Systems and methods for preparing alkali-ion secondary batteries
Patent Information
- Application Number
- PCT/US2025/030375
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-21
- Filing Date
- 2025-05-21
- Publication Date
- 2026-11-12
AI Technical Summary
Conventional alkali-ion battery manufacturing processes are complex, time-sensitive, and expensive, involving multiple steps that require immediate sequential execution within a dedicated manufacturing plant, leading to high capital costs and safety challenges.
A method for assembling alkali-ion batteries that allows for cell subassemblies to be prepared at a neutral voltage, transported to a remote activation location, and activated by charging and discharging protocols, eliminating steps like tap charge, formation, and degassing, and enabling assembly and storage without electrolyte wetting, thus decoupling these processes from the manufacturing plant.
This approach simplifies battery assembly, reduces capital expenditure, and enhances safety by allowing assembly and activation at the deployment site, reducing manufacturing complexity and costs while ensuring stable and corrosion-free operation.
Smart Images

Figure US2025030375_12112026_PF_FP_ABST
Abstract
Description
Attorney Docket No.: 104986-201 SYSTEMS AND METHODS FOR PREPARING ALKALI-ION SECONDARY BATTERIESCROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims the benefit of U.S. Provisional Patent ApplicationNos. 63 / 650,138. filed May 21, 2024, and 63 / 809.477, filed May 21, 2025, which are incorporated by reference as if disclosed herein in their entireties.STATEMENT REGARDING FEDERALLY SPONSORED RESEARCH AND DEVELOPMENT
[0002] This invention was made with government support under DE-AR0001605 awarded by the U.S. Department of Energy'. The government has certain rights in the invention.BACKGROUND
[0003] Alkali-ion battery cell manufacturing is time and capital intensive. Typical manufacturing processes for alkali-ion batteries begin with cell subassemblies being filled with electrolyte, where the cell may begin to experience the copper dissolution corrosion reaction. Then, the cell is charged to a voltage where the copper dissolution is stopped with a “formation’" protocol managed by a series of power electronics, a finishing step to stabilize / passivate cells after they are mechanically assembled. The electrolyte is then allowed to soak within the cell in an aging process that may take 1-2 weeks. The cell is then activated by a series of charging and discharging protocols using an additional set of power electronics. Finally, optional removal of byproduct streams such as gas generated in the previous step(s) is performed. These steps can be repeated before the cell is tested and graded and assembled into a pack, e.g., with multiple connected cells. The pack can then be deployed into a grid-connected battery' product.
[0004] Such production steps for alkali-ion battery cell manufacturing are completed consecutively to prevent corrosion of internal components. As a result, all steps are performed within a single dedicated manufacturing plant environment, where the time-sensitive electrolyte filling and subsequent charging steps are completed in immediate succession.
[0005] Finally, battery cell manufacturing projects are difficult to fund due to high capital costs, 37% of which are for the power electronics used for the formation protocol. In lithium-ion systems, a separate set of power electronics is used to perform a “tap charge,” an initial charging step that brings cells from 0V to 2V to prevent copper corrosion and improve cell yields, performed immediately after cell assembly to minimize corrosion. Moreover, the transportationAttorney Docket No.: 104986-201 of energized cells, and their integration into higher voltage battery packs are regulated by stringent safety standards. Thus, conventional alkali-ion batery cell manufacturing processes are disadvantageously complex, time-sensitive, and expensive, hampering the pace of w idespread adoption thereof.SUMMARY
[0006] Aspects of the present disclosure are directed to a process that simplifies the cell assembly and finishing production process for alkali-ion bateries. In some embodiments, the alkali-ion bateries, e.g., Na-ion batery or K-ion batery, are safely and stably held at neutral voltages while minimizing or preventing corrosion of internal components. Further, the alkali-ion bateries can be assembled and stored without performing electrolyte weting, tap charge, formation, aging, and / or degassing steps at the assembly / storage location. To the extent these steps are desired, they can instead be performed at the deployment site of the alkali-ion batteries itself, remove from the assembly / storage location.
[0007] Aspects of the present disclosure are directed to a method of deploying an alkali-ion batery pack including preparing, at a preparation location, an alkali-ion cell subassembly including a positive electrode and a negative electrode; transporting the alkali-ion cell subassembly to an activation location remote from the preparation location, wherein the alkali-ion cell subassembly is transported at 0V; and activating the alkali-ion cell subassembly at the activation location by a series of charging and discharging protocols. In some embodiments, the method includes filling the alkali-ion cell subassembly with one or more electrolytes. In some embodiments, the method includes assembling, at the activation location, a plurality of alkali-ion cell subassemblies to produce an alkali-ion batery pack. In some embodiments, the method includes removing one or more byproduct streams produced while activating the alkali-ion cell subassembly at the activation location, wherein the byproduct stream includes one or more gases. In some embodiments, the activation location is a deployment location for the alkali-ion batery pack. In some embodiments, preparing an alkali-ion cell subassembly does not include any of: a tap charge process; a formation process; an aging process: and a degassing process.
[0008] In some embodiments, the electrolyte includes an Na+-based electrolyte, K+-based electrolyte, or combinations thereof. In some embodiments, the electrolyte includes NaPF6, FSI:PF6, or combinations thereof. In some embodiments, the positive electrode includes a sodium-ion material, a potassium-ion material, or combinations thereof. In some embodiments, the positive electrode includes NaNii / sFei.sMnt / sCh, NasV2(PO4)3, or combinations thereof. In some embodiments, the negative electrode includes hard carbon. In some embodiments, theAttorney Docket No.: 104986-201 alkali-ion battery pack includes an integrated power electronics system, a battery management system, or combinations thereof. In some embodiments, the alkali-ion battery pack is at least 40 kWh.
[0009] Aspects of the present disclosure are directed to a method of deploying an alkali-ion battery pack including preparing, at a preparation location, one or more alkali-ion cell subassemblies having 0V; transporting the one or more alkali-ion cell subassemblies at 0V to an activation location remote from the preparation location; activating the one or more alkali-ion cell subassemblies by a series of charging and discharging protocols; and deploying the one or more alkali-ion cell subassemblies at a deployment location. In some embodiments, none of the following processes occur prior to or during transporting the one or more alkali-ion cell subassemblies at 0V to an activation location remote from the preparation location: a tap charge process; a formation process; an aging process; and a degassing process. In some embodiments, the alkali-ion cell subassemblies include a positive electrode; a negative electrode; and one or more compatible electrolytes.
[0010] Aspects of the present disclosure are directed to a method of deploying an alkali-ion battery pack including providing a plurality of alkali-ion cell subassemblies at a preparation location; contacting, at the preparation location, the plurality of alkali-ion cell subassemblies with one or more compatible electrolytes at neutral (zero) voltage; transporting the plurality7of alkali-ion cell subassemblies at neutral (zero) voltage to a deployment location remote from the preparation location; assembling the plurality of alkali-ion cell subassemblies, together with an integrated power electronics system, a battery management system, or combinations thereof, to form a neutral alkali-ion battery pack; activating the neutral alkali-ion battery' pack by a series of charging and discharging protocols; removing one or more byproduct streams formed during the initial activation process, and deploying the alkali-ion battery pack. In some embodiments, none of the following processes occur prior to or during transporting the plurality7of alkali-ion cell subassemblies at neutral (zero) voltage to a deployment location remote from the preparation location: a tap charge process; a formation process; an aging process; and a degassing process. In some embodiments, alkali-ion cell subassemblies include a positive electrode including a sodium-ion material, a potassium-ion material, or combinations thereof and a negative electrode including hard carbon. In some embodiments, the compatible electrolytes include an Na+-based electrolyte, K+-based electrolyte, or combinations thereof.Attorney Docket No.: 104986-201 BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The drawings show embodiments of the disclosed subject matter for the purpose of illustrating the invention. However, it should be understood that the present application is not limited to the precise arrangements and instrumentalities shown in the drawings, wherein:
[0012] FIG. 1 is a chart of a method of deploying an alkali-ion battery pack according to some embodiments of the present disclosure;
[0013] FIG. 2 is a chart of a method of deploying an alkali-ion battery pack according to some embodiments of the present disclosure;
[0014] FIGs. 3A-3C are graphs portraying data validating neutral (0V) wetting and aging of Na+-ion cells according to embodiments of the present disclosure and conventional Li'-ion cells; and
[0015] FIGs. 4A-4B are graphs portraying data demonstrating improved utilization of alkali-ion cell subassemblies with increased electrolyte wetting times consistent with embodiments of the present disclosure.DETAILED DESCRIPTION
[0016] Referring now to FIG. 1, some embodiments of the present disclosure are directed to a method 100 of deploying an alkali-ion battery7pack. In some embodiments, at 102, one or more alkali-ion cell subassemblies are prepared. In some embodiments, the alkali-ion cell subassemblies are prepared 102 at a preparation location. In some embodiments, the preparation location is any suitable location to prepare and assemble the components of the alkali-ion cell subassembly. In some embodiments, the preparation location is an alkali-ion battery7manufacturing facility7. In some embodiments, the preparation location is an alkali-ion battery¬ manufacturer’s storage facility.
[0017] In some embodiments, the alkali-ion cell subassemblies include a positive electrode and a negative electrode. As used herein, the term “positive electrode” refers to an electrode of the alkali-ion cell subassembly / battery pack that functions as a cathode during discharge and as an anode during charging. Further, the term “negative electrode” herein refers to an electrode of the alkali-ion cell subassembly / battery pack that functions as an anode during discharge and as a cathode during charging. In some embodiments, the electrodes have a thickness greater than about 0.2mm, 0.25mm, 0.3mm, 0.35mm, 0.4mm, 0.45mm, 0.5mm, 0.55mm, 0.6mm, 0.65mm, 0.7mm. 0.75mm. 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1.0mm, etc.Attorney Docket No.: 104986-201
[0018] Referring again to FIG. 1, in some embodiments, the alkali-ion cell subassemblies include one or more compatible electrolytes. In some embodiments, the electrolytes are contacted with the positive and / or negative electrode via an electrolyte wetting process. As used herein, the term "electrolyte wetting process” refers to a step in the production of the alkali-ion cell subassembly / battery pack where at least one of the positive and negative electrodes are contacted with the electrolyte. In some embodiments, the alkali-ion cell subassemblies include one or more separators. In some embodiments, the separators include a ceramic coating.
[0019] In some embodiments, the positive electrode includes a sodium-ion material, a potassium-ion material, or combinations thereof. In some embodiments, the positive electrode includes NaNii / 3Fei.3Mm / 3O2, NasV2(PO4)3, or combinations thereof. In some embodiments, the negative electrode includes carbon. In some embodiments, the negative electrode includes hard carbon. In some embodiments, the electrolyte includes an Na+-based electrolyte, K+-based electrolyte, or combinations thereof. In some embodiments, the electrolyte includes a dual-salt electrolyte. In some embodiments, the electrolyte includes NaPF6, FSI:PF6, or combinations thereof.
[0020] In some embodiments, at the preparation location, the one or more alkali-ion cell subassemblies are prepared 102 at 0V.
[0021] Referring now to FIG. 1, at 104, the alkali-ion cell subassembly is transported to an activation location. In some embodiments, the alkali-ion cell subassembly is transported 104 from the preparation location to the activation location. In some embodiments the activation location is remote from the preparation location. In some embodiments, the alkali-ion cell subassembly is transported 104 to the activation location remote from the preparation location at OV.
[0022] In some embodiments, at 106, a plurality of alkali-ion cell subassemblies are assembled together. In some embodiments, assembly 106 produces an alkali-ion battery pack. In some embodiments, assembly 106 occurs after transport 104, i.e., at the activation location. In some embodiments, the plurality of alkali-ion cell subassemblies are assembled prior to transportation to the activation location (not pictured), e.g., while preparing 102. In some embodiments, the alkali-ion battery pack includes an integrated power electronics system, a battery management system, or combinations thereof.
[0023] Referring again to FIG. 1, at 108, the one or more alkali-ion cell subassemblies are activated. In some embodiments, the subassemblies are activated 108 by a series of charging andAttorney Docket No.: 104986-201 discharging protocols. In some embodiments, at 110. one or more byproduct streams produced while activating the alkali-ion cell subassemblies at the activation location are removed. In some embodiments, byproduct stream includes one or more gases. In some embodiments, at 112, the one or more alkali-ion cell subassemblies are deployed at a deployment location. In some embodiments, the activation location is the deployment location for the alkali-ion cell subassemblies, e.g., as an alkali-ion battery. In some embodiments, the alkali-ion batter}’ pack is at least 10 kWh, 15 kWh, 20 kWh, 25 kWh, 30 kWh, 35 kWh, etc. In some embodiments, the alkali-ion battery pack is at least 40 kWh.
[0024] Advantageously, the alkali-ion cell subassemblies / battery packs assembled via method 100 and according to other embodiments of the present disclosure are neutral and safe. As the alkali-ion cell subassemblies / alkali-ion battery' packs are at zero volts during providing 102, there is no time constraint on processing, and there are also no electrical hazards associated with their handling. In some embodiments, the alkali-ion cell subassemblies / battery packs consistent with embodiments of the present disclosure allow for storage, transportation, installation, and disassembly in an entirely de-energized 0V state. Embodiments of the present disclosure can be held at neutral voltages without corrosion of internal components. Exemplary alkali-ion batteries according to the present disclosure such as sodium-ion and potassium-ion systems can use aluminum current collectors on the anode and do not corrode or have at least minimal corrosion when the cell potential is in the range of -0.1 to 1 volts. In contrast, for lithium-ion batteries that use copper foils for anode current collectors, the copper will undergo dissolution corrosion reactions when the cell voltage is lower than the operating range of 2-4 volts. The neutral voltage stability and lack of time sensitivity allows for the electrolyte wetting process in the alkali-ion cell manufacturing to occur more thoroughly and uniformly, which removes a constraint on the overall individual size of each cell design.
[0025] Additionally, transportation 104. assembly 106, activation 108, degassing 110, etc., or combinations thereof can be performed remote from where providing 102 is performed. In some embodiments, transportation 104, assembly 106, activation 108, degassing 110, etc. are performed outside of the typical manufacturing plant environment, e.g.. in the field where the grid-connected battery deployment 112 takes place.
[0026] Thus, in some embodiments, battery formation is entirely decoupled from cell assembly operations. Embodiments of the present disclosure can be stored safely and indefinitely at 0V without fear of copper corrosion. As such, in some embodiments, preparing 102 an alkali-ion cell subassembly does not include an electrolyte wetting process; a tap charge process; aAttorney Docket No.: 104986-201 formation process; an aging process; a degassing process; or combinations thereof. In some embodiments, alkali-ion cell subassemblies / battery packs do not undergo an electrolyte wetting process; a tap charge process; a formation process; an aging process; a degassing process; or combinations thereof, until after transportation 104 to the activation location. In some embodiments, none of the following processes occur at the preparation location during method 100: an electrolyte wetting process; a tap charge process; a formation process; an aging process; and a degassing process. In some embodiments, none of the following processes occur at the preparation location during method 100: a tap charge process; a formation process; an aging process; and a degassing process. In some embodiments, the battery pack enables formation and degassing operations at the end-user facility, saving cell manufacturers enormously on capex.
[0027] Referring now to FIG. 2, some embodiments of the present disclosure are directed to a method 200 of deploying an alkali-ion battery pack. In some embodiments, at 202. a plurality of alkali-ion cell subassemblies are provided at a preparation location. As discussed above, in some embodiments, the alkali-ion cell subassemblies include a positive electrode including a sodium-ion material, a potassium-ion material, or combinations thereof. In some embodiments, the positive electrode includes NaNii / 3Fei.3Mni / 3O2. NasV2(PO4)3, or combinations thereof. In some embodiments, the alkali-ion cell subassemblies include a negative electrode including carbon. In some embodiments, the negative electrode includes hard carbon.
[0028] In some embodiments, at 204, the plurality of alkali-ion cell subassemblies is contacted at the preparation location with one or more compatible electrolytes. In some embodiments, the compatible electrolytes include an Na+-based electrolyte, K~ -based electrolyte, or combinations thereof. In some embodiments, the electrolyte includes a dual-salt electrolyte. In some embodiments, the electrolyte includes NaPF6, FSI:PF6, or combinations thereof. In some embodiments, during contacting 204, the alkali-ion cell subassemblies are filled with one or more electrolytes. In some embodiments, contacting 204 occurs at neutral (zero) voltage. In some embodiments, contacting 204 occurs for more than about 24 hours, 48 hours, 72 hours, 96 hours, 100 hours. 200 hours, 300 hours, 400 hours, 500 hours, 600 hours, 700 hours, 800 hours, 900 hours. 1,000 hours, etc.
[0029] Still referring to FIG. 2, in some embodiments, at 206, the plurality of alkali-ion cell subassemblies are transported at neutral (zero) voltage to a location remote from the preparation location. In some embodiments, the location is an activation location. In some embodiments, the location is a deployment location. In some embodiments, the activation location for theAttorney Docket No.: 104986-201 alkali-ion batery pack is the same as the deployment location. In some embodiments, at 208, the plurality of alkali-ion cell subassemblies are assembled at the activation location to form a neutral alkali-ion batery pack. In some embodiments, the plurality7of alkali-ion cell subassemblies are assembled 208 with an integrated power electronics system, a batery7management system, or combinations thereof to form the neutral alkali-ion batery pack.
[0030] In some embodiments, at 210, the neutral alkali-ion batery pack is activated by a series of charging and discharging protocols. In some embodiments, at 212, one or more byproduct streams formed during the initial activation process are removed. In some embodiments, at 214, the alkali-ion batery pack is deployed, e.g., at a deployment location. As discussed above, in some embodiments, none of the following processes occur prior to or during transporting 206: a tap charge process; a formation process; an aging process; and a degassing process. In some embodiments, none of the following processes occur at the preparation location: a tap charge process; a formation process; an aging process; and a degassing process.EXAMPLES
[0031] Referring now to FIGs. 3A-3C, capacity retention characteristics for Na+-ion cells according to embodiments of the present disclosure and conventional Li’-ion cells were demonstrated. Bateries of each type were stored at 0V for 1 week. The Na+-ion cells retained substantially full capacity7after 1 week of 0V storage (FIG. 3A), while the Li’-ion cells exhibited a 5-15% capacity drop (FIG. 3B). Referring specifically to FIG. 3C, copper dissolution, e.g., resulting from 0V storage of Li’-ion cells, can cause complete soft short circuiting in those cells.
[0032] Referring now to FIG. 4A, a full cell Na+-ion batery was prepared using a 150pm NaNii / 3Fei.3Mm / 3O2 electrode. 320pm hard carbon electrode, and about 5.5 mAh / cm2areal capacity. IM NaPFe EC:DMC was used as the electrolyte. The electrodes were soaked in the electrolyte to determine the effect of electrolyte filling (weting) on batery capacity' and cycle life. 3 C / 10 formation cy cles and 5 C / 5 formation cycles were performed at 45°C. C / 5 continuous cycling was performed at 45°C. When comparing 24 hour soak times with 96 hour soak times at 0V, the longer soak times resulted in 28% more accessible capacity (82 mAh / g compared to 64 mAh / g). The longer soak times also provided more stable cycling, with 88.2% capacity7retention compared with 25.3% across 350 cycles. Referring specifically to FIG. 4B, increasing the soaking time to 300 hours accessed more than twice the discharge capacity7relative to a 100 hour soaking time in comparable pouch cells.Attorney Docket No.: 104986-201
[0033] Systems and methods of the present disclosure represent marked improvements in batten¬ assembly and deployment, simplifying these processes and minimizing minerals and manufacturing, e.g., with Na-ion batteries. The methods of the present disclosure enable formation of alkali-ion batteries spatially and / or temporally separated from the battery cell mechanical assembly process. Such methods can eliminate a series of redundant power-electronic equipment and charge-discharge formation protocols by consolidating the process at the point of grid deployment instead of earlier in the cell manufacturing plant. Thus, embodiments of the present disclosure can be used in “direct pack deployment,” with alkali-ion cell subassembly and / or full alkali-ion batteries assembled into a pack architecture that can be discharged to 0V, shipped, and activated directly in the field while avoiding deleterious effects on performance or reliability. This contrasts with standard Li-ion cells and manufacturing processes that form cells individually directly after cell assembly (before pack construction), with corresponding disadvantageous increases in manufacturing complexity, storage and transportation complications, and cost. Without wishing to be bound by theory, methods according to the present disclosure can save 37% of cell manufacturing plant capital costs, as well as 46% of the overall cell manufacturing plant footprint.
[0034] Additionally, the stability of Na-ion systems at neutral 0V and spatially and temporally decoupled Na-ion gigafactory design enable further capex savings by facilitating ultra-large-format cell form factors with thicker electrodes. Larger cells lead to simpler multi-cell pack designs and improve the cost and efficiency of grid connected alkali-ion batteries. The pack design also considerably simplifies safety logistics, as cells at 0V are electrochemically inert and present low or virtually zero fire risk.
[0035] Although the invention has been described and illustrated with respect to exemplary- embodiments thereof, it should be understood by those skilled in the art that the foregoing and various other changes, omissions and additions may be made therein and thereto, without parting from the spirit and scope of the present invention.
Claims
Attorney Docket No.: 104986-201CLAIMSWhat is claimed is:
1. A method of deploying an alkali-ion battery pack, comprising:at a preparation location, preparing an alkali-ion cell subassembly including a positive electrode and a negative electrode;transporting the alkali-ion cell subassembly to an activation location remote from the preparation location, wherein the alkali-ion cell subassembly is transported at 0V; andactivating the alkali-ion cell subassembly at the activation location by a series of charging and discharging protocols.
2. The method according to claim 1, further comprising:filling the alkali-ion cell subassembly with one or more electrolytes.
3. The method according to claim 2, wherein the electrolyte includes an Na+-based electrolyte, K+-based electrolyte, or combinations thereof.
4. The method according to claim 3, wherein the electrolyte includes NaPF6. FSI:PF6, or combinations thereof.
5. The method according to claim 1, wherein the positive electrode includes a sodium-ion material, a potassium-ion material, or combinations thereof.
6. The method according to claim 5, wherein the positive electrode includes NaNii / 3Fei.3Mni / 3C>2, Na3V2(PO4)3. or combinations thereof.
7. The method according to claim 1, wherein the negative electrode includes hard carbon.
8. The method according to claim 1, wherein the activation location is a deployment location for the alkali-ion battery pack.
9. The method according to claim 1, wherein the alkali-ion battery7pack includes an integrated power electronics system, a battery management system, or combinations thereof.Attorney Docket No.: 104986-201 10. The method according to claim 1, further comprising removing one or more byproduct streams produced while activating the alkali-ion cell subassembly at the activation location, wherein the byproduct stream includes one or more gases.
11. The method according to claim 1, further comprising:at the activation location, assembling a plurality of alkali-ion cell subassemblies to produce an alkali-ion battery pack.
12. The method according to claim 1, wherein the alkali-ion battery pack is at least 40 kWh.
13. The method according to claim 1, wherein preparing an alkali-ion cell subassembly does not include any of:a tap charge process;a formation process;an aging process; anda degassing process.
14. A method of deploying an alkali-ion battery pack, comprising:at a preparation location, preparing one or more alkali-ion cell subassemblies having 0V, wherein the alkali-ion cell subassemblies include:a positive electrode;a negative electrode; andone or more compatible electrolytes,transporting the one or more alkali-ion cell subassemblies at 0V to an activation location remote from the preparation location;activating the one or more alkali-ion cell subassemblies by a series of charging and discharging protocols; anddeploying the one or more alkali-ion cell subassemblies at a deployment location.
15. The method according to claim 14, wherein:Attorney Docket No.: 104986-201 the positive electrode includes a sodium-ion material, a potassium-ion material, or combinations thereof, andthe electrolyte includes an Na+-based electrolyte. K+-based electrolyte, or combinations thereof.
16. The method according to claim 15, wherein the positive electrode includes NaNii / 3Fei.3Mni / 3C>2, Na3V2(PO4)3. or combinations thereof.
17. The method according to claim 14, further comprising:at the activation location, assembling a plurality of alkali-ion cell subassemblies to produce an alkali-ion battery pack.
18. The method according to claim 14, wherein none of the following processes occur prior to or during transporting the one or more alkali-ion cell subassemblies at 0V to an activation location remote from the preparation location:a tap charge process;a formation process;an aging process; anda degassing process.
19. A method of deploying an alkali-ion battery pack, comprising:providing a plurality of alkali-ion cell subassemblies at a preparation location, wherein the alkali-ion cell subassemblies include:a positive electrode including a sodium-ion material, a potassium-ion material, or combinations thereof, anda negative electrode including hard carbon,at the preparation location, contacting the plurality of alkali-ion cell subassemblies with one or more compatible electrolytes at neutral (zero) voltage, wherein the compatible electrolytes include an Na+-based electrolyte, K+-based electrolyte, or combinations thereof;Attorney Docket No.: 104986-201 transporting the plurality of alkali-ion cell subassemblies at neutral (zero) voltage to a deployment location remote from the preparation location;assembling the plurality of alkali-ion cell subassemblies, together with an integrated power electronics system, a battery management system, or combinations thereof, to form a neutral alkali-ion battery pack;activating the neutral alkali-ion battery pack by a series of charging and discharging protocols;removing one or more byproduct streams formed during the initial activation process, anddeploying the alkali-ion battery pack.
20. The method according to claim 19. wherein none of the following processes occur prior to or during transporting the plurality of alkali-ion cell subassemblies at neutral (zero) voltage to a deployment location remote from the preparation location:a tap charge process;a formation process;an aging process; anda degassing process.