Molding mold and method for producing molded article

The molding die design with a burr storage space and inclined groove-like recess addresses the inefficiency of stuck burrs by enabling easy removal, thereby improving manufacturing efficiency.

WO2024247931A1PCT designated stage expired Publication Date: 2024-12-05KYORAKU CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/019258
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-30
Filing Date
2024-05-24
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Existing molding processes face inefficiencies due to burrs from molded products becoming stuck in groove-shaped recesses of molds, requiring time and effort to remove, which decreases manufacturing efficiency.

Method used

A molding die design featuring split molds with a burr storage space and a protruding member that can move through a guide hole, along with a groove-like recess with an inner side surface inclined at 60 degrees or less, preventing burrs from fitting into the recess and facilitating easy removal.

Benefits of technology

This design enhances manufacturing efficiency by allowing for straightforward separation of burrs from molded products, reducing the time and effort required for removal and maintaining mold productivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024019258_05122024_PF_FP_ABST
    Figure JP2024019258_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides a molding mold that is capable of suppressing a decrease in production efficiency of a molded article. The present invention provides a molding mold having first and second divided molds that can be open and closed, said molding mold comprising a cavity, a pinch-off part, a burr accommodation space, and a protruding member, wherein: the cavity is a space for molding a desired molded article; the outer surface of the cavity is formed by joining cavity surfaces of the first and second divided molds; the pinch-off part is provided to mating surfaces of the first and second divided molds so as to surround the cavity; the burr accommodation space is provided to the outer side of the pinch-off part and accommodates a burr formed in the periphery of the molded article; the first divided mold is provided with a guide hole at a part opposite to the burr accommodation space; the protruding member is capable of advancement and retraction through the guide hole with respect to the burr accommodation space; the second divided mold is provided with a groove-like recess that is provided opposite from the burr accommodation space and along the pinch-off part; the groove-like recess is provided with an inner side surface that extends along the bottom of the groove-like recess from the pinch-off part; and the inner side surface has a first part that has an inclination angle of not more than 60 degrees with respect to a reference plane which is perpendicular to the opening / closing direction of the first and second divided molds.
Need to check novelty before this filing date? Find Prior Art

Description

Molding molds and manufacturing methods for molded products

[0001] The present invention relates to a molding die and a method for manufacturing a molded product.

[0002] Patent Document 1 discloses a technique in which a protruding member is protruded from a molded product in a die to protrude burrs that have adhered to the periphery of the molded product, thereby separating the burrs from the molded product.

[0003] Japanese Patent Application Laid-Open No. 2007-276125

[0004] In Patent Document 1, the protruding member protrudes into a groove-like recess provided around the pinch-off portion, but burrs separated from the molded product may get stuck in the groove-like recess and become difficult to remove. In this case, it takes time and effort to remove the burrs from the groove-like recess, which reduces the manufacturing efficiency of the molded product.

[0005] The present invention has been made in view of the above circumstances, and aims to provide a molding die that can suppress a decrease in the production efficiency of molded products.

[0006] According to the present invention, the following inventions are provided: [1] A molding die having first and second split dies that can be opened and closed, comprising a cavity, a pinch-off portion, a flash-accommodating space, and an ejection member, the cavity being a space for molding a desired molded product, the cavity surfaces provided in the first and second split dies coming together to form the outer surface of the cavity, the pinch-off portion being provided on the mating surfaces of the first and second split dies so as to surround the cavity, the flash-accommodating space being provided outside the pinch-off portion and configured to accommodate flash formed around the molded product. a space for accommodating a burr, the first split mold having a guide hole at a portion facing the burr accommodating space, the ejection member being configured to be able to advance and retreat into the burr accommodating space through the guide hole, the second split mold having a groove-like recess facing the burr accommodating space and provided along the pinch-off portion, the groove-like recess having an inner side surface extending from the pinch-off portion toward a bottom of the groove-like recess, the inner side surface having a first portion having an inclination angle of 60 degrees or less with respect to a reference plane perpendicular to a direction in which the first and second split molds are opened and closed. [2] The molding mold according to [1], wherein the inner side surface has a second portion located farther from the pinch-off portion than the first portion, and the second portion has an inclination angle with respect to the reference plane greater than that of the first portion. [3] The molding die according to [1] or [2], wherein the inner side surface is provided with a localized recess extending in the advancing / retreating direction of the ejection member at a position facing the ejection member when the ejection member is ejected into the groove-shaped recess. [4] The molding die according to any one of [1] to [3], wherein the molding die comprises a burr clamp portion, the burr clamp portion is provided on the mating surfaces of the first and second split dies outside the pinch-off portion, and the burr accommodating space is provided between the pinch-off portion and the burr clamp portion. [5] The molding die according to [4], wherein the groove-shaped recess has an outer side surface extending from the burr clamp portion toward the bottom of the groove-shaped recess, and the outer side surface has a first portion whose inclination angle with respect to the reference plane is 60 degrees or less.[6] A method for manufacturing a molded product, comprising a molding step and a cutting step, wherein in the molding step, a molded body is formed by molding a parison using a molding die described in any one of [1] to [5], and the molded body comprises the molded product formed in the cavity and the burr connected to the periphery of the molded product, and in the cutting step, the burr is cut off from the molded product by protruding the ejection member into the burr storage space. [7] A molding die having first and second split dies that can be opened and closed, comprising a cavity, a pinch-off portion, a flash accommodating space, and an ejection member, wherein the cavity is a space for molding a desired molded product, and the cavity surfaces provided on the first and second split dies are joined to form the outer surface of the cavity, the pinch-off portion is provided on the mating surfaces of the first and second split dies so as to surround the cavity, and the flash accommodating space is a space provided outside the pinch-off portion and for accommodating flash formed around the molded product, and the first split die is A molding die having a guide hole in a portion facing the burr storage space, the ejection member being configured to be able to advance and retreat into the burr storage space through the guide hole, the second split die having a groove-like recess facing the burr storage space and provided along the pinch-off portion, the groove-like recess having an inner side surface extending from the pinch-off portion toward the bottom of the groove-like recess, the inner side surface having first and second portions, the second portion being provided at a position farther from the pinch-off portion than the first portion, and having a larger inclination angle with respect to a reference plane perpendicular to the opening and closing direction of the first and second split dies than the first portion.[8] A molding die having first and second split dies that can be opened and closed, comprising a cavity, a pinch-off portion, a flash accommodating space, and an ejection member, wherein the cavity is a space for molding a desired molded product, and the outer surface of the cavity is formed by the combination of cavity surfaces provided on the first and second split dies, respectively, the pinch-off portion is provided on the mating surfaces of the first and second split dies so as to surround the cavity, and the flash accommodating space is a space provided outside the pinch-off portion and for accommodating flash formed around the molded product, and the first split a molding die in which the split die has a guide hole at a portion facing the burr storage space, the ejection member is configured to be able to advance and retreat into the burr storage space through the guide hole, the second split die has a groove-like recess facing the burr storage space and provided along the pinch-off portion, the groove-like recess has an inner side extending from the pinch-off portion toward the bottom of the groove-like recess, and the inner side has a local recess extending along the advance and retreat direction of the ejection member at a position facing the ejection member when the ejection member is ejected into the groove-like recess.

[0007] In the molding die of the present invention, a first section with a gentle inclination of 60 degrees or less is provided on the inner side surface of the groove-shaped recess provided along the pinch-off portion, thereby preventing burrs that have been cut off from the molded product from getting stuck in the groove-shaped recess and becoming difficult to remove, and preventing a decrease in the manufacturing efficiency of the molded product.

[0008] FIG. 4A is a front view showing a state in which a parison 2 is placed between first and second split molds 11 and 12 constituting a molding die 1 in a molding step of a manufacturing method according to an embodiment of the present invention. It is a view of the first split mold 11 of FIG. 1 as seen from the parison 2 side. It is a view of the second split mold 12 of FIG. 1 as seen from the parison 2 side. FIG. 4A is a partial perspective view of the molding die 1 of FIG. 1 with the first and second split molds 11 and 12 in a closed state, with a portion cut out. FIG. 4B is a view of the molding die 1 of FIG. 4A as seen from a direction perpendicular to the cross section of FIG. 4A. It is a perspective view of the first split mold 11 and the second split mold 12 of the molding die 1 of FIG. 4A as seen from different directions. FIG. 6A is a view of the first and second split molds 11 and 12 of FIG. 4B in an open state, and FIGS. 6B and 6C are enlarged views of regions B and C in FIG. 6A, respectively. Fig. 7A is a cross-sectional view parallel to the cross-section of Fig. 4B and passing through the central axis of the ejection member 16, and Fig. 7B is an enlarged view of region B in Fig. 7A. Fig. 8A is a cross-sectional view corresponding to Fig. 7A, showing the state after the parison 2 is sandwiched between the first and second split molds 11, 12 and molded to form the molded body 3. Fig. 8B is a view of the molded body 3 extracted from region A in Fig. 8A. Fig. 9A is an enlarged view of region A in Fig. 8A, and Fig. 9B shows the state after a cooling medium is sprayed onto the burr 5 through the burr cooling holes 12i from the state of Fig. 8A. Fig. 10A shows the state in which the burr 5 is being pressed by the ejection member 16 from the state of Fig. 9A, and Fig. 10B shows the state after the burr 5 has been further pressed from the state of Fig. 10A. These are views corresponding to Fig. 7B, showing modified first and second split molds 11, 12.

[0009] The following describes embodiments of the present invention. The various features shown in the following embodiments can be combined with each other. Furthermore, each feature can be an independent invention.

[0010] A method for manufacturing a molded product according to one embodiment of the present invention will be described using Figures 1 to 10. Examples of molded products 4 manufactured by this method include hollow molded products such as ducts and sheet molded products such as door trims. The molded product 4 may be a foam molded product or a non-foam molded product. This method comprises a molding step and a dividing step. It is preferable to include a cooling step between the molding step and the dividing step. Each step will be described below.

[0011] 1. Molding Process As shown in FIGS. 1 and 8 , in the molding process, a parison 2 is molded using a molding die 1 to form a molded body 3. The molded body 3 has a structure in which a flash 5 is connected to the molded article 4. The flash 5 has a thin-walled portion 5a where it connects to the molded article 4, and the flash 5 can be separated from the molded article 4 by tearing the thin-walled portion 5a. The molding method is not particularly limited as long as it can produce a molded body 3 in which the flash 5 is connected to the molded article 4. Examples of the molding method include blow molding and vacuum molding. These molding methods may be direct molding, in which the parison 2 formed by extruding a molten resin is used without cooling, or molding using a cooled parison that has been reheated. However, direct molding is preferred. The shape of the parison 2 is not particularly limited and may be cylindrical or sheet-like. Any resin may be used for molding, including thermoplastic resins such as polyolefin resins, such as polypropylene. In one example, a molded body for a duct is formed by direct blow molding using a cylindrical parison 2.

[0012] 4, the molding die 1 has first and second split dies 11 and 12 that can be opened and closed. The molding die 1 also has a cavity 13, a pinch-off portion 14, a flash storage space 15, and an ejection member 16.

[0013] 4 to 7, the cavity 13 is a space for molding the desired molded product 4, and the divided cavity surfaces 11a, 12a provided in the first and second split molds 11, 12, respectively, are joined together to form the cavity outer surface 13a. In one example, the divided cavities 11b, 12b provided in the first and second split molds 11, 12, respectively, are joined together to form the cavity 13. The cavity outer surface 13a has a shape corresponding to the outer surface of the molded product 4. The parison 2 can be shaped to fit the cavity outer surface 13a by blowing air into the bag-shaped parison 2 within the cavity 13 or by vacuum-suctioning the parison 2 from the cavity outer surface 13a.

[0014] The pinch-off portion 14 is provided on the mating surfaces 17 of the first and second split molds 11, 12 so as to surround the cavity 13. The pinch-off portion 14 is preferably provided around the entire circumference of the cavity 13. In the pinch-off portion 14, the parison 2 is pinched and thinned to form the thin-walled portion 5a. As shown in FIG. 2 , the first split mold 11 is provided with a ridge 11c surrounding the split cavity 11b, and the second split mold 12 is provided with a ridge 12c surrounding the split cavity 12b, and the ridges 11c and 12c are pressed against each other to form the pinch-off portion 14. The widths of the ridges 11c and 12c may be different from each other, and one of the ridges 11c and 12c may be a flat surface. The width of the pinch-off portion 14 is, for example, 0.1 to 3.0 mm, preferably 0.2 to 1.0 mm (0.5 mm in this embodiment). Specific examples of this width include 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.5, 2.0, 2.5, and 3.0 mm, and may be in a range between any two of the values ​​exemplified here.

[0015] The burr accommodating space 15 is a space provided outside the pinch-off portion 14 and for accommodating burrs 5 formed around the molded product 4. The burr accommodating space 15 is preferably provided so as to surround the pinch-off portion 14. The burr accommodating space 15 is preferably an elongated space. Since the burr accommodating space 15 is a space surrounded by the first and second split molds 11, 12, each of the first and second split molds 11, 12 has a portion facing the burr accommodating space 15.

[0016] As shown in Fig. 7, the first split mold 11 has a guide hole 11d in a portion facing the burr storage space 15. The ejection member 16 is configured to be able to advance and retreat into the burr storage space 15 through the guide hole 11d. As shown in Figs. 8 to 10, the ejection member 16 is pushed from the first split mold 11 side toward the burr 5 in the burr storage space 15 and the burr 5 is pressed toward the second split mold 12 side, thereby tearing the thin-walled portion 5a and separating the burr 5 from the molded product 4. As shown in Fig. 2, it is preferable to provide a plurality of guide holes 11d and ejection members 16 along the pinch-off portion 14.

[0017] To enhance the ability to separate the burr 5, the ejection member 16 is preferably positioned as close as possible to the pinch-off portion 14. The distance D1 (shown in FIG. 7B ) between the pinch-off portion 14 and the ejection member 16 is, for example, 3 to 20 mm, preferably 5 to 15 mm (10 mm in this embodiment). The distance D2 between the center axis of the ejection member 16 and the pinch-off portion 14 is, for example, 10 to 30 mm, preferably 15 to 25 mm (20 mm in this embodiment). If these values ​​are too small, the ejection member 16 is more likely to interfere with the second split mold 12, while if these values ​​are too large, the ability to separate the burr 5 may be impaired. Specifically, D1 may be, for example, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, or 20 mm, or may be within a range between any two of the values ​​exemplified here. Specifically, D2 may be, for example, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, or 30 mm, or may be in a range between any two of the values ​​exemplified here.

[0018] The diameter of the ejection member 16 is, for example, 5 to 40 mm, preferably 10 to 30 mm, and more preferably 15 to 25 mm (20 mm in this embodiment). If this value is too small, the breakability of the burr 5 may be reduced, while if this value is too large, the burr accommodation space 15 may become large, which may lead to an increase in mold size. Specific examples of this value are 5, 10, 15, 20, 25, 30, 35, and 40 mm, and may be within a range between any two of the values ​​exemplified here.

[0019] 7B, a recess 16b is provided in the center of the tip surface 16a of the protruding member 16. A tapered surface 16c is provided around the periphery of the tip surface 16a. This makes it easier for the tip surface 16a to bite into the burr 5, making it less likely for the burr 5 to slip relative to the tip surface 16a when the protruding member 16 is protruded, and making it easier for the force applied by the protruding member 16 to be transmitted to the burr 5.

[0020] 6, in this embodiment, the first and second split dies 11 and 12 have groove-like recesses 11e and 12e, respectively, that face the burr-accommodating space 15 and are provided along the pinch-off portion 14. The groove-like recesses 11e and 12e are joined together to form the burr-accommodating space 15. Note that the first split die 11 may not have the groove-like recess 11e, and the portion that faces the burr-accommodating space 15 may be, for example, a flat surface.

[0021] The depth of the groove-like recess 11e of the first split mold 11 is, for example, 0 to 5.0 mm, preferably 1.0 to 4.0 mm, and more preferably 2.0 to 3.0 mm (2.5 mm in this embodiment). A depth of 0 mm means that the portion facing the flash storage space 15 is flat. If this value is too small, the resin extruded from the pinch-off portion 14 tends to move toward the cavity 13 rather than the flash storage space 15, which may result in a bulge of resin on the inner surface of the molded product 4 if the molded product 4 is hollow. If this value is too large, the ability of the ejecting member 16 to break up the flash 5 may be reduced.

[0022] The depth of the groove-like recess 12e of the second split mold 12 is, for example, 10 to 50 mm, preferably 20 to 40 mm, and more preferably 25 to 35 mm (30 mm in this embodiment). If this value is too small, the stroke of the ejection member 16 may be too short, reducing the ability to separate the burr 5. If this value is too large, the burr 5 may become stuck in the groove-like recess 12e and become difficult to remove. Specific examples of this value are 10, 15, 20, 25, 30, 35, 40, 45, and 50 mm, and may be within a range between any two of the values ​​exemplified here.

[0023] The groove-shaped recess 12e of the second split mold 12 has an inner side surface 12f extending from the pinch-off portion 14 toward the bottom 12k of the groove-shaped recess 12e. The inner side surface 12f has a first portion 12f1 whose inclination angle α1 (shown in FIG. 7B ) with respect to a reference plane 19 perpendicular to the opening and closing direction of the first and second split molds 11 and 12 (the left-right direction in FIG. 1 , the up-down direction in FIG. 6A ) is 60 degrees or less (in this embodiment, α1 = 45 degrees). Providing such an inclination portion on the inner side surface 12f prevents the separated burr 5 from getting stuck in the groove-shaped recess 12e and becoming difficult to remove. The angle of the first portion 12f1 is, for example, 15 to 60 degrees, preferably 20 to 55 degrees, and more preferably 25 to 50 degrees. Specifically, this value may be, for example, 15, 20, 25, 30, 35, 40, 45, 50, 55, or 60 degrees, and may be a value between any two of the values ​​exemplified here or less. The first portion 12f1 may be a flat surface or a curved surface (a flat surface in this embodiment). Note that in this embodiment, the mating surface 17 and the reference surface 19 are parallel to each other, so in Figures 4B and 6A, the mating surface 17 and the reference surface 19 are denoted by the same straight line. However, the mating surface 17 and the reference surface 19 may not be parallel to each other.

[0024] The first portion 12f1 is preferably located shallower than the center of the depth direction of the groove-like recess 12e, and more preferably located so as to be connected to the pinch-off portion 14 (i.e., the first portion 12f1 is preferably a connecting portion 12j connected to the pinch-off portion 14). If the inclination angle of the connecting portion 12j connected to the pinch-off portion 14 is too large, the ridge 12c constituting the pinch-off portion 14 will have a thin, protruding shape and will have low strength. However, in this embodiment, the inclination angle of the connecting portion 12j is 60 degrees or less, so that the ridge 12c does not become extremely thin, and a decrease in strength is suppressed. The same applies to the ridge 11c; the inclination angle of the connecting portion 11j connected to the pinch-off portion 14 on the outside of the pinch-off portion 14 is preferably 60 degrees or less (45 degrees in this embodiment). The inclination angle of the connecting portions 11j, 12j may be, for example, specifically, 15, 20, 25, 30, 35, 40, 45, 50, 55, or 60 degrees, and may be in a range between any two of the values ​​exemplified here or less than any one of them.

[0025] Furthermore, if the inclination angle of the connecting portion 12j becomes too large, the burr 5 will be more likely to break off before it is pressed by the pushing member 16, as shown in Figures 9 and 10. In this case, the cooling medium will come into direct contact with the pinch-off portion 14 during the cooling process, making it easier for the molded product 4 to be cooled through the pinch-off portion 14, and defects such as sink marks will be more likely to occur in the molded product 4. However, by setting the inclination angle of the connecting portion 12j to 60 degrees or less, the occurrence of the above-mentioned defects can be suppressed.

[0026] The projected width W of the first portion 12f1 (the length of the projection onto the reference plane 19 in the direction perpendicular to the extension direction of the pinch-off portion 14; shown in FIG. 6C ) is, for example, 1 to 20 mm, and preferably 3 to 10 mm. If this value is too small, the effect of providing the first portion 12f1 may not be fully exerted. If this value is too large, the second split mold 12 is likely to interfere with the ejection member 16. Specific examples of this value are 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, and 20 mm, and may be in a range between any two of the values ​​exemplified here.

[0027] The inner side surface 12f preferably has a second portion 12f2 located farther from the pinch-off portion 14 than the first portion 12f1. The second portion 12f2 may be flat or curved (flat in this embodiment). The second portion 12f2 is preferably provided so as to be continuous with the first portion 12f1. The inclination angle α2 of the second portion 12f2 relative to the reference plane 19 is larger than the inclination angle α1 of the first portion 12f1 (α2 = 75 degrees in this embodiment). This configuration reduces interference between the second split mold 12 and the ejection member 16. The inclination angle α2 of the second portion 12f2 is, for example, 50 to 85 degrees, preferably 60 to 80 degrees. The difference between the inclination angle α2 of the second portion 12f2 and the inclination angle α1 of the first portion 12f1 is, for example, 10 to 50 degrees, preferably 20 to 40 degrees. If this value is too small, the effect of providing the second portion 12f2 may not be fully realized. If this value is too large, the burr 5 may get stuck in the groove-shaped recess 12e and become difficult to remove. Specifically, the inclination angle α2 is, for example, 50, 55, 60, 65, 70, 75, 80, or 85 degrees, and may be in a range between any two of the values ​​exemplified here. Specifically, the difference between the inclination angle α2 and the inclination angle α1 is, for example, 10, 15, 20, 25, 30, 35, 40, 45, or 50 degrees, and may be in a range between any two of the values ​​exemplified here.

[0028] The projected width of the second portion 12f2 is, for example, 1 to 5 mm, specifically, for example, 1, 2, 3, 4, or 5 mm, or may be in a range between any two of the values ​​exemplified here. The projected width of the second portion 12f2 is preferably narrower than the projected width W of the first portion 12f1.

[0029] The inner side surface 12f preferably has a third portion 12f3 located farther from the pinch-off portion 14 than the second portion 12f2. The third portion 12f3 is preferably provided so as to be continuous with the second portion 12f2. The third portion 12f3 has an inclination angle α3 with respect to the reference plane 19 that is greater than the inclination angle α2 of the second portion 12f2 (in this embodiment, α3 = 90 degrees). This configuration makes it even less likely that the second split mold 12 will interfere with the ejection member 16. The inclination angle α3 of the third portion 12f3 is, for example, 80 to 90 degrees, and preferably 85 to 90 degrees.

[0030] 7B , it is preferable that the inner side surface 12f has a local recess 12g extending in the advancing / retracting direction of the ejecting member 16 at a position facing the ejecting member 16 when the ejecting member 16 is ejected into the groove-shaped recess 12e. By providing the local recess 12g, interference between the second split mold 12 and the ejecting member 16 can be avoided, making it easier to bring the ejecting member 16 closer to the pinch-off portion 14 and improving the ability to separate the burr 5. Furthermore, when the burr 5 is pushed into the local recess 12g, a reaction force tends to cause the burr 5 to float in areas other than the local recess 12g or to take on a wavy shape within the groove-shaped recess 12e, making it easier to remove the burr 5 from the groove-shaped recess 12e.

[0031] The depth of the local recess 12g (the depth in the direction perpendicular to the advancing / retracting direction of the protruding member 16 (i.e., the left-right direction in FIG. 7 )) is, for example, 1 to 10 mm, preferably 2 to 8 mm (5 mm in this embodiment). If this value is too small, the effect of providing the local recess 12g may not be fully exhibited, while if this value is too large, the burr 5 may become stuck in the local recess 12g and become difficult to remove. Specific examples of this value include 1, 2, 3, 4, 5, 6, 7, 8, 9, and 10 mm, and may be within a range between any two of the values ​​exemplified here. The width of the local recess 12g (the length in the extending direction of the pinch-off portion 14) is, for example, 5 to 40 mm, preferably 10 to 30 mm, and preferably 25 to 35 mm (20 mm in this embodiment). If this value is too small, the effect of providing the local recess 12g may not be fully exhibited, while if this value is too large, the burr 5 may become stuck in the local recess 12g and become difficult to remove. This value may be, for example, 5, 10, 15, 20, 25, 30, 35, or 40 mm, or may be in a range between any two of the values ​​exemplified here.

[0032] 9A , the molding die 1 preferably includes a burr clamping portion 18. The burr clamping portion 18 is provided on the mating surface 17 of the first and second split dies 11, 12 outside the pinch-off portion 14. The burr containing space 15 is provided between the pinch-off portion 14 and the burr clamping portion 18. By clamping the burr 5 outside the burr containing space 15, the burr 5 is less likely to be displaced when the ejection member 16 is ejected toward the burr 5, thereby improving the ability to separate the burr 5. Although the burr clamping portion 18 clamps the burr 5, it is preferable that the burr clamping portion 18 is not as thin as the pinch-off portion 14 so that the burr 5 is not separated on the burr clamping portion 18 side when the ejection member 16 is ejected toward the burr 5. Therefore, when the first and second split dies 11, 12 are in the closed state, it is preferable that the distance between the first and second split dies 11, 12 at the burr clamping section 18 is wider than the distance between the first and second split dies 11, 12 at the pinch-off section 14.

[0033] The distance D (shown in FIG. 7B ) between the pinch-off portion 14 and the burr clamping portion 18 is, for example, 20 to 150 mm, preferably 30 to 100 mm (40 mm in this embodiment). If this distance is too small, the force applied by the protruding member 16 may act strongly on the portion of the burr 5 that is clamped by the burr clamping portion 18, making the burr 5 more likely to break at this portion. If this distance is too large, the burr 5 may be less easily broken. Specifically, the distance D may be, for example, 20, 30, 40, 50, 60, 70, 80, 90, 100, 110, 120, 130, 140, or 150 mm, or may be within a range between any two of the values ​​exemplified here.

[0034] D1 / D is preferably 0.40 or less, more preferably 0.30 or less (0.25 in this embodiment). D1 / D is, for example, 0.05 to 0.50, and preferably 0.15 to 0.40. D2 / D is preferably 0.50 or less, more preferably 0.35 or less (0.50 in this embodiment). D2 / D is, for example, 0.10 to 0.70, and preferably 0.10 to 0.50. If these values ​​are too small, the ejection member 16 is more likely to interfere with the second split mold 12, while if these values ​​are too large, the ability to separate the burrs 5 may be impaired. Specific examples of D1 / D are 0.05, 0.10, 0.15, 0.20, 0.25, 0.30, 0.35, 0.40, 0.45, and 0.50, and may be in a range between any two of the values ​​exemplified here or less than any of them. Specifically, D2 / D is, for example, 0.10, 0.15, 0.20, 0.25, 0.30, 0.35, 0.40, 0.45, 0.50, 0.55, 0.60, 0.65, or 0.70, and may be a value between any two of the values ​​exemplified here or less. The protruding member may be disposed at the center of the groove-shaped recess 12e in the width direction as shown in FIG. 7B, or may be disposed within the groove-shaped recess 12e at a position closer to the pinch-off portion 14 as shown in FIG. 11. In the latter case, D2 / D becomes a value smaller than 0.50.

[0035] As shown in FIG. 6C , the groove-shaped recess 12e includes an outer side surface 12h extending from the burr clamp portion 18 toward the bottom of the groove-shaped recess 12e. The outer side surface 12h preferably has a first portion 12h1 whose inclination angle with respect to the reference plane 19 is 60 degrees or less. Providing such a portion on the outer side surface 12h prevents the broken burr 5 from getting stuck in the groove-shaped recess 12e and becoming difficult to remove. The angle of the first portion 12h1 is, for example, 15 to 60 degrees, preferably 20 to 55 degrees, and more preferably 25 to 50 degrees (45 degrees in this embodiment). This value may be, for example, 15, 20, 25, 30, 35, 40, 45, 50, 55, or 60 degrees, or may be within a range between or equal to any two of the values ​​exemplified here.

[0036] The first portion 12h1 is preferably provided at a position shallower than the center of the depth direction of the groove-shaped recess 12e, and more preferably provided so as to be contiguous with the burr clamp portion 18. The projected width of the first portion 12h1 is, for example, 1 to 20 mm, and preferably 3 to 10 mm. If this value is too small, the effect of providing the first portion 12h1 may not be fully exerted. If this value is too large, the second split mold 12 is likely to interfere with the ejection member 16. Specific examples of this value are 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, and 20 mm, and may be within a range between any two of the values ​​exemplified here.

[0037] The outer side surface 12h has a second portion 12h2 located farther from the burr clamp portion 18 than the first portion 12h1. The second portion 12h2 is preferably provided so as to be continuous with the first portion 12h1. The second portion 12h2 has a larger inclination angle with respect to the reference plane 19 than the first portion 12h1 (80 degrees in this embodiment). The description of the first portion 12h1 and the second portion 12h2 is the same as the description of the first portion 12f1 and the second portion 12f2.

[0038] In molding using the molding die 1 described above, first, the parison 2 is placed between the first and second split dies 11, 12, which are in the open state as shown in Figure 1, and then the first and second split dies 11, 12 are closed in this state to form a cavity 13, and the parison 2 is molded to form the molded product 3. The portion of the parison 2 that is located inside the cavity 13 is molded into the shape of the molded product 4, and the portion that is located outside the cavity 13 becomes flash 5. The structure shown in Figure 9A is obtained by the above steps.

[0039] 2. Cooling Process As shown in FIG. 9B , in the cooling process, the burr 5 in the burr-accommodating space 15 is cooled. The burr 5 is preferably cooled by spraying a cooling medium (e.g., air) onto the burr 5. The burr 5 is also preferably cooled by spraying the cooling medium onto the burr 5 through the burr-cooling holes 12i provided in the second split mold 12. In this case, the burr 5 is cooled while being pressed against the first split mold 11 by the cooling medium. This makes it easier for the force applied by the ejection member 16 to be transmitted to the burr 5, facilitating its separation. Furthermore, it is preferable that the ejection member 16 protrude from the first split mold 11 at the time of the cooling process. In this case, when the burr 5 is pressed against the first split mold 11, the ejection member 16 easily bites into the burr 5, making it easier for the force applied by the ejection member 16 to be transmitted to the burr 5. The amount of protrusion of the ejection member 16 is, for example, 0.5 to 3 mm, preferably 1.0 to 2.0 mm. The cooling step can be omitted if not required.

[0040] 10A and 10B , in the separating step, the ejection member 16 is ejected into the burr-accommodating space 15 to separate the burr 5 from the molded product 4. In the molding die 1 of this embodiment, the inner side surface 12f of the groove-shaped recess 12e provided along the pinch-off portion 14 is provided with a first portion 12f1 having a gentle inclination of 60 degrees or less. Therefore, the burr 5 is separated from the molded product 4 through the state shown in FIGS. 10A and 10B . In this case, the burr 5 is supported by the first portion 12f1 with a relatively gentle inclination and pressed by the ejection member 16, thereby separating the burr 5 from the molded product 4. This configuration prevents the burr 5 separated from the molded product 4 from getting stuck in the groove-shaped recess 12e and becoming difficult to remove, thereby preventing a decrease in the production efficiency of the molded product 4. In the dividing step, it is preferable to divide the flash 5 over the entire circumference of the molded article 4, but it is also possible to divide the flash 5 in a portion of the outer periphery of the molded article 4. In this case, in a post-processing step after the molded article 4 and the flash 5 are removed together from the molding die 1, the undivided portion can be divided to separate the flash 5 from the molded article 4.

[0041] 1: molding die, 2: parison, 3: molded body, 4: molded product, 5: flash, 5a: thin-walled portion, 11: first split mold, 11a: split cavity surface, 11b: split cavity, 11c: ridge, 11d: guide hole, 11e: groove-like recess, 11j: connecting portion, 12: second split mold, 12a: split cavity surface, 12b: split cavity, 12c: ridge, 12e: groove-like recess, 12f: inner side surface, 12f1: first portion, 12f2: second 2 portion, 12f3: third portion, 12g: local recess, 12h: outer side surface, 12h1: first portion, 12h2: second portion, 12i: burr cooling hole, 12j: connecting portion, 12k: bottom, 13: cavity, 13a: cavity outer surface, 14: pinch-off portion, 15: burr accommodating space, 16: protruding member, 16a: tip surface, 16b: recess, 16c: tapered surface, 17: mating surface, 18: burr clamp portion, 19: reference surface, W: projected width

Claims

1. A molding die having first and second split dies which can be opened and closed, comprising a cavity, a pinch-off portion, a burr storage space, and an ejection member; the cavity is a space for molding a desired molded product, and the outer surface of the cavity is formed by the mating cavity surfaces of the first and second split dies; the pinch-off portion is provided on the mating surfaces of the first and second split dies so as to surround the cavity; the burr storage space is a space provided on the outside of the pinch-off portion and for storing burrs formed around the molded product; the first split die has a guide hole in a portion facing the burr storage space, and the ejection member is configured to be able to advance and retreat into the burr storage space through the guide hole; the second split die has a groove-like recess facing the burr storage space and provided along the pinch-off portion, and the groove-like recess has an inner side surface extending from the pinch-off portion toward the bottom of the groove-like recess, The molding die has a first portion, the inner side surface of which has an inclination angle of 60 degrees or less with respect to a reference plane perpendicular to the opening and closing direction of the first and second split dies.

2. A molding die as claimed in claim 1, wherein the inner side surface has a second portion located farther from the pinch-off portion than the first portion, and the second portion has a larger inclination angle with respect to the reference plane than the first portion.

3. A molding die as described in claim 1, wherein the inner side surface is provided with a local recess extending in the direction of movement of the ejection member at a position opposite the ejection member when the ejection member is ejected into the groove-shaped recess.

4. A molding die as described in claim 1, comprising a burr clamping portion, the burr clamping portion being provided on the mating surfaces of the first and second split dies outside the pinch-off portion, and the burr accommodating space being provided between the pinch-off portion and the burr clamping portion.

5. A molding die as described in claim 4, wherein the groove-shaped recess has an outer side extending from the burr clamp portion toward the bottom of the groove-shaped recess, and the outer side has a first portion whose inclination angle with respect to the reference plane is 60 degrees or less.

6. A method for manufacturing a molded product, comprising: a molding step; and a cutting step, wherein in the molding step, a molded body is formed by molding a parison using a molding die according to any one of claims 1 to 5, and the molded body comprises the molded product formed in the cavity and the burr connected to the periphery of the molded product, and in the cutting step, the burr is cut off from the molded product by protruding the ejection member into the burr storage space.

7. A molding die having first and second split dies which can be opened and closed, comprising a cavity, a pinch-off portion, a burr storage space, and an ejection member, wherein the cavity is a space for molding a desired molded product, and the outer surface of the cavity is formed by the mating cavity surfaces of the first and second split dies, the pinch-off portion is provided on the mating surfaces of the first and second split dies so as to surround the cavity, the burr storage space is a space provided outside the pinch-off portion and for storing burrs formed around the molded product, the first split die has a guide hole in a portion facing the burr storage space, and the ejection member is configured to be able to advance and retreat into the burr storage space through the guide hole, the second split die has a groove-like recess facing the burr storage space and provided along the pinch-off portion, the groove-like recess has an inner side surface extending from the pinch-off portion toward the bottom of the groove-like recess, and the inner side surface has first and second portions, A molding die, wherein the second portion is located farther from the pinch-off portion than the first portion, and has a larger inclination angle with respect to a reference plane perpendicular to the opening and closing direction of the first and second split dies than the first portion.

8. A molding die having first and second split dies which can be opened and closed, comprising a cavity, a pinch-off portion, a burr storage space, and an ejection member, wherein the cavity is a space for molding a desired molded product, and the outer surface of the cavity is formed by the mating cavity surfaces of the first and second split dies, the pinch-off portion is provided on the mating surfaces of the first and second split dies so as to surround the cavity, the burr storage space is a space provided outside the pinch-off portion and for storing burrs formed around the molded product, the first split die has a guide hole in a portion facing the burr storage space, and the ejection member is configured to be able to advance and retreat into the burr storage space through the guide hole, the second split die has a groove-like recess facing the burr storage space and provided along the pinch-off portion, and the groove-like recess has an inner side surface extending from the pinch-off portion toward the bottom of the groove-like recess, The molding die has a local recess on the inner side surface, the local recess extending along the advancing / retreating direction of the ejection member at a position facing the ejection member when the ejection member is ejected into the groove-shaped recess.

Citation Information

Patent Citations

  • Blow mold and blow molding method

    JP2007276125A

  • Blow mold and blow molding method

    JP2010274528A

  • Method for manufacturing molded body, die for molding and apparatus for manufacturing molded body

    JP2019104237A

  • Production method of inner fitting component, production method of intermediate component for inner fitting component, mold, intermediate component and cutting blade

    JP2019155605A