Co2 fixation method, co2 fixation device, and method for recovering valuable metal
The method enhances CO2 fixation and valuable metal recovery by extracting alkaline earth metal ions from solid phases into a liquid phase using a slurry and pulverization process, addressing throughput and space challenges in existing technologies.
Patent Information
- Application Number
- PCT/JP2024/017287
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-30
- Filing Date
- 2024-05-09
- Publication Date
- 2024-12-05
AI Technical Summary
Current methods for CO2 fixation and valuable metal recovery face challenges such as low immobilization throughput, large equipment requirements, and limited installation space due to the difficulty in extracting alkaline earth metals from solid phases into liquid phases efficiently.
A method involving a slurry of alkaline earth metal-containing particles and an aqueous medium, where CO2 is used to extract alkaline earth metal ions into a liquid phase through stirring and mixing, followed by pulverization and separation to increase extraction efficiency, allowing for high-throughput extraction with reduced equipment area.
This approach enables efficient extraction of alkaline earth metals into a liquid phase with reduced equipment installation area and costs, effectively immobilizing CO2 while facilitating valuable metal recovery.
Smart Images

Figure JP2024017287_05122024_PF_FP_ABST
Abstract
Description
CO2 fixation method, CO2 fixation device, and valuable metal recovery method
[0001] The present disclosure provides 2 Immobilization method, CO 2 The present invention relates to an immobilization device and a valuable metal recovery method.
[0002] CO into the atmosphere 2 CO2 emissions reduction 2 One of the fixation technologies is to combine alkaline earth metals such as Mg and Ca contained in ores, steel slag, waste concrete, construction waste, coal ash, cement slag, industrial waste, etc. with CO emitted from factories, power plants, etc. 2 reacting with CO 2 Mineral carbonation, which involves immobilizing gases, is known.
[0003] Patent Document 1 (JP 2011-501726 A) describes "carbon dioxide (CO 2 ) as carbonates. 2 A method for fixing or binding a carbon black or a carbon black comprising the following steps: preparing an aqueous solution of water and coal ash or coal residue; 2 contacting a gas containing CO with the aqueous solution; and 2 reacting the aqueous solution with the CO 2 The method includes a step of fixing or binding the
[0004] Patent Document 2 (JP 2021-524805 A) describes an integrated process for the capture, sequestration and utilization of carbon dioxide, comprising the steps of: a) providing an aqueous slurry containing an aqueous liquid and a particulate solid containing an activated magnesium silicate mineral; b) dissolving the CO 2c) subjecting at least a portion of the magnesium-depleted solid residue from step b) to a particle size classification process to separate the magnesium-depleted solid residue into a fine particle size fraction and a coarse particle size fraction; d) subjecting at least a portion of the coarse particle size fraction from step c) to a particle size reduction process to provide a particle size reduced fraction; e) repeating step b) providing an aqueous slurry comprising the particle size reduced fraction from step d), wherein step e) does not include use of the fine particle size fraction from step c); and f) precipitating magnesium carbonate from the magnesium ions dissolved in steps b) and e) in a precipitation stage.
[0005] Patent Document 3 (WO 2013 / 131193) describes a method for sequestering carbon dioxide from a carbon dioxide-containing gas, the method comprising: contacting the carbon dioxide-containing gas with an aqueous slurry containing an alkaline earth metal-containing material in a carbonation unit for carbonating at least a portion of the alkaline earth metal to produce a carbon dioxide-depleted gas and a carbonate-containing slurry containing precipitable carbonates and substantially free of precipitated alkaline earth metal carbonates; removing the carbonate-containing slurry from the carbonation unit and separating the carbonate-containing slurry into an aqueous phase containing the precipitable carbonates and a solid phase; and supplying the aqueous phase to a precipitator in which alkaline earth metal carbonates are precipitated to produce a precipitated slurry.
[0006] Patent Document 4 (U.S. Pat. No. 1,085,021) describes a method for sequestering carbon dioxide and producing magnesium carbonate, the method comprising: thermally pretreating a magnesium-containing particulate material, wherein 90% of the solid particles have a particle size of about 75 μm or less, for dehydroxylation to produce a pretreated magnesium-containing particulate material; contacting the pretreated magnesium-containing particulate material with water and a carbon dioxide-containing gas to form a carrier slurry and a carbon dioxide-depleted gas; separating the carrier slurry from the carbon dioxide-depleted gas; separating the carrier slurry into at least a carrier aqueous stream and a solids-enriched stream; precipitating the carrier aqueous stream to form a precipitated slurry comprising a magnesium carbonate precipitate; and separating the precipitated slurry to produce a precipitated magnesium carbonate material and a precipitate-depleted stream.
[0007] JP 2011-501726 A JP 2021-524805 A International Publication No. 2013 / 131193 U.S. Patent No. 10,850,231
[0008] CO, which produces a weak acidic aqueous solution, can be used as an acid source to dissolve alkaline earth metals from solid materials such as ores. 2 When using CO 2 CO 3 ... 2 The immobilization requires a large amount of alkaline earth metal-containing solid as a source of alkaline earth metal. 2 This method has issues such as low immobilization throughput and the need for large or multi-tiered reaction vessels. When multiple reaction vessels are arranged in multiple tiers, the installation area becomes large, making it difficult to adopt such a layout in factories with limited installation space.
[0009] The present disclosure provides a CO extraction method that can efficiently extract alkaline earth metals from alkaline earth metal-containing solids into a liquid phase while reducing the installation area of equipment related to the extraction step, thereby reducing costs related to raw materials, equipment, operation, etc. 2 Immobilization method and CO 2 An immobilization device is provided.
[0010] The present inventors have discovered that a slurry containing alkaline earth metal-containing particles and an aqueous medium is mixed with CO in a stirring tank. 2 The inventors have found that alkaline earth metal ions can be extracted into the liquid phase from the alkaline earth metal-containing particles by stirring and mixing the alkaline earth metal source, supplying the slurry in the stirring tank to a grinding device to grind the alkaline earth metal-containing particles in the slurry, and then supplying the slurry containing the ground alkaline earth metal-containing particles back to the stirring tank, thereby enabling alkaline earth metal ions to be extracted into the liquid phase with high efficiency even when the installation area of the equipment related to the extraction step is small.
[0011] The present disclosure includes the following aspects: [Aspect 1] A slurry containing alkaline earth metal-containing particles and an aqueous medium is mixed in a stirring tank with CO 2 Gas, CO 2 CO selected from the group consisting of saturated water and combinations thereof 2 a source of alkaline earth metal-containing particles and a source of alkaline earth metal-containing particles to produce a mixture in which alkaline earth metal ions in the alkaline earth metal-containing particles are extracted into a liquid phase; extracting a slurry containing the alkaline earth metal-containing particles from the stirring tank and supplying it to a crushing device; crushing the alkaline earth metal-containing particles in the crushing device; supplying the crushed slurry containing the alkaline earth metal-containing particles to the stirring tank; subjecting the mixture extracted from the stirring tank to solid-liquid separation to obtain a liquid phase containing the alkaline earth metal ions and a solid phase containing an extraction residue; and precipitating an alkaline earth metal carbonate from the liquid phase containing the alkaline earth metal ions to extract CO in the alkaline earth metal carbonate. 2 and immobilizing CO 2 [Aspect 2] The CO immobilization method according to Aspect 1, further comprising: extracting the slurry containing the alkaline earth metal-containing particles from the stirring tank, separating the slurry containing the alkaline earth metal-containing particles into a light fraction and a heavy fraction in a classifier, and supplying the heavy fraction to the pulverizer. 2 [Aspect 3] The method according to aspect 2, comprising supplying a light fraction liquid phase obtained by solid-liquid separation of the light fraction to the stirring tank. [Aspect 4] The light fraction liquid phase is added with CO 2The method according to claim 3, further comprising: mixing the light fraction with the gas, and then supplying the light fraction liquid phase to the stirring tank. [Aspect 5] The method according to claim 3, further comprising: precipitating an alkaline earth metal carbonate from the light fraction liquid phase obtained by solid-liquid separation of the light fraction, and dissolving CO in the alkaline earth metal carbonate. 2 and supplying the liquid phase separated by the precipitation to the stirring tank. [Aspect 6] The method according to any one of Aspects 1 to 5, wherein the grinding device is a wet mill, an attrition pump, an electric pulse grinding device, an impulse grinding device, or a high-pressure jet nozzle grinding device. [Aspect 7] The method according to any one of Aspects 1 to 6, comprising supplying an alkaline earth metal-containing raw material to the grinding device. [Aspect 8] The method according to any one of Aspects 1 to 7, wherein the stirring and mixing in the stirring tank is performed under atmospheric pressure. [Aspect 9] The method according to any one of Aspects 1 to 7, wherein the CO 2 The method of any one of Aspects 1 to 8, comprising directly introducing a gas into the stirred tank. Aspect 10: The method of any one of Aspects 1 to 9, wherein the alkaline earth metal is magnesium. Aspect 11: The method of any one of Aspects 1 to 10, wherein the alkaline earth metal-containing particles comprise magnesium silicate. Aspect 12: CO 2 a CO pulverizer including: a stirring tank having a gas supply port, a first slurry supply port, and a first slurry discharge port; and a milling device having a second slurry supply port connected to the first slurry supply port of the stirring tank and a second slurry discharge port connected to the first slurry supply port of the stirring tank, the milling device being configured to pulverize the alkaline earth metal-containing particles in a slurry containing alkaline earth metal-containing particles and an aqueous medium, the slurry being extracted from the stirring tank through the first slurry discharge port and supplied through the second slurry supply port, and to discharge the pulverized slurry containing the alkaline earth metal-containing particles through the second slurry discharge port and supply it to the stirring tank through the first slurry supply port. 2 Immobilization device. [Aspect 13] The CO 213. The CO2 immobilization method according to claim 12, wherein the immobilization apparatus further includes a classification apparatus disposed between the first slurry outlet of the stirring tank and the second slurry supply inlet of the pulverization apparatus, the classification apparatus including a third slurry supply inlet, a light fraction discharge outlet, and a heavy fraction discharge outlet, the third slurry supply inlet being connected to the first slurry outlet of the stirring tank, and the heavy fraction discharge outlet being connected to the second slurry supply inlet of the pulverization apparatus. 2 Immobilization device. [Aspect 14] The CO 2 Aspect 14. The CO2 immobilization apparatus according to aspect 13, further comprising a solid-liquid separation device connected to the classification device and a precipitation tank connected to the solid-liquid separation device, wherein the solid-liquid separation device has a light fraction supply port, a first liquid phase outlet, and a first solid phase outlet, the precipitation tank has a liquid phase supply port, a second liquid phase outlet, and a second solid phase outlet, the light fraction supply port of the solid-liquid separation device is connected to the light fraction outlet of the classification device, and the first liquid phase outlet is connected to the liquid phase supply port of the precipitation tank, and the second liquid phase outlet of the precipitation tank is connected to the stirring tank. 2 Immobilization device. [Aspect 15] The CO 2 The immobilization device fixes the CO 2 15. The CO precipitation method according to claim 14, further comprising a gas-liquid mixer disposed between a gas inlet and the second liquid phase outlet of the deposition vessel. 2 [Aspect 16] The CO2 immobilization device according to any one of Aspects 12 to 15, wherein the pulverization device is a wet mill, an attrition pump, an electric pulse pulverization device, an impulse pulverization device, or a high-pressure jet nozzle pulverization device. 2 Aspect 17: A method for producing a CO2 immobilization apparatus according to any one of aspects 1 to 11, comprising pretreating an alkaline earth metal-containing raw material containing a valuable metal and an alkaline earth metal to obtain alkaline earth metal-containing particles and a valuable metal-containing residue, and preparing the slurry using the alkaline earth metal-containing particles. 2 and recovering a product, an intermediate, or both containing the valuable metal from the valuable metal-containing residue. 2A method for recovering valuable metals by immobilizing alkaline earth metal particles in a CO solution according to any one of Aspects 1 to 11. [Aspect 18] A method for recovering valuable metals by immobilizing alkaline earth metal particles in a CO solution according to any one of Aspects 1 to 11. 2 carrying out an immobilization method; and using the solid phase containing the extraction residue as a valuable metal-containing residue, and recovering a valuable metal-containing product, intermediate, or both from the valuable metal-containing residue. 2 A method of immobilizing the waste and recovering valuable metals.
[0012] According to the present disclosure, alkaline earth metals can be extracted from alkaline earth metal-containing particles into a liquid phase with high efficiency while reducing the installation area of equipment related to the extraction process, thereby reducing costs related to raw materials, equipment, operations, etc.
[0013] It should be noted that the above description should not be considered as disclosing all the embodiments of the present invention and all the advantages associated with the present invention.
[0014] CO of the first embodiment 2 FIG. 1 is a flow chart illustrating an outline of a fixation method. 2 FIG. 10 is a flow chart illustrating an outline of the immobilization method of the third embodiment. 2 FIG. 1 is a flow chart illustrating an outline of the immobilization method. 2 Schematic diagram of the immobilization device. 2 1 is a flow chart illustrating an outline of a valuable metal recovery method according to a first embodiment, in combination with an immobilization method. 2 1 is a flow chart illustrating an overview of a valuable metal recovery method according to a second embodiment, which is combined with an immobilization method; 2 FIG. 1 is a top view of an exemplary equipment layout for the extraction process of the immobilization equipment. 2 FIG. 10 is a top view of an exemplary apparatus layout for the extraction process of the immobilization apparatus.
[0015] Hereinafter, the present invention will be described in more detail with reference to the drawings for the purpose of illustrating typical embodiments thereof, but the present invention is not limited to these embodiments.
[0016] [CO 2 Immobilization method - First embodiment] CO of the first embodiment 2 The immobilization method is as follows: (1) In a stirring tank, a slurry containing alkaline earth metal-containing particles and an aqueous medium and CO 2 Gas, CO 2 CO selected from the group consisting of saturated water and combinations thereof 2 (2) extracting a slurry containing alkaline earth metal-containing particles from the stirring tank and supplying it to a crushing device; (3) crushing the alkaline earth metal-containing particles in the crushing device; (4) supplying the crushed slurry containing alkaline earth metal-containing particles to the stirring tank; (5) subjecting the mixture extracted from the stirring tank to solid-liquid separation to obtain a liquid phase containing alkaline earth metal ions and a solid phase containing extraction residue; and (6) precipitating an alkaline earth metal carbonate from the liquid phase containing alkaline earth metal ions to extract CO in the alkaline earth metal carbonate. 2 This includes immobilizing the
[0017] FIG. 1 shows the CO 2 An outline of the immobilization method is shown in a flow diagram. In the flow diagram of the present disclosure, the parts enclosed in a square indicate steps or devices. In FIG. 1, as an optional step, alkaline earth metal-containing particles are obtained by pretreating the alkaline earth metal-containing raw material. An aqueous medium is added to the alkaline earth metal-containing particles to obtain a slurry. CO is added to the slurry in a stirring tank while stirring. 2By mixing the alkaline earth metal-containing particles with the source, a mixture is produced in which alkaline earth metal ions from the alkaline earth metal-containing particles are extracted into a liquid phase. The slurry containing the alkaline earth metal-containing particles is extracted from the stirring tank and fed to a crushing device. The alkaline earth metal-containing particles are crushed in the crushing device, and the slurry is then fed back to the stirring tank. The crushing increases the contact interface area between the alkaline earth metal-containing particles and the liquid phase, or refreshes the reaction surface of the alkaline earth metal-containing particles. As a result, the extraction efficiency of the alkaline earth metal can be improved. In this embodiment, the extraction step and the crushing step are performed in separate devices (stirring tank and crushing device), thereby reducing the installation area of the equipment related to the extraction step and enabling highly efficient extraction of the alkaline earth metal from the alkaline earth metal-containing particles into the liquid phase. Thereafter, the mixture in which the alkaline earth metal ions have been extracted into the liquid phase is subjected to solid-liquid separation to obtain a liquid phase containing the alkaline earth metal ions and a solid phase containing the extraction residue. The alkaline earth metal carbonate is precipitated from the liquid phase, and CO is released into the alkaline earth metal carbonate. 2 is fixed.
[0018] (1) Extraction step: A slurry containing alkaline earth metal-containing particles and an aqueous medium is mixed with CO 2 Gas, CO 2 CO selected from the group consisting of saturated water and combinations thereof 2 By stirring and mixing the alkaline earth metal ions in the alkaline earth metal-containing particles, the alkaline earth metal ions are extracted into the liquid phase.
[0019] The alkaline earth metal-containing particles are not particularly limited as long as they contain an alkaline earth metal. In the present disclosure, "alkaline earth metal" refers to an element of Group 2 of the periodic table. The alkaline earth metal is preferably at least one selected from the group consisting of Mg, Ca, Sr, and Ba, more preferably at least one selected from the group consisting of Mg and Ca, even more preferably containing Mg, and particularly preferably Mg.
[0020] Examples of alkaline earth metal-containing particles include particles of Mg-containing ore, Mg-containing slag, Ca-containing slag, coal ash, clinker kiln dust, waste concrete, concrete sludge, and cement.
[0021] In one embodiment, the alkaline earth metal-containing particles are particles of an Mg-containing ore. Examples of Mg-containing ores include limonite (MgO content: 0.5 to 5% by mass), smectite (MgO content: 5 to 15% by mass), and saprolite (MgO content: 15 to 35% by mass). The Mg-containing ore preferably includes ultramafic rock, and is particularly preferably olivine (composition formula: (Mg, Fe)SiO 4 ) and serpentine (composition formula: (Mg, Fe) 3 Si 2 O 5 (OH) 4 Since olivine and serpentine are high Mg-containing minerals, CO 2 The amount of alkaline earth metal-containing particles required for immobilization can be reduced.
[0022] The alkaline earth metal-containing particles preferably contain magnesium silicate. Olivine, serpentine, and other ores, which are relatively easy to obtain, contain a large amount of Mg in the form of magnesium silicate. Therefore, alkaline earth metal-containing particles containing magnesium silicate are preferable for CO 2 This is advantageous in that immobilization can be carried out more cheaply and easily.
[0023] The alkaline earth metal-containing particles may be formed by pretreating an alkaline earth metal-containing raw material, which may be a material described with respect to the alkaline earth metal-containing particles, such as Mg-containing ore, Mg-containing slag, Ca-containing slag, coal ash, clinker kiln dust, waste concrete, concrete sludge, or cement.
[0024] Pretreatments include, for example, grinding and heat treatment.
[0025] The pulverization can be carried out using a known pulverization device. The pulverization can reduce the average particle size of the alkaline earth metal-containing particles to increase their surface area, or expose the active surface of the alkaline earth metal-containing particles. This can improve the extraction efficiency of the alkaline earth metal. The pulverization can be carried out under conditions that allow the alkaline earth metal-containing particles to have a suitable average particle size, as described below. If necessary, the pulverized alkaline earth metal-containing particles may be classified using a classification device such as a sieve.
[0026] The heat treatment can be carried out using a known heat treatment device. The heat treatment temperature can be, for example, 500°C to 800°C, and the heat treatment time can be 1 minute to 2 hours. The alkaline earth metal-containing particles are preferably heat-treated. By heat-treating the alkaline earth metal-containing raw material, the crystal water in the alkaline earth metal-containing raw material can be removed, and the alkaline earth metal in the alkaline earth metal-containing particles can be activated to a form that is easily eluted into a liquid phase, thereby increasing the extraction efficiency of the alkaline earth metal. The smaller the particle size, the easier it is for heat to be transmitted to the inside of the particle, and the more efficient the heat treatment, so it is preferable to carry out the heat treatment after the above-mentioned pulverization.
[0027] An example of a heat treatment device is a microwave heating device. The microwave heating device can heat the alkaline-earth metal-containing raw material from the inside using electrical energy, thereby reducing the amount of unactivated parts in the alkaline-earth metal-containing raw material.
[0028] In the present disclosure, devices used for pretreatment, such as a pulverizer and a heat treatment device, are collectively referred to as a pretreatment device.
[0029] The average particle size of the alkaline earth metal-containing particles is not particularly limited and can be appropriately determined depending on the volume of the stirring tank, the type and output of the agitator provided in the stirring tank, the type and size of the grinding device, etc. The average particle size of the alkaline earth metal-containing particles can be, for example, within the range of 10 μm to 500 μm, 20 μm to 450 μm, or 100 μm to 400 μm. By setting the average particle size of the alkaline earth metal-containing particles to 10 μm or more, CO 2By setting the average particle size of the alkaline earth metal-containing particles to 500 μm or less, the extraction efficiency of the alkaline earth metal can be improved without excessively increasing the power consumption required for stirring in the extraction step. In the present disclosure, the average particle size of the alkaline earth metal-containing particles is determined by the 50% cumulative volume average diameter D 50 is defined as:
[0030] The aqueous medium is CO 2 The aqueous medium has the ability to dissolve the above-mentioned compounds, and is generally water. In addition to water, the aqueous medium may contain a water-soluble organic solvent such as an alcohol or an ester, as necessary. The aqueous medium may also contain salts such as sodium chloride, potassium chloride, ammonium chloride, sodium sulfate, magnesium sulfate, ammonium hydrogen sulfate, and sodium hydrogen carbonate dissolved therein. The water content in the aqueous medium is preferably 70% by mass or more, more preferably 80% by mass or more, and even more preferably 90% by mass or more.
[0031] The slurry can be prepared by adding alkaline earth metal-containing particles to an aqueous medium and mixing them. In one embodiment, the slurry supplied as a raw material contains 0.5% to 50% by mass of alkaline earth metal-containing particles. The lower the content of alkaline earth metal-containing particles in the slurry, the greater the ratio of the liquid phase to the solid phase (alkaline earth metal-containing particles), thereby increasing the extraction rate of the alkaline earth metals, but requiring larger equipment for extraction. On the other hand, the higher the content of alkaline earth metal-containing particles in the slurry, the smaller the extraction equipment required, but the lower the extraction efficiency of the alkaline earth metals. By setting the content of alkaline earth metal-containing particles in the raw material slurry to 0.5% by mass or more, it is possible to suppress an increase in equipment costs related to the extraction of alkaline earth metals. By setting the content of alkaline earth metal-containing particles in the raw material slurry to 50% by mass or less, it is possible to increase the extraction efficiency of the alkaline earth metals. In one embodiment, the slurry is prepared by CO 2 Contains no externally added acid other than the source.
[0032] CO 2 The source is CO 2 Gas, CO 2In other words, in the extraction step, (1) CO 2 Only CO gas is introduced into the stirred tank. 2 Only saturated water is introduced into the stirred tank; (3) CO 2 Gas and CO 2 In either case, saturated water and / or water may be introduced into the stirring tank.
[0033] CO 2 The gas supply source may be, for example, at least one selected from the group consisting of a coal-fired power plant, an oil-fired power plant, a natural gas power plant, a biomass power plant, a coal-fired boiler, a smelting facility, a neutralization facility, and a roasting facility. 2 The amount of gas emissions is particularly large, so CO 2 By using the immobilization method, CO 2 It can effectively reduce gas emissions. 2 The roasting equipment serving as the gas supply source may be the same as that used in the roasting step described below. 2 The gas may be introduced directly into the stirring vessel, or CO 2 may be introduced into the water or aqueous medium by bubbling or the like. 2 The gas may be mixed and then introduced into the stirring vessel, or a combination of direct introduction and mixed introduction may be used. 2 It is preferable that the CO 2 is produced in another step of the immobilization method, for example, a light liquid phase produced in the classification step described below, or a liquid phase produced in the precipitation step. 2 The amount of water used in the immobilization method can be reduced.
[0034] CO 2 The source of saturated water is not particularly limited, but for example, CO 2 using an amine or a solid adsorbent. 2 CO from exhaust gas 2 CO recovery systems. 2 In the recovery system, CO contained in the exhaust gas is 2 CO dissolved to a saturated concentration 2 Since contained water is produced, this CO 2 The water containing CO 2 In this disclosure, "CO2 "Saturated water" refers to water that is saturated with dissolved CO at the time of supply to the mixing tank. 2 Concentration (g / 100cm 3 ) is CO 2 Solubility in water (g / 100 cm 3 ) is 90% or more, preferably 95% or more, more preferably 98% or more 2 It means that the water contained in the 2 Contains water.
[0035] CO 2 The feed rate of the CO 2 The extraction efficiency can be optimized by taking into consideration design factors such as the saturated solubility of CO, the extraction efficiency, the power required for supply, the volume of the stirring tank, and the output of the stirrer provided in the stirring tank. 2 The feed rate of the source is determined by the CO 2 It is preferable to determine the amount of the compound dissolved so that it becomes saturated at the temperature and pressure during stirring.
[0036] Slurry and CO 2 By stirring and mixing the alkaline earth metal ions in the alkaline earth metal-containing particles in the stirred tank, the alkaline earth metal ions are extracted into the liquid phase. 2 dissolves in the liquid phase of the slurry, lowering the pH of the liquid phase. This promotes dissolution and ionization of the alkaline earth metal in the alkaline earth metal-containing particles into the liquid phase. The stirring tank may be a tank equipped with a stirring device having a stirring blade and a motor. The stirring tank may be equipped with a temperature control mechanism or may be a sealed container equipped with a mechanism for pressurizing the internal atmosphere.
[0037] In one embodiment, the stirring and mixing is performed at a temperature above the freezing point and below the boiling point of the aqueous medium. When the slurry contains a soluble substance, such as sodium chloride, the freezing point of the aqueous medium may drop below 0°C. By performing the stirring and mixing at a temperature above the freezing point of the aqueous medium, the stirring can be performed uniformly and an excessive increase in power consumption due to the stirring and mixing can be prevented. By performing the stirring and mixing at a temperature below the boiling point, the evaporation of the aqueous medium can be suppressed and the CO dissolved in the aqueous medium can be reduced. 2 The concentration can be controlled within a desired range.
[0038] In one embodiment, stirring and mixing is carried out under a pressure atmosphere of atmospheric pressure or higher and 10 MPaG (gauge pressure) or lower, preferably 1.0 MPaG (gauge pressure) or lower, and more preferably 0.5 MPaG (gauge pressure) or lower. 2 The higher the pressure, the more CO 2 is dissolved in the liquid phase of the slurry, thereby increasing the extraction efficiency of the alkaline earth metal. In the present disclosure, alkaline earth metal ions in alkaline earth metal-containing particles can be efficiently extracted into the liquid phase even under a low-pressure atmosphere of 10 MPaG (gauge pressure) or less, particularly atmospheric pressure to 1.0 MPaG (gauge pressure). By using low-pressure conditions, special equipment such as a pressure-resistant reaction vessel, a booster pump, or a gas compressor is not required, and the power consumption related to the extraction of alkaline earth metal ions can be effectively reduced. In one embodiment, stirring is performed under atmospheric pressure.
[0039] The stirring time of the slurry can be appropriately set depending on the extraction efficiency, and is not particularly limited, but can be, for example, 20 minutes to 2 hours.
[0040] The alkaline earth metal ions extracted into the liquid phase may be present in the form of alkaline earth metal hydroxide, alkaline earth metal silicate, or alkaline earth metal silicate double salt. Examples of alkaline earth metal hydroxides include Mg(OH) produced by hydration of MgO or CaO. 2 and Ca(OH) 2 Examples of alkaline earth metal silicates include Mg 2 SiO 4 (Magnesium silicate) and Ca 2 SiO 4 Examples of alkaline earth metal silicate double salts include silicates of alkaline earth metals and alkali metals, Mn, Fe, Co, Ni, Cu, Zn, or Al, or two or more of these. A typical alkaline earth metal silicate double salt is (Mg,Fe)SiO 4 (mafic silicate).
[0041] In one embodiment, the alkaline earth metal ions are present in the form of an alkaline earth metal silicate or a double alkaline earth metal silicate.
[0042] These alkaline earth metal hydroxides, alkaline earth metal silicates, and alkaline earth metal silicate double salts are 2 Upon immobilization, the metal is converted to an alkaline earth metal carbonate or alkaline earth metal bicarbonate. Without being bound by any theory, alkaline earth metal bicarbonate (e.g., magnesium bicarbonate: Mg(HCO 3 ) 2 ) exists only in the liquid phase, and after precipitation, alkaline earth metal carbonate hydrates (e.g., magnesium carbonate hydrate: Mg—CO 2 -H 2 It is believed that the SiO2 is converted into the form of a SiO2-based precipitate.
[0043] (2) Step of feeding to a pulverizer After stirring the slurry, the slurry containing the alkaline earth metal-containing particles is extracted from the stirring tank and fed to a pulverizer. 2 After being mixed with the source, the slurry fed to the milling device also contains ions of alkaline earth metals in the liquid phase.
[0044] (3) Pulverization Step The alkaline earth metal-containing particles contained in the slurry are pulverized in a pulverizer. The pulverizer preferably includes a wet mill, an attrition pump, an electric pulse pulverizer, an impulse pulverizer, or a high-pressure jet nozzle pulverizer. The electric pulse pulverizer or impulse pulverizer can also pulverize the grain boundary interface of the alkaline earth metal-containing particles, which is advantageous in terms of increasing extraction efficiency.
[0045] The grinding time can be appropriately set depending on the type and size of the grinding device, and is not particularly limited, but can be, for example, 2 to 30 minutes.
[0046] As shown by the dotted arrow in Figure 1, the alkaline earth metal-containing raw material may be supplied to a grinding device. This allows the preparation of new slurry containing alkaline earth metal-containing particles in parallel with the grinding of the alkaline earth metal-containing particles contained in the slurry extracted from the stirring tank in the grinding device, and the grinding device in the pretreatment can be omitted. The alkaline earth metal-containing raw material may be subjected to the pretreatment described above, for example, grinding or heat treatment.
[0047] (4) Supplying step to a stirring tank The slurry containing the pulverized alkaline earth metal-containing particles is supplied to a stirring tank, where the extraction step is then carried out again.
[0048] Steps (1) to (4) may be performed continuously or sequentially. When steps (1) to (4) are performed sequentially, they may be performed on the entire amount of the slurry, or the slurry may be divided into two or more portions. When steps (1) to (4) are performed sequentially, a set of steps (1) to (4) may be performed once, or a set of steps (1) to (4) may be repeated multiple times. In one embodiment, steps (1) to (4) are performed continuously, i.e., the extraction step and the grinding step are performed in parallel.
[0049] (5) Solid-liquid separation step The mixture in which alkaline earth metal ions have been extracted into the liquid phase is subjected to solid-liquid separation to produce a liquid phase containing alkaline earth metal ions and a solid phase containing extraction residue. The solid phase of the mixture may contain alkaline earth metal-containing particles as residue. Examples of solid-liquid separation methods include filtration, pressing, sedimentation, and centrifugation.
[0050] Solid-liquid separation can be carried out using a common solid-liquid separator, such as a vacuum separator, a centrifugal separator, a multi-disk separator, a belt press, a screw press, a roller press, a rotary drum screen, a belt screen, a vibrating screen, a thickener, a ceramic filter, a pleated filter, or a multi-plate wave filter.
[0051] (6) Precipitation step: By precipitating alkaline earth metal carbonate from a liquid phase containing alkaline earth metal ions, CO is added to the alkaline earth metal carbonate. 2 The solubility of alkaline earth metal carbonates decreases with increasing temperature. Therefore, the precipitation of alkaline earth metal carbonates can be promoted by increasing the temperature of the liquid phase. The precipitation of alkaline earth metal carbonates can also be achieved by bubbling air through the liquid phase or by placing the liquid phase under reduced pressure.
[0052] The deposition tank may be a tank equipped with a temperature control mechanism, and may be equipped with a pipe and a nozzle for air bubbling, or a vacuum pump.
[0053] The temperature of the liquid phase in the precipitation step can be, for example, 0° C. to 80° C., or 20° C. to 80° C. The precipitation time can be, for example, 10 minutes to 5 hours.
[0054] In the precipitation step, the precipitated alkaline earth metal salt may be separated from the liquid phase.
[0055] [CO 2 Immobilization method - Second embodiment] CO of the second embodiment 2 The immobilization method includes, in step (2), extracting a slurry containing alkaline earth metal-containing particles from the stirring tank, separating the slurry containing alkaline earth metal-containing particles into a light fraction and a heavy fraction in a classification device, and supplying the heavy fraction to a grinding device.
[0056] FIG. 2 shows the CO 2 An outline of the immobilization method is shown in a flow diagram. In FIG. 2, a slurry containing alkaline earth metal-containing particles extracted from an agitation tank is separated into a light fraction and a heavy fraction in a classification device. Particles contained in the heavy fraction contain a relatively large amount of alkaline earth metal, and contain, for example, magnesium silicate as a component. The heavy fraction is supplied to a grinding device, ground in the grinding device, and then fed back to the agitation tank, where step (1) is performed. In this way, by separating the heavy fraction from the light fraction and grinding the heavy fraction and feeding it to the agitation tank, the processing efficiency of the grinding device can be improved. Furthermore, since only the heavy fraction containing a relatively large amount of alkaline earth metal is sent to the extraction step, the extraction efficiency of alkaline earth metals in the agitation tank can also be improved.
[0057] The content of alkaline earth metals in the particles contained in the light fraction is smaller than that in the particles contained in the heavy fraction. The particles contained in the light fraction contain, for example, silicon dioxide (SiO 2On the other hand, since the liquid phase of the light fraction contains alkaline earth metal ions, it is preferable to supply the liquid phase of the light fraction obtained by solid-liquid separation of the light fraction to the stirring tank. This allows the alkaline earth metals contained in the alkaline earth metal-containing raw material to be more effectively removed by CO 2 The light solid phase containing particles is sent to a valuable metal recovery facility if it contains valuable metals, or to post-processing such as residue treatment if it does not contain valuable metals.
[0058] CO in the light liquid phase 2 After mixing with the gas, it is preferable to supply the light fraction liquid phase to the stirring tank. 2 By mixing the gas, the dissolved CO in the slurry in the agitation tank, which may be generated when the light liquid phase is supplied to the agitation tank, is reduced. 2 The CO concentration fluctuation can be suppressed, and the extraction process can be stably carried out. 2 The gas mixture may be, for example, by adding CO 2 Insert the gas introduction nozzle and CO 2 The gas is bubbled into the light liquid phase, or an in-line mixer is installed in the middle of the piping and CO is introduced into the in-line mixer. 2 This can be done by supplying a gas.
[0059] [CO 2 Immobilization method - Third embodiment] CO of the third embodiment 2 In the step (2), the immobilization method comprises extracting a slurry containing alkaline earth metal-containing particles from the stirring tank, separating the slurry containing alkaline earth metal-containing particles into a light fraction and a heavy fraction in a classifier, separating the light fraction into a solid-liquid phase, precipitating alkaline earth metal carbonate from the light fraction liquid phase, and dissolving CO in the alkaline earth metal carbonate. 2 and feeding the liquid phase separated by precipitation into a stirred tank.
[0060] FIG. 3 shows the CO 2The outline of the immobilization method is shown in a flow diagram. In Fig. 3, the light fraction separated in the classification device is separated into a light fraction liquid phase and a light fraction solid phase by solid-liquid separation in step (5). Then, in step (6), alkaline earth metal carbonate is precipitated from the light fraction liquid phase containing alkaline earth metal ions, thereby obtaining CO 2 The liquid phase separated by precipitation is supplied to the stirring tank. According to this embodiment, by sending the light fraction liquid phase to the downstream step (5), the concentration of alkaline earth metal ions in the slurry in the stirring tank is prevented from becoming excessively high, thereby increasing the extraction efficiency in the stirring tank and reducing CO 2 This effect is particularly remarkable when a large amount of alkaline earth metal ions are dissolved in the light fraction liquid phase. In addition, by supplying the liquid phase separated by precipitation to a stirring tank, the CO 2 The amount of water used in the immobilization method can be reduced.
[0061] The liquid phase separated by precipitation contains CO 2 After mixing with the gas, it is preferable to supply the liquid phase to a stirring tank. 2 By mixing the gas, the dissolved CO in the slurry in the agitation tank, which may be generated when the liquid phase is supplied to the agitation tank, is reduced. 2 The CO concentration fluctuation can be suppressed, and the extraction process can be stably carried out. 2 The gas mixture may be, for example, by adding CO 2 Insert the gas introduction nozzle and CO 2 The gas is bubbled into the liquid phase, or an in-line mixer is installed in the middle of the piping, and CO 2 This can be done by supplying a gas.
[0062] The second and third embodiments are combined to produce CO 2For example, when the concentration of alkaline earth metal ions in the light fraction liquid phase obtained by classifying a slurry containing alkaline earth metal-containing particles is less than a predetermined value, the light fraction liquid phase after solid-liquid separation is supplied to a stirring tank, i.e., step (1) (extraction step), and when the concentration is equal to or greater than a predetermined value, the light fraction liquid phase after solid-liquid separation is sent to step (6) (precipitation step), thereby improving the extraction efficiency in the stirring tank and the CO 2 The throughput of immobilization can be further increased.
[0063] [CO 2 Immobilization Device] 2 The immobilization device is 2 The present invention includes a stirring tank having a gas supply port, a first slurry supply port, and a first slurry discharge port, and a milling device having a second slurry supply port connected to the first slurry supply port of the stirring tank and a second slurry discharge port connected to the first slurry supply port of the stirring tank. The milling device is configured to mill alkaline earth metal-containing particles in a slurry containing alkaline earth metal-containing particles and an aqueous medium, the slurry being extracted from the stirring tank through the first slurry discharge port and supplied through the second slurry supply port, and to discharge the slurry containing the milled alkaline earth metal-containing particles through the second slurry discharge port and supply it to the stirring tank through the first slurry supply port.
[0064] FIG. 4 shows an embodiment of the CO 2 A schematic diagram of the immobilization device is shown. 2 In the immobilization apparatus 1, the stirring tank 10 contains CO 2 The tank 10 is provided with a gas supply port 11, a first slurry supply port 12, and a first slurry discharge port 13. The tank 10 is provided with a stirring device having a stirring blade and a motor M. 2 The piping for introducing the CO 2 The gas supply port 11 extends below the surface of the slurry, and CO is supplied from a nozzle provided at the end or midway of the pipe. 2 The CO source is introduced into the slurry. 2 The alkaline earth metal ions in the alkaline earth metal-containing particles are extracted into the liquid phase of the slurry by stirring and mixing with the source.
[0065] The pulverizer 20 includes a second slurry supply port 22 and a second slurry discharge port 23. The second slurry supply port 22 is connected to the first slurry discharge port 13 of the stirring tank 10 via a pump. The second slurry discharge port 23 is connected to the first slurry supply port 12 of the stirring tank 10 via a pump. The slurry in the stirring tank 10 is extracted through the first slurry discharge port 13 and supplied to the pulverizer 20 through the second slurry supply port 22. The alkaline earth metal-containing particles in the slurry are pulverized in the pulverizer 20. The slurry containing the pulverized alkaline earth metal-containing particles is discharged through the second slurry discharge port 23 and supplied to the stirring tank 10 through the first slurry supply port 12. The pulverizer 20 is preferably a wet mill, an attrition pump, an electric pulse crusher, an impulse crusher, or a high-pressure jet nozzle crusher, and more preferably an electric pulse crusher or an impulse crusher.
[0066] 4 further shows a classifier 30 disposed between the first slurry outlet 13 of the stirring tank 10 and the second slurry supply inlet 22 of the milling device 20. The classifier 30 includes a third slurry supply inlet 32, a light fraction outlet 34, and a heavy fraction outlet 33. The third slurry supply inlet 32 is connected to the first slurry outlet 13 of the stirring tank 10. The heavy fraction outlet 33 is connected to the second slurry supply inlet 22 of the milling device 20. In the classifier 30, the slurry is separated into a light fraction and a heavy fraction. The heavy fraction is supplied to the milling device 20, milled in the milling device 20, and then supplied back to the stirring tank 10. The classifier 30 is, for example, a liquid cyclone, a vibrating screen, or a centrifugal separator.
[0067] FIG. 4 further shows a solid-liquid separator 40 connected to the classifier 30 , and a precipitation tank 50 connected to the solid-liquid separator 40 .
[0068] The solid-liquid separator 40 includes a light fraction supply port 42, a first liquid phase outlet 43, and a first solid phase outlet 44. The light fraction supply port 42 of the solid-liquid separator 40 is connected to the light fraction outlet 34 of the classifier 30, and the light fraction is supplied from the classifier 30 to the solid-liquid separator 40. The light fraction is separated into a light fraction liquid phase and a light fraction solid phase in the solid-liquid separator 40, and the light fraction solid phase is discharged from the first solid phase outlet 44. The solid-liquid separator 40 may be, for example, a vacuum separator, a centrifugal separator, a multiple disk separator, a belt press, a screw press, a roller press, a rotary drum screen, a belt screen, a vibrating screen, a thickener, a ceramic filter, a pleated filter, or a multiple plate wave filter.
[0069] The precipitation tank 50 is equipped with a liquid phase supply port 52, a second liquid phase outlet 53, and a second solid phase outlet 54. The first liquid phase outlet 43 of the solid-liquid separation device 40 is connected to the liquid phase supply port 52 of the precipitation tank 50, and the light fraction liquid phase separated in the solid-liquid separation device 40 is supplied to the precipitation tank 50 through the first liquid phase outlet 43 and the liquid phase supply port 52. The precipitation tank 50 is equipped with a temperature control mechanism, and alkaline earth metal carbonates are precipitated from the light fraction liquid phase by raising the temperature of the liquid phase. The alkaline earth metal carbonates are recovered from the second solid phase outlet 54. The precipitation tank 50 may be equipped with an air bubbling mechanism or a vacuum pump in addition to or instead of the temperature control mechanism. The second liquid phase outlet 53 of the precipitation tank 50 is connected to the stirring tank 10. By supplying the liquid phase separated by precipitation to the stirring tank 10 through the second liquid phase outlet 53, CO 2 4, a reservoir tank 70 and a pump are disposed between the second liquid phase outlet 54 and the stirring tank 10. The reservoir tank 70 can temporarily store the liquid phase in order to adjust the amount of the liquid phase supplied to the stirring tank 10.
[0070] FIG. 4 shows the CO 2 Further shown is a gas-liquid mixer 60 disposed between the gas supply port 11 and the second liquid phase outlet 53 of the deposition tank 50. The gas-liquid mixer 60 includes a compressor 82 and a storage tank 84 for supplying CO 2 A gas supply source 80 is connected. 2 CO from gas source 802 The gas is compressed by a compressor 82 and temporarily stored in a storage tank 84. 2 The gas is supplied from the storage tank 84 to the gas-liquid mixer 60, where it is mixed with the liquid phase sent from the precipitation tank 50, and then supplied to the stirring tank 10. The gas-liquid mixer 60 is, for example, an in-line mixer, a microbubble generator, an air diffuser, an ejector, or an aerator.
[0071] 4 further shows a pretreatment device 90 for pretreating the alkaline earth metal-containing raw material. The alkaline earth metal-containing raw material pretreated in the pretreatment device 90 is supplied into the grinding device 20 from a raw material supply port 24 provided in the grinding device 20, ground in the grinding device 20, and added to the slurry extracted from the stirring tank 10. By supplying an aqueous medium to the grinding device 20 instead of the slurry extracted from the stirring tank 10 and grinding the alkaline earth metal-containing raw material in the aqueous medium, CO 2 A starting slurry containing the alkaline earth metal-containing particles and an aqueous medium to be used for immobilization can also be prepared. The pretreatment device 90 is, for example, a grinding device, a heat treatment device, or a combination thereof.
[0072] [Method for recovering valuable metals] 2 In combination with the immobilization method, valuable metals can also be recovered from alkaline earth metal-containing raw materials containing valuable metals. Since alkaline earth metals consume chemicals such as concentrated sulfuric acid used in valuable metal recovery methods such as high-pressure acid leaching (HPAL), atmospheric pressure acid leaching (ATML), and heap leaching, the profitability of the valuable metal recovery process can be reduced. 2 In the immobilization method, alkaline earth metal-containing particles are crushed to expose the alkaline earth metal on the particle surface, and the crushed alkaline earth metal-containing particles are then fed back into the stirring tank to extract and remove the alkaline earth metal, effectively reducing the alkaline earth metal content in the residue. Therefore, according to the present disclosure, valuable metals can be economically recovered from ores containing large amounts of alkaline earth metals, which could not be economically processed using conventional valuable metal recovery methods that use chemicals.
[0073] [Method for recovering valuable metals - First embodiment] CO of the first embodiment 2 The method for recovering valuable metals by immobilizing CO includes the steps of pretreating an alkaline earth metal-containing raw material containing valuable metals and alkaline earth metals to obtain alkaline earth metal-containing particles and a valuable metal-containing residue; preparing the slurry using the alkaline earth metal-containing particles; 2 and recovering a valuable metal-containing product, intermediate, or both from the valuable metal-containing residue. 2 Before the immobilization process, the alkaline earth metal-containing particles and the valuable metal-containing residue are separated, and the former is decomposed into CO 2 The latter is used for immobilization, and the latter for valuable metal recovery. 2 There is no need to excessively increase the capacity of facilities for immobilization and valuable metal recovery, and CO 2 Immobilization and valuable metal recovery can be carried out.
[0074] In Fig. 5, CO 2 The CO of the first embodiment in combination with the immobilization method 2 The outline of the method for recovering valuable metals by immobilizing alkaline earth metals is shown in the flow diagram. In the pretreatment process, alkaline earth metal-containing particles and valuable metal-containing residue are produced from the starting material, and these are supplied to separate subsequent processes. The alkaline earth metal-containing particles are 2 As shown by the dotted arrow in Figure 5, CO 2 In the immobilization step, if valuable metals are contained in the extraction residue obtained by solid-liquid separation of the mixture in which alkaline earth metal ions have been extracted into the liquid phase, the extraction residue may also be used as a valuable metal-containing residue. These valuable metal-containing residues are recovered in the valuable metal recovery step as valuable metal-containing products, valuable metal-containing intermediates, or both.
[0075] In the pretreatment, alkaline earth metal-containing particles and valuable metal-containing residue are obtained from the starting material.
[0076] The starting material contains a valuable metal and an alkaline earth metal. The form of the starting material is not particularly limited and may be, for example, an ore, a solution, a slurry, a powder, a lump, or a molded body. The powder and lump can be obtained, for example, by crushing the ore or by drying and crushing the solution or slurry. The powder or lump may be dried by evaporating and removing free water. The molded body can be obtained, for example, by tableting the ore, powder, or lump. The molded body may be mixed with an agent used in pretreatment, such as fuel for roasting.
[0077] The valuable metal is not particularly limited, but may be, for example, at least one selected from the group consisting of Ni, Co, Fe, Cu, and platinum group metals. In this disclosure, "platinum group metal" (PGM) is a collective term for ruthenium, rhodium, palladium, osmium, iridium, and platinum, and refers to any one or a combination of two or more of these. The valuable metal may include gold, silver, or a combination thereof.
[0078] In one embodiment, the starting material is an ore containing the above-mentioned valuable metals. Examples of such ores include nickel oxide ore, nickel sulfide ore, cobalt ore, iron ore, copper ore, platinum ore, and metal concentrates obtained by flotation of any one or more of these ores. The ore is preferably nickel oxide ore. Examples of nickel oxide ores include limonite (MgO content: 0.5 to 5% by mass), smectite (MgO content: 5 to 15% by mass), and saprolite (MgO content: 15 to 35% by mass).
[0079] The alkaline earth metal preferably includes Mg.
[0080] In one embodiment, the starting material comprises ultramafic rock. Ultramafic rock is olivine (Mg, Fe)SiO 4 ) and serpentine (composition formula: (Mg, Fe) 3 Si 2 O5 (OH) 4 It is preferable that the material contains at least one mineral selected from the group consisting of:
[0081] Pretreatment in the valuable metal recovery method includes a process for changing the chemical composition or properties of the starting material so that it can be separated into alkaline earth metal-containing particles and valuable metal-containing residue, such as oxidizing roasting, sulfating roasting, and salt conversion / solid-liquid separation.
[0082] Pretreatment in the valuable metal recovery method is CO 2 The pretreatment in the immobilization method may further include grinding, heat treatment, or a combination thereof, as described above. For example, the pretreatment may include microwave heating. Microwave heating can be used to effectively activate the alkaline earth metal-containing particles to their interior.
[0083] The oxidizing roasting can be carried out, for example, using a roasting furnace. An exemplary oxidizing roasting method includes the following steps: 2 ), and oxygen or air is supplied to increase the oxygen partial pressure, and the starting material is heated to about 500 to 700°C for oxidative decomposition. The alkaline earth metals are converted into alkaline earth metal oxides and recovered as alkaline earth metal-containing particles. For example, high Mg-containing minerals such as olivine and serpentine are converted into MgO and SiO by oxidative roasting. 2 The pyrolysis product contains Fe 2 O 3 , Mg 2 SiO 4 , (Mg,Fe)SiO 4 or a combination thereof. Valuable metals are also recovered in the form of oxides as a valuable metal-containing residue.
[0084] Sulfation roasting can be carried out using, for example, a rotary kiln, a fluidized bed heating furnace, or an electric furnace. Exemplary sulfation roasting processes include the following steps: The starting material is mixed with sulfur or a sulfur compound such as sodium sulfide, calcium sulfide, pyrrhotite, or pyrite as a reduction promoter, and the mixture is heated to a reduction range for the valuable metal, for example, about 400°C to 680°C for Ni, thereby selectively sulfated. After sulfation, H 2 After forming metal sulfide using S gas or Ca(OH) 2 The alkaline earth metal-containing particles and the valuable metal-containing residue can be separated by solid-liquid separation after adjusting the pH with an alkali such as NaOH to form valuable metal hydroxides. Another exemplary sulfated roasting method involves adding concentrated sulfuric acid to the starting material, followed by oxidative roasting to sulfate the valuable metals.
[0085] The salt conversion and solid-liquid separation can be carried out using, for example, hot water or an acidic aqueous solution such as sulfuric acid, hydrochloric acid, or nitric acid. An exemplary method includes the following steps: The starting material is placed in a vessel, and hot water or an acidic aqueous solution such as sulfuric acid, hydrochloric acid, or nitric acid is added to dissolve the alkaline earth metals and valuable metals in the form of their salts. After the addition of the hot water or acidic aqueous solution, H 2 O 2 , KMnO 4 The dissolution of the alkaline earth metals or valuable metals may be promoted by adding an oxidizing agent such as H 2 After forming metal sulfide using S gas or Ca(OH) 2 After forming valuable metal hydroxides by adjusting the pH using an alkali such as NaOH, alkaline earth metal-containing particles and valuable metal-containing residue can be separated by solid-liquid separation.
[0086] The pretreatment preferably includes oxidizing roasting. The mixture of alkaline earth metal oxides and valuable metal oxides obtained by oxidizing roasting the starting material can be easily separated by a separation step such as gravity separation.
[0087] When fuel containing sulfur components such as sulfur or pyrite is used in the oxidizing roasting, sulfur dioxide is generated during roasting. Therefore, pretreatment may include exhaust gas treatment of sulfur dioxide. A general sulfuric acid plant can be used as the sulfur dioxide exhaust gas treatment equipment. The concentrated sulfuric acid generated by the sulfur dioxide exhaust gas treatment can be used as a product or effectively in the valuable metal recovery method of the present disclosure, particularly in the valuable metal recovery using a high-pressure acid leaching (HPAL) method, an atmospheric acid leaching (ATML) method, or a heap leaching method.
[0088] Pretreatment may further include a separation step. Examples of separation methods include magnetic separation, specific gravity separation, particle size separation, and chemical composition separation. Magnetic separation utilizes magnetic force to separate particles with different magnetic properties. Specific gravity separation utilizes differences in specific gravity to separate particles with different specific gravities depending on their chemical composition. Specific gravity separation can be performed, for example, using a fluidized specific gravity separation device used in coal preparation technology. Particle size separation utilizes differences in particle size to separate particles with different concentrations of valuable metals depending on their size, or when valuable metals in minerals exist in the form of fine particles. Particle size separation can be performed, for example, using a sieve or a centrifuge. Chemical composition separation involves analyzing particles containing special metals such as uranium online using infrared light and selectively blowing away only the particles with an air gun.
[0089] The pretreatment preferably includes separating alkaline earth metal-containing particles from valuable metal-containing residue by gravity separation. In the gravity separation device, when the specific gravity is set to 4, for example, MgO, SiO 2 Substances with low specific gravity such as NiO, CoO, Fe, etc. are used as alkaline earth metal-containing particles. 2 O 3 Substances with a high specific gravity containing valuable metals such as the above can be separated as valuable metal-containing residue.
[0090] The alkaline earth metal-containing particles obtained by the pretreatment may contain, in addition to the alkaline earth metal, other elements such as silicon, aluminum, or two or more of these. The alkaline earth metal and other elements may be present in the alkaline earth metal-containing particles in the form of oxides, sulfates, silicates, or combinations thereof. In one embodiment, the alkaline earth metal-containing particles contain MgO, SiO 2 and Mg 2 SiO 4 Includes.
[0091] The valuable metal-containing residue may contain, in addition to the valuable metal, for example, silicon, aluminum, or two or more of these elements. The valuable metal may be present in the valuable metal-containing residue in the form of an oxide, chloride, sulfide, or a combination thereof. In one embodiment, the valuable metal-containing residue contains NiO, CoO, and Fe. 2 O 3 The compound contains at least one selected from the group consisting of:
[0092] CO using alkaline earth metal-containing particles 2 Immobilization is CO 2 As explained in the immobilization method, when precipitating alkaline earth metal carbonate, the heat generated in the pretreatment, for example, the roasting step, can be reused as a heat source for heating the liquid phase. By reusing the heat generated in the pretreatment, CO 2 Emissions can be reduced or eliminated.
[0093] The produced alkaline earth metal carbonate can be used as an alkaline earth metal carbonate product, or as a neutralizing agent for pH adjustment in the subsequent primary neutralization, final neutralization, or both, when valuable metal recovery in the method of the present disclosure is carried out by high-pressure acid leaching (HPAL), atmospheric acid leaching (ATML), or heap leaching.
[0094] In primary neutralization, final neutralization, etc., which are subsequent processes in HPAL treatment, ATML treatment, or heap leaching treatment, CO 2 Magnesium carbonate (MgCO 3) or magnesium carbonate hydrate is advantageously used as the neutralizing agent. 3 Alternatively, the Mg contained in magnesium carbonate hydrate is MgSO 4 The magnesium carbonate hydrate is converted into the form of magnesium ions and exists in the liquid phase of the tailings dam. Since there are no strict regulations regarding the discharge of magnesium ions into the ocean, the tailings dam can be treated at low cost. As an example of magnesium carbonate hydrate, nesquehonite (MgCO 3 ・3H 2 O), hydromagnesite (Hydromagnesite: Mg 5 (CO 3 ) 4 (OH) 2 ・4H 2 O), and Dypingite (Mg 5 (CO 3 ) 4 (OH) 2 ・5H 2 O) can be mentioned.
[0095] CO generated in primary neutralization, final neutralization, or both 2 The gas is collected and 2 In this embodiment, CO 2 is preferably used in the primary neutralization, the final neutralization, or both. 2 MgCO produced by immobilization 3 Or when magnesium carbonate hydrate is used as a neutralizing agent, CO 2 When considering the entire process of immobilization and valuable metal recovery, CO 2 This allows for a more closed process with respect to CO 2 The immobilization efficiency can be further increased.
[0096] The liquid phase separated from the alkaline earth metal carbonate may be used as cooling water for other equipment or as water or an aqueous solution for slurrying alkaline earth metal-containing particles.
[0097] In valuable metal recovery, valuable metal-containing products, valuable metal-containing intermediates, or both are recovered from valuable metal-containing residues. Examples of valuable metal-containing products include nickel sulfate, cobalt sulfate, cobalt chloride, metallic nickel, and metallic cobalt. Examples of valuable metal-containing intermediates include mixed sulfide precipitate (MSP) and mixed hydroxide precipitate (MHP). Valuable metal-containing products such as nickel sulfate, cobalt sulfate, and cobalt chloride can be produced by refining valuable metal-containing intermediates. Valuable metal-containing products such as metallic nickel and cobalt can be produced by electrolytic refining of valuable metal-containing products such as nickel sulfate, cobalt sulfate, and cobalt chloride.
[0098] Methods for recovering valuable metal-containing products, valuable metal-containing intermediates, or both include, for example, atmospheric pressure acid leaching (ATML), high-pressure acid leaching (HPAL), chlorine dissolution, ammonia dissolution, electric furnace dissolution, and heap leaching. Atmospheric pressure acid leaching and high-pressure acid leaching involve, for example, adding an acid such as concentrated sulfuric acid to a valuable metal-containing residue under atmospheric or high pressure, preferably at high temperature, to ionize the valuable metal and leach it into a liquid phase. The chlorine dissolution method involves, for example, adding hydrochloric acid to the valuable metal-containing residue to form an aqueous solution containing valuable metal chlorides, and recovering the valuable metal in the form of valuable metal chlorides, or reducing the valuable metal chlorides by electrolysis or the like to recover the valuable metal. The ammonia dissolution method involves, for example, adding ammonia to the valuable metal-containing residue to extract the valuable metal in the form of a metal complex salt (e.g., a nickel complex salt), and is also known as the Callon process. The electric furnace melting method involves, for example, using an electric furnace to melt valuable metal-containing residues, and then oxidizing and removing C, Si, Mn, Cr, P, etc. in a mixed gas flow of argon and oxygen to recover the valuable metals or alloys thereof. The heap leaching method involves piling valuable metal-containing residues on an inclined bed or a filter bed, spraying a leachate such as concentrated sulfuric acid over the pile, and recovering the valuable metals leached in the leachate that reaches the bottom of the inclined bed or that has passed through the filter bed.
[0099] In one embodiment, a valuable metal-containing product, a valuable metal-containing intermediate, or both are recovered from a valuable metal-containing residue by the HPAL process. The HPAL process can efficiently recover valuable metals such as Ni and Co even when nickel oxide ore with a low Ni content is used as a starting material. In addition, the HPAL process converts the iron, which accounts for most of the iron in the ore, into hematite (Fe 2 O 3 ) in the leaching residue, the consumption of acid such as concentrated sulfuric acid used to form the leaching slurry can be reduced. 2 By combining the immobilization method with the HPAL method, valuable metals can be recovered more economically.
[0100] [Method for recovering valuable metals - Second embodiment] CO of the second embodiment2 The method for recovering valuable metals by immobilizing CO2 includes the steps of: pretreating an alkaline earth metal-containing raw material containing valuable metals and alkaline earth metals to obtain a composition containing alkaline earth metal-containing particles; preparing the slurry using the composition; 2 and using the solid phase containing the extraction residue as a valuable metal-containing residue to recover a valuable metal-containing product, intermediate, or both from the valuable metal-containing residue. 2 After immobilization, the solid phase containing the extraction residue is used for valuable metal recovery. 2 Although the equipment capacity for immobilization and valuable metal recovery is larger than that of the first embodiment, 2 By eliminating the separation equipment prior to immobilization, the entire plant can be simplified, and the costs associated with capital investment and operation can be reduced. Also, in humid locations such as tropical rainforests, alkaline earth metal-containing particles may contain moisture, making it difficult to separate them from other components. This embodiment allows CO2 to be separated even in locations where particle separation is difficult. 2 Immobilization and valuable metal recovery can be carried out.
[0101] In Fig. 6, CO 2 The CO of the second embodiment in combination with the immobilization method 2 The outline of the method for immobilizing alkaline earth metals and recovering valuable metals is shown in the flow diagram. In the pretreatment step, a composition containing alkaline earth metal-containing particles is produced from a starting material. This composition contains alkaline earth metal-containing particles and, optionally, a valuable metal-containing component, and is then reacted with CO 2 The valuable metal is contained in the alkaline earth metal-containing particles, the valuable metal-containing component, or both. The valuable metal-containing component of the second embodiment corresponds to the valuable metal-containing residue of the first embodiment. 2 In the immobilization method, the mixture removed from the stirring tank is subjected to solid-liquid separation, and the solid phase containing the extraction residue contains valuable metals. By using this extraction residue as a valuable metal-containing residue, the CO 2In the valuable metal recovery step, a valuable metal-containing product, a valuable metal-containing intermediate, or both are recovered, similar to the method of recovering valuable metals by immobilizing the valuable metal.
[0102] In the pretreatment, alkaline earth metal-containing particles are obtained from the starting material. This embodiment can be used to obtain CO 3 without separating any valuable metal-containing components from the alkaline earth metal-containing particles. 2 In carrying out the immobilization method, the CO 2 This differs from the method of immobilizing the waste and recovering valuable metals.
[0103] The starting material is the CO 2 The method for immobilizing the metal and recovering valuable metals has been described above.
[0104] The pretreatment in the valuable metal recovery method includes a step of changing the chemical composition or chemical properties of the starting material. This step may convert the starting material into alkaline earth metal-containing particles and valuable metal-containing components, or may produce alkaline earth metal-containing particles containing valuable metals. Examples of such a step include the CO 2 The methods for immobilizing alkaline earth metals and recovering valuable metals include oxidizing roasting, sulfating roasting, and salt conversion / solid-liquid separation. However, if alkaline earth metal-containing particles and valuable metal-containing components are generated in these processes, they are not separated at this stage. Therefore, the pretreatment is not performed in the same manner as in the first embodiment. 2 This does not include the separation step described as a pretreatment for the method of immobilizing the metal and recovering valuable metals.
[0105] Pretreatment in the valuable metal recovery method is CO 2 The pretreatment in the immobilization method may further include grinding, heat treatment, or a combination thereof, as described above. For example, the pretreatment may include microwave heating. Microwave heating can be used to effectively activate the alkaline earth metal-containing particles to their interior.
[0106] The alkaline earth metal-containing particles obtained by the pretreatment may contain, in addition to the alkaline earth metal, other elements such as silicon, aluminum, or two or more of these. The alkaline earth metal and other elements may be present in the alkaline earth metal-containing particles in the form of oxides, sulfates, silicates, or combinations thereof. In one embodiment, the alkaline earth metal-containing particles contain MgO, SiO 2 and Mg 2 SiO 4 The alkaline earth metal-containing particles may contain valuable metals such as Ni, Co, and Fe.
[0107] The optional valuable metal-containing component may contain, in addition to the valuable metal, for example, silicon, aluminum, or two or more of these elements. The valuable metal may be present in the valuable metal-containing component in the form of an oxide, chloride, sulfide, or a combination thereof. In one embodiment, the valuable metal-containing component is NiO, CoO, and Fe. 2 O 3 The compound contains at least one selected from the group consisting of:
[0108] CO using a composition containing alkaline earth metal-containing particles 2 The immobilization is carried out in the same manner as in the previous step (5), except that the solid phase containing the extraction residue generated in the solid-liquid separation step is used as the residue containing valuable metals. 2 Immobilization method and CO of the first embodiment 2 This is as explained in the method for immobilizing and recovering valuable metals.
[0109] The valuable metal recovery using the valuable metal-containing residue is the CO 2 This is as explained in the method for immobilizing and recovering valuable metals.
[0110] Figure 7 shows a flow diagram of an outline of the HPAL process. In the HPAL process shown in Figure 7, an acid such as concentrated sulfuric acid is added to a valuable metal-containing residue in the form of a slurry in a reactor such as an autoclave under high temperature and pressure to obtain a leaching slurry. The valuable metals contained in the valuable metal-containing residue are ionized by reaction with the concentrated sulfuric acid and leached into the liquid phase of the leaching slurry. Then, a neutralizing agent is added to the leaching slurry in the primary neutralization to adjust the pH to about 1.5. This pH adjustment is intended to precipitate metal ions such as Fe and Al contained in the leaching slurry as oxides in the primary neutralization. When a carbonate such as an alkaline earth metal carbonate is used in the primary neutralization, CO 2 Gas may be generated. 2 The gas is relatively highly concentrated, so CO 2 When reused for fixation, the energy required for gas pumping can be advantageously reduced, and CO 2 The efficiency of fixation can be improved. 2 gas to CO 2 By reusing it for fixation, CO 2 The release can be suppressed.
[0111] Next, the leaching slurry is washed in multiple stages by continuous counter current decantation (CCD) to separate the leachate and the leach residue into solid and liquid. 2 O 3 The leachate from which Fe, Al, etc. have been separated by the CCD contains traces of Cu, Zn, etc., so these elements are separated by adjusting the pH and redox potential of the leachate, and then the pH of the leachate is adjusted to around 5 to selectively precipitate Ni and Co. During the precipitation, H 2When sulfur dioxide gas is used, mixed sulfide precipitate (MSP) is obtained as a valuable metal-containing intermediate. When an alkali is used during precipitation, mixed hydroxide precipitate (MHP) is obtained as a valuable metal-containing intermediate. These valuable metal-containing intermediates can be separated using a solid-liquid separator to obtain valuable metal-containing products. Mn, Mg, and other dissolved elements remain in the solution from which Ni, Co, and other valuable metals have been removed. Therefore, final neutralization is performed to remove these alkaline earth metals until the pH reaches the marine discharge standard value. Specifically, a neutralizing agent is added to the solution during final neutralization to adjust the pH of the solution to approximately 8.5 to approximately 9. This allows metal ions such as Mn and Mg contained in the solution to precipitate as oxides. When carbonates such as alkaline earth metal carbonates are used for final neutralization, CO 2 Gas may be generated. 2 The gas is relatively highly concentrated, so CO 2 When reused for fixation, the energy required for gas pumping can be advantageously reduced, and CO 2 The efficiency of fixation can be improved. 2 gas to CO 2 By reusing it for fixation, CO 2 The release can be suppressed.
[0112] In this HPAL process, concentrated sulfuric acid produced by treating the exhaust gas from the roasting process included in the pretreatment can be used as part or all of the acid for the HPAL treatment.
[0113] In this HPAL process, CO 2 The alkaline earth metal carbonate produced by immobilization can be used as a neutralizing agent for pH adjustment in the primary neutralization, final neutralization, or both. In this embodiment, regenerated CO 2 can be used as a neutralizing agent for pH adjustment in the primary neutralization, final neutralization, or both. 2 The gas was CO as previously described. 2 By reusing it for fixation, CO 2 When considering the entire process of immobilization and valuable metal recovery,2 This allows for a more closed process with respect to CO 2 The immobilization efficiency can be further increased.
[0114] In one embodiment, the HPAL process is used for valuable metal recovery. 2 The immobilization can be highly integrated with non-ferrous metal smelting processes. The valuable metal-containing residue obtained by pretreatment can be used as a raw material for the HPAL process, and CO 2 The alkaline earth metal carbonates produced by immobilization can be used as neutralizing agents for primary neutralization, final neutralization, and pH adjustment of tailings dams, which are subsequent steps in the HPAL treatment. Furthermore, when sulfur-containing fuels are used in roasting, concentrated sulfuric acid produced in a sulfuric acid plant can be used as the acid for the HPAL treatment.
[0115] The method and apparatus of the present disclosure 2 It can be suitably used for immobilization and recovery of valuable metals.
[0116] The following examples illustrate specific embodiments of the present disclosure, but the present invention is not limited thereto.
[0117] Assuming that the slurry residence time (reaction time) in the stirring tank in step (1) (extraction step) is 2 hours in total, 2 Fixation device (Example) and CO using a multi-stage wet mill 2 The layout of the device for the extraction step of the immobilization device (comparative example) was compared. In the extraction step using a wet mill, grinding of alkaline earth metal-containing particles and extraction of alkaline earth metals are carried out simultaneously in the wet mill.
[0118] The conditions of the extraction process used for comparison were as follows: Processing rate of alkaline earth metal-containing raw material: 59 t / h Slurry concentration: 9.1 mass % Slurry specific gravity: 1.0 (assumed to be almost the same as water due to the low concentration) Processing flow rate: 650 m 3 / h
[0119] In one embodiment, CO 2An exemplary equipment layout for the extraction process of the immobilization device is shown in a top view in Figure 8A. With a throughput of 59 t / h, the inner diameter of the stirring tank 10 was set to 12 m and its height to 18 m. One wet mill was installed as the crushing device 20, and a liquid cyclone was installed as the classification device 30. The pump 102, maintenance space 103, and pipe rack 104 are also shown in Figure 8A. The floor area required for the equipment for the extraction process is 38 m (38,000 mm) x 17 m (17,000 mm) = 646 m 2 is.
[0120] In the extraction process using a multistage wet mill, the appropriate dimensions of the wet mill are estimated to be approximately 3 m in inner diameter and 5 m in length, based on a processing rate of 59 t / h. Since the slurry residence time per wet mill is estimated to be approximately 15 minutes, eight wet mills connected in series are required to achieve a total slurry residence time of 2 hours. Considering the space required for maintenance such as filling and replacing the abrasive media, CO extraction using a multistage wet mill is 2 The layout of the equipment involved in the extraction process of the immobilization device is as shown in Figure 8B. Figure 8B shows eight wet mills 101, pumps 102 corresponding to each wet mill, a maintenance space 103, and a pipe rack 104. The floor area required for the equipment involved in the extraction process is 67 m (67,000 mm) x 30 m (30,000 mm) = 2,010 m 2 is.
[0121] From these calculation results, CO 2 The floor space required for the extraction process of the immobilization device is about 1 / 3 (=646 / 2010) compared to when a multistage wet mill is used. 2 The immobilization device can significantly reduce the installation area of the equipment involved in the extraction process.
[0122] It will be apparent to those skilled in the art that the above-described embodiments and examples can be modified in various ways without departing from the basic principles of the present invention, and that various improvements and modifications of the present invention can be made without departing from the spirit and scope of the present invention.
[0123] The method and apparatus of the present disclosure 2It can be advantageously used for the immobilization and recovery of valuable metals.
[0124] 1 CO 2 Immobilization device 10 Stirring tank 11 CO 2 Gas supply port 12 First slurry supply port 13 First slurry discharge port 20 Pulverizer 22 Second slurry supply port 23 Second slurry discharge port 24 Raw material supply port 30 Classifier 32 Third slurry supply port 33 Heavy component discharge port 34 Light component discharge port 40 Solid-liquid separator 42 Light component supply port 43 First liquid phase discharge port 44 First solid phase discharge port 50 Precipitation tank 52 Liquid phase supply port 53 Second liquid phase discharge port 54 Second solid phase discharge port 60 Gas-liquid mixer 70 Storage tank 80 CO 2 Gas supply source 82 Compressor 84 Storage tank 90 Pretreatment device
Claims
1. In a mixing vessel, a slurry containing alkaline earth metal-containing particles and an aqueous medium and CO 2 Gas, CO 2 CO selected from the group consisting of saturated water, and combinations thereof. 2 a source of alkaline earth metal and a slurry containing the alkaline earth metal-containing particles are stirred and mixed to produce a mixture in which alkaline earth metal ions in the alkaline earth metal-containing particles are extracted in a liquid phase; extracting a slurry containing the alkaline earth metal-containing particles from the stirring tank and supplying it to a crushing device; crushing the alkaline earth metal-containing particles in the crushing device; supplying the slurry containing the crushed alkaline earth metal-containing particles to the stirring tank; subjecting the mixture extracted from the stirring tank to solid-liquid separation to obtain a liquid phase containing the alkaline earth metal ions and a solid phase containing an extraction residue; and precipitating an alkaline earth metal carbonate from the liquid phase containing the alkaline earth metal ions to obtain CO in the alkaline earth metal carbonate. 2 and immobilizing CO 2 Immobilization method.
2. The method according to claim 1, further comprising: extracting the slurry containing the alkaline earth metal-containing particles from the stirring tank, separating the slurry containing the alkaline earth metal-containing particles into a light fraction and a heavy fraction in a classifier, and supplying the heavy fraction to the pulverizer. 2 Immobilization method.
3. The method according to claim 2, further comprising subjecting the light fraction to solid-liquid separation to obtain a liquid phase of the light fraction, and supplying the liquid phase to the stirring tank.
4. Add CO to the light fraction phase 2 4. The method of claim 3, comprising feeding the light liquid phase to the stirred tank after mixing with gas.
5. Precipitating an alkaline earth metal carbonate from the light fraction liquid phase obtained by solid-liquid separation of the light fraction, and adding CO 2 and supplying the liquid phase separated by the precipitation to the stirred tank.
6. The method according to any one of claims 1 to 4, wherein the grinding device is a wet mill, an attrition pump, an electric pulse grinding device, an impulse grinding device, or a high pressure jet nozzle grinding device.
7. The method of any one of claims 1 to 4, comprising feeding an alkaline earth metal-containing feedstock to the grinding apparatus.
8. The method according to any one of claims 1 to 4, wherein the stirring and mixing in the stirring tank is carried out under atmospheric pressure.
9. The above CO 2 5. The method of claim 1, comprising introducing a gas directly into the stirred vessel.
10. The method of any one of claims 1 to 4, wherein the alkaline earth metal is magnesium.
11. The method of any one of claims 1 to 4, wherein the alkaline earth metal-containing particles comprise magnesium silicate.
12. CO 2 a stirring tank having a gas supply port, a first slurry supply port, and a first slurry discharge port; and a grinding device having a second slurry supply port connected to the first slurry supply port of the stirring tank, and a second slurry discharge port connected to the first slurry supply port of the stirring tank, the grinding device being configured to grind the alkaline earth metal-containing particles in a slurry containing alkaline earth metal-containing particles and an aqueous medium, the slurry being extracted from the stirring tank through the first slurry discharge port and supplied through the second slurry supply port, discharge the ground slurry containing the alkaline earth metal-containing particles through the second slurry discharge port, and supply the ground slurry to the stirring tank through the first slurry supply port. 2 Immobilization device.
13. The above CO 2 13. The CO2 immobilization apparatus according to claim 12, further comprising a classification device disposed between the first slurry discharge port of the stirring tank and the second slurry supply port of the grinding device, the classification device including a third slurry supply port, a light fraction discharge port and a heavy fraction discharge port, the third slurry supply port being connected to the first slurry discharge port of the stirring tank, and the heavy fraction discharge port being connected to the second slurry supply port of the grinding device. 2Immobilization device.
14. The above CO 2 The CO2 feed system according to claim 13, wherein the fixation apparatus further includes a solid-liquid separation apparatus connected to the classification apparatus and a precipitation tank connected to the solid-liquid separation apparatus, the solid-liquid separation apparatus having a light fraction supply port, a first liquid phase discharge port and a first solid phase discharge port, the precipitation tank having a liquid phase supply port, a second liquid phase discharge port and a second solid phase discharge port, the light fraction supply port of the solid-liquid separation apparatus is connected to the light fraction discharge port of the classification apparatus, the first liquid phase discharge port is connected to the liquid phase supply port of the precipitation tank, and the second liquid phase discharge port of the precipitation tank is connected to the stirring tank. 2 Immobilization device.
15. The above CO 2 The fixation device fixes the CO 2 15. The CO method of claim 14, further comprising a gas-liquid mixer disposed between a gas inlet and the second liquid phase outlet of the deposition vessel. 2 Immobilization device.
16. The CO method according to any one of claims 12 to 15, wherein the grinding device is a wet mill, an attrition pump, an electric pulse grinding device, an impulse grinding device, or a high-pressure jet nozzle grinding device. 2 Immobilization device.
17. A method for producing a CO2-containing slurry according to any one of claims 1 to 4, comprising pretreating an alkaline earth metal-containing raw material containing a valuable metal and an alkaline earth metal to obtain alkaline earth metal-containing particles and a valuable metal-containing residue; and using the alkaline earth metal-containing particles to prepare the slurry. 2 carrying out a fixation method; and recovering a product, an intermediate, or both containing the valuable metal from the valuable metal-containing residue. 2 A method of immobilizing the wastewater and recovering valuable metals.
18. The method according to any one of claims 1 to 4, comprising pretreating an alkaline earth metal-containing raw material containing a valuable metal and an alkaline earth metal to obtain a composition containing alkaline earth metal-containing particles, and using the composition to prepare the slurry. 2carrying out an immobilization method; and using the solid phase containing the extraction residue as a valuable metal-containing residue, and recovering a valuable metal-containing product, intermediate, or both from the valuable metal-containing residue. 2 A method of immobilizing the wastewater and recovering valuable metals.
Citation Information
Patent Citations
Emission reduction system of sequestered flue gas CO2 of coal-fired power plant by wet mineralization
CN102658014A
Device for preparing calcium carbonate whiskers by CO2 mineralization and preparation method of calcium carbonate whiskers
CN108588842A
Method for fixing co2 with alkaline earth metallic silicate
JP1998249153A
Improved integrated chemical method
JP2012500718A
Low carbon footprint magnetic material manufacturing
JP2019525887A
Cited By
Method for sequestering carbon dioxide
WO2026171840A1