Injection molded body for moving body and method for producing injection molded body for moving body
By structuring the injection-molded body into five layers with alternating fiber orientations, the mechanical strength of automobile parts is enhanced through controlled fiber orientation in automobile parts made from thermoplastic resin.
Patent Information
- Application Number
- PCT/JP2026/010242
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-09
- Filing Date
- 2026-03-16
- Publication Date
- 2026-11-12
AI Technical Summary
Conventional injection molded articles for automobile parts made from thermoplastic resin with reinforcing fibers lack sufficient mechanical strength due to uneven orientation of reinforcing fibers in different layers.
The injection-molded body for a mobile body is structured into five layers with alternating orientation directions of reinforcing fibers, where odd-numbered layers have a primary orientation in the first direction and even-numbered layers in the second direction, achieved by supplying molten resin through gates oriented in different directions to control fiber orientation.
This configuration enhances the mechanical strength of the injection-molded body by ensuring continuous change in fiber orientation between layers, resulting in improved structural integrity.
Smart Images

Figure JP2026010242_12112026_PF_FP_ABST
Abstract
Description
Injection molded article for moving body and method for producing injection molded article for moving body
[0001] The present disclosure relates to an injection molded article for a moving body and a method for producing the injection molded article for a moving body.
[0002] Conventionally, there are automobile parts that are injection molded articles (see, for example, Patent Document 1). As shown in FIG. 5, a conventional injection molded article 110 including the one disclosed in Patent Document 1 is formed by injection-molding a molten thermoplastic resin 20 containing reinforcing fibers 21.
[0003] As shown in FIGS. 5 and 6, the injection molded article 110 is constituted by three layers 132, 131, 132 in which the main orientation directions of the reinforcing fibers 21 of adjacent layers differ by 90 degrees. As shown in FIGS. 7 and 8, when the molten thermoplastic resin 20 containing the reinforcing fibers 21 (hereinafter referred to as molten resin) is supplied into the cavity 153 of the mold 150 through the gate 151 oriented in the first direction X, a core layer 131 and skin layers 132 located between the core layer 131 and the molding surfaces of the cavity 153 are formed.
[0004] Here, in the skin layers 132, the reinforcing fibers 21 are likely to be oriented in the first direction X, which is the flow direction of the molten resin, because the skin layers 132 are easily affected by the molding surfaces of the cavity 153 having a temperature lower than that of the molten resin. As a result, the main orientation direction of the reinforcing fibers 21 in the skin layers 132 is the first direction X. In addition, in the core layer 131, the reinforcing fibers 21 are likely to be oriented in a direction orthogonal to both the flow direction of the molten resin and the thickness direction Z, so the main orientation direction of the reinforcing fibers 21 in the core layer 131 is the second direction Y.
[0005] International Publication No. 2020 / 148563
[0006] Further improvement in mechanical strength is required for injection molded articles.
[0007] According to one aspect of the present disclosure, an injection-molded body for a mobile body made of a thermoplastic resin containing reinforcing fibers is provided. The direction perpendicular to the thickness direction of the injection-molded body for a mobile body is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction. The injection-molded body for a mobile body consists of five layers that overlap in the thickness direction. The first direction is the principal orientation direction of the reinforcing fibers in the odd-numbered layers from one side of the thickness direction, and the second direction is the principal orientation direction of the reinforcing fibers in the even-numbered layers from one side of the thickness direction. The orientation tensor of the reinforcing fibers in the first direction and the orientation tensor of the second direction change continuously between adjacent layers.
[0008] According to another aspect of the present disclosure, a method is provided for manufacturing an injection-molded article for a mobile body by supplying a molten thermoplastic resin containing reinforcing fibers into the cavity of a mold. The direction perpendicular to the thickness direction of the cavity is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction. The method for manufacturing the injection-molded article for a mobile body comprises: a first step of supplying the molten thermoplastic resin containing the reinforcing fibers into the cavity through a first gate oriented in the first direction to form a first core layer and a first skin layer located between the first core layer and the molding surface of the cavity, wherein the main orientation direction of the reinforcing fibers is the first direction; and a second step of supplying the molten thermoplastic resin containing the reinforcing fibers into the cavity through a second gate oriented in the second direction to flow the molten first core layer and the molten portion of the first skin layer adjacent to the first core layer in the second direction, thereby forming a second core layer where the main orientation direction of the reinforcing fibers is the first direction, and a second skin layer located between the second core layer and the first skin layer, wherein the main orientation direction of the reinforcing fibers is the second direction.
[0009] Figure 1 is a cross-sectional view showing the layer structure of an injection-molded body for a mobile body according to one embodiment. Figure 2 is a graph showing the relationship between the position in the thickness direction of the injection-molded body in Figure 1 and each orientation tensor. Figure 3 is a cross-sectional view of a mold for molding the injection-molded body in Figure 1. Figure 4A is a cross-sectional view showing the state of the molten resin inside the mold in Figure 3 during the first step, and Figure 4B is a cross-sectional view showing the state of the molten resin inside the mold in Figure 3 during the second step. Figure 5 is a cross-sectional view showing the layer structure of a conventional injection-molded body. Figure 6 is a graph showing the relationship between the position in the thickness direction of the injection-molded body in Figure 5 and each orientation tensor. Figure 7 is a cross-sectional view of a mold for molding the injection-molded body in Figure 5. Figure 8 is a cross-sectional view showing the state of the inside of the mold in Figure 7.
[0010] An embodiment will be described below with reference to Figures 1 to 4B. <Configuration of the injection-molded body> As shown in Figure 1, the injection-molded body for the mobile body (hereinafter referred to as the injection-molded body 10) is made of a thermoplastic resin (hereinafter referred to as the resin 20) containing reinforcing fibers 21.
[0011] The resin 20 is, for example, polypropylene. The reinforcing fiber 21 is, for example, glass fiber. In the following description, the thickness direction of the injection-molded body 10 (vertical direction in Figure 1) will be referred to as the thickness direction Z, the direction perpendicular to the thickness direction Z (horizontal direction in Figure 1) will be referred to as the first direction X, and the direction perpendicular to both the thickness direction Z and the first direction X (orthogonal direction to the plane of the paper in Figure 1) will be referred to as the second direction Y.
[0012] The injection-molded body 10 consists of five overlapping layers 11, 12, 13, 12, and 11 in the thickness direction Z. More specifically, the injection-molded body 10 has first skin layers 11 located at both ends in the thickness direction Z, second skin layers 12 adjacent to the inside of the first skin layers 11 in the thickness direction Z, and second core layers 13 located between the second skin layers 12.
[0013] The primary orientation direction of the reinforcing fibers 21 in the first skin layer 11 and the second core layer 13 is the first direction X. That is, among the five layers 11, 12, 13, 12, 11, the primary orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11 and 13 from one side of the thickness direction Z is the first direction X.
[0014] The primary orientation direction of the reinforcing fibers 21 in the second skin layer 12 is the second direction Y. That is, among the five layers 11, 12, 13, 12, 11, the primary orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 from one side of the thickness direction Z is the second direction Y.
[0015] Figure 2 shows the relationship between the thickness direction position (mm) of the injection-molded body 10, which is the position in the thickness direction Z, and the orientation tensor Ax in the first direction X, the orientation tensor Ay in the second direction Y, and the orientation tensor Az in the thickness direction Z. At any thickness direction position, the sum of the orientation tensors Ax, Ay, and Az is 1.
[0016] As shown in Figure 2, in the first skin layer 11 on the far left of Figure 2, the orientation tensor Ax in the first direction X is larger than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, as we approach the second skin layer 12 in the thickness direction Z, the orientation tensor Ax in the first direction X decreases sharply, while the orientation tensor Ay in the second direction Y increases sharply.
[0017] In the second skin layer 12, the second from the left in Figure 2, the orientation tensor Ay in the second direction Y is greater than the orientation tensor Ax in the first direction X and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ay in the second direction Y increases sharply with increasing position in the thickness direction, and then gradually decreases as it approaches the second core layer 13 in the thickness direction. On the other hand, the orientation tensor Ax in the first direction X decreases sharply with increasing position in the thickness direction, and then gradually increases as it approaches the second core layer 13 in the thickness direction.
[0018] In the second core layer 13, the orientation tensor Ax in the first direction X is greater than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ax in the first direction X gradually increases with increasing position in the thickness direction, and then gradually decreases as it approaches the second core layer 13 in the thickness direction. On the other hand, the orientation tensor Ay in the second direction Y gradually decreases with increasing position in the thickness direction, and then gradually increases as it approaches the second skin layer 12, the second from the right in Figure 2, in the thickness direction.
[0019] In the second skin layer 12, the second from the right in Figure 2, the orientation tensor Ay in the second direction Y is greater than the orientation tensor Ax in the first direction X and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ay in the second direction Y gradually increases with increasing position in the thickness direction, and then decreases sharply as the position in the thickness direction approaches the rightmost first skin layer 11. On the other hand, the orientation tensor Ax in the first direction X gradually decreases with increasing position in the thickness direction, and then increases sharply as the position in the thickness direction approaches the rightmost first skin layer 11.
[0020] In the first skin layer 11 on the far right of Figure 2, the orientation tensor Ax in the first direction X is greater than the orientation tensor Ay in the second direction Y and the orientation tensor Az in the thickness direction Z. Furthermore, the orientation tensor Ax in the first direction X gradually increases with increasing position in the plate thickness direction, while the orientation tensor Ay in the second direction Y gradually decreases with increasing position in the plate thickness direction.
[0021] As explained above, the orientation tensor Ax in the first direction X and the orientation tensor Ay in the second direction Y of the reinforcing fiber 21 change continuously between adjacent layers 11, 12, 13, 12, 11.
[0022] <Method for Manufacturing Injection Molded Articles> Next, a method for manufacturing injection molded articles 10 will be described with reference to Figures 3, 4A, and 4B. The method for manufacturing injection molded articles 10 involves supplying a molten thermoplastic resin containing reinforcing fibers 21 (hereinafter referred to as molten resin) to the cavity 53 of a mold 50.
[0023] As shown in Figure 3, the mold 50 for molding the injection-molded body 10 has a cavity 53. In the following explanation, the thickness direction of the cavity 53 (the direction perpendicular to the plane of the paper in Figure 3) will be referred to as the thickness direction Z, the direction perpendicular to the thickness direction Z (the left-right direction in Figure 3) will be referred to as the first direction X, and the direction perpendicular to both the thickness direction Z and the first direction X (the up-down direction in Figure 3) will be referred to as the second direction Y.
[0024] The mold 50 has a first gate 51 that points in a first direction X and a second gate 52 that points in a second direction Y. The first gate 51 is provided in multiple locations, for example, at one end of the cavity 53 in the first direction X (the left end in Figure 3), spaced apart from each other in the second direction Y. In this embodiment, three first gates 51 are provided.
[0025] The second gate 52 opens, for example, in the center of the cavity 53 in the first direction X and the center in the second direction Y. The method for manufacturing the injection molded body 10 comprises a first step and a second step.
[0026] <First Step> As shown by the white arrow in Figure 3, in the first step, molten resin is supplied to the cavity 53 through the first gate 51. This forms the first core layer 31 and the first skin layer 32, which is located between the first core layer 31 and the molding surface of the cavity 53, and in which the main orientation direction of the reinforcing fibers 21 is the first direction X, as shown in Figure 4A.
[0027] Once the first process is complete, the supply of molten resin is stopped by closing the first gate 51. <Second Process> The second process is performed after the first process.
[0028] As shown by the black arrow in Figure 3, in the second step, molten resin is supplied to the cavity 53 through the second gate 52. This causes the molten first core layer 31 and the molten portion of the first skin layer 32 adjacent to the first core layer 31 to flow in the second direction Y, as shown in Figure 4B, thereby forming a second core layer 13 in which the main orientation direction of the reinforcing fibers 21 is the first direction X, and a second skin layer 12 located between the second core layer 13 and the first skin layer 32 (11), in which the main orientation direction of the reinforcing fibers 21 is the second direction Y.
[0029] <Operation of this embodiment> In the injection-molded body 10, the primary orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11 and 13 is the first direction X, and the primary orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 is the second direction Y. That is, the primary orientation directions of adjacent layers 11, 12, 13, 12, 11 are 90 degrees apart from each other. Furthermore, the injection-molded body 10 does not have an adhesive layer that bonds the layers 11, 12, 13, 12, 11 together but does not contain the reinforcing fibers 21. In other words, the reinforcing fibers 21 are present throughout the entire thickness direction Z of the injection-molded body 10.
[0030] <Effects of this embodiment> (1) The injection-molded body 10 consists of five layers 11, 12, 13, 12, 11 that overlap in the thickness direction Z. Of the five layers 11, 12, 13, 12, 11, the main orientation direction of the reinforcing fibers 21 in the odd-numbered layers 11 and 13 from one side of the thickness direction Z is the first direction X, and the main orientation direction of the reinforcing fibers 21 in the even-numbered layer 12 from one side of the thickness direction Z is the second direction Y. The orientation tensor Ax of the first direction X and the orientation tensor Ay of the second direction Y of the reinforcing fibers 21 change continuously between adjacent layers.
[0031] With this configuration, the above-mentioned effects are achieved, and the mechanical strength of the injection-molded body 10 can be improved. (2) The method for manufacturing the injection-molded body 10 comprises a first step and a second step.
[0032] In this method, in the first step, molten resin is supplied to the cavity 53 through a first gate 51 oriented in a first direction X. This forms a first core layer 31 and a first skin layer 32 located between the first core layer 31 and the molded surface of the cavity 53. In the first skin layer 32, the reinforcing fibers 21 tend to orient in the first direction X, which is the flow direction of the molten resin, because they are easily influenced by the molded surface of the cavity 53, which is at a lower temperature than the molten resin. As a result, the main orientation direction of the reinforcing fibers 21 in the first skin layer 32 is the first direction X. In the first core layer 31, the reinforcing fibers 21 tend to orient in a direction perpendicular to both the flow direction and the thickness direction Z of the molten resin, so the main orientation direction of the reinforcing fibers 21 in the first core layer 31 is the second direction Y.
[0033] Next, in the second step, molten resin is supplied to the cavity 53 through a second gate 52 that is oriented in the second direction Y, which is perpendicular to the thickness direction Z and the first direction X. As a result, the molten first core layer 31 and the molten portion of the first skin layer 32 adjacent to the first core layer 31 flow in the second direction Y, forming a second core layer 13 and a second skin layer 12 located between the second core layer 13 and the first skin layer 11. In the second skin layer 12, the reinforcing fibers 21 tend to orient in the second direction Y, which is the flow direction of the molten resin, because they are easily influenced by the relatively lower temperature of the first skin layer 32 (11). Consequently, the main orientation direction of the reinforcing fibers 21 in the second skin layer 12 is the second direction Y. In the second core layer 13, the reinforcing fibers tend to orient in a direction perpendicular to both the flow direction of the molten resin and the thickness direction Z, so the main orientation direction of the reinforcing fibers 21 in the second core layer 13 is the first direction X.
[0034] Therefore, the injection molded body 10 described in (1) above can be manufactured. <Modification> This embodiment can be implemented with the following modifications. This embodiment and the following modifications can be combined with each other to the extent that they are not technically contradictory.
[0035] The number of first gates 51 in the mold 50 is not limited to three; it may be two or fewer, or four or more. Also, if three or more first gates 51 are provided, the multiple first gates 51 do not necessarily need to be arranged at equal intervals.
[0036] The second gate 52 is not limited to one that opens in the center of the cavity 53 in the first direction X and in the center of the second direction Y. In addition to, or instead of, the second gate 52 in the above embodiment may be provided at least one of the two ends of the second direction Y, as shown by the dashed line in Figure 3.
[0037] - The reinforcing fiber 21 is not limited to glass fiber. The reinforcing fiber 21 may be carbon fiber or aramid resin. - The resin 20 is not limited to polypropylene. Any thermoplastic resin may be used, such as polyethylene terephthalate.
Claims
1. An injection-molded body for a mobile body made of thermoplastic resin containing reinforcing fibers, wherein the direction perpendicular to the thickness direction of the injection-molded body for a mobile body is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, the injection-molded body for a mobile body consists of five layers that overlap in the thickness direction, the primary orientation direction of the reinforcing fibers in the odd-numbered layers from one side of the thickness direction is the first direction, the primary orientation direction of the reinforcing fibers in the even-numbered layers from one side of the thickness direction is the second direction, and the orientation tensor of the reinforcing fibers in the first direction and the orientation tensor of the second direction change continuously between adjacent layers.
2. A method for manufacturing an injection-molded body for a mobile body by supplying a molten thermoplastic resin containing reinforcing fibers to the cavity of a mold, wherein the direction perpendicular to the thickness direction of the cavity is defined as the first direction, and the direction perpendicular to both the thickness direction and the first direction is defined as the second direction, the first step is to supply the molten thermoplastic resin containing the reinforcing fibers to the cavity through a first gate oriented in the first direction, thereby forming a first core layer and a first skin layer located between the first core layer and the molding surface of the cavity, wherein the main orientation direction of the reinforcing fibers is the first direction. A method for manufacturing an injection-molded article for a mobile body, comprising: a second step of supplying the molten thermoplastic resin containing the reinforcing fibers to the cavity through a second gate oriented in the second direction, thereby causing the molten first core layer and the molten portion of the first skin layer adjacent to the first core layer to flow in the second direction, thereby forming a second core layer in which the main orientation direction of the reinforcing fibers is the first direction, and a second skin layer located between the second core layer and the first skin layer, in which the main orientation direction of the reinforcing fibers is the second direction.