impregnation of the metals (pre-impregnation) in particular during the preparation of the support, and preferably during the shaping or by impregnation on an already formed support. When it is / are present, the total content of organic compound(s) containing oxygen and / or nitrogen and / or sulfur present in the catalyst is generally between 1 and 30% by weight, preferably between 1.5 and 25% by weight, and more preferably between 2 and 20% by weight relative to the total weight of the catalyst.When preparing the catalyst requiring a drying step, the drying step(s) following the introduction of the organic compound is (are) carried out at a temperature below 200°C so as to preferably retain at least 30%, preferably at least 50%, and very preferably at least 70% of the quantity of the organic compound introduced calculated on the basis of the carbon remaining on the catalyst. The remaining carbon is measured by elemental analysis according to ASTM D5373.
[0194] Advantageously, the at least one hydrotreatment catalyst may be a fresh catalyst, i.e. a catalyst which has not been used as a catalyst previously in a catalytic unit and in particular in hydrotreatment and / or hydrocracking.
[0195] In one embodiment, the catalyst may also be a regenerated and / or rejuvenated catalyst. A regenerated and / or rejuvenated catalyst is understood to mean a catalyst which has been used as a catalyst in a catalytic unit and in particular in hydrotreatment and / or hydrocracking and which has been subjected to at least one step of partial or total elimination of the coke, for example by calcination (regeneration). The regeneration can be carried out by any means known to those skilled in the art.
[0196] When the regenerated catalyst no longer comprises enough active phase, phosphorus or when it has a ratio or ratios outside the ratios described, the regenerated catalyst can advantageously be rejuvenated by introducing one or more precursors of the active phase and / or the phosphorus into the regenerated catalyst. It is also possible to introduce at least one organic compound simultaneously with the metals and the phosphorus or separately. The organic compound introduced may or may not be identical to the organic compound of the fresh catalyst when this catalyst contained such an organic compound.
[0197] Preferably, the hydrotreatment catalyst(s) are supported on a support chosen from alumina, silica-alumina, and preferably on alumina.
[0198] A preferred catalyst comprises at least one Group VI B metal and / or at least one non-noble Group VIII metal, and an alumina support. An even more preferred catalyst consists of cobalt and / or nickel, molybdenum and alumina.
[0199] In one embodiment, in step i) of hydrotreatment, a gas cut is also obtained.
[0200] Step j) of gas distillation In one embodiment, the method according to the invention further comprises a step j) of gas distillation of at least one gas cut chosen from the cuts obtained in steps a), c) and d) alone or as a mixture, and obtaining at least one LPG cut.
[0201] The objective of this step is to separate the total gas flow into two parts:
[0202] - A flow composed mainly of LPG which can be advantageously sent to the steam cracker
[0203] - A stream composed of the lightest fractions, namely mainly methane, ethane, and in some cases, traces of hydrogen. This stream is generally used as fuel.
[0204] The processes advantageously used to carry out this step consist of a set of distillation columns arranged according to various schemes well known to those skilled in the art. The overall recovery rate of the LPG cut is generally greater than 75%.
[0205] Preferably, this step is carried out within a “gas plant” according to English terminology, a structure well known to those skilled in the art.
[0206] In one embodiment, in step j) of distillation of the gases, a cut comprising methane and ethane (cut 01 / 02) is also obtained.
[0207] In one embodiment, the LPG fraction can be separated into at least one propane fraction and one butanes fraction. The propane fraction is sent to step e) of steam cracking and the butanes fraction is sent to step k) of isomerization of isobutane.
[0208] Step k) of isomerization of isobutane
[0209] In one embodiment, the process according to the invention further comprises a step k) of isomerization of isobutane (i-butane) of at least one butane cut chosen from the cuts obtained in steps e) and j) alone or as a mixture, and obtaining at least one normal-butane cut (n-butane).
[0210] The isomerization step consists mainly of an isobutane / n-butane separation column followed by a set of at least two isomerization reactors containing one or more isobutane / n-butane isomerization catalysts, and a separator allowing the production of a gas cut and a cut composed of a mixture of isobutane and normal-butane (iC4 / nC4). The iC4 / nC4 cut thus obtained is returned to the isobutane / n-butane separation column allowing the production of three streams. At the top of the column, a stream rich in isobutane is returned to said set of at least two isomerization reactors at the bottom of the column, a stream of butanes containing hydrocarbons with 5 carbon atoms and more (C5+) is sent to the steam cracker, and by lateral withdrawal, a stream rich in n-butane is also sent to the steam cracker.
[0211] Advantageously, the reaction takes place under a pressure of between 1.0 and 4.0 MPa, and preferably between 2.0 and 3.5 MPa, as well as at a temperature of between 140 and 250°C, and preferably between 150 and 200°C.
[0212] Advantageously, the isomerization reaction of step k) is carried out at a WH (or hourly volumetric flow rate) of between 1 and 10 h -1 , preferably between 1 and 5 hours" 1 , WH being defined as the ratio between the volume flow rate of feedstock and the volume of isomerization catalyst.
[0213] Advantageously, the hydrogen / hydrocarbon molar ratio (H2 / HC) is between 0.01 and 5 mole / mole, and preferably between 0.01 and 2 mole / mole.
[0214] Preferably, the isomerization catalyst is chosen from conventional isomerization catalysts known to those skilled in the art.
[0215] Preferably, the catalyst comprises an active phase composed of at least one metal from group VII IB of the periodic table,
[0216] The group VIIIB metal(s) are advantageously chosen from iron, cobalt, nickel, ruthenium, rhodium, palladium and platinum, and preferably from cobalt or platinum. Preferably, the content of group VIIIB metal in the isomerization catalyst(s) is advantageously between 0.1 and 5.0% by weight and preferably between 0.1 and 1.0% by weight.
[0217] It is advantageous to use a catalyst comprising a support, preferably amorphous, such as silica, alumina, silica-alumina, titanium dioxide or combinations of these structures, and very preferably alumina.
[0218] Advantageously, the support is chlorinated with a chlorine content of between 5 and 20% by weight and preferably between 5 and 10% by weight.
[0219] In one embodiment, in step k) of isomerization of isobutane (iC4), a gas cut is also obtained.
[0220] This step, which converts isobutane into n-butane, allows for a higher yield of ethylene from the steam cracker. DESCRIPTION OF FIGURES
[0221] Figure 1: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a naphtha cut 9, a diesel cut 10 and a vacuum diesel cut 11. Cuts 4, 6, 10 and 11 are sent to a hydrocracking step d) to obtain a light naphtha cut 17 / 21, and a heavy naphtha cut 18 / 22. Cuts 3, 9, 17 / 21 and possibly 18 / 22 are sent to a steam cracking step e) to obtain an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene). Cut 18 / 22 is sent to a catalytic reforming step f) to obtain a reformate cut 29.Cut 29 is sent to a step g) of transformation and / or separation of the aromatics to obtain an aromatic cut (33 benzene, or 34 paraxylene).
[0222] Figure 2: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a gas cut 2, a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a gas cut 8, a naphtha cut 9, a diesel cut 10, a vacuum diesel cut 11, and a hydroconversion residue cut 12. Cuts 4 and 10 are sent to a first hydrocracking section d-S1) to obtain a gas cut 16, a light naphtha cut 17, a heavy naphtha cut 18 and a purge cut 19. Cuts 6 and 11 are sent to a second hydrocracking section d-S2) to obtain a cut gas 20, a light naphtha cut 21, a heavy naphtha cut 22 and a purge cut 23.Cuts 2, 8, 16, 17, 20, 21 are sent to a steam cracking step e) to obtain a cut 36 comprising H2, H2S, CO and CH4, an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene), a light pyrolysis gasoline cut 40, a heavy pyrolysis gasoline cut 41 and a pyrolysis oil cut 42. Cut 41 is sent to the second hydrocracking section d-S2). Cut 42 is sent to the ebullated bed hydroconversion step c). Cuts 18 and 22 are sent to a catalytic reforming step f) to obtain a hydrogen cut 27, a gas cut 28, and a reformate cut 29. Cut 28 is sent to the steam cracking step e). Cuts 29 and 40 are sent to a step g) of transformation and / or separation of the aromatics to obtain an ethane cut 30, an LPG cut 31, a raffinate cut 32, an aromatic cut (33 benzene, or 34 paraxyiene), and a heavy aromatic cut 35.Cut 12 is sent to a step h) of deasphalting by a solvent 13 to obtain an asphalt cut 14 and a deasphalted oil cut 15. Cut 15 is sent to the second hydrocracking section d-S2). Cuts 3 and 9 are sent to a step i) of hydrotreatment to obtain a gas cut 24, a hydrotreated light naphtha cut 25 and a hydrotreated heavy naphtha cut 26. Cuts 24 and 25 are sent to step e) of steam cracking. Cut 26 is sent to step f) of catalytic reforming.
[0223] Figure 3: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a gas cut 2, a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a gas cut 8, a naphtha cut 9, a diesel cut 10, a vacuum diesel cut 11, and a hydroconversion residue cut 12. Cuts 4 and 10 are sent to a first hydrocracking section d-S1) to obtain a gas cut 16, a light naphtha cut 17, a heavy naphtha cut 18 and a purge cut 19. Cuts 6 and 11 are sent to a second hydrocracking section d-S2) to obtain a cut gas 20, a light naphtha cut 21, a heavy naphtha cut 22 and a purge cut 23.Cuts 17 and 21 are sent to a steam cracking step e) to obtain a cut 36 comprising H2, H2S, CO and CH4, an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene), a light pyrolysis gasoline cut 40, a heavy pyrolysis gasoline cut 41 and a pyrolysis oil cut 42. Cut 41 is sent to the second hydrocracking section d-S2). Cut 42 is sent to the ebullated bed hydroconversion step c). Cuts 18 and 22 are sent to a catalytic reforming step f) to obtain a hydrogen cut 27, a gas cut 28, and a reformate cut 29. Cut 28 is sent to the steam cracking step e). Cuts 29 and 40 are sent to a step g) of transformation and / or separation of the aromatics to obtain an ethane cut 30, an LPG cut 31, a raffinate cut 32, an aromatic cut (33: benzene, or 34: paraxyiene), and a heavy aromatic cut 35.Cut 12 is sent to a step h) of deasphalting by a solvent 13 to obtain an asphalt cut 14 and a deasphalted oil cut 15. Cut 15 is sent to the second hydrocracking section d-S2). Cuts 3 and 9 are sent to a step i) of hydrotreatment to obtain a gas cut 24, a hydrotreated light naphtha cut 25 and a hydrotreated heavy naphtha cut 26. Cut 25 is sent to step e) of steam cracking. Cut 26 is sent to step f) of catalytic reforming. Cuts 2, 8, 16, 20, 24 are sent to a step j) of gas distillation to obtain a cut comprising methane and ethane 43 and an LPG cut 44. Cut 44 is sent to step e) of steam cracking.
[0224] Figure 4: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a gas cut 2, a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a gas cut 8, a naphtha cut 9, a diesel cut 10, a vacuum diesel cut 11, and a hydroconversion residue cut 12. Cuts 4 and 10 are sent to a first hydrocracking section d-S1) to obtain a gas cut 16, a light naphtha cut 17, a heavy naphtha cut 18 and a purge cut 19. Cuts 6 and 11 are sent to a second hydrocracking section d-S2) to obtain a cut gas 20, a light naphtha cut 21, a heavy naphtha cut 22 and a purge cut 23.Cuts 17 and 21 are sent to a steam cracking step e) to obtain a cut 36 comprising H2, H2S, CO and CH4, an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene), a butanes cut 49, a light pyrolysis gasoline cut 40, a heavy pyrolysis gasoline cut 41 and a pyrolysis oil cut 42. Cut 41 is sent to the second hydrocracking section d-S2). Cut 42 is sent to the ebullated bed hydroconversion step c). Cuts 18 and 22 are sent to a catalytic reforming step f) to obtain a hydrogen cut 27, a gas cut 28, and a reformate cut 29. Cut 28 is sent to the steam cracking step e). Cuts 29 and 40 are sent to a step g) of transformation and / or separation of the aromatics to obtain an ethane cut 30, an LPG cut 31, a raffinate cut 32, an aromatic cut (33: benzene, or 34: paraxylene), and a heavy aromatic cut 35.Cut 12 is sent to a step h) of deasphalting by a solvent 13 to obtain an asphalt cut 14 and a deasphalted oil cut 15. Cut 15 is sent to the second hydrocracking section d-S2). Cuts 3 and 9 are sent to a step i) of hydrotreatment to obtain a gas cut 24, a hydrotreated light naphtha cut 25 and a hydrotreated heavy naphtha cut 26. Cut 25 is sent to step e) of steam cracking. Cut 26 is sent to step f) of catalytic reforming. Cuts 2, 8, 16, 20, 24 are sent to a gas distillation step j) to obtain a cut comprising methane and ethane 43, a propane cut 44 and a butane cut 45. Cut 45 and cut 49 are sent to step k) of isomerization of isobutane (iC4) to obtain a gas cut 46, a stream rich in n-butane 47 and a stream containing hydrocarbons with 5 carbon atoms and more (C5+) 48.Cuts 44, 47 and 48 are sent to steam cracking step e).
[0225] Figure 5: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a gas cut 2, a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a gas cut 8, a naphtha cut 9, a diesel cut 10, a vacuum diesel cut 11, and a hydroconversion residue cut 12. Cuts 4 and 10 are sent to a first hydrocracking section d-S1) to obtain a gas cut 16, a light naphtha cut 17, a heavy naphtha cut 18 and a purge cut 19. Cuts 6 and 11 are sent to a second hydrocracking section d-S2) to obtain a cut gas 20, a light naphtha cut 21, a heavy naphtha cut 22, a diesel cut 43 and an unconverted oil cut 44.Cuts 2, 8, 16, 17, 20, 21, 43 and 44 are sent to a steam cracking step e) to obtain a cut 36 comprising H2, H2S, CO and CH4, an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene), a light pyrolysis gasoline cut 40, a heavy pyrolysis gasoline cut 41 and a pyrolysis oil cut 42. Cut 41 is sent to the second hydrocracking section d-S2). Cut 42 is sent to the ebullated bed hydroconversion step c). Cuts 18 and 22 are sent to a catalytic reforming step f) to obtain a hydrogen cut 27, a gas cut 28, and a reformate cut 29. Cut 28 is sent to the steam cracking step e). Cuts 29 and 40 are sent to a step g) of transformation and / or separation of the aromatics to obtain an ethane cut 30, an LPG cut 31, a raffinate cut 32, an aromatic cut (33 benzene, or 34 paraxylene), and a heavy aromatic cut 35.Cut 12 is sent to a step h) of deasphalting by a solvent 13 to obtain an asphalt cut 14 and a deasphalted oil cut 15. Cut 15 is sent to the second hydrocracking section d-S2). Cuts 3 and 9 are sent to a step i) of hydrotreatment to obtain a gas cut 24, a hydrotreated light naphtha cut 25 and a hydrotreated heavy naphtha cut 26. Cuts 24 and 25 are sent to the step e) of steam cracking. Cut 26 is sent to the step f) of catalytic reforming.
[0226] Figure 6: A crude oil feedstock 1 is sent to an atmospheric distillation step a) to obtain a gas cut 2, a naphtha cut 3, a diesel cut 4 and an atmospheric residue cut 5. Cut 5 is sent to a vacuum distillation step b) to obtain a vacuum diesel cut 6 and a vacuum residue cut 7. Cut 7 is sent to an ebullated bed hydroconversion step c) to obtain a gas cut 8, a naphtha cut 9, a diesel cut 10, a vacuum diesel cut 11, and a hydroconversion residue cut 12. Cuts 4 and 10 are sent to a first hydrocracking section d-S1) to obtain a gas cut 16, a light naphtha cut 17, a heavy naphtha cut 18 and a purge cut 19. Cuts 6 and 11 are sent to a second hydrocracking section d-S2) to obtain a cut gas 20, a light naphtha cut 21, a heavy naphtha cut 22 and a purge cut 23.Cuts 2, 8, 16, 17, 20, 21 are sent to a steam cracking step e) to obtain a cut 36 comprising H2, H2S, CO and CH4, an olefinic cut (37 ethylene, or 38 propylene, or 39 butadiene), a light pyrolysis gasoline cut 40, a heavy pyrolysis gasoline cut 41 and a pyrolysis oil cut 42. Cut 41 is sent to the second hydrocracking section d-S2). Cut 42 is sent to the ebullated bed hydroconversion step c). Cuts 18 and 22 are sent to a catalytic reforming step f) to obtain a hydrogen cut 27, a gas cut 28, and a reformate cut 29. Cut 28 is sent to the steam cracking step e). Cuts 29 and 40 are sent to a step g) of transformation and / or separation of the aromatics to obtain an ethane cut 30, an LPG cut 31, a raffinate cut 32, an aromatic cut (33 benzene, or 34 paraxylene), and a heavy aromatic cut 35.Cut 12 is sent to a step h) of deasphalting by a solvent 13 to obtain an asphalt cut 14 and a deasphalted oil cut 15. Cut 15 is sent to the second hydrocracking section d-S2). Cuts 3 and 9 are sent to a step i) of hydrotreatment to obtain a gas cut 24, a hydrotreated light naphtha cut 25 and a hydrotreated heavy naphtha cut 26. Cuts 24, 25 and 26 are sent to the steam cracking step e).
[0227] EXAMPLES
[0228] Example 1: Method according to the embodiment of Figure 2
[0229] The example below illustrates a particular implementation of the method according to the invention without limiting its scope.
[0230] Heavy hydrocarbon feedstock 1 treated in the process is a crude oil from the Middle East and having the properties indicated in the table below. Table 2
[0231] The feed is subjected to a step a) of atmospheric distillation, the cuts obtained are described in the table below.
[0232] Table 3
[0233] The atmospheric residue cut 5 is sent to step b) of vacuum distillation, the cuts obtained are described in the table below.
[0234] Table 4
[0235] The vacuum residue cut 7 and the heavy pyrolysis oil cut 42 from the steam cracking step e) are subjected to a hydroconversion step c) in two ebullated bed reactors in series and in the presence of a NiMo on Alumina ebullated bed hydroconversion catalyst under the conditions indicated in the table below.
[0236] Table 5
[0237] A hydroconversion residue cut 12 obtained in hydroconversion step c) is sent to a deasphalting step h) carried out in an extraction column operating continuously under the conditions presented in the table below.
[0238] Table 6
[0239] At the end of deasphalting step h), a deasphalted oil cut 15 is obtained with a yield of 60%, this yield is related to the feedstock entering the deasphalting step corresponding to the hydroconversion residue cut 12.
[0240] At the end of steps c) and h), a diesel cut 10 from the hydroconversion step c) and a diesel cut 4 from the atmospheric distillation step a) are sent to a fixed-bed hydrocracking step d) in a first section d-S1 carried out under the conditions presented in the following table. Table 7
[0241] A vacuum diesel cut 6 from vacuum distillation step b), the deasphalted oil cut 15, a vacuum diesel cut 11 from ebullated bed hydroconversion step c) and the heavy pyrolysis gasoline cut 41 from steam cracking step e) are sent to fixed bed hydrocracking step d) in a second section d-S2, the conditions of which are presented in the following table.
[0242] Table 8
[0243]
[0244] The naphtha cut 3 from atmospheric distillation step a) and a naphtha cut 9 from ebullated bed hydroconversion step c) are sent to a fixed bed hydrotreatment step i) under the conditions indicated in the following table.
[0245] Table 9
[0246] The heavy naphtha cuts 18, 22 and 26 from the hydrocracking stages d) in sections d-S1 and d-S2 and i) hydrotreatment respectively are sent to a catalytic reforming stage f) and treated under the conditions set out in the following table. Table 10
[0247] WAIT = weighted-average inlet temperature according to Anglo-Saxon terminology or weighted average temperature at the entrance to the reforming stage.
[0248] The reformate cut 29 from the catalytic reforming step f) and the light pyrolysis gasoline cut 40 from the steam cracking step e) are sent to the aromatics transformation and / or separation step g).
[0249] The light naphtha cuts 17, 21, 25 resulting respectively from the fixed bed hydrocracking steps d) in sections d-S1 and DS2 and i) hydrotreatment, the gas cuts 2, 8, 16, 20 resulting respectively from the atmospheric distillation steps a) ebullated bed hydroconversion, d) hydrocracking steps in sections d-S1 and d-S2 and an ethane cut 30, an LPG cut 31 and a paraffin-rich raffinate cut 32 resulting from the aromatics transformation and / or separation step g) are sent to a steam cracking step e) where each of the cuts is cracked under different conditions set out in the following table.
[0250] Table 11
[0251] The entirety of the pyrolysis oil cut 42 obtained in step e) is sent to the ebullated bed hydroconversion step c) because the total flow rate of the latter is less than 5% of the mass of the total charge of streams 42 and 7.
[0252] The following table shows the product yields from the different stages of the process according to example 1.
[0253] Table 12
[0254]
[0255] When the total is greater than 100% for a step, this means that a secondary charge has been injected into said step, such as, for example, hydrogen in steps c) and d).
[0256] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process.
[0257] Table 13
[0258] Compared to the feedstock introduced in atmospheric distillation step a), the process according to Example 1 achieves total mass yields of 80.1% of petrochemical base products. The olefin yields are: 19.2% ethylene, 13.8% propylene and 2.1% butadiene. The aromatic yields are 10.8% benzene and 33.2% paraxylene. In addition, the specific sequence of steps upstream of the steam cracking step limits coke formation.
[0259] Example 2: Method according to the embodiment of Figure 3 In this embodiment, a gas distillation step j) is added. This step will have as its load the gas cuts 2, 8, 16 and 20 from steps a), c) and d).
[0260] The details of the yields of this embodiment are shown in the following table.
[0261] Table 14
[0262]
[0263] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process for this embodiment.
[0264] Table 15
[0265] Example 3: Process according to the embodiment of Figure 4 with the isobutane isomerization step
[0266] In this embodiment, the crude oil feedstock of the process and the operating conditions of steps a) to j) are identical to example 2.
[0267] In this embodiment, a step k) of isomerization of isobutane is added. This step will have as feed, the propane cut 44 and the butane cuts 45 and 49 from the steps e) of steam cracking, for the butane cut 49 and j) of gas distillation, for the propane cut 44 and the butane cut 45. The stream rich in n-butane 47 and the stream containing hydrocarbons with 5 carbon atoms and more 48 are sent to the step e) of steam cracking.
[0268] Thus, cut 45 from gas distillation step j) and cut 49 from steam cracking step e) are sent to isobutane isomerization step k) under the conditions indicated in the following table. Table 16
[0269] The details of the yields of this embodiment are shown in the following table.
[0270] Table 17
[0271]
[0272]
[0273] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process for this embodiment.
[0274] Table 18
[0275] Compared to the feedstock introduced in atmospheric distillation step a), the process according to Example 3 achieves total mass yields of 78.3% of petrochemical base products. The olefin yields are: 22.7% ethylene, 13.9% propylene and 2.2% butadiene. The aromatic yields are 9.8% benzene and 29.8% paraxylene. The process according to Example 3 makes it possible to orient the process towards maximizing the ethylene yield. Example 4: Process according to the embodiment of Figure 5
[0276] In this embodiment, the crude oil feedstock of the process and the operating conditions of steps a) to c), as well as the fixed bed hydrocracking step d) in section d)-S1 are identical to example 1.
[0277] In this embodiment, the fixed bed hydrocracking step in section d-S2) is composed of a hydrotreatment reactor and a single hydrocracking reactor
[0278] A vacuum diesel cut 6 from vacuum distillation step b), the deasphalted oil cut 15, a vacuum diesel cut 11 from ebullated bed hydroconversion step c) and the heavy pyrolysis gasoline cut 41 from steam cracking step e) are thus sent to fixed bed hydrocracking step d) in a second section d-S2) whose operating conditions are presented in the following table.
[0279] Table 19
[0280] The heavy naphtha cut 22 from the hydrocracking step d) in section d-S2) is sent to a catalytic reforming step f). The light naphtha cuts 21, diesel cut 43 and unconverted oil cut 44, from the hydrocracking step d) in section d-S2) are sent to a steam cracking step e).
[0281] The following table shows the product yields from the different stages of the process according to example 4.
[0282] Table 20
[0283] When the total is greater than 100% for a step, this means that a secondary charge has been injected into said step, such as, for example, hydrogen in steps c) and d).
[0284] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process.
[0285] Table 21
[0286] Compared to the feedstock introduced in step a) of atmospheric distillation, the process according to Example 4 makes it possible to achieve total mass yields of 80.5% of basic products for petrochemicals. The olefin yields are: 21.7% ethylene, 14.5% propylene and 3.1% butadiene. The aromatic yields are 10.9% benzene and 30.4% paraxylene. The process according to Example 4 makes it possible to orient production towards a higher yield of olefins, in particular ethylene. Example 5: Process according to the embodiment of Figure 6, the point of this cut between light naphtha and heavy naphtha being at 65°C
[0287] In this embodiment, the crude oil feedstock of the process and the operating conditions of steps a) to h) are identical to example 1.
[0288] The cut-off point between light naphtha and heavy naphtha is 65°C.
[0289] In this embodiment, the stream of hydrotreated heavy naphtha 26 at the outlet of hydrotreatment step i) is sent to the steam cracking unit. This stream 26 with more than 65% paraffinic products is an interesting feedstock for steam cracking step e).
[0290] The hydrotreated heavy naphtha fraction 26 is thus sent to a steam cracking stage e) where it is cracked under the conditions set out in the following table.
[0291] Table 22
[0292] The details of the yields of this embodiment are shown in the following table.
[0293] Table 23
[0294]
[0295] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process for this embodiment.
[0296] Table 24
[0297] Compared to the feedstock introduced in step a) of atmospheric distillation, the process according to Example 5 makes it possible to achieve total mass yields of 80.3% of basic products for petrochemicals. The olefin yields are: 23.6% ethylene, 16.5% propylene and 3.0% butadiene. The aromatic yields are 10.7% benzene and 26.5% paraxylene. The process according to this embodiment makes it possible to orient the process towards the production of olefins. Example 6: Process according to the embodiment of Figure 6, the cutting point between light naphtha and heavy naphtha being at 101°C
[0298] In this embodiment, the crude oil feedstock of the process and the operating conditions of the different stages are identical to Example 5.
[0299] Only the cut point between light naphtha and heavy naphtha is changed: it is now 101 °C. This change in the cut point between light naphtha and heavy naphtha is applied to the hydrotreatment step i) of the naphtha cut obtained in step a), as well as to the diesel hydrocracking steps d-S1) and vacuum gas oil d-S2).
[0300] The details of the yields of this embodiment are shown in the following table.
[0301] Table 25
[0302]
[0303] The following table shows different yields in percentage by weight relative to the weight of the crude oil feedstock entering the process for this embodiment.
[0304] Table 26
[0305] Compared to the feedstock introduced in atmospheric distillation step a), the process according to Example 6 achieves total mass yields of 79.6% of petrochemical base products. The olefin yields are: 26.3% ethylene, 18.4% propylene and 4.1% butadiene. The aromatic yields are 7.1% benzene and 23.6% paraxylene. The process according to Example 6 allows the process to be oriented towards maximizing olefin yields.
Claims
CLAIMS 1. Process for the production of olefins and aromatics from a crude oil feedstock comprising the following steps: a) a step of atmospheric distillation of the crude oil feedstock and obtaining at least one naphtha cut, one diesel cut and one atmospheric residue cut; b) a step of vacuum distillation of the atmospheric residue cut obtained in step a) and obtaining at least one vacuum diesel cut and one vacuum residue cut; c) a step of ebullated bed hydroconversion of at least the vacuum residue cut obtained in step b), carried out in the presence of hydrogen and at least one hydroconversion catalyst, at a temperature of between 300 and 550°C, preferably between 400 and 460°C, under a total pressure of between 2 and 38 MPa, preferably between 10 and 25 MPa, at an hourly space velocity of between 0.05 and 10 h' 1 , preferably 0.1 and 0.2 h' 1and at a hydrogen partial pressure of between 5 and 30 MPa, preferably between 10 and 20 MPa, and obtaining at least one second naphtha cut, a second diesel cut and / or vacuum gas oil; d) a fixed-bed hydrocracking step of at least one diesel cut and / or vacuum gas oil chosen from the cuts obtained in steps a), b) and c) alone or as a mixture, carried out in the presence of hydrogen and at least one hydrocracking catalyst, at a temperature of between 250 and 480°C, preferably between 300 and 420°C under a pressure of between 2 and 25 MPa, at an hourly space velocity of between 0.3 and 6 h' 1 , preferably between 1 and 3 hours 1and at a hydrogen / hydrocarbon volume ratio of between 100 and 2000 L / L, and obtaining at least one light naphtha and / or heavy naphtha cut; e) a step of steam cracking at least one naphtha and / or light naphtha and / or heavy naphtha cut chosen from the cuts obtained in steps a), c) and d) alone or as a mixture, and obtaining at least one olefinic cut; f) a step of catalytic reforming of at least the heavy naphtha cut obtained in step d) and obtaining at least one reformate cut; g) a step of transformation and / or separation of the aromatics from at least the reformate cut obtained in step f) of catalytic reforming and obtaining at least one aromatic cut.
2. Process according to claim 1 in which, in step e) of steam cracking, a pyrolysis oil cut is also obtained.
3. Process according to claim 2 wherein, in step c) of ebullated bed hydroconversion, the vacuum residue cut obtained in step b) is converted together with all or part of the pyrolysis oil cut obtained in step e) of steam cracking.
4. Process according to any one of the preceding claims, in which, in step c) of hydroconversion in an ebullated bed, a hydroconversion residue cut is also obtained.
5. Method according to claim 4 further comprising a step h) of deasphalting the hydroconversion residue cut obtained in step c) in the presence of at least one solvent, and obtaining at least one deasphalted oil cut.
6. Process according to any one of the preceding claims in which, in step e) of steam cracking, a light and / or heavy pyrolysis gasoline cut is also obtained.
7. Process according to any one of claims 5 or 6 in which, fixed bed hydrocracking step d) further comprises fixed bed hydrocracking of the deasphalted oil cut obtained in deasphalting step h).
8. Process according to any one of claims 6 or 7, fixed bed hydrocracking step d) further comprises fixed bed hydrocracking of the heavy pyrolysis gasoline cut obtained in steam cracking step e).
9. Process according to any one of claims 7 or 8, in step d) of hydrocracking, the diesel cuts are cracked in a first hydrocracking section, and the vacuum diesel, deasphalted oil and heavy pyrolysis gasoline cuts are cracked in a second hydrocracking section.
10. Process according to any one of the preceding claims further comprising a step i) of hydrotreatment of the naphtha cut obtained in step a) and / or in step c), and obtaining at least one hydrotreated naphtha cut.
11. Process according to claim 10 in which step i) of hydrotreatment of the naphtha cut obtained in step a) and / or in step c) is followed by a step of separation and obtaining at least one hydrotreated light naphtha cut and / or hydrotreated heavy naphtha cut.
12. Process according to any one of claims 6 to 11 in which step g) of transformation and / or separation of the aromatics further comprises a transformation and / or separation of the aromatics from the light pyrolysis gasoline cut obtained in step e) of steam cracking, preferably jointly with the reformate cut.
13. Process according to any one of the preceding claims in which, in step g) of transformation and / or separation of the aromatics, a raffinate cut is also obtained.
14. Process according to claim 13 in which step e) of steam cracking further comprises steam cracking of the raffinate cut obtained in step g).
15. Method according to any one of the preceding claims further comprising a step j) of distillation of the gases of at least one gas cut chosen from the cuts obtained in steps a), c) and d) alone or as a mixture, and obtaining at least one LPG cut.
16. Method according to the preceding claim, in which said LPG cut is separated into at least one propane cut and one butane cut.
17. Method according to the preceding claim, further comprising a step k) of isomerization of the isobutane included in the butanes cut and obtaining at least one normal-butane cut.
18. Process according to the preceding claim, in which step e) of steam cracking further comprises the steam cracking of the normal-butane cut, obtained in step k).
Citation Information
Patent Citations
Conversion of heavy fuel oil to chemicals
US20190203130A1
System for conversion of crude oil to petrochemicals and fuel products integrating vacuum gas oil hydrotreating and steam cracking
US20210079305A1
Process and system for conversion of crude oil to petrochemicals and fuel products integrating steam cracking, fluid catalytic cracking, and conversion of naphtha into chemical rich reformate
US20180155642A1
Process for upgrading refinery heavy residues to petrochemicals
US20190062655A1
System for conversion of crude oil to petrochemicals and fuel products integrating vacuum gas oil hydrotreating and steam cracking
US20210207044A9
Cited By
Methods and systems for enhanced olefin production by hydrocracking heavy hydrocarbons
WO2026104095A1