Display panel and manufacturing method therefor, and display apparatus

By introducing a partition area design and an undercut structure into the display panel, the isolation pillars surround the opening area and interrupt the light-emitting layer. Combined with a multi-layer encapsulation layer, the problems of water, oxygen, and electrochemical corrosion caused by the openings in the screen are solved, thus protecting the light-emitting devices and improving the reliability of the display panel.

WO2026232462A1PCT designated stage Publication Date: 2026-11-12BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2025/093671
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2025-05-09
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

In the prior art, the laser cutting process at the opening in the display panel exposes the light-emitting material and cathode, forming channels for water, oxygen and electrochemical corrosion, causing the light-emitting devices in the display area to fail and black spots to appear.

Method used

The design employs a partitioned area, including isolation pillars and an undercut structure. The isolation pillars surround the opening area, and the light-emitting layer is interrupted at the location of the isolation pillars. Combined with multiple encapsulation layers, it prevents water, oxygen, and electrochemical corrosion of the channels.

Benefits of technology

It effectively blocks the channels of water, oxygen, and electrochemical corrosion, preventing the failure of light-emitting devices and improving the service life and reliability of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2025093671_12112026_PF_FP_ABST
    Figure CN2025093671_12112026_PF_FP_ABST
Patent Text Reader

Abstract

The present disclosure pertains to the technical field of display, and provides a display panel and a manufacturing method therefor, and a display apparatus. The display panel of the present disclosure is provided with a display region, a partition region, and an opening region, the partition region being located between the display region and the opening region. The display panel comprises a base substrate, and a second planarization layer, a third conductive layer, a light-emitting layer, and an electrode layer sequentially disposed along a direction of the base substrate. The third conductive layer comprises a plurality of isolation pillars located in the partition region, and the isolation pillars surround the opening region. The second planarization layer is provided with a first groove, and an orthographic projection of a side edge of at least one isolation pillar on the base substrate falls within an orthographic projection of the first groove on the base substrate. The first groove and the isolation pillar form an undercut structure configured to disconnect a portion of the electrode layer falling within the first groove. The light-emitting layer extends from the display region to the partition region, and is interrupted at least at the position of each isolation pillar.
Need to check novelty before this filing date? Find Prior Art

Description

Display panel and its manufacturing method, display device Technical Field

[0001] This disclosure belongs to the field of display technology, specifically relating to a display panel and its manufacturing method, and a display device. Background Technology

[0002] To meet users' demands for high screen-to-body ratio and high transmittance in display panels, in-screen aperture (AA Hole) and slotting techniques are typically used, which involves laser cutting away the area where the camera hole would be located. However, this process often results in the light-emitting material and cathode being exposed to air at the cross-section, creating a channel for water, oxygen, and electrochemical corrosion. This can cause the light-emitting devices in the display area to fail and form black spots. Summary of the Invention

[0003] This disclosure aims to at least solve one of the technical problems existing in the prior art, and to provide a display panel and its manufacturing method, as well as a display device.

[0004] In a first aspect, the technical solution adopted to solve the technical problem of this disclosure is a display panel having a display area, a partition area and an opening area, wherein the partition area is located between the display area and the opening area; the display panel includes a substrate and a second planarization layer, a third conductive layer, a light-emitting layer and an electrode layer sequentially disposed along the direction of the substrate.

[0005] The third conductive layer includes a plurality of isolation pillars located in the isolation region, the isolation pillars surrounding the opening region; the second planar layer has a first groove, and the orthographic projection of one side edge of at least one of the isolation pillars on the substrate falls into the orthographic projection of the first groove on the substrate; the first groove and the isolation pillars form an undercut structure for isolating the electrode layer falling into the first groove.

[0006] The light-emitting layer extends from the display area to the partition area and is interrupted at least at the location of each of the partition pillars.

[0007] In some embodiments, the partition area includes a first partition area and a second partition area; the second partition area surrounds the opening area, and the first partition area surrounds the second partition area;

[0008] The plurality of isolation columns include at least one first isolation column located in the first partition area and at least one second isolation column located in the second partition area;

[0009] The first groove is located in the first partition region, and a side edge of the first isolation column falls within a projection of the first groove on the substrate.

[0010] In some embodiments, the display panel further comprises a third planar layer disposed on a side of the third conductive layer close to the light-emitting layer; the third planar layer comprises a first planar portion located in the display region and a first blocking portion located in the second partition region.

[0011] The third planar layer exposes the first isolation column, the first groove and the second isolation column in a middle region between the first planar portion and the first blocking portion.

[0012] In some embodiments, the second planar layer comprises a second planar portion extending from the display region to the first partition region and a second blocking portion located in the second partition region.

[0013] The second planar portion and the second isolation column closest to the first partition region define a second groove disposed on the substrate.

[0014] In some embodiments, the first partition region is provided with a plurality of first isolation columns; two adjacent first isolation columns define a slot and communicate with the first groove.

[0015] In some embodiments, the first partition region is provided with at least three first isolation columns, and two adjacent first isolation columns correspond to one first groove.

[0016] In some embodiments, a surface of each first isolation column away from the substrate is flush.

[0017] In some embodiments, the display panel further comprises a plurality of first redundant traces located in the first partition region and surrounding the aperture region respectively.

[0018] The first redundant traces are one-to-one corresponding to the first isolation columns, and a projection of the first isolation column on the substrate and a projection of the first redundant trace corresponding thereto on the substrate overlap.

[0019] In some embodiments, the display panel further comprises a second conductive layer, a first planar layer and a first conductive layer disposed in sequence on a side of the second planar layer away from the third conductive layer.

[0020] The plurality of first redundant traces are located in the first conductive layer or the second conductive layer.

[0021] In some embodiments, the material of the third planar layer, the second planar layer and the first planar layer is an organic insulating material.

[0022] In some embodiments, the third conductive layer further comprises a plurality of signal lines located in the display area and at least one second redundant trace located in the first partition area;

[0023] Part of the signal lines near the aperture area semi-surround the aperture area; the second redundant trace surrounds the aperture area, and the second redundant trace is multiplexed as the first partition column.

[0024] In some embodiments, the third conductive layer further comprises a plurality of third redundant traces located in the display area and in the first partition area;

[0025] The third redundant trace surrounds the aperture area, and the third redundant trace is multiplexed as the first partition column.

[0026] In some embodiments, the partition area comprises a first partition area and a second partition area; the second partition area surrounds the aperture area, and the first partition area surrounds the second partition area;

[0027] The plurality of partition columns comprises at least one third partition column located in the second partition area;

[0028] The first groove is located in the second partition area, and a side edge of the third partition column falls within the orthogonal projection of the first groove on the substrate substrate; the first groove and the third partition column form an undercut structure for partitioning the electrode layer falling into the first groove.

[0029] In some embodiments, the display panel further comprises a third planar layer arranged on the side of the third conductive layer close to the light-emitting layer; the third planar layer comprises a first planar portion extending from the display area to the first partition area and a first blocking portion located in the second partition area;

[0030] The third planar layer exposes the third partition column and the first groove in the intermediate region between the first planar portion and the first blocking portion.

[0031] In some embodiments, the display panel further comprises a blocking dam located in the second partition area;

[0032] The third partition column comprises a plurality of third partition columns, and each third partition column is located on the side of the blocking dam close to the display area; adjacent two third partition columns define a slot and communicate with the first groove.

[0033] In some embodiments, the display panel further comprises a blocking dam located at the second partition region;

[0034] The third isolation columns comprise a plurality of columns and are distributed on both sides of the blocking dam close to and away from the display region.

[0035] In some embodiments, for the plurality of third isolation columns located on one side of the blocking dam close to the display region, a slot is defined between two adjacent third isolation columns and communicates with a corresponding first groove.

[0036] For the plurality of third isolation columns located on one side of the blocking dam away from the display region, at least one group of two adjacent third isolation columns defines a slot and communicates with a corresponding first groove.

[0037] In some embodiments, the orthographic projection of two adjacent third isolation columns on the substrate substrate covers the orthographic projection of the part of the second planar layer used to form the first groove on the substrate substrate.

[0038] The side of the third isolation column away from the slot wraps around the edge of the part of the second planar layer used to form the first groove away from the first groove.

[0039] In some embodiments, the display panel further comprises an encapsulation layer arranged on the side of the electrode layer away from the light-emitting layer.

[0040] The encapsulation layer extends from the display region to the partition region and covers the part exposed by the electrode layer at the position of each isolation column.

[0041] In some embodiments, the encapsulation layer comprises a first inorganic encapsulation layer, an organic encapsulation layer, and a second inorganic encapsulation layer arranged in sequence in the direction away from the substrate substrate; the first inorganic encapsulation layer and the second inorganic encapsulation layer both extend from the display region to the edge of the opening region.

[0042] The display panel further comprises a blocking dam arranged in the isolation region; the organic encapsulation layer extends from the display region to the partition region and stops at the side of the blocking dam close to the display region.

[0043] In some embodiments, the display panel further comprises a pixel definition layer and a support layer arranged in sequence on the side of the third planar layer close to the light-emitting layer.

[0044] The pixel definition layer and the support layer at least expose the isolation column of the blocking dam close to the display region.

[0045] In some embodiments, the display panel further includes a support structure located on the side of the barrier dam away from the display area; the plurality of isolation columns include at least a plurality of second isolation columns;

[0046] The support structure covers the surfaces of two adjacent second isolation pillars that are away from the substrate and fills the gap between the two adjacent second isolation pillars.

[0047] In some embodiments, the display panel further includes at least two support structures located on both sides of the barrier; the plurality of isolation columns include at least a second isolation column located on both sides of the barrier.

[0048] For any of the support structures, the support structure covers the surfaces of two adjacent second isolation pillars facing away from the substrate and fills the gap between the two adjacent second isolation pillars.

[0049] In some embodiments, the isolation pillar includes a first conductive portion, a second conductive portion, and a third conductive portion arranged sequentially along a direction away from the substrate, wherein the first conductive portion and the third conductive portion both protrude beyond the second conductive portion.

[0050] Secondly, embodiments of this disclosure also provide a method for manufacturing a display panel, used to manufacture a display panel as described in any one of the first aspects; the display panel has a display area, a partition area, and an opening area; the partition area surrounds the opening area; wherein, the manufacturing method includes:

[0051] Provide a substrate;

[0052] A second planar material layer is formed on the substrate.

[0053] A third conductive layer is formed on the side of the second planar material layer opposite to the substrate; the third conductive layer includes a plurality of isolation pillars located in the isolation region, the isolation pillars surrounding the opening region;

[0054] At least the second planar material layer is etched to form a second planar layer with a first groove; the orthographic projection of one side edge of the isolation pillar on the substrate falls within the orthographic projection of the first groove on the substrate; the first groove and the isolation pillar form an undercut structure;

[0055] A light-emitting layer and an electrode layer are sequentially formed on the side of the third conductive layer opposite to the second planar layer; the electrode layer is cut off at the location of the undercut structure; and the light-emitting layer is broken at least at the location of the isolation pillar.

[0056] In some embodiments, after the formation of the third conductive layer and before etching the second planar material layer, the method further includes:

[0057] A third flat layer is formed on the side of the third conductive layer opposite to the second flat material layer; the third flat layer exposes the isolation pillar and the first groove.

[0058] In some embodiments, at least the second planar material layer is etched to form a second planar layer having a first groove, including:

[0059] The first groove is formed by etching the surface of the second planar material layer exposed by the third planar layer and the third conductive layer in a vacuum environment using gas or plasma.

[0060] In some embodiments, the material of the second planar material layer is an organic insulating material; the gas used to etch the second planar material layer is a mixture of carbon tetrafluoride and oxygen.

[0061] Thirdly, embodiments of this disclosure also provide a display device, which includes a display panel as described in any one of the first aspects. Attached Figure Description

[0062] Figure 1 is a schematic diagram of the partition defects using the isolation column design in related technologies.

[0063] Figure 2 is a schematic diagram of the partition defects designed using isolation columns and support structures in related technologies.

[0064] Figure 3 is a plan view of the display panel in Embodiment 1 provided in this disclosure.

[0065] Figure 4 is a plan view of the signal lines and isolation pillars in each area of ​​Embodiment 1 provided in this disclosure.

[0066] Figure 5 is a cross-sectional view of a display panel in the A-A' direction according to Embodiment 1 of this disclosure.

[0067] Figure 6 is a schematic diagram of the partition effect of an undercut structure in Embodiment 1 provided by the present disclosure.

[0068] Figure 7 is a schematic diagram of the partitioning effect of the second isolation column in Embodiment 1 provided by the present disclosure.

[0069] Figure 8 is a cross-sectional view of another display panel in the A-A' direction in Embodiment 1 provided by this disclosure.

[0070] Figure 9 is a schematic diagram of the partition effect of another undercut structure in Embodiment 1 provided by the present disclosure.

[0071] Figure 10 is a schematic diagram of the encapsulation effect of the encapsulation layer in Embodiment 1 provided by the present disclosure.

[0072] Figure 11 is a schematic diagram of the support structure in Embodiment 1 provided in this disclosure.

[0073] Figure 12 is a structural diagram of the isolation column provided in an embodiment of this disclosure.

[0074] Figure 13 is a schematic diagram of the structure of the display panel of Embodiment 2 provided in this disclosure.

[0075] Figure 14 is a schematic diagram of the structure of the display panel of Embodiment 3 provided in this disclosure.

[0076] Figure 15 is a schematic diagram of the support structure in Embodiment 3 provided in this disclosure.

[0077] Figure 16 is a schematic diagram of the support structure in Embodiment 4 provided in this disclosure.

[0078] Figure 17 is a schematic diagram of the support structure in Embodiment 5 provided in this disclosure.

[0079] Figure 18 is a schematic diagram of the support structure in Embodiment 6 provided in this disclosure.

[0080] Figure 19 is a schematic diagram of the support structure in Embodiment 7 provided in this disclosure.

[0081] Figure 20 is a flowchart of a method for manufacturing a display panel according to an embodiment of this disclosure.

[0082] Figures 21a to 21d are schematic diagrams of the process for preparing the undercut structure located in the first partition region according to the embodiments of this disclosure.

[0083] Figures 22a to 22d are schematic diagrams of the process for preparing the undercut structure located in the second partition region according to the embodiments of this disclosure.

[0084] Figure 23 is a flowchart of another method for preparing a display panel according to an embodiment of this disclosure. Detailed Implementation

[0085] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions of the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this disclosure, and not all of them. The components of the embodiments of this disclosure described and shown in the accompanying drawings can generally be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of this disclosure provided in the accompanying drawings is not intended to limit the scope of the claimed disclosure, but merely represents selected embodiments of this disclosure. All other embodiments obtained by those skilled in the art based on the embodiments of this disclosure without inventive effort are within the scope of protection of this disclosure.

[0086] Unless otherwise defined, the technical or scientific terms used in this disclosure shall have the ordinary meaning understood by one of ordinary skill in the art to which this disclosure pertains. The terms “first,” “second,” and similar terms used in this disclosure do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Similarly, the terms “an,” “a,” or “the,” and similar terms do not indicate a quantity limitation, but rather indicate the presence of at least one. The terms “including,” “comprising,” or “containing,” and similar terms mean that the element or object preceding the word encompasses the elements or objects listed following the word and their equivalents, without excluding other elements or objects. The terms “connected,” “linked,” or similar terms are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. The terms “upper,” “lower,” “left,” and “right,” etc., are used only to indicate relative positional relationships, and these relative positional relationships may change accordingly when the absolute position of the described objects changes.

[0087] In this disclosure, "multiple or several" refers to two or more. "And / or" describes the relationship between related objects, indicating that three relationships can exist. For example, A and / or B can represent: A alone, A and B simultaneously, or B alone. The character " / " generally indicates that the preceding and following related objects have an "or" relationship.

[0088] In related technologies, to isolate water, oxygen, and electrochemical corrosion, a common approach is to use an isolation pillar 01 scheme, as shown in Figure 1. This involves designing several SD3 ring-shaped traces (i.e., isolation pillars 01 formed by multiple conductive layers, such as titanium / aluminum / titanium Ti / Al / Ti) near the screen aperture (AA Hole). A wet etching process is used to etch the aluminum (Al) in the titanium / aluminum / titanium (Ti / Al / Ti) layer, forming an undercut structure with a certain lateral concave depth. Afterwards, when the light-emitting layer 02 is deposited on top, the layer is interrupted at the undercut structure, preventing the formation of a continuous film and disrupting the pathway for water and oxygen corrosion, thus achieving the effect of preventing water and oxygen corrosion. The electrode layer 03 deposited on the light-emitting layer 02 will also be broken at the undercut structure. However, since the isolation pillar 01 (SD3) is made of conductive material, even if the electrode layer 03 is broken, it will still overlap with the middle layer (Al) or the lower layer (Ti) of the isolation pillar 01, forming an electrical path. Therefore, the problem of electrochemical corrosion cannot be solved.

[0089] Furthermore, the related technology also adopts a scheme of isolation pillar 01 (SD3) + support structure 04 (PDL+PS), as shown in Figure 2. That is, the support structure 04 (PDL+PS) is filled and covered between two adjacent isolation pillars (SD3), and the support structure 04 (PDL+PS) blocks the passage between the middle layer (Al) and the lower layer (Ti) of the two isolation pillars 01 (SD3). However, observation under a transmission electron microscope shows that the power-off effect of the support structure 04 (PDL+PS) is not ideal. Due to the limitations of the process conditions, the upper surface of the support structure 04 (PDL+PS) is an arc surface with a certain curvature. Therefore, there is a certain risk of overlap between the electrode layer 03 and the upper layer (Ti) of the isolation pillar 01, which forms an electrochemical corrosion channel (as shown by the dashed line), resulting in power-off failure.

[0090] Therefore, it can be seen that the power-off design of the isolation column 01 (SD3) + support structure 04 (PDL+PS) in the relevant technology cannot simultaneously isolate the water-oxygen channel and the electrochemical corrosion channel, thus affecting the service life and reliability of the display panel.

[0091] In view of this, the present disclosure provides a display panel 100. FIG3 is a planar schematic diagram of the display panel provided in the present disclosure. As shown in FIG3, the display panel 100 has a display area AA, a partition area (e.g., a first partition area BB1 and a second partition area BB2) and an opening area CC, wherein the partition area is located between the display area AA and the opening area CC. The display panel 100 includes a substrate 1, and a second planarization layer PLN2, a third conductive layer SD3, a light-emitting layer 2 and an electrode layer 3 sequentially disposed along a direction away from the substrate 1. The third conductive layer SD3 includes multiple isolation pillars (such as one or more combinations of the first isolation pillar 41, the second isolation pillar 42, and the third isolation pillar 43 described below) located in the isolation region, the isolation pillars surrounding the opening region CC; the second planarization layer PLN2 has a first groove 61, the orthographic projection of one side edge of at least one isolation pillar onto the substrate 1 falls within the orthographic projection of the first groove 61 onto the substrate 1; the first groove 61 and the isolation pillar form an undercut structure 7 for isolating the electrode layer 3 falling into the first groove 61; the light-emitting layer 2 extends from the display area AA to the isolation region, and is interrupted at least at the location of each isolation pillar. In this way, water-oxygen channels and electrochemical corrosion channels in the display panel can be isolated, preventing device failure.

[0092] For ease of understanding, the display panel of this disclosure will be described in detail below with reference to specific embodiments.

[0093] Example 1

[0094] As shown in Figure 3, the display panel 100 has a display area AA, a first partition area BB1, a second partition area BB2, and an opening area CC. The second partition area BB2 surrounds the opening area CC, and the first partition area BB1 surrounds the second partition area BB2. The opening area CC contains an in-screen opening H for placing components such as sensors and cameras. Multiple light-emitting devices are disposed within the display area AA, and the light-emitting layer 2 of each device is typically formed as a single surface within the display area AA. The first partition area BB1 and the second partition area BB2 contain partition structures to separate the light-emitting layer 2 from the electrode layer 3 (e.g., cathode) of the light-emitting devices, thereby blocking water-oxygen channels and electrochemical corrosion channels to prevent device failure.

[0095] Figure 4 is a planar schematic diagram of signal lines and isolation pillars in various regions provided in the embodiments of this disclosure; Figure 5 is a cross-sectional view of a display panel in the A-A' direction provided in the embodiments of this disclosure; Figure 6 is a schematic diagram of the isolation effect of an undercut structure provided in the embodiments of this disclosure; and Figure 7 is a schematic diagram of the isolation effect of the second isolation pillar provided in the embodiments of this disclosure. As shown in Figures 4 to 7, the display panel 100 includes a substrate 1, and a second planarization layer PLN2, a third conductive layer SD3, a light-emitting layer 2, and an electrode layer 3 sequentially disposed along a direction away from the substrate 1. The light-emitting layer 2 refers to the light-emitting material layer in the light-emitting device, and the electrode layer 3 refers to the electrode in the light-emitting device, such as a cathode. Optionally, the light-emitting layer 2 and the electrode layer 3 are both laid out across the entire display area AA. The second planarization layer PLN2 is used to planarize the underlying film layer, thereby ensuring that the film layer prepared on it can have a high flatness. The third conductive layer SD3 is a film layer used to arrange panel traces, for example, including at least one signal line (such as the third signal line 53) located in the display area AA. Furthermore, the third conductive layer SD3 is reused as a film layer for arranging isolation pillars, for example including at least one first isolation pillar 41 located in the first isolation region BB1 and at least one second isolation pillar 42 located in the second isolation region BB2. The third signal line 53 is arranged in the same layer as the isolation pillars, which is beneficial to improving the process preparation efficiency and saving costs.

[0096] At least one first isolation pillar 41 and at least one second isolation pillar 42 surround the opening area CC, thereby achieving all-round protection around the opening and preventing water and oxygen erosion and electrochemical corrosion.

[0097] The second planarization layer PLN2 has a first groove 61, which also surrounds the opening area CC. The orthographic projection of one side edge of the first isolation pillar 41 onto the substrate 1 falls within the orthographic projection of the first groove 61 onto the substrate 1. This also means that one side edge of the first isolation pillar 41 protrudes beyond the sidewall of the first groove 61, creating a discontinuity. That is, the first groove 61 and the first isolation pillar 41 form an undercut structure 7, thereby isolating the electrode layer 3 falling into the first groove 61. The edge of the electrode layer 3 falling into the first groove 61 overlaps the sidewall of the first groove 61. Since the second planarization layer PLN2 is an insulating layer, it can completely disrupt the electrochemical corrosion path, preventing electrochemical corrosion. The illustrations in this disclosure only show two first isolation pillars 41; in practice, more can be reasonably set according to needs and space, such as 4, 6, or 8, etc.

[0098] The light-emitting layer 2 extends from the display area AA to the second partition area BB2, and is interrupted at least at the location of each second isolation pillar 42. Simultaneously, the light-emitting layer 2 passes through the first partition area BB1 and is also interrupted at the location of the undercut structure 7. This disclosure, through two partition designs, achieves complete isolation of the water-oxygen channel, effectively preventing the failure of the light-emitting device.

[0099] Optionally, the first groove 61 can be a through groove or a blind groove formed by etching the second planarization layer PLN2. It can be reasonably set according to the effective partition depth of the required undercut structure 7 and the thickness of the second planarization layer PLN2.

[0100] In some embodiments, FIG8 is a cross-sectional view of another display panel provided in the present disclosure along the A-A' direction. As shown in FIG8, the display panel 100 further includes a third planarization layer PLN3 disposed on the side of the third conductive layer SD3 near the light-emitting layer 2; the third planarization layer PLN3 includes a first planar portion 81 located in the display area AA and a first blocking portion 91 located in the second isolation area BB2; the third planarization layer PLN3 exposes a first isolation post 41, a first groove 61 and a second isolation post 42 in the middle region between the first planar portion 81 and the first blocking portion 91.

[0101] In this embodiment, the first planar portion 81 extends from the display area AA to the side of the first isolation pillar 41 closest to it, which is close to the display area AA. The edge of the first planar portion 81 ends at the first isolation pillar 41. Compared with the prior art, this achieves an inward reduction of the edge from the opening area CC towards the display area AA. The third planarization layer PLN3 exposes the first isolation pillar 41 and the first groove 61 underneath it, effectively reducing the thickness of the third planarization layer PLN3 stacked on the first isolation pillar 41, thus facilitating the subsequent etching of the first groove 61.

[0102] Furthermore, the second planarization layer PLN2 includes a second planar portion 82 extending from the display area AA to the first partition area BB1 and a second blocking portion 92 located in the second partition area BB2; a second groove 62 disposed on the substrate 1 is defined between the second planar portion 82 and the second isolation pillar 42 closest to the first partition area BB1.

[0103] In this embodiment, the third planarization layer PLN3 exposes the second isolation pillar 42 beneath it, effectively subtracting the thickness of the second isolation pillar 42 and the third planarization layer PLN3 stacked on the edge of the second planarization layer PLN2 adjacent to the second isolation pillar 42. Furthermore, the inward reduction of the first planarization portion 81 further widens the width of the second groove 62, reducing the risk of residual adhesive within the second groove 62. This is because, under conditions of fluctuations in the exposure and development processes of the subsequent pixel-defining layer (PDL), residual adhesive can form within the second groove 62. The deeper and narrower the second groove 62, the more difficult it is to wash away the residual adhesive. For example, if the third planarization layer PLN3 is retained on the edge of the second planarization layer PLN2 adjacent to the second isolation pillar 42, that is, the thickness of the third planarization layer PLN3 is increased, and the depth of the second groove 62 is at least the sum of the thicknesses of the second planarization layer PLN2 and the third planarization layer PLN3, thus making it difficult to wash away the residual adhesive. Furthermore, a third flat layer PLN3 is retained on the edge of the second flat layer PLN2 adjacent to the second isolation column 42. The side of the third flat layer PLN3 falls into the area where the second groove 62 is located, thus narrowing the width of the second groove 62 and reducing the thickness of the third flat layer PLN3, which makes it difficult to wash off the residual adhesive.

[0104] As shown in Figure 8, both the first flattened portion 81 and the second flattened portion 82 cover the circuit structure located in the display area AA. At least two flattening layers achieve the planarization of the circuit structure, which is beneficial for the fabrication of the upper light-emitting layer 2 and the electrode layer 3. At the same time, the relatively flat surface is beneficial for improving the encapsulation effect of the encapsulation layer 101 on it.

[0105] In some embodiments, as shown in FIG6, the first partition area BB1 is provided with a plurality of first isolation posts 41; a slot 63 is defined between two adjacent first isolation posts 41 and communicates with a first groove 61. The width W1 of the minimum opening of the slot 63 is smaller than the width W2 of the first groove 61.

[0106] Optionally, a set of two adjacent first isolation posts 41 are correspondingly arranged with a first groove 61; the two first isolation posts 41 protrude from the sidewall of the corresponding first groove 61 near the sidewall of the slot 63. The two first isolation posts 41 are respectively close to the sidewall of the slot 63 and the first groove 61, forming an undercut structure 7.

[0107] In some embodiments, as shown in FIG9, a first isolation post 41 is correspondingly disposed with a first groove 61; the side of the first isolation post 41 away from the display area AA protrudes from the sidewall of the corresponding first groove 61. The side of the first isolation post 41 away from the display area AA and the first groove 61 constitute an undercut structure 7.

[0108] In some embodiments, as shown in FIG5 or FIG8, each of the first isolation pillars 41 is flush with the surface of the substrate 1, which is beneficial for the fabrication of the upper light-emitting layer 2 and the electrode layer 3; at the same time, it is beneficial for improving the encapsulation effect of the encapsulation layer 101 on it.

[0109] In some embodiments, as shown in Figures 4 and 5, the display panel 100 further includes a second conductive layer SD2, a first conductive layer PLN1, and a first conductive layer SD1, sequentially disposed on the side of the second planarization layer PLN2 opposite to the third conductive layer SD3. Both the first conductive layer SD1 and the second conductive layer SD2 are film layers used for arranging panel traces. For example, the first conductive layer SD1 includes at least one first signal line 51 located in the display area AA, the second conductive layer SD2 includes at least one second signal line 52 located in the display area AA, and the third conductive layer SD3 includes at least one third signal line 53 located in the display area AA. The first signal line 51, the second signal line 52, and the third signal line 53 all refer to traces connected to an effective voltage. The first planarization layer PLN1 is used to planarize its underlying film layer (e.g., the first conductive layer SD1). The first planarization layer PLN1, the second planarization layer PLN2, and the third planarization layer PLN3 together constitute a planarization film, thereby ensuring that the film layer prepared on top of it can have a high degree of flatness.

[0110] The display panel 100 also includes multiple first redundant traces 54 located in the first partition area BB1 and surrounding the opening area CC. Each first redundant trace 54 is a trace that is not connected to any effective voltage. The multiple first redundant traces 54 are nested sequentially. Each first redundant trace 54 corresponds one-to-one with a first isolation pillar 41, and the orthographic projection of the first isolation pillar 41 on the substrate 1 overlaps with the orthographic projection of its corresponding first redundant trace 54 on the substrate 1, thus ensuring that the upper surfaces of each first isolation pillar 41 are flush. Optionally, the orthographic projection of the first isolation pillar 41 on the substrate 1 may cover the orthographic projection of its corresponding first redundant trace 54 on the substrate 1.

[0111] Multiple first redundant traces 54 are located in the first conductive layer SD1 or the second conductive layer SD2.

[0112] Optionally, as shown in Figure 5, multiple first redundant traces 54 are located in the first conductive layer SD1 and are disposed in the same layer as the first signal line 51. The first redundant traces 54 and the first signal line 51 are made of the same material, and they can be fabricated simultaneously to improve process efficiency. At the same time, by setting the first redundant trace 54 closest to the display area AA, the linewidth of the first signal line 51 can be guaranteed, and it can be prevented from being over-etched.

[0113] It should be noted that when using a dry etching process to form the signal lines (such as the first signal line 51 and the second signal line 52) of the display area AA, the inventors discovered that if there is no structure to block the etching gas from the outermost signal line, the signal line is easily over-etched, resulting in a narrower line width, affecting the voltage signal, and consequently affecting the display effect. Therefore, by adding redundant traces, the consistency of the line width of multiple signal lines in the display area AA can be ensured.

[0114] As shown in Figure 5, optionally, the orthographic projections of the first signal line 51 and the second signal line 52 on the substrate 1 are staggered. The orthographic projections of the third signal line 53 and the second signal line 52 on the substrate 1 are also staggered. Optionally, the orthographic projections of the first signal line 51 and the third signal line 53 on the substrate 1 overlap. For example, the orthographic projection of the third signal line 53 on the substrate covers the orthographic projection of the first signal line 51 on the substrate.

[0115] In some embodiments, as shown in Figures 4 and 5, the third conductive layer SD3 further includes multiple signal lines (i.e., third signal lines 53) located in the display area AA and at least one second redundant trace 55 located in the first isolation area BB1. By setting the second redundant trace 55 closest to the display area AA, the linewidth of the third signal lines 53 can be guaranteed, preventing them from being over-etched.

[0116] The portion of the third signal line 53 near the aperture area CC partially surrounds the aperture area CC, extending beyond the aperture area CC to the opposite display area AA; the second redundant trace 55 surrounds the aperture area CC, and the second redundant trace 55 is multiplexed as the first isolation pillar 41. Optionally, the third signal line 53, the first isolation pillar 41, and the second isolation pillar 42 are arranged in the same layer; the third signal line 53, the first isolation pillar 41, and the second isolation pillar 42 are made of the same material, and all three can be fabricated simultaneously, improving process efficiency.

[0117] In this embodiment, the already set second redundant wiring 55 is reused as the second isolation pillar 42, which optimizes the spatial layout and is conducive to achieving a thinner and lighter panel.

[0118] In some embodiments, FIG10 is a schematic diagram of the encapsulation effect of the encapsulation layer provided in the embodiments of the present disclosure. As shown in FIG10, the display panel further includes an encapsulation layer 101 disposed on the side of the electrode layer 3 away from the light-emitting layer; wherein, the encapsulation layer 101 is laid in a whole layer for encapsulating all the film layers located thereunder. The encapsulation layer 101 extends from the display area AA to the second isolation area BB2, and covers the portion exposed by the electrode layer 3 at the positions of each first isolation post 41 and each second isolation post 42.

[0119] The encapsulation layer 101 can be a single-layer structure or a multi-layer structure, which includes a structure of stacked inorganic and organic layers.

[0120] Optionally, as shown in FIG10, the encapsulation layer 101 includes a first inorganic encapsulation layer (not shown in the figure), an organic encapsulation layer IJP, and a second inorganic encapsulation layer CVD2, which are sequentially disposed along the direction away from the substrate 1; both the first inorganic encapsulation layer and the second inorganic encapsulation layer CVD2 extend from the display area AA to the edge of the opening area CC; the display panel 100 also includes a barrier dam 9 disposed on the side of the second isolation pillar 42 away from the first isolation pillar 41; the organic encapsulation layer IJP extends from the display area AA to the second isolation area BB2 and terminates at the side of the barrier dam 9 near the display area AA. The orthographic projections of the first inorganic encapsulation layer and the second inorganic encapsulation layer CVD2 on the substrate 1 both cover the orthographic projection of the barrier dam 9 on the substrate 1.

[0121] Optionally, the first inorganic encapsulation layer and the second inorganic encapsulation layer CVD2 are made of the same material. For example, the materials of the first inorganic encapsulation layer and the second inorganic encapsulation layer CVD2 may include insulating materials such as silicon oxynitride (SiON), silicon oxide (SiOx), silicon nitride (SiNx), and polymer resin. Inorganic materials such as silicon oxynitride (SiON), silicon oxide (SiOx), and silicon nitride (SiNx) have high density, which can prevent the intrusion of water, oxygen, etc.; the material of the organic encapsulation layer IJP may be a polymer material containing a desiccant or a polymer material that can block moisture, such as a polymer resin, to planarize the surface of the display panel 100 and relieve stress on the first inorganic encapsulation layer and the second inorganic encapsulation layer CVD2. It may also include water-absorbing materials such as a desiccant to absorb water, oxygen, and other substances that have intruded into the interior.

[0122] This embodiment utilizes an inorganic-organic-inorganic three-layer encapsulation film to seal the light-emitting device in the display area AA, effectively preventing moisture and / or oxygen in the opening area CC from spreading to the display area AA and causing degradation of the light-emitting device.

[0123] In some embodiments, as shown in FIG10, the display panel 100 further includes an anode (not shown) and a pixel defining layer PDL sequentially disposed on the side of the third planarization layer PLN3 near the light-emitting layer 2. A pixel opening (not shown) is provided on the pixel defining layer PDL, defining the light-emitting area of ​​the light-emitting device. The portion of the anode directly opposite the pixel opening, the portion of the light-emitting layer 2 falling into the pixel opening, and the portion of the cathode falling into the pixel opening are collectively defined as the light-emitting device. Optionally, the light-emitting device is an OLED device.

[0124] The pixel defining layer (PDL) is located at least in the display area AA. Optionally, the pixel defining layer (PDL) includes a barrier structure located in the display area AA and a fourth blocking portion 94 located in the second partition area BB2. Pixel openings are all disposed on the barrier structure.

[0125] The display panel 100 further includes a support layer disposed on the side of the pixel defining layer PDL away from the anode, the support layer including at least one support portion PS. Optionally, the barrier dam 9 includes at least a second planarization layer PLN2, a third planarization layer PLN3, the pixel defining layer PDL, and the support portion PS stacked sequentially in the direction away from the substrate 1, located in the second isolation region BB2. For example, as shown in FIG10, the third planarization layer PLN3 includes a first barrier portion 91 located in the second isolation region BB2; the second planarization layer PLN2 includes a second barrier portion 92 located in the second isolation region BB2; the first planarization layer PLN1 includes a third planarization portion 83 extending from the display region AA to the first isolation region BB1 and a third barrier portion 93 located in the second isolation region BB2. The barrier dam 9 includes a third barrier portion 93, a second barrier portion 92, a first barrier portion 91, a fourth barrier portion 94, and a support portion PS stacked sequentially in the direction away from the substrate 1. The multi-layered barrier dam 9 has a certain height and can effectively block the organic encapsulation layer IJP located on its side near the display region AA.

[0126] Optionally, the support portion PS is made of the same material as the pixel defining layer PDL. Optionally, the pixel defining layer PDL is made of the same material as the second planarization layer PLN2, for example, both are made of organic insulating material.

[0127] Optionally, the pixel defining layer PDL and the support portion PS expose the second isolation pillar 42 in the second partition area BB2, thereby preventing the pixel defining layer PDL on the second isolation pillar 42 from being etched and deformed by the dry etching process of the undercut structure 7, which would affect the subsequent encapsulation of the organic packaging layer IJP.

[0128] In some embodiments, as shown in FIG11, the display panel 100 further includes a support structure 1021 located in the second isolation region BB2. The support structure 1021 is composed of a portion of the pixel defining layer PDL and a portion of the support layer (i.e., a support portion PS).

[0129] At least a portion of the multiple isolation pillars 42 are located on the side of the barrier dam 9 away from the display area AA. The support structure 1021 is located on the side of the barrier dam 9 away from the display area AA, and the support structure 1021 covers the top surface of two adjacent second isolation pillars 42 facing away from the substrate 1, and fills the gap between the two adjacent second isolation pillars 42. Since the support structure 1021 is composed of an insulating pixel support layer PDL and a support portion PS, it can disconnect power to a certain extent, further preventing electrochemical corrosion.

[0130] In some embodiments, the materials of the third planarization layer PLN3, the second planarization layer PLN2, and the first planarization layer PLN1 are all organic insulating materials.

[0131] The second planarization layer PLN2 is made of an organic insulating material. The first groove 61 can be formed by etching the organic insulating material using a dry etching method. For example, dry etching using a mixture of carbon tetrafluoride and oxygen gas can achieve rapid etching of the organic insulating material without affecting the metal material of the second conductive layer SD2.

[0132] Optionally, as shown in FIG10, the orthographic projection of the second planarization layer PLN2 on the substrate 1 completely covers the orthographic projection of the first planarization layer PLN1 on the substrate 1.

[0133] Optionally, as shown in FIG10, the display panel 100 further includes a passivation layer PVX disposed on the side of the first planarization layer PLN1 near the first conductive layer SD1. The orthographic projection of the first planarization layer PLN1 on the substrate 1 completely covers the orthographic projection of the passivation layer PVX on the substrate 1. For example, the material of the passivation layer PVX is an inorganic material. The thickness of the passivation layer PVX is less than the thickness of the first planarization layer PLN1.

[0134] In some embodiments, as shown in FIG5, the display panel 100 further includes an interlayer insulating layer (ILD) disposed on the side of the first conductive layer SD1 near the substrate 1. The edges of the passivation layer PVX near the opening region CC, the second flat portion 82 near the opening region CC, and the third flat portion 83 near the opening region CC all fall into the side of the interlayer insulating layer near the opening region CC. Optionally, the interlayer insulating layer (ILD) is an inorganic material. Since inorganic materials are difficult to etch, have high process requirements, and have significant application limitations, this disclosure avoids etching grooves on the interlayer insulating layer (ILD) corresponding to the second isolation pillar 42 to cut off the electrode layer 3. This also reflects that the process of this disclosure has lower costs, fewer application limitations, and is convenient and efficient to prepare.

[0135] Optionally, as shown in FIG5, the display panel 100 further includes a metal trace disposed on the side of the interlayer insulating layer (ILD) near the substrate 1, wherein the orthographic projection of the metal trace on the substrate 1 covers the orthographic projection of the second isolation pillar 42 on the substrate 1. The metal trace may be, for example, a first metal trace M1 and / or a second metal trace M2, wherein the orthographic projection of the second metal trace M2 on the substrate 1 covers the orthographic projection of the first metal trace M1 on the substrate 1.

[0136] In this embodiment, the second isolation pillar 42 is positioned directly above the metal traces (M1 and / or M2) to elevate the second isolation pillar 42, thereby facilitating the cutting of the light-emitting layer 2.

[0137] For example, the metal traces can be gate lines, capacitor plates, or the gate electrode of a thin-film transistor.

[0138] In some embodiments, the isolation pillar has a multi-layer structure. Specifically, FIG12 is a structural diagram of the isolation pillar provided in an embodiment of the present disclosure. As shown in FIG12, the isolation pillar includes a first conductive portion 401, a second conductive portion 402, and a third conductive portion 403 arranged sequentially along the direction away from the substrate 1. The first conductive portion 401 and the third conductive portion 403 both protrude from the second conductive portion 402. Thus, the cross-sections of the first conductive portion 401, the second conductive portion 402, and the third conductive portion 403 are in the shape of an "I", which is used to isolate the light-emitting layer 2 and the electrode layer 3.

[0139] Optionally, the first isolation post 41 and the second isolation post 42 adopt the multi-layer structure shown in FIG12. Specifically, the first conductive portion 401 in the first isolation post 41 is disposed in the same layer as the first conductive portion 401 in the second isolation post 42; the second conductive portion 402 in the first isolation post 41 is disposed in the same layer as the second conductive portion 402 in the second isolation post 42; and the third conductive portion 403 in the first isolation post 41 is disposed in the same layer as the third conductive portion 403 in the second isolation post 42.

[0140] Of course, the first isolation pillar 41 and the second isolation pillar 42 can also be selected as a two-layer stacked structure, with the upper conductive part protruding from the lower conductive part.

[0141] For example, the first conductive part 401 and the third conductive part 403 are both made of titanium (Ti); the second conductive part 402 is made of aluminum (Al). That is, the first isolation pillar 41 and the second isolation pillar 42 of this disclosure adopt a titanium / aluminum / titanium (Ti / Al / Ti) three-layer structure.

[0142] Example 2

[0143] As shown in Figure 13, the partition area includes a first partition area BB1 and a second partition area BB2; the second partition area BB2 surrounds the opening area CC, and the first partition area BB1 surrounds the second partition area BB2; the multiple isolation pillars include at least one third isolation pillar 43 located in the second isolation area BB2. At least one third isolation pillar 43 surrounds the opening area CC, thereby achieving all-round protection around the opening and preventing water and oxygen erosion and electrochemical corrosion.

[0144] The first groove 61 is located in the second isolation area BB2. The orthographic projection of one side edge of the third isolation pillar 43 onto the substrate 1 falls within the orthographic projection of the first groove 61 onto the substrate 1. This also means that one side edge of the third isolation pillar 43 protrudes from the sidewall of the first groove 61, forming a discontinuity. That is, the first groove 61 and the third isolation pillar 43 form an undercut structure 7, which can isolate the electrode layer 3 falling into the first groove 61. The edge of the electrode layer 3 falling into the first groove 61 overlaps the sidewall of the first groove 61. Since the second planarization layer PLN2 is an insulating layer, it can completely destroy the electrochemical corrosion path and prevent electrochemical corrosion. The illustration in this disclosure only shows two third isolation pillars 43. In practice, more can be reasonably set according to needs and space, such as 4, 6, or 8, etc. In addition, the light-emitting layer 2 extends from the display area AA to the second isolation area BB2 and is interrupted at least at the position of each third isolation pillar 43 (i.e., the undercut structure 7). This disclosure uses the undercut structure 7 to simultaneously achieve the effects of power cut-off and water and oxygen cut-off.

[0145] Optionally, the first groove 61 can be a through groove or a blind groove formed by etching the second planarization layer PLN2. It can be reasonably set according to the required effective isolation depth of the undercut structure 7 and the thickness of the second planarization layer PLN2. Preferably, since there is no directly contacting conductive layer under the second planarization layer PLN2 located in the second isolation region BB2, the first groove 61 can be directly etched as a through groove to ensure the isolation effect.

[0146] In some embodiments, the display panel 100 further includes a third planarization layer PLN3 disposed on the side of the third conductive layer SD3 near the light-emitting layer 2; the third planarization layer PLN3 includes a first planar portion 81 extending from the display area AA to the first isolation area BB1 and a first blocking portion 91 located in the second isolation area BB2; the third planarization layer PLN3 exposes a third isolation post 43 and a first groove 61 in the middle region between the first planar portion 81 and the first blocking portion 91.

[0147] The orthographic projection of the third planarization layer PLN3 onto the substrate 1 covers all signal lines and redundant traces (e.g., the second redundant trace 55 and the first redundant trace 54) located within the first isolation region BB1.

[0148] In some embodiments, as shown in FIG13, the display panel 100 further includes a blocking dam 9 located in the second partition region BB2. The composition of the blocking dam 9 can be referred to the description of Embodiment 1, specifically including a third blocking portion 93, a second blocking portion 92, a first blocking portion 91, a fourth blocking portion 94 and a support portion PS stacked sequentially along the direction away from the substrate 1. Other detailed structures are shown in Embodiment 1, and repeated parts will not be described again.

[0149] The third isolation pillar 43 includes multiple pillars; this disclosure uses two as an example. Each third isolation pillar 43 is located on the side of the barrier dam 9 closest to the display area AA, so as to complete power isolation on the side of the barrier dam 9 closest to the display area AA. A slot 63 is defined between adjacent third isolation pillars 43 and communicates with the first groove 61 to form a deeper undercut structure 7.

[0150] In some embodiments, as shown in FIG13, two third isolation pillars 43 are provided on the side of the blocking dam 9 near the display area AA as an example. The portion of the second planarization layer PLN2 used to form the first groove 61 is designated as the protrusion 1011, and the first groove 61 penetrates or partially penetrates the protrusion 1011; the orthographic projection of two adjacent third isolation pillars 43 on the substrate 1 covers the orthographic projection of the protrusion 1011 on the substrate 1; in the horizontal direction, the side of the third isolation pillar 43 away from the groove 63 wraps around the edge of the protrusion 1011 away from the first groove 61.

[0151] The surface of the protrusion 1011 facing away from the substrate 1 is arc-shaped. In the direction from the display area AA to the opening area CC, the third isolation pillar 43 includes two sides arranged opposite to each other, one side of which falls on a flat surface, and the other side extends along the arc surface and finally falls on the arc surface of the protrusion 1011.

[0152] In some embodiments, as shown in FIG13, the display panel 100 further includes metal traces disposed on the side of the interlayer insulating layer (ILD) near the substrate 1, wherein the orthographic projection of the metal traces on the substrate 1 covers the orthographic projection of the third isolation pillar 43 on the substrate 1. The metal traces may be, for example, a first metal trace M1 and / or a second metal trace M2, wherein the orthographic projection of the second metal trace M2 on the substrate 1 covers the orthographic projection of the first metal trace M1 on the substrate 1.

[0153] In this embodiment, the third isolation pillar 43 is positioned directly above the metal traces (M1 and / or M2) to elevate the third isolation pillar 43, thereby facilitating the cutting of the light-emitting layer 2.

[0154] For example, the metal traces can be gate lines, capacitor plates, or the gate electrode of a thin-film transistor.

[0155] In some embodiments, as shown in FIG13, the display panel 100 further includes a support structure 1021 located in the second isolation region BB2. The support structure 1021 is composed of a portion of the pixel defining layer PDL and a portion of the support layer (i.e., a support portion PS).

[0156] The multiple isolation pillars also include a portion of the second isolation pillar 42 located on the side of the barrier dam 9 away from the display area AA. The support structure 1021 is located on the side of the barrier dam 9 away from the display area AA, and the support structure 1021 covers the top surface of two adjacent second isolation pillars 42 facing away from the substrate 1, and fills the gap between two adjacent second isolation pillars 42. Since the support structure 1021 is composed of an insulating pixel support layer PDL and a support portion PS, it can disconnect power to a certain extent, further preventing electrochemical corrosion.

[0157] Multiple support structures 1021 can be provided and evenly distributed on the side of the barrier dam 9 near the opening area CC. The specific number is not limited in this embodiment.

[0158] In some embodiments, the third isolation pillar 43 can be a multilayer structure, as shown in FIG12. For example, the third isolation pillar 43 includes a first conductive portion 401, a second conductive portion 402 and a third conductive portion 403 arranged sequentially along the direction away from the substrate 1. The first conductive portion 401 and the third conductive portion 403 both protrude from the second conductive portion 402. Thus, the cross-sections of the first conductive portion 401, the second conductive portion 402 and the third conductive portion 403 are in the shape of an "I", which is used to isolate the light-emitting layer 2 and the electrode layer 3.

[0159] Optionally, as shown in FIG13, the third isolation post 43 and the second isolation post 42 adopt the multi-layer structure shown in FIG12. Specifically, the first conductive portion 401 in the third isolation post 43 is disposed in the same layer as the first conductive portion 401 in the second isolation post 42; the second conductive portion 402 in the third isolation post 43 is disposed in the same layer as the second conductive portion 402 in the second isolation post 42; and the third conductive portion 403 in the third isolation post 43 is disposed in the same layer as the third conductive portion 403 in the second isolation post 42.

[0160] For example, the third isolation pillar 43 and the second isolation pillar 42 of this disclosure adopt a titanium / aluminum / titanium (Ti / Al / Ti) three-layer structure.

[0161] Example 3

[0162] The difference from Embodiment 2 is that a third isolation pillar 43 is added to the side of the barrier dam 9 near the opening area CC. The third isolation pillar 43 is correspondingly arranged with the first groove 61. One third isolation pillar 43 corresponds to one first groove 61; or two adjacent third isolation pillars 43 correspond to one first groove 61. Other aspects of the film structure in the display area AA and the first partition area BB1 are the same as in Embodiment 2, and repeated parts will not be described again.

[0163] As shown in Figure 14, the partition area includes a first partition area BB1 and a second partition area BB2; the second partition area BB2 surrounds the opening area CC, and the first partition area BB1 surrounds the second partition area BB2; the multiple isolation pillars include multiple third isolation pillars 43 located in the second partition area BB2. Each third isolation pillar 43 surrounds the opening area CC, thereby achieving all-round protection around the opening and preventing water and oxygen erosion and electrochemical corrosion. The display panel also includes a barrier dam 9 located in the second partition area. It should be noted that the setting position of the barrier dam 9 is the same in all embodiments of this disclosure. The multiple third isolation pillars 43 are distributed on both sides of the barrier dam 9 near the display area AA and away from the display area AA. In this way, multiple undercut structures 7 are formed by multiple third isolation pillars 43 and corresponding first grooves 61 for multiple power cut-offs to prevent electrochemical corrosion.

[0164] This disclosure uses the example of setting a pair of third isolation columns 43 on the side of the barrier dam 9 closest to the display area AA and setting a pair of third isolation columns 43 on the side of the barrier dam 9 furthest from the display area AA. The actual number of third isolation columns 43 can be adjusted according to the actual product partitioning effect and application.

[0165] Optionally, for the plurality of third isolation pillars 43 located on the side of the barrier dam 9 near the display area AA, a slot 63 is defined between two adjacent third isolation pillars 43 and communicates with a corresponding first groove 61 to form an undercut structure 7; for the plurality of third isolation pillars 43 located on the side of the barrier dam 9 away from the display area AA, at least one set of two adjacent third isolation pillars 43 is defined between a slot 63 and communicates with a corresponding first groove 61 to form another undercut structure 7.

[0166] In some embodiments, as shown in FIG14, the portion of the second planarization layer PLN2 used to form the first groove 61 is designated as a protrusion 1011. This disclosure illustrates two protrusions 1011 located on both sides of the barrier dam 9. Taking one of the protrusions as an example, a first groove 61 penetrates or partially penetrates a protrusion 1011; the orthographic projections of two adjacent third isolation pillars 43 on the substrate 1 cover the orthographic projection of the protrusion 1011 on the substrate 1; in the horizontal direction, the side of the third isolation pillar 43 away from the groove 63 wraps around the edge of the protrusion 1011 away from the first groove 61.

[0167] The surface of the protrusion 1011 facing away from the substrate 1 is arc-shaped. In the direction from the display area AA to the opening area CC, the third isolation pillar 43 includes two sides arranged opposite to each other, one side of which falls on a flat surface, and the other side extends along the arc surface and finally falls on the arc surface of the protrusion 1011.

[0168] In some embodiments, as shown in FIG14, the display panel 100 further includes metal traces disposed on the side of the interlayer insulating layer (ILD) near the substrate 1, wherein the orthographic projection of the metal traces on the substrate 1 covers the orthographic projection of the third isolation pillar 43 on the substrate 1. The metal traces may be, for example, a first metal trace M1 and / or a second metal trace M2, wherein the orthographic projection of the second metal trace M2 on the substrate 1 covers the orthographic projection of the first metal trace M1 on the substrate 1.

[0169] In this embodiment, the third isolation pillar 43 is positioned directly above the metal traces (M1 and / or M2) to elevate the third isolation pillar 43, thereby facilitating the cutting of the light-emitting layer 2.

[0170] For example, the metal traces can be gate lines, capacitor plates, or the gate electrode of a thin-film transistor.

[0171] In some embodiments, as shown in FIG15, the display panel 100 further includes a support structure 1021 located in the second isolation region BB2. The support structure 1021 is composed of a portion of the pixel defining layer PDL and a portion of the support layer (i.e., a support portion PS).

[0172] The multiple isolation pillars also include a portion of the second isolation pillar 42 located on the side of the barrier dam 9 away from the display area AA. The support structure 1021 is located on the side of the barrier dam 9 away from the display area AA, and the support structure 1021 covers the top surface of two adjacent second isolation pillars 42 facing away from the substrate 1, and fills the gap between two adjacent second isolation pillars 42. Since the support structure 1021 is composed of an insulating pixel support layer PDL and a support portion PS, it can disconnect power to a certain extent, further preventing electrochemical corrosion.

[0173] Optionally, the support structure 1021 is mainly located on the side of the third isolation column 43 near the opening area CC.

[0174] Multiple support structures 1021 can be provided and evenly distributed on the side of the barrier dam 9 near the opening area CC. The specific number is not limited in this embodiment.

[0175] Example 4

[0176] The difference from Embodiment 1 is that multiple support structures 1021 are provided in the second partition area BB2 to improve the power-off effect. This technical solution can be applied to scenarios with a wide second partition area BB2, such as foldable products, where the reserved space can be used to add support structures 1021.

[0177] As shown in Figure 16, the display panel also includes support structures 1021 located on both sides of the barrier dam. Taking two support structures as an example, the plurality of isolation pillars include at least two second isolation pillars 42 located on both sides of the barrier dam 9. Optionally, the plurality of isolation pillars include a first isolation pillar 41 and second isolation pillars 42 located on both sides of the barrier dam 9; wherein, the support structure 1021 covers the top surface of two adjacent second isolation pillars 42 facing away from the substrate 1 and fills the gap between two adjacent second isolation pillars 42. The support structure 1021 includes a portion of the pixel limiting layer PDL and a portion of the support layer, i.e., the support portion PS, located in the second isolation region BB2. Since the support structure 1021 is composed of an insulating pixel support layer PDL and a support portion PS, it can disconnect power to a certain extent, further preventing electrochemical corrosion.

[0178] For folding products, which have a wider second partition area BB2, four second isolation pillars 42 can be installed on the side of the blocking dam 9 closest to the display area AA, and seven second isolation pillars 42 can be installed on the side of the blocking dam 9 furthest from the display area AA. Figure 16 shows only two second isolation pillars 42 on the left and right sides of the blocking dam 9, which is only for illustration and does not represent a limitation on the number of second isolation pillars 42 in the actual product. In addition, the actual number of support structures 1021 can also be adjusted according to the actual product partitioning effect and application.

[0179] Furthermore, if there is sufficient space in the second partition area BB2 located on the side of the barrier dam 9 near the display area AA, a third isolation column 43 as shown in Embodiment 2 can be added to the structure in Figure 16 to further improve the partitioning effect. Optionally, the multiple isolation columns include a first isolation column 41, a third isolation column 43 located on the side of the barrier dam 9 near the display area AA, and second isolation columns 42 located on both sides of the barrier dam 9, etc. Repeated structures will not be described further.

[0180] Example 5

[0181] The difference between this embodiment and embodiment 1 is that it has a wider first partition area BB1, so that multiple undercut structures 7 can be set.

[0182] As shown in Figure 17, this embodiment can be applied to scenarios with a relatively wide first isolation area BB1. The reserved width ensures that signal lines can be deployed in the first conductive layer SD1 and the second conductive layer SD2. Thus, for the third conductive layer SD3, no signal lines need to be set in its first isolation area BB1, and the reserved space can be used to set at least three first isolation pillars 41, with each pair of adjacent first isolation pillars 41 corresponding to a first groove 61. To avoid the influence of over-etching the second planarization layer PLN2 on the signal lines beneath it, the first groove 61 in this embodiment is a blind groove.

[0183] Example 6

[0184] As shown in Figure 18, this embodiment adopts the technical solution of the first isolation pillar 41 and the second isolation pillar 42 in Embodiment 1 above. However, the difference from Embodiment 1 is that a wider first redundant trace 54 is used, and the first redundant trace 54 is disposed in the second conductive layer SD2. Optionally, the orthographic projection of the first redundant trace 54 on the substrate 1 at least covers the orthographic projection of the slot 63 between the first isolation pillars 41 on the substrate 1; or the orthographic projection of the first redundant trace 54 on the substrate 1 at least covers the orthographic projection of the first groove 61 on the substrate 1, so as to ensure that the undercut structure 7 is disposed on a relatively flat surface.

[0185] Example 7

[0186] As shown in Figure 19, this embodiment adopts the technical solution of the first isolation pillar 41 and the second isolation pillar 42 in the above embodiment 1. However, the difference from embodiment 1 is that the orthographic projection of the first isolation pillar 41 on the substrate 1 is located on the side of the first redundant trace 54 on the substrate 1 that is far away from the display area AA.

[0187] Optionally, the width of the signal line closest to the opening region CC in the second conductive layer SD2 is greater than the width of other signal lines in the second conductive layer SD2, to prevent the line width from becoming narrow due to over-etching of signal lines near the edge of the display area.

[0188] Regarding other structures of the display panel, they are all common to embodiments 1-7 described above. In some embodiments, the display panel 100 further includes a touch functional layer (not shown in the figure) disposed on the encapsulation layer 101. The touch functional layer includes a touch buffer layer, a first touch metal layer (TMA), a touch insulator layer (TLD), a second touch metal layer (TMB), and a touch protection layer (TOC) disposed sequentially along the direction away from the substrate 1. Specifically, the first and second touch metal layers are not present at the edge of the display area AA near the second transition area BB2, but a touch insulator layer is present. The touch insulator layer and the touch protection layer extend from the display area AA to the second separation area BB2.

[0189] It should be noted that the light-emitting devices involved in the embodiments of this disclosure may include, but are not limited to, organic light-emitting diodes (OLEDs), quantum dot light-emitting diodes (QLEDs), or micro light-emitting diodes (Micro LEDs). Optionally, the light-emitting device is a Micro LED device. Optionally, the display panel 100 is an active-matrix organic light-emitting diode panel, i.e., an AMOLED panel.

[0190] The display panel 100 also includes a pixel driving circuit disposed on the side of the light-emitting device near the substrate 1. The pixel driving circuit is used to drive the corresponding light-emitting device to emit light. The pixel driving circuit includes multiple transistors and a storage capacitor. The pixel driving circuit can adopt a 7T1C (i.e., 7 transistors and 1 capacitor), 5T2C, or 7T2C circuit structure. Of course, other circuit structures can also be used for the pixel driving circuit, which will not be listed here.

[0191] In addition, this disclosure also provides a method for manufacturing a display panel 100, mainly used to manufacture the display panel 100 in the above embodiments. The display panel 100 has a display area AA, a partition area (e.g., a first partition area BB1 and a second partition area BB2), and an opening area CC; the second partition area BB2 surrounds the opening area CC, and the first partition area BB1 surrounds the second partition area BB2. Figure 20 is a flowchart of a method for manufacturing a display panel provided by an embodiment of this disclosure. As shown in Figure 20, the manufacturing method includes steps S11 to S15.

[0192] S11, Provide a substrate.

[0193] The substrate 1 may be made of, but is not limited to, polyimide (PI), polyethylene naphthalene-2,6-dicarboxylate (PEN), polyethylene terephthalate (PET), colorless polyimide (CPI) with flexible properties, thermoplastic polyurethane (TUP), or ultra-thin glass (UTG). The substrate 1 may also be made of rigid, transparent materials such as glass, which can effectively support other film layers on it. In practical applications, appropriate materials can be selected according to actual needs. For example, the substrate 1 may be a single-layer structure or a multi-layer structure. In a multi-layer substrate 1, inorganic thin films can be added between the layers to act as buffer layers. The buffer layer material may be one or more layers of amorphous silicon (a-Si), silicon nitride (SiNx), or silicon oxide (SiOx).

[0194] S12. A second planar material layer is formed on the substrate.

[0195] The second planarization material layer PLN2' is the material layer of the second planarization layer PLN2 to be prepared. Optionally, the material of the second planarization material layer PLN2', or the second planarization layer PLN2, is an organic insulating material.

[0196] For example, the materials may include, but are not limited to, one or more combinations of resin materials such as acrylic, polyimide, epoxy resin, polyester, photoresist, polyacrylate, polyamide, and siloxane; or elastic materials such as urethane and thermoplastic polyurethane (TPU).

[0197] Figures 21a to 21d are schematic flowcharts illustrating the fabrication process of the undercut structure located in the first partition region according to embodiments of this disclosure, such as Embodiment 1 and Embodiments 4 to 7. Specifically, taking Embodiment 1 as an example, as shown in Figure 21a, a pattern including the second planar material layer PLN2' is formed on the substrate 1 through a single patterning process (e.g., a single PLN2 mask process). Of course, the fabrication process of the undercut structure 7 in other embodiments is similar. This disclosure only uses Embodiment 1 as an example for illustration, and repeated content will not be described again.

[0198] In this disclosure, "patterning process" refers to the steps of forming a structure with a specific pattern, which can be a photolithography process. A photolithography process includes one or more steps such as forming a material layer, coating photoresist, exposure, development, etching, and photoresist stripping. Of course, "patterning process" can also be other processes such as imprinting and inkjet printing. "One-time patterning process" means a process of forming patterned layers, parts, components, etc. using a photomask. In this disclosure, "the pattern including the second flat material layer PLN2" mainly retains the display area AA and a portion of the material extending to the first partition area BB1 (i.e., the second flat portion 82 before etching), etches away another portion of the material of the first partition area BB1 and a portion of the material of the second partition area BB2, and retains the second blocking portion 92.

[0199] S13. A third conductive layer is formed on the side of the second flat material layer away from the substrate.

[0200] The third conductive layer SD3 is made of a multilayer structure; this disclosure uses a three-layer titanium / aluminum / titanium as an example. The three-layer titanium / aluminum / titanium is etched twice consecutively to form isolation pillars, at which point the titanium layer protrudes from the aluminum layer; the isolation region includes multiple isolation pillars, each of which surrounds the opening region CC. Exemplarily, firstly, titanium, aluminum, and titanium material layers are deposited sequentially; then, as shown in FIG21b, a patterned second redundant trace 55 is formed by etching once using a mask process (SD3 Mask); finally, as shown in FIG21c, a third conductive layer SD3 with a first isolation pillar 41 and a second isolation pillar 42 is formed by etching a second time using another mask process (AND Mask).

[0201] The third conductive layer SD3 includes at least one first isolation pillar 41 located in the first isolation region BB1 and at least one second isolation pillar 42 located in the second isolation region BB2; both the at least one first isolation pillar 41 and the at least one second isolation pillar 42 surround the opening region CC.

[0202] S14. At least the second planar material layer is etched to form a second planar layer with a first groove.

[0203] After etching to form multiple isolation pillars, a second flat material layer PLN2' is exposed between some adjacent isolation pillars. The exposed areas are etched to form a first groove 61. Thus, the orthographic projection of one side edge of at least one isolation pillar onto the substrate 1 falls into the orthographic projection of the first groove 61 onto the substrate 1, thereby forming an undercut structure 7, which is used to block the water-oxygen erosion path and the electrochemical corrosion path.

[0204] For example, following step S13, after etching to form the first isolation pillar 41, a portion of the surface of the second planar material layer PLN2' is exposed. Taking two adjacent first isolation pillars 41 as an example, a groove 63 is defined between the two adjacent first isolation pillars 41. The groove 63 exposes a portion of the surface of the second planar material layer PLN2' facing away from the substrate 1, as shown in FIG21d. The exposed surface is etched to form a second planar layer PLN2 with a first groove 61. The orthographic projection of one edge of the first isolation pillar 41 on the substrate 1 falls within the orthographic projection of the first groove 61 on the substrate 1; the first groove 61 and the first isolation pillar 41 form an undercut structure 7.

[0205] S15. A light-emitting layer and an electrode layer are sequentially formed on the side of the third conductive layer that is away from the second planarization layer.

[0206] Specifically, electrode layer 3 is cut off at the position of undercut structure 7; light-emitting layer 2 is broken at least at the position of second isolation pillar 42. For example, light-emitting layer 2 is broken at both the position of first isolation pillar 41 and second isolation pillar 42.

[0207] The material of the light-emitting layer 2 is an organic light-emitting material for light-emitting devices. The fabrication process of the light-emitting layer 2 includes, but is not limited to, inkjet printing, spin coating, screen printing, and transfer printing.

[0208] The electrode layer 3 can be a single layer or multiple layers, and the material can be selected from metals. For example, the material of the electrode layer 3 can be selected from at least one of silver (Ag), magnesium (Mg), copper (Cu), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), lithium (Li), calcium (Ca), Ca-LiF alloy, Al-LiF alloy, molybdenum (Mo), titanium (Ti), indium (In), tin (Sn), and zinc (Zn).

[0209] Figures 22a and 22d are schematic flowcharts of the fabrication process of the undercut structure located in the second partition region provided by embodiments of this disclosure, such as embodiments 2 and 3. As shown in Figure 22a, the second planarization material layer PLN2' further includes a protrusion material 1011A located in the second partition region BB2. As shown in Figure 22b, a third conductive material layer SD3' is formed on the side of the protrusion material 1011A facing away from the substrate 1; wherein, the third conductive material layer SD3' encapsulates the protrusion material 1011A; then, the third conductive material layer SD3' is etched once to form an intermediate segment structure. As shown in Figure 22c, the middle position and the two side edges of the intermediate segment structure are then etched a second time to form two adjacent third isolation pillars 43. Finally, as shown in Figure 22d, after etching to form the third isolation pillars 43, part of the surface of the protrusion material 1011A is exposed. The exposed surface of the protrusion material 1011A is etched to form a second planarization layer PLN2 with a first groove 61.

[0210] In some embodiments, after the formation of the third conductive layer SD3 and before etching the second planar material layer PLN2', S13A is also included, as shown in FIG20.

[0211] S13A, A third planarization layer is formed on the side of the third conductive layer opposite to the second planarization material layer PLN2'.

[0212] The third planarization layer PLN3 exposes the isolation pillars and the first groove.

[0213] For embodiments 1, 4, 6, and 7, the third planarization layer PLN3 includes a first planar portion 81 located in the display area AA and a first blocking portion 91 located in the second partition area BB2; the third planarization layer PLN3 exposes a first isolation pillar 41 and a second isolation pillar 42 in the intermediate region between the first planar portion 81 and the first blocking portion 91. Specifically, the third planarization layer PLN3, including the first planar portion 81 and the first blocking portion 91, is formed on the side of the third conductive layer SD3 away from the second planar material layer PLN2' through a single patterning process (e.g., a mask PLN3 Mask process). The first planar portion 81 is located in the display area AA; the first blocking portion 91 is located in the second partition area BB2 and is mainly used to form part of the blocking dam 9. The third planarization layer PLN3 exposes the first isolation pillar 41, that is, exposes the slot 63 between two adjacent first isolation pillars 41, thereby exposing the surface of the second planar material layer PLN2' opposite the slot 63. Because the first flat portion 81 is recessed, it avoids the surface of the second flat material layer PLN2' opposite the slot 63, reducing the film thickness and thus facilitating etching of that surface.

[0214] Simultaneously, the third planarization layer PLN3 also exposes the second isolation pillar 42, thereby exposing the second isolation pillar 42 and the adjacent second planarization layer PLN2. Because the first planarization portion 81 is recessed, it avoids the second groove 62 between the second isolation pillar 42 and the adjacent second planarization layer PLN2. Therefore, it reduces the depth of the second groove 62 and increases its width, which facilitates the washing of residual adhesive left in the second groove 62 from subsequent film preparation processes, reducing the risk of residual adhesive and ensuring barrier performance.

[0215] For embodiments 2 and 3, the third planarization layer PLN3 is laid as a whole, extending from the display area AA to the first isolation area BB1, and ending at the side of the second isolation post 42 and the third isolation post 43 near the display area AA. Moreover, the third planarization layer PLN3 only covers part of the second planarization layer PLN2, and the recessed part of the third planarization layer PLN3 reserves space for washing the second groove 62.

[0216] In some embodiments, for S14, a dry etching process can be used to etch the second planarization material layer PLN2' to form a second planarization layer PLN2 with a first groove 61. Specifically, this includes: using gas or plasma in a vacuum environment to etch the surface of the second planarization material layer PLN2' exposed by the third planarization layer PLN3 and the third conductive layer SD3 to form the first groove 61.

[0217] Taking two adjacent first isolation pillars 41 as an example, a groove 63 is defined between the two adjacent first isolation pillars 41. The groove 63 exposes a portion of the second flat material layer PLN2' facing away from the surface of the substrate 1. The exposed surface can be dry-etched using gas or plasma in a vacuum environment to form a first groove 61. Since the first groove 61 is recessed on one side edge compared to the first isolation pillar 41, the first groove 61 and the first isolation pillar 41 form an undercut structure 7, which can completely isolate the electrode layer 3. At the same time, by utilizing the insulating properties of the inner wall of the first groove 61, the electrochemical corrosion path is completely isolated, effectively avoiding the electrochemical corrosion of the display area AA device.

[0218] Optionally, the material of the second planarization layer PLN2' is an organic insulating material; the gas used to etch the second planarization layer PLN2' is preferably a mixture of carbon tetrafluoride (CF4) and oxygen (O2). Etching the organic insulating material using CF4+O2 is relatively fast, and this mixed gas (CF4+O2) has almost no etching effect on the metal, therefore it will not affect the first isolation pillar 41 and the second isolation pillar 42.

[0219] In some embodiments, before forming the second planar material layer PLN2', the preparation method further includes S11A to S11F, and specific product schematic diagrams are shown in Examples 1 to 7 above.

[0220] S11A, A driving layer 2 is formed on the substrate 1.

[0221] The driving layer 2 includes at least pixel driving circuits for driving light-emitting devices, such as various transistors, storage capacitors, gate lines, data lines, power lines, signal leads, etc.

[0222] S11B. An interlayer insulating layer (ILD) is formed on the side of the driving layer 2 facing away from the substrate 1 using a single patterning process (e.g., a single mask ILD process). The interlayer insulating layer ILD is made of inorganic material. It should be noted that etching inorganic materials is more difficult and not conducive to forming undercut structures.

[0223] S11C. A first conductive layer SD1 with a first signal line 51 and a first redundant trace 54 is formed by etching once through a patterning process (e.g., a mask SD1 Mask).

[0224] The first signal line 51 is located in the display area AA, and the first redundant trace 54 is located in the first isolation area BB1. The first conductive layer SD1 is a single-layer or multi-layer structure, such as a titanium / aluminum / titanium three-layer metal layer.

[0225] S11D: A passivation layer PVX is formed on the side of the first conductive layer SD1 away from the interlayer insulating layer ILD through a single patterning process (e.g., a PVX mask).

[0226] S11E, the pattern of the first planarization layer PLN1 is formed on the side of the passivation layer PVX away from the first conductive layer SD1 through a patterning process (e.g., a PLN1 Mask process).

[0227] The first flat layer PLN1 includes a third flat portion 83 extending from the display area AA to the first partition area BB1 and a third blocking portion 93 located in the second partition area BB2. The third blocking portion 93 is used to form part of the blocking dam 9.

[0228] S11F, a second conductive layer SD2 with a second signal line 52 is formed on the side of the first planarization layer PLN1 opposite to the passivation layer PVX through a single patterning process (e.g., a mask SD2 Mask process).

[0229] The second signal line 52 is located in the display area AA. The second conductive layer SD2 is a single-layer or multi-layer structure, such as a titanium / aluminum / titanium three-layer metal layer.

[0230] In some embodiments, after forming the third planarization layer PLN3 and before etching the second planarization material layer PLN2', the fabrication method further includes steps S13B to S13D, as shown in FIG20: S13B, forming the anode of the light-emitting device on the side of the third planarization layer PLN3 away from the third conductive layer SD3. S13C, forming a pixel-defining layer PDL on the side of the anode away from the third planarization layer PLN3 using a single patterning process (e.g., a single PDL mask process). The pixel-defining layer PDL includes a barrier structure located in the display area AA and a fourth blocking portion 94 located in the second partition area BB2. S13D, forming a pattern including a support portion PS on the side of the pixel-defining layer PDL away from the anode using a single patterning process (e.g., a single PS mask process).

[0231] Optionally, the support PS includes two parts, one of which serves as part of the retaining dam 9, and the other of which serves as part of the support structure 1021.

[0232] Both the pixel-limiting layer (PDL) and the support portion (PS) can be made of inorganic materials. The fourth blocking portion 94 and the support portion (PS) are both part of the blocking dam 9.

[0233] The above fabrication process can be summarized as follows: Substrate 1 → Driving layer 2 → Interlayer insulating layer ILD → First conductive layer SD1 → Passivation layer PVX → First planarization layer PLN1 → Second conductive layer SD2 → Second planarization material layer PLN2' → Third conductive layer SD3 (forming the first isolation pillar 41 and the second isolation pillar 42) → Third planarization layer PLN3 → Anode → Pixel limiting layer PDL → Support PS → Second conductive layer SD2 (forming the first groove 61) → Light emitting layer 2 → Cathode.

[0234] In some embodiments, FIG23 is a flowchart of another method for preparing a display panel provided in this disclosure. As shown in FIG23, before forming the third conductive layer SD3, S21 to S23 are further included. For specific product schematic diagrams, please refer to FIG5, FIG8 or FIG10.

[0235] S21. A third conductive material layer SD3' is formed on the side of the second flat material layer PLN2' away from the substrate 1. As shown in Figure 21b, the third conductive material layer SD3' includes multiple second redundant traces 55. The second redundant traces 55 here are not isolation pillar structures. Taking the titanium-aluminum-titanium three-layer as an example, the cross-section of the second redundant traces 55 is trapezoidal.

[0236] It should be noted that the cross-sections of the first signal line 51, the second signal line 52, and the third signal line 53 in this disclosure are all trapezoidal. The cross-section of the first redundant trace 54 is trapezoidal, and the cross-section of the second redundant trace 55 is trapezoidal in the first etching stage and "I" shaped in the second etching stage.

[0237] S22. A third planarization layer PLN3 is formed on the side of the third conductive material layer SD3' that is opposite to the second planarization material layer PLN2'. The third planarization layer PLN3 includes a first planar portion 81 located in the display area AA and a first blocking portion 91 located in the second isolation area BB2; the third planarization layer PLN3 exposes multiple second redundant traces 55 in the middle region between the first planar portion 81 and the first blocking portion 91.

[0238] S23. A pixel defining layer PDL and a support portion PS are sequentially formed on the side of the third planarization layer PLN3 opposite to the third conductive material layer SD3'. The pixel defining layer PDL exposes multiple second redundant traces 55. In particular, the pixel defining layer PDL exposes the second redundant traces 55 located in the second isolation region BB2. This avoids the problem of photoresist covering the sides of the second redundant traces 55, which would prevent the etching of the second isolation pillar 42. This is because the inventors discovered that, due to process conditions, if the distance between the pixel defining layer PDL and the edge of the second redundant traces 55 it covers is too short, the photoresist covering the second redundant traces 55 will be far away from the sides of the pixel defining layer PDL, thus preventing the subsequent etching of the second isolation pillar 42.

[0239] In S13, the formation of the third conductive layer SD3 includes: as shown in Figure 21c, S24, using a target mask, etching multiple second redundant traces 55, for example, wet etching, to form a first isolation pillar 41 located in the first isolation region BB1 and a second isolation pillar 42 located in the second isolation region BB2.

[0240] In S14, at least the second planar material layer PLN2' is etched to form a second planar layer PLN2 with a first groove 61, including: S25, as shown in FIG21d, using a target mask, using gas or plasma in a vacuum environment, the surface of the second planar material layer PLN2' exposed by the third planar layer PLN3 and the third conductive layer SD3 is etched to form the first groove 61; the first groove 61 and the straight line of the first isolation pillar 41 are separated to form the undercut structure 7.

[0241] Here, the processes for forming the second conductive layer SD2 and the third conductive layer SD3 are carried out continuously, and both use the same target mask, which can reduce process costs and improve fabrication efficiency.

[0242] The above fabrication process can be summarized as follows: Substrate 1 → Driving layer 2 → Interlayer insulating layer ILD → First conductive layer SD1 → Passivation layer PVX → First planarization layer PLN1 → Second conductive layer SD2 → Second planarization material layer PLN2' → Third conductive material layer SD3' → Third planarization layer PLN3 → Anode → Pixel limiting layer PDL → Support PS → Third conductive layer SD3 (forming the first isolation pillar 41 and the second isolation pillar 42) → Second conductive layer SD2 (forming the first groove 61) → Light emitting layer 2 → Cathode.

[0243] It should be noted that, unless otherwise stated, the term "same-layer arrangement" used in this disclosure means that two layers, components, elements, or parts can be formed by the same patterning process and are formed from the same material layer. Therefore, they are in the same layer in terms of layering relationship, but this does not mean that they are equidistant from the substrate, nor does it mean that they are completely identical to other layers between them and the substrate.

[0244] This disclosure also provides a display device comprising the display substrate described in any of the above embodiments. The display device can be, for example, any product with a display function such as a mobile phone, tablet computer, television, monitor, laptop computer, digital photo frame, or in-vehicle device. Other essential components of this display device are readily understood by those skilled in the art and will not be described in detail here, nor should they be construed as limiting the scope of this disclosure.

[0245] It is understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of this disclosure, and this disclosure is not limited thereto. For those skilled in the art, various modifications and improvements can be made without departing from the spirit and substance of this disclosure, and these modifications and improvements are also considered to be within the scope of protection of this disclosure.

Claims

1. A display panel having a display area, a partition area, and an opening area, the partition area being located between the display area and the opening area; the display panel comprising a substrate, and a second planarization layer, a third conductive layer, a light-emitting layer, and an electrode layer sequentially disposed along the direction of the substrate; The third conductive layer includes a plurality of isolation pillars located in the isolation region, the isolation pillars surrounding the opening region; the second planar layer has a first groove, and the orthographic projection of one side edge of at least one of the isolation pillars on the substrate falls into the orthographic projection of the first groove on the substrate; the first groove and the isolation pillars form an undercut structure for isolating the electrode layer falling into the first groove. The light-emitting layer extends from the display area to the partition area and is interrupted at least at the location of each of the partition pillars.

2. The display panel according to claim 1, wherein, The partition area includes a first partition area and a second partition area; the second partition area surrounds the opening area, and the first partition area surrounds the second partition area; The plurality of isolation columns include at least one first isolation column located in the first partition area and at least one second isolation column located in the second partition area; The first groove is located in the first isolation area, and the orthographic projection of one side edge of the first isolation pillar on the substrate falls into the orthographic projection of the first groove on the substrate; the first groove and the first isolation pillar form an undercut structure to isolate the electrode layer falling into the first groove.

3. The display panel according to claim 2, wherein, The display panel further includes a third planarization layer disposed on the side of the third conductive layer near the light-emitting layer; the third planarization layer includes a first planar portion located in the display area and a first blocking portion located in the second partition area; The third flat layer exposes the first isolation post, the first groove, and the second isolation post in the middle region between the first flat portion and the first blocking portion.

4. The display panel according to claim 3, wherein, The second flat layer includes a second flat portion extending from the display area to the first partition area and a second blocking portion located in the second partition area; A second groove is defined on the substrate between the second flat portion and the second isolation post closest to the first partition area.

5. The display panel according to claim 2, wherein, The first partition area is provided with a plurality of first isolation columns; a slot is defined between two adjacent first isolation columns and communicates with the first groove.

6. The display panel according to claim 5, wherein, The first partition area is provided with at least three first isolation columns, and two adjacent first isolation columns correspond to one first groove.

7. The display panel according to claim 5, wherein, Each of the first isolation pillars is flush with the surface of the substrate.

8. The display panel according to claim 5, wherein, The display panel also includes multiple first redundant traces located in the first partition area and respectively surrounding the opening area; The first redundant trace is provided in a one-to-one correspondence with the first isolation pillar, and the orthographic projection of the first isolation pillar on the substrate overlaps with the orthographic projection of the corresponding first redundant trace on the substrate.

9. The display panel according to claim 8, wherein, The display panel further includes a second conductive layer, a first planarization layer, and a first conductive layer sequentially disposed on the side of the second planarization layer opposite to the third conductive layer; The multiple first redundant traces are located in the first conductive layer or the second conductive layer.

10. The display panel according to claim 9, wherein, The materials of the third planarization layer, the second planarization layer, and the first planarization layer are all organic insulating materials.

11. The display panel according to claim 2, wherein, The third conductive layer also includes multiple signal lines located in the display area and at least one second redundant trace located in the first isolation area; The portion of the signal line near the aperture area partially surrounds the aperture area; the second redundant trace surrounds the aperture area, and the second redundant trace is multiplexed as the first isolation pillar.

12. The display panel according to claim 2, wherein, The third conductive layer also includes multiple third redundant traces located in the display area and in the first isolation area; The third redundant trace surrounds the opening area, and the third redundant trace is reused as the first isolation pillar.

13. The display panel according to claim 1, wherein, The partition area includes a first partition area and a second partition area; the second partition area surrounds the opening area, and the first partition area surrounds the second partition area; The plurality of isolation columns includes at least one third isolation column located in the second isolation zone; The first groove is located in the second isolation area, and the orthographic projection of one side edge of the third isolation pillar on the substrate falls into the orthographic projection of the first groove on the substrate; the first groove and the third isolation pillar form an undercut structure to isolate the electrode layer falling into the first groove.

14. The display panel according to claim 13, wherein, The display panel further includes a third planarization layer disposed on the side of the third conductive layer near the light-emitting layer; the third planarization layer includes a first planar portion extending from the display area to the first isolation area and a first blocking portion located in the second isolation area; The third flat layer exposes the third isolation pillar and the first groove in the middle region between the first flat portion and the first blocking portion.

15. The display panel according to claim 14, wherein, The display panel also includes a barrier dam located in the second partition area; The third isolation pillars include multiple pillars, and each of the third isolation pillars is located on the side of the barrier dam closer to the display area; a slot is defined between two adjacent third isolation pillars and communicates with the first groove.

16. The display panel according to claim 13, wherein, The display panel also includes a barrier dam located in the second partition area; The third isolation pillars include multiple pillars, which are distributed on both sides of the barrier dam, near and away from the display area.

17. The display panel according to claim 16, wherein, For the plurality of third isolation pillars located on the side of the barrier dam closer to the display area, a slot is defined between two adjacent third isolation pillars and communicates with a corresponding first groove; For the plurality of third isolation pillars located on the side of the barrier dam away from the display area, at least one set of two adjacent third isolation pillars defines a slot and communicates with a corresponding first groove.

18. The display panel according to claim 15 or 17, wherein, The orthographic projection of two adjacent third isolation pillars on the substrate covers the orthographic projection of the portion of the second planar layer used to form the first groove on the substrate. The third isolation column wraps around the side away from the slot, forming a portion of the second flat layer away from the edge of the first groove.

19. The display panel according to any one of claims 1 to 17, wherein, The display panel also includes an encapsulation layer disposed on the side of the electrode layer opposite to the light-emitting layer; The encapsulation layer extends from the display area to the partition area and covers the portion exposed by the electrode layer at the location of each of the partition pillars.

20. The display panel according to claim 19, wherein, The encapsulation layer includes a first inorganic encapsulation layer, an organic encapsulation layer, and a second inorganic encapsulation layer arranged sequentially along a direction away from the substrate; both the first inorganic encapsulation layer and the second inorganic encapsulation layer extend from the display area to the edge of the opening area; The display panel also includes a barrier dam disposed in the isolation area; the organic encapsulation layer extends from the display area to the isolation area and terminates at the side of the barrier dam closest to the display area.

21. The display panel according to claim 20, wherein, The display panel further includes a pixel defining layer and a support layer sequentially disposed on the third planar layer near the light-emitting layer; The pixel-defining layer and the support layer at least expose the barrier dam near the isolation pillar of the display area.

22. The display panel according to claim 20, wherein, The display panel also includes a support structure located on the side of the barrier dam away from the display area; the plurality of isolation columns include at least a plurality of second isolation columns; The support structure covers the surfaces of two adjacent second isolation pillars that are away from the substrate and fills the gap between the two adjacent second isolation pillars.

23. The display panel according to claim 20, wherein, The display panel also includes at least two support structures located on both sides of the barrier dam; the plurality of isolation columns include at least a second isolation column located on both sides of the barrier dam respectively; For any of the support structures, the support structure covers the surfaces of two adjacent second isolation pillars facing away from the substrate and fills the gap between the two adjacent second isolation pillars.

24. The display panel according to claim 1, wherein, The isolation pillar includes a first conductive portion, a second conductive portion, and a third conductive portion arranged sequentially along a direction away from the substrate, wherein the first conductive portion and the third conductive portion both protrude beyond the second conductive portion.

25. A method for manufacturing a display panel, used to manufacture a display panel as described in any one of claims 1 to 24; the display panel having a display area, a partition area, and an opening area; the partition area surrounding the opening area; wherein, The preparation method includes: Provide a substrate; A second planar material layer is formed on the substrate. A third conductive layer is formed on the side of the second planar material layer opposite to the substrate; the third conductive layer includes a plurality of isolation pillars located in the isolation region, the isolation pillars surrounding the opening region; At least the second planar material layer is etched to form a second planar layer with a first groove; the orthographic projection of one side edge of the isolation pillar on the substrate falls within the orthographic projection of the first groove on the substrate; the first groove and the isolation pillar form an undercut structure; A light-emitting layer and an electrode layer are sequentially formed on the side of the third conductive layer opposite to the second planar layer; the electrode layer is cut off at the location of the undercut structure; and the light-emitting layer is broken at least at the location of the isolation pillar.

26. The preparation method according to claim 25, wherein, After the formation of the third conductive layer and before etching the second planar material layer, the process further includes: A third flat layer is formed on the side of the third conductive layer opposite to the second flat material layer; the third flat layer exposes the isolation pillar and the first groove.

27. The preparation method according to claim 26, wherein, At least the second planar material layer is etched to form a second planar layer having a first groove, including: The first groove is formed by etching the surface of the second planar material layer exposed by the third planar layer and the third conductive layer in a vacuum environment using gas or plasma.

28. The preparation method according to claim 27, wherein, The material of the second planarization layer is an organic insulating material; the gas used to etch the second planarization layer is a mixture of carbon tetrafluoride and oxygen.

29. A display device comprising a display panel as claimed in any one of claims 1 to 24.