METHOD FOR REDUCING OR REMOVING Si, Fe, AND Cu IN ALUMINUM ALLOY

By employing molten tin to exploit solubility differences, the method effectively separates and recovers pure aluminum from alloys, addressing the limitations of existing recycling techniques and improving the recyclability of aluminum scrap by removing impurities like Si, Fe, and Cu.

WO2024232295A1PCT designated stage expired Publication Date: 2024-11-14UNIVERSITY OF TOYAMA
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/016393
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-10
Filing Date
2024-04-26
Publication Date
2024-11-14

AI Technical Summary

Technical Problem

Current methods for recycling aluminum alloys, particularly wrought materials, face challenges due to narrow tolerance ranges for alloying elements like Si, Fe, and Cu, limiting the effectiveness of scrap recycling, while existing techniques such as induced current separation and molten salt electrolysis are not practical.

Method used

A method involving the use of molten tin (Sn) to selectively crystallize and separate Si, Fe, and Cu from aluminum alloys by controlling the melting and crystallization temperatures, leveraging the solubility differences between Al, Si, and Sn, and between Al and Fe/Cu, allowing for the recovery of pure Al and removal of impurities.

Benefits of technology

This method enhances the recyclability of aluminum scrap by effectively separating and recovering solid Al, reducing or removing Si, Fe, and Cu, with Sn being reusable, thereby improving the recycling process and reducing impurities in aluminum products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024016393_14112024_PF_FP_ABST
    Figure JP2024016393_14112024_PF_FP_ABST
Patent Text Reader

Abstract

[Problem] The purpose of the present invention is to provide a method for reducing or removing Si in an aluminum alloy, and reducing or removing Fe and Cu components is also possible. [Solution] This method for reducing or removing Si contained in an aluminum alloy is characterized by comprising: a step for holding the temperature at a melting temperature at which the aluminum alloy and Sn are melted; a step for lowering the temperature from the melting temperature, and holding the temperature at a Si crystallization temperature at which the solid Si is crystallized while maintaining a molten state of Sn and Al, thereby separating the solid Si; and a step for further lowering the temperature and holding the temperature at an Al crystallization temperature at which Al is crystallized but Sn is in a molten state, thereby separating and recovering the solid Al.
Need to check novelty before this filing date? Find Prior Art

Description

Method for reducing or removing Si, Fe, and Cu in aluminum alloys

[0001] The present invention relates to a method for reducing or removing alloy elements required for recycling aluminum materials.

[0002] Various alloying elements are added to aluminum alloys depending on their intended use, such as wrought or cast materials. Cast materials typically contain a relatively large amount of Si for reasons such as good fluidity during casting, a low thermal expansion coefficient, and improved wear resistance. For example, the ADC12 (JIS H 5302) alloy, used as a die-casting alloy, is specified as containing 9.6-12.0% Si. Cu, which has the effect of improving strength, is specified as containing 1.5-3.5% Cu. Although iron is likely to be mixed into the molten metal during scrap recycling, it also acts to prevent seizure on the mold, and ADC12 alloys are specified as containing 1.3% or less Fe. In either case, cast materials have a relatively wide tolerance range for added elements, resulting in a high recycling rate. In contrast, wrought materials have a narrow tolerance range for alloying elements, which is one of the factors that limit the recycling rate of scrap materials.

[0003] For example, Patent Document 1 describes a method for reducing the iron content of aluminum alloys by adding manganese to the molten metal, which crystallizes and removes the Fe as an Al-Fe-Mn-Si intermetallic compound. However, this separation of the intermetallic compound relies on an induced current difference that moves the metal in a non-uniform magnetic field, which is not practical.

[0004] Non-Patent Document 1 proposes a molten salt electrolysis method in which aluminum scrap is used as an anode in molten salt and electrolysis is performed in a solid state, in which only Al migrates to the cathode, but this is not necessarily practical.

[0005] Japanese Patent Publication No. 60-234930

[0006] Development of New Technology for Sustainable Recycling of Aluminum, Tohoku University Press Release, April 26, 2022. AJ McAlister and DJ Kahan: Bulletin of Alloy Phase Diagram, 4(1983), 410. RW Olesinski and GJ Abbaschian: Bulletin of Alloy Phase Diagram, 5(1984), 273. C. P. Wang, MS Wang, YL Deng, JB Zhang, SY Yang, YX Huang and XJ Liu: Journal of Phase Equilibria and Diffusions, 43 (2022), pp. 51-57. H.R. Kotadia, E. Doernberg, JB Patel, Z. Fan, and R. Schmid-Fetzer: Metallurgical and Materials Transactions A, 40A(2009), 2202-2211.

[0007] The present invention aims to provide a method for reducing or eliminating Si in an aluminum alloy, and furthermore, it is possible to reduce or eliminate Fe and Cu components.

[0008] The method for reducing or removing Si in an aluminum alloy according to the present invention is characterized by the steps of: maintaining the temperature at a melting temperature at which the aluminum alloy and Sn are molten; lowering the melting temperature and maintaining the temperature at a Si crystallization temperature at which solid Si crystallizes while maintaining the molten state of Sn and Al; and separating the solid Si; and further lowering the temperature and maintaining the temperature at a solid Al crystallization temperature at which Al crystallizes but Sn remains molten, thereby separating and recovering solid Al.

[0009] Based on the phase diagram of Al and Sn disclosed in Non-Patent Document 2 and the phase diagram of Si and Sn disclosed in Non-Patent Document 3, the solubility of Al and Si in Sn follows the curve shown in Figure 1. Therefore, although approximately 50 mass% of Al dissolves in molten Sn at 873 K, almost no Si dissolves. Furthermore, lowering the temperature of molten Sn to 573 K results in almost no Al dissolution. Focusing on this point, the present invention proposes that when an aluminum alloy and Sn are heated and maintained at 873 K or higher, both Al and Si dissolve, but when the molten metal temperature is lowered to around 873 K, Si crystallizes and can be separated as solid Si. Furthermore, when the molten metal temperature is lowered to around 573 K, Al crystallizes and can be separated and recovered as solid Al, which can be recycled. Furthermore, Sn can be reused.

[0010] The present invention can also reduce Fe after removing Si from the aluminum alloy, and includes a step of maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn melt; and a step of lowering the melting temperature to remove solid Si and / or Al while maintaining the molten state of Sn, Al, and Fe. 3 The method includes a step of maintaining the temperature at a Si crystallization temperature at which Fe crystallizes and separating solid Si, and further lowering the temperature to melt and maintain Fe in the molten Sn while separating Al and / or Al 3 In addition, when the aluminum alloy has a low Si content, a method for reducing or removing Fe contained in the aluminum alloy includes the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn melt; 3 Fe can be separated by crystallization.

[0011] The present invention can also reduce Cu after removing Si from the aluminum alloy, and includes a step of maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn are molten, and a step of lowering the melting temperature to remove solid Si and / or Al while maintaining the molten state of Sn, Al, and Cu. 2 The method includes a step of maintaining the temperature at a Si crystallization temperature at which Cu crystallizes and separating solid Si, and further lowering the temperature to melt and maintain Cu in the molten Sn while adding Al and / or Al 2Furthermore, when the aluminum alloy has a low Si content, a method for reducing or removing Cu contained in the aluminum alloy includes the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn melt; 2 Cu can be separated by crystallization.

[0012] The present invention utilizes the difference in solubility between Si and Al in molten Sn to separate and recover solid Al after separating solid Si, and since Sn can be reused, it is possible to reduce or remove Si from aluminum scrap material, improving recyclability. In addition, it is also possible to reduce Fe and Cu.

[0013] The figure shows the solubility curves of Al and Si in molten Sn using an Al-Si alloy. An explanatory diagram of the Si removal process in an aluminum alloy using molten Sn is shown. (a) shows the experimental furnace when an Al-Si alloy was used, and (b) shows the experimental conditions. A phase diagram of Sn, Al, and Si and experimental values ​​are shown. A projection of the Al-Si-Sn liquidus is shown. A partial enlargement of Figure 5 is shown. An explanatory diagram of the Fe removal process is shown. (a) shows the experimental furnace when an Al-Fe alloy was used, and (b) shows the experimental conditions. A graph plotting the amount of dissolved Al and the experimental values ​​of the Fe concentration in the Sn bath is shown. An explanatory diagram of the Cu removal process is shown.

[0014] The process of the present invention, which uses molten Sn to first remove Si and recover Al, will be described. The melting temperature at which aluminum alloy and Sn melt is a temperature above 873 K, e.g., a heating temperature of approximately 1000 K. In the molten Sn shown in FIG. 1 , approximately 50 mass% of Al dissolves near 873 K, but almost no Si dissolves, which can reach the crystallization temperature of solid Si. Alternatively, if the temperature is lowered to around 573 K, almost no Al dissolves, but Al crystallizes and separates, which can reach the Al crystallization temperature. The present invention utilizes this phenomenon.

[0015] This process is illustrated in Figure 2. (1) Sn and Al-Si alloy (scrap material) are placed in a furnace and heated to a temperature above 873K, for example, about 1000K, causing the entire material to melt. (2) The molten metal is gradually cooled and maintained at 873K, causing solid Si to crystallize and be separated and recovered. (3) The remainder is a molten metal of Sn and Al, which is gradually cooled to 573K, causing solid Al to crystallize and be separated and recovered. (4) The remaining molten Sn can be reused in the aluminum scrap recycling process.

[0016] This process was confirmed experimentally and will be explained based on Figure 3. As shown in the schematic diagram of Figure 3(a), 2 O 3 Sn and Al-Si alloys are placed in a furnace made of aluminum and heated. A carbon holder is used to keep the temperature. The alloy is heated to a temperature 10 to 200 K higher than 873 K. 2 O 3 The mixture was stirred and melted using a rod. Next, the temperature was maintained at 873 K while stirring. The Al-Si alloy used contained 12 mass% Si, and the melting was carried out in an Ar gas atmosphere as shown in Figure 3(b). Figure 4 shows a phase diagram of Sn, Al, and Si, on which the experimental values ​​for the amount of dissolved Al are plotted. Figure 5 shows a phase line projection of the Al-Si-Sn system, and Figure 6 shows the range in which Si crystallizes and Al dissolves in the molten Sn. As a result, it can be seen that the temperature range in which the Al-12% mass Si alloy melts in molten Sn is 573 K or higher and 1150 K or lower.

[0017] Next, from the phase diagram at 800°C and 1000°C shown in Non-Patent Document 4, Al and Al 3It can be seen that Al crystallizes preferentially when cooled below the eutectic point of Fe (1.8 mass% Fe). Based on this, the process of reducing or removing Fe is shown in Figure 7. After Si is crystallized at 873 K, Al and Fe are dissolved in the molten Sn when the Fe content is 1.8 mass% or less. Next, when cooled to 573 K, Fe remains in the molten Sn because the solubility of Fe in solid Al is very low. If this process is repeated, the Fe concentration in the molten Sn will increase, but Al 3 The aluminum is crystallized as an Fe compound, which allows the removal of Fe. Note that scrap material with a low Si content can also be directly held at 573K to remove the Fe from the aluminum.

[0018] This process was confirmed experimentally and will be described with reference to Figure 8. As shown in the schematic diagram of Figure 8(a), 2 O 3 Sn and Al-Fe alloys were placed in a furnace made of aluminum and heated. A carbon holder was used to keep the temperature. The alloys were heated to a temperature 10 to 200 K higher than 1273 K. 2 O 3 The mixture was stirred and dissolved using a rod. The temperature was then maintained at 873 K while stirring. The Al-Fe alloy used contained 10 mass% Fe, and the experiment was carried out in an Ar gas atmosphere, as shown in Figure 8(b). Figure 9 plots the experimental values ​​of the amount of dissolved Al and the Fe concentration in the Sn bath. The Fe concentration can be reduced when the Al content is higher than the initial concentration when the Al-10 mass% Fe alloy shown by the dashed line is introduced into the Sn bath, and when the Fe concentration is equal to or greater than the solubility, i.e., under the conditions of the shaded area in Figure 9.

[0019] Next, the range in which Cu remains in the molten Sn and Al precipitates can be determined by referring to the phase diagram described in Non-Patent Document 5. The Cu removal process based on this diagram is shown in Figure 10. When the temperature of the molten Sn is 573K, Al crystallizes out, but Cu dissolves in the molten Sn. By repeating this process, when the Cu concentration in the molten Sn reaches 3.8mss% or more, Al precipitates. 2It is clear that Cu can also be removed. In the case of Cu, if the Si content is low, the molten metal temperature can be maintained at 573 K, and Cu can be left on the Sn side to remove Cu from Al.

[0020] Molten Sn can be used to remove impurities such as Si, Fe, and Cu from aluminum alloys, making it possible to recycle aluminum scrap containing impurities into aluminum products with low impurity tolerance levels.

Claims

1. A method for reducing or removing Si contained in an aluminum alloy, comprising the steps of: holding the aluminum alloy at a melting temperature at which the aluminum alloy and Sn are melted; lowering the melting temperature and, while maintaining the molten state of Sn and Al, holding the temperature at a Si crystallization temperature at which solid Si crystallizes, and separating the solid Si; and further lowering the temperature and holding the temperature at the Al crystallization temperature at which Al crystallizes but Sn is in a molten state, to separate and recover solid Al.

2. A method for reducing or removing Si and Fe contained in an aluminum alloy, comprising the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn melt; and lowering the melting temperature to remove solid Si and / or Al while maintaining the molten state of Sn, Al, and Fe. 3 The temperature is kept at the Si crystallization temperature at which Fe crystallizes, and solid Si and / or Al 3 A step of separating Fe, further lowering the temperature and separating Al and / or Al while retaining Fe in the molten Sn. 3 A method for reducing or removing Si and Fe in an aluminum alloy, comprising crystallizing and separating Fe.

3. A method for reducing or removing Si and Cu contained in an aluminum alloy, comprising the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn melt; and lowering the melting temperature to remove solid Si and / or Al while maintaining the molten state of Sn, Al, and Cu. 2 The temperature is kept at the Si crystallization temperature at which Cu crystallizes, and solid Si and / or Al 2 A step of separating Cu, further lowering the temperature and separating Al and / or Al while keeping Cu molten in the molten Sn. 2 A method for reducing or removing Si and Cu in an aluminum alloy, comprising crystallizing and separating Cu.

4. A method for reducing or removing Fe contained in an aluminum alloy, comprising the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn are molten; lowering the melting temperature to melt and retain Fe in the molten Sn while removing Al and / or Al. 3 A method for reducing or removing Fe in an aluminum alloy, comprising separating Fe by crystallization.

5. A method for reducing or removing Cu contained in an aluminum alloy, comprising the steps of: maintaining the aluminum alloy at a melting temperature at which the aluminum alloy and Sn are molten; lowering the melting temperature, and melting and retaining Cu in the molten Sn while removing Al and / or Al. 2 A method for reducing or removing Cu in an aluminum alloy, comprising separating Cu by crystallization.

Citation Information

Patent Citations

  • Heat exchanger and method for manufacturing the same

    JP2014234930A

  • Device for extracting metal of waste circuit board in reverse blocking type high-voltage static classification mode

    CN115555133A

  • Methods of recovering and purifying secondary aluminum

    US20090084225A1

  • Crystallisation method for the purification of a molten metal, in particular recycled aluminium

    US20100024602A1

  • Process for the manufacture of aluminum

    US2198673A